Secondary battery and method for manufacturing secondary battery
By directly joining the electrode terminals and collector tabs in the secondary battery and omitting the leads, the problems of low volumetric energy density and complicated assembly in the existing technology are solved, and the manufacturing cost is reduced and the volumetric energy density is improved.
Patent Information
- Application Number
- CN202280092644.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-09-20
- Publication Date
- 2024-10-11
AI Technical Summary
In existing secondary batteries, it is difficult to increase the volumetric energy density due to the spatial arrangement between the output terminal and the electrode body, and the joining operation of the collector tab group and the lead is complicated, resulting in increased manufacturing costs.
Using a direct bonding design, the electrode terminal is installed in the outer packaging container of the secondary battery, and multiple collector tabs are directly bonded to the bonding surface of the electrode terminal, eliminating the lead and using ultrasonic bonding technology for bonding.
The number of components is reduced, the assembly process is simplified, the manufacturing cost is reduced, and the volumetric energy density of the secondary battery is increased.
Smart Images

Figure CN118765461A_ABST
Abstract
Description
Technical Field
[0001] Embodiments of the present invention relate to a secondary battery and a method for manufacturing the secondary battery. Background Art
[0002] In recent years, secondary batteries with high energy density, such as lithium-ion secondary batteries, have been widely used as power sources for electronic devices and electric vehicles. Such secondary batteries are configured to contain an electrode body having a positive electrode and a negative electrode and a non-aqueous electrolyte in a rectangular outer packaging container formed of aluminum or an aluminum alloy. A positive electrode output terminal, a negative electrode output terminal, etc. are provided on the cover of the outer packaging container. The positive electrode output terminal and the negative electrode output terminal are respectively connected to the positive electrode collector ear and the negative electrode collector ear of the electrode body via a positive electrode lead and a negative electrode lead provided in the outer packaging container.
[0003] Prior art literature
[0004] Patent Literature
[0005] Patent Document 1: Japanese Patent Application Publication No. 2008-226625
[0006] Patent Document 2: Japanese Patent Application Publication No. 2017-84695
[0007] Patent Document 3: Japanese Patent No. 6860009
[0008] Patent Document 4: Japanese Patent Application Publication No. 2017-199652
[0009] Patent Document 5: Japanese Patent Application Publication No. 2019-145272
[0010] Patent Document 6: Japanese Patent No. 6777202 Summary of the invention
[0011] [Technical problem to be solved by the invention]
[0012] In the secondary battery as described above, a space for arranging the collector tab and the lead needs to be provided between the output terminal and the electrode body, which makes it difficult to increase the volume energy density of the secondary battery. In addition, the collector tab group and the lead need to be joined, and the lead needs to be joined to the output terminal, which complicates the manufacturing process and becomes the main reason for the increase in manufacturing cost.
[0013] An object of the embodiments of the present invention is to provide a secondary battery and a method for manufacturing the secondary battery that can improve volume energy efficiency and reduce the number of components.
[0014] [Means for solving technical problems]
[0015] According to an embodiment, a secondary battery comprises: an outer packaging container; an electrode terminal installed in the outer packaging container, having a first bonding surface exposed to the outside of the outer packaging container and a second bonding surface exposed in the outer packaging container and opposite to the first bonding surface; and an electrode body housed in the outer packaging container, the electrode body having an electrode group and a collector lug group, the collector lug group including a plurality of collector lugs extending from the electrode group and directly joined to the second bonding surface of the electrode terminal. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is a perspective view showing the appearance of the secondary battery according to the first embodiment.
[0017] Figure 2 is an exploded perspective view of the secondary battery.
[0018] Figure 3 It is a perspective view showing an example of an electrode body.
[0019] Figure 4 It is along Figure 1 A cross-sectional view of the secondary battery taken along line BB.
[0020] Figure 5 It is a plan view showing the back side of the cover of the secondary battery.
[0021] Figure 6 It is along Figure 1 A cross-sectional view of the secondary battery taken along line AA.
[0022] Figure 7 The figure is an assembly diagram of the secondary battery schematically showing a process of ultrasonically bonding an electrode terminal and a collector tab group of the secondary battery.
