A coating device for producing stainless steel wire
By designing a combination of straightening and coating components, the problem of uneven coating of coarse stainless steel wire was solved, and the uniformity and efficiency of coating were improved.
Patent Information
- Application Number
- CN202411173727.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2025-01-07
- Estimated Expiration
- 2044-08-26
AI Technical Summary
Existing stainless steel wire coating equipment is not suitable for stainless steel wires with larger diameters, resulting in uneven coating, especially at bends.
A coating device for stainless steel wire production was designed, including a straightening component and a coating component. The stainless steel wire is straightened by a pressure roller to make it into a straight line, and multi-angle coating is achieved through the cooperation of the bending component and the coating component to ensure the comprehensiveness and uniformity of the coating.
It effectively straightens the bent parts of thick stainless steel wire, ensuring uniform coating, shortening processing time, extending the service life of coating components, and improving the coating effect.
Smart Images

Figure CN118663516B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of stainless steel wire coating devices, in particular to a stainless steel wire production coating device. Background Art
[0002] Stainless steel wire plays a key role in a variety of industrial applications, so different industrial applications require stainless steel wire to have different properties. Usually these properties can be achieved through coating treatment. The coating treatment is completed by coating the surface of the stainless steel wire with a functional fluid to form a film on the surface of the stainless steel wire. For example, when the stainless steel wire is in certain extreme environments (such as strong acid, strong alkali or high salinity environment), the stainless steel may be corroded. An anti-corrosion fluid is coated on the surface of the stainless steel wire, and then dried or cured to give the stainless steel wire surface an additional anti-corrosion layer, and then the coating is completed. The coating of the stainless steel wire can serve as an additional protective layer to increase the corrosion resistance of the stainless steel wire.
[0003] A patent document with publication number CN112657781A discloses a stainless steel wire coating device for medical devices, including an automatic coating device body, a coating device on the automatic coating device body, and a support seat, a vertically sliding lifting plate on the support seat, and a driving mechanism for driving the lifting plate to rise on the support seat. The stainless steel wire coating device for medical devices provided by the present invention can lift the coating device from the sliding device of the automatic coating device body after the coating device performs the first coating, without manual lifting, thereby improving the efficiency of coating.
[0004] In the above technical solution, a layer of fluid is coated on the surface of the stainless steel wire through a coating device. When the fluid forms a film on the surface of the stainless steel wire, the coating work is completed. However, the above technical solution is not suitable for stainless steel wires with thicker diameters. After the stainless steel wires with thicker diameters are unwound by the winding wheel, the thick stainless steel wires will have bends. These bends are prone to uneven coating on the surface of the stainless steel wire when acted upon by the structure of the coating.
[0005] To this end, the present invention provides a coating device for producing stainless steel wire. Summary of the invention
[0006] In order to make up for the deficiencies of the prior art, at least one technical problem raised in the background technology is solved.
[0007] The technical solution adopted by the present invention to solve its technical problem is: a stainless steel wire production coating device described in the present invention comprises a base and two first fixed plates and a second fixed plate fixedly installed above the base, a stainless steel wire winding wheel is movably installed between the two second fixed plates, a stainless steel wire body is wound on the outer side of the stainless steel wire winding wheel, a straightening component is movably installed between the two first fixed plates, a second fluid box is fixedly installed on one side of the base, a coating action box is fixedly installed above the second fluid box, and a first fluid box is fixedly installed above the coating action box;
[0008] The straightening assembly comprises a motor box and a movable plate, two pressing rollers are movably installed between the motor box and the movable plate, electric telescopic rods are fixedly installed on the sides of the motor box and the movable plate, and one end of the two electric telescopic rods is fixedly connected to the corresponding first fixed plate;
[0009] Two component grooves are provided inside the motor box, and fixed motors are fixedly installed inside the two component grooves. A limiting groove is provided in the middle position of the pressure roller, and the fixed motor is fixedly connected to the corresponding pressure roller through a shaft.
[0010] Preferably, the first fluid box and the second fluid box are components made of the same structure, a coating chamber is opened inside the coating action box, and transport chambers are opened on both sides of the coating action box, and the two transport chambers are connected to the coating chamber.
[0011] Preferably, a transport component is fixedly installed inside the transport cavity, the transport component and the straightening component are components made of the same structure, and the transport component is used to transport the stainless steel wire body.
