Electrode assembly and secondary battery
By using the first adhesive layer in the secondary battery to bond the tabs to the empty foil area, welding burrs are avoided. The tabs are away from the current collector and in contact with the isolation film, solving the problem of welding burrs piercing the isolation film and improving energy density. and anti-collision performance.
Patent Information
- Application Number
- CN202410702746.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-31
- Publication Date
- 2024-10-01
AI Technical Summary
Welding burrs are prone to occur when welding tabs and current collectors in existing secondary batteries, causing the isolation film to be punctured, which in turn causes short-circuit failure of the positive and negative electrode plates. Moreover, the installation of multiple layers of insulating glue affects the energy density.
The first tab is bonded to the first empty foil area through the first glue layer to avoid the occurrence of welding burrs. The first glue layer is arranged between the tab and the current collector. The tab is away from the current collector and contacts the isolation film, saving Remove the insulating glue to improve space utilization.
The risk of puncture of the isolation film is reduced, the energy density and collision resistance of the secondary battery are improved, the cost is reduced, and the connection strength and stability are enhanced.
Smart Images

Figure CN118738780A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of battery technology, and in particular to an electrode assembly and a secondary battery. Background Art
[0002] The tab serves as a bridge for electrically connecting the secondary battery to the external circuit. It is usually made of metal material. The tab is welded to the current collector inside the secondary battery, which allows the tab to be conductive with the electrode assembly inside the secondary battery, thereby achieving the purpose of transmitting current.
[0003] In order to facilitate the welding of the tabs, double-sided empty foil areas are usually required on the current collector, and the welding head and welding seat are respectively in contact with the current collector at the empty foil areas on both sides for welding. However, the welding of the tabs and the empty foil areas of the current collector usually produces some welding burrs, which can easily pierce the isolation film and cause the positive and negative electrodes inside the secondary battery to short-circuit and fail. Summary of the invention
[0004] The purpose of the present application is to provide an electrode assembly and a secondary battery, aiming to improve the technical problem that the current collector is prone to welding burrs and puncture of the isolation membrane.
[0005] According to the first aspect of the present application, an electrode assembly is provided, comprising a first pole piece, a separator and a second pole piece, wherein the separator is arranged between the first pole piece and the second pole piece. The first pole piece comprises a first current collector and a first active material layer, wherein the first current collector has a first surface facing the second pole piece, and the first active material layer is arranged on the first surface. The second pole piece comprises a second current collector and a second active material layer, wherein the second current collector has a second surface facing the first active material layer, and the second active material layer is arranged on the second surface. The electrode assembly also comprises a first pole ear and a first adhesive layer. The first surface has a first empty foil area, wherein the first empty foil area, the first active material layer and the separator are enclosed together to form a first space, wherein the first pole ear is partially arranged in the first space, and the first adhesive layer is arranged on the surface of the first pole ear facing the first current collector, so as to bond the first empty foil area to the first pole ear, wherein the first empty foil area is electrically connected to the first pole ear, and the first pole ear is in contact with the separator away from the first current collector.
[0006] In the above technical solution, the first pole ear is bonded to the first empty foil area through the first adhesive layer. No welding head and welding seat are required, and there are no welding burrs. The risk of the isolation membrane being punctured can be reduced. There is no need to set insulating glue to cover the welding burrs. A layer of insulating glue is omitted, so that the first pole ear can directly contact the isolation membrane, which not only reduces the risk of the isolation membrane being punctured, but also makes full use of the space, thereby facilitating the improvement of the energy density of the secondary battery.
[0007] In some preferred embodiments, the electrode assembly further comprises a second pole ear and a second adhesive layer, the second surface has a second empty foil area, the second empty foil area, the second active material layer and the isolation film are enclosed together to form a second space, the second pole ear is partially arranged in the second space, the second pole ear is partially arranged in the second space, and the second adhesive layer is arranged on the surface of the second pole ear facing the second current collector to bond the second empty foil area to the second pole ear, and the surface of the second pole ear away from the second current collector is in contact with the isolation film. The second pole ear is bonded to the second empty foil area through the second adhesive layer, and does not need to be welded by a welding head and a welding seat, and there is no welding burr, so the fourth surface may also not need to be provided with an empty foil area, and the second pole ear can be directly in contact with the isolation film, and no insulating adhesive layer is required, which can make full use of the space and improve the energy density of the secondary battery.
[0008] In some preferred embodiments, when observed along the thickness direction of the first pole piece, the projection of the first hollow foil area on the second pole piece is located on the second active material layer. Since the first pole tab is bonded to the first hollow foil area through the first adhesive layer, there is no welding burr, and pole piece adhesive does not need to be provided on the second active material layer of the second pole piece, which can further improve the space utilization rate and thus improve the energy density of the secondary battery.
[0009] In some preferred embodiments, a pole piece glue is provided on the surface of the first active material layer facing the second active material layer. When observed along the thickness direction of the second pole piece, the projection of the second empty foil area on the first pole piece is located within the projection of the pole piece glue. The lithium ion deintercalation of the first pole piece at the pole piece glue can be alleviated, so that the second pole piece has sufficient margin to embed the lithium ions deintercalated by the first pole piece, and the lithium plating of the secondary battery can be alleviated, wherein the first pole piece is a positive pole piece and the second pole piece is a negative pole piece.
[0010] In some preferred embodiments, a third space is provided on the surface of the first active material layer facing the second active material layer, and the pole piece glue is at least partially contained in the third space. The pole piece glue does not occupy the extra thickness space of the first pole piece, and can reduce lithium plating of the secondary battery while increasing the energy density of the secondary battery.
[0011] In some preferred embodiments, the first current collector further has a third surface, and the first surface and the third surface are arranged opposite to each other along the thickness direction of the first current collector. The first pole piece further has a third active material layer, and the third active material layer is arranged on the third surface. When observed along the thickness direction of the first pole piece, the projection of the first empty foil area falls on the projection of the third active material. That is, the active material does not need to be removed at the position of the third surface corresponding to the first empty foil area, and more third active material layers can be coated on the third surface, so as to make full use of the space and improve the energy density of the secondary battery.
[0012] In some preferred embodiments, along the width direction of the current collector, the length of the first empty foil area is L1, the length of the first adhesive layer is L2, and 0mm≤L1-L2≤5mm. It is convenient to set the tab in the first empty foil area in the width direction of the current collector, and at the same time reserve a gap space of 0mm to 5mm in the width direction of the current collector, which can reduce the direct bonding between the first adhesive layer and the first active material layer, thereby reducing the impact of the first adhesive layer on the battery energy density. When L1-L2=0mm, the first adhesive layer can bond the entire first empty foil area in the length direction to improve the bonding strength. When L1-L2≤5mm, the space occupied by the first adhesive layer can be reduced, and the energy density of the secondary battery can be improved. When L1-L2<0mm, the first adhesive layer may cover the active material, resulting in a loss of energy density.
