Secondary battery
By arranging collector regions with different thicknesses and alternately arranging electrode layers in the secondary battery, the problem of uneven current density distribution is solved, the energy efficiency and durability of the battery are improved, and more uniform dendrite formation is achieved.
Patent Information
- Application Number
- CN202310336307.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-01
AI Technical Summary
In the process of enlargement of secondary batteries, the increase in the size of the current collector leads to uneven current density distribution, causing local heating and uneven formation of dendrites. It is difficult to effectively solve it with existing technology, and the cooling method increases the cost and cannot eliminate the current density distribution. The problem itself.
By arranging regions with different thicknesses in the current collector of the secondary battery along the direction orthogonal to the stacking direction of the electrode layer and the electrolyte layer, and gradually thickening at the end where the current flows in and out, the current density distribution is reduced, and at the same time, Areas with smaller and larger thicknesses are alternately arranged in the negative and positive electrode current collectors to optimize the configuration of the electrode layer and electrolyte layer.
It effectively reduces the current density distribution of the secondary battery, improves the energy efficiency and durability of the battery, reduces the possibility of uneven formation of dendrites, reduces the current density distribution, and thereby improves the overall performance of the battery.
Smart Images

Figure CN118738407A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a secondary battery. Background Art
[0002] In recent years, in order to ensure that many people can afford, trust, and secure sustainable and advanced energy, research and development of secondary batteries that contribute to energy efficiency has been conducted.
[0003] The secondary battery has a structure of stacking electrode layers and electrolyte layers. The electrode layer includes a current collector. A foil-shaped or plate-shaped metal is used as the current collector. A current collector with uniform thickness is usually used. In order to suppress the variation of temperature distribution, a technology is proposed in which the thickness of the first position in the plane orthogonal to the stacking direction of the electrolyte layer is made thicker than the thickness of the second position having higher heat dissipation than the first position (see Patent Document 1).
[0004] [Prior art literature]
[0005] [Patent Document]
[0006] [Patent Document 1] Japanese Patent Application Publication No. 2008-159330 Summary of the invention
[0007] [Problems to be solved by the invention]
[0008] The technology disclosed in Patent Document 1 is to increase the heat dissipation of the secondary battery by increasing the thickness of the electrolyte layer at the position with higher heat dissipation and reducing the thickness of the collector. On the other hand, the above-mentioned structure is suitable for the structure of the bipolar battery with lower heat dissipation in the area on the central side, and cannot be said to be suitable for all the structures of the secondary battery.
[0009] However, in the case of vehicle-mounted secondary batteries, the secondary batteries are sought to be larger depending on their use. When the secondary battery is enlarged, as the size of the collector increases, a current density distribution will inevitably occur inside the battery. When a current density distribution occurs, especially when a large current flows in the collector, problems such as local heat generation and uneven formation of dendrites will occur. Therefore, it is considered to deal with this by controlling or cooling the secondary battery. However, the method is not only costly, but also has the problem of being unable to eliminate the current density distribution itself.
[0010] The present invention is made in view of the above circumstances, and an object of the present invention is to provide a secondary battery capable of reducing current density distribution.
[0011] [Technical means to solve the problem]
[0012] (1) The present invention relates to a secondary battery having an electrode layer and an electrolyte layer, wherein the electrode layer contains an electrode active material and a current collector, and the current collector has regions having different thicknesses in a direction orthogonal to the stacking direction of the electrode layer and the electrolyte layer.
[0013] According to the invention of (1), a secondary battery capable of reducing current density distribution can be provided.
[0014] (2) The secondary battery according to (1), wherein the thickness of the current collector changes continuously from one end portion toward the other end portion in a direction perpendicular to the stacking direction.
[0015] According to the invention of (2), the current density distribution can be more preferably reduced.
[0016] (3) A secondary battery according to (1) or (2), wherein the current collector has, in a direction orthogonal to the stacking direction, a relative portion opposite to the electrode active material layer containing the electrode active material, and a non-relative portion not opposite to the electrode active material layer, and the thickness of the non-relative portion is thicker than the thickness of the relative portion.
[0017] According to the invention of (3), the thickness of the current collector gradually increases toward the end portion where current flows in and out, thereby reducing the current density distribution.
[0018] (4) A secondary battery according to (2), wherein a plurality of groups of electrode layers and electrolyte layers are stacked, the collector is composed of a negative electrode collector and a positive electrode collector, and is arranged in a manner such that regions with smaller thickness in the stacking direction and regions with larger thickness in the stacking direction are alternately arranged in the stacking direction, the direction in which the thickness of the plurality of negative electrode collectors increases is the same direction, and the direction in which the thickness of the plurality of positive electrode collectors increases is the same direction.
