A cross-coupling-resistant temperature-pressure integrated sensing array and its fabrication and packaging method
By designing an anti-cross-coupling temperature-pressure integrated sensing array and employing an isolated cavity and composite material structure, the cross-coupling problem of multi-parameter sensing in flexible sensors was solved, enabling the application of multi-parameter sensors with high response time and stability.
Patent Information
- Application Number
- CN202311122279.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2023-08-31
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2043-08-31
AI Technical Summary
Existing flexible sensors are mostly single-parameter sensors, which suffer from severe cross-coupling and cannot meet the requirements of multi-parameter sensing. Furthermore, their response time, durability, and stability are insufficient.
A temperature-pressure integrated sensing array with anti-cross-coupling is designed, employing a flexible substrate, a sensitive layer, and a flexible top cover structure. By setting isolation cavities and through cavities on the sensitive layer substrate, and combining PDMS/BN and polyimide/boron nitride composite materials, low-coupling integration of temperature and pressure sensing units is achieved, and chemical bonding encapsulation technology is used.
It achieves low-coupling integrated sensing of temperature and pressure, improves response time, durability and stability, enhances sensor repeatability and sensitivity, and is suitable for acquiring multi-parameter environmental data.
Smart Images

Figure CN117232576B_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of flexible electronics, and more specifically, it designs a temperature-pressure integrated sensing array with anti-cross-coupling properties and its fabrication and packaging methods. Background Technology
[0002] Flexible sensors have attracted widespread attention from researchers at home and abroad due to their excellent conformal capability to irregular curved surfaces, light weight, thinness, and flexibility. However, in recent years, with the continuous development of artificial intelligence technology and flexible electronics science, major changes have taken place in high-tech fields such as intelligent robots and wearable devices. As a core device for human-computer interaction, flexible sensors have been subject to higher requirements.
[0003] On the one hand, flexible pressure sensors that convert mechanical force into electrical signals have been well-developed. Many researchers have focused on introducing microstructures to replace common planar structures, such as pyramid structures, hemispherical microstructures, and biomimetic structures, achieving significant progress in improving device sensitivity. However, flexible pressure sensors based on pyramid and hemispherical microstructures are prone to failures such as interface delamination due to poor interfacial adhesion and connection strength, and exhibit significant hysteresis and slow response speed. Flexible pressure sensors based on biomimetic structures often have randomness in their structure, making it difficult to guarantee their stability and repeatability. Therefore, the performance of existing flexible pressure sensors still needs comprehensive improvement in terms of response time, durability, stability, and repeatability.
[0004] On the other hand, existing flexible sensors often only have the ability to sense single functions such as pressure or temperature, or single-point spatial sensing. When sensing multiple parameters, severe cross-coupling limits their widespread application in more scenarios. Enabling flexible sensors to achieve multi-parameter decoupled integrated sensing and arraying is of great practical significance. Summary of the Invention
[0005] To address the problems existing in the prior art, the present invention aims to provide an anti-cross-coupling temperature-pressure integrated sensing array and its fabrication and packaging method, which has the ability to integrate temperature and pressure sensing with low coupling, and features good response time, durability, stability and repeatability.
[0006] To achieve the above objectives, the present invention adopts the following technical solution:
[0007] A temperature-pressure integrated sensing array with anti-cross coupling includes a flexible substrate, a sensitive layer, and a flexible top cover stacked sequentially.
[0008] Multiple through cavities arranged in an array are formed on the flexible substrate;
[0009] The sensitive layer includes a sensitive layer substrate disposed on one side surface of a flexible substrate, and a sensitive unit, an electrode lead, and an electrode disposed on the surface of the sensitive layer substrate. The sensitive unit is disposed at a corresponding position in each through-cavity on the sensitive layer substrate.
[0010] Each sensitive unit includes a pressure sensitive unit and a temperature sensitive unit. The pressure sensitive unit is directly opposite the through cavity corresponding to the sensitive unit, and the temperature sensitive unit is disposed on one side of the pressure sensitive unit. A first isolation cavity is provided on the sensitive layer substrate between the pressure sensitive unit and the temperature sensitive unit. The first isolation cavity extends through the thickness direction of the sensitive layer substrate.
[0011] Both the pressure-sensitive unit and the temperature-sensitive unit are connected to the electrodes via electrode leads.
[0012] A second isolation cavity is formed on the flexible substrate at a position directly opposite to the first isolation cavity, and the second isolation cavity extends through the thickness direction of the flexible substrate;
[0013] The surface of the flexible top cover has protrusions at the positions directly opposite each pressure-sensitive unit.
