Flexible display panel and manufacturing method thereof

By forming a multi-layer open structure and separation layer on the substrate of the flexible display panel, the problem of cracks during the peeling process is solved, the reliability and life of the display panel are improved, and the penetration is prevented.

CN113261105BActive Publication Date: 2024-11-26BOE TECHNOLOGY GROUP CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN201980002646.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-11-28
Publication Date
2024-11-26
Estimated Expiration
2040-03-12

AI Technical Summary

Technical Problem

Existing flexible display panels are prone to cracks during peeling, resulting in moisture or air penetration, reducing reliability and life.

Method used

The peeling force is reduced by forming an opening structure with different widths on the substrate, including a first opening, a second opening, a third opening and a fourth opening, and a separation layer and a packaging layer are used to reduce the peeling force, and the generation of cracks is prevented.

Benefits of technology

It significantly reduces the mechanical force during peeling, reduces the incidence of cracks, improves the reliability and life of the display panel, and prevents air or moisture from penetrating.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113261105B_ABST
    Figure CN113261105B_ABST
Patent Text Reader

Abstract

The present disclosure relates to a method for manufacturing a display panel. The method may include: forming a separation layer having a first opening on a surface of a substrate; forming a flexible substrate layer covering the separation layer and the first opening; forming a TFT layer having a second opening on a surface of the flexible substrate layer opposite to the substrate; removing a portion of the flexible substrate layer located below the second opening; forming a PDL layer covering the TFT layer, a sidewall of the third opening, and a portion of the separation layer in the third opening, thereby forming a fourth opening having a fourth width greater than the first width; forming an encapsulation layer covering the PDL layer and the fourth opening; and separating the flexible substrate layer from the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to display technology, and in particular to a flexible display panel, a method for manufacturing a flexible display panel, and a display device. Background Art

[0002] Flexible display devices are display devices formed on flexible substrates. Recently, stretchable flexible screens have attracted widespread attention due to their wide viewing angles, ease of portability, and their ability to be rolled up, especially for biomedical and wearable applications.

[0003] Typically, stretchable displays are made using flexible layers with island-bridge structures to enhance the stretchability of functional devices. In the island-bridge structure, thin film transistors and electroluminescent devices are manufactured in the islands. These devices are interconnected by interconnects or flexible bridges. These stretchable interconnects can be prepared by the following methods: using highly ductile / compliant electronic materials (such as low-temperature liquid metals) or by designing interconnects to reduce local strains by out-of-plan deformation. The openings in the flexible substrate can be adapted to the strain applied to the stretchable display device and undergo large and reversible deformations. Summary of the invention

[0004] One embodiment of the present disclosure is a method for manufacturing a display panel. The method may include: providing a substrate; forming a separation layer having a first opening on a surface of the substrate, wherein the first opening has a first width and a first thickness; forming a flexible substrate layer covering the separation layer and the first opening; forming a TFT layer having a second opening on a surface of the flexible substrate layer opposite to the substrate, wherein the second opening is located above the first opening and has a second width greater than the first width; removing a portion of the flexible substrate layer located below the second opening, thereby forming a third opening having a third width in the TFT layer and the flexible substrate layer; forming a PDL layer covering the TFT layer, a sidewall of the third opening, and a portion of the separation layer in the third opening, thereby forming a fourth opening having a fourth width greater than the first width in the PDL layer; forming an encapsulation layer covering the PDL layer and the fourth opening; and separating the flexible substrate layer from the substrate.

[0005] Optionally, forming a separation layer having a first opening on the surface of the substrate may include: forming a metal layer having the first thickness on the surface of the substrate; and annealing the metal layer to form a metal oxide layer on a surface of the metal layer opposite to the substrate.

[0006] Optionally, before annealing the metal layer, the method may further include: patterning the metal layer to form the first opening having the first width.

[0007] Optionally, after annealing the metal layer, the method may further include: patterning the metal oxide layer to form the first opening having the first width.

