Secondary battery and electrode component thereof

By designing the active material layer part with gradually decreasing thickness in the secondary battery electrode component, combined with the use of a protective layer, the problem of bending of the electrode component during the rolling process is solved, lithium precipitation of the secondary battery is avoided, and the battery performance is improved. .

CN110660956BActive Publication Date: 2024-10-18CONTEMPORARY AMPEREX TECHNOLOGY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN201811206647.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2018-10-17
Publication Date
2024-10-18
Estimated Expiration
2038-10-17

AI Technical Summary

Technical Problem

During the rolling process, the ends of the secondary battery electrode components cannot be aligned due to the bending of the electric generation area, which affects the coverage of the active material layer, causing lithium deposition and affecting battery performance.

Method used

An electrode member is designed, wherein the active material layer includes a first part and a second part. The first part is located at an end of the active material layer away from the protrusion. The second part is located on a side of the first part close to the protrusion. The thickness of the first part is less than The second part gradually decreases in the direction away from the protrusion. The density of the second part is greater than that of the first part. Under the same force, the elongation rate of the insulating matrix and the elongation rate of the conductive layer do not differ by more than 4% to reduce the generation of electricity. area of ​​curvature.

Benefits of technology

By reducing the length difference between the two ends of the electrode member in the height direction, the overall bending deformation is reduced, lithium precipitation in the secondary battery is avoided, and battery performance is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN110660956B_ABST
    Figure CN110660956B_ABST
Patent Text Reader

Abstract

The present invention provides a secondary battery and an electrode component thereof. The electrode component includes an insulating substrate, a conductive layer and an active material layer. The conductive layer is arranged on the surface of the insulating substrate, and the conductive layer includes a main body and a protrusion extending from the main body, the main body is coated with an active material layer, and the protrusion is not coated with the active material layer. The active material layer includes a first part and a second part, the first part is located at the end of the active material layer away from the protrusion, the second part is located on a side of the first part close to the protrusion, and the thickness of the first part is less than the thickness of the second part. The secondary battery includes an electrode assembly, and the electrode assembly includes the electrode component.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of batteries, and in particular to a secondary battery and an electrode component thereof. Background Art

[0002] The electrode components of secondary batteries generally include a current collector and an active material layer coated on the surface of the current collector. In order to improve the safety performance of secondary batteries, some electrode components select a current collector with a multi-layer structure. Figure 1 and Figure 2 , the current collector includes an insulating substrate 11 and a conductive layer 12 disposed on the surface of the insulating substrate 11, and an active material layer 13 is coated on the surface of the conductive layer 12. The conductive layer 12 includes a main body 121 coated with the active material layer 13 and a protrusion 122 not coated with the active material layer 13. The active material layer 13, the main body 121 and the portion of the insulating substrate 11 corresponding to the main body 121 form an electric generation area P1, and the protrusion 122 and the portion of the insulating substrate 11 corresponding to the protrusion 122 form an electric guide area P2, which is used to electrically connect to the electrode terminal of the secondary battery and realize charging and discharging through the electrode terminal.

[0003] In the production process of the electrode component, the active material layer 13 needs to be rolled to thin the active material layer 13 and improve the energy density. The insulating substrate 11 is a relatively soft material (such as PET plastic) with a large elongation. Figure 2 Since the thickness of the electric generation zone P1 is much greater than that of the electric guide zone P2, the roller 9 only applies pressure on the active material layer 13, so the insulating matrix 11 of the electric generation zone P1 has a large elongation; and during the elongation process, the insulating matrix 11 of the electric generation zone P1 will apply tension to the insulating matrix 11 of the electric guide zone P2 to drive the insulating matrix 11 of the electric guide zone P2 to extend. Correspondingly, the insulating matrix 11 of the electric guide zone P2 will apply a reaction force to the insulating matrix 11 of the electric generation zone P1 to limit the elongation of the insulating matrix 11 of the electric generation zone P1; when the thickness of the electric generation zone P1 is uniform, the reaction force gradually decreases in the direction away from the electric guide zone P2 (that is, the elongation rate of the insulating matrix 11 of the electric generation zone P1 gradually increases). Therefore, referring to Figure 3 After the electrode component is rolled, the length of one end of the electric generating area P1 away from the electric guiding area P2 will be greater than the length of the electric guiding area P2, causing the electrode component to bend as a whole.