[0013] Optionally, along the length direction of the current collector, the width of the first empty foil area is W1, the width of the first adhesive layer is W2, and 0mm≤W1-W2≤5mm. It is convenient to set the pole ear in the first empty foil area in the length direction of the current collector, and at the same time reserve a gap space of 0mm to 5mm in the length direction of the current collector, which can reduce the direct bonding between the first adhesive layer and the first active material layer, thereby reducing the impact of the first adhesive layer on the energy density of the secondary battery, which is not only convenient for the pole ear to be set in the first empty foil area, but also convenient for the pole ear to be bonded and fixed to the current collector through the first adhesive layer. Among them, when W1-W2=0mm, the first adhesive layer can bond the entire first empty foil area in its width direction to improve the bonding strength. When W1-W2≤5mm, the space occupied by the first adhesive layer can be reduced, and the energy density of the secondary battery can be improved.
[0014] In some preferred embodiments, along the width direction of the current collector, the bonding length between the first adhesive layer and the first empty foil area is L3, 4mm≤L3≤24mm. Along the length direction of the current collector, the bonding width between the first adhesive layer and the first empty foil area is W3, 4mm≤W3≤14mm. Sufficient bonding length and bonding width increase the bonding area between the first adhesive layer and the first empty foil area, improve the connection strength, and reduce the influence of the first adhesive layer on the energy density of the secondary battery.
[0015] Optionally, along the thickness direction of the current collector, the thickness of the first adhesive layer is T1, 2 μm≤T1≤50 μm, which can improve the connection strength while reducing the influence of the first adhesive layer on the energy density of the secondary battery.
[0016] In some preferred embodiments, along the width direction of the first pole piece, the bonding length of the first adhesive layer and the first empty foil area is L3, and along the thickness direction of the first pole piece, the overlapping length of the first pole ear and the first current collector along the width direction of the first pole piece is L4, 50% L4≤L3≤150% L4; and / or, along the length direction of the first pole piece, the bonding width of the first adhesive layer and the first empty foil area is W3, and along the thickness direction of the first pole piece, the overlapping width of the first pole ear and the first current collector along the length direction of the first pole piece is W4, 50% W4≤W3≤150% W4. While improving the connection strength between the pole ear and the current collector, the influence of the first adhesive layer on the energy density of the secondary battery is reduced.
[0017] In some preferred embodiments, there is a gap space between the first glue layer and the first active material layer to prevent the first glue layer from directly bonding with the first active material layer, thereby reducing the influence of the first glue layer on the capacity and energy density of the secondary battery.
[0018] In some preferred embodiments, the first adhesive layer includes at least one of epoxy resin, polyolefin, polystyrene, polymethyl methacrylate, phenolic resin or styrene-butadiene rubber. The above materials have excellent bonding properties and chemical corrosion resistance and can adapt to various electrochemical reactions inside the secondary battery.
[0019] In some preferred embodiments, the first adhesive layer includes thermosetting adhesive, hot melt adhesive or pressure sensitive adhesive. Part of the first electrode tab passes through the first adhesive layer and contacts the first empty foil area, thereby achieving electrical connection between the first electrode tab and the first empty foil area.
[0020] In some preferred embodiments, the first adhesive layer is a conductive adhesive layer, and the first electrode tab can be electrically connected to the first empty foil area without the first electrode tab passing through the first adhesive layer.
[0021] In a second aspect, the present application further proposes a secondary battery, comprising an electrode assembly as described in any embodiment of the first aspect above.
[0022] Additional aspects and advantages of the embodiments of the present application will be described, shown, or explained in part in the subsequent description through implementation of the embodiments of the present application. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] One or more embodiments are exemplarily described by corresponding drawings, which do not constitute limitations on the embodiments. Elements with the same reference numerals in the drawings represent similar elements, and unless otherwise stated, the dimensions in the drawings do not constitute proportional limitations.
[0024] Figure 1 A schematic diagram of the stacked structure of an electrode assembly according to some embodiments of the present application;
[0025] Figure 2A diagram showing the winding structure of an electrode assembly according to some embodiments of the present application;
[0026] Figure 3 This is a schematic structural diagram of a first pole piece in some embodiments of the present application;
[0027] Figure 4 for Figure 3 A partial enlarged view of the middle A;
[0028] Figure 5 A schematic diagram of bonding the first electrode tab, the first adhesive layer, and the first current collector in some embodiments of the present application;
[0029] Figure 6 A schematic diagram of bonding the first electrode tab, the first adhesive layer, and the first current collector in some embodiments of the present application;
[0030] Figure 7 A schematic diagram of bonding the first electrode tab, the first adhesive layer, and the first current collector in some embodiments of the present application;
[0031] Figure 8 A schematic diagram of the stacked structure of an electrode assembly according to some embodiments of the present application;
[0032] Fig. 9 A schematic diagram of bonding the first electrode tab, the first adhesive layer, and the first current collector in some embodiments of the present application;
[0033] Fig.10 Schematic diagram of bonding the first electrode tab, the first adhesive layer and the first current collector in some embodiments of the present application (observed along the third direction Z);
[0034] Fig.11 It is a schematic diagram of the stacked structure of the electrode assembly in the prior art.
[0035] Description of reference numerals:
[0036] 100. Electrode assembly;
[0037] 10. first pole piece; 11. first current collector; 111. first surface; 112. third surface; 113. first empty foil area; 12. first active material layer; 13. third active material layer; 14. first space; 15. third space;
[0038] 20. second pole piece; 21. second current collector; 211. second surface; 212. fourth surface; 213. second empty foil area; 22. second active material layer; 23. fourth active material layer; 15. second space;
[0039] 30. Isolation film;
[0040] 40. first pole ear; 41. embedding groove; 42. protrusion;
[0041] 50. First adhesive layer;
[0042] 60. Second pole lug;
[0043] 70, second adhesive layer;
[0044] 80. Pole glue;
[0045] X, first direction; Y, second direction; Z, third direction. DETAILED DESCRIPTION
[0046] In order to make the purpose, technical solutions and advantages of the embodiments of the present application clearer, the technical solutions in the embodiments of the present application will be clearly described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments.
[0047] Reference to "embodiment" in this application means that a particular feature, structure, or characteristic described in conjunction with the embodiment may be included in at least one embodiment of the present application. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments.