[0008] Optionally, an orthographic projection of each of the fourth openings on the substrate may cover an orthographic projection of one of the first openings on the substrate.

[0009] Optionally, a center of an orthographic projection of each of the fourth openings on the substrate may substantially coincide with a center of an orthographic projection of each of the first openings on the substrate.

[0010] Optionally, after forming the PDL layer and before separating the flexible substrate layer from the substrate, the method may further include: forming an EL material layer on the TFT layer.

[0011] Alternatively, separating the flexible substrate layer from the substrate may be performed by mechanical force.

[0012] Optionally, the method may further include: adhering a stretchable film to a surface of the flexible substrate layer opposite to the TFT layer.

[0013] Alternatively, the first width of each of the first openings may be in a range of 1 μm to 5 μm, and at least twice smaller than the third width of each of the third openings.

[0014] Optionally, the first thickness of each of the first openings may be to within the range.

[0015] Optionally, the first width of each of the first openings may be smaller than the second width of each of the second openings and the third width of each of the third openings.

[0016] Optionally, removing the portion of the flexible substrate layer located below the second opening to form a third opening having a third width in the TFT layer and the flexible substrate layer may include: a patterning process, a developing process, and an etching process.

[0017] Optionally, the separation layer is made of molybdenum (Mo) or tungsten (W).

[0018] Optionally, the flexible substrate layer may include polyimide.

[0019] Optionally, the substrate may be a glass substrate.

[0020] Alternatively, the encapsulation layer may include a first inorganic layer, an organic layer, and a second inorganic layer in sequence.

[0021] Optionally, the first inorganic layer may include SiON9, and the second inorganic layer may include SiN x .

[0022] Another embodiment of the present disclosure is a display panel formed by the above method.

[0023] Another embodiment of the present disclosure is a display device including a display panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] The accompanying drawings are intended to provide a further understanding of the technical solution of the present disclosure and are intended to be a part of the specification and used to explain the technical solution of the present disclosure, but do not constitute a limitation on the technical solution of the present disclosure.

[0025] Figure 1 is a diagram illustrating a method of manufacturing a stretchable flexible display panel in the related art;

[0026] Figure 2 is a top view of a portion of a stretchable flexible display panel in the related art;

[0027] Figure 3 is a top view of a pattern of a flexible substrate layer on a substrate according to one embodiment of the present disclosure;

[0028] Figure 4 is an enlarged top view of a pattern of a flexible substrate layer on a substrate according to one embodiment of the present disclosure;

[0029] Figure 5 is an enlarged top view of a pattern of a flexible substrate layer on a substrate according to one embodiment of the present disclosure; and

[0030] 6A to 6F for Figure 3-Figure 5 A cross-sectional view along line AA′ shows a method for manufacturing a stretchable flexible display panel according to an embodiment of the present disclosure. DETAILED DESCRIPTION

[0031] The present disclosure will be further described in detail with reference to the accompanying drawings and embodiments to provide those skilled in the art with a better understanding of the technical solutions of the present disclosure. Figure 1 To Figure 6. When referring to the drawings, like structures and elements are represented by like reference numerals throughout.

[0032] In the description of the following embodiments, specific features, structures, materials or characteristics may be combined in any suitable manner in any one or more embodiments or examples.

[0033] Figure 1 A diagram of a method for manufacturing a stretchable flexible display panel in the related art is shown. A stretchable flexible display panel is generally manufactured by using a flexible substrate layer having an island-bridge structure to further enhance the stretchability of the display panel. Thin film transistors (TFTs) and electroluminescent (EL) devices are manufactured on islands of the flexible substrate layer. In the island-bridge structure, the islands are separated by holes, grooves, or openings and can be connected by interconnects or flexible bridges to reduce the strain applied to the flexible substrate layer. Therefore, the stretchable flexible display panel can withstand significant and reversible deformation.

