Semiconductor device manufacturing apparatus and inspection method
By using a combined structure of a capillary tube and a holder in a semiconductor device manufacturing device, the peeling strength of the press ball is detected, which solves the problems of time-consuming and contamination in the existing technology of removing the sample for external inspection, and achieves fast and accurate testing. Peel load determination.
Patent Information
- Application Number
- CN202280092254.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-25
- Publication Date
- 2024-10-01
AI Technical Summary
In the existing technology, when inspecting the peeling strength of the pressure ball in a semiconductor device, the sample needs to be removed from the device for special inspection, which is time-consuming and involves the risk of sample contamination.
A semiconductor device manufacturing device is designed, which uses a structure that combines a capillary tube and a holder. The peeling strength detection of the crimped ball is realized through a moving mechanism and a controller. The cooperation of the holder and the capillary tube is used to slowly increase the load until peeling or Break and measure the peel strength.
The peeling load of the crimp ball can be measured quickly and accurately without the need for a special measuring device, reducing detection time and effectively preventing sample contamination.
Smart Images

Figure CN118743004A_ABST
Abstract
Description
Technical Field
[0001] This specification discloses a semiconductor manufacturing apparatus and an inspection method for manufacturing a semiconductor device. Background Art
[0002] It is known that there are semiconductor devices that are formed by electrically bonding one or more semiconductor chips to a substrate or other semiconductor chips. When manufacturing the semiconductor device, in order to electrically connect the semiconductor chip electrode to the electrode formed on other semiconductor chips or substrates, a crimping ball bonded to the target surface as the electrode surface is sometimes used. To be specific, the semiconductor device manufacturing apparatus melts the front end of the wire to form a metal ball (so-called free air ball (FAB)), and presses the ball against the target surface to form a crimping ball. Then, the semiconductor device manufacturing apparatus connects other electrodes to the crimping ball directly or via a wire, thereby electrically connecting the target surface to the other electrodes.
[0003] In this case, the mechanical bonding strength between the press-bonded ball and the counterpart surface has a significant impact on the quality of the semiconductor device. Therefore, conventionally, a technique for inspecting the bonding strength between the press-bonded ball and the counterpart surface has been proposed.
[0004] For example, Patent Document 1 discloses the following technology: a press-bonded ball (referred to as a "welding ball" in Patent Document 1) is pressed in a direction parallel to the target surface using a dedicated probe, and the force to peel the press-bonded ball from the target surface, i.e., the peeling strength (also referred to as "shear strength") is measured. Patent Document 1 also discloses the following: by changing the angle of the substrate on which the press-bonded ball is formed, the peeling angle is changed, and the peeling strength is measured. According to the technology of Patent Document 1, the bonding strength of the press-bonded ball to the target surface can be quantitatively determined.
[0005] Prior art literature
[0006] Patent Literature
[0007] Patent Document 1: Japanese Patent Application Publication No. 2004-301813 Summary of the invention
[0008] Problems to be solved by the invention
[0009] However, in the case of the prior art such as Patent Document 1, a probe is used to apply a load to the press-bonded ball. On the other hand, the probe is not provided in a common semiconductor device manufacturing apparatus. Therefore, it is conventionally known that in the case of inspecting the peel strength of the press-bonded ball, after forming the press-bonded ball on the target surface using the semiconductor device manufacturing apparatus, the sample formed with the press-bonded ball must be moved out of the semiconductor device manufacturing apparatus and inspected using a dedicated inspection apparatus. However, as described above, moving the sample out of the semiconductor device manufacturing apparatus is not only time-consuming, but also has concerns about the sample being contaminated.
[0010] Therefore, this specification discloses a semiconductor device manufacturing apparatus capable of inspecting peel strength and an inspection method using a capillary.
[0011] Technical means of solving problems
[0012] The semiconductor device manufacturing device disclosed in this specification is characterized in that it includes: a capillary for inserting a wire, and crimping a ball formed at the front end of the wire to a target surface to form a crimped ball; one or more clamps for holding the wire extending upward from the capillary; a moving mechanism for moving the capillary relative to the target surface; and a controller, after the crimped ball is formed at the inspection point of the target surface, the controller performs a load application process for applying an inspection load to the wire while slowly increasing the inspection load until a peeling point when the crimped ball is peeled off or the wire is broken, and obtains the inspection load at the peeling point as the peeling strength, wherein the load application process is performed by moving the capillary in a direction intersecting the axial direction of the capillary, i.e., the inspection direction, with at least one of the clamps closed.
