Secondary battery

By adjusting the thickness and fluidity index values ​​​​in the electrode composite material layer of the secondary battery to ensure that the liquid flow rate on the positive electrode side is larger than that on the negative electrode side, and using conductive materials such as carbon nanotubes, the electrolyte outflow and salt under high-rate electrification are solved. The problem of uneven concentration improves the high rate characteristics and charge and discharge performance of the battery.

CN118782876APending Publication Date: 2024-10-15TOYOTA BATTERY CO LTD +2
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410358247.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-04-03
Filing Date
2024-03-27
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Under high-rate energization conditions, the charge and discharge performance of the secondary battery is affected by the increase in internal resistance caused by electrolyte outflow and uneven salt concentration, which affects the high-rate characteristics of the battery.

Method used

By adjusting the thickness and fluidity index value in the positive and negative electrode composite material layers, the liquid flow rate on the positive electrode side is larger than that on the negative electrode side, and the fluidity index value of the electrolyte is controlled to be above 0.48×10-6 to ensure uniform distribution of the electrolyte. , using conductive fibrous carbon materials such as carbon nanotubes to improve the fluidity of the electrode composite layer.

Benefits of technology

It effectively suppresses the uneven salt concentration of the electrolyte, improves the high-rate characteristics of the secondary battery, reduces the deterioration of the charge and discharge performance, and improves the overall performance of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118782876A_ABST
    Figure CN118782876A_ABST
Patent Text Reader

Abstract

Provided is a secondary battery having improved high rate characteristics. A secondary battery is provided with an electrode body formed by winding a positive electrode sheet and a negative electrode sheet. Each electrode sheet is formed by laminating an electrode composite material layer on a base material serving as a current collector. In a state of being wound in the form of an electrode sheet, when pressure is applied to the electrode composite material layer for a predetermined time, the weight per unit pressure applied to the electrode composite material layer and the weight of the electrolyte flowing out of the electrode composite material layer per unit volume are used as liquid flow rates. And taking the liquid flow as a liquidity index value of the electrolyte infiltrated into the electrode composite material layer. The predetermined time for applying pressure to the electrode composite layer is set as 3 minutes, and the liquid flow rate is expressed as "gram ((at) 3 minutes) / kPa * cubic millimeter". The secondary battery is configured such that the value obtained by subtracting the liquid flow rate of the negative electrode mixture layer from the liquid flow rate of the positive electrode mixture layer is 0.48 * 10 <-6 > or more.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a secondary battery. Background Art

[0002] In the past, there was a secondary battery having an electrode body formed by winding positive and negative electrode sheets stacked with separators. In a secondary battery having such an electrode body, when a high-rate charge and discharge with a large current is carried out, the electrolyte and the electrode composite material constituting the electrode sheet expand due to heat release, thereby causing the electrolyte impregnated in the electrode body to flow out. Furthermore, this causes the salt concentration of the electrolyte impregnated in the electrode body to become uneven, thereby increasing the internal resistance. As a result, there is a problem of deterioration in charge and discharge performance.

[0003] In order to solve such a problem, the focus is on the fact that the amount of electrolyte flowing out of the electrode composite material tends to increase on the negative electrode side than on the positive electrode side when high-rate power is applied. In addition, as shown in Patent Documents 1 to 4, for example, by balancing the difference in the amount of electrolyte flowing out of the positive electrode side and the negative electrode side, the reduction in charge and discharge performance based on high-rate power application can be suppressed. Prior art literature Patent Literature

[0004] Patent Document 1: Japanese Patent Application Publication No. 2017-174648 Patent Document 2: Japanese Patent Application Publication No. 2017-10882 Patent Document 3: Japanese Patent Application Publication No. 2017-123236 Patent Document 4: Japanese Patent Application Publication No. 2016-66461 Summary of the invention Problems to be solved by the invention

[0005] However, in applications such as electric vehicles that require high-level battery performance, further improvement of secondary battery performance has been sought. Therefore, the impact of high-rate current transfer on the charge and discharge performance of secondary batteries is also required to be further improved, that is, the so-called high-rate characteristics are required to be improved. Means for solving problems

[0006] A secondary battery according to one aspect of the present disclosure comprises an electrode body formed by winding positive and negative electrode sheets stacked with separators, each electrode sheet being formed by stacking an electrode composite material layer on a substrate serving as a current collector, and in a state where the electrode sheets are wound, when a predetermined time and pressure are applied to the electrode composite material layer, and the weight of electrolyte flowing out of the electrode composite material layer per unit pressure applied to the electrode composite material layer and per unit volume of the electrode composite material layer is taken as the fluidity index value of the electrolyte impregnated into the electrode composite material layer, when the predetermined time for applying the pressure to the electrode composite material layer is set to 3 minutes, and when the fluidity index value of the electrolyte is expressed as "g (@3 minutes) / kPa·m3", the value obtained by subtracting the fluidity index value of the negative electrode composite material layer from the fluidity index value of the positive electrode composite material layer is 0.48×10 -6 above.

[0007] In the secondary battery, the fluidity index value of the positive electrode composite material layer may be 7.8×10 -7 Above and 8.8×10 -6 the following.

