A method for preparing copper alloy shock absorber based on laser additive manufacturing technology
Copper alloy shock absorbers are prepared through laser additive manufacturing technology, combined with CuSn10 alloy and specific printing processes, to solve the shock absorption and heat dissipation problems of spacecraft electronic equipment, achieve efficient multi-directional shock absorption and thermal conductivity, and meet the requirements of lightweight and adaptability to high-heat environments.
Patent Information
- Application Number
- CN202111631941.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-12-28
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2041-12-28
AI Technical Summary
When existing technology meets the shock absorption and heat dissipation requirements of spacecraft electronic equipment, there are problems such as increased weight, increased volume, and poor thermal conductivity, making it difficult to achieve lightweight, miniaturization, and adaptability to high-heat environments.
Copper alloy shock absorbers are prepared based on laser additive manufacturing technology. Multi-directional shock absorption is achieved through left-right symmetrical structures and folded structures. CuSn10 alloy is used to enhance thermal conductivity. Combining printing process parameters and heat treatment, the shock absorbers and radiators are realized. Functional integration.
It achieves a high power-to-weight ratio and high thermal environment adaptability, improves thermal conductivity, reduces the frequency of printing cracks, simplifies the production process, reduces R&D costs, and meets the production needs of complex structures and low-demand products.
Smart Images

Figure CN114309650B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of additive manufacturing, and in particular to a method for preparing a copper alloy shock absorber based on laser additive manufacturing technology. Background Art
[0002] With the rapid development of my country's aerospace industry in recent years, spacecraft have raised the requirements for electronic equipment shock absorbers to be lightweight, miniaturized, and resistant to harsh thermal environments. Electronic equipment is both heat-sensitive and vibration-sensitive, so it is necessary to adopt efficient, low-volume and low-weight cost vibration and thermal design measures. Engineering applications generally use a combination of shock absorbers and radiators, and the installation form is generally that the radiator (usually a shell) is installed on the base or the bulkhead through the shock absorber, which has the following problems:
[0003] (1) In order to meet the heat dissipation requirements, the weight of the shell needs to be increased to increase the heat capacity or heat dissipation area, which is not conducive to lightweight design;
[0004] (2) The weight of the radiator is applied to the shock absorber, causing the size and weight of the shock absorber to increase;
[0005] (3) Traditional rubber shock absorbers have poor thermal conductivity, and it is difficult for the heat of electronic equipment to be transferred to the casing through the rubber shock absorber. Summary of the invention
[0006] The purpose of the present invention is to provide a method for preparing a copper alloy shock absorber based on laser additive manufacturing technology, and to realize the functional integration of the shock absorber and the radiator through integrated additive manufacturing, so that the shock absorbing device has a higher power-to-weight ratio and higher thermal environment adaptability, meeting the high requirements of the new generation of aerospace products.
[0007] The technical solution to achieve the purpose of the present invention is:
[0008] A method for preparing a copper alloy shock absorber based on laser additive manufacturing technology comprises the following steps:
[0009] Modeling steps: Establish a shock absorber model. The shock absorber adopts a bilaterally symmetrical structure. There are four layers of plates in the vertical direction. The layers are arranged in a Z shape. There are connection holes between the layers. There are multiple folding teeth at equal intervals on the second layer at the upper end. There are multiple mounting holes on the shock absorber, and the axial direction of the mounting holes is parallel to the direction in which the number of layers of the layers is set.
[0010] Printing steps: The printing material is CuSn10 alloy, and the selective laser melting equipment is used. The protective gas is passed before printing, the substrate is preheated, the scanning speed is set to 500-800mm / s, the printing power is 300W-400W, the powder diameter is 15-53μm, and the printing layer thickness is 30-50μm.