[0013] In this case, the semiconductor device manufacturing apparatus of the present invention is characterized in that: the moving mechanism has a driving motor that outputs power for moving the capillary, and the controller determines the inspection load based on the thrust of the driving motor when moving the capillary in the inspection direction.
[0014] Moreover, the semiconductor device manufacturing apparatus of the present invention may also include: a non-bonding detection unit, which detects the non-bonding of the wire to the target surface based on the power-on state between the wire and the target surface, and the controller determines the time point when the attachment of the wire is detected by the non-bonding detection unit as the peeling time point after the ball is crimped to the inspection point.
[0015] Furthermore, the controller may determine, as the separation timing, a timing at which a deviation between an actual position of the capillary and a command position suddenly decreases when the capillary is moved in the inspection direction in the load application process.
[0016] Moreover, the semiconductor device manufacturing apparatus of the present invention may also include: a front end state detection unit, detecting the state of the front end portion of the wire protruding downward from the capillary, and the controller uses the front end state detection unit to detect the state of the front end portion after the stripping time point, and performs preparatory processing for forming the tail end when there is no tail end at the front end portion.
[0017] Furthermore, the one or more clamps may include: a first clamp which rises and falls in conjunction with the capillary, and which maintains the wire in a state where the crimping ball is connected to the wire and moves upward together with the capillary, thereby breaking the wire; and a second clamp which holds the wire at a position higher than the first clamp, and the controller closes at least the second clamp during the load application process.
[0018] Furthermore, the one or more clamps may include a first clamp but not other clamps, and the first clamp may rise and fall in conjunction with the capillary, and when the crimping ball is connected to the wire, the first clamp maintains the wire and moves upward together with the capillary, thereby breaking the wire, and the controller closes the first clamp during the load application process.
[0019] Moreover, the inspection method disclosed in the present specification is characterized in that it includes the following steps: crimping a ball at the front end of a wire inserted into a capillary to an inspection point on an object surface to form a crimped ball; while holding the wire extending upward from the capillary by a clamp, moving the capillary in a direction intersecting the axial direction of the capillary, i.e., an inspection direction, thereby applying an inspection load to the wire, and applying the inspection load while slowly increasing the inspection load until a peeling point is reached when the crimped ball is peeled off or the wire is broken; and obtaining the inspection load at the peeling point as the peeling strength.
[0020] Effects of the Invention
[0021] According to the technology disclosed in this specification, the peeling load of a press-bonded ball can be measured without using a dedicated measuring device. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] [ Figure 1 ] Figure 1 It is a schematic diagram showing the structure of a semiconductor device manufacturing apparatus.
[0023] [ Figure 2 ] Figure 2 It is a schematic diagram showing the flow of the inspection process of the peeling load.
[0024] [ Figure 3 ] Figure 3 This is a flowchart showing the flow of the inspection process of the peeling load.
[0025] [ Figure 4 ] Figure 4 This is a schematic diagram showing the flow of preparation processing.
[0026] [ Figure 5 ] Figure 5 This is a flowchart showing the flow of the preparation process.
[0027] [ Figure 6 ] Figure 6 It is a schematic diagram showing another flow of the inspection process of the peeling load.
[0028] [ Figure 7 ] Figure 7 This is a flowchart showing another flow of the inspection process of the peeling load.
[0029] [ Figure 8 ] Figure 8 It is a schematic diagram showing another flow of the preparation process.
[0030] [ Fig. 9 ] Fig. 9 It is a schematic diagram showing another flow of the preparation process.
[0031] [ Fig.10 ] Fig.10 is a flowchart showing another flow of the preparation process. DETAILED DESCRIPTION
[0032] Hereinafter, the structure of the semiconductor device manufacturing apparatus 10 will be described with reference to the drawings. Figure 1 1 is a schematic diagram showing the structure of a semiconductor device manufacturing apparatus 10. The semiconductor device manufacturing apparatus 10 is a wire bonding apparatus that mechanically and electrically connects the electrodes of a semiconductor chip to the electrodes of a substrate or other semiconductor chips using a wire. In addition, as described in detail below, the semiconductor device manufacturing apparatus 10 of this example also has a function of inspecting the peel strength of the ball B crimped to the target surface 110, that is, the crimped ball Bb.
