A stable aqueous dispersion system of Lithol Ruby 7B and a preparation method thereof

By adding ionic polymers and polyols to water-based makeup, the dispersion of Lisolbaohong 7B toner is improved, and the problem of uneven dispersion in water is solved, and a high stability and high dispersion water-based dispersion system is achieved. , improves the quality and effect of the product.

CN115670973BActive Publication Date: 2024-11-19GUANG DONG 3 INS TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110831811.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-07-22
Publication Date
2024-11-19
Estimated Expiration
2041-07-22

AI Technical Summary

Technical Problem

Among the existing water-based makeup, the poor hydrophilic Lisolbaohong 7B color powder is unevenly dispersed in the water, resulting in unstable product quality, poor hiding and skin-adhesion, making it difficult to achieve long-term stable dispersion effect.

Method used

By adding ionic polymers and polyols, the electrical properties and dielectric properties of the toner particles are improved, and a stable aqueous dispersion system is formed. The adsorption of ionic polymers is used to make the toner particles evenly suspend, and the characteristics of the water medium are improved through polyols. , achieve long-term suspension stability of toner.

Benefits of technology

It significantly improves the dispersion and stability of Lisolbaohong 7B toner in water, forming a highly dispersed and highly stable aqueous dispersion system, which is suitable for water-based cosmetics, and improves the quality and effect of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003175851560000011
    Figure BDA0003175851560000011
  • Figure BDA0003175851560000071
    Figure BDA0003175851560000071
  • Figure BDA0003175851560000081
    Figure BDA0003175851560000081
Patent Text Reader

Abstract

The present invention provides a method for dispersing Lithol Rubine 7B powder in water. Specifically, the present invention provides a stable aqueous dispersion system of Lithol Rubine 7B, the aqueous dispersion system comprising: color powder, ionic polymer, polyol and water, wherein the ionic polymer is a polyquaternary ammonium salt. The aqueous dispersion system of the present invention has excellent dispersibility and stability, and can be widely used in aqueous cosmetic compositions to improve the quality and effect of products.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of cosmetics, and in particular, relates to a stable aqueous dispersion system of Lithol Rubine 7B and a preparation method thereof. Background Art

[0002] With the popularity of the cosmetics market, more and more new products such as water-based cosmetics are being developed. In such products, color powder provides appearance and coloring power, and the dispersion of color powder in the system greatly affects the product's hiding power, skin adhesion, feel and stability. In the water-based cosmetics currently on the market, color powder often precipitates or floats in the system due to its hydrophobicity and density difference with the medium, resulting in unstable product quality and poor makeup effect, which has become a technical difficulty in the cosmetics industry.

[0003] Lithol Ruby Red 7B is an organic color powder, the main component of which is calcium 3-hydroxy-4-[(4-methyl-2-sulfophenyl)azo]-2-naphthoate, as shown in Formula I. The hydrophilicity of this color powder is poor, and some of it settles in water and a large amount of it floats. Products developed using this type of color powder will directly affect the quality of the product due to uneven dispersion of the color powder.

[0004]

[0005] A series of studies have been conducted on the problem of dispersion of toner with poor hydrophilicity in water. For example, surfactants are added to improve the wettability of the toner surface, including cationic surfactant hexadecyltrimethylammonium bromide (CTAB), nonionic surfactant Span 80, anionic surfactant sodium dodecyl sulfate (SDS), etc.; water-soluble polymers are added to enhance the suspension ability of toner in the medium, including polyvinyl alcohol (PVA), sodium hydroxymethyl cellulose (CMC), etc. However, the results show that the system has a good initial dispersion effect but poor long-term dispersion stability.

[0006] Wu Yang et al. added common surfactants CTAB and Span 80 to improve the dispersibility of nano red selenium powder in ethylene glycol medium. The results showed that after adding 1.5% CTAB, the maximum absorbance was only about 0.7 at 1h; after adding 1.5% Span80, the maximum absorbance was only about 0.5 at 15min. (Wu Yang, Wu Liming, Zhang Zhenzhong, Zhang Hua, Li Linghan. Research on the Dispersion Process of Nano Red Selenium Powder in Ethylene Glycol Medium[J]. Journal of Vacuum Science and Technology, 2019, 39(10):907-911.

[0007] Zhang Ting added the surfactant SDS to improve the dispersibility of nano calcium carbonate. The results showed that after adding 2% SDS, the maximum absorbance reached 2.7 at 0.5h and dropped to 1.2 at 4h. (Zhang Ting. Research on the dispersion technology and dispersion mechanism of nano calcium carbonate for water-based drilling fluid [D]. Southwest Petroleum University, 2014.)

[0008] Qiu Jianmei et al. added water-soluble polymers PVA and CMC to improve the dispersibility of tungsten carbide powder in water medium. The results showed that after adding 1% PVA, the system had a good dispersion effect at 10min-1h, 50% of the powder settled at 4h, and the powder was almost completely settled at 24h; after adding 1% CMC, the system had a good dispersion effect at 10min-4h, and 50% of the powder settled at 24h. (Qiu Jianmei, Zhang Lingjie, Shen Qianhong, Yang Hui, Chen Lesheng, Fan Xianping. Research on the dispersion of tungsten carbide powder in water medium [J]. Rare Metals, 2014, 38(06): 1086-1092.)

