Cylindrical battery

By designing the sealing plate with a central concave shape and applying specific pressing force when riveting and fixing, the interference problem caused by the warping of the cylindrical battery sealing plate during assembly is solved, achieving reliable assembly of the sealing plate and preventing breakage.

CN113228377BActive Publication Date: 2024-10-18PANASONIC ENERGY CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN201980085747.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-12-17
Publication Date
2024-10-18
Estimated Expiration
2039-12-17

AI Technical Summary

Technical Problem

During the riveting and fixing process of the sealing body of a cylindrical sealed battery, the central part of the sealing body tends to warp upward, causing interference with external leads during assembly of the battery module, which may cause damage to the sealing body.

Method used

A sealing plate is designed, which forms a circular shape when viewed from above. The central area is recessed toward the inner side of the battery, and the outer peripheral edge portion is divided into the first part and the second part. Through a specific riveting fixation method, the sealing plate is It can reliably warp toward the inside of the battery during riveting to prevent damage.

Benefits of technology

It effectively prevents the sealing plate from interfering with external leads during the assembly process of the battery module, avoids damage to the sealing plate, and ensures the reliability and stability of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113228377B_ABST
    Figure CN113228377B_ABST
Patent Text Reader

Abstract

The purpose of the present disclosure is to provide a cylindrical battery configured so that the central area of ​​a sealing plate riveted to the opening of an outer can is warped toward the inner side of the battery. A cylindrical battery according to one embodiment of the present disclosure comprises: an electrode body formed by winding a positive electrode plate and a negative electrode plate with a separator between them; an electrolyte; a bottomed cylindrical outer can containing the electrode body and the electrolyte; and a sealing plate (22) riveted to the opening of the outer can with a gasket between them. The sealing plate (22) is circular in a plan view, and has a shape in which its central area (22a) is concave toward the inner side of the battery, and the outer peripheral edge (27) of the sealing plate (22) riveted to the outer can is divided into a first part (27a) and a second part (27b) in the plate thickness direction.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to cylindrical batteries. Background Art

[0002] For example, Patent Document 1 discloses a cylindrical sealed battery. The cylindrical sealed battery includes: a bottomed cylindrical outer can; a cylindrically wound electrode body and an electrolyte housed in the outer can; and a sealing body fixed to the opening of the outer can via an insulating gasket to seal the inside of the battery.

[0003] Prior Art Literature

[0004] Patent Literature

[0005] Patent Document 1: International Publication No. 2015 / 146078 Summary of the invention

[0006] Problem that the invention aims to solve

[0007] In the cylindrical sealed battery described in the above-mentioned Patent Document 1, when the sealing body is riveted and fixed to the opening of the outer can, due to the moment acting on the outer peripheral edge of the sealing body and the radially inward pressing force, the central portion of the sealing body may be warped into a concave shape toward the inner side of the battery, i.e., the lower side, or conversely be warped into a convex shape toward the upper side. There is no problem in the case where the sealing body is warped toward the lower side, but in the case where the central portion becomes the highest point in the state where the battery is erected due to the upward warping of the sealing body, when a plurality of cylindrical sealed batteries are assembled as a battery module, interference may occur with the external lead for extracting the output current from the cylindrical sealed battery, thereby causing the sealing body to be damaged.

[0008] An object of the present disclosure is to provide a cylindrical battery in which a central region of a sealing plate fixed by caulking to an opening of an outer can is formed into a shape that is reliably warped inward of the battery.

[0009] Means for solving problems

[0010] The cylindrical battery disclosed in the present invention comprises: an electrode body formed by winding a positive electrode plate and a negative electrode plate with a separator interposed therebetween; an electrolyte; a bottomed cylindrical outer can containing the electrode body and the electrolyte; and a sealing plate fixed to the opening of the outer can by riveting through a gasket. The sealing plate is formed into a circular shape in a plan view, and has a shape in which the central area thereof is concave toward the inner side of the battery, and the outer peripheral edge portion of the sealing plate fixed to the outer can by riveting is divided into a first part and a second part in the plate thickness direction.