[0048] In the description of the embodiments of the present application, the technical terms "first", "second", etc. are only used to distinguish different objects, and cannot be understood as indicating or implying relative importance or implicitly indicating the number, specific order or primary and secondary relationship of the indicated technical features. In the description of the embodiments of the present application, the meaning of "multiple" is more than two, unless otherwise clearly and specifically defined.
[0049] In the description of the embodiments of the present application, the term "and / or" is only a description of the association relationship of the associated objects, indicating that there may be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0050] The technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.
[0051] The tab serves as a bridge for electrically connecting the secondary battery to the external circuit. It is usually made of metal material. The tab is welded to the current collector inside the secondary battery, which allows the tab to be conductive with the electrode assembly inside the secondary battery, thereby achieving the purpose of transmitting current.
[0052] Please refer to Fig.11In order to facilitate the welding of the positive electrode tab 40a, a double-sided empty foil area (the empty foil area is the area on the current collector where no active material layer is provided) is usually required on the positive electrode collector 11a, the welding seat contacts the positive electrode collector 11a on one side of the empty foil area, and the welding head welds the positive electrode tab 40a and the positive electrode collector 11a on the other side of the empty foil area. The negative electrode sheet 20a is usually arranged similarly.
[0053] However, welding of the positive electrode tab and the positive electrode collector 11a and welding of the negative electrode tab 60a and the negative electrode collector 21a usually produces some welding burrs, which are easy to pierce the separator 30a, and easily cause the positive electrode sheet 10a and the negative electrode sheet 20a in the secondary battery to short-circuit and fail. In order to reduce the risk of piercing the separator 30a, Fig.11 As shown, it is usually necessary to set a double layer of insulating glue 90 at the positive electrode tab 40a, that is, set a layer of insulating glue 90 on one side of the positive electrode current collector 11a, and set the same insulating glue 90 on the other side. The same is true for the negative electrode sheet 20a. The setting of the double layer of insulating glue 90 prevents burrs from piercing the isolation film 30a.
[0054] In addition, two layers of electrode glue 80a are also required on the positive electrode sheet 10a to reduce the impact of the burrs at the negative electrode tab 60a on the positive electrode active material layer 12a, and two layers of electrode glue 80a are also required on the negative electrode sheet 20a to reduce the impact of the burrs at the positive electrode tab 40a on the negative electrode active material layer 22a. However, the setting of multiple layers of glue affects the energy density of the secondary battery.
[0055] In order to improve the above problems, the first aspect of the present application proposes an electrode assembly 100, which is a place where the secondary battery undergoes electrochemical reactions and can store and release electrical energy. The electrode assembly 100 includes a first pole piece 10, a separator 30, a second pole piece 20, a first pole tab 40, a first adhesive layer 50, a second pole tab 60, and a second adhesive layer 70.
[0056] Please refer to Figure 1 The electrode assembly 100 is in a stacked shape, that is, the first electrode sheets 10 and the second electrode sheets 20 are alternately stacked, and the isolation film 30 is disposed between the adjacent first electrode sheets 10 and the second electrode sheets 20. Figure 1 Only a structure in which one first pole piece 10 and one second pole piece 20 are stacked is shown. In some other embodiments, a plurality of first pole pieces 10 and second pole pieces 20 may be alternately stacked.
[0057] In some other embodiments, the electrode assembly 100 is in a wound shape, that is, the first pole piece 10, the isolation film 30 and the second pole piece 20 are stacked and then wound, and the isolation film 30 is arranged between the first pole piece 10 and the second pole piece 20 to separate the two.
[0058] The first pole tab 40 may be bonded to the first pole piece 10 through the first adhesive layer 50, and the first pole tab 40 may lead the current flowing through the first pole piece 10 to an external circuit, or lead the external current to the first pole piece 10. The second pole tab 60 may be bonded to the second pole piece 20 through the second adhesive layer 70, and the second pole piece 20 may lead the current flowing through the second pole piece 20 to an external circuit, or lead the external current to the second pole piece 20, so as to realize the charging and discharging of the secondary battery.
[0059] For the first pole piece 10, please refer to Figure 1 The first pole piece 10 includes a first current collector 11, a first active material layer 12, and a third active material layer 13. Along the thickness direction (third direction Z) of the first current collector 11, the first current collector 11 has a first surface 111 and a third surface 112 that are oppositely disposed. The first active material layer 12 is disposed on the first surface 111, and the third active material layer 13 is disposed on the third surface 112.
[0060] Taking the first pole piece 10 as a positive pole piece as an example, the first current collector 11 as the conductive substrate of the first pole piece 10 can be an overall flat and strip-shaped aluminum foil, copper foil or nickel foil. Taking aluminum foil as an example, aluminum foil has high conductivity, which can effectively reduce the internal resistance of the secondary battery, and is convenient for improving the energy density and power density of the secondary battery. In addition, aluminum foil also has good mechanical strength, which can withstand the expansion and contraction of the secondary battery during the charging and discharging process, and ensure the stability and safety of the secondary battery.
[0061] The first active material layer 12 and the third active material layer 13 both include positive electrode active materials, conductive agents, and adhesives, etc. The above-mentioned material components are mixed and stirred evenly, and coated on the first surface 111 and the third surface 112 of the first current collector 11, thereby obtaining the first active material layer 12 and the third active material layer 13. The positive electrode active material can be selected from one or more of lithium nickel cobalt manganese oxide, lithium cobalt oxide, lithium iron phosphate, lithium nickel cobalt manganese oxide, lithium manganese oxide, lithium iron manganese phosphate, and cobalt-free materials.
[0062] In some embodiments, the first current collector 11 has an area not coated with an active material layer, for example, see Figure 1 and Figure 5 The first surface 111 has a first empty foil area 113, which is an area on the first current collector 11 that is not coated with an active material layer. The third surface 112 can also be provided with a third empty foil area (not shown in the figure), and the double-sided empty foil area is provided. The welding seat can receive the first current collector 11 in the third empty foil area, and the welding head welds the first electrode tab 40 to the first current collector 11 in the first empty foil area 113.
[0063] In the embodiment of the present application, the first pole tab 40 is bonded to the first empty foil area 113 through the first adhesive layer 50, and no welding head and welding seat are required, and no welding burrs exist, so the third surface 112 does not need to be provided with an empty foil area, that is, the position of the third surface 112 corresponding to the first empty foil area 113 does not need to remove the active material. For example, when observing along the thickness direction (third direction Z) of the first pole piece 10, the projection of the first empty foil area 113 falls on the projection of the third active material layer 13, and more third active material layers 13 can be coated on the third surface 112, so as to make full use of the space and improve the energy density of the secondary battery.