[0014] Preferably, the flexible substrate is made of PDMS / BN composite flexible material, wherein the PDMS / BN composite flexible material is prepared by mixing PDMS liquid, crosslinking agent and boron nitride particles in a mass ratio of (8-12):1:(0.5-2);
[0015] The sensitive layer substrate is made of polyimide / boron nitride composite material, which is prepared by mixing boron nitride particles with PI prepolymer solution, wherein the mass of boron nitride particles is 5wt% to 30wt% of PI prepolymer solution.
[0016] Preferably, an air channel is provided on the surface of the flexible substrate on the side opposite to the sensitive layer substrate. Each through cavity is connected to an air channel. One end of the air channel is connected to the through cavity, and the other end of the air channel extends to the sidewall of the flexible substrate.
[0017] Preferably, both the first isolation cavity and the second isolation cavity are rectangular cavities, and the cross-sections of the first isolation cavity and the second isolation cavity are the same;
[0018] In each sensitive unit, the line connecting the centers of the pressure sensitive unit and the temperature sensitive unit is perpendicular to the length direction of the first isolation cavity and the length direction of the second isolation cavity.
[0019] Preferably, the pressure-sensitive unit is made of strain-sensitive metal, and the pressure-sensitive resistance value is 1.5-3kΩ.
[0020] Preferably, the through cavity is circular, and the pressure-sensitive unit is shaped as at least one of serrated, spiral, and / or zigzag.
[0021] The distribution range of each pressure-sensitive unit is located within the through cavity directly opposite that pressure-sensitive unit.
[0022] Preferably, the temperature-sensitive unit is made of a temperature-sensitive metal with a temperature-sensitive resistance value of 1-2kΩ.
[0023] Preferably, the electrode includes a ground electrode and a measuring electrode;
[0024] Each pressure-sensitive unit and each temperature-sensitive unit have a measuring electrode led out through an electrode lead;
[0025] In the same column of sensitive units, all pressure sensitive units and temperature sensitive units share a ground electrode and are connected to the ground electrode through electrode leads.
[0026] The method for fabricating the anti-cross-coupling temperature-pressure integrated sensing array of the present invention, as described above, includes the following steps:
[0027] S1. Prepare a sacrificial layer on the front side of the silicon wafer;
[0028] S2. The sensitive layer substrate is prepared on the sacrificial layer by spin coating;
[0029] S3. The pressure-sensitive unit is patterned on the sensitive layer substrate using a lift-off process to form the pressure-sensitive unit;
[0030] S4. The temperature-sensitive unit is patterned again on the sensitive layer substrate using a peeling process to form the temperature-sensitive unit.
[0031] S5. The electrode and electrode leads are patterned again on the sensitive layer substrate using a stripping process.
[0032] S6. The first isolation cavity on the sensitive layer substrate is prepared by inductively coupled plasma etching;
[0033] S7. The flexible substrate and flexible top cover are prepared using a molding process;
[0034] S8. The flexible substrate, sensitive layer substrate and flexible top cover are packaged using chemical bonding method.
[0035] The packaging method for the anti-cross-coupling temperature-pressure integrated sensing array of the present invention, as described above, includes the following process:
[0036] The surface of the sensitive layer substrate was chemically modified using an aqueous solution of 3-mercaptopropyltrimethoxysilane; the aqueous solution of 3-mercaptopropyltrimethoxysilane was prepared by mixing 3-mercaptopropyltrimethoxysilane and water at a volume ratio of (2-10):100.
[0037] The flexible substrate and the chemically modified sensitive layer substrate are then oxidized using oxygen plasma. The oxygen plasma oxidation process uses a power of 40-80W and a time of 10-40s.
[0038] Then, conformally contact the flexible substrate with the sensitive layer substrate for 8-12 minutes to complete the bonding between the flexible substrate and the sensitive layer substrate;
[0039] The surface of the sensitive layer substrate in the overall structure bonded to the flexible substrate and the sensitive layer substrate is then chemically modified using the 3-mercaptopropyltrimethoxysilane aqueous solution.
[0040] Then, oxygen plasma is used to oxidize the overall structure of the flexible top cover and the flexible substrate bonded to the sensitive layer substrate. The power of the oxygen plasma oxidation treatment is 40-80W and the time is 10-40s.
[0041] The flexible top cover and the flexible substrate are then conformally bonded to the sensitive layer substrate for 8-12 minutes to complete the bonding between the flexible top cover and the sensitive layer substrate, thus completing the packaging of the anti-cross-coupling temperature-pressure integrated sensing array.