[0004] In a secondary battery, the positive and negative electrode components are wound together; if the electricity generation zone P1 is bent, the ends of the electricity generation zone P1 cannot be aligned after winding, resulting in the inability of the active material layer 13 of the negative electrode component to completely cover the active material layer 13 of the positive electrode component; during the charging process, the lithium released from the active material layer 13 of the positive electrode component cannot be fully embedded in the active material layer 13 of the negative electrode component, thereby causing lithium precipitation and affecting the performance of the secondary battery. Summary of the invention

[0005] In view of the problems existing in the background technology, an object of the present invention is to provide a secondary battery and an electrode component thereof, which can reduce the bending of the electricity generation area and avoid lithium deposition in the secondary battery.

[0006] In order to achieve the above objective, the present invention provides a secondary battery and an electrode member thereof.

[0007] The electrode component includes an insulating substrate, a conductive layer and an active material layer. The conductive layer is disposed on the surface of the insulating substrate, and the conductive layer includes a main body and a protrusion extending from the main body, the main body is coated with the active material layer, and the protrusion is not coated with the active material layer. The active material layer includes a first part and a second part, the first part is located at an end of the active material layer away from the protrusion, the second part is located on a side of the first part close to the protrusion, and the thickness of the first part is less than the thickness of the second part.

[0008] The thickness of the first portion gradually decreases in a direction away from the protrusion.

[0009] In the height direction, the ratio of the size of the first portion to the total size of the active material layer is 3% to 20%.

[0010] The density of the second portion is greater than the density of the first portion.

[0011] The difference between the thickness of the first portion and the thickness of the second portion is 0.5 μm to 20 μm.

[0012] The active material layer also includes a third portion, which is located on a side of the second portion close to the protrusion, and has a thickness smaller than that of the second portion; the thickness of the third portion gradually decreases in a direction close to the protrusion.

[0013] The electrode component further comprises a protective layer which is arranged on a side of the protrusion away from the insulating substrate and connected to the third part.

[0014] Under the same applied force, the difference between the elongation of the insulating substrate and the elongation of the conductive layer does not exceed 4%.

[0015] The elongation of the insulating matrix is ​​less than 10%.

[0016] The secondary battery includes an electrode assembly, and the electrode assembly includes the electrode member.

[0017] The beneficial effects of the present invention are as follows: since the thickness of the second part is greater than that of the first part, during the rolling process, the second part is subjected to a greater rolling pressure, while the first part is subjected to a smaller rolling pressure; that is, the portion of the electric generation zone corresponding to the second part has a greater elongation, while the portion of the electric generation zone corresponding to the first part has a smaller elongation. During the rolling process, the electric guide zone is not subjected to force and hardly elongates, so after rolling, the elongation at both ends of the electrode component in the height direction is smaller, while the elongation in the middle of the electrode component is larger. The present application reduces the thickness of the first part, reduces the length difference at both ends of the electrode component in the height direction, reduces the overall bending deformation of the electrode component, and avoids lithium deposition in the secondary battery. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 Schematic diagram of an electrode component in the prior art.

[0019] Figure 2 for Figure 1 Schematic diagram of the electrode component during the roller pressing process.

[0020] Figure 3 for Figure 1 Schematic diagram of the electrode component after roller pressing.

[0021] Figure 4 is a schematic diagram of a secondary battery according to the present invention.

[0022] Figure 5 is a cross-sectional view of an electrode assembly according to the present invention.

[0023] Figure 6 FIG. 1 is a schematic diagram of an electrode component according to the present invention after winding.