[0033] In the semiconductor device manufacturing apparatus 10, a bonding target member such as a substrate 100 is placed on a placement table 42. The upper surface of the bonding target member serves as a target surface 110 to which the wire W is bonded and on which the press-bonded ball Bb is formed.
[0034] The bonding head 12 is provided on the upper side of the mounting table 42. The bonding head 12 bonds the wire W to the target surface 110. The bonding head 12 includes a capillary 14, a first clamper 16, a second clamper 18, a wire tensioner 20, and an air tensioner 22.
[0035] The capillary 14 is a cylindrical member mounted on an ultrasonic horn (not shown). A through hole is formed in the capillary 14 that passes through the axial direction, and a conductor W such as a metal wire is inserted through the through hole. In addition, ultrasonic vibration is imparted to the capillary 14 via the ultrasonic horn during bonding.
[0036] The first clamper 16 and the second clamper 18 are both disposed above the capillary 14 and are members for holding the wire W. The first clamper 16 is raised and lowered together with the capillary 14. The second clamper 18 is disposed above the first clamper 16 and has a fixed height position in the bonding head 12.
[0037] Furthermore, an air tensioner 22 and a wire tensioner 20 are arranged on the upper side of the second clamper 18. The wire tensioner 20 supplies air in an axially downward direction to the wire W, thereby applying appropriate tension to the wire W. Furthermore, the air tensioner 22 supplies air in an axially downward direction or an axially upward direction to the wire W, thereby applying appropriate tension to the wire W.
[0038] The moving mechanism 26 moves the bonding head 12 in the horizontal direction and moves the capillary 14 and the first clamp 16 in the plumb direction. The moving mechanism 26 includes a drive motor 28 and a current sensor 30 for detecting the current value applied to the drive motor 28. Figure 1 In the embodiment, only one drive motor 28 and one current sensor 30 are described, but in fact, one drive motor 28 and one current sensor 30 are provided in each moving direction. In addition, in this example, the capillary 14 is moved, but the moving mechanism 26 may move the mounting table 42 instead of moving the capillary 14, or move the mounting table 42 together with the capillary 14.
[0039] The torch electrode 24 is connected to a high voltage power source (not shown) via a discharge stabilizing resistor (not shown). The torch electrode 24 generates a spark (discharge) based on a control signal from the controller 36, and the heat of the spark melts the tip of the wire W wound from the tip of the capillary 14 to form a ball B, namely, a FAB (Free Air Ball).
[0040] The non-joining sensor 32 functions as a non-joining detection unit that detects the attachment of the tip of the wire W to the target surface 110. The non-joining sensor 32 forms, for example, a circuit from the wire W to the target surface 110, applies a voltage to the circuit, and detects the attachment or grounding of the tip of the wire W to the target surface based on the change in the current value flowing through the circuit. Generally, if the tip of the wire W is grounded to the target surface 110, the current value flowing through the circuit increases. In addition, the non-joining may be determined based on the change in the deviation between the command position and the actual position of the capillary 14 instead of the non-joining sensor 32.
[0041] The front end camera 34 functions as a front end state detection unit that detects the state of the front end portion of the wire W that protrudes downward from the capillary 14. The front end camera 34 captures the front end portion of the wire W. The controller 36 determines the state of the front end portion of the wire W based on the inspection image obtained by the front end camera 34. The state of the front end portion includes, for example, the presence or absence of a ball B and the presence or absence of a tail end Tw.
[0042] The controller 36 controls the driving of each part. The controller 36 is physically a computer having a processor 38 and a memory 40. The controller 36 controls the driving of each part and performs a wire bonding process for electrically and mechanically connecting two electrodes using a wire W. Here, since the control of a normal wire bonding process is already known, only an outline is described here. In the case of a normal wire bonding process, the controller 36 first operates the torch electrode 24 to melt the front end of the wire W to form a ball B (so-called FAB). Then, the controller 36 drives the bonding head 12 to perform the first (1st) bonding of the ball B to the first electrode (for example, the electrode of a semiconductor chip). Hereinafter, the ball B that is crimped to the object surface 110 in the 1st bonding will be referred to as a "crimped ball Bb".