[0008] In the secondary battery, the thickness of the positive electrode composite material layer may be greater than or equal to 0.034 mm and less than or equal to 0.050 mm.

[0009] In the secondary battery, the fluidity index value of the negative electrode composite material layer may be 2.4×10 -6 Above and 1.1×10 -5 the following.

[0010] In the secondary battery, the thickness of the negative electrode composite material layer may be greater than or equal to 0.060 mm and less than or equal to 0.080 mm.

[0011] In the secondary battery, the positive electrode composite material layer may contain a conductive fibrous carbon material.

[0012] Effects of the Invention According to the present invention, high-rate characteristics can be improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0013] Figure 1 It is a perspective view of a secondary battery. Figure 2 This is an exploded view of the electrode body. Figure 3 is a side view of a secondary battery. Figure 4 Schematic diagram showing the structure of a positive electrode mixture layer in the secondary battery of this embodiment. Figure 5Schematic diagram showing the structure of a positive electrode composite material layer in a secondary battery of a reference example. Figure 6 It is a schematic diagram showing the arrangement of positive and negative electrodes and separators. Figure 7 It is an explanatory diagram showing a process of preparing a sample used for measuring a liquid flow rate. Figure 8 It is an explanatory diagram showing a process of preparing a sample used for measuring a liquid flow rate. Fig. 9 It is an explanatory diagram showing a method of measuring a liquid flow rate. Fig.10 This is a flowchart showing a method for measuring the amount of electrolyte outflow. Fig.11 It is an explanatory diagram showing a method of measuring a liquid flow rate. Fig.12 It is an explanatory diagram showing the distribution of lithium ions in a non-powered state of a secondary battery according to a reference example. Fig.13 It is an explanatory diagram showing the distribution of lithium ions in a secondary battery of a reference example in a high-rate power-on state. Fig.14 It is an explanatory diagram showing the distribution of lithium ions in a secondary battery of a reference example in a high-rate power-on state. Fig.15 It is an explanatory diagram showing the distribution of lithium ions in the secondary battery of the present embodiment in a non-powered state. Fig.16 It is an explanatory diagram showing the distribution of lithium ions in the secondary battery of the present embodiment in a high-rate power-on state. Fig.17 It is an explanatory diagram showing the distribution of lithium ions in the secondary battery of the present embodiment in a high-rate power-on state. Fig.18 This is a table showing the influence of the liquid flow rate of the positive and negative electrode composite material layer on the high rate characteristics of the secondary battery. Fig.19 This is a diagram showing the influence of the liquid flow rate of the positive and negative electrode composite material layer on the high-rate characteristics of the secondary battery. DETAILED DESCRIPTION

[0014] Hereinafter, one embodiment of a secondary battery and an electrode body thereof will be described with reference to the drawings. (Secondary battery) like Figure 1 As shown, the secondary battery 1 includes an electrode body 10 integrating a positive electrode 3, a negative electrode 4 and a separator 5, and a case 20 accommodating the electrode body 10. The secondary battery 1 of this embodiment is a lithium ion secondary battery in which the electrode body 10 in the case 20 is impregnated with a non-aqueous electrolyte solution (not shown).

[0015] In detail, in the secondary battery 1 of the present embodiment, the positive electrode 3, the negative electrode 4 and the separator 5 have a sheet-like appearance and are stacked. Furthermore, by winding the stack of the positive electrode 3, the negative electrode 4 and the separator 5, the separator 5 is sandwiched between the positive electrode 3 and the negative electrode 4, and an electrode body 10 is formed in which the positive and negative electrodes and the separator 5 are alternately arranged in their radial direction.

[0016] The case 20 of the present embodiment includes a flat, substantially rectangular box-shaped case body 21 and a lid member 22 that closes an open end 21 x of the case body 21. The electrode body 10 of the present embodiment has a flat outer shape corresponding to the box shape of the case 20.

[0017] (Electrode sheet and electrode body) If further details are given, Figure 2 As shown, in the secondary battery 1 of this embodiment, the positive electrode 3 and the negative electrode 4 each include an electrode sheet 35 . The electrode sheet 35 includes a current collector 31 and an electrode composite material layer 32 stacked on the current collector 31 . The current collector 31 has a sheet-like shape.

[0018] Specifically, for the electrode sheet 35P for the positive electrode 3, a composite material paste 37P containing a lithium transition metal oxide as a positive electrode active material is applied on a substrate 36P made of aluminum or the like constituting the positive electrode collector 31P. And, for the electrode sheet 35N for the negative electrode 4, a slurry-like composite material paste 37N containing a carbon-based material as a negative electrode active material is applied on a substrate 36N made of copper or the like constituting the negative electrode collector 31N. Furthermore, these composite material pastes 37P and 37N each contain a binder. In the secondary battery 1 of the present embodiment, by drying these composite material pastes 37P and 37N, a positive electrode composite material layer 32P and a negative electrode composite material layer 32N corresponding to them are formed on the positive and negative electrode sheets 35P and 35N, respectively. Here, the positive and negative electrode sheets 35P and 35N refer to the electrode sheet 35P for the positive electrode 3 and the electrode sheet 35N for the negative electrode 4. The positive electrode composite material layer 32P is also referred to as a composite material layer 32 for the electrode sheet 35P of the positive electrode 3 , and the negative electrode composite material layer 32N is also referred to as a composite material layer 32 for the electrode sheet 35N of the negative electrode 4 .