[0019] According to the invention of (4), the energy efficiency per unit volume of the secondary battery can be improved.
[0020] (5) A secondary battery according to (2) or (4), wherein a plurality of groups of electrode layers and electrolyte layers are stacked, the collector is composed of a negative electrode collector and a positive electrode collector, and is arranged in a manner such that regions with smaller thickness in the stacking direction and regions with larger thickness in the stacking direction are alternately arranged in the stacking direction, the rates of change of the thickness of the plurality of negative electrode collectors in a direction orthogonal to the stacking direction are respectively equal, and the rates of change of the thickness of the plurality of positive electrode collectors in a direction orthogonal to the stacking direction are respectively equal.
[0021] According to the invention of (5), the energy efficiency per unit volume of the secondary battery can be improved.
[0022] Effects of the Invention
[0023] According to the present invention, a secondary battery capable of reducing current density distribution can be provided. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a schematic cross-sectional view showing the structure of the secondary battery of this embodiment.
[0025] Figure 2 It is a schematic cross-sectional view showing the structure of a conventional secondary battery.
[0026] Figure 3 It is a diagram showing a simulation model of the secondary battery according to the present embodiment.
[0027] Figure 4 It is a diagram showing the simulation results of the secondary battery according to the present embodiment. DETAILED DESCRIPTION
[0028] Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings. Figure 1 As shown, the secondary battery 1 of the present embodiment is configured by stacking a plurality of secondary batteries 10a and 10b as the minimum unit of the secondary battery, which is a set of a pair of electrode layers and an electrolyte. Figure 1 In the embodiment, the number of stacked layers of the minimum unit secondary battery in the secondary battery 1 is 2, but the number of stacked layers is not particularly limited.
[0029] [Secondary battery]
[0030] The secondary batteries 10a and 10b are not particularly limited, and examples thereof include lithium ion secondary batteries and lithium metal batteries that use lithium ions as a charge transfer medium. Examples of lithium ion secondary batteries include non-aqueous electrolyte batteries and solid batteries that have an electrolyte. Examples of the solid battery include semi-solid lithium ion batteries that have a gel electrolyte and all-solid lithium ion batteries that have a solid electrolyte.
[0031] Secondary batteries 10a and 10b are preferably lithium metal batteries. Lithium metal batteries easily form dendrites at the negative electrode, and if current density distribution is generated, the dendrites are also formed unevenly. As a result, the positive electrode and the solid electrolyte layer move from the part with more lithium metal precipitation to the part with less lithium metal precipitation, and there is a possibility that the durability of the battery is reduced. However, the secondary battery of this embodiment can reduce the current density distribution, so it is considered that the formation of dendrites in the lithium metal battery is also easy to be uniform.
[0032] Since the configurations of the secondary batteries 10a and 10b are substantially the same, the configuration of the secondary battery 10a will be described below. The configuration of the secondary battery 10b is denoted by the same reference numerals in the drawings, and description thereof will be omitted.
[0033] like Figure 1 As shown, the secondary battery 10a has an electrode layer and an electrolyte layer 40. The negative electrode layer as the electrode layer includes a negative electrode active material layer 22 containing a negative electrode active material as an electrode active material, and a negative electrode collector 21 as a collector. Similarly, the positive electrode layer as the electrode layer includes a positive electrode active material layer 32 containing a positive electrode active material as an electrode active material, and a positive electrode collector 31 as a collector. The stacking direction of the electrode layer and the electrolyte layer 40 is Figure 1 The direction D1 in FIG. 1 is the direction D2 that is perpendicular to the stacking direction.
[0034] The negative electrode current collector 21 is not particularly limited, and examples thereof include copper foil, etc. The detailed structure of the negative electrode current collector 21 is described later. The negative electrode active material layer 22 contains a negative electrode active material, and may further contain a solid electrolyte, a conductive additive, a binder, and the like.
[0035] The negative electrode active material is not particularly limited as long as it can absorb and release lithium ions, and examples thereof include metallic lithium, lithium alloys, metal oxides, metal sulfides, metal nitrides, Si, SiO, carbon materials, etc. Examples of carbon materials include artificial graphite, natural graphite, hard carbon, soft carbon, etc.
[0036] The positive electrode current collector 31 is not particularly limited, and examples thereof include aluminum foil, etc. The detailed structure of the positive electrode current collector 31 is described later. The positive electrode active material layer 32 contains a positive electrode active material, and may further contain a solid electrolyte, a conductive additive, a binder, and the like.
