A free-form laser additive method for a single layer of heterogeneous materials in arbitrary regions

By combining fused deposition and selective laser melting technology, free-form laser additive manufacturing of dissimilar materials in any area of ​​a single layer is realized, which solves the contradiction between precision and forming accuracy in the existing technology, improves the bonding strength of materials and adapts to complex surface shapes. ability.

CN115255384BActive Publication Date: 2024-10-18ZHEJIANG UNIV OF TECH
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202210836131.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-07-15
Publication Date
2024-10-18
Estimated Expiration
2042-07-15

AI Technical Summary

Technical Problem

There is a contradiction between accuracy and forming accuracy in existing metal additive manufacturing methods. Selective laser melting technology has high accuracy but cannot realize the laying of a single layer of arbitrary dissimilar materials, while laser direct energy deposition technology has low forming accuracy.

Method used

Combining fused deposition technology and selective laser melting technology, materials are first pre-prepared through fused deposition, and then remelted using selective laser melting to achieve layer-by-layer 3D forming, using metal polymer composites and easy-to-degrease polymer binders for metallurgy combine.

Benefits of technology

It achieves high-precision and dense metallurgical bonding, improves the bonding strength of materials and the ability to adapt to complex surface shapes, and expands the applicable scenarios and complexity of additive manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115255384B_ABST
    Figure CN115255384B_ABST
Patent Text Reader

Abstract

The present invention discloses a free-form laser additive method for heterogeneous materials in any area of ​​a single layer. The method pre-deposits materials by means of molten deposition, and then re-melts the material layer by means of selective laser melting to achieve superposition molding. The method has the precision of powder spreading and the flexible material selectivity of powder spraying, and can achieve molding of different materials in any area and free shape in a single-layer scanning direction, and can also achieve gradient molding in the superposition direction. At the same time, since the deposited material has better support, the complexity of printing is higher than that of powder spraying additive, and the support can be easily removed by degreasing without damage caused by mechanical removal. Compared with molten deposition, the method has a denser organizational structure, and since the molten material has a certain adhesion, additive can be performed on more complex surfaces such as curved surfaces, with higher precision, thus expanding the applicable scenarios.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a free-shape laser material adding method for a single-layer arbitrary-region heterogeneous material. Background Art

[0002] With the continuous development of additive manufacturing technology, its application fields are increasing, and its quality and prospects are getting better and better. At present, the commercial metal additive manufacturing methods mainly include selective laser melting technology with pre-set powder bed and laser direct energy deposition technology with synchronous powder feeding. Selective laser melting has a small spot and high precision, but it cannot perform single-layer arbitrarily selected heterogeneous material laying additive; although laser direct energy deposition can freely change the type of material, its forming accuracy is lower than selective laser melting.

[0003] Fused deposition technology is a common additive manufacturing method for plastic materials, and is currently also used in laser additive manufacturing. Metal polymer composite particles or wires are used to melt and deposit the green embryo of the part, which is composed of metal powder bonded by organic matter. The green embryo is degreased and sintered to remove the organic matter and combine the metal powders to form a shape. This forming method is low in cost, but the density is low, which affects the mechanical properties of the formed part.

[0004] Based on these problems in current additive manufacturing, the present invention has designed a free-form laser additive method for heterogeneous materials in a single layer in any area - laser-assisted cladding deposition technology. The present invention uses molten deposition to pre-set each layer of material, and then combines the selective laser melting method to re-melt each layer of material to achieve high-precision additive manufacturing. Compared with the sintering method with molten deposition as pre-treatment, the present invention uses a more dense metallurgical bonding method with higher bonding strength. Summary of the invention

[0005] The present invention proposes a free-form laser additive method for heterogeneous materials in arbitrary regions of a single layer, which combines the advantages of the precision of selective laser melting and the flexibility of material combination of direct energy deposition, and can achieve a relatively dense metallurgical bond.

[0006] The technical solution of the present invention is as follows:

[0007] A free-form laser additive method for heterogeneous materials in a single layer in any area, the method combines two 3D forming technologies, namely fused deposition modeling (FDM) and selective laser melting (SLM); the material is first pre-deposited by fused deposition, and then re-melted by selective laser melting to achieve layer-by-layer 3D forming.

