Spin torque oscillator with antiferromagnetic coupling auxiliary layer and operation method thereof
By introducing an antiferromagnetic coupling auxiliary layer and a non-magnetic spacer layer into the spin torque oscillator, combined with the electromagnet guiding bias magnetic field, the problem of large peak width of the spin torque oscillator in the existing technology is solved and the Q factor is improved. and performance, suitable for high-frequency communication devices.
Patent Information
- Application Number
- CN202080079839.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-12-31
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2040-12-31
AI Technical Summary
The existing spin torque oscillator has a wide peak width at the oscillation frequency and a low Q factor, making it difficult to meet the performance requirements of high-frequency communication devices.
Adopting a spin torque oscillator structure with an antiferromagnetic coupling auxiliary layer, including a spin polarization layer of a first ferromagnetic material, a ferromagnetic oscillation layer of a second ferromagnetic material, a non-magnetic spacer layer and an antiferromagnetic coupling layer , the auxiliary layer is antiferromagnetically coupled to the ferromagnetic oscillation layer through the nonmagnetic coupling layer, and an electromagnet is configured near the device layer stack to guide the bias magnetic field, and the magnetization state is adjusted to reduce the peak width.
It achieves a narrower peak width at the oscillation frequency, improves Q factor and performance, and is suitable for high-frequency communication devices.
Smart Images

Figure CN114730570B_ABST
Abstract
Description
[0001] Related Applications
[0002] This application claims the benefit of priority to U.S. Non-Provisional Patent Application No. 16 / 887,563, filed on May 29, 2020; and U.S. Non-Provisional Patent Application No. 16 / 887,715, filed on May 29, 2020, the entire contents of which are hereby incorporated by reference into this document for all purposes. Technical Field
[0003] The present disclosure relates generally to the field of microelectronic magnetic devices, and in particular to a spin torque oscillator having an antiferromagnetic coupling auxiliary layer and a method of operating the same. Background Art
[0004] Periodic pulse patterns with frequencies in the gigahertz range are employed in many electronic applications, such as wireless communication systems, radars, wireless network devices, automotive communication devices, and sound synthesizers. Although many spin torque oscillator (STO) devices that generate periodic pulses with frequencies greater than 10 GHz are known in the art, many such STO devices have a wide peak width and a low Q factor at the oscillation frequency. Summary of the invention
[0005] According to an embodiment of the present disclosure, a spin torque oscillator includes a first electrode, a second electrode, and a device layer stack located between the first electrode and the second electrode. The device layer stack includes: a spin polarization layer including a first ferromagnetic material, an auxiliary layer including a third ferromagnetic material, a ferromagnetic oscillation layer including a second ferromagnetic material located between the spin polarization layer and the auxiliary layer, a non-magnetic spacer layer located between the spin polarization layer and the ferromagnetic oscillation layer, and a non-magnetic coupling layer located between the ferromagnetic oscillation layer and the auxiliary layer. The auxiliary layer is antiferromagnetically coupled to the ferromagnetic oscillation layer through the non-magnetic coupling layer, and the auxiliary layer has a magnetization coupled to the magnetization of the ferromagnetic oscillation layer.
[0006] In a first embodiment, the electromagnet is located near the device layer stack and is configured to direct the bias magnetic field through the device layer stack. In a second embodiment, at least one of the first electrode or the second electrode includes a ferromagnetic material having a fixed magnetization, and includes a ferromagnetic electrode layer and a ferromagnetic pillar protruding from the ferromagnetic electrode layer toward the device layer stack, the ferromagnetic pillar having a lateral width substantially the same as the lateral width of the device layer stack, and the lateral width of the ferromagnetic electrode layer is greater than the lateral width of the ferromagnetic pillar, so that an annular horizontal surface of the ferromagnetic electrode layer surrounds the base of the ferromagnetic pillar to provide a notch at the junction of the ferromagnetic electrode layer and the ferromagnetic pillar. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1A and Figure 1Bare vertical cross-sectional views of two alternative configurations of a first exemplary spin torque oscillator according to a first embodiment of the present disclosure.
[0008] Figure 2 is a schematic diagram of a first exemplary periodic signal generator according to the first embodiment of the present disclosure.
[0009] Figure 3 is a schematic diagram of a second exemplary periodic signal generator according to the first embodiment of the present disclosure.
[0010] Figure 4A is a vertical cross-sectional view of a first exemplary spin torque oscillator in the absence of an external magnetic field and in the absence of a spin current according to the first embodiment of the present disclosure.
[0011] Figure 4B is a vertical cross-sectional view of a first exemplary spin torque oscillator in the presence of an external magnetic field and in the absence of a spin current according to the first embodiment of the present disclosure.
[0012] Figure 4C is a vertical cross-sectional view of a first exemplary spin torque oscillator in the presence of an external magnetic field and in the presence of a spin current according to the first embodiment of the present disclosure.
[0013] Figure 5 is a vertical cross-sectional view of a second exemplary spin torque oscillator according to the second embodiment of the present disclosure.
[0014] Figure 6 is a schematic diagram of a third exemplary periodic signal generator according to the second embodiment of the present disclosure.
[0015] Figure 7 is a schematic diagram of a fourth exemplary periodic signal generator according to the second embodiment of the present disclosure.
[0016] Figure 8 is a vertical cross-sectional view of a second exemplary spin torque oscillator in the presence of a spin current according to a second embodiment of the present disclosure.
[0017] Fig. 9 is a vertical cross-sectional view of a parallel connection of two second exemplary spin torque oscillators according to a second embodiment of the present disclosure. DETAILED DESCRIPTION
[0018] As described above, the present disclosure relates to an STO with an antiferromagnetic coupling auxiliary layer and an operating method thereof, various aspects of which are described in detail below. The STO with an antiferromagnetic coupling auxiliary layer has a narrower peak width at the oscillation frequency, which provides improved Q factor and performance in various communication devices or other devices employing the STO.
[0019] The drawings are not drawn to scale. Multiple instances of an element may be repeated where a single instance of an element is shown, unless explicitly described or otherwise clearly indicated that there is no repetition of an element. Serial numbers such as "first," "second," and "third" are used only to identify similar elements, and different serial numbers may be used throughout the specification and claims of this disclosure. The term "at least one" element refers to all possibilities including the possibility of a single element and the possibility of multiple elements.