[0009] Therefore, there is an urgent need in the art for a uniform and long-term stable aqueous dispersion system of Lithol Rubine 7B. Summary of the invention

[0010] The purpose of the present invention is to provide a stable aqueous dispersion system of Lithol Rubine 7B and a preparation method thereof.

[0011] In a first aspect of the present invention, an aqueous dispersion system of Lithol Rubine 7B is provided, wherein the dispersion system comprises the following components in parts by weight:

[0012] (a) 0.2-5 parts by weight (preferably 0.2-3 parts by weight, more preferably 0.5-2 parts by weight, and further preferably 0.5-1.5 parts by weight) of Lithol Ruby 7B toner;

[0013] (b) 0.1-10 parts by weight of an ionic polymer (preferably 0.2-8 parts by weight, more preferably 0.25-5 parts by weight, for example 0.5, 1, 1.5, 2, 2.5, 3, 3.5, 4);

[0014] (c) 20-50 parts by weight of polyol (preferably 30-49.5 parts by weight, more preferably 40-49.25 parts by weight, further preferably 45-49.25 parts by weight, for example 49.25, 49, 48.23, 48.15, 48, 47.5);

[0015] (d) 20-50 parts by weight of water (preferably 30-49.5 parts by weight, more preferably 40-49.25 parts by weight, further preferably 45-49 parts by weight, for example 49.25, 49, 48.23, 48.15, 48, 47.5).

[0016] In another preferred embodiment, the ionic polymer is a polyquaternary ammonium salt.

[0017] In another preferred embodiment, the polyquaternary ammonium salt exhibits cationic properties.

[0018] In another preferred embodiment, the polyquaternium salt is selected from the following group: polyquaternium-6, polyquaternium-7, polyquaternium-10, polyquaternium-11, polyquaternium-22, polyquaternium-24, polyquaternium-28, polyquaternium-37, polyquaternium-39, polyquaternium-55, polyquaternium-56, or a combination thereof.

[0019] In another preferred embodiment, the polyquaternium salt is selected from the following group: polyquaternium-7, polyquaternium-11, polyquaternium-22, polyquaternium-39, polyquaternium-55, or a combination thereof.

[0020] In another preferred embodiment, the polyquaternium salt is selected from the group consisting of polyquaternium-7, polyquaternium-22, or a combination thereof, preferably polyquaternium-22.

[0021] In another preferred embodiment, the polyol includes C 2 -C 8 triol, tetraol, or a combination thereof.

[0022] In another preferred embodiment, the polyol includes C 2 -C 6 triol, tetraol, or a combination thereof.

[0023] In another preferred embodiment, the polyol is selected from the group consisting of glycerol, pentaerythritol, or a combination thereof.

[0024] In another preferred embodiment, the mass ratio of the polyol to water is 0.8-1.2:0.8-1.2, preferably 1:1.

[0025] In another preferred embodiment, the dispersed system comprises the following components in parts by weight:

[0026] (a) 0.2-5 parts by weight (preferably 0.2-3 parts by weight, more preferably 0.5-2 parts by weight, and further preferably 0.5-1.5 parts by weight) of Lithol Ruby 7B toner;

[0027] (b) 0.1-10 parts by weight of an ionic polymer (preferably 0.2-8 parts by weight, more preferably 0.25-5 parts by weight, for example 0.5, 1, 1.5, 2, 2.5, 3, 3.5, 4);

[0028] (c) 20-49.75 parts by weight (preferably 30-49.5 parts by weight, more preferably 40-49.25 parts by weight, and further preferably 45-49 parts by weight) of polyol;

[0029] (d) 20-49.75 parts by weight (preferably 30-49.5 parts by weight, more preferably 40-49.25 parts by weight, and further preferably 45-49 parts by weight) of water;

[0030] (e) 0-0.5 parts by weight (preferably 0.01-0.2 parts by weight, more preferably 0.01-0.1 parts by weight, such as 0.02, 0.05, 0.08) of a rheology modifier;

[0031] (f) Emulsifier: 0-3 parts by weight (preferably 0-2 parts by weight, more preferably 0.05-2 parts by weight, for example 0.1, 0.2, 0.5, 1, 1.5).

[0032] In another preferred embodiment, the rheology regulator is selected from the following group: xanthan gum, tapioca starch, ammonium acryloyldimethyltaurate / behenyl alcohol polyether-25 methacrylate crosspolymer, polyacrylate crosspolymer-6, sodium hyaluronate, sodium polyacrylate, carbomer, carrageenan, disteardimonium hectorite, hydroxyethyl acrylate / sodium acryloyldimethyltaurate copolymer, acrylic acid (esters) / C10-C30 alkyl acrylate crosspolymer, gelatin, cellulose gum, or a combination thereof.

