Electrode assembly and secondary battery

By arranging a transition zone and an insulating layer on the current collector of the electrode assembly, the problem of the active material layer falling off when the electrode lug is cut and the risk of short-circuit explosion when the secondary battery vibrates is solved, achieving more efficient battery assembly manufacturing and safe use. .

CN118738409APending Publication Date: 2024-10-01CONTEMPORARY AMPEREX TECHNOLOGY CO LTD

Patent Information

Application Number
CN202411146718.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2019-08-14
Publication Date
2024-10-01

AI Technical Summary

Technical Problem

During the cutting process of electrode ears, the active material layer easily falls off, resulting in material waste and increased costs. At the same time, the force of vibration of the secondary battery may cause the active material layer to fall off, increasing the risk of short circuit and explosion.

Method used

An electrode assembly is designed, in which a transition zone is set on the current collector of the first pole piece and the second pole piece to prevent the tool from directly acting on the active material layer, and the insulating layer reduces the transmission force and overlap area, reducing the risk of falling off. .

Benefits of technology

It effectively avoids the active material layer from falling off during the cutting process, reduces the risk of short circuit and explosion, and improves the safety and efficiency of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118738409A_ABST
    Figure CN118738409A_ABST
Patent Text Reader

Abstract

The invention relates to an electrode assembly and a secondary battery. The electrode assembly comprises a first pole piece, a second pole piece and a diaphragm, and the diaphragm separates the first pole piece from the second pole piece. The first pole piece comprises a first current collector and a first active material layer, the first current collector comprises a first main body part and a first tab, and the first tab extends from the first main body part along one longitudinal end; the first main body part comprises a first coating area and a first transition area, and the first transition area is arranged between the first tab and the first coating area; the first active material layer is coated on the surface of the first coating area, and the first transition area and the first tab are not coated with the first active material layer. The second pole piece comprises a second current collector and a second active substance layer, the second current collector comprises a second main body part and a second tab, the second tab extends from the second main body part along one longitudinal end, and the second active substance layer is coated on the surface of the second main body part. The edge, away from the first coating area, of the first transition area does not exceed the edge of the second active material layer and is the cutting edge of the first tab.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of batteries, and in particular to an electrode assembly and a secondary battery. Background Art

[0002] The electrode assembly of a secondary battery includes a pole piece and a diaphragm, and the pole piece includes a current collector and an active material layer coated on the surface of the current collector. In order to facilitate electrical connection with the electrode terminal of the secondary battery, a pole ear is usually cut out on the current collector. Before cutting the pole ear, the current collector has a coated area coated with an active material layer and an uncoated area not coated with the active material layer, and the pole ear is formed by cutting the uncoated area. In the process of cutting the pole ear, the tool can easily act on the active material layer, causing the risk of the active material layer falling off, resulting in material waste. Summary of the invention

[0003] In view of the problems existing in the background technology, the object of the present invention is to provide an electrode assembly and a secondary battery.

[0004] In order to achieve the above objectives, the present invention provides an electrode assembly and a secondary battery.

[0005] The electrode assembly includes a first pole piece, a second pole piece and a diaphragm, and the diaphragm separates the first pole piece from the second pole piece. The first pole piece includes a first current collector and a first active material layer, and the first current collector includes a first main body and a first pole ear, and the first pole ear extends from one end of the first main body in the longitudinal direction. The first main body includes a first coating area and a first transition area, and the first transition area is arranged between the first pole ear and the first coating area; the first active material layer is coated on the surface of the first coating area, and the first transition area and the first pole ear are not coated with the first active material layer. The second pole piece includes a second current collector and a second active material layer, and the second current collector includes a second main body and a second pole ear, and the second pole ear extends from one end of the second main body in the longitudinal direction, and the second active material layer is coated on the surface of the second main body. Along the direction from the first main body to the first pole ear, the edge of the first transition area away from the first coating area does not exceed the edge of the second active material layer.

[0006] The first pole piece is a positive pole piece, the second pole piece is a negative pole piece, and along the direction from the first main body portion to the first pole ear, the edge of the second active material layer exceeds the edge of the first active material layer.

[0007] Along the direction from the first main body portion to the first electrode tab, the edge of the first transition region exceeds the edge of the first active material layer by at least 0.5 mm.

[0008] The first pole piece further includes an insulating layer, which is at least partially coated on the surface of the first transition region.

[0009] The insulating layer includes a first portion and a second portion, wherein the first portion is coated on the surface of the first transition region, and the second portion extends from the first portion and is coated on the surface of the first electrode tab.

[0010] Along the direction from the first main body portion to the first electrode tab, an edge of the second portion away from the first portion exceeds an edge of the second active material layer.

[0011] Along the direction from the first main body portion to the first electrode tab, an edge of the second portion away from the first portion exceeds an edge of the second active material layer by 0.3 mm to 14 mm.