[0011] Effects of the Invention

[0012] According to the cylindrical battery disclosed herein, the central area of ​​the sealing plate fixed to the opening of the outer can can be reliably warped toward the inner side of the battery. Therefore, it is possible to prevent the sealing plate from interfering with the external lead wire for extracting the output current from the cylindrical battery when assembled as a battery module and causing damage. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 This is a cross-sectional view along the axial direction of a cylindrical battery according to one embodiment.

[0014] Figure 2 It is a cross-sectional view of the sealing body.

[0015] Figure 3 (a) is a radial half cross-sectional view showing the sealing body and its vicinity before riveting. Figure 3 (b) is a radial half cross-sectional view showing the sealing body and its vicinity when riveted and fixed.

[0016] Figure 4 (a) to (c) are enlarged cross-sectional views showing modified examples of the outer peripheral edge portion of the sealing plate. DETAILED DESCRIPTION

[0017] Hereinafter, the embodiments of the present disclosure will be described in detail with reference to the accompanying drawings. In this description, specific shapes, materials, numerical values, directions, etc. are examples for facilitating the understanding of the present disclosure and can be appropriately changed according to the use, purpose, specifications, etc. In addition, in the following, when multiple embodiments, variations, etc. are included, it is envisaged from the beginning that these characteristic parts will be used in appropriate combinations.

[0018] Figure 1 It is a cross-sectional view of a cylindrical battery 10 as one embodiment of the present disclosure. Figure 2 2 is a cross-sectional view of the sealing body 20. The cylindrical battery 10 is, for example, a non-aqueous electrolyte secondary battery. Figure 1 as well as Figure 2 In FIG. 1 , the axial center line O is indicated by a dashed line. Hereinafter, in the cylindrical battery 10 , the sealing body side is referred to as “upper”, and the bottom side of the outer can is referred to as “lower”.

[0019] like Figure 1 As shown, the cylindrical battery 10 includes: a bottomed cylindrical outer can 12; an electrode body 14 and an electrolyte (not shown) accommodated inside the outer can 12; and a sealing body 20 fixed to the opening of the outer can 12 by caulking through an insulating gasket 16.

[0020] The outer can 12 is formed, for example, by deep drawing a plate made of a steel material mainly composed of iron. A groove portion 13 is formed at an upper end portion 12a forming an opening of the outer can 12. The groove portion 13 is formed in an annular shape in a plan view, and is formed to protrude inwardly in the radial direction of the outer can 12, for example, in a substantially U-shape. The groove portion 13 becomes a portion on which the outer peripheral edge portion of the sealing body 20 is placed when the outer can 12 is riveted and fixed.

[0021] The outer can 12 contains a cylindrical electrode body 14 formed by winding a positive electrode plate 30 and a negative electrode plate 32 with a separator 34 interposed therebetween, together with an electrolyte. A lower insulating member 36 is interposed between the electrode body 14 and the bottom 12b of the outer can 12. A negative electrode lead 33 is connected to the negative electrode plate 32 constituting the electrode body 14.

[0022] A material that can ensure insulation and has no influence on battery characteristics is used for the lower insulating member 36. As a material used for the lower insulating member 36, a polymer resin is preferable, and examples thereof include polypropylene (PP) resin and polybutylene terephthalate (PBT) resin.

[0023] In the present embodiment, the negative electrode lead 33 is connected to the negative electrode plate 32 at the outermost peripheral position of the electrode body 14. The negative electrode lead 33 extends from the electrode body 14 and is bent radially inward, and is connected to the bottom 12b of the outer can 12 at the lower side of the lower insulating member 36. Thus, in the cylindrical battery 10 of the present embodiment, the outer can 12 functions as a negative electrode terminal. The details of the positive electrode plate 30, the negative electrode plate 32, and the separator 34 constituting the electrode body 14 will be described later.

