Composite glass sheet and method for producing same
Through the cleaning of vinegar water, glass cleaner, lemon juice and baking soda powder and the fully automatic cutting machine, as well as the sandwiching and laminating equipment of polymeric materials, the problem of offset and sliding of composite glass laminates during the lamination process was solved, achieving for higher accuracy and quality.
Patent Information
- Application Number
- CN202411223153.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-10-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The lack of a limiting mechanism during the lamination process of composite glass laminates may cause the glass laminates to shift or slide, affecting processing accuracy and quality.
Use vinegar water, glass cleaner, lemon juice and baking soda to clean and cut the glass plate. Use a fully automatic glass cutting machine to cut the glass plate and prepare interlayer materials such as polybutylene terephthalate (PBT), polyethylene carbonate (PC), etc., and by setting up pressurized cylinders, pneumatic suction cups, positioning plates and other equipment for precise lamination to ensure the positioning of the glass plates during lamination.
It improves the lamination accuracy and processing quality of composite glass laminates, reduces sliding phenomena, and improves the quality of finished products.
Smart Images

Figure CN118721892A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of composite vitreous glass plate production, in particular to a composite vitreous glass plate and a manufacturing method thereof. Background Art
[0002] Composite glass processing is a technology that combines two or more layers of glass through a specific process. This technology can improve the strength, heat resistance, sound insulation, anti-bullet and other properties of glass, and is widely used in construction, automobiles, aerospace and other fields.
[0003] For example, a method for manufacturing a composite glass laminate composed of a layered body of a polyvinyl acetal film containing a plasticizer and a polyvinyl acetal film poor in plasticizer, as disclosed in CN 104816521 B. Specifically, the invention relates to a method for manufacturing a layered body, the layered body consisting of at least one film A containing polyvinyl acetal PA and a maximum of 16 weight % of a plasticizer WA and at least one film B containing polyvinyl acetal PB and a minimum of 16 weight % of a plasticizer WB between two glass plates, characterized in that at least one film A is adhered to at least one film B or at least one of the glass plates by means of a liquid, and the layered body can be subsequently pressed into a composite glass laminate. However, when the glass layers are subjected to a composite pressing operation by a pressing device, there is a lack of a corresponding limiting mechanism to limit the glass layers, so that during the pressing operation, the glass layers may be offset or slipped, which affects the accuracy of the composite processing and reduces the quality of the composite glass layers, and has certain limitations.
[0004] Therefore, we propose a composite vitreous glass plate and a method for manufacturing the same to solve the above problems. Summary of the invention
[0005] The object of the present invention is to provide a composite glass plate and a method for manufacturing the same, so as to solve the problem that when the glass layers are subjected to a composite pressing operation by a pressing device, there is a lack of a corresponding limiting mechanism to limit the glass layers, so that during the pressing operation, the glass layers may be offset or slipped, thereby affecting the accuracy of the composite processing.
[0006] To achieve the above object, the present invention provides the following technical solution: a composite vitreous glass plate and a method for manufacturing the same. The composite vitreous glass plate is manufactured by the following steps: S1, including glass plate A and glass plate B, the cleaning agent is selected from at least one of vinegar water, glass cleaner, lemon juice and baking soda; S2. Cut the glass plates A and B into corresponding sizes and shapes according to the required sizes. A fully automatic glass cutting machine may be used; S3, heating the cut glass sheets A and B to soften them for easy lamination; S4. preparing an interlayer material, wherein the interlayer material comprises at least one substance selected from polybutylene terephthalate (PBT), polycarbonate (PC), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polymethyl methacrylate (PMMA), polyurethane (PUR) and / or mixtures and copolymers thereof; S5, placing the glass sheet A and the glass sheet B in a pressing device, and starting the pressing device to perform a pressing process; S6. Placing the composite glass sheet A and glass sheet B in a cooling chamber to gradually cool them down to reduce the problem of cracking or deformation of the composite glass sheet A and glass sheet B.