[0012] The hardness of the insulating layer is greater than the hardness of the first current collector.

[0013] The insulating layer comprises an inorganic filler and a binder, and the weight ratio of the inorganic filler to the binder is 0.4-6.5.

[0014] The first pole tab and the second pole tab are located on the same side of the electrode assembly in the longitudinal direction. The second active material layer includes a substrate area and a thinning area extending from the substrate area, and the thickness of the thinning area is less than the thickness of the substrate area. In the longitudinal direction, the thinning area is connected to the side of the substrate area close to the second pole tab. The second pole piece also includes a third active material layer, which is coated on the surface of the second pole tab and connected to the thinning area. Along the direction from the thinning area to the third active material layer, the size of the third active material layer is larger than the size of the thinning area.

[0015] The second main body includes a second coating area and a second transition area, wherein the second transition area is disposed between the second tab and the second coating area. The second active material layer is coated on the surface of the second coating area, and the second transition area is not coated with the second active material layer.

[0016] The secondary battery includes the electrode assembly.

[0017] The beneficial effects of the present invention are as follows: By setting a first transition zone on the current collector, the present application can prevent the first active material layer from falling off during the cutting of the first pole ear. At the same time, the first transition zone can also reduce the force transmitted to the first active material layer when the secondary battery vibrates, reducing the risk of the first active material layer falling off. In addition, the present application can also reduce the overlapping area of ​​the first transition zone and the second active material layer, reduce the probability of impurities falling between the two, and reduce the risk of contact and short circuit between the two. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 is a schematic diagram of a secondary battery according to the present invention.

[0019] Figure 2 FIG. 1 is a schematic diagram of a first embodiment of an electrode assembly according to the present invention.

[0020] Figure 3 for Figure 2 A cross-sectional view of the electrode assembly taken along line AA.

[0021] Figure 4 for Figure 2 A cross-sectional view of the electrode assembly taken along line BB.

[0022] Figure 5 for Figure 4 An enlarged view of the electrode assembly at box C.

[0023] Figure 6 for Figure 4 An enlarged view of the electrode assembly at box D.

[0024] Figure 7 for Figure 4 Schematic diagram of the first pole piece in the unfolded state.

[0025] Figure 8 for Figure 7 Schematic diagram of the first current collector of the first pole piece.

[0026] Fig. 9 for Figure 7 Schematic diagram of the first pole piece during the forming process.

[0027] Fig.10 for Figure 4 Schematic diagram of the second pole piece in the unfolded state.

[0028] Fig.11 for Fig.10 Schematic diagram of the second current collector of the second pole piece.

[0029] Fig.12 is a schematic diagram of a second embodiment of an electrode assembly according to the present invention.

[0030] Fig.13 for Fig.12 A cross-sectional view of the electrode assembly taken along line EE.

[0031] Fig.14 for Fig.13 An enlarged view of the electrode assembly at box F.

[0032] Fig.15 for Fig.13 Schematic diagram of the second pole piece in the unfolded state.

[0033] Fig.16 FIG. 4 is a schematic diagram of a third embodiment of an electrode assembly according to the present invention.

[0034] Fig.17 for Fig.16 An enlarged view of the electrode assembly at box G.

[0035] Fig.18 for Fig.16 Schematic diagram of the second pole piece in the unfolded state.

[0036] The reference numerals are described as follows:

[0037] 1First pole piece

[0038] 11 The first fluid collector

[0039] 111 First main body

[0040] 111a First coating area

[0041] 111b First transition zone

[0042] 112 First Tab

[0043] 12First active material layer

[0044] 13 Insulation layer

[0045] 131 Part 1

[0046] 132 Part 2

[0047] 2 Second pole piece

[0048] 21 Second Collection

[0049] 211 Second Main Body

[0050] 211a Second coating area

[0051] 211b Second transition zone

[0052] 212 Second tab

[0053] 22 Second active material layer

[0054] 221 matrix area

[0055] 222 Thinning area

[0056] 23Third active material layer

[0057] 3 Diaphragm

[0058] 4-electrode assembly

[0059] 5 Shell

[0060] 6 Top cover

[0061] 7-electrode terminal

[0062] 8 Current collecting components

[0063] X vertical

[0064] Y horizontal

[0065] Z thickness direction DETAILED DESCRIPTION

[0066] In order to make the purpose, technical solution and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application.

[0067] In the description of this application, unless otherwise clearly specified and limited, the terms "first", "second", and "third" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance; the term "plurality" refers to more than two (including two); unless otherwise specified or explained, the term "connection" should be understood in a broad sense, for example, "connection" can be a fixed connection, a detachable connection, an integral connection, an electrical connection, or a signal connection; "connection" can be a direct connection or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0068] In the description of this specification, it should be understood that the directional words such as "upper" and "lower" described in the embodiments of the present application are described from the perspectives shown in the drawings and should not be understood as limiting the embodiments of the present application. The present application is further described in detail below through specific embodiments and in conjunction with the drawings.