[0043] Then, the controller 36 maintains the state in which the wire W is connected to the crimping ball Bb, and performs the second bonding (2nd bonding), that is, in the state in which the first clamper 16 and the second clamper 18 are opened, the capillary 14 is moved to the right above the second electrode (for example, the electrode of the substrate), and the capillary 14 is lowered to bond the wire W to the second electrode. Finally, the controller 36 raises the capillary 14 in the state in which the first clamper 16 is opened, and after the tail end is exposed, the first clamper 16 is closed, and the capillary 14 is raised, thereby breaking the wire W. In addition, during this bonding process, the controller 36 appropriately confirms the state of the front end of the wire W, specifically, confirms whether there is a ball B or a tail end Tw, based on the inspection image obtained by the front camera 34.
[0044] However, the press-bonded ball Bb formed in the first bonding is press-bonded to the electrode of the semiconductor device, which has a significant impact on the electrical and mechanical quality of the semiconductor device. Therefore, it is conventionally required to quantitatively evaluate the bonding strength of the press-bonded ball Bb to the mating surface 110.
[0045] Therefore, some industry insiders have proposed using a special probe to press the press-bonded ball Bb in a direction parallel to the target surface 110, and measuring the force that causes the press-bonded ball Bb to peel off from the target surface 110 as the peeling load Fa. According to the technology, the bonding strength of the press-bonded ball Bb can be quantitatively evaluated. However, the semiconductor device manufacturing apparatus 10 does not have such a probe for measuring the peeling load Fa. Therefore, in order to measure the peeling load Fa of the press-bonded ball Bb, the sample formed with the press-bonded ball Bb by the semiconductor device manufacturing apparatus 10 must be moved to the outside of the semiconductor device manufacturing apparatus 10 and placed in a special measuring device. However, as described above, measuring the peeling load Fa outside the semiconductor device manufacturing apparatus 10 is not only time-consuming, but there is also a concern that the sample may be contaminated during the movement of the sample.
[0046] Therefore, in this example, the semiconductor device manufacturing apparatus 10 is provided with a function of measuring the peeling load Fa, so that the peeling load Fa can be detected by the semiconductor device manufacturing apparatus 10. This will be described in detail below.
[0047] Figure 2 is a schematic diagram showing the inspection process of the peeling load Fa, Figure 3 This is a flowchart showing the flow of inspection.
[0048] In this example, after the press-bonded ball Bb is formed, the capillary 14 is moved in a predetermined inspection direction while at least one of the clamps is closed. The inspection direction is a direction intersecting the axial direction of the capillary 14, and in this example, it is a horizontal direction. At this time, the controller 36 slowly increases the thrust in the inspection direction, and determines a value proportional to the thrust when the press-bonded ball Bb is peeled off from the target surface 110 or the wire W is broken as the peeling load Fa.
[0049] Specifically, the controller 36 closes the first clamper 16 and opens the second clamper 18, and moves the front end of the wire W close to the torch electrode 24, operates the torch electrode 24, and forms a ball B at the front end of the wire W (S10). Then, the bonding head 12 is moved, and the capillary 14 is moved to the inspection point P1 on the target surface 110 (S12).
[0050] Then, the controller 36 opens the first clamper 16, lowers the capillary 14, and grounds the ball B at the inspection point P1 (S14, S16). If the non-bonding sensor 32 detects that the ball B is grounded at the inspection point P1 (S16 is Yes), the controller 36 closes the second clamper 18 and further lowers the capillary 14 to press the ball B and press it to the target surface 110 for the first bonding (S18). Thus, the pressed ball Bb is formed at the inspection point P1.
[0051] When the press-bonded ball Bb is formed, the controller 36 drives the drive motor 28 of the moving mechanism 26 to move the capillary 14 in a predetermined inspection direction (in this example, the horizontal direction), thereby applying a predetermined inspection load Fd from the capillary 14 to the wire W (S20). At this time, the controller 36 increases the inspection load Fd stepwise until the press-bonded ball Bb is peeled off from the target surface 110 or the wire W is broken (S26).