[0064] For the second pole piece 20, please refer to Figure 1 , the second pole piece 20 includes a second current collector 21, a second active material layer 22 and a fourth active material layer 23. Along the thickness direction (third direction Z) of the second current collector 21, the second current collector 21 has a second surface 211 and a fourth surface 212 that are arranged opposite to each other, the second active material layer 22 is arranged on the second surface 211, and the fourth active material layer 23 is arranged on the fourth surface 212. When the first pole piece 10 and the second pole piece 20 are stacked, the first surface 111 is arranged facing the second pole piece 20, and the second surface 211 is arranged facing the first pole piece 10.
[0065] Taking the second electrode sheet 20 as a negative electrode sheet as an example, the second current collector 21 can be made of aluminum foil, copper foil or nickel foil that is flat and strip-shaped. Taking copper foil as an example, copper foil has high conductivity and can effectively reduce the internal resistance of the secondary battery. In addition, aluminum foil also has good mechanical strength and can withstand the expansion and contraction of the secondary battery during the charging and discharging process, thereby ensuring the stability and safety of the secondary battery.
[0066] The second active material layer 22 and the fourth active material layer 23 include negative electrode active materials, conductive agents, and adhesives, etc. The above-mentioned material components are mixed and stirred evenly, and coated on the second surface 211 and the fourth surface 212 of the second current collector 21, thereby obtaining the second active material layer 22 and the fourth active material layer 23. The negative electrode active material can be selected from one or more of graphite, soft carbon, hard carbon, carbon fiber, elemental silicon, silicon oxide, and silicon alloy.
[0067] In some embodiments, the second current collector 21 has an area not coated with an active material layer, for example, see Figure 1 The second surface 211 has a second empty foil area 213 , and the second empty foil area 213 is an area on the second current collector 21 that is not coated with an active material layer.
[0068] In the embodiment of the present application, the second pole tab 60 is bonded to the second empty foil area 213 through the second adhesive layer 70, and welding through a welding head and a welding seat is not required, and there is no welding burr, so the fourth surface 212 may not need to be provided with an empty foil area. For example, when observing along the thickness direction of the second pole piece 20 (the third direction Z), the projection of the second empty foil area 213 falls on the projection of the fourth active material layer 23, making full use of the space and improving the energy density of the secondary battery.
[0069] It can be understood that when the electrode assembly 100 adopts a winding structure, the first pole sheet 10 is wound along its length direction (first direction X), and there are multiple thickness directions of the first current collector 11 after winding. In the embodiments of the present application, observing along the thickness direction of the second pole sheet 20 usually refers to observing along the thickness direction at the corresponding place. For example, "observing along the thickness direction of the second pole sheet 20, the projection of the second empty foil area 213 falls on the projection of the fourth active material layer 23", here it is observing along the thickness direction of the second pole sheet at the second empty foil area 213.
[0070] For the isolation film 30, please refer to Figure 1 and Figure 2 The isolation film 30 is disposed between the first electrode 10 and the second electrode 20 to insulate and separate the first electrode 10 and the second electrode 20. The isolation film 30 may be a PE isolation film or a PP isolation film containing ceramics. In some embodiments, the isolation film 30 is bonded between the first electrode 10 and the second electrode 20. For example, when the first electrode 10 and the second electrode 20 are stacked, the first active material layer 12 is disposed facing the second active material layer 22, and the isolation film 30 is provided with an adhesive layer (not shown in the figure), so that the isolation film 30 can be directly bonded between the first active material layer 12 and the second active material layer 22, thereby improving the integrity of the electrode assembly 100.
[0071] For the first adhesive layer 50, please refer to Figure 1 as well as Figures 2 to 5 The first adhesive layer 50 is disposed on the surface of the first electrode tab 40 facing the first current collector 11 to bond the first empty foil area 113 to the first electrode tab 40 . The first electrode tab 40 facing away from the first current collector 11 can directly contact the isolation film 30 .
[0072] The first adhesive layer 50 is bonded between the first empty foil area 113 and the first pole ear 40, and can bond and fix the first pole ear 40 to the first current collector 11. Since the first pole ear 40 is directly bonded and fixed to the first current collector 11 through the first adhesive layer 50, it is not only convenient to operate, but also there are no welding burrs, the risk of the separator 30 being pierced is reduced, and there is no need to set an insulating adhesive on the first pole ear 40 or the first empty foil area 113, so that the first pole ear can directly contact the separator, which can save the space occupied by the insulating adhesive, and can reduce the cost while improving the energy density of the secondary battery.
[0073] The first adhesive layer 50 includes at least one of thermosetting adhesive, pressure-sensitive adhesive or hot-melt adhesive.
[0074] For example, the first adhesive layer 50 may be made of hot melt adhesive, and the first adhesive layer 50 may be firstly bonded to the first empty foil area 113, and then the first pole tab 40 may be bonded to the first adhesive layer 50 by hot pressing, and the hot pressing causes the first adhesive layer 50 to melt and bond between the first empty foil area 113 and the first pole tab 40, and after the first adhesive layer 50 is cured, the first pole tab 40 and the first current collector 11 may be fixed. The first adhesive layer 50 may also be made of pressure sensitive adhesive, and when the first pole tab 40, the first adhesive layer 50 and the first current collector 11 are pressed, the first adhesive layer 50 may be bonded to the first current collector 11 and the first pole tab 40. The first adhesive layer 50 may also be made of thermosetting adhesive, and after the first adhesive layer 50 is bonded to the first empty foil area 113, it is cured by hot pressing, so that the first pole tab 40 and the first current collector 11 are fixed.
[0075] The first adhesive layer 50 may be made of a variety of materials, for example, the first adhesive layer 50 includes at least one of epoxy resin, polyolefin, polystyrene, polymethyl methacrylate, phenolic resin or styrene-butadiene rubber. Exemplarily, the first adhesive layer 50 includes epoxy resin, which has excellent bonding properties and chemical corrosion resistance, strong bonding properties and small swelling after being soaked, and can adapt to various electrochemical reactions inside the secondary battery. The epoxy resin can be cured by heating or reacting with a curing agent to form a solid first adhesive layer 50.
[0076] Part of the first pole tab 40 passes through the first adhesive layer 50 and contacts the first empty foil area 113, thereby achieving electrical connection between the first pole tab 40 and the first empty foil area 113. It should be noted that when the first pole tab 40 partially passes through the first adhesive layer 50 and contacts the first empty foil area 113, the material of the first adhesive layer 50 can be an insulating material or a conductive adhesive. When the first pole tab 40 does not pass through the first adhesive layer 50, the first adhesive layer 50 is a conductive adhesive.
[0077] For example, in some embodiments, the first adhesive layer 50 is conductive, and when the first adhesive layer 50 is bonded between the first electrode tab 40 and the first current collector 11, the first electrode tab 40 is electrically connected to the first current collector 11. For example, the first adhesive layer 50 includes conductive metal fillers such as silver, copper, and nickel, so that the first adhesive layer 50 is conductive, which facilitates the electrical connection between the first electrode tab 40 and the first current collector 11.