[0023] Figure 8 It is a perspective view showing an end portion on the cover side of a secondary battery according to a second embodiment.
[0024] Fig. 9 It is along Figure 8 A cross-sectional view of the cover portion of the secondary battery taken along line CC.
[0025] Fig.10 It is a perspective view showing an end portion on the cover side of a secondary battery according to a third embodiment.
[0026] Fig.11 It is along Fig.10 A cross-sectional view of the cover portion of the secondary battery taken along line DD.
[0027] Fig.12 It is a perspective view showing an end portion on the cover side of a secondary battery according to a fourth embodiment.
[0028] Fig.13 It is along Fig.12 A cross-sectional view of the cover portion of the secondary battery taken along line EE. DETAILED DESCRIPTION
[0029] Hereinafter, a secondary battery according to an embodiment of the present invention will be described with reference to the drawings.
[0030] In addition, the disclosure is only an example, and the content that can be easily thought of by those skilled in the art while maintaining the main purpose of the invention is of course also included in the scope of the present invention. In addition, in order to make the description clearer, the drawings sometimes schematically show the width, thickness, shape, etc. of each part compared with the actual way, but it is only an example and does not limit the interpretation of the present invention. In addition, in this specification and each figure, the same reference numerals are marked for the same elements as those described previously in the figures that have appeared, and the detailed description is sometimes appropriately simplified or omitted.
[0031] (First Embodiment)
[0032] The secondary battery according to the first embodiment will be described in detail.
[0033] Figure 1 It is a perspective view showing the appearance of the secondary battery according to the first embodiment.
[0034] As shown in the figure, the secondary battery 10 is a non-aqueous electrolyte secondary battery such as a lithium ion battery, and includes a flat, substantially rectangular outer container 12 and an electrode body 30 described later housed together with a non-aqueous electrolyte in the outer container 12. The outer container 12 is, for example, an outer can (battery case) formed of a metal plate such as aluminum, aluminum alloy, iron, or stainless steel.
[0035] The outer packaging container 12 has a container body 16 with an open top and a rectangular plate-shaped cover 14 welded to the container body 16 and closing the opening of the container body 16, and the interior is formed airtight. The cover 14 is provided with a positive terminal 20 and a negative terminal 21 as a pair of output terminals, a pressure release valve (safety valve) 22, and an injection port 29 (see Figure 2 The injection port 29 is sealed by a disc-shaped sealing cover 25 .
[0036] Here, the longitudinal direction of the cover 14 and the container body 16 is defined as X, the width direction of the cover 14 and the container body 16 perpendicular to the longitudinal direction X is defined as Y, and the height direction of the container body 16 is defined as Z.
[0037] Figure 2 It is an exploded perspective view of a secondary battery.
[0038] As shown in the figure, the container body 16 of the outer packaging container 12 has a rectangular long side wall 16a, a rectangular long side wall 16b spaced apart and parallel to the long side wall 16a, a pair of short side walls 16c and a bottom wall 16d facing each other. A rectangular upper opening 17 is defined by the upper edges of the pair of long side walls 16a and 16b and the upper edges of the pair of short side walls 16c.
[0039] The cover 14 is formed in a rectangular plate shape having a size substantially equal to that of the upper opening 17. The outer periphery of the cover 14 is welded to the upper periphery of the container body 16 and fixed to the container body 16 in a state of closing the upper opening 17.
[0040] Rectangular recesses 26 are formed at both ends of the cover 14 in the longitudinal direction X, and sealing materials such as gaskets 28 made of an insulator such as synthetic resin or glass are installed in these recesses 26. Rectangular through holes T1 and T2 are provided in the center of each recess 26 and gasket 28. Two rectangular plate-shaped insulators 36 are provided on the inner surface side of the cover 14. The insulators 36 are arranged at positions opposite to the recesses 26. A rectangular through hole T3 is formed in each insulator 36.
