Rapid activation method of proton exchange membrane fuel cell
By increasing the humidity through back pressure and activating the hydrogen evolution reaction with an external power source, the three-phase boundaries and electron transmission channels are optimized, which solves the problems of long activation time and high cost of proton exchange membrane fuel cells and achieves a faster and more efficient activation process.
Patent Information
- Application Number
- CN202410864105.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-30
- Publication Date
- 2024-10-15
AI Technical Summary
Existing proton exchange membrane fuel cells have long activation times, high costs, and low production efficiency, making it difficult to quickly achieve optimal performance.
Rapidly increase the humidity of the proton exchange membrane through a reasonable back pressure, and use an external power supply to force the hydrogen evolution reaction at the cathode to optimize the three-phase boundary and electron transmission channels, thereby accelerating the activation process. High and low load cycles are used to activate the catalyst and shorten the activation time.
It significantly shortens the activation time of proton exchange membrane fuel cells, reduces manufacturing costs and gas usage, improves battery performance, and achieves faster chemical performance activation and proton transport channel establishment.
Smart Images

Figure CN118782828A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of proton exchange membrane fuel cells, in particular to a rapid activation method for proton exchange membrane fuel cells. Background Art
[0002] Hydrogen energy is an important carrier for the large-scale utilization of renewable energy, and fuel cell technology is one of the ways to efficiently utilize hydrogen energy, especially in the automotive field, which has broad application prospects. Proton exchange membrane fuel cell (PEMFC) is the largest type of fuel cell currently in development, with special advantages such as no pollution to the environment, high energy conversion efficiency and power density, low emissions and heat radiation, and low noise pollution.
[0003] Activation is an important part of the production of proton exchange membrane fuel cells. After this activation cycle, the fuel cell will achieve optimal performance. During this running-in period, as the mass transfer channel is successfully established and the three-phase boundary (TPB) in the catalyst layer is optimized, the performance of the battery will gradually increase and reach a peak. The specific effects of activation include the following processes: humidification of the proton exchange membrane, establishment of proton transfer channels, establishment of electron transfer channels, establishment of water transfer channels, optimization of electrode microstructure, and improvement of catalyst activity and utilization. However, the current activation scheme is time-consuming, costly, and has low production efficiency. Summary of the invention
[0004] The purpose of the present invention is to provide a rapid activation method for a proton exchange membrane fuel cell in order to reduce the activation time of the proton exchange membrane fuel cell. The humidity of the proton exchange membrane is quickly increased by a reasonable back pressure, and then a hydrogen evolution reaction is forced to occur at the cathode by an external power supply, thereby improving the activity of the catalyst on the cathode side, completing TPB optimization and establishing an electron transmission channel, thereby accelerating the activation process.
[0005] The purpose of the present invention can be achieved by the following technical solutions:
[0006] A method for rapid activation of a proton exchange membrane fuel cell, the method comprising:
[0007] S1. Connect the circuit and gas path of the proton exchange membrane fuel cell, connect the battery anode to hydrogen, connect the cathode to oxygen, connect the external power supply to the fuel cell, wherein the negative electrode of the power supply is connected to the cathode of the fuel cell, and the positive electrode is connected to the anode of the fuel cell;
[0008] S2, setting the purge parameters, and then purge the proton exchange membrane fuel cell, and connect the anode and cathode to nitrogen;
[0009] S3, connecting the battery anode to hydrogen and the cathode to nitrogen until the anode gas cavity is filled with uniform hydrogen;
[0010] S4, turn on the external power supply for initial activation, and then switch to nitrogen purge;
[0011] S5, connecting the cathode and anode of the fuel cell to a load;
[0012] S6. Execute high and low load cycles to complete the entire activation process.
[0013] Furthermore, the setting of the purge parameters specifically includes: setting the nitrogen flow rate, controlling the change of the back pressure and the temperature range.