[0042] Compared with the prior art, the present invention has at least the following beneficial technical effects:
[0043] Traditional flexible sensors can only sense and test one parameter, limiting their information acquisition capabilities and making it difficult to meet the sensing needs of various applications. To address this issue, this invention employs a highly efficient integration of resistive pressure and temperature sensing units, enabling the simultaneous acquisition of environmental data for multiple parameters and thus expanding its application scope. To reduce cross-coupling between the temperature and pressure sensing units, an isolation cavity is created between them (specifically, a first isolation cavity is created on the sensing layer substrate, and a second isolation cavity is created on the flexible substrate). This reduces the impact of strain generated by the pressure sensing unit under pressure on the temperature sensing unit. Furthermore, since the thermal conductivity of air is much lower than that of the materials used in the sensing layer substrate and the flexible substrate, heat generated by the self-heating effect of the temperature sensing unit can be effectively prevented from being transferred to the pressure sensing unit. Experimental testing shows that the anti-cross-coupling temperature-pressure integrated sensing array of this invention possesses the capability of low-coupling integrated sensing of temperature and pressure, and exhibits good response time, durability, stability, and repeatability.
[0044] Furthermore, in order to reduce the impact of the self-heating effect of the temperature-sensitive unit on the measurement accuracy, the present invention dops the polyimide and / or PDMS with boron nitride (BN), which effectively reduces the thermal conductivity of the flexible substrate and the sensitive layer substrate material, enabling the temperature-sensitive unit to quickly reach equilibrium with the external ambient temperature.
[0045] Furthermore, in order to further improve the pressure sensing sensitivity, a through cavity was opened on the flexible substrate, and the pressure sensing unit was designed as a sawtooth divergent shape according to its strain distribution, which showed high sensitivity. In addition, the pressure sensing unit also showed high sensitivity when the shape was spiral and zigzag, but slightly lower than that of the sawtooth divergent shape.
[0046] The preparation method described in this invention enables the anti-cross-coupling temperature-pressure integrated sensing array of this invention to be compatible with MEME fabrication processes, with high preparation accuracy, good processing consistency, and easy mass production.
[0047] The encapsulation method described in this invention, compared with traditional encapsulation methods that rely on van der Waals forces or adhesive bonding, solves the failure modes such as easy separation and detachment at the interface connection, while ensuring the high degree of morphological preservation of the material surface, greatly improving the stability and repeatability of the sensor. Attached Figure Description
[0048] Figure 1 This is an exploded schematic diagram of an anti-cross-coupling temperature-pressure integrated sensing array according to an embodiment of the present invention;
[0049] Figure 2 This is a schematic diagram of the back side of the flexible substrate according to an embodiment of the present invention;
[0050] Figure 3 This is a cross-sectional view of the flexible substrate according to an embodiment of the present invention;
[0051] Figure 4 This is a schematic diagram of the sensitive layer according to an embodiment of the present invention;
[0052] Figure 5(a) is a simulation result diagram of the pressure-sensitive unit of the embodiment of the present invention; Figure 5(b) is a schematic diagram of the pressure-sensitive unit (sawtooth divergent shape) of the embodiment of the present invention; Figure 5(c) is a schematic diagram of the pressure-sensitive unit (spiral shape) of the embodiment of the present invention; Figure 5(d) is a schematic diagram of the pressure-sensitive unit (broken line shape) of the embodiment of the present invention.
[0053] Figure 6 This is a schematic diagram of the temperature-sensitive unit according to an embodiment of the present invention;
[0054] Figure 7 This is a schematic diagram of the flexible top cover structure according to an embodiment of the present invention;
[0055] Figure 8The simplified equivalent circuit diagram is provided for an embodiment of the present invention.
[0056] Figure 9 A process flow diagram of the preparation method provided in the embodiments of the present invention;
[0057] Figure 10 A schematic diagram of the packaging method provided in an embodiment of the present invention.
[0058] In the attached diagram: 1. Flexible substrate; 1-1. Through cavity; 1-2. Second isolation cavity; 1-3. Air flow channel; 2. Sensitive layer substrate; 2-1. First isolation cavity; 3. Pressure sensitive unit; 4. Temperature sensitive unit; 5. Electrode lead; 5-1. Ground electrode; 5-2. Measuring electrode; 6. Flexible top cover; 6-1. Flexible protrusion; 7. Sacrificial layer. Detailed Implementation
[0059] To make the objectives and technical solutions of this invention clearer and easier to understand, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. The specific embodiments described herein are for illustrative purposes only and are not intended to limit the invention.
[0060] In the description of this invention, it should be understood that the terms "center," "upper," "lower," "front," "rear," "left," "right," "vertical," "horizontal," "top," "bottom," "inner," and "outer," etc., indicate the orientation or positional relationship based on the orientation or positional relationship shown in the accompanying drawings. They are used only for the convenience of describing the invention and for simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the invention. Furthermore, the terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of that feature. In the description of this invention, unless otherwise stated, "a plurality of" means two or more.
