Inductor core loss detection method and system
By irradiating the inductor core with incident rays and generating reflected ray images, the problem of slicing the inductor core for loss detection is solved, realizing non-destructive testing and real-time loss assessment, reducing costs and supporting periodic performance sampling inspections of in-service cores.
Patent Information
- Application Number
- CN202511643993.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-11
- Publication Date
- 2026-02-06
AI Technical Summary
In existing technologies, inductor core loss testing requires slicing or grinding into powder, which renders the core unusable after testing, increases costs, and makes it difficult to achieve non-destructive performance evaluation.
An inductor core is irradiated with incident rays and reflected rays are received to generate a reflected ray image. The real-time total loss is evaluated in a non-contact manner, including adjusting the incident angle and using low-energy and medium-energy rays to generate low-energy, medium-energy, and inner-layer reflected images, and the surface and internal losses are evaluated respectively.
It enables non-destructive testing, allowing the magnetic core to continue to be used, reducing testing costs, supporting regular performance sampling of in-service inductor magnetic cores, avoiding equipment downtime losses, and providing real-time loss assessment and fault warning.
Smart Images

Figure CN121476248A_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of material performance testing technology, and in particular to a method and system for detecting the loss of inductor cores. Background Technology
[0002] An inductor is a passive electronic component in a circuit used to store magnetic field energy and impede changes in current. It is widely used in filtering, energy storage, choking, and resonance applications. An inductor mainly consists of three parts: a coil, a magnetic core, and auxiliary structures (framework, shielding, etc.). Among these, the performance of the magnetic core directly determines the overall efficiency and stability of the inductor.
[0003] During the use of inductor cores, inductor cores will generate losses, and the loss characteristics of inductor cores will change with operating conditions. Currently, the loss detection of inductor cores is usually carried out by X-ray diffraction or scanning with electron microscopy. However, both X-ray diffraction and electron microscopy scanning methods require the inductor core to be sliced or ground into powder, which makes the cores after testing unusable in actual use. This not only increases the testing cost, but also makes it difficult to achieve non-destructive performance evaluation of in-service inductor cores. Summary of the Invention
[0004] This application provides a method and system for detecting the loss of inductor cores, which can solve the problem that existing X-ray diffraction and electron microscopy scanning methods require slicing or grinding the inductor core into powder, resulting in the cores after testing being unable to continue to be used in practice. This not only increases the testing cost, but also makes it difficult to achieve non-destructive performance evaluation of in-service inductor cores.
[0005] In a first aspect, this application provides a method for detecting inductor core loss, including: The inductor core is irradiated with incident rays, and the reflected rays reflected by the inductor core are received. Generate a reflected ray image based on the reflected ray; The real-time total loss of the inductor core is evaluated based on the reflected ray image. In some embodiments, In some embodiments, irradiating the inductor core with incident rays and receiving reflected rays reflected by the inductor core includes: The inductor core is irradiated with incident rays, and the incident angle of the incident rays is adjusted. Receive the angle-reflected rays from the inductor core at the incident angle; The incident angle is obtained based on the average intensity of the reflected rays at the angle. The inductor core is illuminated based on the detected incident angle, and the reflected rays reflected by the inductor core are received.
[0006] In some embodiments, the reflected rays include low-energy reflected rays and medium-energy reflected rays; The process of illuminating the inductor core based on the detected incident angle and receiving the reflected rays reflected by the inductor core includes: Based on the detected incident angle, the inductor core is irradiated with low-energy rays, and the low-energy reflected rays reflected by the inductor core are received. The inductor core is irradiated with medium-energy rays based on the detected incident angle, and the medium-energy reflected rays reflected by the inductor core are received.
[0007] In some embodiments, the reflected ray image includes a low-energy reflected image, a medium-energy reflected image, and an inner layer reflected image; The generation of the reflected ray image based on the reflected ray includes: The low-energy reflection image is generated based on the low-energy reflection ray; The medium-energy reflection image is generated based on the medium-energy reflection ray; The difference in surface reflection is obtained based on the penetrating power of the low-energy rays and the medium-energy rays; The inner layer reflection image is obtained based on the surface reflection difference, the low-energy reflection image, and the medium-energy reflection image.
[0008] In some embodiments, generating a low-energy reflection image based on the low-energy reflection ray specifically involves: Receive the low-energy reflected rays and generate a low-energy electrical signal based on the low-energy reflected rays; The low-energy reflection image is generated based on the low-energy electrical signal; The generation of the medium-energy reflection image based on the medium-energy reflection ray specifically involves: Receive the medium-energy reflected rays and generate a medium-energy electrical signal based on the medium-energy reflected rays; The medium-energy reflection image is generated based on the medium-energy electrical signal.