[0069] Reference Figure 1 The secondary battery of the present application includes an electrode assembly 4 , a shell 5 , a top cover plate 6 , an electrode terminal 7 and a current collecting member 8 .

[0070] The electrode assembly 4 is the core component of the secondary battery to realize the charging and discharging functions. Figure 2 and Figure 3 The electrode assembly 4 includes a first electrode plate 1, a second electrode plate 2 and a diaphragm 3, and the diaphragm 3 separates the first electrode plate 1 and the second electrode plate 2.

[0071] The electrode assembly 4 may be a wound structure. Specifically, the first pole piece 1 and the second pole piece 2 are each one, and the first pole piece 1 and the second pole piece 2 are strip structures. The first pole piece 1, the diaphragm 3 and the second pole piece 2 are stacked in sequence and wound more than two times to form the electrode assembly 4. The electrode assembly 4 may be flat.

[0072] Alternatively, the electrode assembly 4 may also be a laminated structure. Specifically, a plurality of first pole sheets 1 and a plurality of second pole sheets 2 are provided, the plurality of first pole sheets 1 and second pole sheets 2 are alternately stacked, and the diaphragm 3 separates the first pole sheet 1 and the second pole sheet 2.

[0073] The housing 5 may have a hexahedral shape or other shapes. A receiving cavity is formed inside the housing 5 to accommodate the electrode assembly 4 and the electrolyte. The housing 5 has an opening formed at one end, and the electrode assembly 4 can be placed in the receiving cavity of the housing 5 through the opening. The housing 5 may be made of a conductive metal material, preferably, the housing 5 is made of aluminum or an aluminum alloy.

[0074] The top cover plate 6 is disposed on the housing 5 and covers the opening of the housing 5, thereby sealing the electrode assembly 4 in the housing 5. The top cover plate 6 may be a metal plate and is connected to the housing 5 by welding. There are two electrode terminals 7 and are disposed on the top cover plate 6. There are two current collecting members 8, one current collecting member 8 connects one electrode terminal 7 and the first pole piece 1 of the electrode assembly 4, and the other current collecting member 8 connects the other electrode terminal 7 and the second pole piece 2 of the electrode assembly 4.

[0075] The electrode assembly of the present application is described below with reference to different embodiments.

[0076] In the first embodiment, referring to Figures 4 to 6 The first pole piece 1 includes a first current collector 11 and a first active material layer 12. The first current collector 11 includes a first main body 111 and a first pole ear 112. The first pole ear 112 extends from one end of the first main body 111 along the longitudinal direction X. The first active material layer 12 is coated on the surface of the first main body 111. The first pole piece 1 can be a positive pole piece. Correspondingly, the first current collector 11 is an aluminum foil, and the first active material layer 12 includes a ternary material, lithium manganate or lithium iron phosphate. There can be multiple first pole ears 112. After the first pole piece 1 is wound and formed, multiple first pole ears 112 are stacked together and welded to the current collecting component 8.

[0077] The second pole piece 2 includes a second current collector 21 and a second active material layer 22. The second current collector 21 includes a second main body 211 and a second pole ear 212. The second pole ear 212 extends from one end of the second main body 211 along the longitudinal direction X, and the second active material layer 22 is coated on the surface of the second main body 211. The second pole piece 2 can be a negative pole piece. Correspondingly, the second current collector 21 is a copper foil, and the second active material layer 22 includes graphite or silicon. There can be multiple second pole ears 212. After the second pole piece 2 is wound and formed, multiple second pole ears 212 are stacked together and welded to the current collecting member 8.

[0078] In this embodiment, refer to Figure 2 The first electrode tab 112 and the second electrode tab 212 are respectively located on both sides of the electrode assembly 4 along the longitudinal direction X.

[0079] During the use of the battery, the lithium ions in the first active material layer 12 pass through the diaphragm 3 and are embedded in the second active material layer 22. In order to ensure that the lithium ions can be embedded in the second active material layer 22 as much as possible and reduce the risk of lithium plating, the second active material layer 22 needs to have a larger width. Specifically, both ends of the second active material layer 22 along the longitudinal direction X exceed the first active material layer 12. In other words, along the direction from the first main body 111 to the first pole ear 112, an edge T2 of the second active material layer 22 close to the first pole ear 112 exceeds an edge of the first active material layer 12 close to the first pole ear 112; along the direction from the first pole ear 112 to the first main body 111, another edge of the second active material layer 22 away from the first pole ear 112 exceeds another edge of the first active material layer 12 away from the first pole ear 112.