[0014] Furthermore, in S3, the specific steps of connecting the battery anode to hydrogen and the cathode to nitrogen until the anode gas cavity is filled with uniform hydrogen are as follows:
[0015] The battery anode is connected to hydrogen, the cathode is connected to nitrogen, and the back pressure is set. At the same time, the cooling chamber of the proton exchange membrane fuel cell is kept dry and kept at room temperature. The above state is maintained for a certain period of time until the anode gas chamber is filled with uniform hydrogen.
[0016] Further, when the back pressure is set in S3, the gas back pressure in the cathode chamber of the fuel cell is greater than or equal to the gas back pressure in the anode chamber.
[0017] Furthermore, the difference between the gas back pressure in the cathode chamber and the gas back pressure in the anode chamber is within the back pressure range.
[0018] Further, the initial activation by turning on the external power supply is specifically as follows:
[0019] Turn on the external power supply, set the power supply current, keep it for a certain period of time, then turn off the power supply for initial activation.
[0020] Furthermore, the power supply current is obtained according to the effective active area of the fuel cell.
[0021] Further, the execution of high and low load cycles is specifically as follows:
[0022] The current density is loaded from open circuit to rated power point at a certain speed, and then the current density is loaded at a certain amplitude. In the process of loading the current density at a certain amplitude, each operating point is maintained for a certain time and repeated many times until the iteration termination condition is met, and then the load is slowly reduced.
[0023] Furthermore, the certain amplitude is the amplitude from the rated power point to the maximum power.
[0024] Furthermore, the iteration termination condition is that the difference between two adjacent high-power potentials of the operating point is less than a potential threshold.
[0025] Compared with the prior art, the present invention has the following beneficial effects:
[0026] The present invention first introduces nitrogen and hydrogen into the cathode and anode, quickly increases the humidity of the proton exchange membrane through a reasonable back pressure, and then forces the cathode to undergo a hydrogen evolution reaction through an external power source, thereby increasing the activity of the catalyst on the cathode side, completing TPB optimization and the establishment of an electron transmission channel, thereby accelerating the activation process. Finally, the gas is switched to hydrogen / oxygen, and the proton exchange membrane fuel cell is activated through a short-term, rapid high and low cyclic current density to effectively activate the chemical properties of the catalyst, while completing the active humidification process of the proton exchange membrane to establish a proton transmission channel, thereby completing all the goals of the activation process. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 is a flow chart of the present invention;
[0028] Figure 2 The test results of the polarization curves of the unactivated and fully activated fuel cells when the first set of parameters is used in the present invention;
[0029] Figure 3 The test results of the polarization curves of the unactivated and fully activated fuel cells when the second set of parameters is used in the present invention;
[0030] Figure 4 The polarization curve test results of the unactivated and fully activated fuel cells when the third set of parameters is used in the present invention. DETAILED DESCRIPTION
[0031] The present invention is described in detail below in conjunction with the accompanying drawings and specific embodiments. This embodiment is implemented based on the technical solution of the present invention, and provides a detailed implementation method and specific operation process, but the protection scope of the present invention is not limited to the following embodiments.
[0032] The present invention proposes a rapid activation method for a proton exchange membrane fuel cell. First, nitrogen and hydrogen are introduced into the cathode and anode to quickly increase the humidity of the proton exchange membrane through a reasonable back pressure. Secondly, an external power source is used to force the cathode to undergo a hydrogen evolution reaction, thereby increasing the activity of the catalyst on the cathode side, thereby accelerating the activation process. Finally, the gas is switched to hydrogen / oxygen, and the proton exchange membrane fuel cell is activated by short-term, rapid high and low circulating current density loading to effectively activate the chemical properties of the catalyst, while completing the active humidification process of the proton exchange membrane. The rapid activation method for a proton exchange membrane fuel cell of the present invention can reduce the activation time of the proton exchange membrane fuel cell to 40 minutes. On the one hand, it greatly shortens the activation time. On the other hand, by shortening the activation time and the initial hydrogen and nitrogen cycles, the amount of gas used is reduced, thereby reducing the manufacturing cost of the proton exchange membrane fuel cell. The present invention solves the problem that the traditional activation process of the proton exchange membrane fuel cell is long and costly.