[0009] In some embodiments, evaluating the real-time total loss of the inductor core based on the reflected ray image includes: The real-time surface loss of the inductor core is evaluated based on the low-energy reflection image. The internal real-time loss of the inductor core is evaluated based on the reflection image of the inner layer. The real-time total loss of the inductor core is obtained based on the surface real-time loss and the internal real-time loss.
[0010] In some embodiments, the low-energy reflection image includes a low-energy reflection intensity image and a low-energy reflection density image; The evaluation of the real-time surface loss of the inductor core based on the low-energy reflection image includes: The degree of surface grain growth of the inductor core is evaluated based on the low-energy reflection intensity image. The degree of surface ion migration of the inductor core is evaluated based on the low-energy reflection density image. The real-time surface loss of the inductor core is obtained based on the degree of surface grain growth and the degree of surface ion migration.
[0011] In some embodiments, evaluating the internal real-time loss of the inductor core based on the inner layer reflection image includes: Based on the reflection image of the inner layer, the internal reflection image of the inductor core is evaluated using the corresponding model of the inner and outer structures; The real-time loss of the inner layer of the inductor core is evaluated based on the inner layer reflection image. The real-time loss of the inner layer of the inductor core is evaluated based on the inner layer reflection image. The internal real-time loss is obtained based on the real-time loss of the inner layer and the real-time loss of the inner layer.
[0012] In some embodiments, the inner layer reflection image includes an inner layer reflection intensity image and an inner layer reflection density image; The method of evaluating the real-time loss of the inner layer of the inductor core based on the inner layer reflection image includes: The degree of inner layer grain growth of the inductor core is evaluated based on the inner layer reflection intensity image. The degree of ion migration in the inner layer of the inductor core is evaluated based on the inner layer reflectance density image. The real-time loss of the inner layer is obtained based on the degree of grain growth and the degree of ion migration in the inner layer.
[0013] Secondly, this application provides an inductor core loss detection system, comprising: An X-ray irradiation module is used to irradiate the inductor core with incident rays and to receive reflected rays reflected by the inductor core; An image generation module is used to generate a reflected ray image based on the reflected ray; A loss assessment module is used to assess the real-time total loss of the inductor core based on the reflected ray image.
[0014] The technical solutions provided in this application have the following advantages compared with the prior art: The inductor core loss detection method and system provided in this application embodiment irradiate the inductor core with incident rays and receive the reflected rays reflected by the inductor core; generate a reflected ray image based on the reflected rays; and evaluate the real-time total loss of the inductor core based on the reflected ray image. Through a non-contact method of "incident ray irradiation + reflected ray imaging," the original structure and integrity of the core are not damaged. The core does not need to be disassembled or cut during the detection process, and can be directly reinstalled into the circuit for continued use after the detection is completed, significantly reducing detection costs (no additional spare cores are required). It also supports periodic performance sampling inspections of in-service inductor cores, avoiding equipment downtime losses due to destructive testing. This solves the problem that existing X-ray diffraction and electron microscopy methods require slicing or grinding the inductor core into powder, rendering the tested core unusable, increasing detection costs, and making it difficult to achieve non-destructive performance evaluation of in-service inductor cores. Attached Figure Description
[0015] The accompanying drawings, which are incorporated in and form part of this specification, illustrate embodiments consistent with the invention and, together with the description, serve to explain the principles of the invention.
[0016] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, for those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0017] One or more embodiments are illustrated by way of example with reference numerals in the accompanying drawings. These illustrations do not constitute a limitation on the embodiments. Elements with the same reference numerals in the drawings are denoted as similar elements. Unless otherwise stated, the figures in the drawings are not to be limited by scale.
[0018] Figure 1 A flowchart of an inductor core loss detection method provided in an embodiment of this application; Figure 2 This is a schematic diagram of the structure of an inductor core loss detection system provided in an embodiment of this application. Detailed Implementation
[0019] To make the objectives, technical solutions, and advantages of the embodiments of this application clearer, the technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.
[0020] The following disclosure provides numerous different embodiments or examples for implementing various structures of the invention. To simplify the disclosure, specific examples of components and arrangements are described below. These are merely examples and are not intended to limit the scope of the invention. Furthermore, reference numerals and / or letters may be repeated in different examples. Such repetition is for simplification and clarity and does not in itself indicate a relationship between the various embodiments and / or arrangements discussed.
[0021] An inductor is a passive electronic component in a circuit used to store magnetic field energy and impede changes in current. It is widely used in filtering, energy storage, choking, and resonance applications. Its performance is determined by key parameters such as inductance, DC resistance, and rated current. Among these, the performance of the magnetic core directly determines the overall efficiency and stability of the inductor.