[0080] During the forming process of the first pole piece 1, it is necessary to form the first pole ear 112 on the first current collector 11 by cutting. If cutting is performed along the edge of the first active material layer 12, the tool can easily act on the first active material layer 12 due to process errors, causing the active material in the first active material layer 12 to fall off, resulting in material waste. Relatively speaking, the active material in the first active material layer 12 is relatively expensive, so cutting along the edge of the first active material layer 12 will result in a high cost of the first pole piece 1.

[0081] In order to prevent the cutter from acting on the first active material layer 12, the present application increases the size of the first main body 111 along the longitudinal direction X to increase the distance between the first active material layer 12 and the first electrode tab 112 in the longitudinal direction X. Fig. 9 The first main body 111 includes a first coating area 111a and a first transition area 111b, and the first transition area 111b is arranged between the first electrode tab 112 and the first coating area 111a; the first active material layer 12 is coated on the surface of the first coating area 111a, and the first transition area 111b and the first electrode tab 112 are not coated with the first active material layer 12.

[0082] Fig. 9 The dotted line shows the movement trajectory of the tool during the process of cutting the first electrode tab 112. During the process of cutting the first electrode tab 112, a certain distance is maintained between the tool and the first active material layer 12 to avoid the tool from acting on the first active material layer 12 due to process errors and prevent the active material of the first active material layer 12 from falling off. Figure 7 and Figure 8 After the cutting is completed, a first transition area 111 b not coated with the first active material layer 12 is formed on the first main body 111 .

[0083] When the secondary battery vibrates, the current collecting member 8 will pull the first main body 111 through the first pole ear 112. If there is no first transition zone 111b, stress concentration will occur at the root of the first pole ear 112, and the first active material layer 12 near the root of the first pole ear 112 is easy to fall off. However, by providing the first transition zone 111b, the present application can reduce the force transmitted to the first active material layer 12 and reduce the risk of the active material in the first active material layer 12 falling off.

[0084] After the electrode assembly 4 is wound, the first pole piece 1 and the second pole piece 2 are stacked together. The surface of the first coating area 111a is coated with the first active material layer 12, so the gap between the first coating area 111a and the second active material layer 22 of the second pole piece 2 is small; while the first transition area 111b is not coated with the first active material layer 12, so the gap between the first transition area 111b and the second active material layer 22 of the second pole piece 2 is large.

[0085] Impurities (such as metal particles, etc.) are generated during the welding process between the first pole tab 112 and the current collecting member 8, and since the gap between the first transition region 111b and the second active material layer 22 is relatively large, the impurities are easily dropped into the gap. During the charging and discharging process, the first pole piece 1 and the second pole piece 2 will expand, and the expansion may squeeze the impurities dropped into the gap, so that the impurities pierce the diaphragm 3, causing the risk of short circuit.

[0086] Preferably, refer to Figure 5 , along the direction from the first main body 111 to the first pole ear 112, the edge T1 of the first transition zone 111b away from the first coating zone 111a does not exceed the edge T2 of the second active material layer 22. In this way, the overlapping area of ​​the first transition zone 111b and the second active material layer 22 can be reduced, thereby reducing the risk of contact and short circuit between the two. At the same time, the present application also reduces the size of the gap between the first transition zone 111b and the second active material layer 22 along the longitudinal direction X, thereby reducing the risk of impurities falling into the gap. In addition, in the longitudinal direction X, the edge T1 of the first transition zone 111b shrinks into the second active material layer 22, thereby reducing the risk of impurities adsorbed by the edge T1.

[0087] During the process of cutting the first electrode tab 112 , burrs may be generated on the edge T1 of the first transition region 111 b away from the first coating region 111 a , and the burrs may easily pierce the separator 3 .

[0088] During the use of the battery, lithium ions in the first active material layer 12 pass through the separator 3 and are embedded in the second active material layer 22. If the burrs on the edge T1 of the first transition zone 111b contact the lithium-embedded area of ​​the second active material layer 22, a large amount of heat will be generated instantly, causing an explosion risk. If the burrs on the edge T1 of the first transition zone 111b contact the non-lithium-embedded area of ​​the second active material layer 22, less heat will be generated, and the safety risk will be lower.

[0089] During the use of the battery, the lithium ions in the first active material layer 12 diffuse freely to the surroundings. Therefore, in the longitudinal direction X, the size of the lithium-embedded area of ​​the second active material layer 22 is slightly larger than the size of the first active material layer. In order to reduce safety risks, along the direction from the first main body 111 to the first pole ear 112, the edge of the first transition zone 111b exceeds the edge of the first active material layer 12 by at least 0.5mm. In other words, in the longitudinal direction X, the size of the first transition zone 111b is greater than or equal to 0.5mm. At this time, even if the burrs on the edge T1 of the first transition zone 111b pierce the diaphragm 3, they will only contact the non-lithium-embedded area of ​​the second active material layer 22, thereby avoiding explosion and reducing safety risks.