[0019] Furthermore, in the secondary battery 1 of the present embodiment, the positive and negative electrode sheets 35P and 35N are respectively shaped into a strip shape. In the electrode body 10 of the present embodiment, the positive and negative electrode sheets 35P and 35N stacked with the separator 5 sandwiched therebetween are wrapped around the width direction ( Figure 2 The winding is performed on a winding axis 10x extending in the left-right direction (in the center).

[0020] in addition, Figure 2 In the figure, the separator 5 and each electrode sheet 35 are wound in a form in which the electrode sheet 35P constituting the positive electrode 3 is wound inside. However, this figure shows an example of the structure of the electrode body 10, and sometimes the separator 5 and each electrode sheet 35 are wound in a form in which the electrode sheet 35N constituting the negative electrode 4 is wound inside. And thereby, it is determined whether the electrode sheet 35 disposed on the outermost shell of the electrode body 10 is the electrode sheet 35P constituting the positive electrode 3 or the electrode sheet 35N constituting the negative electrode 4.

[0021] And, if Figure 1 to Figure 3 As shown, the cover member 22 of the housing 20 is provided with a positive terminal 38P and a negative terminal 38N protruding to the outside of the housing 20. In addition, an uncoated portion 39 where the electrode composite material layer 32 is not formed on the collector 31 is formed on each electrode sheet 35. In the secondary battery 1 of the present embodiment, the electrode sheet 35P constituting the positive electrode 3 is electrically connected to the positive terminal 38P, and the electrode sheet 35N constituting the negative electrode 4 is electrically connected to the negative terminal 38N by utilizing these uncoated portions 39.

[0022] Specifically, the electrode body 10 of the present embodiment has a winding axis 10x extending along the length direction ( Figure 1 In this state, the uncoated portion 39P of the electrode sheet 35P constituting the positive electrode 3 is connected to the positive electrode terminal 38P by the connecting member 40P. Similarly, the uncoated portion 39N of the electrode sheet 35N constituting the negative electrode 4 is connected to the negative electrode terminal 38N by the connecting member 40N.

[0023] Furthermore, the electrolyte 50 is injected into the case 20. That is, the electrolyte 50 of the secondary battery 1, which is a lithium ion secondary battery, is an electrolyte obtained by dissolving a lithium salt as a supporting salt in an organic solvent. Thus, in the secondary battery 1 of the present embodiment, the electrolyte 50 is impregnated into the electrode body 10 sealed in the case 20.

[0024] (High rate characteristic countermeasures) like Figure 4 As shown, in the secondary battery 1 of this embodiment, the positive electrode composite material layer 32P forming the electrode body 10 contains carbon nanotubes CNT as the conductive fibrous carbon material 51. That is, the carbon nanotubes CNT are applied to the substrate 36P for the positive electrode 3 together with the positive electrode active material 52P in the state of composite material paste 37P (see Figure 2 ). In the secondary battery 1 of the present embodiment, the carbon nanotubes CNT dispersed in the positive electrode composite material layer 32P thus function as a conductive material that forms a conductive path of the positive electrode active material 52P located near the carbon nanotubes CNT.

[0025] And, for example, in Figure 5 When the positive electrode material layer 32BP of the reference example shown contains a granular substance such as carbon black CB as the conductive material, the positive electrode material layer 32BP has a dense structure, which tends to reduce the fluidity of the electrolyte 50 impregnated in the positive electrode material layer 32BP.

[0026] In contrast, in the secondary battery 1 of this embodiment, Figure 4 As shown, by including the fibrous carbon nanotubes CNT, a large number of fine gaps are formed in the positive electrode composite material layer 32P. In the secondary battery 1 of the present embodiment, the electrolyte 50 impregnated in the positive electrode composite material layer 32P has high fluidity.

[0027] And, if Figure 6 As shown, in the secondary battery 1 of the present embodiment, the positive electrode composite material layer 32P constituting the positive electrode 3 and the negative electrode composite material layer 32N constituting the negative electrode 4 have inherent thicknesses Dp and Dn, respectively. Furthermore, these positive electrode composite material layers 32P and negative electrode composite material layers 32N respectively have inherent fluidity index values ​​indicating the fluidity of the electrolyte 50 after impregnation. In the secondary battery 1 of the present embodiment, by managing the thicknesses Dp and Dn of these positive electrode composite material layers 32P and negative electrode composite material layers 32N, and managing the fluidity index value of the electrolyte 50 after impregnation, the high rate characteristics of the secondary battery 1 can be improved.