[0033] In another preferred embodiment, the rheology modifier is selected from the following group: xanthan gum, tapioca starch, ammonium acryloyldimethyltaurate / beheneth-25 methacrylate crosspolymer, polyacrylate crosspolymer-6, sodium hyaluronate, or a combination thereof.

[0034] In another preferred embodiment, the emulsifier is selected from the following group: cocamidopropyl betaine, sodium cocoyl methyl taurate, sodium cocoyl glycinate, sodium fatty acyl glutamate, sodium lauryl sulfate, sodium lauryl fatty alcohol polyoxyethylene ether sulfate, sodium cocoyl isethionate, sodium laureth sulfate, dodecyltrimethylammonium chloride, hexadecyltrimethylammonium chloride, Span 80, or a combination thereof.

[0035] In another preferred embodiment, the emulsifier is selected from the following group: sodium stearoyl glutamate, sodium lauryl sulfate, Span 80, sodium lauryl fatty alcohol polyoxyethylene ether sulfate, sodium cocoyl isethionate, or a combination thereof.

[0036] In another preferred embodiment, the dispersion system further comprises a pH regulator.

[0037] In another preferred embodiment, the pH of the dispersed system is in the range of 5.5 to 8.5.

[0038] In another preferred embodiment, the pH of the dispersed system is in the range of 6-8.

[0039] In another preferred embodiment, the pH adjuster is selected from the following group: sodium citrate, sorbic acid, sodium metaphosphate, disodium hydrogen phosphate, sodium hydroxide, triethanolamine, or a combination thereof.

[0040] In another preferred embodiment, the particle size of the Lithol Rubine 7B toner is 1-1.5 μm.

[0041] In a second aspect of the present invention, a cosmetic composition is provided, comprising:

[0042] (a) an aqueous dispersion of Lithol Rubine 7B according to the first aspect of the present invention; and

[0043] (b) a cosmetically acceptable carrier.

[0044] In another preferred embodiment, the cosmetically acceptable carrier does not significantly affect the dispersibility of the dispersed system.

[0045] In another preferred embodiment, the cosmetically acceptable carrier is selected from the following group: flavors, preservatives, salts, antibacterial agents, antioxidants, or a combination thereof.

[0046] In the third aspect of the present invention, there is provided a use of the aqueous dispersion system of Lithol Rubine 7B as described in the first aspect of the present invention for preparing a cosmetic composition, wherein the cosmetic composition is a water-soluble cosmetic product.

[0047] In another preferred embodiment, the cosmetic composition comprises a water-soluble eyeliner.

[0048] In another preferred embodiment, the cosmetic composition is not suitable for use in hair care products.

[0049] In a fourth aspect of the present invention, there is provided a method for preparing an aqueous dispersion of Lithol Rubine 7B as described in the first aspect of the present invention, comprising the following steps:

[0050] (a) mixing Lithol Ruby Red 7B toner, polyol, and ionomer (emulsifier) ​​to obtain a toner mixture;

[0051] (b) mixing the toner mixture described in step (a) with water (rheology modifier) ​​to obtain the dispersion system.

[0052] In another preferred embodiment, the mixing method is magnetic stirring at a speed of 2000 rpm for 5 to 30 min.

[0053] In another preferred embodiment, the step (b) comprises: adding water to the toner mixture while stirring, and mixing to obtain the dispersed system.

[0054] It should be understood that within the scope of the present invention, the above-mentioned technical features of the present invention and the technical features specifically described below (such as embodiments) can be combined with each other to form a new or preferred technical solution. Due to space limitations, they will not be described one by one here. BRIEF DESCRIPTION OF THE DRAWINGS

[0055] Figure 1 Optical photographs showing the dispersion effect of the aqueous dispersion system of the present invention with the addition of different ionic polymers; ae are polyquaternium-7, polyquaternium-11, polyquaternium-22, polyquaternium-39, and polyquaternium-55, respectively.

[0056] Figure 2 Optical photographs of the aqueous dispersion system of the present invention to which different ionic polymers are added after centrifugation at 8000 rpm for 10 minutes are shown; ae are polyquaternium-7, polyquaternium-11, polyquaternium-22, polyquaternium-39, and polyquaternium-55, respectively.

[0057] Figure 3 Optical photographs showing the dispersing effect of the aqueous dispersion system of the present invention with the addition of different mass concentrations of polyquaternium-22; ah is 0.5%, 1%, 1.5%, 2%, 2.5%, 3%, 3.5%, and 4%, respectively.

[0058] Figure 4 Optical photographs of the aqueous dispersion system of the present invention to which different mass concentrations of polyquaternium-22 were added after centrifugation at 8000 rpm for 30 minutes are shown; ah is 0.5%, 1%, 1.5%, 2%, 2.5%, 3%, 3.5%, and 4%, respectively.

[0059] Figure 5 Optical photographs showing the dispersion effect of the aqueous dispersion system of the present invention with the addition of different rheology modifiers; ae are xanthan gum, tapioca starch, ammonium acryloyldimethyltaurate / behenyl alcohol polyether-25 methacrylate crosspolymer, polyacrylate crosspolymer-6, and sodium hyaluronate, respectively.