[0008] In the present invention, the material used for additive manufacturing is a solid metal polymer composite material with a certain strength, which becomes a viscous melt after high-temperature melting, and has a certain supporting strength after deposition and cooling. The material is composed of metal and polymer binder (organic matter), and the polymer binder should have the property of easy degreasing, and will not have a significant impact on the material composition of the part itself after laser sintering. Specifically, the present invention is based on the molten deposition technology of wire feeding, and the material is pre-set by wire feeding. The metal polymer composite material is a metal powder added to an organic wire, and a metal powder bonded by an organic matter is formed after molten deposition, such as stainless steel metal polymer composite wire, copper metal polymer composite wire, etc.

[0009] Different from the powder laying and powder spraying methods, the present invention uses FDM to lay the material bed. Due to the use of FDM's pre-set material method, a single layer of heterogeneous materials can be laid in a free shape in any area, and then SLM is used for selective melting, so that simultaneous additive manufacturing of different materials and gradient materials can be achieved.

[0010] The material placement method of molten deposition can achieve free-shape paving of any area of ​​heterogeneous materials on the same layer by replacing nozzles carrying different materials, so as to achieve three-dimensional forming of different materials in the single-layer scanning direction, and thus superimpose the gradient three-dimensional forming of different materials in the stacking direction.

[0011] The melted material has a certain flexibility and can be attached to more complex surfaces such as curved surfaces. Compared with powder-laying additive manufacturing, it can adapt to more working conditions, and compared with powder-spraying additive manufacturing, it has better additive precision.

[0012] Since the material is pre-set by FDM, the fluidity of the metal powder is reduced, and it has a good support effect, and can be used directly as a support. At the same time, since the adhesive of the material is easy to degrease, the support of the formed parts is better to remove. Compared with the mechanical removal method used for metallurgical bonding support, it is more gentle and will not cause damage to the parts.

[0013] Unlike the pre-set powder bed additive method, the support is a metallurgical bond printed together with the part, with a high bonding strength, and needs to be removed by mechanical processing. The support of the parts formed by laser-assisted fused deposition is a solid metal polymer composite material that is fused and deposited, and has a certain interface with the laser remelted part body. The support is easier to remove without damaging the part body. Because of the support, the complexity of the parts that can be made is much higher than that of the synchronous powder feeding additive method without support.

[0014] The laser melting of each layer is performed by selective laser melting, so that a dense metallurgical bond is formed inside the part, which has better mechanical properties than the sintering method with incomplete metallurgical bonding using molten deposition as a pre-treatment. At the same time, the placement method of the viscous melt formed by molten deposition has certain flexibility and adhesion, and the powder bed can be pre-placed in more complex situations such as curved surfaces to achieve repair and additive manufacturing on curved surfaces. Different from curved surface repair and additive manufacturing with coaxial powder feeding, the method of the present invention has higher precision and can form more complex shapes.

[0015] The beneficial effects of the present invention are:

[0016] The present invention relates to a method for free-form laser additive manufacturing of arbitrary selected areas of a single layer of heterogeneous materials. The method uses molten deposition to pre-place materials, and then uses selective laser melting to re-melt the material layer to achieve superimposed molding. The method has the precision of powder spreading and the flexible material selectivity of powder spraying. It can realize the molding of different materials in arbitrary areas and free shapes in the scanning direction of a single layer, and can also realize gradient molding in the superimposed direction. At the same time, because the deposited material has better support, the complexity of printing is higher than that of powder spraying additives. At the same time, the easy degreasing of the material adhesive can make the support relatively simple to remove by degreasing, without the damage of mechanical removal.

[0017] The present invention can realize free-form addition of heterogeneous materials in the scanning direction, and further realize free-area gradient material forming of heterogeneous materials in the deposition direction, providing a new idea for the problem of removing supports in additive manufacturing, and can add materials and repair on substrates with more complex surfaces. Compared with molten deposition, this method has a denser organizational structure, and because the molten material has a certain adhesion, it can be added on more complex surfaces such as curved surfaces with higher precision, expanding the application scenarios. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 Flowchart of additive manufacturing of Example 1. DETAILED DESCRIPTION

[0019] The present invention is further described below by means of specific embodiments, but the protection scope of the present invention is not limited thereto.