[0024] Figure 7 for Figure 6 Schematic diagram of the electrode component after expansion.

[0025] Figure 8 for Figure 7 Section view along line AA.

[0026] Fig. 9 for Figure 7 Schematic diagram of the electrode component during the forming process.

[0027] Fig.10 for Fig. 9 Section view along line BB.

[0028] Fig.11 for Fig. 9 Schematic diagram of the electrode component after roller pressing.

[0029] Fig.12 FIG. 4 is a schematic diagram of another embodiment of an electrode component according to the present invention.

[0030] Fig.13 for Fig.12 Section view along line CC.

[0031] Fig.14 FIG. 4 is a schematic diagram of another embodiment of an electrode component according to the present invention.

[0032] Fig.15 for Fig.14 Sectional view along line DD.

[0033] The reference numerals are described as follows:

[0034] 1 Electrode component P2 Electric guide area

[0035] 11 insulating substrate 2 positive electrode component

[0036] 12 conductive layer 3 negative electrode component

[0037] 121 main body 4 diaphragm

[0038] 122 protrusion 5 housing

[0039] 13 active material layer 6 top cover plate

[0040] 131 Part 1 7 Electrode Terminal

[0041] 132 Part 2 8 Adapter

[0042] 133 Part 3 9 Roller

[0043] 14 Protective layer X width direction

[0044] 15 Conductive structure Y thickness direction

[0045] P1 electrogenerating zone Z height direction DETAILED DESCRIPTION

[0046] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present application and its application or use. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without carrying out creative work are within the scope of protection of this application.

[0047] In the description of the present application, it should be understood that the use of terms such as "first" and "second" to limit components is only for the convenience of distinguishing the corresponding components. Unless otherwise stated, the above terms have no special meaning and therefore cannot be understood as limiting the scope of protection of the present application.

[0048] The secondary battery of the present invention includes an electrode assembly, referring to Figure 5 The electrode assembly includes a positive electrode component 2, a negative electrode component 3 and a separator 4, and the separator 4 is arranged between the positive electrode component 2 and the negative electrode component 3. The positive electrode component 2, the separator 4 and the negative electrode component 3 are stacked and wound into a flat shape. The electrode assembly is a core component for realizing the charging and discharging functions of the secondary battery.

[0049] The secondary battery of the present invention can be a soft pack battery, and the electrode assembly formed by winding the positive electrode component 2, the separator 4 and the negative electrode component 3 is directly packaged in a packaging bag. The packaging bag can be an aluminum-plastic film.

[0050] Of course, the secondary battery of the present application may also be a hard shell battery. Figure 4 The secondary battery mainly includes an electrode assembly, a shell 5, a top cover plate 6, an electrode terminal 7 and a switching plate 8.

[0051] The housing 5 may have a hexahedral shape or other shapes. A cavity is formed inside the housing 5 to accommodate the electrode assembly and the electrolyte. The housing 5 has an opening at one end, and the electrode assembly can be placed in the receiving cavity of the housing 5 through the opening. The housing 5 may be made of a conductive metal material such as aluminum or aluminum alloy, or may be made of an insulating material such as plastic.

[0052] The top cover plate 6 is disposed on the housing 5 and covers the opening of the housing 5, thereby enclosing the electrode assembly in the housing 5. The electrode terminal 7 is disposed on the top cover plate 6, the upper end of the electrode terminal 7 protrudes to the upper side of the top cover plate 6, and the lower end can pass through the top cover plate 6 and extend into the housing 5. The adapter 8 is disposed in the housing 5 and fixed to the electrode terminal 7. There are two electrode terminals 7 and two adapters 8, the positive electrode component 2 is electrically connected to one electrode terminal 7 via one adapter 8, and the negative electrode component 3 is electrically connected to the other electrode terminal 7 via the other adapter 8.

[0053] In the secondary battery, at least one of the positive electrode member 2 and the negative electrode member 3 employs an electrode member 1 described later.