[0041] The positive terminal 20 is formed of a conductive metal into a substantially rectangular parallelepiped shape, and has a flange 20a integrally on the outer periphery of one end. The end face (upper surface) on the flange 20a side of the positive terminal 20 constitutes a first bonding surface S1 exposed to the outside of the secondary battery 10. The end face (lower surface) on the other end side of the positive terminal 20 constitutes a second bonding surface S2 exposed in the outer packaging container 12. The first bonding surface S1 and the second bonding surface S2 are substantially parallel to each other. The positive terminal 20 is mounted on the cover 14 via a gasket 28. The end of the positive terminal 20 on the opposite side of the flange 20a is inserted into the gasket 28, the recess 26, and the through holes T1, T2, and T3 of the insulator 36, and extends into the container body 16.
[0042] The negative terminal 21 is constructed in the same manner as the positive terminal 20. That is, the negative terminal 21 is formed of a conductive metal into a substantially rectangular parallelepiped shape, and has a flange 21a integrally formed on the outer periphery of one end. The end surface (upper surface) on the flange 21a side of the negative terminal 21 constitutes a first bonding surface S1 exposed to the outside of the secondary battery 10. The end surface (lower surface) on the other end side of the negative terminal 21 constitutes a second bonding surface S2 exposed in the outer packaging container 12. The first bonding surface S1 and the second bonding surface S2 are substantially parallel to each other. The negative terminal 21 is mounted on the cover 14 via a gasket 28. The end of the negative terminal 21 on the opposite side of the flange 21a is inserted through the gasket 28, the recess 26, and the through holes T1, T2, and T3 of the insulator 36, and extends into the container body 16.
[0043] In addition, as the conductive metal forming the positive electrode terminal 20 and the negative electrode terminal 21 , for example, aluminum, an aluminum alloy, copper, or a copper alloy can be used.
[0044] The cover 14 is provided with a safety valve (pressure release valve) 22 that functions as a gas exhaust mechanism and an injection port 29 for a non-aqueous electrolyte. The safety valve 22 is formed in the central portion of the cover 14 in the longitudinal direction X and is disposed between the positive terminal 20 and the negative terminal 21. The safety valve 22 is formed by making a portion of the cover 14 approximately half the thickness of the plate of the other regions. Gas is generated in the outer packaging container 12 by an abnormal mode of the secondary battery 10, and when the internal pressure of the outer packaging container 12 rises to a predetermined value or more, the safety valve 22 opens to reduce the internal pressure and prevent the outer packaging container 12 from rupturing or other undesirable situations.
[0045] The injection port 29 is formed in the lid body 14 between the positive electrode terminal 20 and the safety valve 22. After the non-aqueous electrolyte is injected into the outer container 12 through the injection port 29, the injection port 29 is sealed by, for example, a disk-shaped sealing cap 25.
[0046] Figure 3 It is a perspective view showing an example of an electrode body.
[0047] In one example, a so-called wound type electrode body is used as the electrode body 30 housed in the outer packaging container 12. Figure 3 As shown, the electrode body 30 has, for example, an electrode group 74, which is formed by winding a sheet-like positive electrode plate 70 and a negative electrode plate 72 into a spiral shape around a winding axis C with a sheet-like separator 73 sandwiched therebetween. The electrode group 74 is further compressed in the radial direction in such a way that the cross-sectional shape becomes a quadrilateral shape that is substantially the same as the cross-sectional shape of the outer packaging container 12, thereby forming a flat rectangular shape. The separator 73 is arranged at the outermost layer (outermost periphery) of the electrode group 74. The electrode group 74 is maintained in a wound state by a stop tape, etc., which is not shown in the figure.
[0048] The positive electrode plate 70 has, for example: a strip-shaped positive electrode collector 70a made of metal foil; a positive electrode active material layer 70b formed on at least one surface of the positive electrode collector 70a; and a plurality of long strip-shaped positive electrode collector ears 32 extending from multiple locations on the long sides of the positive electrode collector 70a in a direction parallel to the winding axis C.
[0049] The negative electrode plate 72 comprises: a strip-shaped negative electrode collector 72a made of metal foil; a negative electrode active material layer 72b formed on at least one surface of the negative electrode collector 72a; and a plurality of negative electrode collector ears 33 each in the form of a long strip extending from multiple locations on the long side of the negative electrode collector 72a in a direction parallel to the winding axis C.