[0061] See Figures 1-4This invention discloses an anti-cross-coupling temperature-pressure integrated sensing array, comprising a flexible substrate 1, a sensitive layer, and a flexible top cover 6 stacked sequentially. The flexible substrate 1 has multiple through-cavities 1-1 arranged in an array. The sensitive layer includes a sensitive layer substrate 2 disposed on one side of the flexible substrate 1, and sensitive units, electrode leads, and electrodes disposed on the surface of the sensitive layer substrate 2. Sensitive units are disposed at corresponding positions in each through-cavity 1-1 on the sensitive layer substrate 2. Each sensitive unit includes a pressure-sensitive unit 3 and a temperature-sensitive unit 4. The pressure-sensitive unit 3 is directly opposite the corresponding through-cavity 1-1, and the temperature-sensitive unit 4 is disposed on one side of the pressure-sensitive unit 3. A first isolation cavity 2-1 is provided on the sensitive layer substrate 2 between the pressure-sensitive unit 3 and the temperature-sensitive unit 4. An isolation cavity 2-1 extends through the thickness direction of the sensitive layer substrate 2. Due to the strain generated by the sensitive layer substrate 2 under pressure, the first isolation cavity 2-1 can effectively prevent the strain from being transmitted to the temperature sensitive unit 4. Secondly, the temperature sensitive unit 4 will experience a self-heating effect during measurement, and the first isolation cavity 2-1 can effectively prevent heat from diffusing to the pressure sensitive unit 3. Both the pressure sensitive unit 3 and the temperature sensitive unit 4 are connected to the electrode through the electrode lead 5. A second isolation cavity 1-2 is formed on the flexible substrate 1 at a position directly opposite to the first isolation cavity 2-1, and the second isolation cavity 1-2 extends through the thickness direction of the flexible substrate 1. The surface of the flexible top cover 6 has a protrusion at a position directly opposite to each pressure sensitive unit 3, thereby realizing the concentration of flexible pressure and improving sensitivity. In addition, the protrusion can be a flexible protrusion 6-1.
[0062] In a preferred embodiment of the present invention, the flexible substrate 1 is made of a PDMS / BN composite flexible material, wherein the PDMS / BN composite flexible material is prepared by mixing PDMS liquid, crosslinking agent and boron nitride particles in a mass ratio of (8-12):1:(0.5-2); the sensitive layer substrate 2 is made of a polyimide / boron nitride composite material, wherein the polyimide / boron nitride composite material is prepared by mixing boron nitride particles with a PI prepolymer solution, and the mass of the boron nitride particles is 5wt% to 30wt% of the PI prepolymer solution. This scheme effectively reduces the thermal conductivity of the flexible substrate 1 and the sensitive layer substrate 2 while maintaining flexibility, allowing the temperature-sensitive unit to quickly reach equilibrium with the external ambient temperature.
[0063] In a preferred embodiment of the present invention, an air channel 1-3 is provided on the surface of the flexible substrate 1 opposite to the sensitive layer substrate 2. Each through cavity 1-1 is correspondingly connected to an air channel 1-3. One end of the air channel 1-3 is connected to the through cavity 1-1, and the other end of the air channel 1-3 extends to the sidewall of the flexible substrate 1. By designing the air channel 1-3, the pressure inside and outside the through cavity 1-1 can be ensured to be the same, thus enabling accurate pressure measurement.
[0064] In a preferred embodiment of the present invention, both the first isolation cavity 2-1 and the second isolation cavity 1-2 are rectangular cavities, the cross-sections of the first isolation cavity 2-1 and the second isolation cavity 1-2 are the same, and the positions and shapes of the first isolation cavity 2-1 and the second isolation cavity 1-2 are consistent; in each sensitive unit, the line connecting the centers of the pressure sensitive unit 3 and the temperature sensitive unit 4 is perpendicular to the length direction of the first isolation cavity 2-1 and the length direction of the second isolation cavity 1-2.
[0065] As a preferred embodiment of the present invention, the pressure-sensitive unit 3 is made of strain-sensitive metals such as gold or Karma alloy, and the pressure-sensitive resistance value is 1.5-3kΩ.
[0066] In a preferred embodiment of the present invention, the through cavity 1-1 is circular in shape. The circular cavity design is beneficial to improving the pressure sensing sensitivity. See [link to previous section] Figures 5(b)-5(c) The pressure-sensitive unit 3 is shaped as at least one of sawtooth divergent, spiral, and / or zigzag. The distribution range of each pressure-sensitive unit 3 is located within the through cavity 1-1 directly opposite to the pressure-sensitive unit 3. Referring to Figure 5(a), the strain distribution results of the sensitive layer substrate 2 under the support of the circular cavity 1-1 are shown. The figure shows the radial and tangential strain curves along the radial direction. The radial strain curve is always greater than zero, while the tangential strain curve passes through a zero point at a certain position. The average radial strain is much greater than the average tangential strain. It can be seen that designing the pressure-sensitive unit 3 as a sawtooth divergent wire grid, which is only affected by radial strain, can effectively improve the sensitivity of pressure sensing.