[0007] Preferably, vinegar water is selected in step S1, by adding a portion of white vinegar to water in the same proportion, and then pouring the mixture into a spray bottle, spraying the vinegar water on the glass surface with a sprayer, and then wiping it with a wet sponge or soft cloth, and then wiping it dry with a clean cloth. Vinegar can remove some stubborn stains and impurities, and eliminate the greasy feeling and scale on the glass surface.
[0008] Preferably, in step S2, the fully automatic glass cutting machine starts the power supply, sets the size to be cut, places the glass plate A or the glass plate B on the machine, presses the blow button, firmly holds the glass plate A or the glass plate B in the designated position, and the machine cuts automatically. After the cutting is completed, press the stop button, then press the blow switch, and finally clean the cutting table and the broken glass with a piece of cloth.
[0009] Preferably, the temperature of the heating device in step S3 is 110° C.-130° C., and the heating time is 4-5 hours.
[0010] Preferably, at least one polycarbonate (PC) is selected in step S4.
[0011] Preferably, the working process of the pressing device is as follows: The first step is to place glass plate A at the bottom of the pressure plate, start the pneumatic suction cup to absorb glass plate A, then place glass plate B on the top of the placement rack, and fill the interlayer material between glass plate A and glass plate B.
[0012] The second step is to start the pressurized cylinder, which drives the pressure plate to press down, so that the glass plate A, glass plate B and interlayer materials are pressed together. At the same time, the pressure plate pulls the pull rope, and the pull rope drives the closed plate to rise. The rising of the closed plate drives the positioning plate to rise.
[0013] Step 3: When the positioning plate is higher than the placement frame, the elastic force of the spring drives the slide bar and the positioning plate to move inward, so that the positioning plates around press the glass plates A and B in the middle, thereby facilitating the positioning of the glass plates A and B when pressing them together.
[0014] Preferably, the glass cleaner selected in step S1 generally contains decontamination and antistatic ingredients, can quickly remove fingerprints and stains, and is not prone to residual spots. When using, just spray it on the glass surface and then wipe it with a paper towel or sponge.
[0015] Preferably, in step S1, lemon juice and baking soda are mixed in appropriate amounts to form a paste, and then the paste is evenly applied to the glass surface, left for a few minutes, and then wiped clean with a sponge, and finally rinsed with water. Lemon juice has the effect of eliminating odor and sterilizing, while baking soda has the effect of removing dirt and deodorizing.
[0016] A method for manufacturing a composite vitreous glass plate comprises the following steps: S1. A glass plate A and a glass plate B are included. A cleaning agent is selected from at least one of vinegar water, glass cleaner, lemon juice and baking soda. The vinegar water is selected by adding a portion of white vinegar to water in the same proportion, and then pouring the mixture into a spray bottle, spraying the vinegar water on the glass surface with a sprayer, and then wiping with a wet sponge or soft cloth, and then wiping dry with a clean cloth. Vinegar can remove some stubborn stains and impurities, and eliminate the greasy feeling and scale on the glass surface; S2. Cut glass plate A and glass plate B into corresponding sizes and shapes according to the required size. You can use a fully automatic glass cutting machine. Start the power of the fully automatic glass cutting machine, set the required cutting size, put glass plate A or glass plate B on the machine, press the blow button, firmly fix glass plate A or glass plate B in the specified position, the machine will cut automatically, after the cutting is completed, press the stop button, then press the blow switch, and finally clean the cutting table and the broken glass with a piece of cloth; S3, heating the cut glass sheets A and B to soften them for easy lamination, the temperature of the heating device is 110°C-130°C, and the heating time is 4-5 hours; S4, preparing a sandwich material, the sandwich material comprising at least one substance selected from polybutylene terephthalate (PBT), polycarbonate (PC), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polymethyl methacrylate (PMMA), polyurethane (PUR) and / or mixtures and copolymers thereof, at least one polycarbonate (PC) is selected; S5, placing the glass sheet A and the glass sheet B in a pressing device, and starting the pressing device to perform a pressing process; S6. Placing the composite glass sheet A and glass sheet B in a cooling chamber to gradually cool them down to reduce the problem of cracking or deformation of the composite glass sheet A and glass sheet B.