[0022] During the use of inductor cores (such as ferrite cores, manganese-zinc ferrite cores, etc.), inductor cores will generate losses, and the loss characteristics of inductor cores will change with operating conditions. Currently, the loss detection of inductor cores is usually carried out by X-ray diffraction or scanning with an electron microscope. However, both X-ray diffraction and electron microscopy scanning methods require the inductor core to be sliced or ground into powder, which makes the cores after testing unusable in actual use. This not only increases the testing cost, but also makes it difficult to achieve non-destructive performance evaluation of in-service inductor cores.
[0023] Firstly, such as Figure 1 As shown, to address the aforementioned technical problems, this application provides a method for detecting inductor core loss, including: S101: Irradiate the inductor core with incident rays and receive the reflected rays reflected by the inductor core; S102: Generate a reflected ray image based on the reflected ray; S103: Evaluate the real-time total loss of the inductor core based on the reflected ray image.
[0024] It should be noted that traditional X-ray diffraction and electron microscopy scanning methods require slicing or powdering the inductor core, rendering it completely unusable after testing. However, the embodiments of this application utilize a non-contact method of "incident X-ray irradiation + reflected X-ray imaging," which avoids damaging the original structure and integrity of the core. The core does not need to be disassembled or cut during testing, and can be directly reinstalled into the circuit for continued use after testing, significantly reducing testing costs (eliminating the need for additional spare cores). It also supports periodic performance sampling inspections of in-service inductor cores, avoiding equipment downtime losses due to destructive testing. Furthermore, traditional testing requires removing the core from the circuit... Offline analysis after disassembly cannot reflect the loss state of the magnetic core under actual working conditions (such as dynamic current and real-time temperature), resulting in a "disconnect between detection results and actual operating conditions". The method provided in this application embodiment can directly detect the magnetic core of the inductor in operation in the circuit. The incident rays can penetrate the surface of the magnetic core and capture the microstructural changes related to real-time loss (such as differences in reflected signals caused by grain distortion and ion migration). The reflected ray image is then quickly mapped to total loss data, realizing real-time linkage evaluation of "operating conditions and loss", providing dynamic data support for inductor fault early warning and life prediction.
[0025] In some embodiments, irradiating the inductor core with incident rays and receiving reflected rays reflected by the inductor core includes: The inductor core is irradiated with incident rays, and the incident angle of the incident rays is adjusted. Receive the angle-reflected rays from the inductor core at the incident angle; The incident angle is obtained based on the average intensity of the reflected rays at the angle. The inductor core is illuminated based on the detected incident angle, and the reflected rays reflected by the inductor core are received.
[0026] It should be noted that the interaction between the rays and the internal microstructures of the magnetic core (such as grains and defects) differs under different incident angles, resulting in significant differences in the intensity and information content of the reflected signal. By following the process of "adjusting the incident angle - receiving the reflected rays at the angle - calculating the average intensity - determining the detection incident angle," the angle with the optimal average intensity of the reflected signal (usually a lower average intensity) can be selected. At this angle, the rays can interact more efficiently with the key structures inside the magnetic core that affect loss (such as magnetic domain boundaries, grain boundaries, and ion migration traces), making the "loss-related information" contained in the reflected rays richer. This avoids weak signals or missing information due to improper angles, laying the foundation for generating clear reflected ray images and accurately assessing the total loss.
[0027] It should be noted that if random angle illumination is used directly, the incident angle will be inconsistent in different detection scenarios (such as different batches of magnetic cores or different detection periods of the same magnetic core), which will lead to large fluctuations in the intensity of reflected signals and make the detection results incomparable. By "determining the detection incident angle", a unified optimal angle standard can be provided for each detection, ensuring that the reflected ray signal acquisition environment is consistent under different conditions and reducing the error caused by angle fluctuations.
[0028] In some embodiments, the reflected rays include low-energy reflected rays and medium-energy reflected rays; The process of illuminating the inductor core based on the detected incident angle and receiving the reflected rays reflected by the inductor core includes: Based on the detected incident angle, the inductor core is irradiated with low-energy rays, and the low-energy reflected rays reflected by the inductor core are received. The inductor core is irradiated with medium-energy rays based on the detected incident angle, and the medium-energy reflected rays reflected by the inductor core are received.
[0029] It should be noted that low-energy rays have weak penetrating power (such as X-rays <10keV) and can only act on the surface of the magnetic core (usually <0.1mm deep). Their reflected signals can accurately reflect the surface state of the magnetic core, such as local ion migration and grain distortion. Medium-energy rays have moderate penetrating power (such as X-rays 10-50keV) and can penetrate to the shallow layer of the magnetic core (usually 0.1-1mm deep). Their reflected signals can capture microscopic changes inside the shallow layer, such as grain growth and local ion migration (these are the core causes of increased hysteresis loss and eddy current loss in the magnetic core). Combining the two can avoid the detection blind spots of single-energy rays. It will not miss key changes inside the shallow layer due to using only low-energy rays, nor will it ignore the impact of the surface state on the overall loss due to using only medium-energy rays (such as surface oxidation increasing additional contact resistance loss).