[0050] The positive electrode collector ear 32 and the negative electrode collector ear 33 can also be formed by punching the collector, respectively. That is, each collector and collector ear is formed, for example, by a metal foil. The thickness of the metal foil, that is, the thickness of each collector ear is preferably greater than 5 μm and less than 50 μm. By making the thickness greater than 5 μm, the breakage of the collector and the collector ear during manufacturing can be prevented, and a high current collection efficiency can be achieved. In addition, the dissolution of the collector ear when a large current flows can be avoided. By setting the thickness to less than 50 μm, the increase in the thickness of the electrode body can be suppressed, and the number of cycles constituting the electrode body can be increased. Preferably, the thickness of the metal foil is greater than 10 μm and less than 20 μm. The material of the metal foil can vary depending on the type of active material used in the positive and negative electrodes, for example, aluminum, aluminum alloy, copper or copper alloy can be used.
[0051] By overlapping and winding the positive electrode plate 70, the separator 73, and the negative electrode plate 72, a plurality of positive electrode collector tabs 32 are arranged and stacked in the thickness direction of the electrode group 74 to form a positive electrode collector tab group 32A. Similarly, a plurality of negative electrode collector tabs 33 are arranged and stacked in the thickness direction of the electrode group 74 to form a negative electrode collector tab group 33A. The positive electrode collector tab group 32A and the negative electrode collector tab group 33A extend from one end of the axial direction of the electrode group 74 in the same axial direction, and are arranged to be separated from each other in the longitudinal direction of the electrode group 74 orthogonal to the axial direction.
[0052] like Figure 2 As shown, the electrode body 30 is housed in the container body 16 in an orientation such that the winding axis C is consistent with the height direction Z of the outer packaging container 12 and the one end face 31 of the electrode group 74, the positive electrode collector tab group 32A, and the negative electrode collector tab group 33A are located on the lid 14 side. The one end face 31 of the electrode group 74 is opposed to the lid 14 with a predetermined interval. The positive electrode collector tab group 32A is located on one end side of the length direction X of the electrode body 30. The end of the positive electrode collector tab group 32A on the extended side is bent in the width direction Y, extends in a direction substantially parallel to the one end face 31 of the electrode group 74, and faces the positive terminal 20. The negative electrode collector tab group 33A is located on the other end side of the length direction X of the electrode body 30. The end of the negative electrode collector tab group 33A on the extended side is bent in the width direction Y, extends in a direction substantially parallel to the one end face 31 of the electrode group 74, and faces the negative terminal 21.
[0053] In addition, the extended end of the positive electrode collector tab group 32A can also be centrally clamped by a retaining cover (also called a backup lead) bent into a U shape. Similarly, the extended end of the negative electrode collector tab group 33A can also be centrally clamped by a retaining cover bent into a U shape.
[0054] Next, the internal structure of the assembled secondary battery 10 will be described.
[0055] Figure 4 It is along Figure 1 A cross-sectional view of the secondary battery taken along line BB, Figure 5 is a top view showing the inner surface side of the cover body, Figure 6 It is along Figure 1 A cross-sectional view of a secondary battery along line AA.
[0056] like Figure 4 As shown, the cover 14 is fixed to the upper edge of the container body 16, and the upper opening of the container body 16 is hermetically closed. The positive terminal 20 is mounted on the outer surface of the cover 14 via the gasket 28. The first joint surface S1 of the positive terminal 20 is exposed to the outside of the secondary battery 10 and is located at a position substantially parallel to the outer surface of the cover 14. The positive terminal 20 extends into the container body 16 through the through hole T1 of the gasket 28, the through hole T2 of the cover 14, and the through hole T3 of the insulator 36. The second joint surface S2 of the positive terminal 20 is exposed in the container body 16 and is located at a position substantially parallel to the inner surface of the cover 14. In addition, the second joint surface S2 is substantially parallel to the end surface 31 of the electrode body 30 with a gap therebetween. The cover 14 and the positive terminal 20 are electrically insulated by the gasket 28 and the insulator 36.