[0033] The flow chart of the method of the present invention is as follows Figure 1As shown, the method comprises the following steps:
[0034] S1, connect the circuit and gas path of the proton exchange membrane fuel cell, connect the anode of the battery to hydrogen, and connect the cathode to oxygen;
[0035] S2, setting the purge parameters, and then purge the proton exchange membrane fuel cell, and connect the anode and cathode to nitrogen;
[0036] S3, connecting the battery anode to hydrogen and the cathode to nitrogen until the anode gas cavity is filled with uniform hydrogen;
[0037] S4, turn on the external power supply for initial activation, and then switch to nitrogen purge;
[0038] S5, connecting the cathode and anode of the fuel cell to a load;
[0039] S6. Execute high and low load cycles to complete the entire activation process.
[0040] In S1, connect the oxygen on the test bench to the cathode inlet, connect the hydrogen to the anode inlet, and connect the water circuit normally. Connect the external power supply to the fuel cell, where the negative electrode of the power supply is connected to the cathode of the fuel cell, and the positive electrode is connected to the anode of the fuel cell.
[0041] In S2, the control parameters on the test bench are set, the nitrogen flow rate is 0-5NLPM, the back pressure gradually increases from 0 to 50kPa, the temperature is 20-70℃, and the purge is 1 minute.
[0042] In S3, ventilation is performed, and the anode gas is switched to hydrogen, with a flow rate of 8.5 NLPM, a gas humidity of 0-70%, and a back pressure of 50 kPa. At the same time, the cathode gas is kept as nitrogen, with a flow rate of 8.5 NLPM, a gas humidity of 0-70%, and a back pressure of 40 kPa. The cooling chamber is kept at room temperature without water. Keep it for 1 minute to ensure that the anode gas chamber is filled with uniform hydrogen.
[0043] In S4, the external power supply is turned on, the power supply current is set to 60-100 A, and the power supply is turned off after 10 minutes. After the initial activation is completed, the nitrogen purge is switched on.
[0044] In S5, the circuit is switched to connect the positive and negative electrodes of the fuel cell to the test bench accordingly.
[0045] In S6, high and low load cycles: complete the current density loading from open circuit to rated power point at a certain speed, and then load the current density at a certain amplitude. In the process of loading the current density at a certain amplitude, each operating point is maintained for a certain time and repeated many times until the iteration termination condition is met, and then the load is slowly reduced. In the above process, the current density loading from open circuit to rated power point does not need to be iteratively run. The process of loading the current density at a certain amplitude, that is, the loading above the rated power, requires multiple iterative runs. At this time, the iteration termination condition is that the difference between the two adjacent high power potentials of the operating point is less than the potential threshold. The selection of potential is initially determined by each stack design. Both the operating point and the high power point are output by the fuel cell. Both the operating point and the high power point are output by the fuel cell.
[0046] For example, you can first complete the current density loading from open circuit to rated power point at a speed of 100mA / s. Then load the current density at the range of rated power to maximum power, maintain each operating point for 1 minute, and repeat 6 times or more. Finally, slowly reduce the load to avoid the risk of battery damage under high voltage conditions.
[0047] When performing step S2, both chambers of the fuel cell are filled with nitrogen gas, and the flow rate and time are not set fixedly until the air in the gas chamber is exhausted.
[0048] When step S3 is implemented, the gas back pressure (P Ca ) must be greater than or equal to the anode chamber gas back pressure (P An ), ΔP=P Ca -P An The back pressure is kept within the range of 0≤ΔP≤30KPa to avoid damage to the proton exchange membrane of the fuel cell.
[0049] When implementing step S4, the power supply current is set according to the effective active area of the fuel cell, and the unit area is 30-100 mA / cm 2 set up.