[0034] Flexible substrate layers with island-bridge configurations can be prepared by utilizing highly ductile / compliant electronic materials (e.g., low-temperature liquid metals), and the interconnects or bridges can be designed into different shapes or configurations to, for example, relieve local strains through out-of-plane deformation.

[0035] like Figure 1 As shown, the flexible substrate layer is usually made of polyimide (PI) and is first manufactured on a rigid substrate such as a glass substrate. After the subsequent manufacturing process, a thin film encapsulation (TFE) layer may be used to encapsulate the manufactured components and prevent air and moisture from penetrating into the stretchable flexible display panel. Then, a laser lift-off (LLO) process may be performed to peel the flexible substrate layer from the rigid substrate. The stretchable substrate may then be adhered to the surface of the flexible substrate layer opposite to the TFE layer. However, as Figure 2 As shown in FIG, since the flexible substrate layer is in direct contact with the rigid substrate, a large peeling force is required to peel the flexible substrate layer from the rigid substrate. However, this large peeling force will cause large-area cracks around the bridge and edge of the flexible substrate layer, as shown in FIG. Figure 2 As shown by the arrow in , the reliability and life of the display panel are affected. In addition, because cracks are more likely to occur at the edge of the island of the flexible substrate layer, such as Figure 1 As shown by the solid line in FIG, the side surface of the flexible substrate layer can be easily exposed. In this way, moisture or air will penetrate into the flexible display panel through the cracks at the edges of the islands of the flexible display panel, thereby reducing the reliability and life of the flexible display panel.

[0036] An embodiment of the present disclosure provides a method for manufacturing a stretchable flexible display panel, which includes the following steps S10 to S70.

[0037] In one embodiment, step S10 includes: providing a substrate 500, and forming a separation layer 510 having first openings 515 on a surface of the substrate 500. Each of the first openings may have a first width and a first thickness. Figure 3 FIG. 2 shows a top view of a separation layer on a substrate according to an embodiment of the present disclosure. Figure 3 As shown, the first opening 210 is a plurality of grooves having an elliptical shape. The elliptical shape has two opposite long sides parallel to each other, and two opposite short sides respectively have an arc shape. The plurality of elliptical grooves are arranged to form a plurality of islands 220 connected by a plurality of bridges 230, thereby forming an island-bridge structure. Figure 3 As shown, in one embodiment, because the two short sides of the elliptical groove have arc shapes respectively, one side of the bridge 230 may have a curved concave shape to achieve greater strain caused by bending, folding and stretching.

[0038] Will refer to FIG. 6A to FIG. 6E A method of manufacturing a stretchable flexible display panel according to some embodiments of the present disclosure is described in more detail. FIG. 6A to FIG. 6E for Figures 3 to 5 A cross-sectional view along line AA′ shows a method for manufacturing a stretchable flexible display panel according to an embodiment of the present disclosure.

[0039] In one embodiment, forming a separation layer having a first opening on a surface of a substrate includes forming a metal layer having a first thickness on the surface of the substrate, and annealing the metal layer to form a metal oxide layer on a surface of the metal layer opposite to the substrate.

[0040] In one embodiment, forming a separation layer having a first opening on the surface of the substrate further comprises: before annealing the metal layer, patterning the metal layer to form a first opening having a first width. In one embodiment, forming a separation layer having a first opening on the surface of the substrate further comprises: after annealing the metal layer, patterning the metal layer to form a first opening having a first width.

[0041] like Fig. 6A As shown, the substrate 500 may be a rigid substrate, such as a glass substrate, etc. The separation layer 510 may be formed on the surface of the substrate 500 by a technique such as vacuum deposition, chemical vapor deposition, or sputtering.

[0042] The separation layer 510 may be a metal layer and may be made of molybdenum Mo or tungsten W. The thickness of the metal layer may be about to In one embodiment, the metal layer is subjected to heat treatment or annealing treatment at a high temperature of about 350° C., for example, in an air atmosphere or an oxygen environment. Thus, during the heating or annealing treatment, a metal oxide layer, for example, a molybdenum oxide layer or a tungsten oxide layer, is formed on the surface of the metal layer opposite to the substrate.