[0057] The extended end of the positive electrode collector tab group 32A is parallel to the second joint surface S2 of the positive electrode terminal 20 and directly contacts the second joint surface S2. In addition, the extended end of the positive electrode collector tab group 32A is directly joined (welded) to the second joint surface S2 by ultrasonic joining described later. Thus, the positive electrode terminal 20 is electrically connected to the positive electrode plate 70 of the electrode body 30 via the positive electrode collector tab group 32A.
[0058] In the case of ultrasonic bonding, Figure 5 As shown, a mold mark (a mold pressing mark) M remains in the portion located on the electrode body 30 side within the extension of the positive electrode collector tab group 32A. In one example, a mold mark (pressing mark) M consisting of three rectangular recesses arranged along the longitudinal direction X remains in the extension of the positive electrode collector tab group 32A.
[0059] like Figure 4 and Figure 6As shown, the negative terminal 21 is mounted on the outer surface of the cover 14 via the gasket 28. The first joint surface S1 of the negative terminal 21 is exposed to the outside of the secondary battery 10 and is located at a position substantially parallel to the outer surface of the cover 14. The negative terminal 21 extends into the container body 16 through the through hole T1 of the gasket 28, the through hole T2 of the cover 14, and the through hole T3 of the insulator 36. The second joint surface S2 of the negative terminal 21 is exposed in the container body 16 and is located at a position substantially parallel to the inner surface of the cover 14. In addition, the second joint surface S2 is substantially parallel to the end surface 31 of the electrode body 30 with a gap therebetween. The cover 14 and the negative terminal 21 are electrically insulated by the gasket 28 and the insulator 36.
[0060] The extended end of the negative electrode collector tab group 33A is parallel to the second joint surface S2 of the negative electrode terminal 21 and directly contacts the second joint surface S2. In addition, the extended end of the negative electrode collector tab group 33A is directly joined (welded) to the second joint surface S2 by ultrasonic joining described later. Thus, the negative electrode terminal 21 is electrically connected to the negative electrode plate 72 of the electrode body 30 via the negative electrode collector tab group 33A.
[0061] In the case of ultrasonic bonding, Figure 5 As shown, a mold mark (a mold pressing mark) M remains in the portion located on the electrode body 30 side within the extension of the negative electrode collector tab group 33A. In one example, a mold mark (pressing mark) M consisting of three rectangular recesses arranged along the length direction X remains at the extension end of the negative electrode collector tab group 33A.
[0062] In the outer packaging container 12, a rectangular frame-shaped insulating member 48 is provided between the electrode body 30 and the cover 14, surrounding the positive electrode collector tab group 32A and the negative electrode collector tab group 33A. The insulating member 48 is formed into a sheet or plate with a predetermined thickness by an insulating material such as a synthetic resin. In one example, the insulating member 48 is attached to the inner surface of the container body 16, covering the area between the end of the upper opening side of the container body 16 and the end face 31 of the electrode body 30 throughout the entire circumference. The positive electrode collector tab group 32A and the negative electrode collector tab group 33A are electrically insulated from the container body 16 by the insulating member 48.
[0063] The above-mentioned joining of the collector tab group and the electrode terminal is performed by laser welding, ultrasonic welding, resistance welding, etc. According to the present embodiment, the collector tab group and the electrode terminal are joined by ultrasonic welding.
[0064] Figure 7 It is a diagram schematically showing the bonding process.
[0065] like Figure 7As shown, in one example, the double heads (die H and anvil AN) of the ultrasonic bonding device are arranged to sandwich the negative terminal 21 and the extension of the negative collector tab group 33A from both sides, while the extension of the negative collector tab group 33A is in contact with the second bonding surface S2 of the negative terminal 21 mounted on the cover body 14. The die H is in contact with the outer surface side of the negative collector tab group 33A (the outer surface on the opposite side of the negative terminal 21), and the negative collector tab group 33A is pressed toward the second bonding surface S2 of the negative terminal 21 with a predetermined load. The anvil AN on the other side is in contact with the first bonding surface S1 of the negative terminal 21, and the negative terminal 21 is pressed toward the negative collector tab group 33A with a predetermined load. In this state, the die H and the anvil AN are ultrasonically vibrated in opposite phases. By applying a load and ultrasonic vibration to the bonding interface, the oxide film and dirt on the bonding interface are removed, and the metal atoms are bonded to each other by inter-electron force. That is, the bonding interface is the second bonding surface S2 , and the extended portion of the negative electrode current collector tab group 33A is bonded to the second bonding surface S2 of the negative electrode terminal 21 , and is directly bonded to the negative electrode terminal 21 .