[0067] As a preferred embodiment of the present invention, the temperature-sensitive unit 4 is made of temperature-sensitive metals such as platinum or copper, and the temperature-sensitive resistors are distributed at a certain distance from the pressure-sensitive unit to avoid significant mutual influence. The temperature-sensitive resistor value is 1-2kΩ.
[0068] In a preferred embodiment of the present invention, the electrode includes a ground electrode 5-1 and a measuring electrode 5-2; each pressure-sensitive unit 3 and each temperature-sensitive unit 4 has a measuring electrode 5-2 led out through an electrode lead; among the sensitive units located in the same column, all pressure-sensitive units 3 and temperature-sensitive units 4 share a ground electrode 5-1 and are connected to the ground electrode 5-1 through an electrode lead. This scheme significantly reduces the number of ground electrodes 5-1 used, thus reducing the number of leads by nearly half without increasing the manufacturing complexity.
[0069] This invention also proposes a method for fabricating a cross-coupling-resistant temperature-pressure integrated sensing array as described above, comprising the following steps:
[0070] S1. Prepare a sacrificial layer 7 on the front side of the silicon wafer;
[0071] S2. The sensitive layer substrate 2 is prepared on the sacrificial layer by spin coating;
[0072] S3. The pressure-sensitive unit 3 is patterned on the sensitive layer substrate 2 using a peeling process to form the pressure-sensitive unit 3;
[0073] S4. The temperature-sensitive unit 4 is patterned again on the sensitive layer substrate 2 using a peeling process to form the temperature-sensitive unit 4.
[0074] S5. The electrode and electrode leads are patterned again on the sensitive layer substrate 2 using a stripping process.
[0075] S6. The first isolation cavity 2-1 on the sensitive layer substrate 2 is prepared by inductively coupled plasma etching;
[0076] S7. The flexible substrate 1 and the flexible top cover 6 are prepared by machining a mold, which can be a polytetrafluoroethylene mold, and the molding process is used.
[0077] S8. The three parts of flexible substrate 1, sensitive layer substrate 2 and flexible top cover 6 are encapsulated using chemical bonding method.
[0078] Furthermore, the S2 process includes: spin-coating a polyimide / boron nitride (PI / BN) prepolymer solution, followed by solvent removal and imidization treatment using a stepped heating method to obtain a polyimide / boron nitride (PI / BN) composite flexible film.
[0079] Furthermore, the S7 process includes: machining a polytetrafluoroethylene mold using a CNC machining center, pouring in a PDMS / BN prepolymer solution, heating and curing it, and then demolding to obtain the structured PDMS / BN flexible substrate and flexible top cover.
[0080] The present invention also proposes a packaging method for a temperature-pressure integrated sensor array with anti-cross-coupling as described above, comprising the following steps:
[0081] The surface of the sensitive layer substrate 2 was chemically modified using an aqueous solution of 3-mercaptopropyltrimethoxysilane; the aqueous solution of 3-mercaptopropyltrimethoxysilane was prepared by mixing 3-mercaptopropyltrimethoxysilane and water at a volume ratio of (2-10):100.
[0082] The flexible substrate 1 and the chemically modified sensitive layer substrate 2 are then oxidized using oxygen plasma. The power of the oxygen plasma oxidation treatment is 40-80W and the time is 10-40s.
[0083] Then, make conformal contact between the flexible substrate 1 and the sensitive layer substrate 2 for 8-12 minutes to complete the bonding between the flexible substrate 1 and the sensitive layer substrate 2;
[0084] The surface of the sensitive layer substrate 2 in the overall structure where the flexible substrate 1 and the sensitive layer substrate 2 are bonded is then chemically modified using the 3-mercaptopropyltrimethoxysilane aqueous solution.
[0085] Then, oxygen plasma is used to oxidize the overall structure of the flexible top cover 6 and the flexible substrate 1 bonded to the sensitive layer substrate 2. The power of the oxygen plasma oxidation treatment is 40-80W and the time is 10-40s.
[0086] The flexible top cover 6 and the flexible substrate 1 are then bonded to the sensitive layer substrate 2 in a conformal contact for 8-12 minutes to complete the bonding between the flexible top cover 6 and the sensitive layer substrate 2, thus completing the packaging of the anti-cross-coupling temperature-pressure integrated sensing array.
[0087] Example
[0088] In this embodiment, the pressure-sensitive unit 3 is designed as a sawtooth-shaped filament grid, the overall resistance is designed as 1.5kΩ, and the electrodes are designed as rectangular structures of equal size to connect the electrode leads 5.
[0089] Reference Figure 6 The resistance bar of the temperature-sensitive unit 4 is designed in a zigzag shape, which effectively reduces the unit size and improves the integration. The overall resistance is designed to be 1.5kΩ. The resistance bar electrodes are designed in a rectangular structure of equal size to connect the electrode leads 5.