[0078] In some embodiments, please refer to Figure 6 and Figure 7, the surface of the first pole tab 40 facing the first adhesive layer 50 may also be provided with a plurality of protrusions 42 or a plurality of embedding grooves 41. When the first adhesive layer 50 is bonded between the first pole tab 40 and the first empty foil area 113, the protrusions 42 may be embedded in the first adhesive layer 50, or the first adhesive layer 50 may be embedded in the embedding grooves 41 of the first pole tab 40, which may increase the friction between the first adhesive layer 50 and the first pole tab 40, increase the bonding area between the first adhesive layer 50 and the first pole tab 40, and thus improve the connection strength between the first pole tab 40 and the first current collector 11. Optionally, the first empty foil area 113 may also be provided with protrusions 42 or embedding grooves 41 in a similar manner to further improve the connection strength between the first pole tab 40 and the first current collector 11.
[0079] Please refer to Figure 1 and Figure 8 When the isolation film 30 is disposed between the first electrode sheet 10 and the second electrode sheet 20, the first empty foil area 113, the first active material layer 12 and the isolation film 30 together enclose the first space 14, the first electrode tab 40 is partially disposed in the first space 14, and the first adhesive layer 50 is bonded between the first empty foil area 113 and the first electrode tab 40. The first electrode tab 40 can be firstly bonded to the first empty foil area 113 through the first adhesive layer 50, and then the isolation film 30 covers the first empty foil area 113.
[0080] Since the first pole tab 40 and the first empty foil area 113 of the first current collector 11 are bonded and fixed by the first adhesive layer 50, no welding seat and welding head are required for welding, so more third active material layers 13 can be set on the third surface 112, and the setting of the single-sided empty foil area can make full use of the internal space of the secondary battery and improve the energy density of the secondary battery. At the same time, no welding burrs will be generated on either the first surface 111 or the third surface 112, which can reduce the risk of the isolation film 30 being pierced, and the first surface 111 and the third surface 112 do not need insulating glue to cover the burrs, which can not only make full use of the space and improve the energy density, but also reduce the cost.
[0081] Similarly, the second empty foil area 213, the second active material layer 22 and the isolation film 30 are enclosed together to form a second space 24, the second pole ear 60 is partially disposed in the second space 24, the second adhesive layer 50 is disposed on the surface of the second pole ear 60 facing the second current collector 21, and the second adhesive layer 70 is bonded between the second empty foil area 213 and the second pole ear 60. The risk of the isolation film 30 being punctured can be further reduced, and the second surface 211 and the fourth surface 212 do not need insulating glue to cover the burrs, so that the surface of the second pole ear 60 away from the second current collector 21 can be directly in contact with the isolation film 30, further improving the space utilization and the energy density.
[0082] Optional, see Figure 1, along the third direction Z, the first active material layer 12 is provided with a pole piece glue 80 at the position corresponding to the second empty foil area 213. For example, when observed along the thickness direction (third direction Z) of the second pole piece 20, the projection of the second empty foil area 213 on the first pole piece 10 falls on the pole piece glue 80, which can alleviate the lithium ion deintercalation of the first pole piece 10 at the pole piece glue 80, so that the second pole piece 20 has sufficient residual lithium ions embedded in the deintercalation of the first pole piece 10, which can alleviate the lithium plating of the secondary battery. It should be noted that in this embodiment, the first pole piece 10 is a positive pole piece, and the second pole piece 20 is a negative pole piece. When the isolation film 30 is arranged between the first pole piece 10 and the second pole piece 20, the isolation film 30 may also cover the pole piece glue 80.
[0083] Please refer to Figure 2 The surface of the first active material layer 12 facing the second active material layer 22 is provided with a third space 15, and the pole piece glue 80 is at least partially accommodated in the third space 15. The pole piece glue 80 does not occupy the extra thickness space of the first pole piece 10, and can reduce the lithium plating of the secondary battery while improving the energy density of the secondary battery.
[0084] In some embodiments, please refer to Figure 1 , when observed along the thickness direction (third direction Z) of the first pole piece 10, the projection of the first empty foil area 113 on the second pole piece 20 is located on the second active material layer 22. Since the first pole tab 40 is bonded to the first empty foil area 113 through the first adhesive layer 50, there is no welding burr, and the pole piece adhesive 80 does not need to be provided on the second active material layer 22 of the second pole piece 20, which can further improve the space utilization rate, thereby improving the energy density of the secondary battery.
[0085] Regarding the size of the first adhesive layer 50, if the size of the first adhesive layer 50 is too small, it may cause unstable bonding with the first current collector 11 or the first electrode tab 40. If the size of the first adhesive layer 50 is too large, it occupies a large space and is easy to bond with the first active material layer 12, affecting the capacity and energy density of the secondary battery.
[0086] In the embodiments of this application, please refer to Figure 8 and Fig. 9 , along the width direction (second direction Y) of the first current collector 11, the length of the first empty foil area 113 is L1, the length of the first adhesive layer 50 is L2, 0mm≤L1-L2≤5mm, so that the first pole tab 40 is conveniently arranged in the first empty foil area 113 in the width direction (second direction Y) of the first current collector 11. Among them, when L1-L2=0mm, the first adhesive layer 50 can bond the entire first empty foil area 113 in its length direction, thereby improving the bonding strength. When L1-L2≤5mm, the space occupied by the first adhesive layer 50 can be reduced, thereby improving the energy density of the secondary battery.
[0087] Optionally, there is a gap space between the first adhesive layer 50 and the first active material layer 12, for example, a gap space of less than 5 mm is reserved in the width direction (second direction Y) of the first current collector 11, so as to reduce direct adhesion between the first adhesive layer 50 and the first active material layer 12, thereby reducing the influence of the first adhesive layer 50 on the battery energy density.
[0088] Along the length direction (first direction X) of the first current collector 11, the width of the first empty foil area 113 is W1, the width of the first adhesive layer 50 is W2, 0mm≤W1-W2≤5mm, so that the first pole tab 40 is conveniently arranged in the first empty foil area 113 in the length direction (first direction X) of the first current collector 11. When W1-W2=0mm, the first adhesive layer 50 can bond the entire first empty foil area 113 in the width direction, thereby improving the bonding strength. When W1-W2≤5mm, the space occupied by the first adhesive layer 50 can be reduced, thereby improving the energy density of the secondary battery.