[0066] By the same ultrasonic bonding method as described above, the extension of the positive electrode collector tab group 32A is bonded to the second bonding surface S2 of the positive electrode terminal 20, and is directly bonded to the positive electrode terminal 20. The ultrasonic bonding of the positive electrode terminal 20 and the positive electrode collector tab group 32A may be performed simultaneously with the bonding of the negative electrode terminal 21 and the negative electrode collector tab group 33A, or may be performed sequentially.
[0067] After the positive electrode collector tab group 32A and the negative electrode collector tab group 33A are ultrasonically bonded to the positive electrode terminal 20 and the negative electrode terminal 21, respectively, the electrode body 30 is placed in the container body 16, and the lid 14 is fixed to the upper edge of the container body 16 by laser welding or the like. Thus, the secondary battery 10 is assembled.
[0068] In the case of using the above ultrasonic bonding, such as Figures 4 to 6 As shown in FIG. 1 , mold marks (pressing marks of the mold) M are respectively left on the outer surface of the extended portion of each collector tab group 32A, 33A. In one example, a mold mark (pressing mark) M consisting of three rectangular recesses arranged along the length direction X is left on the outer surface of each tab group. Figure 1 As shown, a plurality of dot-shaped pressing marks caused by the anvil AN remain on the first joining surface S1 of the positive electrode terminal 20 and the first joining surface S1 of the negative electrode terminal 21 .
[0069] According to the secondary battery 10 of the first embodiment configured as above, the conventional lead wire is omitted, and each electrode terminal is directly joined to the collector tab group of the electrode body 30. In this way, by omitting the lead wire, the number of components can be reduced, and the manufacturing cost can be reduced. At the same time, the joining operation of the collector tab group and the lead wire is not required, which can simplify the assembly operation and reduce the manufacturing cost.
[0070] Furthermore, by omitting the lead wire, the space for installing the lead wire is not required. Therefore, the space between the cover body 14 and the end face 31 of the electrode body 30 can be reduced, thereby increasing the volume energy density of the secondary battery. In one example, the interval D1 (see Figure 4 ) can be set to 1 / 2 or less compared to a secondary battery with a lead. Thus, when the height of the conventional secondary battery is the same as that of the outer packaging container, the height of the contained electrode body can be increased to increase the battery capacity. Alternatively, when the battery capacity is the same as that of the conventional secondary battery, the height of the outer packaging container can be reduced to miniaturize the secondary battery.
[0071] As described above, according to the first embodiment, a secondary battery capable of increasing volume energy density and reducing manufacturing costs can be obtained.
[0072] In the other embodiments described below, the same parts and components as those in the first embodiment are denoted by the same reference numerals as those in the first embodiment, and their description is omitted or simplified, and the description focuses on the parts different from the first embodiment.
[0073] (Second Embodiment)
[0074] Figure 8 is a perspective view showing a secondary battery according to a second embodiment with its container body omitted. Fig. 9 It is along Figure 8 A cross-sectional view of the cover body and electrode terminal of line CC.
[0075] As shown in the figure, according to the secondary battery 10 of the second embodiment, the positive electrode terminal 20 and the negative electrode terminal 21 each have a third joint surface S3 exposed to the outside in addition to the first joint surface S1 exposed to the outside and the second joint surface S2 exposed in the outer container 12 .
[0076] The first joining surface S1 has, for example, a rectangular shape, and extends approximately parallel to the upper surface of the cover body 14. At the same time, the first joining surface S1 is substantially parallel to the second joining surface S2. The third joining surface S3 has, for example, a rectangular shape, and extends approximately parallel to the upper surface of the cover body 14. The third joining surface S3 is arranged to be arranged in the length direction X with the first joining surface S1, and is substantially parallel to the second joining surface S2. In the length direction X, the first joining surface S1 is located on the central side of the cover body 14, and the third joining surface S3 is located on one end side of the cover body 14.