[0020] The same reference numerals represent the same elements or similar elements. Unless otherwise specified, elements with the same reference numerals are assumed to have the same composition and the same function. Unless otherwise specified, "contact" between elements refers to direct contact between elements providing an edge or surface shared by the elements. If two or more elements are not in direct contact with each other, the two elements are "separated" from each other. As used herein, a first element positioned "on" a second element may be positioned on the outside of the surface of the second element or on the inside of the second element. As used herein, if there is physical contact between the surface of the first element and the surface of the second element, the first element is "directly" positioned on the second element. As used herein, if there is a conductive path consisting of at least one conductive material between the first element and the second element, the first element is "electrically connected to" the second element. As used herein, "magnetization" refers to the magnetization direction of a magnetic material.
[0021] As used herein, "layer" refers to a portion of a material including an area having a thickness. A layer may extend over the entirety of an underlying or overlying structure, or may have an extent that is less than the extent of an underlying or overlying structure. A layer may extend horizontally, vertically, and / or along a tapered surface. A substrate may be a layer, may include one or more layers therein, or may have one or more layers thereon, above, and / or below.
[0022] As used herein, a first surface and a second surface "vertically coincide" with each other if the second surface is above or below the first surface and if there is a vertical plane or a substantially vertical plane that includes the first surface and the second surface. A substantially vertical plane is a plane that extends straight along a direction that deviates from the vertical direction at an angle of less than 5 degrees. A vertical plane or a substantially vertical plane is straight along the vertical direction or a substantially vertical direction and may or may not include curvature along a direction perpendicular to the vertical direction or the substantially vertical direction.
[0023] Figure 1A and Figure 1B Two different configurations of a first exemplary spin torque oscillator 100 according to a first embodiment of the present disclosure are shown. The STO 100 comprises a first electrode 110. Figure 1AIn a configuration where the magnetic pole 250 of the electromagnet to be described below is not electrically connected to the first electrode 110, the first electrode 110 may include any suitable conductive material. In one embodiment, the first electrode includes a non-magnetic conductive material such as a metal (e.g., Al, W, Ti, Cu, etc.), a metal alloy, or a metal nitride (e.g., TiN, WN, TaN, etc.).
[0024] exist Figure 1B In a configuration in which the material of the magnetic pole 250 is also used to form the first electrode 110, and the magnetic pole 250 contacts the first electrode 110, the first electrode may include any suitable first soft magnetic material. As used herein, a soft magnetic material refers to a ferromagnetic material having an intrinsic coercive force of less than 1000 A / m. Soft magnetic materials are easily magnetized and easily demagnetized, and can be used to enhance and / or guide the magnetic flux generated by an electric current. Exemplary soft magnetic materials that can be used for the first electrode 110 include nickel-iron alloys, soft ferrites, and nickel-iron-chromium alloys. In one embodiment, the first soft magnetic material of the first electrode 110 may have an intrinsic coercive force in the range of 1 A / m to 100 A / m.
[0025] The first electrode 110 may be formed on a substrate (not shown) having a thickness sufficient to provide mechanical support for the first electrode 110. For example, the substrate may be an insulating substrate (such as a quartz substrate or a ceramic substrate, such as a sapphire substrate), or a semiconductor substrate or a conductive substrate having an insulating layer (such as a silicon oxide or aluminum oxide layer) thereon, on which the first electrode 110 may be formed.
[0026] The STO device layer stack 111 is located on the top surface of the first electrode 110. The STO device layer stack 111 includes, from bottom to top or from top to bottom, an optional non-magnetic seed layer 112, a spin polarization layer 120 including a first ferromagnetic material, a non-magnetic spacer layer 130, a ferromagnetic oscillation layer 140 including a second ferromagnetic material that may be the same as or different from the first ferromagnetic material, a coupling layer 150, and an anti-ferromagnetic coupling auxiliary layer 160 including a third ferromagnetic material that may be the same as or different from the first ferromagnetic material and the second ferromagnetic material and has a magnetization coupled to the magnetization of the ferromagnetic oscillation layer 140. Although the present disclosure is described using an embodiment in which the layers of the device layer stack are arranged from bottom to top, embodiments in which the device layer stack is arranged from top to bottom are explicitly contemplated herein.
[0027] The various layers of the device layer stack 111 may have vertically overlapping sidewalls, i.e., sidewalls that are located in the same vertical plane. The horizontal cross-sectional shape of each layer in the device layer stack 111 may be the same, or may be substantially the same if their sidewalls have a non-zero taper angle. The horizontal cross-sectional shape of the device layer stack 111 may be circular, elliptical, rectangular, a rounded polygon (i.e., a polygon modified to provide rounded corners), or any closed two-dimensional curve shape that is generally non-intersecting. The lateral dimensions of the device layer stack 111 (such as a diameter or a side of a rectangle) may be in the range of 10 nm to 200 nm, such as 20 nm to 100 nm, but smaller and larger lateral dimensions may also be used.
[0028] The optional non-magnetic seed layer 112 can be used to enhance the crystalline properties of the material layer deposited thereon. For example, the non-magnetic seed layer 112 can include chromium, copper, tantalum, ruthenium, hafnium, niobium, tungsten, nickel aluminum alloy, or a combination or alloy thereof. The thickness of the non-magnetic seed layer 112 can be in the range of 1 nm to 2 nm, although smaller and larger thicknesses can also be used.
[0029] The first ferromagnetic material of the spin polarization layer 120 may include: Fe, Co, Ni, a ferromagnetic alloy including at least one of Fe, Co and Ni, or a magnetic Heusler alloy, and / or may be substantially composed thereof. The thickness of the spin polarization layer 120 may be in the range of 1 nm to 3 nm, such as 1.2 nm to 2 nm, but smaller and larger thicknesses may also be used. As will be discussed below, the thickness of the spin polarization layer 120 may be determined based on the magnetic moment-thickness product of the spin polarization layer 120, i.e., based on the product of the magnetic moment (which is the magnitude of magnetization) and the thickness of the spin polarization layer 120.