[0043] In one embodiment, the metal layer is patterned, such as by photolithography, to produce a separation layer having a first opening, such as Fig. 6A As shown. The size (e.g., width and thickness) of the first opening and the shape of the first opening may vary based on the stretching requirements. The patterning process may include the steps of applying a photoresist layer on the metal layer, patterning the photoresist layer, and etching the underlying metal layer using the patterned photoresist layer as a mask.

[0044] Figure 4 FIG. 1 shows an enlarged top view of a pattern of a flexible substrate layer on a substrate according to an embodiment of the present disclosure. Figure 4 As shown, some of the first openings 210 may be formed in an H shape to better isolate the islands 220, thereby obtaining the desired flexibility. The islands 220 are connected by bridges 230 having straight lines. The islands of the cyclic pattern are formed by the arrangement of the H-shaped first openings, such as Figure 4 shown.

[0045] Figure 5 FIG. 1 shows an enlarged top view of a pattern of a flexible substrate layer on a substrate according to an embodiment of the present disclosure. The first openings 210 are straight elliptical shapes separated from each other. The width of the first openings is small, so that the bridges 230 are short in this island-bridge configuration. The arrangement of the openings also forms a repeating pattern of islands, such as Figure 5 The "width" of the first opening in this article refers to the width of the ellipse in a direction perpendicular to the long side of the ellipse, for example, along Figures 3 to 5 The size (eg, width) of the first opening and the shape of the first opening may vary according to the stretching requirements. The width of the first opening may be in the range of about 1 μm to 5 μm.

[0046] In one embodiment, Figure 6B As shown, step S20 includes: forming a flexible substrate layer 520 covering the separation layer and the first opening. The flexible substrate layer 520 covers the separation layer 510 and fills the first opening 515. The flexible substrate layer can be made of a polymer such as polyimide. The thickness of the flexible substrate layer can be in the range of about 5μm to 25μm. In one embodiment, first, a polymer solution such as a polyimide solution can be used to coat the separation layer. Then, a step such as vacuum heat drying (HVCD) and baking in an oven is used to cure the coating of the polymer solution to form a flexible substrate layer on the substrate.

[0047] In one embodiment, Figure 6C As shown, step S30 includes: forming a thin film transistor (TFT) layer 530 having a second opening 525 on a surface of the flexible substrate layer 520 opposite to the substrate. The second opening may be above the first opening and have a second width, which is greater than the first width of the first opening. The TFT layer may include a thin film transistor array, which includes a plurality of thin film transistors separated from each other. Forming the TFT layer may include: forming a planarization (PLN) layer on the thin film transistor array so that the TFT layer has a flat surface on the side opposite to the substrate. As shown Figure 6C As shown, the TFT layer has a second opening located above the first opening. The second width of the second opening is greater than the first width of the first opening. The orthographic projection of the second opening on the substrate may cover the orthographic projection of the first opening on the substrate. In one embodiment, the central axis of each second opening may coincide with or substantially coincide with the central axis of one of the first openings. That is, the center of the orthographic projection of the second opening on the substrate may coincide with or substantially coincide with the center of the orthographic projection of the first opening on the substrate.