[0030] It should be noted that, since the surface layer of the inductor core is in direct contact with the external environment, changes in its microstructure are usually different from changes in the microstructure inside the inductor core. Therefore, it is necessary to separately detect the surface layer of the inductor core. Among these, the signal intensity of low-energy reflected rays is more sensitive to "surface ion distribution and grain growth" (e.g., surface Fe). 3+ / Fe 2+ The proportional change is directly related to the surface oxidation loss); the signal intensity of medium-energy reflected rays is more sensitive to the "shallow crystal plane integrity", and the state of shallow grains and ions can be inferred from the signal peak shape and intensity changes.
[0031] In some embodiments, the reflected ray image includes a low-energy reflected image, a medium-energy reflected image, and an inner layer reflected image; The generation of the reflected ray image based on the reflected ray includes: The low-energy reflection image is generated based on the low-energy reflection ray; The medium-energy reflection image is generated based on the medium-energy reflection ray; The difference in surface reflection is obtained based on the penetrating power of the low-energy rays and the medium-energy rays; The inner layer reflection image is obtained based on the surface reflection difference, the low-energy reflection image, and the medium-energy reflection image.
[0032] It should be noted that low-energy rays, due to their shallow penetration, produce images primarily composed of surface signals. While medium-energy rays penetrate to the interior, their images still contain some surface reflection signals. Directly analyzing the interior using the medium-energy reflection images would introduce errors. Based on the difference in penetration ability between low-energy and medium-energy rays, a "reflection signal component belonging only to the surface" (i.e., surface reflection difference) can be calculated. This component is then removed from the medium-energy reflection image, ultimately yielding a "pure internal signal image without surface interference" (inner-surface reflection image). For example, if there is slight oxidation on the surface of the magnetic core, the low-energy image will show abnormal signals, and the medium-energy image will also exhibit slight fluctuations due to the oxide layer. The inner-surface reflection image can eliminate this interference, clearly revealing whether there is grain distortion caused by thermal aging inside, thus avoiding misjudging surface losses as internal losses.
[0033] In some embodiments, generating a low-energy reflection image based on the low-energy reflection ray specifically involves: Receive the low-energy reflected rays and generate a low-energy electrical signal based on the low-energy reflected rays; The low-energy reflection image is generated based on the low-energy electrical signal; The generation of the medium-energy reflection image based on the medium-energy reflection ray specifically involves: Receive the medium-energy reflected rays and generate a medium-energy electrical signal based on the medium-energy reflected rays; The medium-energy reflection image is generated based on the medium-energy electrical signal.
[0034] It should be noted that low-energy reflected rays (such as <10keV X-rays) can be received by low-energy dedicated detectors (such as silicon PIN detectors), while medium-energy reflected rays (such as 10-50keV X-rays) can be received by medium-energy dedicated detectors (such as CdTe detectors). This avoids signal distortion caused by mismatch in detector energy response (e.g., low-energy detectors have low sensitivity to medium-energy rays, which can naturally filter out medium-energy signal interference). After receiving the rays, a unified analog-to-digital conversion (AD conversion) and image reconstruction algorithm (such as grayscale mapping based on ray intensity) are used to ensure that ray signals of the same intensity correspond to the same image grayscale value. This ensures the comparability of detection images of different energies and batches, and avoids analysis errors caused by inconsistent conversion standards.
[0035] In some embodiments, evaluating the real-time total loss of the inductor core based on the reflected ray image includes: The real-time surface loss of the inductor core is evaluated based on the low-energy reflection image. The internal real-time loss of the inductor core is evaluated based on the reflection image of the inner layer. The real-time total loss of the inductor core is obtained based on the surface real-time loss and the internal real-time loss.
[0036] It should be noted that the real-time surface loss is calculated solely based on low-energy reflection images (exclusive surface signals) to avoid internal signal interference; the real-time internal loss is calculated solely based on inner-layer reflection images (pure internal signals) to exclude surface interference. Both types of losses are calculated based on "pure signals without impurities," resulting in higher accuracy when evaluated separately. The total real-time loss is obtained by directly summing "surface loss + internal loss," rather than indirectly calculating it based on a single signal. This makes the calculation logic more direct, and the results more closely reflect the actual working state of the magnetic core (e.g., surface loss 5W, internal loss 20W, total loss 25W, the value can be directly compared with the loss threshold of the circuit design).
[0037] In some embodiments, the low-energy reflection image includes a low-energy reflection intensity image and a low-energy reflection density image; The evaluation of the real-time surface loss of the inductor core based on the low-energy reflection image includes: The degree of surface grain growth of the inductor core is evaluated based on the low-energy reflection intensity image. The degree of surface ion migration of the inductor core is evaluated based on the low-energy reflection density image. The real-time surface loss of the inductor core is obtained based on the degree of surface grain growth and the degree of surface ion migration.