[0077] The third joint surface S3 is formed at substantially the same height as the first joint surface S1 and is located on the same plane as the first joint surface S1. A groove G extending in the width direction Y is provided between the first joint surface S1 and the third joint surface S3. The first joint surface S1 and the third joint surface S3 are separated in the length direction X via the groove G. In the present embodiment, the third joint surface S3 is formed to be slightly smaller than the first joint surface S1.
[0078] like Fig. 9 As shown, the first joining surface S1 of the positive terminal 20 and the negative terminal 21 functions as a contact surface against which the anvil AN contacts during ultrasonic bonding. That is, when the collector tab group is ultrasonically bonded to the electrode terminal, the anvil AN of the ultrasonic bonding device is pressed against the first joining surface S1, and ultrasonic bonding is performed while the mold H is pressed against the collector tab group. The (positive, negative) collector tab group 32A (33A)) is bonded in the area of the second bonding surface S2 that is opposite to the first bonding surface S1. After bonding, a plurality of dot-shaped pressing marks (recesses) remain on the first bonding surface S1, and a plurality of pressing marks M remain on the (positive, negative) collector tab group 32A (33A).
[0079] The third joint surfaces S3 of the positive terminal 20 and the negative terminal 21 function as joint surfaces for joining bus bars (connection members) B1 and B2. The bus bars B1 and B2 are joined to the third joint surfaces S3 of the positive terminal 20 and the negative terminal 21, respectively, by laser welding, for example.
[0080] As described above, according to the second embodiment, the bonding surface of the electrode terminal exposed to the outside has a first bonding surface S1 for ultrasonic bonding and a third bonding surface S3 for bonding to the bus bar. Therefore, it is possible to combine direct bonding of the collector tab group to the electrode terminal and bonding of the bus bar to the flat third bonding surface S3 without a pressing mark, such as laser welding. By bonding the bus bar to the flat third bonding surface S3 without a pressing mark, it is possible to suppress the occurrence of bonding defects and achieve improved reliability.
[0081] In the second embodiment, the arrangement of the first bonding surface S1 and the third bonding surface S3 may be opposite to that of the above embodiment. That is, the third bonding surface S3 may be arranged on the central part side of the cover body 14, and the first bonding surface S1 may be arranged on one end side of the cover body 14. The arrangement of the bonding surfaces may be selected according to the positional relationship with the electrode body 30.
[0082] (Third Embodiment)
[0083] Fig.10 is a perspective view showing a secondary battery according to a third embodiment with the container body omitted. Fig.11 It is along Fig.10 A cross-sectional view of the cover body and the electrode terminal along line DD.
[0084] As shown in the figure, according to the secondary battery 10 of the third embodiment, there is an insulating cover 40 installed on the positive terminal 20 and the negative terminal 21 shown in the above-mentioned second embodiment. The insulating cover 40 is formed into a roughly rectangular cap shape by an insulating material. The insulating cover 40 is installed on the positive terminal 20 and the negative terminal 21, and covers the first joint surface S1 with remaining pressing marks. In one example, after the collector ear group is directly ultrasonically bonded to the positive terminal 20 and the negative terminal 21, the insulating cover 40 covers the first joint surface S1 with remaining pressing marks of the anvil, and then the bus bars B1 and B2 are laser welded to the third joint surface S3 of the positive terminal 20 and the third joint surface S3 of the negative terminal 21.
[0085] By providing the insulating cover 40 as described above, it is possible to improve the insulation of the electrode terminal and improve the safety.
[0086] (Fourth Embodiment)
[0087] Fig.12 is a perspective view showing a secondary battery according to a third embodiment with its container body omitted. Fig.13 It is along Fig.12 A cross-sectional view of the cover body and the electrode terminal of line EE.
[0088] As shown in the figure, according to the secondary battery 10 of the fourth embodiment, similarly to the aforementioned second embodiment, the positive terminal 20 and the negative terminal 21 have a first joint surface S1 and a third joint surface S3, respectively. According to the fourth embodiment, the first joint surface S1 is formed to be lower than the third joint surface S3. The interval (height H1) between the first joint surface S1 and the second joint surface S2 is shorter than the interval (height H2) between the third joint surface S3 and the second joint surface S2. In other words, in the positive terminal 20 and the negative terminal 21, the thickness H1 of the portion of the first joint surface S1 is formed to be thinner than the thickness H2 of the portion of the third joint surface S3 (H1≤H2).