[0017] Compared with the prior art, the present invention has the following beneficial effects: 1. After selecting glass plate A and glass plate B, use vinegar water cleaner to clean glass plate A and glass plate B. Vinegar can remove some stubborn stains and impurities, and eliminate the greasy feeling and scale on the glass surface. The fully automatic glass cutting machine is used to cut glass plate A and glass plate B to the required size. The interlayer material can be polycarbonate (PC). The pressing equipment improves the accuracy of the composite of glass plate A and glass plate B and improves the quality of the composite processing.
[0018] 2. By setting a pressurized cylinder, a pressing plate, a placement rack, a closed plate, a pneumatic suction cup, a pull rope and a positioning plate, when performing the pressing operation, place the glass plate A at the bottom of the pressing plate, start the pneumatic suction cup to adsorb the glass plate A, then place the glass plate B on the top of the placement rack, and fill the interlayer material between the glass plates A and B, then start the pressurized cylinder, the pressurized cylinder drives the pressing plate to press down, so that the glass plates A, B and the interlayer material are pressed together, and at the same time, the pressing plate pulls the pull rope, the pull rope drives the closed plate to rise, and the rising of the closed plate drives the positioning plate to rise. When the positioning plate is higher than the placement rack, the elastic force of the spring drives the sliding rod and the positioning plate to move inward, so that the positioning plates around press the glass plates A and B in the middle, thereby facilitating the positioning of the glass plates A and B during pressing, reducing sliding during pressing, improving the accuracy of the glass plate composite processing, and making the quality of the finished product higher.
[0019] 3. By setting a cleaning roller, an auxiliary roller, a nozzle and a liquid collecting box, when the glass plates A and B are placed, first, they are pressed and transmitted by two cleaning rollers, and the nozzle blows air to assist in cleaning the glass plates A and B. The auxiliary roller is used for quick drying of the glass plates A and B after cleaning, thereby reducing the influence of dust on the glass plates A and B. The liquid collecting box is used to collect the sewage after cleaning. A hot air blower, an air guide cavity and a pneumatic suction cup are provided. The hot air blower is started to blow out hot air and enter the air guide cavity, which is convenient for heat conduction to the pressing plate and the placing frame, and can assist in the pressing of the glass plates A and B. The pneumatic suction cup is used for the adsorption, fixation and removal of the glass plate A. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a process flow chart of the present invention; Figure 2 It is a main cross-sectional overall schematic diagram of the pressing device of the present invention; Figure 3 It is a schematic diagram of the pressing state of the present invention; Figure 4 For the present invention Figure 2A is an enlarged structural diagram; Figure 5 For the present invention Figure 3 The enlarged structural diagram at B in FIG. Figure 6 It is a schematic diagram of the overall structure of the pressing device of the present invention.
[0021] In the figure: 1. bottom plate; 2. column; 3. top plate; 4. glass plate A; 5. glass plate B; 6. cleaning roller; 7. pressurized cylinder; 8. pressure plate; 9. placement rack; 10. hot air blower; 11. sealed plate; 12. auxiliary roller; 13. nozzle; 14. liquid collecting box; 15. air guide chamber; 16. pneumatic suction cup; 17. pulley; 18. pull rope; 19. slide rod; 20. spring; 21. positioning plate; 22. interlayer material. DETAILED DESCRIPTION
[0022] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0023] Embodiment 1: The composite vitreous glass plate is made by the following steps: S1, including glass plate A4 and glass plate B5, the cleaning agent is selected from at least one of vinegar water, glass cleaner, lemon juice and baking soda; S2. Cut the glass plates A4 and B5 into corresponding sizes and shapes according to the required sizes. A fully automatic glass cutting machine may be used. S3, heating the cut glass sheets A4 and B5 to soften them for easy lamination; S4, preparing an interlayer material 22, wherein the interlayer material 22 comprises at least one substance selected from polybutylene terephthalate (PBT), polycarbonate (PC), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polymethyl methacrylate (PMMA), polyurethane (PUR) and / or mixtures and copolymers thereof; S5, placing the glass sheet A4 and the glass sheet B5 in a pressing device, and starting the pressing device to perform a pressing process; S6. Place the composite glass sheet A4 and the glass sheet B5 in a cooling chamber to gradually cool them down, so as to reduce the problem of cracking or deformation of the composite glass sheet A4 and the glass sheet B5.