[0024] The electrode body 14 is accommodated in the outer can 12 at the lower side of the groove 13. An upper insulating member 38 is arranged on the electrode body 14 so that the upper end face of the electrode body 14 in the axial direction does not contact the sealing body 20 and the groove 13 of the outer can 12. The upper insulating member 38 can use a material that can ensure insulation and has no effect on battery characteristics. As a material used for the upper insulating member 38, a polymer resin is preferred, and examples thereof include polypropylene (PP) resin and polybutylene terephthalate (PBT) resin.

[0025] The sealing body 20 is fixed to the upper end portion 12a of the outer can 12 by caulking through the gasket 16. Thus, the interior of the cylindrical battery 10 is sealed, and the sealing body 20 and the outer can 12 are electrically insulated.

[0026] The sealing body 20 includes a sealing plate 22, an insulating plate 24, and a terminal plate 26. The sealing body 20 has a current interruption mechanism. The sealing plate 22 is circular in a plan view and functions as a valve body. The insulating plate 24 is arranged in contact with the surface of the sealing plate 22 on the inner side of the battery.

[0027] The insulating plate 24 is formed in an annular shape in a plan view and has an opening 24 a in the center.

[0028] The terminal plate 26 has a circular shape when viewed from above, and is arranged opposite to the sealing plate 22 with the insulating plate 24 sandwiched therebetween. The sealing plate 22 and the terminal plate 26 are connected to each other at their center portions via the opening 24a of the insulating plate 24, for example, by laser welding or the like. The other end of a positive lead 31 that connects one end to the positive plate 30 constituting the electrode body 14 is connected to the terminal plate 26. The positive lead 31 extends from the electrode body 14 through the upper insulating member 38 and is connected to the terminal plate 26 of the sealing body 20, for example, by laser welding or the like. Thus, in the cylindrical battery 10 of the present embodiment, the positive plate 30 of the electrode body 14 is electrically connected to the sealing plate 22 via the positive lead 31 and the terminal plate 26, and the sealing plate 22 exposed to the outside of the battery in the upper end surface of the cylindrical battery 10 acts as a positive terminal.

[0029] The current interruption mechanism works as follows. A vent hole 26a is provided in the terminal plate 26, and a vent hole 24b is provided in the insulating plate 24. Therefore, if the internal pressure of the battery rises, the sealing plate 22 is subjected to the pressure through the vent hole 26a of the terminal plate 26 and the vent hole 24b of the insulating plate 24. As a result, as the internal pressure of the battery rises, the sealing plate 22 pulls the connection part with the terminal plate 26 to the outside of the battery to play a role. In addition, if the internal pressure of the battery reaches a given value, the connection part of the terminal plate 26 with the sealing plate 22 or the groove 26b provided in the terminal plate 26 will break, and the current path between the sealing plate 22 and the terminal plate 26 will be blocked. Afterwards, if the internal pressure of the battery rises further after the current interruption mechanism works, the thin-walled part of the sealing plate 22, that is, the inclined area 22b described later, will break, and the gas inside the battery will be discharged. That is, the sealing plate 22 acts as a valve body that opens the valve at a given working pressure to release the internal pressure of the battery.

[0030] The sealing plate 22 can be produced by pressing a plate of aluminum or an aluminum alloy. Aluminum and aluminum alloy are preferred as the material of the sealing plate 22 because of their excellent flexibility.

[0031] The sealing plate 22 is circular in plan view. Figure 2 As shown, the surface (or upper surface) of the central area 22a of the sealing plate 22 on the outer side of the battery is formed as a flat surface. A protrusion 25, such as a flat truncated cone, is formed on the surface (or lower surface) of the central area 22a of the sealing plate 22 on the inner side of the battery. The protrusion height of the protrusion 25 is set to be substantially the same as the plate thickness of the insulating plate 24. By forming such a protrusion 25, the sealing plate 22 and the terminal plate 26 can be easily and reliably connected, and a space for the insulating plate 24 to be interposed between the sealing plate 22 and the terminal plate 26 can be ensured.