[0028] If described in detail, the secondary battery 1 of the present embodiment has a so-called double-sided laminated structure in which the electrode composite material layer 32 is laminated on both sides of the sheet-shaped substrate 36 constituting the positive and negative electrode sheets 35. That is, in the electrode sheet 35P constituting the positive electrode 3, the amount of a single side laminated on one of the front and back sides of the substrate 36 constitutes the single-sided thickness Dhp of the positive electrode composite material layer 32P. In the electrode sheet 35N constituting the negative electrode 4, the amount of a single side laminated on one of the front and back sides of the substrate 36 constitutes the single-sided thickness Dhn of the negative electrode composite material layer 32N. In addition, the value obtained by doubling these single-sided thicknesses Dhp and Dhn constitutes the amount of both sides of the electrode composite material layer 32 laminated on the substrate 36, that is, the double-sided thickness Ddp of the positive electrode composite material layer 32P and the double-sided thickness Ddn of the negative electrode composite material layer 32N. In the present embodiment, the values ​​of the double-side thicknesses Ddp and Ddn are managed as the thickness Dp of the positive electrode composite material layer 32P and the thickness Dn of the negative electrode composite material layer 32N, respectively.

[0029] Specifically, in the secondary battery 1 of this embodiment, the thickness Dp of the positive electrode composite material layer 32P is controlled by adjusting the pressing pressure, speed, etc. when applying the composite material paste 37P to the carbon nanotubes CNT as the conductive material and the substrate 36P.

[0030] For example, in the secondary battery 1 of the present embodiment, carbon nanotubes CNT having a specific surface area value of 150 or more and 300 or less by the BET method are used. The unit of the BET specific surface area value is [m 2 / g] (square meter / gram). In addition, the pressing pressure is set to, for example, 40 kN or more and 100 kN or less. In addition, the coating speed is set to, for example, a range of 6 m / min and 120 m / min. In the secondary battery 1 of the present embodiment, the thickness Dp of the positive electrode composite material layer 32P is controlled to, for example, 0.034 mm or more and 0.050 mm or less.

[0031] In the secondary battery 1 of this embodiment, the thickness Dn of the negative electrode composite material layer 32N is controlled by adjusting the carbon-based material such as graphite and the binder and thickener added to the composite material paste 37N, as well as the pressing pressure, coating speed, and the like.

[0032] For example, in the secondary battery 1 of the present embodiment, the binder added to the composite paste 37N uses styrene-butadiene copolymer (SBR), styrene-acrylic acid copolymer (SAR), etc. The thickener uses carboxymethyl cellulose (CMC), etc.

[0033] Furthermore, the pressing pressure is set to, for example, 10 kN or more and 50 kN or less. Furthermore, the coating speed is set to, for example, a range of 6 m or more and 120 m or less. In the secondary battery 1 of the present embodiment, the thickness Dn of the negative electrode composite material layer 32N is controlled to, for example, 0.060 mm or more and 0.080 mm or less.

[0034] Furthermore, in the secondary battery 1 of the present embodiment, the thickness Dp of the positive electrode composite material layer 32P and the thickness Dn of the negative electrode composite material layer 32N, as well as their density and porosity are controlled. For example, the density of the positive electrode composite material layer 32P is controlled to be greater than 2.2g / cc and less than 2.9g / cc. Furthermore, the density of the negative electrode composite material layer 32N is controlled to be greater than 0.9g / cc and less than 1.2g / cc. Furthermore, the porosity of the positive electrode composite material layer 32P is controlled to be greater than 37% and less than 51%, for example. Furthermore, the porosity of the negative electrode composite material layer 32N is controlled to be greater than 45% and less than 55%, for example.

[0035] In addition, the electrolyte 50 of the present embodiment uses, for example, ethylene carbonate (EC), ethyl methyl carbonate (EMC), dimethyl carbonate (DMC), etc. Furthermore, their composition ratio is set, for example, in the manner of EC=1, 1≦EMC≦1.5, 1≦DMC≦1.5. In addition, in this case, the specific gravity of the electrolyte 50 is in the range of 1.1 or more and 1.3 or less. Thus, the electrolyte 50 of the present embodiment has a viscosity based on its composition.

[0036] In the secondary battery 1 of the present embodiment, the fluidity index value of the electrolyte 50 impregnated into the electrode composite material layer 32 uses the liquid flow rate Q. Specifically, the liquid flow rate Q represents the weight of the electrolyte 50 flowing out of the electrode composite material layer 32 per unit pressure and per unit volume acting on the electrode composite material layer 32 by applying pressure to the electrode composite material layer 32 in a state wound in the form of an electrode sheet 35 for a specified time. In addition, in the secondary battery 1 of the present embodiment, the specified time for applying pressure to the electrode composite material layer 32 is set to 3 minutes, and the liquid flow rate Q is expressed as [g (@3min) / kPa·mm -3 ]("g(@3min) / kPa·mm3"). Therefore, in the secondary battery 1 of the present embodiment, the liquid flow rate Qp on the positive electrode 3 side is 7.8×10 -7 Above and 8.8×10 -6 The following values. In addition, “×10 -7 " is "10 to the power of -7", "×10 -6 ” is “10 to the negative sixth power” (the same applies hereinafter). In the secondary battery 1 of the present embodiment, the liquid flow rate Qn on the negative electrode 4 side is 2.4×10 -6 Above and 1.1×10 -5 The following values.

[0037] More specifically, in the secondary battery 1 of the present embodiment, as shown in the following equation, the liquid flow rate Q, which is an index of the fluidity of the electrolyte 50 impregnated into the electrode mixture layer 32, is configured so that the positive electrode 3 side is larger than the negative electrode 4 side.

[0038] Qp>Qn···(1) Specifically, the value obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side preferably satisfies the following formula (2).