[0052] Specifically, the controller 36 moves the capillary 14 in the inspection direction while the second clamp 18 is closed, thereby applying a specified inspection load Fd to the conductor W (S20). Here, the inspection load Fd can also be determined based on the current value applied to the drive motor 28. That is, the inspection load Fd is usually proportional to the thrust of the drive motor 28, and the thrust of the drive motor 28 is roughly proportional to the applied current value. Therefore, the controller 36 can also perform current feedback control on the drive motor 28, for example, so that the current value sensed by the current sensor 30 becomes a value proportional to the inspection load Fd. Moreover, in step S20, as long as a load can be applied to the conductor W, the first clamp 16 can be closed instead of the second clamp 18, or the second clamp 18 can be closed together with the first clamp 16.
[0053] When the test load Fd is applied and the pressed ball Bb is peeled off from the target surface 110 or the wire W is broken (Yes in step S22), the controller 36 proceeds to step S28. In addition, in this example, if the wire W is detected to be attached by the non-bonding sensor 32 after the pressed ball Bb is formed, it is determined that the peeling time point has occurred. In addition, as another embodiment, the deviation between the command position and the actual position of the capillary 14 can be monitored, and the time point when the deviation decreases sharply can be detected as the peeling time point when the peeling etc. occurs.
[0054] On the other hand, if peeling of the press-bonded ball Bb does not occur (S22: No), the controller 36 continues to apply the test load Fd until a predetermined reference time has passed (S24: Yes). The reference time is not particularly limited and is, for example, several seconds.
[0055] When the reference time has passed, the controller 36 updates the current test load Fd with a predetermined increase value ΔF as a new test load Fd (S26), and applies the updated test load Fd (S20). Next, the processing of steps S20 to S26 is repeated until the press-bonded ball Bb is peeled off.
[0056] On the other hand, when peeling of the press-bonded ball Bb occurs (Yes in S22), the controller 36 determines the inspection load Fd at that time as the peeling load Fa (S28). The determined peeling load Fa is stored in the memory 40 and is presented to the operator as needed. The operator can quantitatively evaluate the bonding strength of the press-bonded ball Bb based on the presented peeling load Fa.
[0057] If the peeling load Fa can be obtained, the controller 36 then exposes the tail end for the next bonding (S30). Specifically, the controller 36 raises the capillary 14 while the first clamp 16 is open and the second clamp 18 is closed, thereby causing the wire W to protrude from the front end of the capillary 14 by a predetermined distance. Next, the first clamp 16 is finally closed and the second clamp 18 is opened (S32), and the inspection process is completed.
[0058] As is clear from the above description, according to this example, even without removing the sample to the outside of the semiconductor device manufacturing apparatus 10, the peeling load Fa of the press-bonded ball Bb can be inspected in the semiconductor device manufacturing apparatus 10. As a result, compared with the prior art in which the peeling load Fa is measured using a dedicated measuring device, the time for measuring the peeling load Fa can be reduced, and sample contamination can be effectively prevented.
[0059] However, when the inspection of the peeling load Fa is completed, the state of the front end of the wire W must be in a state in which the next bonding can be started. Specifically, it must be in a state in which the tail end Tw of the wire W protrudes downward from the capillary 14 by a predetermined distance and the ball B does not exist at the front end of the wire W. Therefore, when the inspection of the peeling load Fa is completed, the controller 36 uses the front end camera 34 to photograph the front end of the wire W, confirms the presence or absence of the ball B based on the obtained inspection image, and performs preparation processing for the next bonding process based on the result.
[0060] Figure 4 is a schematic diagram showing the flow of the preparation process, Figure 5 3 is a flowchart showing the flow of the preparation process. In the preparation process, as described above, first, the front end camera 34 is used to confirm whether there is a ball B at the front end of the wire W (S36). If the confirmation result shows that there is no ball B at the front end of the wire W (S36 is No), then Figure 2In the case of the state of step S32, it can be determined that an appropriate tail end Tw has been formed, so the controller 36 does not perform special processing but ends the preparation processing. On the other hand, in the case where the ball B remains at the front end of the wire W (S36 is Yes), the controller 36 destroys the ball B to form the tail end Tw (S38 to S46). Specifically, the controller 36 moves the capillary 14 to a location different from the inspection point P1, that is, the preparation point P2, while closing the first clamp 16 and opening the second clamp 18. The preparation point P2 can be set on the same sample as the inspection point P1, or it can be set on a component surface different from the sample where the inspection point P1 is set.