[0030] The non-magnetic spacer layer 130 includes a non-magnetic metal, semiconductor material, or dielectric metal oxide material having a thickness that allows charge tunneling, and / or is substantially composed of them. For example, the non-magnetic spacer layer 130 may include any one of chromium, copper, tantalum, ruthenium, hafnium, niobium, tungsten, nickel aluminum alloy, zinc selenide, copper indium selenide, magnesium oxide, or aluminum oxide. The thickness of the non-magnetic spacer layer 130 may be in the range of 0.8nm to 3nm. In the case where a tunneling dielectric material is used for the non-magnetic spacer layer 130, the thickness of the non-magnetic spacer layer 130 may be in the range of 0.8nm to 1.2nm. The thickness of the non-magnetic spacer layer 130 may be selected so that the combination of the spin polarization layer 120, the non-magnetic spacer layer 130, and the ferromagnetic oscillation layer 140 is used as a spin valve or a magnetic tunnel junction.
[0031] The second ferromagnetic material of the ferromagnetic oscillation layer 140 may include: Fe, Co, Ni, a ferromagnetic alloy including at least one of Fe, Co and Ni, or a magnetic Heusler alloy, and / or may be substantially composed thereof. The thickness of the ferromagnetic oscillation layer 140 may be in the range of 2nm to 15nm, such as 4nm to 10nm, but smaller and larger thicknesses may also be used. The thickness of the spin ferromagnetic oscillation layer 140 may be determined based on the magnetic moment-thickness product of the ferromagnetic oscillation layer 140. In one embodiment, the ferromagnetic oscillation layer 140 has a larger magnetic moment-thickness product than the spin polarization layer 120. In one embodiment, the ratio of the magnetic moment-thickness product of the ferromagnetic oscillation layer 140 to the magnetic moment-thickness product of the spin polarization layer 120 may be in the range of 1.2 to 5, such as 2 to 4. Setting the ratio of the magnetic moment-thickness product of the ferromagnetic oscillation layer 140 to the magnetic moment-thickness product of the spin polarization layer 120 in the range of 1.2 to 5 results in antiferromagnetic alignment of the vertical component (i.e., axial component) of the magnetization of the spin polarization layer 120 with the vertical component of the magnetization of the ferromagnetic oscillation layer 140 during operation as a spin valve or as a magnetic tunnel junction. If the materials of the ferromagnetic oscillation layer 140 and the spin polarization layer 120 are the same, the thickness of the ferromagnetic oscillation layer 140 is 1.2 to 5 times that of the spin polarization layer 120. If the materials of the ferromagnetic oscillation layer 140 and the spin polarization layer 120 are different and have different magnetic moments, the thickness of the layer may be adjusted to obtain a magnetic moment-thickness product ratio in the range of 1.2 to 5.
[0032] The non-magnetic coupling layer 150 includes and / or is substantially composed of a metal material that provides anti-ferromagnetic coupling between the ferromagnetic oscillation layer 140 and the anti-ferromagnetic coupling auxiliary layer 160. For example, the anti-ferromagnetic coupling layer 150 may include and / or may be substantially composed of ruthenium, rhodium, and / or iridium. The thickness of the non-magnetic coupling layer 150 may be in the range of 0.4 nm to 2 nm, such as 0.6 nm to 1.5 nm, but smaller and larger thicknesses may also be used.
[0033] The third ferromagnetic material of the antiferromagnetic coupling auxiliary layer 160 may include: Fe, Co, Ni, a ferromagnetic alloy including at least one of Fe, Co and Ni, or a magnetic Heusler alloy, and / or may be substantially composed of them. In the absence of a current flowing through the stack 111, the magnetization of the antiferromagnetic coupling auxiliary layer 160 is completely antiparallel to the magnetization of the ferromagnetic oscillation layer 140. However, as will be described below, under various operating conditions of the first exemplary spin torque oscillator 100, the magnetization of the antiferromagnetic coupling auxiliary layer 160 may be completely or partially antiparallel to the magnetization of the ferromagnetic oscillation layer 140. The thickness of the antiferromagnetic coupling auxiliary layer 160 may be in the range of 2nm to 100nm, such as 2nm to 20nm, but smaller and larger thicknesses may also be used. As will be discussed below, the thickness of the antiferromagnetic coupling auxiliary layer 160 may be determined based on the magnetic moment-thickness product of the ferromagnetic oscillation layer 140. In one embodiment, the antiferromagnetic coupling auxiliary layer 160 has a larger magnetic moment-thickness product than the ferromagnetic oscillation layer 140. In one embodiment, the ratio of the magnetic moment-thickness product of the antiferromagnetic coupling assist layer 160 to the magnetic moment-thickness product of the ferromagnetic oscillation layer 140 may be in the range of 2 to 10. Setting the ratio of the magnetic moment-thickness product of the antiferromagnetic coupling assist layer 160 to the magnetic moment-thickness product of the ferromagnetic oscillation layer 140 in the range of 2 to 10 results in antiferromagnetic alignment of the in-plane component (i.e., horizontal component) of the magnetization of the antiferromagnetic coupling assist layer 160 with the in-plane component of the magnetization of the ferromagnetic oscillation layer 140 during operation of the spin torque oscillator 100. If the antiferromagnetic coupling assist layer 160 and the ferromagnetic oscillation layer 140 are of the same material, the thickness of the antiferromagnetic coupling assist layer 160 is 2 to 10 times that of the ferromagnetic oscillation layer 140. If the antiferromagnetic coupling assist layer 160 and the ferromagnetic oscillation layer 140 are of different materials and have different magnetic moments, the thickness of the layer may be adjusted to obtain a magnetic moment-thickness product ratio in the range of 2 to 10.
[0034] Generally speaking, the device layer stack 111 may be formed on the first electrode 110. The layer stack includes, from bottom to top or from top to bottom: a spin polarization layer 120 including a first ferromagnetic material, a nonmagnetic spacer layer 130, a ferromagnetic oscillation layer 140 including a second ferromagnetic material, a coupling layer 150 contacting the ferromagnetic oscillation layer 140, and an antiferromagnetic coupling auxiliary layer 160 including a third ferromagnetic material and having a magnetization coupled to the ferromagnetic oscillation layer 140. An optional nonmagnetic seed layer 112 may be formed directly on the top surface of the first electrode 110 below the other layers of the device layer stack 111. The device layer stack 111 may be formed as a pillar structure with vertical sidewalls.