[0012] Preferably, a plurality of coating components are movably installed inside the coating chamber, a plurality of bending components are installed between the coating action box and the second fluid box, and the plurality of bending components are used to swing the plurality of coating components.
[0013] Preferably, the coating assembly includes a connecting pipe connected to the first fluid box or the second fluid box and a flat soft block fixedly arranged at one end of the connecting pipe, and a coating head is fixedly installed on the upper end of the flat soft block.
[0014] Preferably, the lower end of the flat soft block is fixedly installed inside the coating chamber, one end of the connecting tube is connected to the first fluid box or the second fluid box, the other end of the connecting tube is inside the coating chamber, and the flat soft block is a component made of rubber material.
[0015] Preferably, a flat soft block and a second supporting spring are fixedly mounted on both sides of the flat soft block, and one end of the flat soft block and the second supporting spring are both fixedly connected to the inside of the coating chamber.
[0016] Preferably, the bending assembly includes a driving motor fixedly mounted on the upper and lower sides of a coating action box, and a coaxial winding wheel and a coaxial unwinding wheel connected to the driving motor through an axis, a pulling rope is arranged around the outer sides of the coaxial winding wheel and the coaxial unwinding wheel, one end of the pulling rope is connected to the center position of the upper end of the flat soft block, and a support plate is movably mounted on one end of the coaxial unwinding wheel, and the support plate is fixedly mounted on the upper and lower sides of the coating action box.
[0017] Preferably, the pulling rope includes a first sliding rope slidably installed inside the coating chamber and a horizontal sliding rope, one end of the first sliding rope is mounted around the outside of the coaxial winding wheel or the coaxial unwinding wheel, one end of the second sliding rope is fixedly connected to the flat soft block, and a horizontal sliding rope is fixedly connected between the second sliding rope and the first sliding rope.
[0018] Preferably, a plurality of horizontal cylindrical cavities are provided inside the coating action box, the horizontal sliding rope is located inside the corresponding horizontal cylindrical cavity, a limiting sliding column is fixedly installed on the outer side of the horizontal sliding rope, and the limiting sliding column is slidably installed inside the horizontal cylindrical cavity.
[0019] The beneficial effects of the present invention are as follows:
[0020] 1. The device for producing coating of stainless steel wire described in the present invention unwinds the stainless steel wire body by rotating the stainless steel wire winding wheel, one end of the stainless steel wire body is located between two limit grooves, and while the stainless steel wire winding wheel rotates, driven by two fixed motors, the two pressure rollers respectively rotate forward and reverse, and the rotation of the two pressure rollers cooperates with the rotation of the stainless steel wire winding wheel to drive one end of the stainless steel wire body to move. Because the stainless steel wire body is relatively thick, part of the stainless steel wire body will be bent after being unwound by the stainless steel wire winding wheel, and the bent part of the stainless steel wire body will be straightened when passing through the two pressure rollers, so that one end of the stainless steel wire body becomes a straight line when passing through the two pressure rollers, and the straightened stainless steel wire body is easier to be coated.
[0021] 2. The device for producing coating on stainless steel wire described in the present invention has the stainless steel wire body clamped by the transport component inside the transport cavity. Since the transport component and the straightening component are components made of the same structure, the two transport components have a transmission effect, allowing the straightened stainless steel wire body to continuously move inside the coating action box. During the movement of the stainless steel wire body, the coating work is performed, thereby strengthening the processing process of the stainless steel wire body and shortening the processing time of the stainless steel wire body.
[0022] 3. A stainless steel wire production coating device described in the present invention, under the rotation of the coaxial winding wheel and the coaxial unwinding wheel of the multiple bending components, the flat soft blocks of the multiple coating components continuously swing back and forth, and the structure for the swinging of the flat soft blocks is arranged on the outside of the coating action box. At this time, the fluid coated inside the coating chamber will not affect the bending component, and the bending component can play a swinging role on the coating component for a long time. The flat soft blocks continuously swing back and forth, and when coating the stainless steel wire body, it will not be just a vertical upward angle, but there will be coating angles of different acute angles, and it can be coated to the angle hidden position of the stainless steel wire body, so that the coating of the stainless steel wire body is more comprehensive. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The present invention will be further described below in conjunction with the accompanying drawings.