[0039] Qp-Qn≧0.48×10 -6 ···(2) Likewise, it is more preferable that the value obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side satisfies the following formula (3).

[0040] Qp-Qn≧0.66×10 -6 ···(3) Therefore, the secondary battery 1 of the present embodiment can improve the high-rate characteristics of the secondary battery 1 .

[0041] (Method for measuring liquid flow rate) like Figure 7 and Figure 8 As shown, when measuring the liquid flow rate Q, samples 60 used in measuring the liquid flow rate Q are prepared from the positive and negative electrode sheets 35 constituting the electrode body 10 of the secondary battery 1 .

[0042] Specifically, first, a strip-shaped sample sheet 62 having a predetermined length L and a predetermined width W is cut out from the actual electrode sheet 35. Next, the sample sheet 62 is wound around a rod-shaped member 63, and the wound sample sheet 62 is fixed by a winding fixing tape (not shown). Thereafter, in this state, the rod-shaped member 63 on which the sample sheet 62 is wound is removed, thereby forming a measurement sample 60 having a structure as a wound body similar to the electrode body 10 of the secondary battery 1.

[0043] like Fig. 9 As shown, in the secondary battery 1 of this embodiment, the sample 60 formed as described above is arranged in a measurement case 64 constituted as a sealed container. Then, in this state, a pressure P is applied to the sample 60 for a predetermined time, thereby measuring the weight of the electrolyte 50 flowing out of the electrode composite material layer 32.

[0044] Specifically, if Fig.10 As shown, first, the electrolyte 50 is filled into the shell 64 to which the sample 60 is added, thereby the electrolyte 50 is impregnated into the sample 60, and in detail, the electrolyte 50 is impregnated into the electrode composite material layer 32 (step 101). In addition, the hole portion of the sample 60 formed by pulling out the rod-shaped member 63 as described above is sealed liquid-tightly, for example, by inserting a rod-shaped rubber plug 65. Next, the electrolyte 50 in the shell 64 is discharged, thereby forming a state in which only the sample 60 impregnated with the electrolyte 50 is arranged in the shell 64 (step 102). Thereafter, in this state, the shell 64 is pressurized to a specified pressure P using a pressurizing device 66 connected to the shell 64 (step 103).

[0045] Next, the pressurized state is maintained for a predetermined time t (step 104: No). In addition, as described above, in the secondary battery 1 of the present embodiment, the predetermined time t is "3 minutes". Furthermore, after the predetermined time t has passed (step 104: Yes), the weight of the electrolyte 50 accumulated in the housing 64, that is, the electrolyte 50 flowing out of the sample 60 due to the pressurization, is measured and taken as the electrolyte outflow Fw (step 105). And, in the secondary battery 1 of the present embodiment, the liquid flow rate Qs of each sample 60 is calculated based on the electrolyte outflow Fw measured in step 105.

[0046] If detailed, Fig.11 As shown, in the secondary battery 1 of the present embodiment, the prescribed pressure P acting on the sample 60 in the shell 64 is changed to implement the above-mentioned pressurized electrolyte outflow Fw measurement. For example, the first prescribed pressure P1 is set to "37kPa", the second prescribed pressure P2 is set to "104kPa", and the third prescribed pressure P3 is set to "165kPa", and the pressurized electrolyte outflow Fw measurement is respectively performed. And, regarding the pressurized measurement under these prescribed pressures P1, P2, and P3, for example, without changing the sample 60, each prescribed pressure P1, P2, and P3 is measured for 3 minutes in order from low to high. And, thereby, the electrolyte outflow Fw1, Fw2, and Fw3 obtained at each prescribed pressure P1, P2, and P3 are associated with each prescribed pressure P1, P2, and P3 and plotted on the XY coordinates.

[0047] That is, the weight of the electrolyte 50 flowing out of the sample 60 by pressurization, i.e., the electrolyte outflow Fw, becomes a value corresponding to the predetermined pressure P acting on the sample 60. Therefore, by plotting the measurement results on the XY coordinates as described above, a linear approximation (y=ax+b) representing the relationship between them can be obtained. And, in the secondary battery 1 of the present embodiment, the liquid flow rate Qs of each sample 60 expressed as [g(@3min) / kPa] is calculated based on the slope of the linear approximation.

[0048] And, if Figure 7 and Figure 8 As shown, in the secondary battery 1 of this embodiment, the volume V of the electrode composite layer 32 in the sample 60 is determined by the length L and width W of the sample sheet 62 constituting the sample 60 and the thickness D of the electrode composite layer 32 as shown in the following formula.

[0049] V=D×L×W···(4) Specifically, in the secondary battery 1 of the present embodiment, the length L of the sample sheet 62 is specified as "500 mm" and the width W is specified as "55 mm". Furthermore, as described above, the liquid flow rate Q, which is an index value of the fluidity of the electrolyte 50 impregnated in the electrode composite material layer 32 of the electrode body 10 constituting the secondary battery 1, is expressed as "g (@3 minutes) / kPa·cubic millimeter". That is, the liquid flow rate Q represents the value of the weight of the electrolyte 50 flowing out of the electrode composite material layer 32 per unit pressure and per unit volume acting on the electrode composite material layer 32 by applying a pressure P to the electrode composite material layer 32 in a state wound in the form of an electrode sheet 35 for a specified time t. Therefore, as shown in the following formula, the liquid flow rate Q, which is an index value of fluidity, is a value obtained by dividing the liquid flow rate Qs of each sample 60 by the volume V of the electrode composite material layer 32 in the sample 60.