[0054] Figures 6 to 11 FIG. 1 is a schematic diagram of a first embodiment of an electrode component 1 of the present invention. Figures 6 to 11 The electrode component 1 includes an insulating substrate 11 , a conductive layer 12 and an active material layer 13 .

[0055] The insulating substrate 11 may be made of a PET (polyethylene terephthalate) film or a PP (polypropylene) film, and may have a thickness of 1 μm to 20 μm.

[0056] There are two conductive layers 12, which are respectively arranged on the two surfaces of the insulating substrate 11. Specifically, the material of the conductive layer 12 is selected from at least one of a metal conductive material and a carbon-based conductive material; the metal conductive material is preferably at least one of aluminum, copper, nickel, titanium, silver, nickel-copper alloy, and aluminum-zirconium alloy, and the carbon-based conductive material is preferably at least one of graphite, acetylene black, graphene, and carbon nanotubes. The conductive layer 12 can be formed on the surface of the insulating substrate 11 by at least one of vapor deposition and electroless plating. Among them, the vapor deposition method is preferably physical vapor deposition (PVD), such as thermal evaporation deposition.

[0057] The active material layer 13 includes an active material, and the active material may be determined according to the polarity of the electrode component 1; for example, when the electrode component 1 is positive, the active material may be lithium manganese oxide or lithium iron phosphate, and when the electrode component 1 is negative, the active material may be graphite or silicon. The active material, binder, conductive agent and solvent may be made into a slurry, and then the slurry is coated on the outer surface of the conductive layer 12 away from the insulating substrate 11, and the slurry is cured to form the active material layer 13. There are two active material layers 13 and they are coated on the two conductive layers 12 respectively.

[0058] The active material layer 13 only covers a portion of the conductive layer 12. Figure 7 and Figure 8 The conductive layer 12 includes a main body 121 and a protrusion 122 extending from the main body 121 . The main body 121 is coated with the active material layer 13 , and the protrusion 122 is not coated with the active material layer 13 .

[0059] For the convenience of description, the active material layer 13, the main body 121, and the portion of the insulating substrate 11 corresponding to the main body 121 are referred to as the electric generation area P1, and the protrusion 122 and the portion of the insulating substrate 11 corresponding to the protrusion 122 are referred to as the electric guide area P2. During the use of the secondary battery, the active material layer 13 of the electric generation area P1 undergoes an electrochemical reaction with the electrolyte, etc., resulting in a charge and discharge process; and the electric guide area P2 is connected to the adapter 8, thereby leading the current to the outside of the secondary battery.

[0060] Reference Figure 7 , the electrical guide area P2 is multiple and arranged at intervals along the width direction X; in the secondary battery, the positive and negative electrode components 1 are wound to form an electrode assembly, referring to Figure 6 After the electrode component 1 is wound and formed, the multiple electrical guide areas P2 are stacked along the thickness direction Y and fixed to the adapter sheet 8 by welding.

[0061] Since the conductive layer 12 is relatively thin, the burrs generated by the conductive layer 12 during the cutting process are relatively small, and it is difficult to pierce the diaphragm 4 of more than ten microns, thereby avoiding short circuits and improving safety performance. In addition, when a foreign object pierces the electrode component 1 of the secondary battery, since the conductive layer 12 is relatively thin, the burrs generated by the conductive layer 12 at the part pierced by the foreign object are relatively small, and it is difficult to pierce the diaphragm 4, thereby avoiding short circuits and improving safety performance.

[0062] The electrode component 1 further includes a protective layer 14, which is disposed on a side of the protrusion 122 away from the insulating substrate 11 and connected to the active material layer 13. The protective layer 14 includes a binder and an insulating material, and the insulating material includes at least one of aluminum oxide and aluminum oxyhydroxide. The binder, the insulating material and the solvent are mixed together to prepare a slurry, which is coated on the surface of the protrusion 122 and forms the protective layer 14 after curing. The hardness of the protective layer 14 is greater than the hardness of the conductive layer 12.