[0037] There is no particular limitation on the positive electrode active material as long as it can absorb and release lithium ions. Examples of the positive electrode active material include LiCoO2, Li(Ni 5 / 10 Co 2 / 10 Mn 3 / 10 )O2、Li(Ni 6 / 10 Co 2 / 10 Mn 2 / 10 )O2、Li(Ni 8 / 10 Co 1 / 10 Mn 1 / 10 )O2、Li(Ni 0.8 Co 0.15 Al 0.05 )O2、Li(Ni 1 / 6 Co 4 / 6 Mn 1 / 6 )O2、Li(Ni 1 / 3 Co 1 / 3 Mn 1 / 3 )O2, LiCoO4, LiMn2O4, LiNiO2, LiFePO4, lithium sulfide, sulfur, etc.
[0038] When the electrolyte layer 40 is a layer having a solid electrolyte, the solid electrolyte is not particularly limited as long as it is a material that can conduct lithium ions. Examples of the solid electrolyte include oxide-based solid electrolytes and sulfide-based solid electrolytes.
[0039] When the electrolyte layer 40 is a layer having an electrolyte, as the electrolyte, for example, a non-aqueous electrolyte containing an organic solvent and a lithium salt can be cited. As the organic solvent, there is no particular limitation, for example, propylene carbonate, ethylene carbonate, diethyl carbonate, etc. can be cited. As the lithium salt, there is no particular limitation, for example, LIPF6, LiBF4, LiClO4, LiCF3SO3 (LiFSI), LiN (SO2F) 2 (LiTFSI), etc. can be cited. When the electrolyte layer 40 is a layer having an electrolyte, it is preferably provided with a separator. The electrolyte may be impregnated in the separator. As the separator, known materials such as non-woven fabrics and microporous films can be used.
[0040] (Current Collector)
[0041] like Figure 1 As shown, the negative electrode current collector 21 as a current collector has a non-opposing portion 21a1 that is not opposed to the negative electrode active material layer 22, and an opposing portion 21b1 that is opposed to the negative electrode active material layer 22 in the stacking direction D1. The thickness of the negative electrode current collector 21 in the stacking direction D1 is different at different locations in the direction D2 (hereinafter referred to as "orthogonal direction D2") orthogonal to the stacking direction D1. In the present embodiment, the negative electrode current collector 21 is inclined in a manner that expands from the end 21b on the opposing portion 21b1 side to the end 21a on the non-opposing portion 21a1 side. As a result, the thickness of the negative electrode current collector 21 changes continuously in a manner that increases from the end 21b on the opposing portion 21b1 side toward the end 21a on the non-opposing portion 21a1 side.
[0042] like Figure 1 As shown, the positive electrode current collector 31 as a current collector also has the same structure as the negative electrode current collector 21. That is, the positive electrode current collector 31 has a non-opposing portion 31a1 that is not opposed to the positive electrode active material layer 32, and an opposing portion 31b1 that is opposed to the positive electrode active material layer 32 in the stacking direction D1. The thickness of the positive electrode current collector 31 changes continuously in a manner of increasing thickness from the end 31b on the opposing portion 31b1 side toward the end 31a on the non-opposing portion 31a1 side. In this embodiment, the non-opposing portion 21a1 and the non-opposing portion 31a1 are respectively formed on different end sides in the orthogonal direction D2. As a result, it is easy to form the secondary battery 10a in a manner in which the thickness of the secondary battery 10a in the orthogonal direction D2 is uniform.
[0043] The non-opposing portions 21a1 and 31a1 are electrically connected to the collector tabs or the lead tabs. Therefore, the ends 21a and 31a are the ends on the side where the current flows in and out of the secondary battery 10a. That is, by configuring the negative electrode collector 21 and the positive electrode collector 31 so that the thickness of the ends on the side where the current flows in and out is relatively thick, the current density distribution of the secondary battery 10a can be reduced. The reason is described below.
[0044] Figure 2 1 is a diagram schematically showing the structure of a conventional secondary battery 100. The secondary battery 100 includes a negative electrode current collector 20, an electrode body 4, and a positive electrode current collector 30. The electrode body 4 is a layer in which the negative electrode active material layer, the electrolyte layer, and the positive electrode active material layer are stacked. The thickness of the negative electrode current collector 20 and the positive electrode current collector 30 in the stacking direction D1 is equal at all locations in the orthogonal direction D2.