[0050] Q=Qs / V···(5) Furthermore, in the secondary battery 1 of this embodiment, by utilizing this point, the above Figure 7 to Figure 11 In each of the steps shown, the liquid flow rate Q is measured as an index value of the fluidity of the electrolyte solution 50 impregnated into the electrode mixture layer 32 constituting the electrode body 10 of the secondary battery 1 .

[0051] (effect) like Figure 12 to Figure 14 As in the secondary battery 1B of the reference example shown in FIG. 1 , when high-rate current is applied, the salt concentration of the electrolyte 50 tends to vary between the positive electrode 3 and the negative electrode 4. Fig.13 During high rate discharge as shown, the lithium ion concentration on the negative electrode 4 side tends to increase. Fig.14 During high rate charging as shown, the lithium ion concentration on the negative electrode 4 side tends to decrease. The resulting uneven salt concentration increases the internal resistance, thereby deteriorating the charge and discharge performance.

[0052] In this regard, in the secondary battery 1 of the present embodiment, as described above, the thicknesses Dp and Dn of the positive electrode composite material layer 32P and the negative electrode composite material layer 32N constituting the electrode body 10 are managed. Furthermore, for these positive electrode composite material layers 32P and negative electrode composite material layers 32N, the liquid flow rates Qp and Qn, which are indicators of the fluidity of the electrolyte 50 impregnated therein, are managed, respectively.

[0053] The results, such as Figure 15 to Figure 17 As shown, even when high-rate current is applied, the salt concentration of the electrolyte 50 is unlikely to vary between the positive electrode 3 and the negative electrode 4. This can suppress deterioration in charge and discharge performance of the secondary battery 1 due to high-rate current application.

[0054] Next, the effects of this embodiment will be described. (1) The secondary battery 1 includes an electrode body 10 formed by winding an electrode sheet 35P for a positive electrode 3 and an electrode sheet 35N for a negative electrode 4, which are stacked with a separator 5. Each electrode sheet 35P and 35N is formed by stacking an electrode composite layer 32 on a substrate 36 as a current collector 31. In addition, when a pressure P is applied to the electrode composite layer 32 for a predetermined time t in a state in which the electrode sheet 35 is wound, the weight of the electrolyte 50 flowing out of the electrode composite layer 32 per unit pressure and per unit volume applied to the electrode composite layer 32 is taken as a liquid flow rate Q. Furthermore, the liquid flow rate Q is taken as an index value of the fluidity of the electrolyte 50 impregnated into the electrode composite layer 32. When the predetermined time t in which the pressure P is applied to the electrode composite layer 32 is 3 minutes, the liquid flow rate Q is expressed as "g (@3 minutes) / kPa·mm3". The value (Qp-Qn) obtained by subtracting the liquid flow rate Qn of the negative electrode composite material layer 32N from the liquid flow rate Qp of the positive electrode composite material layer 32P is 0.48×10 -6 The above method is used to construct.

[0055] According to the above configuration, high-rate current conduction can suppress variations in salt concentration in the electrolyte 50 impregnated into the electrode assembly 10 . This can improve the high-rate characteristics of the secondary battery 1 .

[0056] (2) The liquid flow rate Qp of the positive electrode composite material layer 32P is 7.8×10 -7 Above and 8.8×10 -6 The thickness Dp of the positive electrode composite material layer 32P is 0.034 mm or more and 0.050 mm or less. Furthermore, the liquid flow rate Qn of the negative electrode composite material layer 32N is 2.4×10 -6 Above and 1.1×10 -5 The thickness Dn of the negative electrode mixture layer 32N is 0.060 mm or more and 0.080 mm or less. This can effectively improve the high rate characteristics of the secondary battery 1.

[0057] (3) The positive electrode composite material layer 32P contains carbon nanotubes CNT as the conductive fibrous carbon material 51 . That is, by including the fibrous carbon nanotubes CNT, a large number of fine gaps are formed in the positive electrode composite material layer 32P, thereby ensuring high fluidity of the electrolyte solution 50 impregnated in the positive electrode composite material layer 32P.

[0058] In addition, the above-mentioned embodiment can be implemented by changing as follows. The above-mentioned embodiment and the following modification examples can be implemented in combination with each other within the range of no technical contradiction.

[0059] In the above-mentioned embodiment, the secondary battery 1 has a so-called double-sided laminated structure in which the electrode composite material layer 32 is laminated on both sides of the sheet-shaped substrate 36 constituting the positive and negative electrode sheets 35. Therefore, the thickness Ddp and Ddn of both sides of the positive electrode composite material layer 32P and the negative electrode composite material layer 32N are used as the thickness Dp of the positive electrode composite material layer 32P and the thickness Dn of the negative electrode composite material layer 32N. However, it is not limited to this, and it can also be applied to the so-called single-sided laminated structure in which the positive and negative electrode sheets 35 have the electrode composite material layer 32 laminated only on one side of the substrate 36. In this case, the single-sided thickness Dhp of the positive electrode composite material layer 32P and the single-sided thickness Dhn of the negative electrode composite material layer 32N can be used as the thickness Dp and Dn of the positive electrode composite material layer 32P and the negative electrode composite material layer 32N, respectively.