[0038] It should be noted that the low-energy reflection intensity image is sensitive to changes in grain size (fine grains have low reflection intensity and wide peaks, while coarse grains have high reflection intensity and narrow peaks). The surface grain size (e.g., growing from an initial 5μm to 8μm) can be directly calculated using the peak shape parameters (e.g., peak height, half-width at half-maximum) of the intensity image. Grain growth leads to increased resistance to the movement of surface magnetic domain walls, directly increasing hysteresis loss. The low-energy reflection density image reflects the uniformity of surface ion distribution (ion migration leads to a decrease in local ion density, corresponding to a decrease in image grayscale value). The degree of ion migration can be quantified by the difference in grayscale distribution of the density image (e.g., a 20% decrease in ion density in a local area). Ion migration disrupts the integrity of the surface lattice, increases the resistance of the eddy current path, and leads to an increase in eddy current loss.
[0039] It should be noted that the low-energy reflection intensity image specifically reflects grain growth (unaffected by ion migration), and the low-energy reflection density image specifically reflects ion migration (unaffected by grain size). After the two are quantized independently, the total loss can be calculated through a preset "micro-loss" correlation model (such as surface real-time loss = grain growth loss coefficient × grain size change + ion migration loss coefficient × migration degree), thus avoiding signal confusion in a single dimension.
[0040] It should be noted that the low-energy reflection image can capture early degradation that cannot be identified by the naked eye or macroscopic parameters (such as a slight narrowing of the peak width in the low-energy reflection intensity image, indicating that grain growth has begun; a slight decrease in local grayscale in the density image, indicating that ions have begun to migrate). Combined with the "microscopic change - loss trend" model, the development direction of surface loss can be predicted in advance (such as the surface loss will exceed the threshold after 300 hours at the current grain growth rate), realizing "microscopic early warning - early intervention" to avoid core failure caused by the accumulation of surface loss (such as surface cracking and short circuit).
[0041] In some embodiments, evaluating the internal real-time loss of the inductor core based on the inner layer reflection image includes: Based on the reflection image of the inner layer, the internal reflection image of the inductor core is evaluated using the corresponding model of the inner and outer structures; The real-time loss of the inner layer of the inductor core is evaluated based on the inner layer reflection image. The real-time loss of the inner layer of the inductor core is evaluated based on the inner layer reflection image. The internal real-time loss is obtained based on the real-time loss of the inner layer and the real-time loss of the inner layer.
[0042] It should be noted that the inner layer reflection image mainly reflects the state of the shallow interior of the magnetic core (e.g., 0.1-1 mm). This method, however, derives the inner layer reflection image from the inner layer image using an "internal-external structure correspondence model," extending the detection range to deeper layers. The microstructure of the magnetic core (e.g., grain size, ion distribution) exhibits a "shallow-deep" correlation (e.g., grain growth caused by thermal aging typically diffuses gradually from the surface to the deeper layers, and ion migration also follows a specific depth distribution pattern). Based on this correlation, the "internal-external structure correspondence model" can be used to detect the inner layer... The shallow structural features clearly defined in the reflection image (such as the shallow grain growth rate and ion migration direction) are used to infer the internal structural state of the deeper layers, thereby generating the inner layer reflection image. For example, if the inner layer image shows that the shallow grains grow at a rate of 0.2 μm / 100 h, the model can deduce that the deep grains grow synchronously at a rate of 0.15 μm / 100 h, and generate the corresponding inner layer reflection image of the deep layer state. This achieves full-depth assessment of internal losses from "shallow" to "deep", avoiding the omission of deep layer losses (such as eddy current losses caused by deep ion migration) due to insufficient detection depth.
[0043] It should be noted that the real-time loss of the inner layer is calculated directly based on the reflection image of the inner layer, reflecting the loss inside the shallow layer (such as hysteresis loss caused by shallow grain distortion and eddy current loss caused by local ion migration); the real-time loss of the inner layer is calculated based on the derived reflection image of the inner layer, reflecting the loss inside the deep layer (such as additional loss caused by deep grain boundary defects and deep ion migration loss accumulated over long-term aging). Through the quantitative results of both, the dominant region of internal loss can be quickly located: if the proportion of the inner layer loss is high, it indicates that the loss mainly originates from the shallow layer (possibly related to recent operating current overload or poor local heat dissipation); if the proportion of the inner layer real-time loss is abnormally high, it indicates that the loss has penetrated into the deep layer (possibly due to irreversible degradation caused by long-term thermal aging), providing a clear direction for targeted operation and maintenance (such as shallow layer repair and deep layer heat dissipation optimization).