[0032] The sealing plate 22 has an inclined region 22b integrally on the outer peripheral side of the central region 22a. In the inclined region 22b, the surface on the outer side of the battery rises radially outward to form an inclined surface. Thus, the surface on the outer side of the battery of the sealing plate 22 has a shape in which the central region 22a is recessed toward the inner side of the battery due to the presence of the inclined region 22b.

[0033] In the sealing plate 22, a space 23 having a roughly triangular cross section is formed on the battery inner side of the inclined region 22b. As a result, the inclined region 22b becomes a thin-walled portion whose thickness gradually becomes thinner as it moves radially outward. By forming the inclined region as a thin-walled portion in this way, when the battery internal pressure rises and the pressure acts on the inclined region 22b of the sealing plate 22 from the battery inner side, a rupture occurs at the thinnest portion of the inclined region 22b (i.e., the position corresponding to the vertex of the triangular space 23).

[0034] In addition, in the present embodiment, an example is described in which the inclined region 22b is formed as a thin-walled portion in which the thickness of the sealing plate 22 gradually becomes thinner as it goes radially outward, but the present invention is not limited to this, and the inclined region 22b may be formed as a thin-walled portion in which the thickness gradually becomes thicker as it goes radially outward.

[0035] A protrusion 22c having a circular ring shape in a plan view is formed on the surface of the sealing plate 22 on the inner side of the battery. The protrusion 22c is located radially outward from the inclined region 22b on the surface on the outer side of the battery. The protrusion 22c is formed so that its front end is inclined radially inward, and the insulating plate 24 is embedded and held inside the protrusion 22c.

[0036] The outer peripheral edge portion 27 of the sealing plate 22 riveted and fixed to the outer can 12 is divided into a first part 27a and a second part 27b in the plate thickness direction. Before the sealing plate 22 is riveted and fixed, a space is provided between the first part 27a and the second part 27b. More specifically, the first part 27a and the second part 27b are divided into two parts from the branch start position 28 in the plate thickness of the sealing plate 22. The first part 27a has a shape that is bent obliquely upward relative to the radial direction from the branch start position 28 and then bent in the radial direction. The second part 27b has a shape that is bent obliquely downward relative to the radial direction from the branch start position 28 and then bent in the radial direction. The first part 27a and the second part 27b are opposite to each other in the plate thickness direction of the sealing plate 22, and a cutout portion 29 opening toward the radial outside is formed between the two. The shape of the outer peripheral edge portion 27 of such a sealing plate 22 can be formed in stages, for example, by performing multiple pressing processes.

[0037] The branching start position 28 of the first portion 27a and the second portion 27b is preferably located radially outward of the opening peripheral edge portion 12c of the outer can 12 when the sealing plate 22 is fixed by riveting. Thus, when the sealing plate 22 is fixed by riveting, the first portion 27a and the second portion 27b are compressed in a state of being integrated with each other, and as a result, a radially inward pressing force G (see FIG. 24 ) can be effectively generated on the sealing plate 22. Figure 3 ).

[0038] In addition, the first portion 27a and the second portion 27b are preferably symmetrical with respect to the radial line C passing through the branch start position 28 therebetween. By forming such a shape, when the sealing plate 22 is flattened during riveting, a pressing force in the radially inner direction can be generated on the sealing plate 22. However, the present invention is not limited thereto, and the first portion 27a and the second portion 27b may also be asymmetrical with respect to the radial line C passing through the branch start position 28 therebetween.

[0039] A material that can ensure insulation and has no influence on battery characteristics can be used for the insulating plate 24. As a material used for the insulating plate 24, a polymer resin is preferable, and examples thereof include polypropylene (PP) resin and polybutylene terephthalate (PBT) resin.

[0040] The insulating plate 24 has a skirt portion 24c extending toward the inner side of the battery at its outer periphery. The terminal plate 26 is embedded and held in the inner periphery of the skirt portion 24c. Thus, the outer periphery of the terminal plate 26 is assembled in a state of being engaged with the skirt portion 24c, and the positional displacement of the terminal plate 26 relative to the insulating plate 24 can be reliably prevented.