[0063] The electrode component 1 further includes a plurality of conductive structures 15, each conductive structure 15 being welded to an area of ​​the protrusion 122 that is not covered by the protective layer 14. Figure 6 After the electrode component 1 is wound, the multiple conductive structures 15 are stacked along the thickness direction Y, and there is a conductive structure 15 between every two adjacent electrical guide areas P2. The multiple conductive structures 15 are welded to the adapter sheet 8 at the same time, thereby realizing the busbar output of the two conductive layers 12.

[0064] The active material layer 13 includes a first portion 131 and a second portion 132 . The first portion 131 is located at the end of the active material layer 13 away from the protrusion 122 , and the second portion 132 is located on a side of the first portion 131 close to the protrusion 122 . The thickness of the first portion 131 is smaller than that of the second portion 132 .

[0065] The electrode component 1 of the first embodiment can be formed according to the following steps:

[0066] (i) A conductive layer 12 is formed on the surface of an insulating substrate 11 by vapor deposition or chemical plating, thereby preparing a composite strip.

[0067] (II) Reference Fig. 9 , the active material layer 13 and the protective layer 14 are simultaneously coated on the surface of the conductive layer 12 ; during coating, the thickness of the active material layer 13 at one end away from the protective layer 14 is reduced.

[0068] (iii) rolling the active material layer 13 to compact the active material layer 13 and increase its density.

[0069] (iv) After rolling, a metal foil (such as aluminum foil) is welded on the conductive layer 12, and then the metal foil, the protective layer 14, the conductive layer 12 and the insulating substrate 11 are cut at the same time to obtain Figure 7 The electrode component 1 is shown.

[0070] Fig.11 The shape of the electrode component 1 after the rolling process of step (iii) is shown. Since the thickness of the second portion 132 is greater than that of the first portion 131, during the rolling process, the second portion 132 is subjected to a greater rolling pressure, while the first portion 131 is subjected to a smaller rolling pressure; that is, the portion of the electrical generating area P1 corresponding to the second portion 132 has a greater elongation, while the portion of the electrical generating area P1 corresponding to the first portion 131 has a smaller elongation. During the rolling process, the electrical guide area P2 is not subjected to force and is almost not stretched, therefore, referring to Fig.11 After rolling, the elongation of the electrode component 1 along the height direction Z is small at both ends, while the elongation of the middle part of the electrode component 1 is large. The present application reduces the thickness of the first part 131, reduces the length difference between the two ends of the electrode component 1 along the height direction Z, reduces the overall bending deformation of the electrode component 1, and avoids lithium deposition in the secondary battery.

[0071] Since the elastic modulus of the insulating matrix 11 is relatively small, when the electric generation area P1 is rolled, the insulating matrix 11 of the electric generation area P1 will extend toward the inner side of the protrusion 122, causing the insulating matrix 11 inside the protrusion 122 to bulge and deform, and the protrusion 122 is easily cracked under the force of the insulating matrix 11. In the present application, the protective layer 14 has a relatively high strength, and can provide support for the protrusion 122 during the rolling process of the electrode component 1, limit the deformation of the protrusion 122, reduce the probability of cracks in the protrusion 122, and improve the current carrying capacity of the electrode component 1.

[0072] During the operation of the secondary battery, the protrusion 122 may fall off due to factors such as vibration; preferably, the protective layer 14 is connected to the active material layer 13, so that the protective layer 14 can be fixed to the active material layer 13, increasing the bonding force of the protective layer 14 on the electrode component 1, improving the anti-vibration ability, and preventing the protective layer 14 from falling off together with the protrusion 122. At the same time, the protrusion 122 is most likely to crack near the root of the active material layer 13 (that is, the junction of the protrusion 122 and the main area 121), so when the protective layer 14 is connected to the active material layer 13, the protrusion 122 can be prevented from cracking, thereby improving the current capacity of the electrode component 1.

