A crushing device for processing microelectronic raw materials
By using magnetic grinding balls and retractable adsorption mechanisms in the crushing device, the problem of difficult separation between steel balls and materials in existing ball mills is solved, and the magnetic grinding balls and powders after crushing microelectronic raw materials is realized, which improves the equipment Operational ease and efficiency.
Patent Information
- Application Number
- CN202410772116.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-16
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-06-16
AI Technical Summary
After the existing ball mill is grinding, it is difficult to separate the steel ball from the material, and additional treatment is required, which affects the efficiency.
A crushing device for processing microelectronic raw materials is designed, using magnetic grinding balls and retractable adsorption mechanisms. The magnetic grinding balls are adsorbed and separated by electromagnets and electric push rods, and the magnetic grinding balls are realized by using an annular push plate and filter cartridge. Separation and discharge of powder.
After the microelectronic raw materials are crushed, the magnetic grinding balls and powder are effectively separated, which simplifies the subsequent processing process and improves the operation convenience and efficiency of the equipment.
Smart Images

Figure CN118437467B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of pulverizing equipment, in particular to a pulverizing device for processing microelectronic raw materials. Background Art
[0002] With the continuous development of electronic technology, the speed of electronic products being updated is getting faster and faster. Many old electronic products are discarded, which contain a large number of circuit boards. These circuit boards often contain a large number of valuable metal elements, such as gold, silver, copper, etc. If they are not recycled, they will cause waste and damage to the earth's resources. Through recycling, not only can resources be utilized to the greatest extent, but also pollution to the natural environment can be reduced. In order to better recycle useful materials in discarded circuit boards and reduce pollution, circuit boards are often crushed into powder, and then separated and extracted using physical and chemical methods.
[0003] At present, a ball mill is often used to process waste circuit boards into powder. The existing ball mill is to load a certain number of steel balls into its cylinder as grinding media. When the cylinder of the ball mill rotates, the steel balls are attached to the cylinder lining due to inertia and centrifugal force and are carried away by the cylinder. When they are brought to a certain height, they are thrown down due to their own gravity. The falling steel balls crush the materials in the cylinder like projectiles. However, when the existing ball mill is discharged after grinding, the steel balls will also be discharged. It is necessary to separate the steel balls from the materials and then reintroduce the steel balls into the cylinder, which is inconvenient. To this end, a crushing device for processing microelectronic raw materials is proposed. Summary of the invention
[0004] The object of the present invention is to provide a pulverizing device for processing microelectronic raw materials to solve the problems raised in the above-mentioned background technology.
[0005] To achieve the above-mentioned object, the present invention provides the following technical solutions: a pulverizing device for processing microelectronic raw materials, comprising a frame and a tank body rotatably mounted on the frame, the tank body comprising a pulverizing area and a control area, the diameter of the control area is smaller than the diameter of the pulverizing area, a feeding channel is arranged on the surface of the pulverizing area, a plurality of magnetic grinding balls are arranged inside the pulverizing area, a retractable adsorption mechanism is arranged in the control area, and the adsorption mechanism can be moved from the control area into the pulverizing area;
[0006] The adsorption mechanism includes an electric push rod, an electromagnet, a filter cartridge, an annular push plate and a side plate. The side plates are provided in two groups and are located at both ends of the electromagnet, and the diameter of the side plates is equal to the inner diameter of the control area. The filter cartridge is fixedly installed on one side of the electromagnet. The filter cartridge and the electromagnet are both cylindrical and coaxially arranged. The fixed end of the electric push rod is installed on the inner surface of the control area, and the telescopic end of the electric push rod is fixedly connected to the side plate. One side of the filter cartridge is set as an opening, and the annular push plate is sleeved on the surface of the electromagnet. The annular push plate can be close to or away from the opening of the filter cartridge.
[0007] Preferably, a connecting rod is fixedly connected between the two groups of side plates, the annular push plate is fixedly connected to the limiting plate, the connecting rod passes through the limiting plate and slides with it, a first spring is sleeved on the surface of the connecting rod, one end of the first spring is fixedly connected to the limiting plate, and the other end of the first spring is fixedly connected to the side plate, and a control mechanism is provided on the surface of the side plate, which can form motion interference with the limiting plate, so that the limiting plate is kept away from the filter cartridge and the first spring is in an elastic force storage state.