[0041] The terminal plate 26 is formed into a circle with a smaller diameter than the insulating plate 24 in a plan view, and the central portion is formed into a thin-walled portion. The terminal plate 26 is preferably formed of aluminum or an aluminum alloy like the sealing plate 22. As a result, the sealing plate 22 and the central portion of the terminal plate 26 can be easily connected to each other. As a connection method, laser welding is preferably used. A vent hole 26a is formed through the outer periphery of the terminal plate 26.

[0042] The sealing body 20 is assembled as follows. First, the sealing plate 22, the insulating plate 24, and the terminal plate 26 constituting the sealing body 20 are prepared. Next, the terminal plate 26 is fitted inside the skirt portion 24c of the insulating plate 24, and then the insulating plate 24 is fitted inside the protrusion 22c of the sealing plate 22. The two steps of fitting the above components may be reversed in order.

[0043] The sealing plate 22 and the terminal plate 26 are preferably connected after the above steps are completed. Since the sealing plate 22 and the terminal plate 26 can be connected in a state where they are positioned and held relative to each other, the variation in connection strength can be reduced.

[0044] Next, the electrode body 14 will be described. Figure 1 In the example shown, a cylindrical electrode body 14 is used in which a positive electrode plate 30 and a negative electrode plate 32 are wound with a separator 34 interposed therebetween.

[0045] The positive electrode plate 30 can be produced, for example, in the following manner. First, the positive electrode active material and the binder are kneaded so that they are uniform in the dispersion medium to produce a positive electrode mixture slurry. Polyvinylidene fluoride is preferably used as the binder, and N-methylpyrrolidone is preferably used as the dispersion medium. It is preferred to add a conductive agent such as graphite and carbon black to the positive electrode mixture slurry. The positive electrode mixture slurry is applied to the positive electrode collector and dried to form a positive electrode mixture layer. At this time, a positive electrode collector exposed portion on which a positive electrode mixture layer is not formed is provided on a portion of the positive electrode collector. Next, the positive electrode mixture layer is compressed to a given thickness with a roller, and the compressed electrode plate is cut into a given size. Finally, the positive electrode lead 31 is connected to the exposed portion of the positive electrode collector to obtain the positive electrode plate 30.

[0046] As the positive electrode active material, a lithium transition metal composite oxide that can store and release lithium ions can be used. As the lithium transition metal composite oxide, the general formula LiMO2 (M is C o , Ni, and at least one of Mn), LiMn2O4, and LiFePO4. These can be used alone or in combination of two or more, or at least one selected from the group consisting of Al, Ti, Mg, and Zr can be added, or they can be used in substitution with transition metal elements.

[0047] The negative electrode plate 32 can be produced, for example, in the following manner. First, the negative electrode active material and the binder are kneaded so that they are uniform in the dispersion medium to produce a negative electrode mixture slurry. Styrene butadiene (SBR) copolymer is preferably used as the binder, and water is preferably used as the dispersion medium. A thickener such as carboxymethyl cellulose is preferably added to the negative electrode mixture slurry. The negative electrode mixture slurry is applied to the negative electrode collector and dried to form a negative electrode mixture layer. At this time, a negative electrode collector exposed portion on which the negative electrode mixture layer is not formed is provided on a portion of the negative electrode collector. Next, the negative electrode mixture layer is compressed to a given thickness using a roller, and the compressed electrode plate is cut into a given size. Finally, the negative electrode lead 33 is connected to the exposed portion of the negative electrode collector to obtain the negative electrode plate 32.

[0048] As the negative electrode active material, a carbon material or a metal material that can contain and release lithium ions can be used. As the carbon material, graphite such as natural graphite and artificial graphite can be exemplified. As the metal material, silicon, tin and their oxides can be cited. The carbon material and the metal material can be used alone or in a mixture of two or more.