[0089] Optionally, a gap space of less than 5 mm can be reserved in the length direction (first direction X) of the first current collector 11 to reduce direct bonding between the first adhesive layer 50 and the first active material layer 12, thereby reducing the influence of the first adhesive layer 50 on the energy density of the secondary battery, which not only facilitates the first pole ear 40 to be set in the first empty foil area 113, but also facilitates the first pole ear 40 to be bonded and fixed to the first current collector 11 through the first adhesive layer 50.
[0090] Optionally, along the width direction of the first current collector 11 (second direction Y), the bonding length between the first adhesive layer 50 and the first empty foil area 113 is L3, 4mm≤L3≤24mm. Along the length direction of the first current collector 11 (first direction X), the bonding width between the first adhesive layer 50 and the first empty foil area 113 is W3, 4mm≤W3≤14mm. Sufficient bonding length and bonding width increase the bonding area between the first adhesive layer 50 and the first empty foil area 113, improve the connection strength, and reduce the influence of the first adhesive layer 50 on the energy density of the secondary battery. The first adhesive layer 50 is usually bonded to the first empty foil area 113 as a whole, and the width W2 of the first adhesive layer 50 is the bonding width W3 between the first adhesive layer 50 and the first empty foil area 113, that is, W2=W3.
[0091] In some embodiments, along the width direction of the first pole piece 10 (second direction Y), the bonding length of the first adhesive layer 50 and the first empty foil area 113 is L3; along the thickness direction of the first pole piece 10 (third direction Z), the overlapping length of the first pole tab 40 and the first current collector 11 along the width direction of the first pole piece 10 is L4, 50% L4≤L3≤150% L4; and / or, along the length direction of the first pole piece 10 (first direction X), the bonding width of the first adhesive layer 50 and the first empty foil area 113 is W3; along the thickness direction of the first pole piece 10, the overlapping width of the first pole tab 40 and the first current collector 11 along the length direction of the first pole piece 10 is W4, 50% W4≤W3≤150% W4. While improving the connection strength between the first pole tab 40 and the first current collector 11, the influence of the first adhesive layer 50 on the energy density of the secondary battery is reduced.
[0092] Regarding the thickness of the first adhesive layer 50, if the thickness of the first adhesive layer 50 is too large, the energy density of the secondary battery will be affected. If the thickness of the first adhesive layer 50 is too small, it is easy to cause unstable bonding between the first pole tab 40 and the first current collector 11. In the embodiment of the present application, along the thickness direction of the first current collector 11 (the third direction Z), the thickness of the first adhesive layer 50 is T1, 2μm≤T1≤50μm. When the first current collector 11, the first adhesive layer 50 and the first pole tab 40 are hot-pressed, the first adhesive layer 50 can make the first adhesive layer 50 stably bonded to the first pole tab 40 and the first current collector 11, which can improve the connection strength while reducing the influence of the first adhesive layer 50 on the energy density of the secondary battery.
[0093] Furthermore, 15μm≤T1≤25μm, 15μm to 25μm is usually the finished thickness of the first adhesive layer 50. During the preparation of the secondary battery, there is a high temperature environment, which causes the first adhesive layer 50 to rebound. 15μm to 25μm is usually the thickness after rebound, which can reduce the tab 40 from escaping from the current collector 11.
[0094] In the second aspect, the present application also proposes a secondary battery, including an electrode assembly 100 as described in any embodiment of the first aspect above. The secondary battery can be a lithium-ion battery, a nickel-hydrogen battery, a lead-acid battery, a nickel-cadmium battery or a lithium iron phosphate battery.
[0095] Experiment 1: [Drop test of lithium-ion battery]
[0096] Example 1: Preparation of lithium-ion battery
[0097] <Preparation of positive electrode sheet>
[0098] The positive electrode active material lithium iron phosphate, the positive electrode conductive agent acetylene black, and the positive electrode binder polyvinylidene fluoride (PVDF, weight average molecular weight 5×10 5) are mixed in a mass ratio of 94:3:3, N-methylpyrrolidone (NMP) is added as a solvent, and stirred under a vacuum mixer until the solid content is 75wt% and the system is uniform. The positive electrode slurry is evenly coated on one surface of a positive electrode current collector aluminum foil with a thickness of 6um, and dried at 90°C to obtain a positive electrode sheet with a single-sided positive electrode active material layer (thickness 80μm). Afterwards, the above steps are repeated on the other surface of the aluminum foil, and a first empty foil area is reserved on one surface of the aluminum foil. The first empty foil area has a width of 10mm and a length of 22mm to obtain a positive electrode sheet with a double-sided positive electrode active material layer.
[0099] A first adhesive layer of epoxy resin is bonded to the first empty foil area, the bonding width of the first adhesive layer in the first empty foil area is 8 mm, a gap of 1 mm is reserved on both sides with the positive electrode active material layer, the bonding length is 21 mm, a gap of 1 mm is reserved with the positive electrode active material layer in the length direction, and the thickness of the first adhesive layer is 20 μm.
[0100] An aluminum sheet is used as the positive electrode tab, the positive electrode tab is bonded to the first adhesive layer of epoxy resin, and fixed to the current collector by hot pressing.
[0101] <Preparation of negative electrode sheet>
[0102] The negative electrode active material graphite powder, conductive agent conductive carbon black (Super P), and binder styrene butadiene rubber (SBR) were mixed in a weight ratio of 97.5:1:1.5, and then deionized water was added as a solvent to prepare a slurry with a solid content of 50wt%, and stirred evenly. The slurry was evenly coated on one surface of a negative electrode current collector copper foil with a thickness of 5μm, and dried at 110℃ to obtain a negative electrode active material with a weight of 9.1mg / cm 2 Single-sided negative electrode sheet. After the above steps are completed, the single-sided coating of the negative electrode sheet has been completed. Afterwards, the above steps are repeated on the other surface of the negative electrode sheet to obtain a negative electrode sheet coated with a negative electrode active material layer on both sides. A second empty foil area is reserved on the negative electrode sheet, and the width of the second empty foil area is 10mm and the length is 22mm. The first glue layer of epoxy resin is bonded to the first empty foil area, and the bonding width of the first glue layer in the first empty foil area is 8mm. A gap of 1mm is reserved on both sides with the negative electrode active material layer, and the bonding length is 21mm. A gap of 1mm is reserved with the negative electrode active material layer in the length direction, and the first glue layer is embedded in the embedding groove.
[0103] A nickel sheet is used as the negative electrode tab, the negative electrode tab is bonded to the first adhesive layer of epoxy resin, and is fixed to the current collector by hot pressing.
[0104] <Preparation of Separator Film>
[0105] A polyethylene (PE) porous film with a thickness of 8 μm was used as the isolation membrane.