[0008] Preferably, the control mechanism includes a first air cavity, an air pipe and a piston member. The first air cavity is opened inside the side plate close to the crushing zone. The plate member of the piston member is installed in the first air cavity. The rod portion of the piston member is located outside the side plate. One end of the air pipe is through-connected with the first air cavity. The other end of the air pipe is through-connected with a cylinder. A piston plate is installed in the cylinder. A round rod is fixedly connected to the surface of the piston plate. A second spring is sleeved on the surface of the round rod. One end of the round rod passes through the cylinder and is fixedly connected to a wedge-shaped stopper. The wedge-shaped stopper can form motion interference with the annular push plate.
[0009] Preferably, a baffle is fixedly connected to the inner surface of the control area, and the baffle is located in the moving direction of the limit plate. When the adsorption mechanism moves back from the crushing area to the inside of the control area, the baffle forms a motion interference with the limit plate and the annular push plate, and the annular push plate and the inclined surface of the wedge-shaped stopper form a relative movement, so that the wedge-shaped stopper moves to the outside of the annular push plate.
[0010] Preferably, the first air cavity is connected to the second air cavity through a connecting tube, two groups of movable plates are arranged inside the second air cavity, the movable plates are sealingly and slidably connected inside the second air cavity, the opposite sides of the two groups of movable plates are fixedly connected with electrode sheets, and the opposite sides of the two groups of movable plates are fixedly connected to the inner surface of the second air cavity through a third spring.
[0011] Preferably, the two groups of electrode sheets are connected in series with the electromagnet via a wire, and the electromagnet is cut off from power by controlling the two groups of electrode sheets to separate.
[0012] Preferably, when the adsorption mechanism moves from the control area to the crushing area, the inner wall of the crushing area forms a motion interference with the piston, so that the piston moves in the first air cavity, and the gas in the first air cavity is transported to the inside of the cylinder and the second air cavity through the air pipe.
[0013] Preferably, a connecting channel is provided outside the crushing zone and the control zone, and a connecting port between the crushing zone and the connecting channel is lower than a connecting port between the control zone and the connecting channel.
[0014] Preferably, solenoid valve bodies are provided inside the connecting channel and the material conveying channel for controlling the opening and closing of the connecting channel and the material conveying channel.
[0015] Preferably, it also includes a driving mechanism, which includes a motor arranged on a frame, a driving wheel is fixedly mounted on the power end of the motor and the surface of the tank body, and two groups of the driving wheel surfaces are sleeved with conveyor belts.
[0016] Compared with the prior art, the present invention has the following beneficial effects:
[0017] The present invention provides an adsorption mechanism. After the microelectronic raw materials are crushed, the electric push rod can be driven to extend, driving the electromagnet and the filter cartridge to move to the crushing area. The electromagnet can adsorb the magnetic grinding balls to separate the magnetic grinding balls from the microelectronic raw materials, making it convenient for the microelectronic raw materials to be discharged separately.
[0018] The present invention can push the magnetic grinding balls into the filter cartridge by arranging an annular push plate, and the annular push plate can cover the opening of the filter cartridge. At this time, the power supply of the electromagnet can be cut off, and the magnetic grinding balls can fall into the filter cartridge. When the driving mechanism drives the tank body to rotate as a whole, the magnetic grinding balls can roll freely inside the filter cartridge, and the magnetic grinding balls collide with each other, and the microelectronic raw material powder attached to the surface of the magnetic grinding balls can be shaken off. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a schematic diagram of the overall structure of the present invention;
[0020] Figure 2 is a cross-sectional view of the present invention;
[0021] Figure 3 For the present invention Figure 2 Schematic diagram of the structure of the part;
[0022] Figure 4 A partial cross-sectional view from another angle of the present invention;
[0023] Figure 5 For the present invention Figure 3 The enlarged view of point A in the middle;
[0024] Figure 6 For the present invention Figure 3 The enlarged view of point B in the middle;
[0025] Figure 7 For the present invention Figure 4 Enlarged view of point C in the middle.