[0060] In the above embodiment, the liquid flow rate Q, which is an index value of the fluidity of the electrolyte 50, is expressed as [g (@3min) / kPa·mm -3 ] ("g (@3 min) / kPa · cubic millimeter"). In this case, the liquid flow rate Qp of the positive electrode composite material layer 32P is 7.8×10 -7 Above and 8.8×10 -6 The liquid flow rate Qn of the negative electrode composite material layer 32N is 2.4×10 -6 Above and 1.1×10 -5 The following values. Furthermore, the thickness Dp of the positive electrode composite material layer 32P is greater than or equal to 0.034 mm and less than or equal to 0.050 mm. The thickness Dn of the negative electrode composite material layer 32N is greater than or equal to 0.060 mm and less than or equal to 0.080 mm. However, this is not limited to this, and these values ​​can be arbitrarily changed within the range satisfying the relationship of the above formula (2). Preferably, it can be within the range satisfying the relationship of the above formula (3).

[0061] · It can be further expanded to a range that satisfies the relationship of the above formula (1) according to the level required by the high rate characteristics. That is, it can be a configuration in which "the fluidity index value of the electrolyte 50 impregnated into the electrode composite material layer 32 is larger on the positive electrode 3 side than on the negative electrode 4 side". In this case, for example, as the fluidity index value, an index value other than the liquid flow rate Q described in detail in the above embodiment, such as a value including the concept of outflow speed, can also be used.

[0062] Furthermore, the density and porosity of the positive electrode composite material layer 32P and the negative electrode composite material layer 32N can be changed arbitrarily. The pressing pressure and speed when applying the composite material paste 37 to the substrate 36 can also be changed arbitrarily. The conductive material, the binder and the thickening material can also be changed arbitrarily.

[0063] In the above embodiment, the positive electrode composite material layer 32P contains carbon nanotubes CNT as the conductive fibrous carbon material 51. However, this is not limited to this, and for example, other conductive fibrous carbon materials such as carbon nanofibers (CNF) may be used as the conductive material. In addition, specifications such as the so-called BET specific surface area value may also be changed arbitrarily. The positive electrode composite material layer 32P does not necessarily need to contain such a conductive fibrous carbon material 51.

[0064] In the above embodiment, the sample 60 used for measuring the liquid flow rate Q is formed using a sample sheet 62 having a length L of "500 mm" and a width W of "55 mm". However, this is not limiting, and the size of the sample sheet 62, that is, the volume V of the electrode composite material layer 32 in the sample 60 formed using the sample sheet 62 can also be changed arbitrarily.

[0065] In the above embodiment, when measuring the liquid flow rate Q, the prescribed time t for applying pressure to the electrode composite material layer 32 is set to 3 minutes, and the weight of the electrolyte 50 flowing out of the sample 60 due to the pressurization, i.e., the electrolyte outflow Fw, is measured. However, this is not limited to this, and the prescribed time t can also be changed arbitrarily.

[0066] · In addition, in the above-mentioned embodiment, the first prescribed pressure P1 is set to "37kPa", the second prescribed pressure P2 is set to "104kPa", and the third prescribed pressure P3 is set to "165kPa", and the measurement of the electrolyte outflow Fw based on the pressurization is carried out. The electrolyte outflow Fw1, Fw2, and Fw3 obtained for each of the prescribed pressures P1, P2, and P3 are associated with each prescribed pressure P1, P2, and P3 and plotted on the XY coordinates, thereby calculating the liquid flow rate Qs for each sample 60. However, it is not limited to this, and the measurement of the electrolyte outflow Fw based on the pressurization can be performed twice or more than four times. In addition, at each time of implementation, the value of the pressure P acting on the electrode composite material layer 32 of the sample 60 can also be changed arbitrarily.

[0067] In the above embodiment, the secondary battery 1 is a lithium ion secondary battery. However, the present invention is not limited to this, and the above embodiment can also be applied to secondary batteries 1 other than lithium ion secondary batteries.

[0068] The terminal shapes of the positive terminal 38P and the negative terminal 38N are not limited to Figure 1 The shape shown in the figure can be changed arbitrarily. The shape of the case 20 as the outer shape of the secondary battery 1 is not necessarily limited to a flat rectangular box shape, and can be changed arbitrarily to a cylindrical shape, for example.

[0069] Next, technical ideas that can be grasped from the above-mentioned embodiment and modified examples will be described. (A) An electrode body formed by winding positive and negative electrode sheets stacked with separators, each electrode sheet being formed by stacking an electrode composite material layer on a substrate serving as a current collector, and the fluidity index value of the electrolyte impregnated in the above-mentioned electrode composite material layer is larger on the positive electrode side than on the negative electrode side. Example

[0070] Examples and the like are described below for further specifying the configuration and effects of the present invention, but the present invention is not limited to these examples. Fig.18 and Fig.19 The table and the graph show in a list the test results on the influence of the liquid flow rates Qp and Qn of the positive electrode composite material layer 32P and the negative electrode composite material layer 32N constituting the electrode assembly 10 on the high rate characteristics of the secondary battery 1 .