[0090] Reference Figure 7 The flexible top cover 6 is designed as a semi-circular protrusion at the center of the pressure-sensitive unit 3, thereby concentrating the flexible pressure and improving the sensitivity.
[0091] Reference Figure 8 The above is the equivalent circuit diagram of the flexible sensing array. Each column of sensitive units is led out by a ground electrode lead 5-1, and each sensitive unit is led out by a reference electrode lead 5-2. This can reduce the number of leads by half without increasing the difficulty of the process.
[0092] In this embodiment, the flexible substrate 1 is made of PDMS / BN composite flexible material, the sensitive layer substrate 2 is made of polyimide / boron nitride composite material, the flexible substrate 1 is provided with air flow channels 1-3, the first isolation cavity 2-1 and the second isolation cavity 1-2 are both rectangular cavities, the through cavity 1-1 is circular in shape, each pressure sensitive unit 3 and each temperature sensitive unit 4 is led out with a measuring electrode 5-2 through an electrode lead; among the sensitive units located in the same column, all pressure sensitive units 3 and temperature sensitive units 4 share a ground electrode 5-1 and are connected to the ground electrode 5-1 through an electrode lead.
[0093] Reference Figure 9 The fabrication method of the temperature-pressure integrated sensing array with anti-cross-coupling in this embodiment includes the following steps:
[0094] S1. Silicon wafer cleaning: A silicon oxide sacrificial layer 7 with a thickness of 500nm is prepared on the front side of the cleaned silicon wafer using a thermal oxidation process.
[0095] S2. A polyimide / boron nitride (PI / BN) prepolymer solution is spin-coated onto the silicon oxide sacrificial layer 7 at a low speed of 500 rpm and a high speed of 1500 rpm. The mass of the boron nitride particles in the polyimide / boron nitride (PI / BN) prepolymer solution is 10 wt% of the PI prepolymer solution. Then, it is placed on a hot plate and dried at 100°C for 2 h to remove the solvent in the polyimide / boron nitride (PI / BN) solution. It is then kept at 120°C for 2 h, at 180°C for 2 h, at 240°C for 2 h, and at 300°C for 3 h for imidization treatment to obtain a polyimide / boron nitride (PI / BN) flexible composite film with an overall thickness of 5 μm as the sensitive layer substrate 2.
[0096] S3. Using positive adhesive AZ4620, a uniform coating is applied to the flexible substrate 2, followed by photolithography and hardening. A 10nm monolayer thin film of metallic chromium is deposited by magnetron sputtering as an adhesion layer, followed by a 50nm monolayer thin film of gold. The film is then patterned into pressure-sensitive unit 3 through a lift-off process.
[0097] S4. Using positive adhesive AZ4620, a uniform coating is applied to the flexible substrate 2, followed by photolithography and hardening. A 20nm monolayer thin film of metallic titanium is deposited by magnetron sputtering as an adhesion layer, and then a 100nm monolayer thin film of platinum is deposited. The film is then patterned into temperature-sensitive unit 4 through a lift-off process.
[0098] S5. Using positive adhesive AZ4620, a uniform coating is applied to the flexible substrate 2, followed by photolithography and hardening. A 20nm monolayer thin film of metallic chromium is deposited by magnetron sputtering as an adhesion layer, followed by a 300nm monolayer thin film of gold. The film is then patterned into electrode leads 5 through a lift-off process.
[0099] S6. An aluminum Al mask was prepared by lift-off process, and then etched by inductively coupled plasma with parameters of oxygen 80ccm, argon 10ccm and etching time of 30min to pattern the sensitive layer substrate 2.
[0100] S7. Use a CNC machining center to process the polytetrafluoroethylene mold. Mix PDMS liquid / crosslinking agent / boron nitride particles thoroughly in a mass ratio of 9:1:0.5. After vacuum degassing for 1 hour, pour the mixture into the polytetrafluoroethylene mold and heat it at 100℃ for 1.5 hours to cure. The resulting PDMS / BN substrate 1 and top cover 6 have a thickness of 400-600μm, a circular cavity 1-1 with a diameter of 3mm, an air channel 1-3 with a width of 500μm and a depth of 250μm, and a PDMS / BN top cover 6 with a thickness of 100-300μm and a hemispherical protrusion with a diameter of 500μm.
[0101] S8. Etch away the sacrificial silicon oxide 7 in BOE solution, pick up the released structure, and chemically bond it with the PDMS / BN top cap 6 and the PDMS / BN substrate 1. Then, align and encapsulate it under a light microscope to complete the fabrication of the flexible temperature-pressure integrated pressure sensing array.