[0026] In the accompanying drawings, the list of components represented by each reference numeral is as follows: 1. frame; 2. tank body; 21. crushing area; 22. control area; 23. connecting channel; 24. feeding channel; 3. driving mechanism; 31. transmission wheel; 32. conveyor belt; 33. motor; 4. adsorption mechanism; 41. electric push rod; 42. electromagnet; 43. filter cartridge; 44. annular push plate; 45. side plate; 46. baffle; 47. first spring; 48. connecting rod; 49. limit plate; 5. control mechanism; 51. first air cavity; 52. air pipe; 53. piston member; 54. cylinder body; 55. piston plate; 56. round rod; 57. second spring; 58. wedge-shaped stopper; 6. connecting pipe; 7. second air cavity; 8. movable plate; 9. electrode sheet; 10. third spring. DETAILED DESCRIPTION
[0027] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0028] See also Figure 1-Figure 4 , a pulverizing device for processing microelectronic raw materials is shown in the figure, comprising a frame 1 and a tank body 2 rotatably mounted on the frame 1, the tank body 2 comprising a pulverizing area 21 and a control area 22, the diameter of the control area 22 is smaller than the diameter of the pulverizing area 21, a feeding channel 24 is arranged on the surface of the pulverizing area 21, a plurality of magnetic grinding balls are arranged inside the pulverizing area 21, a retractable adsorption mechanism 4 is arranged in the control area 22, and the adsorption mechanism 4 can be moved from the control area 22 into the pulverizing area 21;
[0029] The adsorption mechanism 4 includes an electric push rod 41, an electromagnet 42, a filter cartridge 43, an annular push plate 44 and a side plate 45. Two groups of side plates 45 are provided and are located at both ends of the electromagnet 42, and the diameter of the side plate 45 is equal to the inner diameter of the control area 22. The filter cartridge 43 is fixedly installed on one side of the electromagnet 42. The filter cartridge 43 and the electromagnet 42 are both arranged in a cylindrical shape and are coaxially arranged. The fixed end of the electric push rod 41 is installed on the inner surface of the control area 22, and the telescopic end of the electric push rod 41 is fixedly connected to the side plate 45. One side of the filter cartridge 43 is arranged as an opening, and the annular push plate 44 is sleeved on the surface of the electromagnet 42. The annular push plate 44 can be close to or away from the opening of the filter cartridge 43.
[0030] Furthermore, it also includes a driving mechanism 3, which includes a motor 33 arranged on the frame 1, and transmission wheels 31 are fixedly installed on the power end of the motor 33 and the surface of the tank body 2, and conveyor belts 32 are sleeved on the surfaces of two sets of transmission wheels 31.
[0031] In this embodiment, when the microelectronic raw material is crushed, the adsorption mechanism 4 is located inside the control area 22, and the side plate 45 in the adsorption mechanism 4 is equal to the inner diameter of the control area 22. The side plate 45 can effectively isolate the crushing area 21 and the control area 22 to prevent the microelectronic raw material from entering the control area 22 during crushing. After the microelectronic raw material is crushed, the electric push rod 41 is driven to extend, driving the electromagnet 42 and the filter cartridge 43 to move to the crushing area 21, and the electromagnet 42 can adsorb the magnetic grinding balls to separate the magnetic grinding balls from the microelectronic raw material. In addition, the annular push plate 44 can push the magnetic grinding balls to separate the magnetic grinding balls from the microelectronic raw material. The balls are moved to allow the magnetic grinding balls to enter the filter cartridge 43, and the annular push plate 44 can cover the opening of the filter cartridge 43. At this time, the power supply of the electromagnet 42 can be cut off, and the magnetic grinding balls can fall into the filter cartridge 43. When the driving mechanism 3 drives the tank body 2 to rotate as a whole, the magnetic grinding balls can roll freely inside the filter cartridge 43, and the magnetic grinding balls collide with each other, and the microelectronic raw material powder attached to the surface of the magnetic grinding balls can be shaken off and fall into the bottom of the crushing area 21 through the filter holes on the surface of the filter cartridge 43, and then all the microelectronic raw material powder can be discharged through the feed channel 24.
[0032] See also Figure 3-Figure 7 A connecting rod 48 is fixedly connected between the two groups of side plates 45, the annular push plate 44 is fixedly connected to the limit plate 49, the connecting rod 48 passes through the limit plate 49 and slides with it, a first spring 47 is sleeved on the surface of the connecting rod 48, one end of the first spring 47 is fixedly connected to the limit plate 49, and the other end of the first spring 47 is fixedly connected to the side plate 45, and a control mechanism 5 is provided on the surface of the side plate 45, the control mechanism 5 can form motion interference with the limit plate 49, so that the limit plate 49 is kept away from the filter cartridge 43, so that the first spring 47 is in an elastic force storage state.