[0060] Figure 6 Optical photographs showing the dispersion effect of the aqueous dispersion system of the present invention with the addition of different emulsifiers: ad are Tween 80, sodium stearoyl glutamate, sodium lauryl sulfate, and Span 80, respectively.

[0061] Figure 7 The optical photographs of the dispersion effect of the aqueous dispersion system with no ionic polymer added but only water (a); only water and glycerol added (b); only water and propylene glycol added (c); and only water and butylene glycol added (d) are shown.

[0062] Figure 8The optical photographs show the dispersion effects of aqueous dispersion systems without adding ionic polymers but only adding water and glycerol (a); adding only water and propylene glycol (b); adding only water and butylene glycol (c) after centrifugation at 2000 rpm for 10 minutes.

[0063] Fig. 9 The optical photograph shows the dispersion effect of the aqueous dispersion system of the present invention after standing for 5 months. DETAILED DESCRIPTION

[0064] After extensive and in-depth research, the inventor unexpectedly discovered a stable aqueous dispersion system of Lithol Rubine 7B for the first time.

[0065] Specifically, the present invention obtains a highly dispersed and highly stable Lithol Rubine 7B suspension by adding ionic polymers and polyols. The stable Lithol Rubine 7B dispersion system of the present invention can be widely used in aqueous cosmetic compositions to improve the quality and effect of the products. The present invention is completed on this basis.

[0066] Specifically, the aqueous dispersion system of the present invention, on the one hand, adds an ionic polymer that can improve the surface electrical properties of the solid particles of the toner, and adsorbs to the surface of the toner particles through strong adsorption, so that there is repulsion between the toner particles and the toner particles are evenly suspended in the medium. On the other hand, polyols that can improve the characteristics of the aqueous medium are used to synergistically enhance the dispersibility of Lithol Rubine 7B, which has poor hydrophilicity, and the solid particles of the toner are effectively dispersed evenly and suspended stably for a long time by adjusting the electrical properties of the surface of the toner particles and the properties of the medium.

[0067] The aqueous dispersion system of the present invention has excellent stability and can still maintain a high degree of dispersion after centrifugation at 8000 rpm for 30 minutes. The aqueous dispersion system of the present invention can be widely used in cosmetic compositions to improve the quality and effect of products. The present invention is completed on this basis.

[0068] Lithol Ruby Red 7B

[0069] Lithol Red 7B is a hydrophobic color powder with a blue-dark red dry powder appearance. It is insoluble in ethanol, but yellow-red when dissolved in hot water. It is magenta when exposed to concentrated sulfuric acid, and a magenta precipitate after dilution. Its aqueous solution will form a brown-red precipitate when exposed to hydrochloric acid, and brown when exposed to sodium hydroxide. It has bright color and strong tinting power.

[0070] The main component of the toner is calcium 3-hydroxy-4-[(4-methyl-2-sulfophenyl)azo]-2-naphthoate (Formula I), which belongs to azo lake toner. The precursor of this type of toner is water-soluble, and contains sulfonic acid and carboxylic acid groups in the molecule, but it generates water-insoluble toner after reacting with a precipitant, so it is not easy to disperse evenly in water.

[0071] The toner has poor hydrophilicity and partially settles and largely floats in water.

[0072]

[0073] As used herein, the terms "color powder", "Lithol Rubine 7B", "color powder of the present invention", etc. are used interchangeably.

[0074] Ionic polymer

[0075] Ionic polymer refers to a class of polymers containing ions.

[0076] Ionic polymer of the present invention is a polyquaternary ammonium salt. Different from the solubilizing effect of conventional polyquaternary ammonium salt, the present invention utilizes the superior adsorption capacity of polyquaternary ammonium salt, and is added into the dispersion system of the present invention and can be used for improving the electrical property on the surface of toner particles, making the toner particles positively charged, and then repelling each other, thereby improving the dispersibility of toner and making it stably suspended in the dispersion system. Therefore, the aqueous dispersion system of the present invention comprising polyquaternary ammonium salt can be used for various hydrophobic cosmetic compositions.

[0077] The polyquaternium salt of the present invention is a polyquaternium salt exhibiting cationic properties, selected from the following group: polyquaternium-1, polyquaternium-2, polyquaternium-4, polyquaternium-6, polyquaternium-7, polyquaternium-10, polyquaternium-11, polyquaternium-15, polyquaternium-16, polyquaternium-18, polyquaternium-19, polyquaternium-22, polyquaternium-24, polyquaternium-28, polyquaternium-30, polyquaternium-32, polyquaternium-33, polyquaternium-35, polyquaternium-37, polyquaternium-39, polyquaternium-43, polyquaternium-44, polyquaternium Polyquaternium-46, Polyquaternium-47, Polyquaternium-49, Polyquaternium-50, Polyquaternium-51, Polyquaternium-52, Polyquaternium-53, Polyquaternium-55, Polyquaternium-56, Polyquaternium-57, Polyquaternium-61, Polyquaternium-62, Polyquaternium-63, Polyquaternium-64, Polyquaternium-65, Polyquaternium-67, Polyquaternium-68, Polyquaternium-69, Polyquaternium-73, Polyquaternium-74, Polyquaternium-75, Polyquaternium-76, Polyquaternium-78, Polyquaternium-80, Polyquaternium-104, or a combination thereof.