[0024] Figure 1 It is an overall stereogram of the present invention;
[0025] Figure 2 It is a three-dimensional schematic diagram of the straightening assembly and the stainless steel wire winding wheel in the present invention;
[0026] Figure 3 It is a three-dimensional schematic diagram of the straightening assembly in the present invention;
[0027] Figure 4 This is a three-dimensional schematic diagram of the disassembly of the straightening component in the present invention;
[0028] Figure 5 It is a three-dimensional schematic diagram of the coating component and the bending component in the present invention;
[0029] Figure 6 It is a three-dimensional schematic diagram of the coating component in the present invention;
[0030] Figure 7 It is a three-dimensional schematic diagram of the bending component in the present invention;
[0031] Figure 8 It is a plan view of the pulling rope in the present invention.
[0032] In the figure: 1, first fluid box; 2, coating action box; 21, coating chamber; 22, transport chamber; 23, transport assembly; 24, horizontal cylindrical chamber; 3, second fluid box; 4, base; 41, first fixed plate; 411, electric telescopic rod; 42, second fixed plate; 5, straightening assembly; 51, motor box; 511, component slot; 512, fixed motor; 52, pressure roller; 521, limit slot; 53, moving plate; 6, stainless steel wire Reel; 7. Stainless steel wire body; 8. Coating assembly; 81. Connecting pipe; 82. First supporting spring; 83. Flat soft block; 84. Coating head; 85. Second supporting spring; 9. Bending assembly; 91. Driving motor; 92. Coaxial reel; 93. Coaxial unreel; 94. Support plate; 95. Pulling rope; 951. First sliding rope; 952. Horizontal sliding rope; 953. Second sliding rope; 96. Limit sliding column. DETAILED DESCRIPTION
[0033] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.
[0034] Embodiment 1: Figure 1-4 As shown, a stainless steel wire production coating device according to an embodiment of the present invention comprises a base 4 and two first fixed plates 41 and a second fixed plate 42 fixedly mounted above the base 4, a stainless steel wire winding wheel 6 is movably mounted between the two second fixed plates 42, a stainless steel wire body 7 is wound on the outer side of the stainless steel wire winding wheel 6, a straightening assembly 5 is movably mounted between the two first fixed plates 41, a second fluid box 3 is fixedly mounted on one side of the base 4, a coating action box 2 is fixedly mounted above the second fluid box 3, and a first fluid box 1 is fixedly mounted above the coating action box 2;
[0035] The straightening assembly 5 includes a motor box 51 and a movable plate 53, two pressing rollers 52 are movably installed between the motor box 51 and the movable plate 53, and electric telescopic rods 411 are fixedly installed on the sides of the motor box 51 and the movable plate 53, and one end of the two electric telescopic rods 411 is fixedly connected to the corresponding first fixed plate 41;
[0036] Two component grooves 511 are provided inside the motor box 51 , and fixed motors 512 are fixedly installed inside the two component grooves 511 . A limiting groove 521 is provided in the middle of the pressure roller 52 , and the fixed motor 512 is fixedly connected to the corresponding pressure roller 52 through a shaft.
[0037] Specifically, in the conventional technical solution, the stainless steel wire body 7 is usually rolled up. In the present technical solution, the thick stainless steel wire body 7 is rolled up inside the stainless steel wire winding wheel 6, and the stainless steel wire body 7 is unwound by the rotation of the stainless steel wire winding wheel 6. One end of the stainless steel wire body 7 is located between the two limit grooves 521. While the stainless steel wire winding wheel 6 rotates, the two pressure rollers 52 are driven by the two fixed motors 512 to rotate forward and reverse respectively. The rotation of the two pressure rollers 52 cooperates with the rotation of the stainless steel wire winding wheel 6 to drive one end of the stainless steel wire body 7 to move. Because the stainless steel wire body 7 is relatively thick, after being unwound by the stainless steel wire winding wheel 6, part of the stainless steel wire body 7 will When the stainless steel wire body 7 at the bent part passes through the two pressure rollers 52, the bent part of the stainless steel wire body 7 will be straightened, so that one end of the stainless steel wire body 7 becomes a straight line when passing through the two pressure rollers 52, and one end of the stainless steel wire body 7 passes through the interior of the coating action box 2, and the fluid inside the first fluid box 1 and the second fluid box 3 is used to coat the part of the stainless steel wire body 7 inside the coating action box 2. The coated stainless steel wire body 7 is then dried or cured to complete the coating work, and the thick stainless steel wire body 7 is straightened to prevent the bent part of the stainless steel wire body 7 from entering the coating action box 2. The device can also process the thick stainless steel wire body 7.