[0073] Along the height direction Z, the ratio of the size of the first part 131 to the total size of the active material layer 13 is 3% to 20%. Since the elastic modulus of the insulating matrix 11 is small, during the rolling process, the insulating matrix 11 corresponding to the second part 132 will exert a force on the insulating matrix 11 corresponding to the first part 131 to drive the insulating matrix 11 corresponding to the first part 131 to extend; along the direction away from the electrical guide area P2, the force gradually decreases. If the ratio of the size of the first part 131 to the total size of the active material layer 13 is less than 3%, then driven by the force, the end of the electrical generation area P1 away from the electrical guide area P2 will still have a large extension, and the effect of reducing the length difference between the two ends of the electrode member 1 along the height direction Z is limited. If the ratio of the size of the first part 131 to the total size of the active material layer 13 is greater than 20%, the capacity of the active material layer 13 will be reduced, affecting the energy density.

[0074] During roller pressing, the roller pressure applied to the second portion 132 is the largest. Therefore, after compaction, the density of the second portion 132 is greater than that of the first portion 131 .

[0075] The difference between the thickness of the first portion 131 and the thickness of the second portion 132 is 0.5 μm to 20 μm. If the thickness difference is less than 0.5 μm, the first portion 131 will still be subjected to a large roller pressure, and the end of the electric generation area P1 away from the electric guide area P2 will still have a large extension, which has a limited effect on reducing the length difference between the two ends of the electrode member 1 along the height direction Z. If the thickness difference is greater than 20 μm, the capacity of the active material layer 13 will be reduced, affecting the energy density.

[0076] Usually, the elongation of the insulating matrix 11 is greater than that of the conductive layer 12. Therefore, during the rolling process, the insulating matrix 11 will exert a force on the conductive layer 12 to drive the conductive layer 12 to extend. If the difference between the elongation of the insulating matrix 11 and the elongation of the conductive layer 12 is too large, the conductive layer 12 is easily broken under the force, affecting the current carrying capacity of the conductive layer 12. Therefore, preferably, under the same force, the difference between the elongation of the insulating matrix 11 and the elongation of the conductive layer 12 does not exceed 4%. In addition, the elongation refers to the percentage of the elongation of the material to the original length under a certain pressure.

[0077] The greater the elongation of the insulating matrix 11, the greater the length difference between the two ends of the electrode member 1 along the height direction Z. At the same time, it is easier to break the conductive layer 12 during the rolling process. Therefore, the elongation of the insulating matrix 11 is preferably less than 10%. Furthermore, the elongation of the insulating matrix 11 is preferably 1% to 3%.

[0078] In order to simplify the description, only the differences between the other two embodiments and the first embodiment are mainly introduced below, and the parts not described can be understood with reference to the first embodiment.

[0079] Fig.12 and Fig.13 Schematic diagram of a second embodiment of the electrode component of the present invention. Fig.12 and Fig.13 In the second embodiment, the thickness of the first portion 131 gradually decreases in the direction away from the protrusion 122. In order to reduce the length difference between the two ends of the electrode member 1 along the height direction Z, it is necessary to reduce the elongation rate of the end of the electric generating area P1 away from the electric guiding area P2; therefore, in the first portion 131, the farther away from the protrusion 122, the smaller its thickness needs to be, so as to reduce the length difference between the two ends of the electrode member 1 along the height direction Z.

[0080] Reference Figure 8 In the first embodiment, the first part 131 is evenly coated, so the first part 131 and the second part 132 have a large thickness difference at the junction; during rolling, the stress will be concentrated at the junction of the first part 131 and the second part 132, so the conductive layer 12 is easily broken under the action of stress, affecting the current carrying capacity. In the second embodiment, the first part 131 gradually becomes thinner in the direction away from the protrusion 122, so as to achieve a smooth transition between the first part 131 and the second part 132 at the junction, thereby dispersing the stress, reducing the stress concentration, and avoiding the stress from cutting the conductive layer 12.