[0102] refer to Figure 10 This diagram illustrates the chemical bonding encapsulation method. First, a flexible polyimide / boron nitride (PI / BN) composite material is contacted with an aqueous solution of 3-mercaptopropyltrimethoxysilane (volume ratio 1:100) for 2 seconds, then removed. Next, it is fully reacted in distilled water, where a hydrolysis reaction occurs at one end of the 3-mercaptopropyltrimethoxysilane to generate molecular crosslinks, and a nucleophilic reaction occurs at the other end to bond with the substrate and the polyimide / boron nitride (PI / BN). Second, the flexible substrate 1 and the sensitive layer substrate 2 are jointly oxidized using an oxygen plasma generator with parameters of 60W power and 20 seconds. Finally, after conformal contact between the flexible substrate 1 and the sensitive layer substrate 2 for 10 minutes, strong siloxane bonds are formed, completing the bonding between the flexible substrate 1 and the sensitive layer substrate 2. The entire structure bonded to the flexible substrate 1 and the sensitive layer substrate 2 was then contacted with an aqueous solution of 3-mercaptopropyltrimethoxysilane (volume ratio 1:100) for 2 seconds, then removed. Next, it was allowed to react fully in distilled water. Hydrolysis occurred at one end of the 3-mercaptopropyltrimethoxysilane, resulting in molecular cross-linking, while at the other end, a nucleophilic reaction occurred with the substrate, bonding with polyimide / boron nitride (PI / BN). The entire structure bonded to the flexible substrate 1 and the sensitive layer substrate 2, along with the flexible top cover 6, underwent oxidation treatment using an oxygen plasma generator with parameters of 60W power and 20 seconds. Finally, after conformal contact of the entire structure bonded to the flexible substrate 1 and the sensitive layer substrate 2, along with the flexible top cover 6, for 10 minutes, strong siloxane bonds were formed, completing the overall encapsulation.
[0103] The main technical specifications of the anti-cross-coupling temperature-pressure integrated sensor array fabricated in this embodiment are as follows:
[0104] 1. Pressure measurement range: 0-500 kPa;
[0105] 2. Response time: less than 20ms;
[0106] 3. Durability: Over 40,000 cycles of loading;
[0107] 4. Temperature measurement range: 0-150℃;
[0108] 5. Temperature measurement accuracy: ±1℃;
[0109] As can be seen, the temperature-pressure integrated sensing array of the present invention, which is resistant to cross-coupling, has the ability to integrate and sense temperature and pressure with low coupling, and has the characteristics of good response time, durability, stability and repeatability.
[0110] The above description is only one embodiment of the present invention, and not all or the only embodiment. Any equivalent modifications made by those skilled in the art to the technical solution of the present invention after reading the present invention specification shall be covered by the claims of the present invention.
Claims
1. A temperature-pressure integrated sensing array with anti-cross-coupling properties, characterized in that, It includes a flexible substrate (1), a sensitive layer and a flexible top cover (6) stacked in sequence. Multiple through cavities (1-1) are arranged in an array on the flexible substrate (1). The sensitive layer includes a sensitive layer substrate (2) disposed on one side surface of a flexible substrate (1) and a sensitive unit, an electrode lead and an electrode disposed on the surface of the sensitive layer substrate (2). The sensitive unit is provided on the sensitive layer substrate (2) at a corresponding position in each through cavity (1-1). Each sensitive unit includes a pressure sensitive unit (3) and a temperature sensitive unit (4). The pressure sensitive unit (3) is directly opposite the through cavity (1-1) corresponding to the sensitive unit. The temperature sensitive unit (4) is disposed on one side of the pressure sensitive unit (3). A first isolation cavity (2-1) is provided on the sensitive layer substrate (2) between the pressure sensitive unit (3) and the temperature sensitive unit (4). The first isolation cavity (2-1) penetrates the thickness direction of the sensitive layer substrate (2). Both the pressure-sensitive unit (3) and the temperature-sensitive unit (4) are connected to the electrode via electrode leads (5); A second isolation cavity (1-2) is provided on the flexible substrate (1) at a position directly opposite to the first isolation cavity (2-1), and the second isolation cavity (1-2) extends through the thickness direction of the flexible substrate (1); The surface of the flexible top cover (6) has protrusions at the position directly opposite each pressure-sensitive unit (3); The flexible substrate (1) is made of PDMS / BN composite flexible material, wherein the PDMS / BN composite flexible material is made by mixing PDMS liquid, crosslinking agent and boron nitride particles in a mass ratio of (8-12):1:(0.5~2); The sensitive layer substrate (2) is made of polyimide / boron nitride composite material, wherein the polyimide / boron nitride composite material is made by mixing boron nitride particles with PI prepolymer solution, and the mass of boron nitride particles is 5wt%~30wt% of PI prepolymer solution.