[0024] In step S1, vinegar water is selected by adding a portion of white vinegar to water in the same proportion, and then pouring the mixture into a spray bottle, spraying the vinegar water on the glass surface with a sprayer, and then wiping it with a wet sponge or soft cloth, and then wiping it dry with a clean cloth. Vinegar can remove some stubborn stains and impurities, and eliminate the greasy feeling and scale on the glass surface.
[0025] In step S2, the fully automatic glass cutting machine starts the power supply, sets the required cutting size, places the glass plate A4 or glass plate B5 on the machine, presses the blow button, firmly fixes the glass plate A4 or glass plate B5 in the specified position, and the machine will cut automatically. After the cutting is completed, press the stop button, then press the blow switch, and finally clean the cutting table with a piece of cloth and clean the broken glass.
[0026] In step S3, the temperature of the heating device is 110° C.-130° C., and the heating time is 4-5 hours.
[0027] In step S4, at least one polycarbonate (PC) is selected.
[0028] Embodiment 2: The composite vitreous glass plate is made by the following steps: S1, including glass plate A4 and glass plate B5, the cleaning agent is selected from at least one of vinegar water, glass cleaner, lemon juice and baking soda; S2. Cut the glass plates A4 and B5 into corresponding sizes and shapes according to the required sizes. A fully automatic glass cutting machine may be used. S3, heating the cut glass sheets A4 and B5 to soften them for easy lamination; S4, preparing an interlayer material 22, wherein the interlayer material 22 comprises at least one substance selected from polybutylene terephthalate (PBT), polycarbonate (PC), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polymethyl methacrylate (PMMA), polyurethane (PUR) and / or mixtures and copolymers thereof; S5, placing the glass sheet A4 and the glass sheet B5 in a pressing device, and starting the pressing device to perform a pressing process; S6. Place the composite glass sheet A4 and the glass sheet B5 in a cooling chamber to gradually cool them down, so as to reduce the problem of cracking or deformation of the composite glass sheet A4 and the glass sheet B5.
[0029] The glass cleaner selected in step S1 generally contains decontamination and anti-static ingredients, can quickly remove fingerprints and stains, and is not easy to leave residual spots. When using, just spray it on the glass surface and then wipe it with a paper towel or sponge.
[0030] In step S2, the fully automatic glass cutting machine starts the power supply, sets the required cutting size, places the glass plate A4 or glass plate B5 on the machine, presses the blow button, firmly fixes the glass plate A4 or glass plate B5 in the specified position, and the machine will cut automatically. After the cutting is completed, press the stop button, then press the blow switch, and finally clean the cutting table with a piece of cloth and clean the broken glass.
[0031] In step S3, the temperature of the heating device is 120° C.-130° C., and the heating time is 4 hours.
[0032] In step S4, at least one polycarbonate (PC) is selected.
[0033] Embodiment 3: The composite vitreous glass plate is made by the following steps: S1, including glass plate A4 and glass plate B5, the cleaning agent is selected from at least one of vinegar water, glass cleaner, lemon juice and baking soda; S2. Cut the glass plates A4 and B5 into corresponding sizes and shapes according to the required sizes. A fully automatic glass cutting machine may be used. S3, heating the cut glass sheets A4 and B5 to soften them for easy lamination; S4, preparing an interlayer material 22, wherein the interlayer material 22 comprises at least one substance selected from polybutylene terephthalate (PBT), polycarbonate (PC), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polymethyl methacrylate (PMMA), polyurethane (PUR) and / or mixtures and copolymers thereof; S5, placing the glass sheet A4 and the glass sheet B5 in a pressing device, and starting the pressing device to perform a pressing process; S6. Place the composite glass sheet A4 and the glass sheet B5 in a cooling chamber to gradually cool them down, so as to reduce the problem of cracking or deformation of the composite glass sheet A4 and the glass sheet B5.