[0011] Compared with the prior art, the present invention has the following significant advantages:
[0012] (1) The present invention provides a method for preparing a copper alloy shock absorber based on laser additive manufacturing technology. The shock absorber achieves shock absorption in different directions through a folding structure in the horizontal and vertical directions, so that the shock absorption efficiency in the horizontal and vertical directions within the 20-2000Hz frequency band is not less than 50%. By using CuSn10 alloy to enhance the thermal conductivity, the thermal conductivity of the device is not less than 100W (m*K), realizing the functional integration of the shock absorber and the heat sink.
[0013] (2) The present invention has developed new printing process parameters for CuSn10 alloy, and the density of the sample after heat treatment is higher than 99%. The tensile strength at room temperature is not less than 550Mpa, the yield strength is not less than 400Mpa, the elongation after fracture is not less than 20%, and the cross-sectional shrinkage is not less than 20%. The frequency of printing cracks is effectively reduced, and the one-time forming of copper alloy parts with complex structures is achieved, which reduces the subsequent processing allowance, shortens the development cycle, and reduces the R&D cost, meeting the production needs of products with complex structures and low demand. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 A perspective view of the shock absorber model.
[0015] Figure 2 This is a side view of the shock absorber model.
[0016] Figure 3 Schematic diagram of the directions to print for the shock absorber. DETAILED DESCRIPTION
[0017] The present invention is further described below in conjunction with the accompanying drawings and specific embodiments. Example 1
[0018] A method for preparing a copper alloy shock absorber based on laser additive manufacturing technology in this embodiment includes the following steps:
[0019] Modeling steps: Establish the shock absorber model in the computer as follows Figure 1 As shown, the shock absorber is 8mm high and adopts a bilaterally symmetrical structure. There are four layers of plates in the vertical direction. The layers are arranged in a Z shape, and there are connection holes 2 between the layers. Counting from the top to the bottom, the second layer is the thickest, and there are multiple folding teeth 3 at equal intervals on it. The entire shock absorber is provided with four mounting holes 4; the axial direction of the mounting holes is parallel to the direction in which the layers are set. The vertical spacing of the layers 1 is 0.5mm, the aperture of the connection hole 2 at the connection of the layers is Φ0.5mm, and the folding teeth 3 in the horizontal direction are 1mm wide and 0.5mm apart. Add block supports 5 to the mounting holes of the additive manufacturing model according to Figure 3The slices are sliced in the direction shown (with the lateral long side connected to the substrate, and the mounting hole 4 is axially parallel to the upper end plane of the substrate 6) to reduce the support and the printing height. The slice thickness is 30μm.
[0020] Printing process steps: The printing material is CuSn10 alloy, and the selective laser melting equipment is used. Before printing, argon protection is required to make the oxygen content in the forming chamber lower than 1000ppm, and the substrate 6 is preheated to 80°C. The scanning speed is set to 500mm / s, the printing power is 300W, the powder diameter is 15-53μm, and the printing layer thickness is 30μm for printing.
[0021] Heat treatment steps: Heat treatment is performed within 12 hours after printing is completed. When the temperature in the forming chamber drops below 70°C, the substrate is removed, the residual powder is removed, and the sample is heated to 220°C under nitrogen protection for 2 hours, and the furnace is cooled to room temperature. After the heat treatment is completed, the sample is taken out, the block support 5 is removed, and the surface is sandblasted.
[0022] After testing, the density of the product obtained after heat treatment is 99.3%, the horizontal and vertical vibration reduction efficiency in the 20-2000Hz frequency band is 55% and 65% respectively, and the thermal conductivity of the device is 108W (m*K). The tensile strength measured at room temperature is 562Mpa, the yield strength is 420Mpa, the elongation after fracture is 23%, and the cross-sectional shrinkage is 24%. Example 2
[0023] In this embodiment, a method for preparing a copper alloy shock absorber based on laser additive manufacturing technology includes the following steps:
[0024] Modeling steps: Establish the shock absorber model in the computer as follows Figure 1 As shown, the height of the shock absorber is 15mm, the vertical spacing of the layers 1 is 1.5mm, the diameter of the connection hole 2 at the layer connection is Φ1.5mm, and the width of the folding teeth 3 in the horizontal direction is 2mm and the spacing is 1.5mm. Add block support 5 to the mounting hole of the additive manufacturing model. Figure 3 The slices were sliced in the direction shown, with a thickness of 50 μm.