[0078] The polyquaternary ammonium salt is a block copolymer comprising blocks selected from the group consisting of polydimethyldiallylammonium chloride, polyacrylamide, polyacrylic acid, or a combination thereof.

[0079] The polyquaternium salt is selected from the following group: polyquaternium-7, polyquaternium-11, polyquaternium-22, polyquaternium-39, polyquaternium-55, or a combination thereof.

[0080] The polyquaternary ammonium salt comprises one or more of the structural units shown in formula II-IV:

[0081]

[0082] in,

[0083] n is an integer from 0 to 10,000; m is an integer from 0 to 10,000; l is an integer from 0 to 10,000.

[0084] The ionic polymer is selected from the group consisting of polyquaternium-7, polyquaternium-22, or a combination thereof.

[0085] The structural formulas of the polyquaternium salt-7 and polyquaternium salt-22 are as follows:

[0086]

[0087] The relative molecular mass of the polyquaternium salt-7 is 8.0×10 4 -3.0×10 6 .

[0088] The relative molecular mass of the polyquaternium salt-7 is 1.2×10 5 .

[0089] The relative molecular mass of the polyquaternium salt-22 is 8.0×10 4 -3.0×10 6 .

[0090] The relative molecular mass of the polyquaternium salt-22 is 4.5×10 5 .

[0091] Aqueous dispersion system of the present invention

[0092] As used herein, the terms "dispersion system", "aqueous dispersion system", "dispersion system of the present invention", "aqueous dispersion system of the present invention" and the like are used interchangeably and refer to a dispersion system with water as the main component or very hydrophilic in which the Lithol Ruby 7B toner can be dispersed and stably suspended in large quantities and uniformly.

[0093] The dispersion system described in the present invention is a suspension comprising toner, ion polymer, polyol and water.

[0094] The dispersion system does not need to add other related dispersing aids, that is, only polyols and ionic polymers are added, so as to obtain a dispersion liquid with excellent dispersibility, and the system can be kept stable for up to 5 months.

[0095] One or more additional ingredients may be added to the dispersion system, as long as the additional ingredients do not substantially affect the aqueous dispersion system of the present invention (such as decreased dispersibility, color difference, etc.).

[0096] The dispersion system may include other ingredients that have no significant effect on the dispersion performance, wherein the other ingredients are selected from the group consisting of an emulsifier, a rheology regulator, a pH regulator, or a combination thereof.

[0097] The dispersion system may or may not contain a rheology regulator and / or an emulsifier, and the rheology regulator and / or the emulsifier have no obvious promoting or inhibiting effect on the dispersion performance of the dispersion system.

[0098] Preferably, based on the total weight of the dispersed system, the dispersed system comprises:

[0099] (a) 0.2% to 5% of Lithol Rubine 7B toner, preferably 0.5% to 2%, more preferably 0.5% to 1.5%, further preferably 1%;

[0100] (b) 0.1%-10% ionomer, preferably 0.25%-5%, for example 0.5%, 1%, 1.5%, 2%, 2.5%, 3%, 3.5%, 4%;

[0101] (c) 0-0.5% rheology modifier, preferably 0.01%-0.2%, more preferably 0.01%-0.1%, for example 0.02%, 0.05%, 0.08%;

[0102] (d) 0-3% emulsifier, preferably 0-2%, more preferably 0.05-2%, for example 0.1%, 0.2%, 0.5%, 1%, 1.5%;

[0103] (e) 20% to 49.75% of a polyol, preferably 30% to 49.5%, more preferably 40% to 49.25%;

[0104] (f) 20% to 49.75% water, preferably 40% to 49.5%, more preferably 45% to 49.25%.

[0105] Cosmetic composition

[0106] Based on the aqueous dispersion system of the present invention, the present invention also provides a cosmetic composition comprising the aqueous dispersion system. In addition to the aqueous dispersion system of the present invention, the cosmetic composition also includes a cosmetically acceptable carrier.

[0107] The cosmetic composition can be used to prepare water-soluble cosmetics, preferably water-based eyeliner and water-soluble eye shadow.

[0108] The cosmetic composition is not suitable for use in hair care products.

[0109] The cosmetically acceptable carrier or excipient is selected from the following group: flavors, preservatives, salts, antibacterial agents, antioxidants, or combinations thereof.

[0110] For example, a fragrance may be added to the dispersion of the present invention to obtain a desired fragrance.

[0111] Preservatives can be added to the dispersion system of the present invention to further obtain long-term storage performance. Representative preservatives are selected from the following group: alcohols, parabens, formaldehyde releasers, methylchloroisothiazolinone, methylisothiazolinone, iodopropynyl butylcarbamate or a combination thereof.