[0035] The second (upper) electrode 190 may be formed directly on the top surface of the device layer stack 111. In one embodiment, the second electrode 190 may be formed directly on the top surface of the antiferromagnetic coupling assist layer 160. The second electrode 190 may be formed of the same material as the first electrode 110.
[0036] The dielectric layer 220 surrounds the device layer stack 111. The dielectric layer 220 includes a dielectric material such as silicon oxide, silicon nitride, a dielectric metal oxide (eg, aluminum oxide), or silicon carbide nitride.
[0037] An electromagnet 240 including a conductive coil 230 surrounding a soft magnetic pole 250 is located near at least one side of the device layer stack 111. The conductive coil 230 includes a conductive material such as copper, silver, gold, aluminum, tungsten, or ruthenium. Figure 1A and Figure 1B Schematically illustrated in FIG. 5 is a conductive coil 230 having a single loop, but embodiments of coil 230 having multiple loops, such as a spiral around a magnetic pole, are expressly contemplated herein.
[0038] The soft magnetic pole 250 includes any soft magnetic material, such as a nickel-iron alloy, a soft ferrite, or a nickel-iron-chromium alloy. In one embodiment, the soft magnetic material may have an intrinsic coercive force in the range of 1 A / m to 100 A / m. Figure 1A In the first configuration of the STO 100 shown, the dielectric layer 220 separates the soft magnetic pole 250 from the first electrode and the second electrode (110, 190). Figure 1B In the second configuration of the STO 100 shown, the soft magnetic pole 250 is in contact with the first and second electrodes (110, 190) and is made of the same soft magnetic material as the first and second electrodes. In one embodiment, the electromagnet 240 and the device layer stack 111 can be embedded in the dielectric material layer 220.
[0039] Figure 1A and Figure 1B The structure shown is a first exemplary spin torque oscillator 100. The electromagnet 240 is configured to direct a bias magnetic field through the device layer stack 111 when the electromagnet is turned on by applying a current to the coil 230. The control circuit (not shown) is configured to apply a bias voltage or current between the first electrode 110 and the second electrode 190 to cause a spin current to flow through the device layer stack 111 between the electrodes (110, 190), which will be described in more detail below. The first exemplary spin torque oscillator 100 can be used to provide a periodic signal generator that can generate a periodic sinusoidal output or a periodic pulse pattern.
[0040] refer to Figure 2, shows a first exemplary periodic signal generator according to a first embodiment of the present disclosure. The first periodic signal generator includes Figure 1A and Figure 1B The first exemplary spin torque oscillator 100, control circuit 305 and heterodyne mixer circuit shown are configured to output a periodic signal with a frequency in the range of 2 GHz to 100 GHz and are described in S. Kisilev et al., published in Nature, Vol. 425, p. 380, September 25, 2003, which is incorporated herein by reference in its entirety. The first exemplary periodic signal generator may include a control circuit 305 configured to induce a direct current flowing through the device layer stack 111 by applying a direct current bias voltage between the first electrode 110 and the second electrode 190 to induce a spin current through the device layer stack 111, and / or configured to provide a current through the coil 230 of the electromagnet 240 to generate a magnetic field in the electromagnet 240.
[0041] The heterodyne mixer circuit includes an inductor 310 connected between a DC voltage source and an electrical output terminal of the STO 100. The output signal from the device layer stack 111 can be transmitted to an operational amplifier 330 through a capacitor 320. The output signal from the operational amplifier 330 can be mixed with the output signal from the scanning signal generator 340 in a mixer 350. The output signal from the mixer 350 is fed to a bandpass filter 360. The filter 360 passes signals in the range of 25 MHz to 100 MHz. The output signal from the bandpass filter 360 can then be amplified by another operational amplifier 370 and can pass through a diode detector 380 to generate a microwave frequency output signal. The first periodic signal generator can generate a periodic pulse signal with a narrow pulse width in the range of 2 GHz to 100 GHz (such as 5 GHz to 30 GHz), but lower and higher frequencies can also be used. Other output / mixer circuits can also be used.
[0042] refer to Figure 3 , showing a second exemplary periodic signal generator according to the first embodiment of the present disclosure, which can be connected in parallel configuration Figure 1A and Figure 1B The first exemplary spin torque oscillator 100 may be configured to include multiple instances (such as two or more instances) of the first exemplary spin torque oscillator 100. Figure 2 The first exemplary periodic signal generator is derived. In this case, it is possible to modify Figure 1A and Figure 1B The first exemplary structure is used to form a plurality of device layer stacks 111. The plurality of instances of the spin torque oscillator 100 in the second exemplary periodic signal generator can generate a stable high frequency output signal.
[0043] The device layer stack 111 can be tuned by a magnetic field from an electromagnet 240 or by a spin current generated by applying a bias voltage between the first electrode and the second electrode (110, 190). Figure 4A , shows the alignment of the magnetization of the component layers within the device layer stack 111 in the first exemplary spin torque oscillator 100 in the absence of an external magnetic field (i.e., when no current flows through the coil 230 of the electromagnet) and in the absence of a bias spin current flowing through the device layer stack 111 according to the first embodiment of the present disclosure. Figure 1A The structure of FIG. 4A to FIG. 4C , but it should be understood that it is possible to use Figure 1B structure instead.
[0044] Under this condition, the magnetization of the spin polarization layer 120 and the ferromagnetic oscillation layer 140 may be ferromagnetically coupled, and the magnetization of the ferromagnetic oscillation layer 140 and the magnetization of the antiferromagnetic coupling auxiliary layer 160 may be antiferromagnetically coupled. For example, the magnetization of the ferromagnetic oscillation layer 140 and the magnetization of the spin polarization layer 120 may be in-plane magnetization parallel to the interface between the spin polarization layer 120 and the non-magnetic spacer layer 130, while the electromagnet 140 is turned off and the spin current does not flow through the device layer stack 111. For example, the magnetization of the ferromagnetic oscillation layer 140 and the magnetization of the antiferromagnetic coupling auxiliary layer 160 may be in-plane magnetization antiparallel to each other and parallel to the interface between the ferromagnetic oscillation layer 140 and the coupling layer 150, while the electromagnet 140 is turned off and the spin current does not flow through the device layer stack 111.