[0033] Furthermore, the control mechanism 5 includes a first air cavity 51, an air pipe 52 and a piston member 53. The first air cavity 51 is opened inside the side plate 45 close to the crushing area 21. The plate of the piston member 53 is installed in the first air cavity 51. The rod of the piston member 53 is located outside the side plate 45. One end of the air pipe 52 is connected to the first air cavity 51. The other end of the air pipe 52 is connected to the cylinder 54. The piston plate 55 is installed inside the cylinder 54. A round rod 56 is fixedly connected to the surface of the piston plate 55. A second spring 57 is sleeved on the surface of the round rod 56. One end of the round rod 56 passes through the cylinder 54 and is fixedly connected to a wedge-shaped stopper 58. The wedge-shaped stopper 58 can form motion interference with the annular push plate 44.
[0034] Furthermore, when the adsorption mechanism 4 moves from the control area 22 to the crushing area 21, the inner wall of the crushing area 21 forms a motion interference on the piston 53, so that the piston 53 moves in the first air cavity 51, and the gas in the first air cavity 51 is transported to the inside of the cylinder 54 and the second air cavity 7 through the air pipe 52.
[0035] Furthermore, the first air cavity 51 is connected to the second air cavity 7 through a connecting tube 6, and two groups of movable plates 8 are arranged inside the second air cavity 7. The movable plates 8 are sealingly and slidably connected inside the second air cavity 7, and the opposite sides of the two groups of movable plates 8 are fixedly connected with electrode sheets 9, and the opposite sides of the two groups of movable plates 8 are fixedly connected to the inner surface of the second air cavity 7 through a third spring 10.
[0036] Furthermore, the two groups of electrode sheets 9 are connected in series with the electromagnet 42 through a wire, and the electromagnet 42 is cut off from power by controlling the two groups of electrode sheets 9 to separate.
[0037] In this embodiment, the movement and reset of the annular push plate 44 are achieved by the cooperation of the first spring 47, the control mechanism 5, the limit plate 49 and the wedge-shaped stopper 58. In the initial state, the wedge-shaped stopper 58 abuts against the surface of the annular push plate 44, forming a moving interference with the annular push plate 44. At this time, the first spring 47 is in an extended state; in the process of the electric push rod 41 driving the adsorption mechanism 4 to move from the control area 22 to the crushing area 21, the state of the annular push plate 44 is stationary in the early stage, and moves toward the side of the filter cartridge 43 in the later stage. Specifically, before the piston member 53 contacts the side wall of the crushing area 21, the wedge-shaped stopper 58 abuts against the surface of the annular push plate 44, forming a moving interference with the annular push plate 44, and the annular push plate 44 remains stationary. During this process, the electromagnet 42 is energized to adsorb the magnetic grinding balls; after the piston member 53 contacts the side wall of the crushing area 21, it is blocked by the side wall of the crushing area 21 and pushes The movable piston member 53 moves, and the plate member of the piston member 53 squeezes the gas in the first air chamber 51, so that the gas enters the cylinder 54 through the air pipe 52, pushing the piston plate 55 in the cylinder 54 to move, thereby driving the round rod 56 and the wedge-shaped stopper 58 to move. At this time, the second spring 57 is extended, and the wedge-shaped stopper 58 is away from the annular push plate 44, and no longer forms a motion interference with the annular push plate 44. Therefore, the extended first spring 47 is contracted, driving the annular push plate 44 to move toward the side of the filter cartridge 43, and the annular push plate 44 can push the magnetic grinding ball attached to the electromagnet 42 to move it into the filter cartridge 43; in addition, the piston member 53 can also squeeze the gas in the first air chamber 51 into the second air chamber 7, so that the two groups of movable plates 8 are away from each other, thereby driving the two groups of electrode sheets 9 to separate, disconnecting the power supply of the electromagnet 42, and allowing the magnetic grinding ball to move freely inside the filter cartridge 43.