[0044] In some embodiments, the inner layer reflection image includes an inner layer reflection intensity image and an inner layer reflection density image; The method of evaluating the real-time loss of the inner layer of the inductor core based on the inner layer reflection image includes: The degree of inner layer grain growth of the inductor core is evaluated based on the inner layer reflection intensity image. The degree of ion migration in the inner layer of the inductor core is evaluated based on the inner layer reflectance density image. The real-time loss of the inner layer is obtained based on the degree of grain growth and the degree of ion migration in the inner layer.
[0045] It should be noted that the inner-layer reflection intensity image is sensitive to changes in grain size. Grain growth leads to increased coherence of crystal plane reflection, resulting in higher peak height and narrower peak width. The degree of grain growth (e.g., from an initial 8 μm to 12 μm) can be quantified by peak shape parameters (e.g., full width at half maximum, peak-to-height ratio) of the intensity image. Grain growth directly increases the resistance to magnetic domain wall movement, leading to increased hysteresis loss. The inner-layer reflection density image reflects the uniformity of ion distribution; ion migration leads to a decrease in ion density in local areas (e.g., Fe). 3+ The migration of lattice vacancies corresponds to "sparse regions" with decreased gray values in the density image. The degree of ion migration can be calculated by the gray value difference in the density image (e.g., a 25% decrease in local ion density). Disordered ion distribution will destroy the uniformity of the magnetic field, increase the resistance of the eddy current path, and thus lead to increased eddy current loss. Through the direct correlation between "image features - microscopic changes - loss type", it is possible to quickly determine whether the real-time increase in loss in the inner layer is due to hysteresis loss (grain-dominated) or eddy current loss (ion-dominated), avoiding the dilemma of traditional assessment that only knows the increase in loss but does not know the cause.
[0046] It should be noted that the inner layer reflection image has removed surface signal interference and only reflects the state of the shallow inner layer (e.g., 0.1-1mm). Evaluating the inner layer loss based on this two-dimensional image avoids the influence of surface degradation (e.g., oxidation, scratches) on the results. If a medium-energy reflection image without surface removal is used directly, surface oxidation may lead to an overall low intensity signal, misjudging it as a lack of inner layer grain growth. However, the inner layer reflection image has removed surface interference; the intensity image only reflects the true reflection characteristics of the inner layer grains, and the density image only reflects the true distribution of ions in the inner layer, ensuring that the calculation of "grain growth degree" and "ion migration degree" is not affected by surface factors. For example, if there is slight oxidation on the core surface, but no obvious grain growth or significant ion migration in the inner layer, this method can conclude that "there is no abnormality in the inner layer loss," avoiding misjudgment of inner layer loss due to surface interference and ensuring the accuracy of the evaluation results.
[0047] In summary, the inductor core loss detection method provided in this application involves irradiating the inductor core with incident rays and receiving the reflected rays reflected by the inductor core; generating a reflected ray image based on the reflected rays; and evaluating the real-time total loss of the inductor core based on the reflected ray image. This non-contact method of "incident ray irradiation + reflected ray imaging" eliminates the need to damage the original structure and integrity of the core. The core does not need to be disassembled or cut during the detection process, and can be directly reinstalled into the circuit for continued use after the detection is completed, significantly reducing detection costs (no additional spare cores are required). It also supports periodic performance sampling inspections of in-service inductor cores, avoiding equipment downtime losses due to destructive testing. This method solves the problem that existing X-ray diffraction and electron microscopy methods require slicing or grinding the inductor core into powder, rendering the tested core unusable and increasing detection costs. It also makes it difficult to achieve non-destructive performance evaluation of in-service inductor cores.
[0048] Secondly, such as Figure 2 As shown in the figure, this application provides an inductor core loss detection system, including: The X-ray irradiation module 10 is used to irradiate the inductor core with incident X-rays and to receive reflected X-rays reflected by the inductor core. Image generation module 20 is used to generate a reflected ray image based on the reflected ray; Loss assessment module 30 is used to assess the real-time total loss of the inductor core based on the reflected ray image. In some embodiments, irradiating the inductor core with incident rays and receiving reflected rays reflected by the inductor core includes: The inductor core is irradiated with incident rays, and the incident angle of the incident rays is adjusted. Receive the angle-reflected rays from the inductor core at the incident angle; The incident angle is obtained based on the average intensity of the reflected rays at the angle. The inductor core is illuminated based on the detected incident angle, and the reflected rays reflected by the inductor core are received.
[0049] In some embodiments, the reflected rays include low-energy reflected rays and medium-energy reflected rays; The process of illuminating the inductor core based on the detected incident angle and receiving the reflected rays reflected by the inductor core includes: Based on the detected incident angle, the inductor core is irradiated with low-energy rays, and the low-energy reflected rays reflected by the inductor core are received. The inductor core is irradiated with medium-energy rays based on the detected incident angle, and the medium-energy reflected rays reflected by the inductor core are received.