[0090] Reference Figure 5 and Figure 7 The first pole piece 1 further includes an insulating layer 13, which is at least partially coated on the surface of the first transition region 111b. The insulating layer 13 can be filled into the gap between the first transition region 111b and the second active material layer 22 of the second pole piece 2, thereby reducing impurities falling into the gap and further reducing the risk of short circuit. Furthermore, coating the insulating layer 13 in the first transition region 111b can also prevent the first transition region 111b from being electrically connected to the second active material layer 22 of the second pole piece 2 through metal impurities.

[0091] The insulating layer 13 includes a first portion 131 and a second portion 132. The first portion 131 is coated on the surface of the first transition region 111b, and the second portion 132 extends from the first portion 131 and is coated on the surface of the first electrode tab 112. Preferably, the first portion 131 completely covers the surface of the first transition region 111b.

[0092] The first portion 131 can be filled into the gap between the first transition region 111b and the second active material layer 22 of the second pole piece 2, thereby reducing impurities falling into the gap and further reducing the risk of short circuit. Furthermore, coating the first portion 131 on the surface of the first transition region 111b can also prevent the first transition region 111b from being electrically connected to the second active material layer 22 of the second pole piece 2 through metal impurities.

[0093] Reference Fig. 9In the process of forming the first electrode sheet 1, the first active material layer 12 and the insulating layer 13 are first coated on the surface of the first current collector 11, and then the first electrode tab 112 is cut out. The insulating layer 13 is generally coated with equal width. If the second portion 132 is not retained on the first electrode tab 112, the tool needs to move along the edge of the insulating layer 13 when cutting the first electrode tab 112, which requires high cutting accuracy and is difficult to achieve; in addition, after cutting, the burrs on the edge T1 of the first transition zone 111b are large and easy to puncture the diaphragm 3.

[0094] Therefore, in the process of cutting the first pole tab 112, the present application directly acts on the insulating layer 13 with the cutter. After the cutting is completed, the insulating layer 13 forms a first portion 131 remaining on the first transition region 111b and a second portion 132 remaining on the first pole tab 112. In addition, when the cutter cuts on the insulating layer 13, the burrs on the edge T1 of the first transition region 111b can be effectively reduced, thereby reducing the risk of the diaphragm 3 being punctured.

[0095] Reference Figure 5 , along the direction from the first main body 111 to the first pole ear 112, the edge T3 of the second portion 132 away from the first portion 131 exceeds the edge T2 of the second active material layer 22. The second portion 132 can be filled into the gap between the first pole ear 112 and the second active material layer 22, thereby reducing impurities falling into the gap and reducing the risk of short circuit. Furthermore, the second portion 132 can also reduce the risk of the burrs on the edge of the first pole ear 112 being electrically connected to the second active material layer 22 after piercing the diaphragm 3.

[0096] There are multiple first pole ears 112 and they are arranged in layers. The multiple first pole ears 112 are gathered together and welded to the current collecting member 8. In the process of gathering the first pole ears 112, the roots of some first pole ears 112 close to the first transition zone 111b are easily bent, causing the roots of these first pole ears 112 to be inserted between the first pole sheet 1 and the second pole sheet 2, causing the risk of short circuit. The second part 132 of the present application can support the first pole ear 112 and reduce the risk of bending at the root of the first pole ear 112. In addition, since the edge T3 of the second part 132 exceeds the edge T2 of the second active material layer 22, even if the first pole ear 112 is bent in the area not coated with the second part 132, a certain distance is maintained between the bent position and the second active material layer 22, and the risk of the first pole ear 112 contacting the second active material layer 22 is low.

[0097] Along the direction from the first main body 111 to the first pole tab 112, the edge T3 of the second portion 132 away from the first portion 131 exceeds the edge of the second active material layer 22 by 0.3 mm to 14 mm. If the edge T3 of the second portion 132 exceeds the edge T2 of the second active material layer 22 by less than 0.3 mm, when the first pole tab 112 is bent in the area not coated with the second portion 132, the distance between the bent position and the second active material layer 22 is small, and there is still a risk of contact between the first pole tab 112 and the second active material layer 22. If the edge T3 of the second portion 132 exceeds the edge T2 of the second active material layer 22 by more than 14 mm, the first pole tab 112 is less bendable, occupies a large space, and affects the energy density of the secondary battery.

[0098] The hardness of the insulating layer 13 is greater than the hardness of the first current collector 11. The insulating layer 13 with high hardness can effectively support the first electrode tab 112 and prevent the root of the first electrode tab 112 near the first transition region 111b from bending.