[0106] <Electrolyte Preparation>
[0107] In a dry argon atmosphere, ethylene carbonate, ethyl methyl carbonate and diethyl carbonate were mixed in a mass ratio of 30:50:20 to obtain an organic solution, and then lithium hexafluorophosphate was added to the organic solvent to dissolve and mix evenly to obtain an electrolyte with a lithium salt concentration of 1.15 mol / L.
[0108] <Preparation of lithium-ion batteries>
[0109] The prepared separator, positive electrode sheet, separator, and negative electrode sheet are stacked in order, wound to obtain an electrode assembly, and the electrode assembly is hot pressed at a pressure of 5 MPa, a temperature of 65°C, and a holding time of 10 seconds. The electrode assembly is placed in an aluminum-plastic film packaging bag, and the positive electrode tab and the negative electrode tab are extended from the top seal of the packaging bag. After dehydration at 80°C, the electrolyte is injected and packaged.
[0110] Comparative Example 1 is different from Example 1 in that the positive electrode tab is welded to the positive electrode collector, and the negative electrode tab is welded to the negative electrode collector.
[0111] Drop test method: pre-treat the lithium-ion battery at 25°C, let it stand for 60 minutes at room temperature, and then test the voltage of the lithium-ion battery before the drop test; load the lithium-ion battery into the fixture, and use the drop device to drop freely from a position 1.5m above the ground in the following order: head-tail-head right corner-tail right corner-head left corner-tail left corner (angle: 45±15°), and repeat 6 rounds. After the drop, let it stand for 24 hours at room temperature, measure and record the voltage of the lithium-ion battery, and check the appearance of the lithium-ion battery before and after the test and take pictures. The drop test pass judgment criteria: no smoke, no leakage, voltage drop <30mV. Test 100 lithium-ion batteries, the number of batteries that failed the test is X, and the test failure rate is X / 100. The test results are shown in Table 1 below.
[0112] Table 1
[0113] Connection Drop test failure rate Comparative Example 1 welding 12% Example 1 Bonding 4%
[0114] According to Table 1 above, combined with Example 1 and Comparative Example 1, it can be seen that when the tab and the current collector are bonded with the first adhesive layer, the drop test pass rate is significantly better than that of Comparative Example 1. Comparative Example 1 uses welding, and welding burrs are easy to pierce the isolation membrane. When the lithium-ion battery falls or collides, it is more likely to cause the burrs to pierce the isolation membrane, resulting in a short circuit between the positive and negative electrodes, causing the lithium-ion battery to fail. In Example 1, the first adhesive layer is used for bonding, and there are no welding burrs, which can effectively reduce the risk of the isolation membrane being pierced, thereby improving the collision resistance of the lithium-ion battery.
[0115] At the same time, it is difficult to weld all the overlapping parts of the pole ear and the current collector by welding, and the connection area is small, while the bonding method can bond all the overlapping areas of the pole ear and the current collector, and after pressing, the first adhesive layer fills the gap between the pole ear and the current collector, and the setting of the embedded groove makes the connection area between the pole ear and the current collector larger, thereby improving the connection strength; the greater the connection strength, the better the deformation resistance of the pole ear, which can reduce the tearing of the pole ear and reduce the risk of leakage; and reduce the short circuit of the pole ear with the pole ear of the other polarity due to bending and skewing, thereby reducing the drop failure rate.
[0116] Experiment 2: Energy density test and tensile strength test
[0117] Taking the lithium-ion batteries of the above-mentioned embodiment 1 and comparative example 1 as examples, energy density tests were conducted on them. Among them, in comparative example 1, the positive electrode uses two pieces of insulating glue with a thickness of 8μm and a length and width of 15*30 respectively to cover the empty foil areas on both sides of the positive electrode tab, and a positive electrode sheet glue with a thickness of 8μm and a length and width of 15mm*30mm is used to cover the position of the positive electrode active material layer corresponding to the negative electrode tab. The negative electrode uses two pieces of insulating glue with a thickness of 8μm and a length and width of 14mm*28mm respectively to cover the empty foil areas on both sides of the negative electrode tab, and a negative electrode sheet glue with a thickness of 8μm and a length and width of 15mm*30mm is used to cover the position of the positive electrode active material layer corresponding to the negative electrode tab.
[0118] The relevant parameters in Examples 2 to 9 are shown in Table 2 below.
[0119] Energy density test method: Prepare a square lithium-ion battery using the above preparation method, charge the battery to 4.2V at a constant current of 1C, then charge the battery to 0.05C at a constant voltage of 4.2V, and discharge the battery to 2.5V at a constant current of 0.2C, and record the discharge energy E; measure the dimensions of the square battery and calculate its volume, which is V; then the energy density W = E / V. The test results are shown in Table 2 below.
[0120] Tensile strength test method: disassemble the battery to obtain the positive electrode and the negative electrode. Taking the positive electrode as an example, use a high-speed rail tensile testing machine to fix the pole ear at the lower end of the tensile testing machine, and fix the current collector at the upper end of the high-speed rail tensile testing machine, keep the two ends in the same vertical plane, set the tensile testing machine speed to 50mm / min, pull the pole ear and the current collector, and record the tension F (in N) when the pole ear and the current collector are pulled apart.
[0121] Table 2
[0122]
[0123]
[0124] In combination with the above Table 2, according to Examples 1 to 9 and Comparative Example 1, it can be seen that when the first adhesive layer is used to bond the pole ear and the current collector, the tensile strength is significantly higher than that of Comparative Example 1. This is because it is difficult to weld all the overlapping parts of the pole ear and the current collector by welding, and the connection area is small, while the bonding method can bond all the overlapping areas of the pole ear and the current collector, and after pressing, the first adhesive layer fills the gap between the pole ear and the current collector, and the setting of the embedded groove makes the connection area between the pole ear and the current collector larger, thereby improving the connection strength.
[0125] In Example 1 and Examples 3 to 9, the tensile strength is better than that in Example 2. In Example 1 and Examples 3 to 9, the width of the first adhesive layer is greater than 4mm, which can increase the connection area between the tab and the current collector, and the tab improves the connection strength. In Example 1 and Examples 3 to 8, the energy density is higher than that in Example 9. This may be because the width of the first adhesive layer is too large, which may cause the first adhesive layer to be directly bonded to the active material layer, affecting the battery capacity. In addition, in combination with Examples 8 and 9, the effect of increasing the width of the first adhesive layer on improving the tensile strength is not obvious. This may be because part of the first adhesive layer is bonded to the active material layer, resulting in poor bonding effect of this part. Therefore, in this application, the width of the first adhesive layer is selected to be 4mm≤W2≤14mm, that is, the bonding width of the first adhesive layer and the first empty foil area is 4mm≤W3≤14mm.