[0045] refer to Figure 4B , shows the alignment of the magnetization of the component layers within the device layer stack 111 in the first exemplary spin torque oscillator 100 in the presence of an external magnetic field and in the absence of a bias spin current according to the first embodiment of the present disclosure. In this case, the electromagnet 240 can be turned on without applying a bias voltage between the first electrode and the second electrode (110, 190). In other words, no spin current flows between the first electrode 110 and the second electrode 190. The electromagnet 240 can be turned on by passing a direct current through the conductive coil 230, which generates a magnetic field in the soft magnetic material pole 250. The magnetic field generated by the electromagnet 240 is directed through the soft magnetic material pole 250 and generates a bias magnetic field within the adjacent device layer stack 111 to tune the frequency of the STO 100. The bias magnetic field aligns the various magnetizations of the magnetic layers (120, 140, 160) in the direction of the bias magnetic field, which can be upward or downward. In the illustrated example, the magnetization of the spin polarization layer 120 , the magnetization of the ferromagnetic oscillation layer 140 , and the magnetization of the antiferromagnetic coupling auxiliary layer 160 may be aligned upward in a vertical direction.
[0046] The bias magnetic field is vertical within the device layer stack 111, and the magnitude of the bias magnetic field can be selected to overcome the antiferromagnetic alignment of the axial component (i.e., the vertical component) of the magnetization of the ferromagnetic oscillation layer 140 and the axial component of the magnetization of the antiferromagnetic coupling auxiliary layer 160. In other words, the bias magnetic field overcomes the tendency of the magnetization of the ferromagnetic oscillation layer 140 and the magnetization of the antiferromagnetic coupling auxiliary layer 160 to be antiferromagnetically coupled to each other. Therefore, the axial component of the magnetization of the ferromagnetic oscillation layer 140 and the axial component of the magnetization of the antiferromagnetic coupling auxiliary layer 160 can be parallel to the bias magnetic field while the electromagnet 240 is turned on. In one embodiment, the magnetization of the ferromagnetic oscillation layer 140 and the magnetization of the spin polarization layer 120 can be axial magnetization parallel to the bias magnetic field while the electromagnet 240 is turned on and the spin current does not flow through the device layer stack 111.
[0047] refer to Figure 4C , shows the alignment of the magnetization of the component layers within the device layer stack 111 in the first exemplary spin torque oscillator 100 in accordance with the first embodiment of the present disclosure in the presence of an external magnetic field generated by the electromagnet 140 when current flows through the coil 230 and in the presence of a DC bias spin current. A DC bias voltage may be applied between the first electrode 110 and the second electrode 190 to generate a spin current in the device layer stack 111. The directions of the bias magnetic field and the spin current in the device layer stack 111 may be antiparallel.
[0048] The magnetization of the spin polarization layer 120 oscillates (e.g., precesses) with a lower spin current than the magnetization of the ferromagnetic oscillation layer 140. The magnetization of the ferromagnetic oscillation layer 140 oscillates (e.g., precesses) with a higher spin current, which causes the inclination and precession of the magnetization. The magnetization of the spin polarization layer 120 (which has a lower magnetic moment-thickness product) follows the magnetization of the ferromagnetic oscillation layer 140 in an antiparallel direction, and the azimuth angle of the in-plane component of the magnetization of the ferromagnetic oscillation layer 140 may be the same as the azimuth angle of the in-plane component of the magnetization of the spin polarization layer 120.
[0049] The layer stack of the spin polarization layer 120, the non-magnetic spacer layer 130 and the ferromagnetic oscillation layer 140 acts as a spin valve or a magnetic tunnel junction, depending on whether the non-magnetic spacer layer is conductive or insulating. The spin polarization of the current occurs through the spin valve or through the magnetic tunnel junction. The spin polarized electrons preferentially pass through the non-magnetic spacer layer 130 so that the axial component of the magnetization of the spin polarization layer 120 is antiferromagnetically aligned with the axial component of the magnetization of the ferromagnetic oscillation layer 140.
[0050] When the ratio of the magnetic moment-thickness product of the ferromagnetic oscillation layer 140 to the magnetic moment-thickness product of the spin polarization layer 120 is in the range of 1.2 to 5, such as 1.4 to 3, the axial component of the magnetization of the ferromagnetic oscillation layer 140 can be aligned parallel to the bias magnetic field, and the axial component of the magnetization of the spin polarization layer 120 can be aligned antiparallel to the bias magnetic field to minimize the total energy of the magnetic configuration of the spin valve or the magnetic tunnel junction. However, this configuration is energetically unfavorable to the magnetization of the spin polarization layer 120, and causes the magnetization of the spin polarization layer 120 to tilt away from the vertical direction, thereby generating an in-plane component of the magnetization of the spin polarization layer 120. In the presence of a bias magnetic field, the in-plane component of the magnetization of the spin polarization layer 120 precesses around the vertical direction.
[0051] The in-plane component of the magnetization of the spin polarization layer 120 tilts the magnetization of the ferromagnetic oscillation layer 140 away from the vertical direction. The substantial ferromagnetic coupling between the magnetization of the spin polarization layer 120 and the magnetization of the ferromagnetic oscillation layer 140 causes the tilt of the magnetization of the ferromagnetic oscillation layer 140 to be locked along the direction of the in-plane component of the magnetization of the spin polarization layer 120. In other words, the in-plane component of the magnetization of the ferromagnetic oscillation layer 140 may have the same azimuth angle around the vertical axis as the in-plane component of the magnetization of the spin polarization layer 120. Therefore, the magnetization of the spin polarization layer 120 and the magnetization of the ferromagnetic oscillation layer 140 precess synchronously around the vertical direction at the same precession frequency.