[0112] Preferably, the alcohol is selected from the group consisting of phenoxyethanol, 1,3-butylene glycol, 1,2-pentanediol, 1,2-hexanediol, ethylhexylglycerin, or a combination thereof;

[0113] Preferably, the parabens are selected from the group consisting of methyl paraben, ethyl paraben, propyl paraben, butyl paraben, isopropyl paraben and isobutyl paraben, or a combination thereof;

[0114] Preferably, the formaldehyde releaser is selected from the group consisting of 1,3-dihydroxymethyl-5,5-dimethylhydantoin (DMDMH), imidazolidinyl urea, diazoimidazolidinyl urea and sodium hydroxymethylglycinate, or a combination thereof.

[0115] The antioxidant is selected from the group consisting of tocopherol, tocopherol acetate, tocopherol succinate, a tocopherol mixture, or a combination thereof.

[0116] Preparation method

[0117] The preparation method of the aqueous dispersion system of Lithol Ruby 7B of the present invention comprises the following steps:

[0118] (a) providing all components except water in the aqueous dispersion system (including toner, ion polymer and polyol, etc.), and mixing them to obtain a toner mixture;

[0119] (b) adding water to the toner mixture in step (a) while stirring, thereby obtaining the aqueous dispersion system.

[0120] The mixing is performed by magnetic stirring at a speed of 2000 rpm for 5 to 30 minutes.

[0121] The preparation method comprises the following steps:

[0122] (1) Weigh polyol, color powder, and ion polymer into container A and stir magnetically at 2000 rpm for 10 min;

[0123] (2) Continue to use magnetic stirring at 2000 rpm for 5 min, adding an appropriate amount of deionized water during the stirring process;

[0124] (3) After stirring, ultrasonicate for 5 min, and finally magnetically stir at 2000 rpm for 30 min.

[0125] The main advantages of the present invention include:

[0126] 1) The aqueous dispersion system of the present invention significantly improves the dispersibility of Lithol Ruby Red 7B color powder in water, and the dispersibility of the color powder in the cosmetic composition prepared using the aqueous dispersion system of the present invention is improved, thereby improving the appearance and coloring strength of the composition;

[0127] 2) The aqueous dispersion system of the present invention is stable in long-term suspension, which is beneficial to the formulation stability of the end product.

[0128] The present invention will be further described below in conjunction with specific examples. It should be understood that these examples are intended only to illustrate the present invention and are not intended to limit the scope of the present invention. The experimental methods for the unrecorded specific conditions in the following examples are usually based on conventional conditions or the conditions recommended by the manufacturer. Unless otherwise stated, percentages and parts are weight percentages and weight parts.

[0129] Materials and methods

[0130] The raw materials used in the examples are all commercially available products.

[0131] The centrifuge is Hunan Xiangyi H1650-W centrifuge.

[0132] The instrument for absorbance testing was a UV-1800 ultraviolet-visible spectrophotometer purchased from Shimadzu Instruments (Suzhou) Co., Ltd.

[0133] Dispersion performance test method:

[0134] First, directly observe and judge the dispersibility of the configured dispersed system. If it can be judged directly, then make the judgment directly;

[0135] If it is not possible to judge directly, centrifuge the dispersion system at a certain speed for a period of time. The centrifugal speed and time should be based on a certain degree of differentiation. Observe the amount of residual color powder in the upper liquid to judge the dispersion performance.

[0136] If it is difficult to judge by directly observing the upper liquid, the middle section of the upper liquid is taken for absorbance test. Since the absorbance test of the original upper liquid exceeds the range, the upper liquid is diluted for absorbance test. The dilution multiple is based on the range of 0-4. The ultimate goal is to screen out a better system. However, the present invention is not intended to protect the most preferred system.

[0137] Example 1.

[0138] Weigh each component according to the raw material ratio shown in Table 1, and then follow the steps below:

[0139] (1) Weigh the raw material components (including toner, polyol, and ion polymer) except water as shown in Table 1, add them into container A, and stir them magnetically at 2000 rpm for 10 minutes to obtain a toner mixture;

[0140] (2) Continue to use magnetic stirring at 2000 rpm for 5 min, and add deionized water weighed as shown in Table 1 during the stirring process;

[0141] (3) After the stirring was completed, ultrasonic treatment was performed for 5 min, and finally magnetic stirring was performed at a rotation speed of 2000 rpm for 30 min to obtain samples 1-5.

[0142] Table 1 Sample formulation of Example 1 (weight / g)

[0143]

[0144]

[0145] The dispersion effects of samples 1-5 are as follows: Figure 1 As shown in ae. The results show that the hydrophobic color powder is evenly dispersed, without floating and precipitation, and has bright colors without obvious agglomeration (the sample remaining on the wall of the vial is the color powder that was "thrown" to the wall of the bottle during the stirring process and was not evenly dispersed). It shows that the aqueous dispersion system of the present invention has good dispersing effect and excellent dispersing performance. And using the above-mentioned polyquaternary ammonium salt as an ionic polymer can obtain a dispersion system with excellent dispersing performance, indicating that adding a specific ionic polymer can significantly improve the dispersing performance of the dispersion system.