2. The temperature-pressure integrated sensing array with anti-cross-coupling as described in claim 1, characterized in that, An air channel (1-3) is provided on the side surface of the flexible substrate (1) opposite to the sensitive layer substrate (2). Each through cavity (1-1) is connected to an air channel (1-3). One end of the air channel (1-3) is connected to the through cavity (1-1), and the other end of the air channel (1-3) extends to the side wall of the flexible substrate (1).
3. The temperature-pressure integrated sensing array with anti-cross-coupling as described in claim 1, characterized in that, Both the first isolation cavity (2-1) and the second isolation cavity (1-2) are rectangular cavities, and the cross-sections of the first isolation cavity (2-1) and the second isolation cavity (1-2) are the same; In each sensitive unit, the line connecting the centers of the pressure sensitive unit (3) and the temperature sensitive unit (4) is perpendicular to the length direction of the first isolation cavity (2-1) and the length direction of the second isolation cavity (1-2).
4. The temperature-pressure integrated sensing array with anti-cross-coupling according to claim 1, characterized in that, The pressure-sensitive unit (3) is made of strain-sensitive metal and has a pressure-sensitive resistance value of 1.5-3kΩ.
5. A temperature-pressure integrated sensing array with anti-cross-coupling as described in claim 1 or 4, characterized in that, The through cavity (1-1) is circular in shape, and the pressure-sensitive unit (3) is shaped in at least one of the following: serrated, spiral, or zigzag. The distribution range of each pressure-sensitive unit (3) is located within the range of the through cavity (1-1) directly opposite the pressure-sensitive unit (3).
6. The temperature-pressure integrated sensing array with anti-cross-coupling according to claim 1, characterized in that, The temperature-sensitive unit (4) is made of a temperature-sensitive metal with a temperature-sensitive resistance value of 1-2kΩ.
7. The temperature-pressure integrated sensing array with anti-cross-coupling according to claim 1, characterized in that, The electrodes include a ground electrode (5-1) and a measuring electrode (5-2); Each pressure-sensitive unit (3) and each temperature-sensitive unit (4) has a measuring electrode (5-2) led out through an electrode lead. In the sensitive units located in the same column, all pressure sensitive units (3) and temperature sensitive units (4) share a ground electrode (5-1) and are connected to the ground electrode (5-1) through electrode leads.
8. The method for fabricating the anti-cross-coupling temperature-pressure integrated sensing array according to any one of claims 1-7, characterized in that, Includes the following steps: S1. Prepare a sacrificial layer (7) on the front side of the silicon wafer. S2. The sensitive layer substrate is prepared on the sacrificial layer by spin coating (2). S3. The pressure-sensitive unit (3) is patterned on the sensitive layer substrate (2) by a peeling process to form the pressure-sensitive unit (3). S4. The temperature-sensitive unit (4) is patterned again on the sensitive layer substrate (2) by peeling process to form the temperature-sensitive unit (4). S5. The electrode and electrode leads are patterned again on the sensitive layer substrate (2) using a stripping process. S6. The first isolation cavity (2-1) on the sensitive layer substrate (2) is prepared by inductively coupled plasma etching. S7. The flexible substrate (1) and the flexible top cover (6) are prepared by using a molding process; S8. The three parts of the flexible substrate (1), sensitive layer substrate (2) and flexible top cover (6) are encapsulated by chemical bonding method.
9. The packaging method for the anti-cross-coupling temperature-pressure integrated sensing array according to any one of claims 1-7, characterized in that, The process includes the following: The surface of the sensitive layer substrate (2) was chemically modified using an aqueous solution of 3-mercaptopropyltrimethoxysilane; the aqueous solution of 3-mercaptopropyltrimethoxysilane was prepared by mixing 3-mercaptopropyltrimethoxysilane and water in a volume ratio of (2~10):
100. The flexible substrate (1) and the chemically modified sensitive layer substrate (2) are then oxidized using oxygen plasma. The power of the oxygen plasma oxidation treatment is 40-80W and the time is 10-40s. Then, the flexible substrate (1) and the sensitive layer substrate (2) are made into conformal contact for 8-12 minutes to complete the bonding between the flexible substrate (1) and the sensitive layer substrate (2); The surface of the sensitive layer substrate (2) in the overall structure of the flexible substrate (1) and the sensitive layer substrate (2) bonded together is then chemically modified using the aqueous solution of 3-mercaptopropyltrimethoxysilane. Then, oxygen plasma is used to oxidize the overall structure of the flexible top cover (6) and the flexible substrate (1) bonded to the sensitive layer substrate (2). The power of the oxygen plasma oxidation treatment is 40-80W and the time is 10-40s. The flexible top cover (6) and the flexible substrate (1) are then bonded to the sensitive layer substrate (2) in a conformal contact for 8-12 minutes to complete the bonding between the flexible top cover (6) and the sensitive layer substrate (2), thus completing the packaging of the anti-cross-coupling temperature-pressure integrated sensing array.