[0052] The axial component of the magnetization of the antiferromagnetic coupling auxiliary layer 160 remains parallel to the direction of the bias magnetic field within the device layer stack 111 while the electromagnet 240 is turned on and a spin current flows through the device layer stack 111. Due to the antiferromagnetic properties of the coupling between the antiferromagnetic coupling auxiliary layer 160 and the ferromagnetic oscillation layer 140, the in-plane component of the magnetization of the ferromagnetic oscillation layer 140 and the in-plane component of the magnetization of the antiferromagnetic coupling auxiliary layer 160 are antiferromagnetically coupled to each other while the electromagnet 240 is turned on and a spin current flows through the device layer stack 111. Therefore, the auxiliary layer 160 increases the tilt angle of the magnetization of the ferromagnetic oscillation layer 140, which reduces the peak width of the signal output by the STO 100.
[0053] The magnetization of the antiferromagnetic coupling auxiliary layer 160 is coupled to the magnetization of the ferromagnetic oscillation layer 140, and precesses around the vertical axis at the same precession frequency as the magnetization of the spin polarization layer 120. The azimuth angle of the in-plane component of the magnetization of the ferromagnetic oscillation layer 140 may be the same as the azimuth angle of the in-plane component of the magnetization of the spin polarization layer 120, and may be offset by 180 degrees relative to the azimuth angle of the in-plane component of the magnetization of the antiferromagnetic coupling auxiliary layer 160.
[0054] According to one aspect of the present disclosure, a ratio of the moment-product thickness of the antiferromagnetic coupling assisting layer 160 to the moment-product thickness of the ferromagnetic oscillation layer 140 is in the range of 2 to 10 to provide stability for the vertical component of the antiferromagnetic coupling assisting layer 160 to ensure that the vertical component of the antiferromagnetic coupling assisting layer 160 remains parallel to the bias magnetic field, while providing sufficient antiferromagnetic coupling between the in-plane component of the magnetization of the antiferromagnetic coupling assisting layer 160 and the in-plane component of the ferromagnetic oscillation layer 140 to increase the tilt angle of the magnetization of the ferromagnetic oscillation layer 140. During the synchronous precession, during the precession of the magnetization of the spin polarization layer 120, the ferromagnetic oscillation layer 140, and the antiferromagnetic coupling assisting layer 160, the in-plane component of the magnetization of the antiferromagnetic coupling assisting layer 160 and the in-plane component of the ferromagnetic oscillation layer 140 remain locked in antiferromagnetic alignment (i.e., azimuthally different by 180 degrees).
[0055] Figure 5 A second exemplary spin torque oscillator 500 according to a second embodiment of the present disclosure is shown. The second exemplary STO 500 includes the same device layer stack 111 as described above with respect to the first exemplary STO 100. Therefore, for the sake of brevity, the device layer stack 111 layers will not be described again. The second exemplary STO 500 does not include the electromagnet 240 of the first embodiment. Instead, the second exemplary STO 500 includes at least one notch that generates a magnetic field, as will be described below.
[0056] The second exemplary STO 500 includes a first electrode 510 and a second electrode 590. The first electrode 510 includes a first ferromagnetic electrode layer 510L and a first ferromagnetic pillar 510P protruding from the first ferromagnetic electrode layer 510L toward the device layer stack 111. The second electrode 590 includes a second ferromagnetic electrode layer 590L and a second ferromagnetic pillar 590P protruding from the second ferromagnetic electrode layer 590L toward the device layer stack 111.
[0057] At least one of the first electrode 510 and / or the second electrode 590 includes a fixed ferromagnetic material with a fixed magnetization direction, such as Fe, Co, Ni, or an alloy thereof. In one embodiment, the fixed magnetization direction is parallel to the interface between the spin polarization layer 120 and the non-magnetic spacer layer 130. In one embodiment, the first electrode 510 and / or the second electrode 590 may include a pinned soft magnetic material or a hard magnetic material. If the electrode includes a pinned soft magnetic material, it may also include a synthetic ferromagnetic structure (SAF) that includes an antiferromagnetic pinned layer and a ferromagnetic layer stack separated from the soft magnetic material by a conductive non-magnetic spacer.
[0058] The first ferromagnetic pillar 510P has a lateral width (e.g., diameter) substantially the same as the lateral width (e.g., diameter) of the device layer stack 111. The lateral dimension (e.g., width) of the first electrode layer 510L is greater than the lateral dimension of the first ferromagnetic pillar 510P, so that the annular horizontal surface 510S of the first ferromagnetic electrode layer 510L surrounds the base of the vertical first ferromagnetic pillar 510P. Therefore, the first electrode 510 includes a notch 510N at the junction of the first ferromagnetic electrode layer 510L and the first ferromagnetic pillar 510P. When current flows between the first electrode 510 and the second electrode 590, the annular horizontal surface 510S generates a stray magnetic field along the side surface of the first ferromagnetic pillar 510P. The vertical component of the stray magnetic field is applied to the layers of the device layer stack 111 and is used as a bias magnetic field in the first embodiment instead of the bias magnetic field generated by the electromagnet 140. Preferably, the depth of the notch 510N is greater than its width to generate a vertical stray magnetic field. The notch may also act as a shield to stabilize the STO 500 frequency against external fields.
[0059] The second ferromagnetic pillar 590P has a lateral width (e.g., diameter) substantially the same as the lateral width (e.g., diameter) of the device layer stack 111. The lateral dimension (e.g., width) of the second ferromagnetic electrode layer 590L is greater than the lateral dimension of the second ferromagnetic pillar 590P, so that the annular horizontal surface 590S of the second electrode layer 590L surrounds the base of the vertical second ferromagnetic pillar 590P. Therefore, the second electrode 590 includes a notch 590N at the junction of the second ferromagnetic electrode layer 590L and the second ferromagnetic pillar 590P. When current flows between the first electrode 510 and the second electrode 590, the annular horizontal surface 590S generates a stray magnetic field along the side surface of the second ferromagnetic pillar 590P. The vertical component of the stray magnetic field is applied to the layers of the device layer stack 111 and is used as a bias magnetic field in the second embodiment instead of the bias magnetic field generated by the electromagnet 140. Preferably, the depth of the notch 590N is greater than its width to generate a vertical stray magnetic field. The notch may also act as a shield to stabilize the STO 500 frequency against external fields.