[0049] As the separator 34, a microporous membrane with polyolefins such as polyethylene (PE) and polypropylene (PP) as the main component can be used. The microporous membrane can be used as a single layer or as a stack of two or more layers. In a stacked separator with more than two layers, it is preferred to set the layer with polyethylene (PE) having a low melting point as the main component as the middle layer, and the polypropylene (PP) having excellent oxidation resistance as the surface layer. Furthermore, inorganic particles such as aluminum oxide (Al2O3), titanium oxide (TiO2) and silicon oxide (SiO2) can be added to the separator 34. Such inorganic particles can be carried in the separator, and can also be coated on the surface of the separator together with an adhesive.

[0050] As the non-aqueous electrolyte solution, a solution obtained by dissolving a lithium salt as an electrolyte salt in a non-aqueous solvent can be used.

[0051] As non-aqueous solvent, cyclic carbonate, linear carbonate, cyclic carboxylic acid ester and linear carboxylic acid ester can be used, and these preferably use by mixing more than 2 kinds.As cyclic carbonate, ethylene carbonate (EC), propylene carbonate (PC) and butylene carbonate (BC) can be exemplified.In addition, cyclic carbonate obtained by replacing a part of hydrogen with fluorine such as fluoroethylene carbonate (FEC) can also be used.As linear carbonate, dimethyl carbonate (DMC), ethyl methyl carbonate (EMC), diethyl carbonate (DEC) and methylpropyl carbonate (MPC) etc. can be exemplified.As cyclic carboxylic acid ester, gamma-butyrolactone (γ-BL) and gamma-valerolactone (γ-VL) can be exemplified, and as linear carboxylic acid ester, methyl pivalate, ethyl pivalate, methyl isobutyrate and methyl propionate can be exemplified.

[0052] Examples of lithium salts include LiPF6, LiBF4, LiCF3SO3, LiN(CF3SO2)2, LiN(C2F5SO2)2, LiN(CF3SO2)(C4F9SO2), LiC(CF3SO2)3, LiC(C2F5SO2)3, LiAsF6, LiClO4, Li2B 10 Cl 10 and Li2B 12 Cl 12 Among these, LiPF6 is particularly preferred, and its concentration in the non-aqueous electrolyte is preferably 0.5 to 2.0 mol / L. Other lithium salts such as LiBF4 may also be mixed with LiPF6.

[0053] Next, refer to Figure 3 The riveting and fixing of the sealing body 20 will be described. Figure 3 (a) is a cross-sectional view showing the radial half of the sealing body 20 and its vicinity before riveting and fixing, Figure 3 (b) is a cross-sectional view of the sealing body 20 and its vicinity in the radial direction half when the sealing body 20 is fixed by riveting. Figure 3 In (a) and (b), the positive electrode lead 31, the electrode body 14, and the like are omitted from illustration.

[0054] When the sealing body 20 is riveted and fixed to the outer can 12, Figure 3 As shown in (a), the outer peripheral edge portion 27 of the sealing plate 22 is placed on the groove portion 13 of the outer can 12 via the gasket 16. In this state, Figure 3 As shown in (b), the upper end portion 12a of the outer can 12 is bent radially inward using a die (not shown), and the sealing body 20 is riveted and fixed.

[0055] At this time, the maximum pushing force F acts on the outer peripheral edge 27 of the sealing plate 22 at the position corresponding to the peripheral edge 12c of the opening of the outer can 12. As a result, the first part 27a and the second part 27b, which are formed by branching into two parts before riveting and fixing, are in a state of being flattened into one body, and at this time, a radially inward pressing force G acts on the outer peripheral edge 27 of the sealing plate 22. In addition, the sealing plate 22 has a shape in which the central area 22a of the surface on the outer side of the battery is concave toward the inner side of the battery due to the presence of the inclined area 22b. Therefore, during riveting and fixing, the sealing plate 22 is reliably assembled in a shape in which the central area 22a is warped downward (in the direction of arrow A) into a concave shape by the radially inward pressing force G acting on the outer peripheral edge 27.