[0038] Furthermore, a baffle 46 is fixedly connected to the inner surface of the control area 22, and the baffle 46 is located in the moving direction of the limit plate 49. When the adsorption mechanism 4 moves back from the crushing area 21 to the inside of the control area 22, the baffle 46 forms a motion interference with the limit plate 49 and the annular push plate 44, and the annular push plate 44 and the inclined surface of the wedge-shaped stopper 58 form a relative movement, so that the wedge-shaped stopper 58 moves to the outside of the annular push plate 44. In this embodiment, when the adsorption mechanism 4 moves back from the crushing area 21 to the inside of the control area 22, the baffle plate 46 will form a motion interference with the annular push plate 44, and make the annular push plate 44 and the wedge-shaped stopper 58 move back to the initial position, so that the wedge-shaped stopper 58 will again form a motion interference with the annular push plate 44. Specifically, when the annular push plate 44 moves relatively along the inclined surface of the wedge-shaped stopper 58, the wedge-shaped stopper 58 will move to the outside of the annular push plate 44, and the round rod 56 and the piston plate 55 will move accordingly, and the second spring 57 will be stretched. When the annular push plate 44 moves to the initial position, the stretched second spring 57 is reset, driving the piston plate 55, the round rod 56 and the wedge-shaped stopper 58 to move to the initial position, so that the wedge-shaped stopper 58 can continue to form a motion interference with the annular push plate 44. In addition, when the adsorption mechanism 4 moves back from the crushing area 21 to the control area 22, the annular push plate 44 is blocked by the baffle 46, so that the annular push plate 44 and the filter cartridge 43 move relative to each other, and the annular push plate 44 is moved away from the filter cartridge 43, so that the magnetic grinding balls inside the filter cartridge 43 can roll back into the tank body 2.
[0039] Furthermore, a connecting passage 23 is provided outside the crushing zone 21 and the control zone 22 , and a connecting port between the crushing zone 21 and the connecting passage 23 is lower than a connecting port between the control zone 22 and the connecting passage 23 .
[0040] Furthermore, electromagnetic valve bodies are disposed inside the connecting channel 23 and the material conveying channel 24 to control the connection and disconnection of the connecting channel 23 and the material conveying channel 24 .
[0041] In this embodiment, during actual use, some magnetic grinding balls will roll down into the control area 22, and the magnetic grinding balls that fall into the control area 22 can fall into the crushing area 21 through the connecting channel 23; the feed channel 24 is used to input or discharge microelectronic raw materials. When inputting raw materials, the drive mechanism 3 is used to rotate the feed channel 24 upward, and when discharging raw materials, the drive mechanism 3 is used to rotate the feed channel 24 downward.
[0042] The solenoid valve body in this embodiment can be used with any existing model to meet the on-off control of the connecting channel 23 and the feeding channel 24; at the same time, a button can be set on the outer surface of the tank body 2, and a battery assembly can be set on the tank body 2 or any other part to provide corresponding power for the solenoid valve body, and pressing the button can control the switch of the solenoid valve body.
[0043] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0044] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A pulverizing device for processing microelectronic raw materials, comprising a frame (1) and a tank (2) rotatably mounted on the frame (1), characterized in that: The tank body (2) comprises a crushing zone (21) and a control zone (22); a material conveying channel (24) is arranged on the surface of the crushing zone (21); the diameter of the control zone (22) is smaller than the diameter of the crushing zone (21); a plurality of magnetic grinding balls are arranged inside the crushing zone (21); a retractable adsorption mechanism (4) is arranged inside the control zone (22); and the adsorption mechanism (4) can be moved from the control zone (22) into the crushing zone (21); The adsorption mechanism (4) comprises an electric push rod (41), an electromagnet (42), a filter cartridge (43), an annular push plate (44) and a side plate (45); two sets of the side plates (45) are provided and are located at both ends of the electromagnet (42); the diameter of the side plates (45) is equal to the inner diameter of the control area (22); the filter cartridge (43) is fixedly mounted on one side of the electromagnet (42); the filter cartridge (43) and the electromagnet (42) are both cylindrical and coaxially arranged; the fixed end of the electric push rod (41) is mounted on the inner surface of the control area (22); the telescopic end of the electric push rod (41) is fixedly connected to the side plate (45); one side of the filter cartridge (43) is provided with an opening; the annular push plate (44) is sleeved on the surface of the electromagnet (42); the annular push plate (44) can be close to or away from the opening of the filter cartridge (43); A connecting rod (48) is fixedly connected between the two groups of side plates (45); the annular push plate (44) is fixedly connected to the limiting plate (49); the connecting rod (48) penetrates the limiting plate (49) and slidably cooperates therewith; a first spring (47) is sleeved on the surface of the connecting rod (48); one end of the first spring (47) is fixedly connected to the limiting plate (49); the other end of the first spring (47) is fixedly connected to the side plate (45); a control mechanism (5) is provided on the surface of the side plate (45); the control mechanism (5) can form motion interference with the limiting plate (49), so that the limiting plate (49) is kept away from the filter cartridge (43), and the first spring (47) is in an elastic force storage state; The control mechanism (5) comprises a first air cavity (51), an air pipe (52) and a piston member (53). The first air cavity (51) is provided inside the side plate (45) close to the crushing zone (21). The plate member of the piston member (53) is mounted in cooperation with the inside of the first air cavity (51). The rod portion of the piston member (53) is located outside the side plate (45). One end of the air pipe (52) is connected to the first air cavity (51). The other end of the air pipe (52) is connected to the cylinder (54). A piston plate (55) is mounted in cooperation with the inside of the cylinder (54). A round rod (56) is fixedly connected to the surface of the piston plate (55). A second spring (57) is sleeved on the surface of the round rod (56). One end of the round rod (56) passes through the cylinder (54) and is fixedly connected to a wedge-shaped stopper (58). The wedge-shaped stopper (58) can form motion interference with the annular push plate (44).
2. A pulverizing device for processing microelectronic raw materials according to claim 1, characterized in that: A baffle (46) is fixedly connected to the inner surface of the control zone (22), and the baffle (46) is located in the moving direction of the limit plate (49). When the adsorption mechanism (4) moves back from the crushing zone (21) to the inside of the control zone (22), the baffle (46) forms a motion interference with the limit plate (49) and the annular push plate (44), and the annular push plate (44) and the inclined surface of the wedge-shaped stopper (58) form a relative movement, so that the wedge-shaped stopper (58) moves to the outside of the annular push plate (44).
3. A pulverizing device for processing microelectronic raw materials according to claim 2, characterized in that: The first air cavity (51) is connected to the second air cavity (7) via a connecting tube (6); two groups of movable plates (8) are arranged inside the second air cavity (7); the movable plates (8) are sealingly and slidably connected inside the second air cavity (7); electrode plates (9) are fixedly connected to opposite sides of the two groups of movable plates (8); and opposite sides of the two groups of movable plates (8) are fixedly connected to the inner surface of the second air cavity (7) via a third spring (10).
4. A pulverizing device for processing microelectronic raw materials according to claim 3, characterized in that: The two groups of electrode sheets (9) are connected in series with the electromagnet (42) via a wire, and the electromagnet (42) is cut off from power by controlling the two groups of electrode sheets (9) to separate.
5. A pulverizing device for processing microelectronic raw materials according to claim 4, characterized in that: When the adsorption mechanism (4) moves from the control area (22) to the crushing area (21), the inner wall of the crushing area (21) forms a motion interference with the piston member (53), so that the piston member (53) moves in the first air cavity (51), and the gas in the first air cavity (51) is transported to the inside of the cylinder (54) and the second air cavity (7) through the air pipe (52).
6. The pulverizing device for processing microelectronic raw materials according to claim 1, characterized in that: The crushing zone (21) and the control zone (22) are provided with a connecting channel (23) in communication with each other outside, and the connecting port of the crushing zone (21) and the connecting channel (23) is lower than the connecting port of the control zone (22) and the connecting channel (23).
7. A pulverizing device for processing microelectronic raw materials according to claim 6, characterized in that: The connecting channel (23) and the material conveying channel (24) are both provided with electromagnetic valve bodies for controlling the opening and closing of the connecting channel (23) and the material conveying channel (24).
8. The pulverizing device for processing microelectronic raw materials according to claim 1, characterized in that: The machine also comprises a driving mechanism (3), the driving mechanism (3) comprising a motor (33) arranged on the frame (1), a driving wheel (31) being fixedly mounted on the power end of the motor (33) and the surface of the tank body (2), and two sets of the driving wheels (31) being sleeved with conveyor belts (32) on their surfaces.
Citation Information
Patent Citations
Ball mill with filter screen
CN209287434U
Vertical mill for processing neodymium-iron-boron magnetic material
CN210906498U
Silicon crystal sufficient crusher
CN219129499U