[0050] When implementing step S6, each current density in the loading process has its corresponding working condition, and the water, gas, and electricity settings should be implemented according to the standard working conditions of each battery. The number of repeated cycles is determined based on the difference between two adjacent high-power potentials. When the difference between the two potentials is ≤5mV, the cycle is stopped, and then the load is reduced to complete the entire activation process.
[0051] For an active area of 300cm 2 The 90KW fuel cell stack is set to use the first set of parameters in this experiment. The method of the present invention may include the following steps:
[0052] S1. Connect the electricity and gas circuits: Connect the oxygen on the test bench to the cathode inlet, the hydrogen to the anode inlet, and the water circuit to normal connection. Connect the external power supply to the fuel cell, with the negative pole of the power supply connected to the cathode of the fuel cell and the positive pole connected to the anode of the fuel cell.
[0053] S2. Purge: Set the control parameters on the test bench to 5 NLPM nitrogen flow, gradually increase the back pressure from 0 to 50 kPa, and set the temperature to 23°C for 1 minute.
[0054] S3, ventilation: Switch the anode gas to hydrogen, flow rate 8.5NLPM, gas humidity 0%, back pressure 50kPa. At the same time, the cathode gas is kept as nitrogen, flow rate 8.5NLPM, gas humidity 0%, back pressure 40kPa, and the cooling chamber is kept at room temperature without water. Keep it for 1 minute to ensure that the anode gas chamber is filled with uniform hydrogen.
[0055] S4. Turn on the external power supply: set the power supply current to 60A, keep it for 3 minutes, then turn it off, turn it on again, keep it for 3 minutes, then turn it off. Switch to nitrogen purge after the initial activation is completed.
[0056] S5. Switching circuit: Connect the positive and negative electrodes of the fuel cell to the test bench accordingly.
[0057] S6, high and low load cycle: first complete the cycle from open circuit to 1700mA / cm at a speed of 100mA / s 2 The current density is 1700mA / cm 2 ~2100mA / cm 2 Each operating point was maintained for 1 min and repeated 3 times. 2 ~2100mA / cm 2 The current density is pulled by the amplitude, and each operating point is maintained for 1 minute, and repeated 3 times. Finally, the load is slowly reduced to avoid the risk of battery damage under high voltage. Among them, 1700mA / cm 2 Rated point, 1700mA / cm 2 The above is the overload point.
[0058] Each current density has its corresponding working condition during the loading process, and the water, gas, and electricity settings should be implemented according to the standard working conditions of each battery. When the difference between two adjacent high-power potentials is ≤5mV, the cycle is stopped, and then the load is reduced to complete the entire activation process.
[0059] Polarization curve tests were performed on unactivated and fully activated fuel cells respectively. The results are as follows: Figure 2 The performance of the fuel cell after activation using the first set of parameters is significantly improved compared to that before activation. 2Under the condition of 100 % activation, the voltage of the unactivated battery is 0.645 V, while the voltage of the activated battery is 0.686 V, which increases by 41 mV, and the high-frequency resistance decreases by 16 mΩ. This proves that the fuel cell activated by this method has better performance.
[0060] For a set of active area of 300cm 2 The 90KW fuel cell stack of the present invention is used to replace the parameters of some steps of the present invention, and the second set of parameters is used to perform the following steps of the present invention:
[0061] S1 connects the electric and gas circuits: connect the oxygen on the test bench to the cathode inlet, the hydrogen to the anode inlet, and the water circuit is connected normally. Connect the external power supply to the fuel cell, with the negative pole of the power supply connected to the cathode of the fuel cell and the positive pole connected to the anode of the fuel cell.
[0062] S2 purge: Set the control parameters on the test bench, nitrogen flow rate 5NLPM, back pressure gradually increased from 0 to 50kPa, temperature 23℃, purge for 1 minute.