[0061] Then, the controller 36 opens the first clamper 16, lowers the capillary 14, and joins the ball B to the preparatory point P2 (S40). Then, the capillary 14 is raised to expose the tail end of the wire W protruding from the bottom of the capillary 14 by a predetermined distance (S42). Then, the controller 36 closes the first clamper 16 (S44), and raises the capillary 14, thereby breaking the wire W (S46). As a result, the wire W of a predetermined length, that is, the tail end Tw, is pulled out from the front end of the capillary 14, so that the next joining process can be smoothly started.
[0062] However, the semiconductor device manufacturing apparatus 10 having both the first clamper 16 and the second clamper 18 has been described above as an example, but there is also a semiconductor device manufacturing apparatus 10 that has only the first clamper 16 and does not have the second clamper 18. In the case of the semiconductor device manufacturing apparatus 10, after forming the press-bonded ball Bb, the capillary 14 is moved in the inspection direction with the first clamper 16 closed, thereby applying the inspection load Fd to the wire W.
[0063] Figure 6 and Figure 7 1 is a schematic diagram and a flowchart showing the flow of the inspection process of the peeling load Fa in the semiconductor device manufacturing apparatus 10 having only the first clamper 16. Figure 6 , Figure 7As shown, in the case of the semiconductor device manufacturing apparatus 10 having only the first clamper 16, when the inspection load Fd is applied to the wire W (S60), the first clamper 16 is closed instead of the second clamper 18. Furthermore, in the case of the semiconductor device manufacturing apparatus 10 having only the first clamper 16, after peeling of the press-bonded ball Bb occurs (Yes in S62), the capillary 14 is raised (S70) without exposing the tail end, and the process is terminated. In this way, even in the semiconductor device manufacturing apparatus 10 having only one clamper for holding the wire W, the load in the inspection direction can be applied to the wire W by closing the one clamper (i.e., the first clamper 16) and moving the capillary 14 in the inspection direction, thereby determining the peeling load Fa.
[0064] If the peel load Fa can be determined, a preparation process for the next bonding process is performed. Figure 8 , Fig. 9 is a schematic diagram showing the flow of the preparation process, Fig.10 4 is a flowchart showing the flow of the preparation process. The preparation process is greatly different depending on whether there is a ball B at the tip of the wire W. When the ball B is present (S72 is Yes), the controller 36 executes Figure 8 The controller 36 performs steps S74 to S82 shown in FIG. 1 . Specifically, the controller 36 keeps the first clamp 16 closed and moves the capillary 14 to the preparatory point P2 (S74). Then, the controller 36 opens the first clamp 16 and causes the ball B to engage with the preparatory point P2 (S76). Then, the controller 36 keeps the first clamp 16 open and causes the capillary 14 to rise, thereby exposing the tail end (S78). If the wire W protrudes from the lower side of the capillary 14 for a sufficiently long distance, the controller 36 closes the first clamp 16 (S80), and then causes the capillary 14 to rise, thereby breaking the wire W (S82).
[0065] On the other hand, when there is no ball B at the front end of the wire W, the controller 36 executes Fig. 9 Steps S84 to S88 and steps S78 to S82 are shown. Specifically, the controller 36 maintains the state of closing the first clamp 16, and moves the capillary 14 to the preparatory point P2 (S84). Subsequently, the controller 36 maintains the state of closing the first clamp 16, joins the wire W to the preparatory point P2 (S86), and then opens the first clamp 16 (S88). The processing after opening the first clamp 16 is the same as the case where the ball B exists. That is, the capillary 14 is raised to expose the tail end (S78), and then the first clamp 16 is closed to break the wire W (S80, S82). In addition, by performing the preparation processing as described above, even for a semiconductor device manufacturing device 10 having only one clamp, the tail end Tw can be properly formed, so that the next joining process can be properly started.
[0066] In addition, the structure described above is an example. As long as the load application process of applying the inspection load Fd to the wire W after the crimping ball Bb is formed, the inspection load Fd is slowly increased until the peeling point such as peeling occurs, and the inspection load Fd at the peeling point is determined as the peeling load Fa, other structures can also be appropriately changed. The load application process is performed by moving the capillary 14 along the inspection direction in a state where at least one clamp is closed. For example, in the example, the inspection direction (i.e., the direction of the inspection load Fd) is horizontal, but the inspection direction can be any direction that intersects the axis of the capillary, and is not limited to the horizontal direction, and can also be other directions. Moreover, in this example, the inspection load Fd is increased in stages, but as long as it is increased slowly, the inspection load Fd can also be increased continuously.