[0081] Fig.14 and Fig.15 FIG. 1 is a schematic diagram of a third embodiment of an electrode component of the present invention. Fig.14 and Fig.15 In the third embodiment, the active material layer 13 further includes a third portion 133, which is located on a side of the second portion 132 close to the protrusion 122, and the thickness of the third portion 133 is less than the thickness of the second portion 132. The third portion 133 is located at one end of the active material layer 13 close to the protrusion 122.

[0082] During the rolling process, the main body 121 is subjected to the rolling pressure, while the protrusion 122 is not subjected to the rolling pressure, so the stress is concentrated at the junction of the two. Fig.13 In the second embodiment, the protrusion 122 is directly adjacent to the second portion 132, and the second portion 132 has a relatively large thickness. Therefore, the stress at the junction of the main body 121 and the protrusion 122 is relatively large, and the main body 121 and the protrusion 122 are easily separated and cracks are formed, which affects the flow capacity. In the third embodiment, by reducing the thickness of the third portion 133, the stress at the junction of the main body 121 and the protrusion 122 can be reduced, and the probability of cracks can be reduced.

[0083] Furthermore, the thickness of the third portion 133 gradually decreases along the direction close to the protrusion 122. The third portion 133 gradually becomes thinner along the direction close to the protrusion 122, so as to achieve a smooth transition between the first portion 131 and the third portion 133 at the junction, thereby dispersing stress, reducing stress concentration, and avoiding stress cutting the conductive layer 12.

[0084] Since the protrusion 122 is adjacent to the third portion 133 , the protection layer 14 is connected to the third portion 133 .

Claims

1. An electrode component (1) of a secondary battery, comprising an insulating substrate (11), a conductive layer (12) and an active material layer (13); The conductive layer (12) is arranged on the surface of the insulating substrate (11), and the conductive layer (12) comprises a main body (121) and a protrusion (122) extending from the main body (121), the main body (121) is coated with an active material layer (13), and the protrusion (122) is not coated with the active material layer (13); The active material layer (13) comprises a first portion (131) and a second portion (132), wherein the first portion (131) is located at an end of the active material layer (13) away from the protrusion (122), and the second portion (132) is located at a side of the first portion (131) close to the protrusion (122), and the thickness of the first portion (131) is smaller than the thickness of the second portion (132); The material of the conductive layer (12) is a metal conductive material, and the metal conductive material is at least one of aluminum, copper, nickel, titanium, and silver; The thickness of the first portion (131) gradually decreases in a direction away from the protrusion (122).

2. The electrode component (1) according to claim 1, characterized in that Along the height direction (Z), the ratio of the size of the first portion (131) to the total size of the active material layer (13) is 3% to 20%.

3. The electrode component (1) according to claim 1, characterized in that The density of the second portion (132) is greater than the density of the first portion (131).

4. The electrode component (1) according to claim 1, characterized in that The difference between the thickness of the first portion (131) and the thickness of the second portion (132) is 0.5 μm to 20 μm.

5. The electrode component (1) according to any one of claims 1 to 4, characterized in that: The active material layer (13) further includes a third portion (133), the third portion (133) is located on a side of the second portion (132) close to the protrusion (122), and the thickness of the third portion (133) is smaller than the thickness of the second portion (132); The thickness of the third portion (133) gradually decreases in a direction approaching the protrusion (122).

6. The electrode component (1) according to claim 5, characterized in that The electrode component (1) further comprises a protective layer (14) which is arranged on a side of the protrusion (122) away from the insulating substrate (11) and is connected to the third part (133).

7. The electrode component (1) according to claim 1, characterized in that Under the same applied force, the difference between the elongation of the insulating substrate (11) and the elongation of the conductive layer (12) does not exceed 4%.

8. The electrode component (1) according to claim 7, characterized in that The elongation of the insulating substrate (11) is less than 10%.

9. A secondary battery, characterized in that: The invention comprises an electrode assembly, wherein the electrode assembly comprises the electrode component (1) according to any one of claims 1 to 8.

Citation Information

Patent Citations

  • A secondary battery and electrode member thereof

    CN208955106U