[0048] In one embodiment, Fig.6D As shown, step S40 includes: removing a portion of the flexible substrate layer 520 below the second opening 525, thereby forming a third opening 535 having a third width in the TFT layer 530 and the flexible substrate layer 520. Typically, the width of the third opening may be in the range of approximately 5 μm to 15 μm. In some cases, the width of the third opening may be increased to 200 μm, but a large opening may sacrifice display resolution due to increased spacing between islands. In one embodiment, patterning, developing, and etching processes may be performed on the flexible substrate layer to remove a portion of the flexible substrate below the second opening. In this way, a plurality of third openings are formed in the flexible substrate layer and the TFT layer. Each of the third openings has a third width. The third width of the third opening is greater than the first width of the first opening. The orthographic projection of the third opening on the substrate may cover the orthographic projection of the first opening on the substrate. The third opening may include a previous second opening and have the same width as the second opening, such as Fig.6D As shown. The sidewall of the third opening may include the side surface of the TFT layer and the side surface of the flexible substrate layer. The bottom surface of the third opening may include a separation layer and a first opening exposing the underlying substrate. In one embodiment, the central axis of each third opening coincides or substantially coincides with the central axis of one of the first openings. That is, the center of the orthographic projection of the third opening on the substrate may coincide or substantially coincide with the center of the orthographic projection of the first opening on the substrate.

[0049] In one embodiment, Fig. 6EAs shown, step S50 includes: forming a pixel definition layer (PDL) layer 540 on the TFT layer. The PDL layer defines a plurality of pixel wells on the TFT layer. The PDL layer also covers the sidewalls of the third opening (i.e., the side surface of the TFT layer and the side surface of the flexible substrate layer) and a portion of the separation layer at the bottom of the third opening, thereby forming a fourth opening 545 having a fourth width. In this way, the sidewalls of the fourth opening are covered by the PDL layer, and the bottom surface of each fourth opening includes a portion of the PDL layer, a portion of the separation layer, and a first opening exposing the underlying substrate. Because the sidewalls of the third opening are covered by the PDL layer, each fourth opening has a fourth width, which is greater than the first width of the first opening but less than the third width of the third opening. The orthographic projection of each fourth opening on the substrate covers the orthographic projection of one of the first openings on the substrate. The thickness of the PDL layer may be in the range of 1 μm to 5 μm. The width of the fourth opening may be in the range of 2 μm to 13 μm. In one embodiment, the central axis of the fourth opening coincides or substantially coincides with the central axis of the first opening. The center of the orthographic projection of the fourth opening on the substrate coincides or substantially coincides with the center of the orthographic projection of the first opening on the substrate.

[0050] In one embodiment, Fig. 6F As shown, step S60 includes: forming an encapsulation layer 550 covering the PDL layer and the fourth opening. The encapsulation layer can protect the flexible display panel from external environments such as moisture and air. The encapsulation layer can have a substantially uniform thickness. In one embodiment, the encapsulation layer uses a thin film encapsulation (TFE) layer, which includes a first inorganic layer, an organic layer, and a second inorganic layer in sequence. The first inorganic layer may include SiON9 with a thickness of about to about The thickness of the organic layer may be approximately in the range of about 8 μm to about 10 μm. The second inorganic layer may include SiN x , thickness is about to about The TFE layer covers the side surface and the bottom surface of the fourth opening. Therefore, the TFE layer covers a portion of the PDL layer and a portion of the separation layer at the bottom surface of the fourth opening. In addition, the TFE layer fills the first opening and directly contacts the lower substrate in the first opening. Fig. 6F As shown, the openings between the islands may be referred to as PI openings. The width of the PI opening is equal to the width of the third opening. Because the second opening is formed in the TFT layer, which is fabricated on the flexible substrate layer, the width of the second opening in the TFT layer may be equal to or less than the width of the third opening in the flexible substrate layer.

[0051] In one embodiment, after forming the PDL layer and before separating the flexible substrate layer from the substrate, the method further includes: forming an electroluminescent (EL) layer in a plurality of pixel wells on the TFT layer. The EL layer may include at least one of a cathode layer, a hole injection layer, a hole transport layer, a light emitting layer, an electron injection layer, an electron transport layer, and an anode layer, or a combination thereof.

[0052] In one embodiment, step S70 includes: separating the flexible substrate layer from the substrate. In one embodiment, a mechanical force is applied to separate the flexible substrate layer from the substrate. In step S70, a laser lift-off (LLO) process may be used to peel the flexible substrate layer from the substrate.

