A method for manufacturing a solar cell using an inverted pyramid velvet surface
By using a masking structure to perform laser or plasma etching to form an inverted pyramid texture during the manufacturing process of solar cells, and depositing a passivation film, the problems of heavy metal contamination and texture uniformity control are solved, and the performance and production of solar cells are improved. efficiency.
Patent Information
- Application Number
- CN202110992690.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-08-27
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-08-27
AI Technical Summary
The preparation method of inverted pyramid suede in the prior art has problems such as heavy metal pollution, potential environmental pollution risks, and difficulty in controlling the size and uniformity of the suede, which affects the performance and production efficiency of solar cells.
The first masking structure is used for laser or plasma etching to form an inverted pyramid texture, and the second masking structure is used for passivation film deposition to avoid heavy metal contamination, ensure the size and uniformity of the texture, and improve the passivation quality.
The preparation of inverted pyramid suede without heavy metal pollution has been achieved, the control accuracy of the suede size and passivation quality have been improved, and the performance and production efficiency of solar cells have been improved.
Smart Images

Figure CN113707764B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing a solar cell using an inverted pyramid velvet surface. Background Art
[0002] In the process of manufacturing heterojunction solar cells, texturing and cleaning are one of the essential key steps. Texturing can form a pyramid velvet surface on the surface of the cell to reduce the reflection of incident light and increase the short-circuit current.
[0003] The general texturing of single crystal or cast single crystal silicon wafers is assisted by additives, using alkaline solution for anisotropic reaction to form a positive pyramid texture. However, the positive pyramid texture has poor light absorption when the light is not direct or the ambient light is mostly scattered light, and the protruding pyramid tip is easily damaged by wear in the subsequent process, resulting in passivation failure and PN junction damage, affecting the yield and efficiency of the cell.
[0004] Therefore, the inverted pyramid velvet has better weak light absorption ability than the forward pyramid velvet, and the sunken velvet is less susceptible to damage from subsequent processes. At present, most inverted pyramid velvets are prepared by using metal ion-assisted velveting to form holes and then anisotropically reacting with alkaline solutions. However, the above method has high requirements for the subsequent cleaning of silicon wafers, and is prone to heavy metal pollution, which affects the surface passivation of silicon wafers; secondly, heavy metal ions in the solution, such as silver ions and copper ions, pose a hidden danger to environmental pollution, and the cost of waste liquid treatment in the later stage is high, which is not conducive to large-scale production; thirdly, the size and uniformity of the inverted pyramid velvet play a key role in the subsequent battery production, and the use of metal ion-assisted velveting often cannot uniformly control the size of the velvet. Summary of the invention
[0005] The purpose of the present invention is to provide a method for manufacturing a solar cell using an inverted pyramid velvet surface, which is different from the traditional inverted pyramid velvet surface preparation method and improves the velvet preparation effect.
[0006] The purpose of the present invention is achieved through the following technical solutions:
[0007] A method for manufacturing a solar cell using an inverted pyramid velvet surface comprises the following steps:
[0008] Step A, performing inverted pyramid texturing on a semiconductor substrate;
[0009] Step B, passivating the surface of the semiconductor substrate processed in step A.
[0010] Compared with the prior art, the advantages of the present invention are:
[0011] (1) The size of the inverted pyramid can be uniformly controlled by utilizing the mesh size of the first masking structure, which is beneficial to experimental design and production requirements;
[0012] (2) Using dry methods such as laser etching or plasma etching avoids heavy metal pollution during the process, which is beneficial to subsequent passivation and efficiency improvement;
[0013] (3) The first passivation is performed using the second masking structure to uniformly cover the inverted pyramid groove surface, and then the second masking structure is removed to perform the second passivation, which is beneficial for the overall coverage of the passivation film layer on the surface of the semiconductor substrate and is beneficial for improving the passivation quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a structural diagram of an embodiment of the first masking structure or the second masking structure of the present invention.
[0015] Figure 2 This is a distribution diagram of an embodiment of laser etching using the first masking structure of the present invention, in which the laser, the mask plate and the silicon wafer are shown from top to bottom.
[0016] Figure 3 It is a simplified process flow diagram of an embodiment of the present invention. DETAILED DESCRIPTION
[0017] A method for manufacturing a solar cell using an inverted pyramid velvet surface comprises the following steps:
[0018] Step A, performing inverted pyramid texturing on a semiconductor substrate;
[0019] Step B, passivating the surface of the semiconductor substrate processed in step A.