[0146] The dispersion effect after centrifugation at 8000rpm for 10 minutes is as follows Figure 2 The results show that the samples 1 and 3, which added polyquaternium-7 and polyquaternium-22 as ionic polymers, had less color powder centrifuged and had a better dispersion effect.

[0147] In order to further screen a better dispersion system, the inventors took the upper liquid of sample 1 and sample 3 after centrifugation to compare their maximum absorbance values. Since direct testing exceeded the instrument range, the upper liquid was diluted 10 times to test its peak absorbance value (maximum absorbance value). The maximum absorbance value of sample 1 was 1.113, and the maximum absorbance value of sample 3 was 1.434. The maximum absorbance value of sample 3 was relatively higher, and the dispersion effect was better.

[0148] Example 2.

[0149] This example is to verify the dispersibility of the aqueous dispersion system of the present invention when different amounts of polyquaternium-22 are added.

[0150] Weigh each component according to the raw material ratio shown in Table 2, and then operate according to the steps described in Example 1 to obtain samples 6-13.

[0151] After centrifugation at 8000 rpm for 30 minutes, the supernatant was diluted 10 times and then subjected to absorbance test. The peak absorbance is shown in Table 2 below.

[0152] Table 2 Example 2 sample formula (weight / g) and peak absorbance value of the treated sample

[0153]

[0154] The dispersion effects of samples 6-13 are as follows: Figure 3 The dispersion effect after centrifugation is shown in Figure 4 As shown in ah.

[0155] As shown in Table 2, the peak absorbance of samples 6-13 after centrifugal dilution treatment increases with the increase of polyquaternium-22 content, among which the absorbance of samples 10-12 exceeds 2.8, indicating that the dispersion effect of adding 2.5-4wt% of ionic polymer is better.

[0156] Example 3.

[0157] This example is to verify the dispersibility of the aqueous dispersion system of the present invention when a rheology modifier is added.

[0158] Weigh each component according to the raw material ratio shown in Table 3, and then follow the steps below:

[0159] 1. Weigh the color powder, ion polymer and polyol into container A, stir magnetically at 2000 rpm for 10 min, and heat to 90°C;

[0160] 2. Weigh water into container B, stir magnetically at 700 rpm for 10 min, add rheology modifier during stirring, and heat to 90°C;

[0161] 3. Stir container A magnetically at 2000 rpm for 5 min, and pour the material in container B into container A while it is still hot;

[0162] 4. Ultrasonication for 5 min, and finally magnetic stirring at 2000 rpm for 30 min to obtain samples 14-18.

[0163] Table 3 Sample formulation of Example 3 (weight / g)

[0164]

[0165] The dispersion effects of samples 14-18 are as follows Figure 5 As shown in ae. It is shown that adding different rheology modifiers can obtain a color powder dispersion system with excellent dispersion effect. Therefore, the aqueous dispersion system of the present invention can be added with a rheology modifier to prepare a product including the aqueous dispersion system of the present invention.

[0166] Example 4.

[0167] This example is to verify the dispersibility of the aqueous dispersion system of the present invention when an emulsifier is added.

[0168] The components were weighed according to the raw material ratios shown in Table 4, and then the steps described in Example 1 were followed to obtain samples 19-22, except that an emulsifier was also added to container A.

[0169] Table 4 Formula of Example 4 Sample (weight / g)

[0170] raw material Sample 19 Sample 20 Sample 21 Sample 22 Toner 0.2 0.2 0.2 0.2 glycerin 9.63 9.63 9.63 9.63 Polyquaternium-22 0.5 0.5 0.5 0.5 Twain 80 0.04 0 0 0 Sodium Stearoyl Glutamate 0 0.04 0 0 Sodium Lauryl Sulfate 0 0 0.04 0 Span 80 0 0 0 0.04 water 9.63 9.63 9.63 9.63

[0171] The dispersion effects of samples 19-22 are as follows Figure 6 As shown in ad in the figure. As can be seen from the figure, adding an emulsifier can obtain an aqueous dispersion system with excellent dispersibility. Therefore, the aqueous dispersion system of the present invention can be added with an emulsifier to prepare a product including the aqueous dispersion system of the present invention.

[0172] Comparative Example 1.

[0173] This example is to verify the dispersibility of the dispersion system when no ionic polymer is added.

[0174] Weigh each component according to the raw material ratio shown in Table 5, and then operate according to the steps described in Example 1 to obtain comparative samples C1-C4.

[0175] Table 5 Formula of Comparative Example 1 Sample (weight / g)

[0176] raw material Sample C1 Sample C2 Sample C3 Sample C4 Toner 0.2 0.2 0.2 0.2 glycerin 0 9.9 0 0 Propylene glycol 0 0 9.9 0 Butanediol 0 0 0 9.9 water 19.8 9.9 9.9 9.9

[0177] The dispersion effects of samples C1-C4 are as follows: Figure 7 As shown in ad.