[0063] S3 ventilation: Switch the anode gas to hydrogen, with a flow rate of 8.5NLPM, a gas humidity of 50%, and a back pressure of 50kPa. At the same time, the cathode gas is kept as nitrogen, with a flow rate of 8.5NLPM, a gas humidity of 50%, and a back pressure of 30kPa. The cooling chamber is kept at room temperature without water. Keep it for 1 minute to ensure that the anode gas chamber is filled with uniform hydrogen.
[0064] S4 Turn on the external power supply: Set the power supply current to 90A, keep it for 3 minutes, then turn it off, turn it on again, keep it for 3 minutes, then turn it off. Switch to nitrogen purge after the initial activation is completed.
[0065] S5 switching circuit: connect the positive and negative electrodes of the fuel cell to the test bench accordingly.
[0066] S6 high and low load cycle: first complete the cycle from open circuit to 1700mA / cm at a rate of 100mA / s 2 The current density is 1700mA / cm 2 ~2100mA / cm 2 Each operating point was maintained for 1 min and repeated 3 times. 2 ~2100mA / cm 2 The current density is pulled with a certain amplitude, and each operating point is maintained for 1 minute, and repeated 3 times. Finally, the load is slowly reduced to avoid the risk of battery damage under high voltage conditions.
[0067] Polarization curve tests were performed on unactivated and fully activated fuel cells respectively. The results are as follows: Figure 3The performance of the fuel cell after the activation operation of the present invention using the second set of parameters is significantly improved compared to that before activation. 2 Under the condition of , the voltage of the unactivated battery is 0.645V, while the voltage of the activated battery is 0.693V, which increases by 48mV, and the high-frequency resistance decreases by 16.5mΩ.
[0068] For a set of active area of 300cm 2 The 90KW fuel cell stack of the present invention is used to replace the parameters of some steps of the present invention, adopt the third set of parameters, and perform the following steps:
[0069] S1 connects the electric and gas circuits: connect the oxygen on the test bench to the cathode inlet, the hydrogen to the anode inlet, and the water circuit is connected normally. Connect the external power supply to the fuel cell, with the negative pole of the power supply connected to the cathode of the fuel cell and the positive pole connected to the anode of the fuel cell.
[0070] S2 purge: Set the control parameters on the test bench, nitrogen flow rate 5NLPM, back pressure gradually increased from 0 to 50kPa, temperature 23℃, purge for 1 minute.
[0071] S3 ventilation: Switch the anode gas to hydrogen, with a flow rate of 8.5NLPM, a gas humidity of 70%, and a back pressure of 50kPa. At the same time, the cathode gas is kept as nitrogen, with a flow rate of 8.5NLPM, a gas humidity of 70%, and a back pressure of 30kPa. The cooling chamber is kept at room temperature without water. Keep it for 1 minute to ensure that the anode gas chamber is filled with uniform hydrogen.
[0072] S4 turns on the external power supply: set the power supply current to 100A, keep it for 3 minutes, then turn it off, turn it on again, keep it for 3 minutes, then turn it off. Switch to nitrogen purge after the initial activation is completed.
[0073] S5 switching circuit: connect the positive and negative electrodes of the fuel cell to the test bench accordingly.
[0074] S6 high and low load cycle: first complete the cycle from open circuit to 1700mA / cm at a rate of 100mA / s 2 The current density is 1700mA / cm 2 ~2100mA / cm 2 Each operating point was maintained for 1 min and repeated 3 times. 2 ~2100mA / cm 2 The current density is pulled with a certain amplitude, and each operating point is maintained for 1 minute, and repeated 3 times. Finally, the load is slowly reduced to avoid the risk of battery damage under high voltage conditions.
[0075] Polarization curve tests were performed on unactivated and fully activated fuel cells respectively. The results are as follows: Figure 3 The performance of the fuel cell after the activation condition with the third set of parameters is significantly improved compared with that before activation. 2 Under the condition of , the voltage of the unactivated battery is 0.645V, while the voltage of the activated battery is 0.693V, which increases by 48mV, and the high-frequency resistance decreases by 16.5mΩ.