[0038] like Figure 5 As shown, the first fluid box 1 and the second fluid box 3 are components made of the same structure. A coating chamber 21 is opened inside the coating action box 2. Transport chambers 22 are opened on both sides of the coating action box 2. The two transport chambers 22 are connected to the coating chamber 21. A transport component 23 is fixedly installed inside the transport chamber 22. The transport component 23 and the straightening component 5 are components made of the same structure. The transport component 23 is used to transport the stainless steel wire body 7.
[0039] Specifically, the stainless steel wire body 7 is clamped by the transport component 23 inside the transport cavity 22. Because the transport component 23 and the straightening component 5 are components made of the same structure, the two transport components 23 have a transmission effect, allowing the straightened stainless steel wire body 7 to continuously move inside the coating action box 2. During the movement of the stainless steel wire body 7, the coating work is carried out to strengthen the processing process of the stainless steel wire body 7.
[0040] like Figure 5 As shown, a plurality of coating components 8 are movably installed inside the coating chamber 21 , and a plurality of bending components 9 are installed between the coating action box 2 and the second fluid box 3 . The plurality of bending components 9 are used to swing the plurality of coating components 8 .
[0041] Specifically, when the stainless steel wire body 7 is transmitted inside the coating action box 2, the bending component 9 can drive the coating component 8 to swing continuously, that is, the coating component 8 applies the fluid to the surface of the stainless steel wire body 7 by smearing or spraying during the swinging process. Because the interior of the coating action box 2 is to be coated or sprayed with fluid, when the coating work is performed, the fluid or the atomized fluid will fall into the coating action box 2. Therefore, when a swinging structure for the bending component 9 is set inside the coating action box 2, it is easily affected by the fluid, thereby shortening the service life of the swinging structure. The present device solves this problem by setting the bending component 9 outside the coating action box 2, thereby extending the service life of the structure that plays a swinging role for the coating component 8.
[0042] like Figure 6 As shown, the coating component 8 includes a connecting tube 81 connected to the first fluid box 1 or the second fluid box 3 and a flat soft block 83 fixedly arranged at one end of the connecting tube 81, a coating head 84 is fixedly installed on the upper end of the flat soft block 83, and the lower end of the flat soft block 83 is fixedly installed inside the coating chamber 21, one end of the connecting tube 81 is connected to the first fluid box 1 or the second fluid box 3, and the other end of the connecting tube 81 is inside the coating chamber 21, the flat soft block 83 is a component made of rubber material, and the flat soft block 83 and the second support spring 85 are fixedly installed on both sides of the flat soft block 83, and one end of the flat soft block 83 and the second support spring 85 are fixedly connected to the inside of the coating chamber 21.
[0043] Specifically, the connecting pipe 81 at the corresponding position is used to transmit the fluid inside the first fluid box 1 or the second fluid box 3, and then the fluid is coated out through the coating head 84. The lower end of the flat soft block 83 is fixedly connected to the inside of the coating chamber 21, but the upper end of the flat soft block 83 can be bent, so the upper end of the flat soft block 83 is fixed by the first support spring 82 and the second support spring 85. The first support spring 82 is located on the left side of one side of the flat soft block 83, and the second support spring 85 is located on the right side of one side of the flat soft block 83. The first support spring 82 and the second support spring 85 gives a supporting force to the upper end of the flat soft block 83 so that the coating head 84 can face vertically upward. The stainless steel wire body 7 is between the two coating heads 84 on the same vertical line. The two coating heads 84 can coat the surface of the stainless steel wire body 7 through the internal fluid. By arranging the coating structure for the stainless steel wire body 7 both above and below, the stainless steel wire body 7 can be coated more comprehensively. By arranging multiple coating heads 84 arranged above and below for swinging spraying, the surface of the stainless steel wire body 7 can be coated multiple times to increase the coating thickness on the outside of the stainless steel wire body 7.