[0034] In step S1, lemon juice and baking soda are mixed in proper amounts to form a paste, and then the paste is evenly applied to the glass surface. After leaving it for a few minutes, it is wiped clean with a sponge and finally rinsed with water. Lemon juice has the effect of eliminating odor and sterilizing, while baking soda has the effect of removing dirt and deodorizing.
[0035] In step S2, the fully automatic glass cutting machine starts the power supply, sets the required cutting size, places the glass plate A4 or glass plate B5 on the machine, presses the blow button, firmly fixes the glass plate A4 or glass plate B5 in the specified position, and the machine will cut automatically. After the cutting is completed, press the stop button, then press the blow switch, and finally clean the cutting table with a piece of cloth and clean the broken glass.
[0036] In step S3, the temperature of the heating device is 110° C.-120° C., and the heating time is 5 hours.
[0037] In step S4, at least one polycarbonate (PC) is selected.
[0038] See also Figure 1-6 The present invention provides a technical solution: a composite vitreous glass plate and a method for manufacturing the same, comprising a bottom plate 1, a glass plate A4, a glass plate B5, an interlayer material 22 and columns 2 symmetrically fixed around the top of the bottom plate 1, a top plate 3 being fixedly connected to the top of the columns 2, a cleaning roller 6 being symmetrically installed on one side of the columns 2, and a pressurized cylinder 7 being fixedly installed at the bottom of the top plate 3.
[0039] A pressing plate 8 is fixedly connected to the bottom end of the telescopic part of the pressurized cylinder 7, a placing rack 9 is fixedly connected to the top middle of the bottom plate 1, a hot air blower 10 is installed at the bottom of the placing rack 9, a hot air blower 10 is installed on the top of the pressing plate 8, a sealing plate 11 is connected to the outside of the placing rack 9, an auxiliary roller 12 is symmetrically installed on the other side of the column 2, a nozzle 13 is installed on one side of the cleaning roller 6, and the nozzle 13 is symmetrically arranged up and down, and a liquid collecting box 14 is fixedly connected to the bottom of the column 2 by bolts.
[0040] An air guide cavity 15 is provided inside the pressing plate 8, an air guide cavity 15 is provided at the bottom of the placing rack 9, an air outlet of the hot air blower 10 is connected to the air guide cavity 15, and a pneumatic suction cup 16 is symmetrically installed at the bottom of the pressing plate 8. The pneumatic suction cup 16 is symmetrically arranged around the bottom of the pressing plate 8, and the bottom surface of the pneumatic suction cup 16 is flush with the bottom surface of the pressing plate 8.
[0041] Pulleys 17 are fixedly installed around the bottom of the top plate 3, and a pull rope 18 is wound around the outer side of the pulley 17. One end of the pull rope 18 is fixedly connected to the top of the pressure plate 8, and the other end of the pull rope 18 is fixedly connected to the top of the closed plate 11. A slide rod 19 is slidably connected to the side of the closed plate 11, and one end of the slide rod 19 close to the placement frame 9 is fixedly connected to a positioning plate 21. A spring 20 is slidably connected to the outer side of the slide rod 19, and one end of the spring 20 is fixedly connected to the closed plate 11, and the other end of the spring 20 is fixedly connected to the positioning plate 21.
[0042] Working process and principle of pressing equipment: When using the device, first, Figure 1-6As shown, during the pressing operation, the glass plate A4 is placed at the bottom of the pressing plate 8, the pneumatic suction cup 16 is started to adsorb the glass plate A4, and then the glass plate B5 is placed on the top of the placement rack 9. When the glass plates A4 and B5 are placed, they are first pressed and transmitted by two cleaning rollers 6, and the nozzle 13 blows air to assist in cleaning the glass plates A4 and B5. The auxiliary roller 12 is used for quick drying of the glass plates A4 and B5 after cleaning, thereby reducing the influence of dust on the glass plates A4 and B5. The liquid collection box 14 is used to collect the sewage after cleaning.