[0020] The metal polymer composite wire material in the embodiment is a metal polymer composite material produced by Shenzhen Shenghua 3D Technology Co., Ltd.

[0021] Example 1

[0022] The present invention uses a free-form laser additive method to form parts in any area of ​​a single layer of heterogeneous materials:

[0023] Use a computer to check the model of the formed part, add the required support structure, and classify the support structure into metal support structure area and non-metal support structure area. The non-metal structure area will not be laser remelted after molten deposition. Layer the model and plan the path, generate the mechanical execution command and send it to the forming equipment. The model is attached. Figure 1 .

[0024] Choose a 3D printer with independent dual nozzles, load stainless steel metal polymer composite wire and copper metal polymer composite wire, the printer has better atmosphere protection to avoid oxidation;

[0025] According to the generated program, the first layer is melt deposited, with a nozzle temperature of 200℃, a speed of 60mm / s, a layer thickness of 0.5mm, a platform temperature of 60℃, and a chamber temperature of 40℃. Then the laser is used to remelt the area that needs to be fully metallized. The laser remelting is divided into two times. The first time the power is low, and the working parameters are: power 400w, speed 20mm / s, most of the binder is ablated. The second time the power is high, and the working parameters are: power 1kw, speed 20mm / s, to melt the metal powder and achieve high-density metal deposition;

[0026] Then the second layer of melt deposition and laser remelting are carried out. This process is repeated multiple times to achieve layer-by-layer deposition of metal parts.

[0027] Take out the formed part, remove the support by degreasing or manual removal, and obtain a full metal part with a relatively smooth surface and high strength.

[0028] The parts are then subjected to post-processing such as polishing.

[0029] in:

[0030] The metal polymer composite wire should be easy to degrease, and after melting, it should be a polymer wire with a certain adhesion to the metal, and the polymer will not have a significant impact on the material composition of the part itself after laser sintering.

[0031] The device responsible for laying metal polymer composite wires should be able to pre-place the powder bed in the selected area, and should have multiple melting nozzles carrying different materials to meet the free-form laying of any area of ​​the same layer of heterogeneous materials.

[0032] After forming, the parts need to be supported. Compared with mechanical removal, it is easier to remove the support without damaging the parts.

[0033] Due to the selection of molten deposition as the material placement method, the molten metal polymer composite wire has a certain flexibility and adhesion, and the powder bed can be pre-placed on more complex surfaces such as curved surfaces, thereby realizing additive forming on more complex surfaces such as curved surfaces.

[0034] The contents described in the embodiments of this specification are merely an enumeration of implementation forms of the inventive concept. The protection scope of the present invention should not be regarded as limited to the specific forms described in the embodiments. The protection scope of the present invention also includes equivalent technical means that can be thought of by those skilled in the art based on the inventive concept.

Claims

1. A free-form laser additive method for a single layer of arbitrary region heterogeneous materials, characterized in that: The method combines two 3D forming technologies, namely, melt deposition technology and selective laser melting technology; firstly, materials are pre-placed by melt deposition, and then re-melted by selective laser melting to achieve layer-by-layer 3D forming; The material used for the additive is a metal polymer composite wire, and the metal polymer composite wire is a stainless steel metal polymer composite wire or a copper metal polymer composite wire; The working parameters of fused deposition are: nozzle temperature 200℃, speed 60mm / s, layer thickness 0.5mm, platform temperature 60℃, chamber temperature 40℃; laser remelting is divided into two times, the first working parameters are: power 400w, speed 20mm / s, and the second working parameters are: power 1kw, speed 20mm / s.

2. The free-form laser additive method for a single-layer arbitrary region of heterogeneous materials as claimed in claim 1, characterized in that: The molten deposition method achieves free-form paving of heterogeneous materials in any area of ​​the same layer by replacing nozzles carrying different materials.

Citation Information

Patent Citations

  • Laser-targeting multi-metal fused deposition additive manufacturing process and device

    CN106563804A

  • Multipath wire feed laser fused deposition modeling (LFDM) device and method

    CN106926447A

  • Selective laser melting and filament feeding composite multi-material forming device and forming method

    CN106944622A

  • Gradient brazing filler metal layer preparation based on laser fusion deposition additive manufacturing technology and integrated brazing process

    CN110303154A