[0045] Figure 2 The symbol "Rc1" in the figure means the resistance value per unit length of the negative electrode current collector. The symbol "Rc2" means the resistance value per unit length of the positive electrode current collector. The symbol "Rele" means the resistance value per unit length of the electrode body 4. Figure 2 The resistance value of the current path C1 is set to Rc2+Rele+Rc1×5. Similarly, the resistance value of the current path C2 is set to Rc2×5+Rele+Rc1. Here, the materials of the collectors in the positive electrode and the negative electrode are different, so the resistance values of Rc1 and Rc2 are different. Assuming the case of Rc1<Rc2, the resistance of the current path C1 becomes <the resistance of the current path C2. Therefore, it is considered that the current is easily concentrated in the current path C1, causing current density distribution. In the case of causing current density distribution, there is a possibility of problems such as uneven formation of dendrites in metal lithium batteries.
[0046] Here, the secondary battery 10a of this embodiment is configured such that the thickness of the end portions 21a and 31a of the negative electrode current collector 21 and the positive electrode current collector 31 on the side where current flows in and out is thicker than the end portions 21b and 31b. As a result, the resistance near the side where current flows in and out of the current collector is relatively low, so that, for example, Figure 1 In the case of Rc1<Rc2, current easily flows in the direction D2 perpendicular to the positive electrode current collector 31. Thus, the current density distribution of the secondary battery 10a is reduced.
[0047] The difference between the thickness of end 21a and end 21b, and the difference between the thickness of end 31a and end 31b, i.e., the thickness difference α, varies depending on the materials constituting the negative electrode collector 21 and the positive electrode collector 31, and is preferably greater than 10 μm, and more preferably greater than 20 μm.
[0048] The length of the negative electrode collector 21 and the positive electrode collector 31 in the orthogonal direction D2 varies depending on the material constituting the negative electrode collector 21 and the positive electrode collector 31, and is not particularly limited, and is preferably 500 mm or more, for example. The reason is that the longer the length of the negative electrode collector 21 and the positive electrode collector 31 in the orthogonal direction D2, the easier it is to generate the current density distribution of the secondary battery 10a. According to the configuration of this embodiment, the current density distribution of the secondary battery 10a can be reduced.
[0049] Figure 3 This is a diagram showing a simulation model for performing current allowable calculation on the secondary battery 10 a of the present embodiment using an electrochemical model (Newman model basis) and a 2D finite element method. Figure 3 and Figure 1 The configuration of each component corresponds to. Figure 3 , the negative electrode current collector 21 is made of copper, and the thickness on the end 21b side is 5μm. The negative electrode active material layer 22 is a metal lithium layer, and the thickness is 26.8μm. The electrolyte layer 40 is a solid electrolyte layer, and the thickness is 20μm. The thickness of the positive electrode active material layer 32 is 80μm. The material of the positive electrode current collector 31 is aluminum, and the thickness on the end 31b side is 7.5μm. Current is applied from the end 31a (equivalent to 1.7C). Current is drawn from the end 21a and grounded. COMSOL Multiphysics (registered trademark) can be used as the current extraction analysis software.
[0050] Figure 4 is Figure 3 Under the simulation conditions of , a graph showing the relationship between the thickness difference α and the maximum current density in the negative electrode active material layer 22 when the difference between the thickness of the end 21a and the thickness of the end 21b and the difference between the thickness of the end 31a and the thickness of the end 31b, that is, the thickness difference α, is set to 0 μm, 5 μm, 10 μm, and 20 μm, respectively. A larger maximum current density means a larger current density distribution in the negative electrode active material layer 22.
[0051] Figure 3 Table 1 below shows the relationship between the thickness difference α and the current density in the electrolyte layer 40 when the thickness difference α is 0 μm, 5 μm, 10 μm, and 20 μm in the simulation conditions.
[0052] [Table 1]
[0053]
[0054]
[0055] like Figure 4 As shown in Table 1, the thicker the thickness difference α is, the higher the effect of reducing the current density distribution in the electrode body 4 is, especially in Figure 3 Under the simulation conditions of , by setting the thickness difference α to be greater than 10 μm, the current density distribution in the electrode body 4 can be preferably reduced.
[0056] As a manufacturing method of the secondary battery 10a, the current collector of the above embodiment is used as the current collector, and there is no particular limitation thereto, and a known method can be used. For example, a method can be cited, including: a step of arranging an electrode composite material containing an electrode active material on the surface of the current collector by a wet method or a dry method to form an electrode layer; a step of stacking an electrolyte layer and an electrode layer to obtain a stack; and a step of punching the stack.
[0057] like Figure 1 As shown, the secondary battery 1 includes a secondary battery 10a and a secondary battery 10b as the minimum unit secondary batteries. When a plurality of minimum unit secondary batteries are stacked to form a secondary battery, the electrode body 4 may be arranged on the side of another adjacent secondary battery as in the secondary battery 10b.