[0060] In one embodiment, the sidewalls of the layers of the device layer stack 111 vertically coincide with the sidewalls of the first ferromagnetic pillar 510 and / or the second ferromagnetic pillar 590P.
[0061] refer to Figure 6 , showing a third exemplary periodic signal generator according to the second embodiment of the present disclosure. By replacing the first exemplary spin torque oscillator 100, it is possible to Figure 2 The first periodic signal generator derives the second periodic signal generator.
[0062] refer to Figure 7, shows a fourth exemplary periodic signal generator according to the second embodiment of the present disclosure, which can be connected in parallel configuration Figure 5 The second exemplary spin torque oscillator 500 may be configured to include multiple instances (such as two or more instances) of the second exemplary spin torque oscillator 500. Figure 6 A third exemplary periodic signal generator is derived.
[0063] refer to Figure 8 , shows the alignment of the magnetization of the component layers within the device layer stack 111 in the second exemplary spin torque oscillator 500 in the presence of a DC bias spin current according to the second embodiment of the present disclosure. A DC bias voltage may be applied between the first electrode and the second electrode (510, 590) by the control circuit 305. One or more notches (510N, 590N) generate a magnetic field having a vertical direction antiparallel to the direction of the spin current, and the electromagnet 240 may be omitted. The magnetic field acts similarly to the external magnetic field generated by the electromagnet 240 of the first embodiment, and is used to generate a magnetic field similar to the external magnetic field generated by the electromagnet 240 of the first embodiment, as described above with reference to Figure 4C The approach described for the first embodiment precesses the magnetization of the layers of the device layer stack 111 .
[0064] refer to Fig. 9 , shows a parallel connection of two second exemplary spin torque oscillators 500 according to the second embodiment of the present invention. In this case, each first electrode layer 510L of multiple instances of the second exemplary spin torque oscillator 500 includes a corresponding portion of the common first electrode layer 510L, and each second electrode layer 590L of multiple instances of the second exemplary spin torque oscillator 500 includes a corresponding portion of the common second electrode layer 590L.
[0065] The spin torque oscillator of the embodiment of the present disclosure can be used for microwave signal generation in cellular phones, communication devices, sound analyzers or other communication devices. The synchronous precession of the in-plane components of various ferromagnetic layers provides a narrow oscillation frequency width with high intensity (e.g., the voltage or power output detected from the STO within the integral frequency). Therefore, compared with the STO of the prior art, the spin torque oscillator of the embodiment of the present disclosure can provide higher intensity and narrower frequency peaks (e.g., having a smaller half width at half maximum) .
[0066] Although specific preferred embodiments are mentioned above, it will be understood that the present disclosure is not limited thereto. It will be appreciated by those of ordinary skill in the art that various modifications may be made to the disclosed embodiments, and such modifications are intended to fall within the scope of the present disclosure. Embodiments employing specific structures and / or configurations are shown in the present disclosure, and it should be understood that the present disclosure may be practiced with any other compatible structures and / or configurations that are functionally equivalent, provided that such substitutions are not explicitly prohibited or otherwise considered impossible by those of ordinary skill in the art. All publications, patent applications, and patents cited herein are incorporated herein by reference in their entirety.
Claims
1. A spin torque oscillator, comprising: a first electrode; a second electrode; a device layer stack between the first electrode and the second electrode, wherein the device layer stack comprises: a spin polarization layer, the spin polarization layer comprising a first ferromagnetic material; an auxiliary layer, the auxiliary layer comprising a third ferromagnetic material; a ferromagnetic oscillation layer, the ferromagnetic oscillation layer comprising a second ferromagnetic material located between the spin polarization layer and the auxiliary layer; a non-magnetic spacer layer, the non-magnetic spacer layer being located between the spin polarization layer and the ferromagnetic oscillation layer; and a nonmagnetic coupling layer, the nonmagnetic coupling layer being located between the ferromagnetic oscillation layer and the auxiliary layer, wherein the auxiliary layer is antiferromagnetically coupled to the ferromagnetic oscillation layer through the nonmagnetic coupling layer, and the auxiliary layer has a magnetization coupled to the magnetization of the ferromagnetic oscillation layer; an electromagnet located proximate the device layer stack and configured to direct a bias magnetic field through the device layer stack; and a control circuit configured to apply a bias voltage between the first electrode and the second electrode to induce a spin current flowing through the device layer stack between the first electrode and the second electrode, in: The magnetization of the ferromagnetic oscillation layer is ferromagnetically coupled to the magnetization of the spin polarization layer while the spin current does not flow through the device layer stack and the electromagnet is switched off, and The magnetization of the ferromagnetic oscillation layer and the magnetization of the spin polarization layer are in-plane magnetizations parallel to an interface between the spin polarization layer and the nonmagnetic spacer layer while the electromagnet is switched off and the spin current does not flow through the device layer stack. 2 . The spin torque oscillator according to claim 1 , wherein the ferromagnetic oscillation layer has a larger magnetic moment-thickness product than the spin polarization layer. 3 . The spin torque oscillator according to claim 2 , wherein a ratio of a magnetic moment-thickness product of the ferromagnetic oscillation layer to a magnetic moment-thickness product of the spin polarization layer is in a range of 1.2 to 5. 4 . 4 . The spin torque oscillator according to claim 2 , wherein the auxiliary layer has a larger magnetic moment-thickness product than that of the ferromagnetic oscillation layer. 5 . The spin torque oscillator according to claim 4 , wherein a ratio of a magnetic moment-thickness product of the auxiliary layer to a magnetic moment-thickness product of the ferromagnetic oscillation layer is in a range of 2 to 10. 6 .
6. The spin torque oscillator of claim 1, wherein the magnetization of the ferromagnetic oscillation layer and the magnetization of the spin polarization layer are axial magnetizations parallel to the bias magnetic field while the electromagnet is turned on and the spin current does not flow through the device layer stack.
7. The spin torque oscillator of claim 6 , wherein the magnetization of the spin polarization layer follows the magnetization of the ferromagnetic oscillation layer in an antiparallel direction, and an azimuth angle of an in-plane component of the magnetization of the ferromagnetic oscillation layer is the same as an azimuth angle of the in-plane component of the magnetization of the spin polarization layer, while the electromagnet is turned on and the spin current flows through the device layer stack.