[0067] Explanation of symbols
[0068] 10: Semiconductor device manufacturing equipment
[0069] 12: Joint head
[0070] 14: Capillary
[0071] 16: First gripper
[0072] 18: Second gripper
[0073] 20: Line tensioner
[0074] 22: Air tensioner
[0075] 24: Torch electrode
[0076] 26: Mobile mechanism
[0077] 28: Drive motor
[0078] 30: Current sensor
[0079] 32: Sensor not engaged
[0080] 34: Front camera
[0081] 36: Controller
[0082] 38: Processor
[0083] 40: Memory
[0084] 42: Loading table
[0085] 100: Substrate
[0086] 110: Object surface
[0087] B: Ball
[0088] Bb: Press ball
[0089] P1: Checkpoint
[0090] P2: Preparation point
[0091] W: Wire
Claims
1. A semiconductor device manufacturing apparatus, Features include: A capillary tube for inserting a wire through, and for pressing a ball formed at a front end of the wire to a target surface to form a pressed ball; One or more holders for holding the wire extending upward from the capillary; A moving mechanism to move the capillary relative to the target surface; as well as Controller, After the crimped ball is formed at the inspection point of the object surface, the controller performs a load application process of applying an inspection load to the wire while slowly increasing the inspection load until the peeling point when the crimped ball is peeled off or the wire is broken, and obtains the inspection load at the peeling point as the peeling strength. The load application process is performed by moving the capillary in a direction intersecting the axial direction of the capillary, i.e., the inspection direction, while at least one of the clamps is closed.
2. The semiconductor device manufacturing apparatus according to claim 1, Features The moving mechanism includes a driving motor that outputs power for moving the capillary. The controller determines the inspection load based on a thrust of the drive motor when moving the capillary in the inspection direction.
3. The semiconductor device manufacturing apparatus according to claim 1 or 2, Features Also includes: a non-joining detection unit for detecting non-joining of the lead wire to the target surface based on a state of conduction between the lead wire and the target surface, The controller determines the time point at which the adhesion of the wire is detected by the non-joining detection unit after the ball is pressed against the inspection point as the separation time point.
4. The semiconductor device manufacturing apparatus according to claim 1 or 2, Features The controller determines, as the separation timing, a timing at which a deviation between an actual position of the capillary and a command position suddenly decreases when the capillary is moved in the inspection direction in the load application process.
5. The semiconductor device manufacturing apparatus according to any one of claims 1 to 4, Features Also includes: a front end state detection unit for detecting the state of the front end portion of the wire protruding downward from the capillary, The controller detects the state of the leading end portion by the leading end state detecting unit after the peeling time point, and performs a preparation process for forming the trailing end when the leading end portion does not have a trailing end.
6. The semiconductor device manufacturing apparatus according to any one of claims 1 to 5, Features The one or more holders include: A first clamper is raised and lowered in conjunction with the capillary, maintains the wire in a state where the crimping ball is connected to the wire, and moves upward together with the capillary, thereby breaking the wire; as well as a second clamper that holds the wire at a position higher than the first clamper, The controller closes at least the second clamper during the load application process.
7. The semiconductor device manufacturing apparatus according to any one of claims 1 to 5, Features The one or more clamps include a first clamp but do not include other clamps, the first clamp is raised and lowered in conjunction with the capillary, and in a state where the crimping ball is connected to the wire, the first clamp maintains the wire and moves upward together with the capillary, thereby breaking the wire. The controller closes the first clamper during the load application process.
8. A method of checking, Features The steps include: The ball at the tip of the wire inserted into the capillary is crimped to the inspection point of the target surface to form a crimped ball; In a state where the wire extending upward from the capillary is held by a clamp, the capillary is moved in a direction intersecting the axial direction of the capillary, i.e., in a testing direction, thereby applying a testing load to the wire, and the testing load is applied while gradually increasing until the crimped ball is peeled off or the wire is broken; as well as The inspection load at the peeling point is obtained as the peeling strength.