[0044] like Figure 7As shown, the bending assembly 9 includes a driving motor 91 fixedly mounted on the upper and lower sides of the coating action box 2, and a coaxial winding wheel 92 and a coaxial unwinding wheel 93 connected to the driving motor 91 through an axis, and a pulling rope 95 is arranged around the outer sides of the coaxial winding wheel 92 and the coaxial unwinding wheel 93, and one end of the pulling rope 95 is connected to the center position of the upper end of the flat soft block 83, and a support plate 94 is movably mounted on one end of the coaxial unwinding wheel 93, and the support plate 94 is fixedly mounted on the upper and lower sides of the coating action box 2.
[0045] Specifically, when the bent stainless steel wire body 7 is straightened and enters the coating chamber 21, the point where the stainless steel wire body 7 is most sharply bent may not be as good as the originally straight stainless steel wire body 7 after being straightened, because the most sharply bent part of the stainless steel wire body 7 will still have a certain arc angle after being straightened, thereby forming a certain angle, which will result in a hidden surface at the angle of this part when being coated, and this surface is not easy to be coated. In the present invention, when the stainless steel wire body 7 is transmitted inside the coating chamber 21, it is driven by multiple sets of drive motors 91 to rotate multiple coaxial winding wheels 92 and coaxial unwinding wheels 93, one pulling rope 95 is wound on the coaxial winding wheel 92, and the other pulling rope 95 is unwound on The coaxial unwinding wheel 93 is on the coaxial unwinding wheel 93, so when the coaxial winding wheel 92 and the coaxial unwinding wheel 93 rotate synchronously, one pulling rope 95 will be wound up and the other pulling rope 95 will be unwound, and the wound pulling rope 95 will pull an adjacent flat soft block 83 to swing. At this time, the first supporting spring 82 on one side of the flat soft block 83 will be compressed, and the unwound pulling rope 95 will no longer pull the other adjacent flat soft block 83. Originally, the flat soft block 83 was bent, and the second supporting spring 85 was compressed. After the pulling rope 95 connected to the flat soft block 83 was unwound, under the action of the restoring force of the second supporting spring 85, the flat soft block 83 changes from bending to straight, which is equivalent to swinging halfway, and the second fluid box 3 and the coating action are connected. Between the boxes 2, the number of bending components 9 is two more than the number of coating components 8, and the same is true between the first fluid box 1 and the coating action box 2, that is, under the rotation of the coaxial winding wheel 92 and the coaxial unwinding wheel 93 of the multiple bending components 9, the flat soft blocks 83 of the multiple coating components 8 continuously swing back and forth, and the structure for the swing of the flat soft blocks 83 is arranged on the outside of the coating action box 2. At this time, the fluid coated inside the coating chamber 21 will not affect the bending component 9, and the bending component 9 can play a swinging role on the coating component 8 for a long time. The flat soft block 83 swings back and forth continuously, and when coating the stainless steel wire body 7, it will not be just a vertical upward angle, but there will be coating angles of different acute angles, which can be coated on the stainless steel wire body 7. The angle hidden position of the steel wire body 7 (this angle hidden position is similar to the bending position of the Z-shaped steel wire), a certain angle among the coating angles of different acute angles is directly opposite to this angle hidden position, so this position can be fully coated, and the vertical coating angle is not directly opposite to this position, so the coating is not comprehensive enough, and the inclination angles of different acute angles can avoid the accumulation of the coating fluid on the surface of the stainless steel wire body 7, because the coating is always carried out at a vertical angle, the fluid coated on the surface of the stainless steel wire body 7 will drip at the same position, and the dripping fluid will accumulate, thereby corroding or wearing the body, and the swinging coating method ensures that the fluid on the surface of the stainless steel wire body 7 will drip at multiple positions to avoid fluid accumulation. After the stainless steel wire body 7 is coated,The coating is then transferred to the outside of the coating action box 2 for subsequent drying or curing, thus completing the coating work.
[0046] Embodiment 2: Figure 8 As shown, compared with Example 1, another embodiment of the present invention is: the pulling rope 95 includes a first sliding rope 951 and a horizontal sliding rope 952 slidably installed inside the coating chamber 21, one end of the first sliding rope 951 is mounted around the outside of the coaxial winding wheel 92 or the coaxial unwinding wheel 93, one end of the second sliding rope 953 is fixedly connected to the flat soft block 83, and the horizontal sliding rope 952 is fixedly connected between the second sliding rope 953 and the first sliding rope 951. A plurality of horizontal cylindrical cavities 24 are also provided inside the coating action box 2, and the horizontal sliding rope 952 is located inside the corresponding horizontal cylindrical cavity 24. A limiting sliding column 96 is fixedly installed on the outside of the horizontal sliding rope 952, and the limiting sliding column 96 is slidably installed inside the horizontal cylindrical cavity 24.