[0025] Printing process steps: The printing material is CuSn10 alloy, and the selective laser melting equipment is used. Before printing, argon protection is required to make the oxygen content in the forming chamber lower than 1000ppm, and the substrate 6 is preheated to 80°C. The scanning speed is set to 800mm / s, the printing power is 400W, the powder diameter is 15-53μm, and the printing layer thickness is 50μm for printing.
[0026] Heat treatment steps: Heat treatment is performed within 12 hours after printing is completed. When the temperature in the forming chamber drops below 70°C, the substrate is removed, the residual powder is removed, and the sample is heated to 180°C under nitrogen protection for 1 hour, and the furnace is cooled to room temperature. After the heat treatment is completed, the sample is removed, the block support is removed, and the surface is sandblasted.
[0027] After testing, the density of the product obtained after heat treatment is 99.1%, the horizontal and vertical vibration reduction efficiency in the 20-2000Hz frequency band is 60% and 69% respectively, and the thermal conductivity of the device is 101W (m*K). The tensile strength measured at room temperature is 552Mpa, the yield strength is 402Mpa, the elongation after fracture is 25%, and the cross-sectional shrinkage is 26%.
[0028] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A method for preparing a copper alloy shock absorber based on laser additive manufacturing technology, characterized in that: The following steps are involved: Modeling steps: Establish a shock absorber model. The shock absorber adopts a bilaterally symmetrical structure. There are four layers of plates in the vertical direction. The layers are arranged in a Z shape. There are connection holes between the layers. There are multiple folding teeth at equal intervals on the second layer at the upper end. There are multiple mounting holes on the shock absorber, and the axial direction of the mounting holes is parallel to the direction in which the number of layers of the layers is set. Printing steps: The printing material is CuSn10 alloy, and the selective laser melting equipment is used. The protective gas is passed before printing, and the substrate is preheated. The scanning speed is 500-800mm / s, the printing power is 300W-400W, the powder diameter is 15-53μm, and the printing layer thickness is 30-50μm.
2. The method for preparing a copper alloy shock absorber based on laser additive manufacturing technology according to claim 1, characterized in that: The process also includes a heat treatment step of heating to 180-220°C under protective gas and keeping the temperature for 1-2 hours, and then cooling the furnace to room temperature.
3. The method for preparing a copper alloy shock absorber based on laser additive manufacturing technology according to claim 2, characterized in that: After heat treatment is complete, the block supports are removed and the surface is sandblasted.
4. The method for preparing a copper alloy shock absorber based on laser additive manufacturing technology according to claim 3, characterized in that: The heat treatment must be performed within 12 hours after printing is completed.
5. The method for preparing a copper alloy shock absorber based on laser additive manufacturing technology according to claim 1, characterized in that: The shock absorber height is 8-15 mm.
6. The method for preparing a copper alloy shock absorber based on laser additive manufacturing technology according to claim 1, characterized in that: The spacing between the layers is 0.5-1.5mm; the hole diameter at the connection of the layers is Φ0.5-1.5mm; the width of the folding teeth is 1-2mm, and the spacing is 0.5-1.5mm.
7. The method for preparing a copper alloy shock absorber based on laser additive manufacturing technology according to claim 1, characterized in that: The preheating temperature of the substrate is 80°C.
Citation Information
Patent Citations
Axial variable stiffness friction damper
CN111664208A
Preparation method of cold deformation and heat treatment reinforced additive manufacturing Cu-Ni-Sn alloy
CN113351879A