8. The spin torque oscillator of claim 7 , wherein the magnetization of the ferromagnetic oscillation layer and the magnetization of the auxiliary layer are in-plane magnetizations, which are antiparallel to each other and parallel to an interface between the ferromagnetic oscillation layer and the nonmagnetic spacer layer, while the electromagnet is turned off and the spin current does not flow through the device layer stack.
9. The spin torque oscillator of claim 8, wherein the axial component of the magnetization of the ferromagnetic oscillation layer and the axial component of the magnetization of the auxiliary layer are parallel to the bias magnetic field while the electromagnet is turned on and the spin current does not flow through the device layer stack.
10. The spin torque oscillator of claim 9, wherein: the magnetization of the auxiliary layer is coupled to the magnetization of the ferromagnetic oscillation layer and precesses about a vertical axis at the same precession frequency as the magnetization of the spin polarization layer while the electromagnet is turned on and the spin current flows through the device layer stack; and The azimuth angle of the in-plane component of the magnetization of the ferromagnetic oscillation layer is shifted by 180 degrees relative to the azimuth angle of the in-plane component of the magnetization of the auxiliary layer while the electromagnet is turned on and the spin current flows through the device layer stack.
11. The spin torque oscillator of claim 1 , wherein: The first ferromagnetic material of the spin polarization layer includes: Fe, Co, Ni, a ferromagnetic alloy including at least one of Fe, Co or Ni, or a magnetic Heusler alloy; The non-magnetic spacer layer comprises non-magnetic metal, semiconductor material, magnesium oxide or aluminum oxide; The second ferromagnetic material of the ferromagnetic oscillation layer includes: Fe, Co, Ni, a ferromagnetic alloy including at least one of Fe, Co or Ni, or a magnetic Heusler alloy; The nonmagnetic coupling layer comprises ruthenium, rhodium or iridium; and The third ferromagnetic material of the auxiliary layer includes: Fe, Co, Ni, a ferromagnetic alloy including at least one of Fe, Co or Ni, or a magnetic Heusler alloy.
12. The spin torque oscillator of claim 11, wherein: The thickness of the spin polarization layer is in the range of 1 nm to 3 nm; The thickness of the non-magnetic spacer layer is in the range of 0.8 nm to 3 nm; The thickness of the ferromagnetic oscillation layer is in the range of 2 nm to 15 nm; The thickness of the nonmagnetic coupling layer is in the range of 0.4 nm to 2 nm; and The thickness of the auxiliary layer is in the range of 2 nm to 100 nm.
13. A periodic signal generator, comprising: At least one spin torque oscillator according to claim 1; and A signal amplifier circuit is configured to output a microwave signal having a frequency in the range of 2 GHz to 100 GHz.
14. The periodic signal generator of claim 13, further comprising a plurality of said spin torque oscillators configured in parallel.
15. A method of operating a spin torque oscillator, the spin torque oscillator comprising: a first electrode; a second electrode; a device layer stack between the first electrode and the second electrode, wherein the device layer stack comprises: a spin polarization layer, the spin polarization layer comprising a first ferromagnetic material; an auxiliary layer, the auxiliary layer comprising a third ferromagnetic material; a ferromagnetic oscillation layer, the ferromagnetic oscillation layer comprising a second ferromagnetic material located between the spin polarization layer and the auxiliary layer; a non-magnetic spacer layer, the non-magnetic spacer layer being located between the spin polarization layer and the ferromagnetic oscillation layer; and a nonmagnetic coupling layer located between the ferromagnetic oscillation layer and the auxiliary layer, wherein the auxiliary layer is antiferromagnetically coupled to the ferromagnetic oscillation layer through the nonmagnetic coupling layer, and the auxiliary layer has a magnetization coupled to the magnetization of the ferromagnetic oscillation layer; and an electromagnet located proximate the device layer stack and configured to direct a bias magnetic field through the device layer stack; The method comprises: The electromagnet is turned on to generate a bias magnetic field without causing a spin current to flow through the device layer stack so that the magnetization of the ferromagnetic oscillation layer, the magnetization of the spin polarization layer, and the magnetization of the auxiliary layer are axial magnetizations parallel to the direction of the bias magnetic field.
16. The method of claim 15, further comprising causing the spin current to flow through the device layer stack when the electromagnet is turned on, such that: The magnetization of the spin polarization layer follows the magnetization of the ferromagnetic oscillation layer in an antiparallel direction, and the azimuth angle of the in-plane component of the magnetization of the ferromagnetic oscillation layer is the same as the azimuth angle of the in-plane component of the magnetization of the spin polarization layer; The magnetization of the auxiliary layer is coupled to the magnetization of the ferromagnetic oscillation layer and precesses around a vertical axis at the same precession frequency as the magnetization of the spin polarization layer; and The azimuth angle of the in-plane component of the magnetization of the ferromagnetic oscillation layer is shifted by 180 degrees relative to the azimuth angle of the in-plane component of the magnetization of the auxiliary layer.
17. The method of claim 16, further comprising disconnecting the electromagnet and the spinning current such that: The magnetization of the ferromagnetic oscillation layer is ferromagnetically coupled to the magnetization of the spin polarization layer, and the magnetization of the ferromagnetic oscillation layer and the magnetization of the spin polarization layer are in-plane magnetizations parallel to an interface between the spin polarization layer and the nonmagnetic spacer layer; and The magnetization of the ferromagnetic oscillation layer and the magnetization of the auxiliary layer are in-plane magnetizations that are antiparallel to each other and parallel to an interface between the ferromagnetic oscillation layer and the nonmagnetic spacer layer.
18. The method of claim 16, further comprising providing a microwave signal from the spin torque oscillator to a communication device.
Citation Information
Patent Citations
Spin torque oscillator with an antiferromagnetically coupled assist layer and methods of operating the same
US11239016B2
Spin torque oscillator with an antiferromagnetically coupled assist layer and methods of operating the same
US20210376793A1
Magnetic head, magnetic sensor, and magnetic recording / reproducing apparatus
US20130107395A1