[0056] When the riveting is completed and the cylindrical battery 10 is removed from the mold, the sealing plate 22 and the sealing body 20 including the sealing plate 22 are rebounded to the position where the cylindrical battery 10 is removed from the mold. Figure 3 The position indicated by the two-dot chain line in (b) of FIG. 2 can be returned to the desired position by setting the shapes of the first portion 27a and the second portion 27b of the outer peripheral edge portion 27 of the sealing plate 22, the size of the cutout portion 29, etc.

[0057] As described above, according to the cylindrical battery 10 of the present embodiment, the sealing plate 22 forms a circular shape in a plan view, and has a shape in which its central area 22a is recessed toward the inner side of the battery, and the outer peripheral edge portion 27 of the sealing plate 22 riveted and fixed to the outer can 12 is divided into a first part 27a and a second part 27b in the plate thickness direction. Before the sealing plate 22 is riveted and fixed, a space is provided between the first part 27a and the second part 27b. Thus, when the sealing plate 22 and the sealing body 20 including it are riveted and fixed to the outer can 12, they can be reliably assembled in a shape that warps downward. Therefore, when the cylindrical battery assembled in a shape in which the sealing body 20 is warped upward is assembled as a battery module, it is possible to prevent interference with the external lead for extracting the output current from the cylindrical battery 10 and damage to the sealing body 20.

[0058] In addition, the cylindrical battery according to the present disclosure is not limited to the above-described embodiment and its modified examples, and various changes and improvements can be made within the scope of the matters described in the claims of the present application.

[0059] For example, Figure 4 As shown in (a), the first portion 27a and the second portion 27b formed on the outer peripheral edge portion 27 of the sealing plate 22 may be formed in a Y-shape toward the radially outer side, or may be formed as shown in Figure 4 As shown in (b) and (c) of FIG. 1 , the first portion 27a and the second portion 27b do not expand in the plate thickness direction, and the cutout portion 29 is formed in a V-shape or a U-shape.

[0060] Description of Reference Numerals

[0061] 10 cylindrical battery, 12 outer can, 12a upper end, 12b bottom, 12c peripheral edge, 13 groove, 14 electrode body, 16 gasket, 20 sealing body, 22 sealing plate, 22a central area, 22b inclined area, 22c protrusion, 23 space, 24 insulating plate, 24a opening, 24b, 26a vents, 24c skirt, 25 protrusion, 26 terminal plate, 26b groove, 27 peripheral edge, 27a first part, 27b second part, 29 branch start position, 29 groove, 30 positive plate, 31 positive lead, 32 negative plate, 33 negative lead, 34 separator, 36 lower insulating member, 38 upper insulating member, F pushing force, G pressing force, C radial line, O center line.

Claims

1. A cylindrical battery comprising: An electrode body formed by winding a positive electrode plate and a negative electrode plate with a separator between them; Electrolyte; a bottomed cylindrical outer container for accommodating the electrode assembly and the electrolyte; and a sealing plate fixed to the opening of the outer can by riveting via a gasket, The sealing plate is circular in plan view and has a shape in which its central area is recessed toward the inner side of the battery. The outer peripheral edge of the sealing plate is riveted and fixed to the outer can. A groove portion is provided on the outer peripheral surface of the sealing plate. The outer peripheral edge of the sealing plate is divided into a first part and a second part in the direction of the plate thickness by the groove portion.

2. The cylindrical battery according to claim 1, wherein: The cutout portion is provided on the outer peripheral side of the sealing plate relative to a branching start position of the first portion and the second portion, and the branching start position is located radially outward relative to a peripheral edge of the opening of the outer can.

3. The cylindrical battery according to claim 1 or 2, wherein: The first portion and the second portion are symmetrically shaped with respect to a radial line passing through a branch start position therebetween.

Citation Information

Patent Citations

  • Cylindrical sealed battery and battery pack

    WO2015146078A1

  • Cylindrical sealed battery and battery pack

    CN106030855A

  • Cylindrical battery

    CN107431179A

  • JP1973102517U