[0099] The insulating layer 13 includes an inorganic filler and a binder, and the weight ratio of the inorganic filler to the binder is 4.1-9.6. If the ratio is greater than 9.6, the adhesion between the inorganic fillers and the bonding strength between the insulating layer 13 and the first current collector 11 may be insufficient, and the insulating layer 13 is easy to fall off when in contact with the electrolyte. If the ratio is lower than 4.1, the insulating effect of the insulating layer 13 is difficult to meet the requirements; furthermore, the inorganic filler is less and cannot play a role in supporting the first pole ear 112, causing the first pole ear 112 to easily fold during the winding process of the first pole piece 1. The inorganic filler can be selected from one or more of boehmite, Al2O3, SiO2 and TiO2. The binder can be polyvinylidene fluoride.

[0100] In this embodiment, refer to Fig.10 and Fig.11 The second active material layer 22 completely covers the second main body 211. The second electrode 2 also includes a third active material layer 23, which is coated on the surface of the second electrode tab 212 and connected to the second active material layer 22. The second active material layer 22 and the third active material layer 23 are integrally formed.

[0101] Specifically, graphite, conductive agent acetylene black, thickener CMC, and binder SBR can be mixed, solvent deionized water is added, and the negative electrode slurry is formed by stirring, and then the negative electrode slurry is applied to the surface of the second current collector 21. After the negative electrode slurry is solidified, a negative electrode active material layer is formed, and then the second pole ear 212 is cut out. During cutting, the cutter can act directly on the negative electrode active material layer. After cutting, the portion of the negative electrode active material layer retained on the second main body 211 is the second active material layer 22, and the portion of the negative electrode active material layer retained on the second pole ear 212 is the third active material layer 23. Cutting on the negative electrode active material layer can reduce the burrs at the cutting point and reduce the risk of the diaphragm 3 being punctured. In addition, relatively speaking, the active material of the negative electrode active material layer is relatively cheap, so part of the negative electrode active material layer can be directly cut off.

[0102] Other embodiments of the electrode assembly of the present application are described below. In order to simplify the description, only the differences between other embodiments and the first embodiment are mainly introduced below, and the parts not described can be understood with reference to the first embodiment.

[0103] Reference Figures 12 to 15 In the second embodiment, the first electrode tab 112 and the second electrode tab 212 are located on the same side of the electrode assembly along the longitudinal direction X.

[0104] During the molding process of the second pole piece 2, the second active material layer 22 is usually cold pressed to increase the density of the second active material layer 22. During cold pressing, stress concentration is easily generated at the end of the second active material layer 22 close to the second pole tab 212, causing the risk of the second current collector 21 breaking.

[0105] Preferably, the second active material layer 22 includes a base region 221 and a thinned region 222 extending from the base region 221, and the thickness of the thinned region 222 is less than the thickness of the base region 221. In the longitudinal direction X, the thinned region 222 is connected to a side of the base region 221 close to the second electrode tab 212. Preferably, the thickness of the thinned region 222 gradually decreases in a direction away from the base region 221.

[0106] In the present application, by reducing the thickness of the thinned area 222 , during the cold pressing process of the second pole piece 2 , stress concentration at the edge T4 of the thinned area 222 away from the base area 211 can be reduced, thereby avoiding the second current collector 21 from breaking.

[0107] Reference Fig.14, along the direction from the base area 221 to the skived area 222, the edge T1 of the first transition area 111b away from the first coating area 111a exceeds the connection between the base area 221 and the skived area 222, and does not exceed the edge T4 of the skived area 222 away from the base area 221. If the edge T1 of the first transition area 111b does not exceed the connection between the base area 221 and the skived area 222, it will lead to waste of active materials in the skived area 222. Although reducing the thickness of the skived area 222 will increase the gap between the first transition area 111b and the skived area 222, the first portion 131 coated on the first transition area 111b can make up for the safety risk caused by the increase in the gap, so the present application can still meet the requirements.

[0108] In the second embodiment, the third active material layer 23 is connected to the thinning area 222. The thickness of the third active material layer 23 is less than the thickness of the substrate area 221. When cutting the second pole ear 212, the larger the size of the third active material layer 23 along the longitudinal direction X, the smaller the size of the thinning area 222 along the longitudinal direction X. The present application can reduce the overlapping area of ​​the second active material layer 22 and the first transition area 111b by reducing the size of the thinning area 222, thereby reducing the risk of short circuit. By increasing the size of the third active material layer 23, the probability of bending at the root of the second pole ear 212 can be reduced, thereby reducing the risk of short circuit. Taking all factors into consideration, along the direction from the thinning area 222 to the third active material layer 23, the size of the third active material layer 23 is larger than the size of the thinning area 222.

[0109] Reference Fig.14 In the longitudinal direction X, the edge T1 of the first transition region 111b shrinks into the second active material layer 22. Therefore, even if the root of the second electrode tab 212 is bent, the risk of contacting the edge T1 of the first transition region 111b is small. Therefore, the present application can effectively reduce the risk of short circuit and improve safety performance.