[0047] Specifically, when the pulling rope 95 is unwinding or rewinding, the limit sliding column 96 moves back and forth inside the horizontal cylindrical cavity 24, and the limit sliding column 96 is fixedly connected to the horizontal sliding rope 952, so the limit sliding column 96 can only move inside the horizontal cylindrical cavity 24 to limit the length of the pulling rope 95 to be reeled or unwound, and then limit the swing angle of the flat soft block 83, so that the flat soft block 83 can better coat the surface of the stainless steel wire body 7. The second sliding rope 953 is inclined, so the limit When the sliding column 96 moves toward the first sliding rope 951 inside the coating head 84, that is, when the pulling rope 95 is wound, the second sliding rope 953 moves toward the first sliding rope 951. Because the horizontal sliding rope 952 moves laterally, the second sliding rope 953 and its sliding groove will contact and scratch the fluid that may adhere to the surface of the second sliding rope 953, thereby preventing the solidification of the fluid on the surface of the second sliding rope 953 from affecting the movement of the second sliding rope 953, thereby extending the working life of the pulling rope 95.
[0048] Working principle: The stainless steel wire body 7 is unwound by the rotation of the stainless steel wire winding wheel 6. One end of the stainless steel wire body 7 is located between the two limit grooves 521. While the stainless steel wire winding wheel 6 rotates, the two pressure rollers 52 are driven by the two fixed motors 512 to rotate forward and reverse respectively. The rotation of the two pressure rollers 52 cooperates with the rotation of the stainless steel wire winding wheel 6 to drive one end of the stainless steel wire body 7 to move. Because the stainless steel wire body 7 is relatively thick, after being unwound by the stainless steel wire winding wheel 6, part of the stainless steel wire body 7 will be bent. When the stainless steel wire body 7 at the bent part passes through the two pressure rollers 52, it will straighten the bent part of the stainless steel wire body 7, so that when one end of the stainless steel wire body 7 passes through the two pressure rollers 52, It becomes a straight line, and one end of the stainless steel wire body 7 passes through the interior of the coating action box 2. When the bent stainless steel wire body 7 is straightened and enters the coating chamber 21, the point where the stainless steel wire body 7 is originally bent the most severely may not be as good as the originally straight stainless steel wire body 7 after being straightened, because the stainless steel wire body 7 with the most severe bending will still have a certain arc angle after being straightened, thus forming a certain angle, which will cause a hidden surface in the angle of this part when being coated, and this surface is not easy to be coated. In the present invention, when the stainless steel wire body 7 is transmitted inside the coating chamber 21, it is driven by multiple sets of drive motors 91 to rotate multiple coaxial winding wheels 92 and coaxial unwinding wheels 93, and a pulling rope 95 is wound in The first support spring 82 on one side of the flat soft body block 83 is compressed, and the unwinding pull rope 95 will no longer pull the other adjacent flat soft body block 83. Originally, the flat soft body block 83 was bent, and the second support spring 85 was compressed. After the pulling rope 95 connected to the flat soft body block 83 was unwound, the flat soft body block 83 changed from being bent to being straight under the restoring force of the second support spring 85. When it is swung halfway, between the second fluid box 3 and the coating action box 2, the number of bending components 9 is two more than the number of coating components 8, and the same is true between the first fluid box 1 and the coating action box 2, that is, under the rotation of the coaxial winding wheel 92 and the coaxial unwinding wheel 93 of the multiple bending components 9, the flat soft blocks 83 of the multiple coating components 8 continuously swing back and forth, and the structure for the swinging of the flat soft blocks 83 is arranged on the outside of the coating action box 2. At this time, the fluid coated inside the coating chamber 21 will not affect the bending component 9, and the bending component 9 can play a swinging role on the coating component 8 for a long time. The flat soft block 83 continuously swings back and forth, and after the stainless steel wire body 7 is coated, it is transmitted to the outside of the coating action box 2 for subsequent drying or curing.The coating work is completed.