[0020] The specific method of step B is to place a second masking structure with mesh holes on the surface of the semiconductor substrate, perform a first passivation film deposition, and then remove the second masking structure to perform a second passivation film deposition. The first passivation film deposition can first cover the groove surface of the inverted pyramid velvet surface to avoid that the groove surface of the inverted pyramid velvet surface cannot be evenly covered when the full surface film layer is passivated.
[0021] Before the step B treatment, the semiconductor substrate is pickled.
[0022] The second masking structure is a mesh mask plate whose mesh size is adapted to the individual size of the inverted pyramid velvet surface and whose mesh distribution is uniform.
[0023] The first passivation film deposition and the second passivation film deposition are amorphous silicon film or silicon dioxide film deposition.
[0024] The specific method of step A is to place a first masking structure with mesh holes on the surface of the semiconductor substrate, perform etching, and then remove the first masking structure to perform texturing.
[0025] The specific process of step A is:
[0026] a1, placing a first masking structure on the surface of the semiconductor substrate;
[0027] a2, under the protection of the first masking structure, performing laser etching or plasma etching on the surface of the semiconductor substrate to form holes evenly distributed on the surface of the semiconductor substrate;
[0028] a3, removing the first masking structure, and performing a texturing process on the semiconductor substrate to form an inverted pyramid texturing surface.
[0029] In the step a2, if laser etching is used, there is no special requirement for the wavelength and frequency of the laser, as long as uniform holes can be formed on the surface of the semiconductor substrate; if plasma etching is used, the etching gas can be one or a combination of fluorine-containing gases such as CF4 and NF3.
[0030] The first masking structure is a mesh mask plate that is resistant to laser or plasma etching and has uniform mesh distribution. The mesh mask plate is preferably made of aluminum alloy or graphite carbon fiber.
[0031] The mesh cross-section of the first masking structure is square, and the side length is 1um-1mm; the mesh cross-section of the first masking structure is circular, and the diameter is 1um-1mm.
[0032] The specific method of step a3 is to remove the first masking structure, clean the surface of the semiconductor substrate to remove the residual substances after etching, and then perform a texturing process to form an inverted pyramid texture surface.
[0033] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0034] The present invention is described in detail below with reference to the accompanying drawings and embodiments:
[0035] like Figures 1 to 3 It is a schematic diagram of an embodiment of a method for manufacturing a solar cell using an inverted pyramid velvet surface provided by the present invention.
[0036] A method for manufacturing a solar cell using an inverted pyramid velvet surface comprises the following steps:
[0037] S1. Place a mask plate made of aluminum alloy on the surface of the silicon wafer. The mask plate is a uniformly distributed square mesh structure with a side length of 2um. The size of the mask plate is comparable to that of the silicon wafer, and the thickness of the mask plate is 0.5mm.
[0038] S2. Under the protection of the mask plate, the surface of the silicon wafer is laser etched to form uniform holes on the surface of the silicon wafer. The wavelength of the laser is between 400-700nm, preferably green light with a wavelength of 500-560nm. The holes formed on the silicon wafer are about 1.5um;
[0039] S3. Remove the mask plate, clean the surface of the silicon wafer with a solution to remove the residual substances from the laser etching, and then treat the silicon wafer again with an alkaline solution, so that an inverted pyramid velvet surface is finally formed on the surface of the silicon wafer. The cleaning solution uses an acid solution such as HF, the mass percentage of HF acid is 1%-8%, the mass percentage of deionized water is 92%-99%, the treatment time of the silicon wafer in the HF acid solution is 1-6 minutes, and the treatment temperature is 20℃-30℃; the alkaline solution is a mixture of potassium hydroxide, a velvet-making additive and water, wherein the mass percentage of potassium hydroxide is 1%-5%, and the mass percentage of the velvet-making additive is 0.5%~1%. The velvet-making time is 8~12 minutes, and the velvet-making temperature is 75℃-85℃;
[0040] S4, cleaning the silicon substrate sheet with the inverted pyramid velvet surface formed, wherein the cleaning solution is an acid solution such as HF for the cleaning solution, the mass percentage of HF acid is 1%-8%, the mass percentage of deionized water is 92%-99%, the treatment time of the silicon sheet in the HF acid solution is 2-3 minutes, and the treatment temperature is 20°C-30°C;
[0041] S5. Place a mask plate on the surface of the cleaned silicon wafer, wherein the mask plate is a uniformly distributed square mesh structure, the side length of the mesh is 2um, the outer dimensions of the mask plate are comparable to the dimensions of the silicon wafer, and the thickness of the mask plate is 0.5mm; under the protection of the mask plate, deposit a passivation film on the surface of the silicon wafer, wherein the passivation film is an amorphous silicon film layer, and the amorphous silicon layer is deposited by PECVD, silane and hydrogen are introduced, the deposition power density is 0.005-0.03w / cm2, the deposition thickness is 3-10nm, and the deposition time is 50-250s; the purpose of depositing the passivation film under the protection of the mask plate is mainly to allow a layer of film to be uniformly deposited on the surface of the inverted pyramid groove first;
[0042] S6, removing the mask plate, and performing surface passivation film deposition on the silicon wafer again, wherein the passivation film deposition is the same as step S5.