[0076] The comparison of key control parameters in the above three groups of experiments is shown in Table 1.
[0077] Table 1 Control parameter comparison
[0078]
[0079]
[0080] The preferred specific embodiments of the present invention are described in detail above. It should be understood that a person skilled in the art can make many modifications and changes based on the concept of the present invention without creative work. Therefore, any technical solution that can be obtained by a person skilled in the art through logical analysis, reasoning or limited experiments based on the concept of the present invention on the basis of the prior art should be within the scope of protection determined by the claims.
Claims
1. A method for rapid activation of a proton exchange membrane fuel cell, characterized in that: Methods include: S1. Connect the circuit and gas path of the proton exchange membrane fuel cell, connect the battery anode to hydrogen, connect the cathode to oxygen, connect the external power supply to the fuel cell, wherein the negative electrode of the power supply is connected to the cathode of the fuel cell, and the positive electrode is connected to the anode of the fuel cell; S2, setting the purge parameters, and then purge the proton exchange membrane fuel cell, and connect the anode and cathode to nitrogen; S3, connecting the battery anode to hydrogen and the cathode to nitrogen until the anode gas cavity is filled with uniform hydrogen; S4, turn on the external power supply for initial activation, and then switch to nitrogen purge; S5, connecting the cathode and anode of the fuel cell to a load; S6. Execute high and low load cycles to complete the entire activation process.
2. The rapid activation method of a proton exchange membrane fuel cell according to claim 1, characterized in that: The purge parameters are specifically set as follows: setting the nitrogen flow rate, controlling the back pressure change and the temperature range.
3. The rapid activation method of a proton exchange membrane fuel cell according to claim 1, characterized in that: In S3, the specific steps of connecting the battery anode to hydrogen and the cathode to nitrogen until the anode gas cavity is filled with uniform hydrogen are as follows: The battery anode is connected to hydrogen, the cathode is connected to nitrogen, and the back pressure is set. At the same time, the cooling chamber of the proton exchange membrane fuel cell is kept dry and kept at room temperature. The above state is maintained for a certain period of time until the anode gas chamber is filled with uniform hydrogen.
4. The rapid activation method of a proton exchange membrane fuel cell according to claim 3, characterized in that: When the back pressure is set in S3, the gas back pressure in the cathode chamber of the fuel cell is greater than or equal to the gas back pressure in the anode chamber.
5. The rapid activation method of a proton exchange membrane fuel cell according to claim 4, characterized in that: The difference between the gas back pressure in the cathode chamber and the gas back pressure in the anode chamber is within the back pressure range.
6. The rapid activation method of a proton exchange membrane fuel cell according to claim 1, characterized in that: The specific steps of turning on the external power supply for initial activation are as follows: Turn on the external power supply, set the power supply current, keep it for a certain period of time, then turn off the power supply for initial activation.
7. A method for rapid activation of a proton exchange membrane fuel cell according to claim 6, characterized in that: The power supply current is obtained based on the effective active area of the fuel cell.
8. The method for rapid activation of a proton exchange membrane fuel cell according to claim 1, characterized in that: The execution of high and low load cycles is specifically as follows: The current density is loaded from open circuit to rated power point at a certain speed, and then the current density is loaded at a certain amplitude. In the process of loading the current density at a certain amplitude, each operating point is maintained for a certain time and repeated many times until the iteration termination condition is met, and then the load is slowly reduced.
9. The method for rapid activation of a proton exchange membrane fuel cell according to claim 8, characterized in that: The certain amplitude is the amplitude from the rated power point to the maximum power.
10. The rapid activation method of a proton exchange membrane fuel cell according to claim 8, characterized in that: The iteration termination condition is that the difference between two adjacent high power potentials of the operating point is less than the potential threshold.