[0053] According to some embodiments of the present disclosure, since there is a separation layer between the flexible substrate layer and the substrate, the mechanical force required to peel the flexible substrate layer from the substrate is significantly reduced compared to the related art. In addition, since the first width of the first opening is much smaller than the third width of the third opening, the contact area between the encapsulation layer and the substrate is significantly reduced. Therefore, if cracks are generated during peeling, cracks are easily generated at the edge of the first opening of the TFE layer, such as Fig. 6F As shown by the solid line in the middle. Since the first width of the first opening is much smaller than the fourth width of the fourth opening, any cracks generated are far away from the flexible substrate layer. Therefore, the side surface of the flexible substrate layer is still completely covered and protected by the TFE layer. In this way, no air or moisture will penetrate into the display panel through the cracks, thereby improving the reliability and life of the display panel.

[0054] In one embodiment, after separating the flexible substrate layer from the substrate, the method of forming a display panel may further include: adhering a stretchable film to a surface of the flexible substrate layer opposite to the TFT layer.

[0055] In one embodiment, before attaching the stretchable film, a temporary protection film (TPF) may be formed on a surface of the encapsulation layer opposite to the substrate as a protection layer to protect the encapsulation layer during separation of the flexible substrate layer from the substrate.

[0056] After the stretchable film is adhered, the temporary protective film may be removed, and subsequent processes of forming a touch layer, a polarizer layer, and a cover glass may then be performed to complete the manufacture of the stretchable flexible display panel.

[0057] Some embodiments of the present disclosure provide a method for manufacturing a stretchable flexible display panel. A separation layer having a first opening is formed between the flexible substrate layer and the substrate, and an encapsulation layer having a fourth opening is used to protect the stretchable flexible display panel. The width of the first opening of the separation layer is much smaller than the width of the fourth opening of the flexible substrate layer, so that during the separation of the flexible substrate layer from the underlying substrate, cracks are generated in the encapsulation layer instead of any cracks in the flexible substrate layer, thereby reducing the disconnection of traces caused by cracks. At the same time, the cracks are away from the side surface of the flexible substrate layer. Therefore, the encapsulation layer can still effectively protect the display panel and prevent air or moisture from penetrating into the display panel through the cracks, thereby improving the reliability and life of the display panel.

[0058] Another embodiment of the present disclosure further provides a display panel, which is manufactured by a method of an embodiment of the present disclosure. The stretchable flexible display panel may include a stretchable substrate, and a flexible substrate layer 520, a TFT layer 530, a PDL layer 540 and an encapsulation layer 550 on the stretchable substrate in sequence.

[0059] Another embodiment of the present disclosure further provides a display device, which includes a display panel according to one embodiment of the present disclosure.

[0060] Compared with the prior art, the beneficial effects of the display device provided in some embodiments of the present disclosure are the same as those of the above-mentioned display panel, and therefore will not be described in detail here.

[0061] In one embodiment, the display device may be any product or component having a display function, such as a mobile phone, a tablet computer, a television, a monitor, a notebook computer, a digital photo frame, or a navigator.

[0062] Unless otherwise defined, the technical terms or scientific terms used in this disclosure are intended to have the common meaning of those of ordinary skill in the art. The words "first", "second" and similar words used in this disclosure do not represent any order, quantity or importance, but are only used to distinguish different components. The words "include" or "comprise" etc. refer to that the element or item before the word includes the element or item listed after the word and its equivalent, and do not exclude other parts or objects. "Coupling" etc. are not limited to physical connection or mechanical connection, but can include direct electrical connection or indirect electrical connection. "Up", "down", "left", "right" etc. are only used to indicate relative position relationship. When the absolute position of the object being described changes, the relative position relationship can also change accordingly.