[0050] In some embodiments, the reflected ray image includes a low-energy reflected image, a medium-energy reflected image, and an inner layer reflected image; The generation of the reflected ray image based on the reflected ray includes: The low-energy reflection image is generated based on the low-energy reflection ray; The medium-energy reflection image is generated based on the medium-energy reflection ray; The difference in surface reflection is obtained based on the penetrating power of the low-energy rays and the medium-energy rays; The inner layer reflection image is obtained based on the surface reflection difference, the low-energy reflection image, and the medium-energy reflection image.
[0051] In some embodiments, generating a low-energy reflection image based on the low-energy reflection ray specifically involves: Receive the low-energy reflected rays and generate a low-energy electrical signal based on the low-energy reflected rays; The low-energy reflection image is generated based on the low-energy electrical signal; The generation of the medium-energy reflection image based on the medium-energy reflection ray specifically involves: Receive the medium-energy reflected rays and generate a medium-energy electrical signal based on the medium-energy reflected rays; The medium-energy reflection image is generated based on the medium-energy electrical signal.
[0052] In some embodiments, evaluating the real-time total loss of the inductor core based on the reflected ray image includes: The real-time surface loss of the inductor core is evaluated based on the low-energy reflection image. The internal real-time loss of the inductor core is evaluated based on the reflection image of the inner layer. The real-time total loss of the inductor core is obtained based on the surface real-time loss and the internal real-time loss.
[0053] In some embodiments, the low-energy reflection image includes a low-energy reflection intensity image and a low-energy reflection density image; The evaluation of the real-time surface loss of the inductor core based on the low-energy reflection image includes: The degree of surface grain growth of the inductor core is evaluated based on the low-energy reflection intensity image. The degree of surface ion migration of the inductor core is evaluated based on the low-energy reflection density image. The real-time surface loss of the inductor core is obtained based on the degree of surface grain growth and the degree of surface ion migration.
[0054] In some embodiments, evaluating the internal real-time loss of the inductor core based on the inner layer reflection image includes: Based on the reflection image of the inner layer, the internal reflection image of the inductor core is evaluated using the corresponding model of the inner and outer structures; The real-time loss of the inner layer of the inductor core is evaluated based on the inner layer reflection image. The real-time loss of the inner layer of the inductor core is evaluated based on the inner layer reflection image. The internal real-time loss is obtained based on the real-time loss of the inner layer and the real-time loss of the inner layer.
[0055] In some embodiments, the inner layer reflection image includes an inner layer reflection intensity image and an inner layer reflection density image; The method of evaluating the real-time loss of the inner layer of the inductor core based on the inner layer reflection image includes: The degree of inner layer grain growth of the inductor core is evaluated based on the inner layer reflection intensity image. The degree of ion migration in the inner layer of the inductor core is evaluated based on the inner layer reflectance density image. The real-time loss of the inner layer is obtained based on the degree of grain growth and the degree of ion migration in the inner layer.
[0056] The device embodiments described above are merely illustrative. The units described as separate components may or may not be physically separate. The components shown as units may or may not be physical units; that is, they may be located in one place or distributed across multiple network units. Some or all of the modules can be selected to achieve the purpose of this embodiment according to actual needs.
[0057] Through the above description of the embodiments, those skilled in the art can clearly understand that each embodiment can be implemented using software plus a general-purpose hardware platform, or of course, using hardware. Based on this understanding, the above technical solutions, in essence or the parts that contribute to the related technology, can be embodied in the form of a software product. This computer software product can be stored in a computer-readable storage medium, such as ROM / RAM, magnetic disk, optical disk, etc., and includes several instructions to cause a computer device (which may be a personal computer, server, or network device, etc.) to execute the methods described in the various embodiments or some parts of the embodiments.
[0058] It should be understood that the terminology used herein is for the purpose of describing particular exemplary embodiments only and is not intended to be limiting. Unless the context clearly indicates otherwise, the singular forms “a,” “an,” and “described” as used herein may also mean including the plural forms. The terms “comprising,” “including,” “containing,” and “having” are inclusive and therefore indicate the presence of stated features, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, steps, operations, elements, components, and / or combinations thereof. The method steps, processes, and operations described herein are not construed as requiring them to be performed in a specific order described or illustrated unless the order of execution is explicitly indicated. It should also be understood that additional or alternative steps may be used. The above description is merely a specific embodiment of the invention to enable those skilled in the art to understand or implement the invention. Various modifications to these embodiments will be readily apparent to those skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the invention. Therefore, the invention is not to be limited to the embodiments shown herein, but is to be accorded the widest scope consistent with the principles and novel features claimed herein.