[0049] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A stainless steel wire coating production device, comprising a base (4) and two first fixed plates (41) and a second fixed plate (42) fixedly mounted above the base (4), a stainless steel wire winding wheel (6) being movably mounted between the two second fixed plates (42), a stainless steel wire body (7) being arranged on the outer side of the stainless steel wire winding wheel (6), and characterized in that: A straightening assembly (5) is movably mounted between the two first fixed plates (41); a second fluid box (3) is fixedly mounted on one side of the base (4); a coating action box (2) is fixedly mounted above the second fluid box (3); and a first fluid box (1) is fixedly mounted above the coating action box (2); The straightening assembly (5) comprises a motor box (51) and a movable plate (53), two pressure rollers (52) are movably installed between the motor box (51) and the movable plate (53), electric telescopic rods (411) are fixedly installed on the sides of the motor box (51) and the movable plate (53), and one end of the two electric telescopic rods (411) is fixedly connected to the corresponding first fixed plate (41); Two component grooves (511) are provided inside the motor box (51), and a fixed motor (512) is fixedly installed inside each of the two component grooves (511); a limiting groove (521) is provided in the middle of the pressure roller (52), and the fixed motor (512) is fixedly connected to the corresponding pressure roller (52) via a shaft; The first fluid box (1) and the second fluid box (3) are components made of the same structure. A coating chamber (21) is provided inside the coating action box (2). Transport chambers (22) are provided on both sides of the coating action box (2). Both transport chambers (22) are connected to the coating chamber (21). A plurality of coating components (8) are movably installed inside the coating chamber (21), a plurality of bending components (9) are installed between the coating action box (2) and the second fluid box (3), and the plurality of bending components (9) are used to swing the plurality of coating components (8); The coating assembly (8) comprises a connecting pipe (81) connected to the first fluid box (1) or the second fluid box (3) and a flat soft block (83) fixedly arranged at one end of the connecting pipe (81), and a coating head (84) is fixedly mounted on the upper end of the flat soft block (83); The lower end of the flat soft block (83) is fixedly mounted inside the coating chamber (21); one end of the connecting tube (81) is connected to the first fluid box (1) or the second fluid box (3); the other end of the connecting tube (81) is located inside the coating chamber (21); and the flat soft block (83) is a component made of rubber material; A flat soft block (83) and a second supporting spring (85) are fixedly mounted on both sides of the flat soft block (83), and one end of the flat soft block (83) and the second supporting spring (85) are both fixedly connected to the inside of the coating chamber (21); The bending assembly (9) comprises a driving motor (91) fixedly mounted on the upper and lower sides of the coating action box (2), and a coaxial winding wheel (92) and a coaxial unwinding wheel (93) connected to the driving motor (91) via an axis, a pulling rope (95) is arranged around the outer sides of the coaxial winding wheel (92) and the coaxial unwinding wheel (93), one end of the pulling rope (95) is connected to the center position of the upper end of the flat soft block (83), and a support plate (94) is movably mounted on one end of the coaxial unwinding wheel (93), and the support plate (94) is fixedly mounted on the upper and lower sides of the coating action box (2).
2. A stainless steel wire production coating device according to claim 1, characterized in that: A transport component (23) is fixedly installed inside the transport cavity (22); the transport component (23) and the straightening component (5) are components made of the same structure; the transport component (23) is used to transport the stainless steel wire body (7).
3. A stainless steel wire production coating device according to claim 2, characterized in that: The pulling rope (95) includes a first sliding rope (951) and a horizontal sliding rope (952) which are slidably installed inside the coating chamber (21), one end of the first sliding rope (951) is installed around the outside of the coaxial winding wheel (92) or the coaxial unwinding wheel (93), the flat soft block (83) is fixedly connected to one end of the second sliding rope (953), and the horizontal sliding rope (952) is fixedly connected between the second sliding rope (953) and the first sliding rope (951).
4. A stainless steel wire production coating device according to claim 3, characterized in that: The coating action box (2) is also provided with a plurality of horizontal columnar cavities (24) inside. The horizontal sliding rope (952) is located inside the corresponding horizontal columnar cavity (24). A limit sliding column (96) is fixedly installed outside the horizontal sliding rope (952). The limit sliding column (96) is slidably installed inside the horizontal columnar cavity (24).
Citation Information
Patent Citations
Stainless steel wire coating device for medical instruments
CN112657781A
Steel wire straightening machine for stainless steel wire production and use method of steel wire straightening machine
CN113351796A
Automatic gluing device for optical cable production
CN115770699A
Steel wire surface treatment device
CN214292552U