[0178] The results show that when polyols and ionic polymers are not added (the color powder is directly dispersed in water), the color powder sinks to the bottom or floats on the interface due to surface effects, indicating that the color powder itself has poor dispersibility in water and is basically unable to disperse; when polyols are added, the dispersibility of the color powder is improved, indicating that polyols can improve the dispersibility of the color powder of the present invention, but the dispersion effect is still not ideal.

[0179] The color powder of samples C3 and C4 obviously sank to the bottom when left standing, and the system showed obvious color unevenness. In sample C2 where only glycerol was added as the polyol, the color powder also sank to the bottom, but the amount of color powder dispersed in the water increased significantly, and the color of the supernatant in the water was darker. It is speculated that the effect of triols on improving dispersibility may be more obvious than that of diols.

[0180] Samples C2-C4 were centrifuged at 2000 rpm for 10 min ( Figure 8 ), the toners of samples C3 and C4 were basically completely separated by centrifugation. In comparison, the toners of sample C2 were not completely separated by centrifugation, and a large amount of toners were still dispersed in the supernatant of the centrifuge, indicating that glycerol can improve the dispersibility of toners in water, but the dispersibility still needs to be further improved.

[0181] Test Example 1. Long-term stability

[0182] The sample 10 was left to stand for 5 months to observe its stability.

[0183] Dispersion effect Fig. 9 As shown, it is shown that the aqueous dispersion system of the present invention has excellent long-term stability, and the aqueous makeup prepared by the aqueous dispersion system of the present invention has a long shelf life.

[0184] All documents mentioned in the present invention are cited as references in this application, just as each document is cited as reference individually. In addition, it should be understood that after reading the above teachings of the present invention, those skilled in the art can make various changes or modifications to the present invention, and these equivalent forms also fall within the scope defined by the claims attached to this application.

Claims

1. An aqueous dispersion system of Lithol Rubine 7B, characterized in that: The dispersed system consists of the following components in parts by weight: Wherein, the ionic polymer is polyquaternium-22; the rheology modifier is selected from the following group: xanthan gum, tapioca starch, ammonium acryloyldimethyltaurate / behenyl alcohol polyether-25 methacrylate crosspolymer, polyacrylate crosspolymer-6, sodium hyaluronate, or a combination thereof; the emulsifier is selected from the following group: Tween 80, sodium stearoyl glutamate, sodium lauryl sulfate, Span 80, or a combination thereof; The main component of the Lithol Ruby Red 7B toner is calcium 3-hydroxy-4-[(4-methyl-2-sulfophenyl)azo]-2-naphthoate, as shown in Formula I; The content of the ionic polymer is 0.25-5wt%; The mass ratio of the glycerol to water is 0.8-1.2:0.8-1.

2.

2. The aqueous dispersion system of Lithol Rubine 7B according to claim 1, characterized in that: The dispersed system consists of the following components in parts by weight:

3. The aqueous dispersion system of Lithol Rubine 7B according to claim 1, characterized in that: The dispersed system consists of the following components in parts by weight:

4. The aqueous dispersion system of Lithol Rubine 7B according to claim 1, characterized in that The dispersed system consists of the following components in parts by weight:

5. The aqueous dispersion system of Lithol Rubine 7B according to claim 1, characterized in that: The mass ratio of the glycerol to water is 1:

1.

6. The aqueous dispersion system of Lithol Rubine 7B according to claim 1, characterized in that: The pH of the dispersed system is in the range of 5.5 to 8.

5.

7. The aqueous dispersion system of Lithol Rubine 7B according to claim 1, characterized in that: The particle size of the Lithol Ruby Red 7B toner is 1-1.5 μm.

8. The aqueous dispersion system of Lithol Rubine 7B according to claim 1, characterized in that: The dispersed system consists of the following components in parts by weight: Wherein, the rheology modifier is selected from the following group: xanthan gum, tapioca starch, ammonium acryloyldimethyltaurate / beheneth-25 methacrylate crosspolymer, polyacrylate crosspolymer-6, sodium hyaluronate, or a combination thereof; The emulsifier is selected from the following group: Tween 80, sodium stearoyl glutamate, sodium lauryl sulfate, Span 80, or a combination thereof.

9. A cosmetic composition, characterized in that The cosmetic composition comprises: (a) an aqueous dispersion of Lithol Rubine 7B according to any one of claims 1 to 8; and (b) a cosmetically acceptable carrier.

10. The use of the aqueous dispersion system of Lithol Rubine 7B according to any one of claims 1 to 8, characterized in that: The invention is used for preparing a cosmetic composition, wherein the cosmetic composition is a water-soluble cosmetic product.

11. The use according to claim 10, characterized in that The cosmetic composition includes a water-soluble liquid eyeliner.

12. A method for preparing an aqueous dispersion of Lithol Rubine 7B according to any one of claims 1 to 8, characterized in that: The following steps are involved: (a) mixing Lithol Ruby Red 7B toner, glycerol, an ionomer and an emulsifier to obtain a toner mixture; (b) mixing the toner mixture described in step (a) with water and a rheology modifier to obtain the aqueous dispersion system.