[0089] As described above, by reducing the thickness H1 of the first joining surface S1 of the electrode terminal, that is, the portion ultrasonically joined to the collector tab group, ultrasonic joining can be facilitated. Basically, ultrasonic joining is easier when the sheet material to be joined is thinner.
[0090] In addition, in the aforementioned second embodiment, third embodiment, and fourth embodiment, the other structures of the secondary battery 10 are the same as those of the secondary battery of the first embodiment. Therefore, in any of the second embodiment, third embodiment, and fourth embodiment, the same effects as those of the aforementioned first embodiment, i.e., a secondary battery with increased volume energy density and reduced manufacturing cost, can be obtained.
[0091] Several embodiments of the present invention have been described, but these embodiments are provided as examples and are not intended to limit the scope of the invention. These embodiments can be implemented in various other ways, and various omissions, substitutions, and changes can be made without departing from the scope of the subject matter of the invention. These embodiments and their variations are included in the scope and subject matter of the invention, and are also included in the invention described in the claims and their equivalents.
[0092] For example, the electrode body is not limited to a so-called wound electrode body in which an electrode plate is wound, but may also be a so-called stacked electrode body in which a plurality of electrode plates are stacked in the thickness direction. In addition, the electrode body contained in the outer packaging container is not limited to a single one, but may be a plurality of electrode bodies.
[0093] The forming materials, shapes, sizes, etc. of the elements constituting the secondary battery are not limited to those in the above-mentioned embodiment, and various changes can be made as necessary.
Claims
1. A secondary battery comprising: Outer packaging container; an electrode terminal mounted on the outer packaging container, having a first joint surface exposed outside the outer packaging container and a second joint surface exposed inside the outer packaging container and opposite to the first joint surface; and The electrode body is accommodated in the outer packaging container, and comprises an electrode group and a collector tab group. The collector tab group comprises a plurality of collector tabs extending from the electrode group and directly joined to the second joining surface of the electrode terminal.
2. The secondary battery according to claim 1, wherein The first joint surface has a plurality of pressing marks, The collector tab group has a plurality of pressing marks.
3. The secondary battery according to claim 1 or 2, wherein: The electrode terminal has a third joint surface that is exposed outside the outer container and arranged in line with the first joint surface, and the collector tab group is joined to a region of the second joint surface that faces the first joint surface.
4. The secondary battery according to claim 3, wherein The secondary battery further includes an insulating cover that is attached to the electrode terminal and covers the first joint surface.
5. The secondary battery according to claim 3, wherein In the electrode terminal, a thickness between the first joint surface and the second joint surface is thinner than a thickness between the third joint surface and the second joint surface.
6. The secondary battery according to claim 1, wherein The outer packaging container comprises: a rectangular container body having an upper opening; and a rectangular plate-shaped cover body fixed to the container body and closing the upper opening. The electrode terminal is mounted on the cover, and the first joint surface and the second joint surface extend substantially parallel to the cover. The electrode group of the electrode body has an end surface facing the inner surface of the cover body with a gap therebetween. The collector tab group extends from the one end surface and is joined to the second joining surface.
7. A method for manufacturing a secondary battery, the secondary battery comprising: an outer packaging container; an electrode terminal having a first bonding surface and a second bonding surface opposite to the first bonding surface, mounted on the outer packaging container; and an electrode body accommodated in the outer packaging container, The manufacturing method of the secondary battery comprises the following steps: The collector tab group of the electrode body is arranged to abut against the second joint surface of the electrode terminal, While the anvil of the ultrasonic bonding device is pressed against the first bonding surface in a manner of clamping the electrode terminal and the collector lug group from both sides, and the mold of the ultrasonic bonding device is pressed against the collector lug group, the anvil and the mold are subjected to ultrasonic vibration, thereby applying ultrasonic waves to the electrode terminal and the collector lug group, and ultrasonically bonding the collector lug group to the second bonding surface of the electrode terminal.