[0126] Furthermore, in Example 1 and Examples 3 to 6, the energy density is not only higher than that in Examples 7 to 9, but also the tensile strength is higher than that in Example 2. In Examples 7 to 9, as the width of the first adhesive layer increases, the effect of improving the tensile strength becomes less and less obvious, because the width of the first adhesive layer is greater than the width of the first empty foil area, part of the first adhesive layer is directly bonded to the active material layer, and the part bonded to the active material layer has little effect on improving the connection strength. In Example 1 and Examples 3 to 6, the width of the first adhesive layer is less than or equal to the width of the first empty foil area, which can reduce direct bonding with the active material layer, and a sufficient width can improve the connection strength, and the effect on energy density is also small.
[0127] In Example 3, the tensile strength and energy density are both high. In Example 6, the width of the first empty foil area is consistent with the width of the first adhesive layer, so that the first adhesive layer can fully bond the first empty foil area in the width direction to improve the bonding strength; while in Examples 7 to 9, the width of the first adhesive layer is too large. Although the first empty foil area can be fully bonded in the width direction, it has a greater impact on the energy density. Therefore, in this application, the width difference between the first empty foil area and the first adhesive layer is selected to be 0mm≤W1-W2≤5mm. Based on the same inventive concept, the width difference in the length direction of the first adhesive layer can also be selected to be 0 to 5mm. From Examples 6-9, when W2≥W1, the tensile strength is basically unchanged, while the energy density decreases as W2 increases.
[0128] The above descriptions are merely embodiments of the present application and are not intended to limit the patent scope of the present application. Any equivalent structure or equivalent process transformation made using the contents of the present application specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. An electrode assembly, comprising a first pole piece, a separator and a second pole piece, wherein the separator is arranged between the first pole piece and the second pole piece; the first pole piece comprises a first current collector and a first active material layer, the first current collector has a first surface facing the second pole piece, and the first active material layer is arranged on the first surface; the second pole piece comprises a second current collector and a second active material layer, the second current collector has a second surface facing the first active material layer, and the second active material layer is arranged on the second surface; characterized in that The electrode assembly also includes a first electrode tab and a first glue layer; The first surface has a first empty foil area, and the first empty foil area, the first active material layer and the isolation film together enclose a first space, the first pole ear portion is arranged in the first space, and the first glue layer is arranged on the surface of the first pole ear facing the first current collector to bond the first empty foil area and the first pole ear, the first empty foil area is electrically connected to the first pole ear, and the surface of the first pole ear facing away from the first current collector is in contact with the isolation film.
2. The electrode assembly according to claim 1, characterized in that: The electrode assembly also includes a second electrode tab and a second glue layer. The second surface has a second empty foil area. The second empty foil area, the second active material layer and the isolation membrane together enclose a second space. The second electrode tab is partially arranged in the second space, and the second glue layer is arranged on the surface of the second electrode tab facing the second current collector to bond the second empty foil area to the second electrode tab. The surface of the second electrode tab facing away from the second current collector is in contact with the isolation membrane.
3. The electrode assembly according to claim 1, characterized in that: Observing along the thickness direction of the first pole piece, the projection of the first empty foil area on the second pole piece is located on the second active material layer.
4. The electrode assembly according to claim 2, characterized in that: A pole piece glue is provided on the surface of the first active material layer facing the second active material layer; Observing along the thickness direction of the second pole piece, the projection of the second empty foil area on the first pole piece is located within the projection of the pole piece glue; Among them, the first pole piece is a positive pole piece, and the second pole piece is a negative pole piece.
5. The electrode assembly according to claim 1, characterized in that: A third space is provided on the surface of the first active material layer facing the second active material layer, and the electrode glue is at least partially contained in the third space.
6. The electrode assembly according to claim 1, characterized in that: The first current collector further has a third surface, and along the thickness direction of the first current collector, the first surface and the third surface are arranged opposite to each other; The first pole piece further has a third active material layer, and the third active material layer is arranged on the third surface. When observed along the thickness direction of the first pole piece, the projection of the first empty foil area falls on the projection of the third active material.
7. The electrode assembly according to claim 1, characterized in that: Along the width direction of the first pole piece, the length of the first empty foil area is L1, the length of the first adhesive layer is L2, 0mm≤L1-L2≤5mm; and / or, Along the length direction of the first pole piece, the width of the first empty foil area is W1, the width of the first adhesive layer is W2, and 0mm≤W1-W2≤5mm.
8. The electrode assembly according to claim 1, characterized in that: Along the width direction of the first pole piece, the bonding length between the first adhesive layer and the first empty foil area is L3, 4mm≤L3≤24mm; Along the length direction of the first pole piece, the bonding width between the first adhesive layer and the first empty foil area is W3, 4mm≤W3≤14mm; Along the thickness direction of the first pole piece, the thickness of the first adhesive layer is T1. 2μm≤T1≤50μm.
9. The electrode assembly according to claim 1, characterized in that: Along the width direction of the first pole sheet, the bonding length between the first adhesive layer and the first empty foil area is L3; observed along the thickness direction of the first pole sheet, along the width direction of the first pole sheet, the overlapping length between the first pole ear and the first current collector is L4, 50% L4≤L3≤150% L4; and / or, Along the length direction of the first pole piece, the bonding width between the first adhesive layer and the first empty foil area is W3; observed along the thickness direction of the first pole piece, along the length direction of the first pole piece, the overlapping width between the first pole ear and the first current collector is W4, 50%W4≤W3≤150%W4.
10. The electrode assembly according to claim 7, characterized in that: Along the length direction of the first current collector, there is a gap space between the first glue layer and the first active material layer; and / or, Along the width direction of the first current collector, a gap space is provided between the first glue layer and the first active material layer.
11. The electrode assembly according to claim 1, characterized in that: The first adhesive layer includes at least one of epoxy resin, polyolefin, polystyrene, polymethyl methacrylate, phenolic resin or styrene-butadiene rubber.
12. The electrode assembly according to claim 1, characterized in that The first adhesive layer includes at least one of hot melt adhesive, pressure sensitive adhesive or thermosetting adhesive, and a portion of the first electrode tab passes through the first adhesive layer and contacts the first empty foil area.
13. The electrode assembly according to claim 1, characterized in that: The first adhesive layer is a conductive adhesive layer.
14. A secondary battery, characterized in that: An electrode assembly comprising the electrode assembly as claimed in any one of claims 1 to 13.
Citation Information
Cited By
Secondary battery, electronic device, and method for manufacturing secondary battery
CN119381512A
Secondary battery, electronic device, and method for manufacturing secondary battery
CN119381512B
Battery cell and battery
CN120545638A
Secondary battery and electronic device
CN120749364A
Secondary battery and electronic device
CN120749364B