[0043] In this embodiment, the two-time coating can avoid the uneven phenomenon that the film layer covers the upper surface of the silicon wafer thicker and the inverted pyramid grooves less when deposited once.
[0044] The above descriptions are only preferred embodiments of the present invention and are not intended to limit the patent scope of the present invention.
[0045] Obviously, those skilled in the art can make various changes and modifications to the invention without departing from the spirit and scope of the invention. Thus, if these modifications and variations of the invention fall within the scope of the claims of the invention and their equivalents, the invention is also intended to include these modifications and variations.
Claims
1. A method for manufacturing a solar cell using an inverted pyramid velvet surface, characterized in that: It includes the following steps, Step A, performing inverted pyramid texturing on the semiconductor substrate; the specific method of step A is to place a first masking structure with mesh holes on the surface of the semiconductor substrate and then perform etching to form holes on the surface of the semiconductor substrate, and then remove the first masking structure to perform texturing; Step B, performing surface passivation on the semiconductor substrate processed in step A; The specific method of step B is to place a second masking structure with mesh holes on the surface of the semiconductor substrate, perform a first passivation film deposition to deposit on the groove surface of the inverted pyramid velvet surface, and then remove the second masking structure to perform a second passivation film deposition; The second masking structure is a mesh mask plate with mesh sizes adapted to the individual sizes of the inverted pyramid velvet surface and meshes evenly distributed; The specific process of step A is: a1, placing a first masking structure on the surface of the semiconductor substrate; a2, under the protection of the first masking structure, performing laser etching or plasma etching on the surface of the semiconductor substrate to form holes evenly distributed on the surface of the semiconductor substrate; a3, removing the first masking structure, and performing a texturing process on the semiconductor substrate to form an inverted pyramid texturing surface; The specific method of step a3 is to remove the first masking structure, clean the surface of the semiconductor substrate to remove the residual substances after etching, and then perform alkaline liquid texturing treatment to form an inverted pyramid texturing surface.
2. The method for manufacturing a solar cell using an inverted pyramid velvet surface according to claim 1, characterized in that: Before the step B, the semiconductor substrate is pickled for 2-3 minutes at a temperature of 20°C-30°C.
3. The method for manufacturing a solar cell using an inverted pyramid velvet surface according to claim 1, characterized in that: The first passivation film deposition and the second passivation film deposition are both amorphous silicon film or silicon dioxide film deposition, and the deposition thicknesses of the first passivation film deposition and the second passivation film deposition are 3-10 nm respectively.
4. The method for manufacturing a solar cell using an inverted pyramid velvet surface according to claim 1, characterized in that: The first masking structure is a mesh mask plate which is resistant to laser or plasma etching and has uniform mesh distribution.
5. The method for manufacturing a solar cell using an inverted pyramid velvet surface according to claim 4, characterized in that: The mesh cross-section of the first masking structure is square, with a side length of 1um-1mm; or the mesh cross-section of the first masking structure is circular, with a diameter of 1um-1mm.
6. The method for manufacturing a solar cell using an inverted pyramid velvet surface according to claim 1, characterized in that: The semiconductor substrate is a silicon wafer used to manufacture heterojunction solar cells.
7. The method for manufacturing a solar cell using an inverted pyramid velvet surface according to any one of claims 1 to 6, characterized in that: In the step a2, the laser wavelength of the laser etching process is between 400-700 nm, and the etching gas of the plasma etching process is one or a combination of fluorine-containing gases.
8. The method for manufacturing a solar cell using an inverted pyramid velvet surface according to claim 7, characterized in that: The specific process of step a3 is to remove the first masking structure, clean the surface of the semiconductor substrate with acid solution for 1-6 minutes at a temperature of 20°C-30°C, remove the residual substances after etching, and then perform alkaline liquid texturing treatment for 8-12 minutes at a temperature of 75°C-85°C to form an inverted pyramid velvet surface.
Citation Information
Patent Citations
Inverted pyramid structure of polysilicon surface and fabrication method of inverted pyramid structure
CN105047734A
Photovoltaic cell and photovoltaic module
CN112466968A
Method for Producing an Optoelectronic Component
US20180254383A1