Claims
1. A method for detecting the loss of an inductor core, characterized in that, include: The inductor core is irradiated with incident rays, and the reflected rays reflected by the inductor core are received. Generate a reflected ray image based on the reflected ray; The real-time total loss of the inductor core is evaluated based on the reflected ray image.
2. The inductor core loss detection method according to claim 1, characterized in that, The step of irradiating the inductor core with incident rays and receiving the reflected rays reflected by the inductor core includes: The inductor core is irradiated with incident rays, and the incident angle of the incident rays is adjusted. Receive the angle-reflected rays from the inductor core at the incident angle; The incident angle is obtained based on the average intensity of the reflected rays at the angle. The inductor core is illuminated based on the detected incident angle, and the reflected rays reflected by the inductor core are received.
3. The inductor core loss detection method according to claim 2, characterized in that, The reflected rays include low-energy reflected rays and medium-energy reflected rays; The process of illuminating the inductor core based on the detected incident angle and receiving the reflected rays reflected by the inductor core includes: Based on the detected incident angle, the inductor core is irradiated with low-energy rays, and the low-energy reflected rays reflected by the inductor core are received. The inductor core is irradiated with medium-energy rays based on the detected incident angle, and the medium-energy reflected rays reflected by the inductor core are received.
4. The inductor core loss detection method according to claim 3, characterized in that, The reflected ray images include low-energy reflected images, medium-energy reflected images, and inner layer reflected images; The generation of the reflected ray image based on the reflected ray includes: The low-energy reflection image is generated based on the low-energy reflection ray; The medium-energy reflection image is generated based on the medium-energy reflection ray; The difference in surface reflection is obtained based on the penetrating power of the low-energy rays and the medium-energy rays; The inner layer reflection image is obtained based on the surface reflection difference, the low-energy reflection image, and the medium-energy reflection image.
5. The inductor core loss detection method according to claim 4, characterized in that, The generation of the low-energy reflection image based on the low-energy reflection ray specifically involves: Receive the low-energy reflected rays and generate a low-energy electrical signal based on the low-energy reflected rays; The low-energy reflection image is generated based on the low-energy electrical signal; The generation of the medium-energy reflection image based on the medium-energy reflection ray specifically involves: Receive the medium-energy reflected rays and generate a medium-energy electrical signal based on the medium-energy reflected rays; The medium-energy reflection image is generated based on the medium-energy electrical signal.
6. The inductor core loss detection method according to claim 4, characterized in that, The evaluation of the real-time total loss of the inductor core based on the reflected ray image includes: The real-time surface loss of the inductor core is evaluated based on the low-energy reflection image. The internal real-time loss of the inductor core is evaluated based on the reflection image of the inner layer. The real-time total loss of the inductor core is obtained based on the surface real-time loss and the internal real-time loss.
7. The inductor core loss detection method according to claim 6, characterized in that, The low-energy reflection image includes a low-energy reflection intensity image and a low-energy reflection density image; The evaluation of the real-time surface loss of the inductor core based on the low-energy reflection image includes: The degree of surface grain growth of the inductor core is evaluated based on the low-energy reflection intensity image. The degree of surface ion migration of the inductor core is evaluated based on the low-energy reflection density image. The real-time surface loss of the inductor core is obtained based on the degree of surface grain growth and the degree of surface ion migration.
8. The inductor core loss detection method according to claim 6, characterized in that, The evaluation of the internal real-time loss of the inductor core based on the reflection image of the inner layer includes: Based on the reflection image of the inner layer, the internal reflection image of the inductor core is evaluated using the corresponding model of the inner and outer structures; The real-time loss of the inner layer of the inductor core is evaluated based on the inner layer reflection image. The real-time loss of the inner layer of the inductor core is evaluated based on the inner layer reflection image. The internal real-time loss is obtained based on the real-time loss of the inner layer and the real-time loss of the inner layer.
9. The inductor core loss detection method according to claim 8, characterized in that, The inner layer reflection image includes an inner layer reflection intensity image and an inner layer reflection density image; The method of evaluating the real-time loss of the inner layer of the inductor core based on the inner layer reflection image includes: The degree of inner layer grain growth of the inductor core is evaluated based on the inner layer reflection intensity image. The degree of ion migration in the inner layer of the inductor core is evaluated based on the inner layer reflectance density image. The real-time loss of the inner layer is obtained based on the degree of grain growth and the degree of ion migration in the inner layer.
10. An inductor core loss detection system, characterized in that, include: An X-ray irradiation module is used to irradiate the inductor core with incident rays and to receive reflected rays reflected by the inductor core; An image generation module is used to generate a reflected ray image based on the reflected ray; A loss assessment module is used to assess the real-time total loss of the inductor core based on the reflected ray image.