[0043] Fill interlayer material 22 between glass plate A4 and glass plate B5, start the hot air blower 10 to blow out hot air, and let it enter the air guide cavity 15, so as to facilitate heat conduction to the pressing plate 8 and the placement rack 9, and assist in the pressing of glass plate A4 and glass plate B5. The pneumatic suction cup 16 is used for adsorption, fixation and removal of glass plate A4.
[0044] Then the pressurizing cylinder 7 is started, and the pressurizing cylinder 7 drives the pressing plate 8 to press down, so that the glass plates A4, B5 and the interlayer material 22 are pressed together. At the same time, the pressing plate 8 pulls the pull rope 18, and the pull rope 18 drives the sealed plate 11 to rise, and the rising of the sealed plate 11 drives the positioning plate 21 to rise. When the positioning plate 21 is higher than the placement frame 9, the elastic force of the spring 20 drives the sliding rod 19 and the positioning plate 21 to move inward, so that the positioning plates 21 on all sides press the glass plates A4 and B5 in the middle, thereby facilitating the positioning of the glass plates A4 and B5 during pressing, and reducing sliding during pressing.
[0045] The contents not described in detail in this specification belong to the prior art known to professional and technical personnel in this field.
[0046] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A composite vitreous glass plate and a method for producing the same, characterized in that: The composite vitreous glass plate is made by the following steps: S1, comprising a glass plate A (4) and a glass plate B (5), wherein a cleaning agent is selected from at least one of vinegar water, glass cleaner, lemon juice and baking soda; S2. Cut the glass plate A (4) and the glass plate B (5) into corresponding sizes and shapes according to the required dimensions. A fully automatic glass cutting machine may be used; S3, heating the cut glass sheet A (4) and glass sheet B (5) to soften them for easy lamination; S4, preparing an interlayer material (22), wherein the interlayer material (22) comprises at least one substance selected from polybutylene terephthalate (PBT), polycarbonate (PC), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polymethyl methacrylate (PMMA), polyurethane (PUR) and / or mixtures and copolymers thereof; S5, placing the glass sheet A (4) and the glass sheet B (5) in a pressing device, and starting the pressing device to perform a pressing process; S6. Place the composite glass sheet A (4) and the glass sheet B (5) in a cooling chamber to gradually cool them down, so as to reduce the possibility of cracking or deformation of the composite glass sheet A (4) and the glass sheet B (5).
2. The composite vitreous glass plate and the method for manufacturing the same according to claim 1, characterized in that: In step S1, vinegar water is selected by adding a portion of white vinegar to water in the same proportion, and then pouring the mixture into a spray bottle, spraying the vinegar water on the glass surface with a sprayer, and then wiping it with a wet sponge or soft cloth, and then wiping it dry with a clean cloth. Vinegar can remove some stubborn stains and impurities, and eliminate the greasy feeling and scale on the glass surface.
3. The composite vitreous glass plate and the method for manufacturing the same according to claim 1, characterized in that: In step S2, the fully automatic glass cutting machine is powered on, the required cutting size is set, the glass plate A (4) or the glass plate B (5) is placed on the machine, the air blowing button is pressed, the glass plate A (4) or the glass plate B (5) is firmly fixed at the specified position, and the machine will cut automatically. After the cutting is completed, the stop button is pressed, and then the air blowing switch is pressed. Finally, a piece of cloth is used to clean the cutting table and the broken glass.
4. The composite vitreous glass plate and the method for manufacturing the same according to claim 1, characterized in that: In step S3, the temperature of the heating device is 110° C.-130° C., and the heating time is 4-5 hours.
5. The composite vitreous glass plate and the method for manufacturing the same according to claim 1, wherein: In step S4, at least one polycarbonate (PC) is selected.