[0110] Reference Figures 16 to 18 Compared with the first embodiment, the third embodiment can omit the third active material layer 23. Specifically, the second main body 211 includes a second coating area 211a and a second transition area 211b, and the second transition area 211b is arranged between the second electrode 212 and the second coating area 211a. The second active material layer 22 is coated on the surface of the second coating area 211a, and the second transition area 211b is not coated with the second active material layer 22.

[0111] By providing the second transition area 211b, it is possible to prevent the tool from acting on the second active material layer 22 due to process errors. Compared with the first embodiment, the third embodiment can save the second active material layer 22.

[0112] When the secondary battery vibrates, the current collecting member 8 will pull the second main body 211 through the second pole ear 212. If there is no second transition zone 211b, stress concentration will occur at the root of the second pole ear 212, and the second active material layer 22 near the root of the second pole ear 212 is easy to fall off. However, by providing the second transition zone 211b, the present application can reduce the force transmitted to the second active material layer 22 and reduce the risk of the active material in the second active material layer 22 falling off.

Claims

1. An electrode assembly, characterized in that: It comprises a first pole piece (1), a second pole piece (2) and a diaphragm (3), wherein the diaphragm (3) separates the first pole piece (1) from the second pole piece (2); The first pole piece (1) comprises a first current collector (11) and a first active material layer (12); the first current collector (11) comprises a first main body (111) and a first pole tab (112); the first pole tab (112) extends from one end of the first main body (111) along a longitudinal direction (X); The first main body (111) comprises a first coating region (111a) and a first transition region (111b), wherein the first transition region (111b) is arranged between the first pole tab (112) and the first coating region (111a); the first active material layer (12) is coated on the surface of the first coating region (111a), and the first transition region (111b) and the first pole tab (112) are not coated with the first active material layer (12); The second pole piece (2) comprises a second current collector (21) and a second active material layer (22); the second current collector (21) comprises a second main body (211) and a second pole tab (212); the second pole tab (212) extends from one end of the second main body (211) along a longitudinal direction (X); and the second active material layer (22) is coated on a surface of the second main body (211); Along the direction from the first main body (111) to the first pole tab (112), an edge (T1) of the first transition zone (111b) away from the first coating zone (111a) does not exceed the edge of the second active material layer (22), and an edge (T1) of the first transition zone (111b) away from the first coating zone (111a) is a cutting edge for cutting the first pole tab (112).

2. The electrode assembly according to claim 1, characterized in that: The first pole piece (1) is a positive pole piece, the second pole piece (2) is a negative pole piece, and along the direction from the first main body (111) to the first pole ear (112), the edge of the second active material layer (22) exceeds the edge of the first active material layer (12).

3. The electrode assembly according to claim 2, characterized in that: Along the direction from the first main body (111) to the first electrode tab (112), the edge of the first transition region (111b) exceeds the edge of the first active material layer (12) by at least 0.5 mm.

4. The electrode assembly according to any one of claims 1 to 3, characterized in that: The first pole piece (1) further comprises an insulating layer (13), wherein the insulating layer (13) is at least partially coated on the surface of the first transition region (111b).

5. The electrode assembly according to claim 4, characterized in that: The insulating layer (13) comprises a first portion (131) and a second portion (132), wherein the first portion (131) is coated on the surface of the first transition region (111b), and the second portion (132) extends from the first portion (131) and is coated on the surface of the first pole tab (112).

6. The electrode assembly according to claim 5, characterized in that: Along the direction from the first main body (111) to the first electrode tab (112), the edge of the second portion (132) away from the first portion (131) exceeds the edge of the second active material layer (22).

7. The electrode assembly according to claim 6, characterized in that: Along the direction from the first main body (111) to the first electrode tab (112), the edge of the second portion (132) away from the first portion (131) exceeds the edge of the second active material layer (22) by 0.3 mm to 14 mm.

8. The electrode assembly according to claim 4, characterized in that: The hardness of the insulating layer (13) is greater than the hardness of the first current collector (11).

9. The electrode assembly according to claim 4, characterized in that: The insulating layer (13) comprises an inorganic filler and a binder, and the weight ratio of the inorganic filler to the binder is 4.1-9.

6.

10. The electrode assembly according to claim 9, characterized in that: The inorganic filler includes one or more of boehmite, Al2O3, SiO2 and TiO2.

11. The electrode assembly according to claim 9, characterized in that: The binder includes polyvinylidene fluoride.

12. The electrode assembly according to claim 1, characterized in that The first electrode tab (112) and the second electrode tab (212) are located on the same side of the electrode assembly (4) along the longitudinal direction (X); The second active material layer (22) comprises a base region (221) and a thinned region (222) extending from the base region (221), and the thickness of the thinned region (222) is smaller than the thickness of the base region (221); In the longitudinal direction (X), the thinned region (222) is connected to a side of the base region (221) close to the second electrode tab (212); The second pole piece (2) further comprises a third active material layer (23), wherein the third active material layer (23) is coated on the surface of the second pole tab (212) and connected to the thinned area (222).