[0063] The principles and embodiments of the present disclosure are set forth in the specification. The description of the embodiments of the present invention is only used to help understand the methods of the present disclosure and their core ideas. At the same time, for those of ordinary skill in the art, the present disclosure relates to the scope of the present disclosure, and the technical embodiments of the present disclosure are not limited to the specific combination of technical features, and without departing from the concept of the present invention, other technical embodiments formed by combining technical features or equivalent features of technical features should also be covered. For example, a technical embodiment can be obtained by replacing the above-mentioned features (but not limited to) as disclosed in the present disclosure with similar features.

Claims

1. A method for manufacturing a display panel, include: providing a substrate; forming a separation layer having a first opening on a surface of the substrate, wherein the first opening has a first width and a first thickness; forming a flexible substrate layer covering the separation layer and the first opening; forming a thin film transistor layer having a second opening on a surface of the flexible substrate layer opposite to the substrate, wherein the second opening is located above the first opening and has a second width greater than the first width; removing a portion of the flexible substrate layer located below the second opening, thereby forming a third opening having a third width in the thin film transistor layer and the flexible substrate layer; forming a pixel defining layer covering the thin film transistor layer, the sidewall of the third opening, and a portion of the separation layer in the third opening, thereby forming a fourth opening having a fourth width greater than the first width; forming an encapsulation layer covering the pixel defining layer and the fourth opening; and The flexible substrate layer is separated from the substrate.

2. The method according to claim 1, wherein the separation layer having the first opening is formed on the surface of the substrate include: forming a metal layer having the first thickness on the surface of the substrate; as well as The metal layer is annealed to form a metal oxide layer on a surface of the metal layer opposite to the substrate.

3. The method according to claim 2, before annealing the metal layer, include: The metal layer is patterned to form the first opening having the first width.

4. The method according to claim 2, further comprising: include: The metal oxide layer is patterned to form the first opening having the first width.

5. The method according to claim 1, in, An orthographic projection of each of the fourth openings on the substrate covers an orthographic projection of one of the first openings on the substrate.

6. The method of claim 5, wherein a center of an orthographic projection of each of the fourth openings on the substrate substantially coincides with a center of an orthographic projection of one of the first openings on the substrate.

7. The method according to claim 1, after forming the pixel defining layer and before separating the flexible substrate layer from the substrate, further comprising: include: An electroluminescent material layer is formed on the thin film transistor layer.

8. The method according to claim 1, in, Separating the flexible substrate layer from the substrate is performed by mechanical force.

9. The method according to claim 1, further comprising: include: A stretchable film is adhered to a surface of the flexible substrate layer opposite to the thin film transistor layer.

10. The method according to claim 1, in, The first width of each of the first openings is in a range of 1 μm to 5 μm, and is at least two times smaller than the third width of each of the third openings.

11. The method according to claim 1, in, The first thickness of each of the first openings is to within the range.

12. The method according to claim 1, in, The first width of each of the first openings is smaller than the second width of each of the second openings and the third width of each of the third openings.

13. The method according to claim 1, wherein the portion of the flexible substrate layer located below the second opening is removed, thereby forming a third opening having a third width in the thin film transistor layer and the flexible substrate layer. include: Patterning process, developing process and etching process.

14. The method according to claim 1, in, The separation layer is made of molybdenum or tungsten.

15. The method according to claim 1, in, The flexible substrate layer includes polyimide.

16. The method according to claim 1, wherein the substrate is a glass substrate.

17. The method according to claim 1, wherein the encapsulation layer comprises a first inorganic layer, an organic layer, and a second inorganic layer in sequence.

18. The method according to claim 17, in, The first inorganic layer includes SiON 9 , and the second inorganic layer includes SiN x .

19. A display panel formed by the method according to any one of claims 1 to 18.

20. A display device comprising the display panel according to claim 19.

Citation Information

Patent Citations

  • Thin film transistor structure

    CN102130178A

  • Organic Light-emitting Diode Display With Bent Substrate

    CN105789252A

  • Method for stripping flexible display panel

    CN108695446A

  • Method for manufacturing flexible display device

    CN109075254A

  • Flexible substrate, array substrate, display panel, manufacturing method and display device

    CN109192858A