6. The composite vitreous glass plate and the method for manufacturing the same according to claim 1, characterized in that: The working process of the pressing device is as follows: The first step is to place the glass plate A (4) at the bottom of the pressing plate (8), start the pneumatic suction cup (16) to absorb the glass plate A (4), then place the glass plate B (5) on the top of the placement frame (9), and fill the interlayer material (22) between the glass plate A (4) and the glass plate B (5); Step 2: Then, the pressurizing cylinder (7) is started, and the pressurizing cylinder (7) drives the pressing plate (8) to press downward, so that the glass plate A (4), the glass plate B (5) and the interlayer material (22) are pressed together. At the same time, the pressing plate (8) pulls the pull rope (18), and the pull rope (18) drives the sealing plate (11) to rise. The rising of the sealing plate (11) drives the positioning plate (21) to rise. Step 3: When the positioning plate (21) is higher than the placement frame (9), the elastic force of the spring (20) drives the slide bar (19) and the positioning plate (21) to move inward, so that the positioning plates (21) on all sides press the glass plate A (4) and the glass plate B (5) in the middle, thereby facilitating the positioning of the glass plate A (4) and the glass plate B (5) when pressing together.
7. The composite vitreous glass plate and the method for manufacturing the same according to claim 1, characterized in that: The glass cleaner selected in step S1 generally contains decontamination and anti-static ingredients, can quickly remove fingerprints and stains, and is not easy to leave residual spots. When using, just spray it on the glass surface and then wipe it with a paper towel or sponge.
8. The composite vitreous glass plate and the method for manufacturing the same according to claim 1, wherein: In step S1, lemon juice and baking soda are mixed in proper amounts to form a paste, and then the paste is evenly applied to the glass surface. After leaving it for a few minutes, it is wiped clean with a sponge and finally rinsed with water. Lemon juice has the effect of eliminating odor and sterilizing, while baking soda has the effect of removing dirt and deodorizing.
9. A method for manufacturing a composite vitreous glass plate, characterized in that: The steps include: S1, including glass plate A (4) and glass plate B (5), the cleaning agent is selected from at least one of vinegar water, glass cleaner, lemon juice and baking soda, the vinegar water is selected, by adding a portion of white vinegar to water in the same proportion, then pouring the mixture into a spray bottle, spraying the vinegar water on the glass surface with a sprayer, then wiping with a wet sponge or soft cloth, and then wiping dry with a clean cloth, the vinegar can remove some stubborn stains and impurities, and eliminate the greasy feeling and scale on the glass surface; S2. Cut the glass plate A (4) and the glass plate B (5) into the corresponding size and shape according to the required size. A fully automatic glass cutting machine can be used. Turn on the power of the fully automatic glass cutting machine, set the required cutting size, place the glass plate A (4) or the glass plate B (5) on the machine, press the blow button, firmly fix the glass plate A (4) or the glass plate B (5) in the specified position, and the machine will cut automatically. After the cutting is completed, press the stop button, then press the blow switch, and finally clean the cutting table and the broken glass with a piece of cloth; S3, heating the cut glass sheets A (4) and B (5) to soften them for easy lamination, the temperature of the heating device being 110° C.-130° C. and the heating time being 4-5 hours; S4, preparing an interlayer material (22), wherein the interlayer material (22) comprises at least one substance selected from the group consisting of polybutylene terephthalate (PBT), polycarbonate (PC), polyethylene terephthalate (PET), polyethylene naphthalate (PEN), polymethyl methacrylate (PMMA), polyurethane (PUR) and / or mixtures and copolymers thereof, and at least one polycarbonate (PC) is selected; S5, placing the glass sheet A (4) and the glass sheet B (5) in a pressing device, and starting the pressing device to perform a pressing process; S6. Place the composite glass sheet A (4) and the glass sheet B (5) in a cooling chamber to gradually cool them down, so as to reduce the possibility of cracking or deformation of the composite glass sheet A (4) and the glass sheet B (5).
Citation Information
Patent Citations
Composite pane, composed of a polymeric pane and a glass pane
CN106457792A
Composite material plate processing device and method
CN113580719A
Positioning device of bending machine
CN115430738A
Laminating machine for producing laminated special glass
CN116691113A
Automotive laminated glass processing device and process thereof
CN117510061A