13. The electrode assembly according to claim 12, characterized in that: Along the direction from the thinned area (222) to the third active material layer (23), the size of the third active material layer (23) is larger than the size of the thinned area (222).

14. The electrode assembly according to claim 12, characterized in that: Along the direction from the first main body (111) to the first electrode tab (112), the edge of the first transition region (111b) away from the first coating region (111a) does not exceed the outer edge of the thinned region (222).

15. The electrode assembly according to claim 12, characterized in that: The first pole piece (1) further comprises an insulating layer (13), the insulating layer (13) being at least partially coated on the surface of the first transition region (111b), the insulating layer (13) comprising a first portion (131) and a second portion (132), the first portion (131) being coated on the surface of the first transition region (111b), and the second portion (132) extending from the first portion (131) and being coated on the surface of the first pole lug (112); Along the direction from the first main body (111) to the first pole tab (112), the outer edge of the thinned area (222) does not exceed the outer edge of the second portion (132).

16. The electrode assembly according to claim 1, characterized in that The first electrode tab (112) and the second electrode tab (212) are respectively located on two sides of the electrode assembly (4) along the longitudinal direction (X).

17. The electrode assembly according to claim 1, characterized in that The second main body (211) comprises a second coating area (211a) and a second transition area (211b), and the second transition area (211b) is arranged between the second electrode tab (212) and the second coating area (211a); The second active material layer (22) is coated on the surface of the second coating area (211a), and the second transition area (211b) is not coated with the second active material layer (22).

18. The electrode assembly according to claim 1, characterized in that Along the direction from the first main body (111) to the first pole lug (112), an edge (T2) of the second active material layer (22) close to the first pole lug (112) exceeds an edge of the first active material layer (12) close to the first pole lug (112); Along the direction from the first electrode tab (112) to the first main body (111), another edge of the second active material layer (22) away from the first electrode tab (112) exceeds another edge of the first active material layer (12) away from the first electrode tab (112).

19. The electrode assembly according to claim 1, characterized in that: The gap between the first transition region (111b) and the second active material layer (22) of the second pole piece (2) is greater than the gap between the first coating region (111a) and the second active material layer (22) of the second pole piece (2).

20. The electrode assembly according to claim 19, characterized in that The first pole piece (1) further comprises an insulating layer (13), wherein the insulating layer (13) is at least partially coated on the surface of the first transition region (111b), and a first portion (131) of the insulating layer (13) is filled into a gap between the first transition region (111b) and the second active material layer (22) of the second pole piece (2).

21. The electrode assembly according to any one of claims 1 to 3 and 5 to 20, characterized in that: The electrode assembly (4) is a laminated structure.

22. The electrode assembly according to claim 21, characterized in that There are a plurality of first pole pieces (1) and a plurality of second pole pieces (2); The first pole piece (1) and the second pole piece (2) are alternately stacked, and the diaphragm (3) separates the first pole piece (1) and the second pole piece (2).

23. The electrode assembly according to claim 22, characterized in that There are a plurality of first pole tabs (112); the plurality of first pole tabs (112) are stacked and arranged, and the plurality of first pole tabs (112) are gathered and welded together.

24. The electrode assembly according to any one of claims 1 to 3 and 5 to 20, characterized in that: The electrode assembly (4) is a wound structure.

25. The electrode assembly according to claim 24, characterized in that The first pole piece (1) and the second pole piece (2) are both one piece, and the first pole piece (1) and the second pole piece (2) are strip-shaped structures; The first pole piece (1), the separator (3) and the second pole piece (2) are stacked and wound more than two times to form an electrode assembly (4).

26. The electrode assembly according to claim 25, characterized in that There are a plurality of first pole tabs (112); after the first pole sheet (1) is wound and formed, the plurality of first pole tabs (112) are stacked and welded together.

27. The electrode assembly according to claim 25, characterized in that There are a plurality of second pole tabs (212); after the second pole sheet (2) is wound and formed, the plurality of second pole tabs (212) are stacked and welded together.

28. The electrode assembly according to any one of claims 1-3 and 5-20, characterized in that: The first current collector (11) is an aluminum foil, and the first active material layer (12) comprises a ternary material, lithium manganese oxide or lithium iron phosphate.

29. A secondary battery, characterized in that: An electrode assembly comprising any one of claims 1-28.

Citation Information

Patent Citations

  • Battery pole piece and preparation method thereof and battery containing same

    CN101662011A

  • Lithium ion secondary battery element and lithium ion secondary battery

    CN109088091A

  • Anode pole piece and electricity core thereof

    CN206250284U

  • Electrode assembly and secondary battery

    CN208819984U

Cited By

  • Secondary battery, preparation method thereof and electronic device

    CN119905642A

  • Secondary battery, method of manufacturing the same, and electronic device

    CN119905642B