[0058] The secondary battery 1 is housed in an outer casing. The outer casing is not particularly limited, and examples thereof include laminated films.
[0059] like Figure 1 As shown, the secondary battery 1 is a stack of a plurality of negative electrode collectors 21 and a positive electrode collector 31 sandwiching an electrode body 4. The top and bottom of the stacking direction D1 of the stacked plurality of minimum units of the secondary battery 1 are preferably parallel. Thus, the length of the stacking direction D1 of the secondary battery 1 is equal in all parts of the orthogonal direction D2. Therefore, it is easy to configure the minimum unit of the secondary battery 1 without gaps, and the shape of the secondary battery 1 is also easy to fit the configuration space. As a result, the energy efficiency per unit volume of the secondary battery 1 can be improved.
[0060] The following example illustrates a configuration in which the upper and lower sides of a stacked secondary battery 1 are parallel in the stacking direction D1. The negative electrode collector 21 and the positive electrode collector 31 have a region with a smaller thickness and a larger region in the stacking direction D1, and are trapezoidal in cross-section. Therefore, for example, the negative electrode collector 21 and the positive electrode collector 31 are arranged in a manner that the non-opposing portion 21a1 and the different end sides of the orthogonal direction D2 of the non-opposing portion 31a1 are alternately arranged. The multiple negative electrode collectors 21 preferably have the same direction in which the thickness increases. And the rates of change of the thickness in the orthogonal direction D2 are preferably equal. The multiple negative electrode collectors 21 can have the same shape. Similarly, the multiple positive electrode collectors 31 preferably have the same direction in which the thickness increases. And the rates of change of the thickness in the orthogonal direction D2 are preferably equal. The multiple positive electrode collectors 31 can have the same shape. In addition, the shape of the electrode body 4 is set to be a parallelogram in cross section corresponding to the shapes of the negative electrode collector 21 and the positive electrode collector 31. However, the thickness of the negative electrode active material layer 22, the electrolyte layer 40, and the positive electrode active material layer 32 in the stacking direction D1 is preferably uniform in the orthogonal direction D2. With the above configuration, the upper and lower surfaces of the stacking direction D1 of a plurality of stacked secondary batteries of the secondary battery 1 can be made parallel.
[0061] As mentioned above, although the preferred embodiment of the present invention has been described, the present invention is not limited to the above embodiment, and modifications and improvements within the scope that can achieve the object of the present invention are included in the present invention.
[0062] Reference numerals
[0063] 1 Secondary battery
[0064] 10a, 10b Secondary battery (smallest unit of secondary battery)
[0065] 21 negative electrode current collector (current collector)
[0066] 21a1 Non-opposing part
[0067] 21b1 relative part
[0068] 31 positive electrode current collector (current collector)
[0069] 31a1 Non-opposing part
[0070] 31b1 Relative part
[0071] D1 stacking direction
Claims
1. A secondary battery comprising an electrode layer and an electrolyte layer, and The electrode layer comprises an electrode active material and a current collector. The current collector has a region having different thickness in a stacking direction, in a direction perpendicular to a stacking direction of the electrode layer and the electrolyte layer. 2 . The secondary battery according to claim 1 , wherein a thickness of the current collector changes continuously from one end portion toward the other end portion in a direction perpendicular to the stacking direction.
3. The secondary battery according to claim 1 or 2, wherein the current collector has a facing portion facing the electrode active material layer containing the electrode active material and a non-facing portion not facing the electrode active material layer in a direction orthogonal to the stacking direction, The thickness of the non-opposing portion is thicker than the thickness of the opposing portion.
4. The secondary battery according to claim 2, wherein a plurality of sets of the electrode layer and the electrolyte layer are stacked. The current collector is composed of a negative electrode current collector and a positive electrode current collector, and is arranged in a manner that a region with a smaller thickness in the stacking direction and a region with a larger thickness in the stacking direction are alternately arranged in the stacking direction. The directions in which the thicknesses of the plurality of negative electrode current collectors increase are in the same direction, The directions in which the thicknesses of the plurality of positive electrode current collectors increase are the same direction.
5. The secondary battery according to claim 2, wherein a plurality of sets of the electrode layer and the electrolyte layer are stacked. The current collector is composed of a negative electrode current collector and a positive electrode current collector, and is arranged in a manner that a region with a smaller thickness in the stacking direction and a region with a larger thickness in the stacking direction are alternately arranged in the stacking direction. The thickness change rates of the plurality of negative electrode current collectors in a direction perpendicular to the stacking direction are equal to each other. The thickness change rates of the plurality of positive electrode current collectors in a direction perpendicular to the stacking direction are equal.