[0071] To explain in detail, the columns (1) and (2) in the table are the liquid flow rates Qsp and Qsn on the positive electrode 3 side and the negative electrode 4 side of each sample 60 described in detail in the above embodiment. That is, in this characteristic test, the measurement of the liquid flow rates Qsp and Qsn of each sample 60 is carried out by the method described in detail in the above embodiment for "Example 1" to "Example 4" and "Comparative Example 1" to "Comparative Example 7". Therefore, the units of the liquid flow rates Qsp and Qsn of each sample 60 shown in the columns (1) and (2) in these tables are [g (@3min) / kPa].

[0072] If described in further detail, in this characteristic test, the electrode composite material layer 32 of each sample 60 corresponding to "Example 1" to "Example 4" and "Comparative Example 1" to "Comparative Example 7" has inherent thicknesses Dp and Dn. In addition, in the table, the thickness Dp of the positive electrode composite material layer 32P and the thickness Dn of the negative electrode composite material layer 32N shown in the specification column (3) (4) are the thicknesses Ddp and Ddn on both sides, respectively. Moreover, all of these samples 60 are formed using a sample sheet 62 with a length L of "500mm" and a width W of "55mm". That is, as shown in formula (4) in the above embodiment, the electrode composite material layer 32 of each sample 60 in "Example 1" to "Example 4" and "Comparative Example 1" to "Comparative Example 7" has an inherent volume V based on the difference in its thickness D. In addition, in the table, the values ​​shown in columns (5) and (6) are the liquid flow rates Qp and Qn per unit volume obtained by dividing the liquid flow rates Qsp and Qsn of each sample 60 by the inherent volume V of the electrode composite material layer 32 of each sample 60 according to the above formula (5). Therefore, the units of the liquid flow rates Qp and Qn are [g (@3min) / kPa·mm -3 ].

[0073] Moreover, the value in column (7) of the table is the value obtained by subtracting the value in column (6) from the value in column (5), that is, the value (Qp - Qn) obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side. In addition, regarding the evaluation index of the high-rate performance shown in column (8) of the table, the "resistance increase rate" is used. That is, this resistance increase rate is the increase rate [%] of the internal resistance (CD-IR) after performing a charge-discharge cycle test in which charging and discharging are repeatedly performed for a certain period of time with a large current (tens of amperes or more) equivalent to high-rate charging and discharging. Therefore, the smaller the value of the high-rate performance shown in each figure, the smaller the deterioration of the charge-discharge performance based on high-rate charging and discharging. That is, it shows more excellent high-rate performance.

[0074] As Fig.18 and Fig.19 shown, in "Example 1" to "Example 4", the values shown in column (7) of the table are all "positive". That is, the value obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side is "positive" (Qp - Q > 0). That is, when comparing the liquid flow rates Qp and Qn as the fluidity index values of this electrolyte 50, it is larger on the positive electrode 3 side than on the negative electrode 4 side (Qp > Qn). The "resistance increase rate (%)" as the evaluation index values of the high-rate performance in these "Example 1" to "Example 4" are "107", "110", "107", and "108" respectively, and they are all excellent values.

[0075] In contrast, except for "Comparative Example 1", in "Comparative Example 2" to "Comparative Example 7", the values obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side are all "negative" (Qp - Qn < 0). That is, when comparing these liquid flow rates Qp and Qn, it is smaller on the positive electrode 3 side than on the negative electrode 4 side (Qp < Qn). When the required level of the "resistance increase rate (%)" as the evaluation index value of the high-rate performance is set to "114", the values of the "resistance increase rate (%)" in these "Comparative Example 2" to "Comparative Example 7" are all larger than the required level value. That is, as a result, a significant improvement effect of the high-rate performance is not obtained. In addition, in "Comparative Example 1", although the value obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side is slightly "positive", its "resistance increase rate (%)" is "114".

[0076] Moreover, when comparing "Example 1" to "Example 4", "Example 1", "Example 3", and "Example 4" show particularly excellent high-rate performance. In addition, when comparing these "Example 1" to "Example 4", the value shown in column (7) of this table is the smallest in "Example 2". The value of "Example 2" is "0.48×10 -6 ".

[0077] Based on the test results, in the above embodiment, the relationship of formula (2) is derived as the preferred numerical range. That is, it can be confirmed that when the liquid flow rate Q is expressed as "g (@3min) / kPa·m3", the preferred numerical range is "Qp-Qn≧0.48×10 -6 " is appropriate.

[0078] In addition, regarding the improvement effect of the high-rate characteristics when the value obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side is "positive", this change point can also be found from the test results of "Example 1" to "Example 4".

[0079] If detailed, Fig.19 In the figure, the auxiliary line m1 is recorded, which is a point where the value obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side is "0" and the point representing the test result of "Example 2" is used as a reference. It is thus confirmed that the area where the high-rate characteristics are improved relatively sharply as the value obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side increases. In addition, the figure confirms the area where higher high-rate characteristics are obtained, which is represented by the auxiliary line m2 using the points representing the test results of "Example 1", "Example 3" and "Example 4" as a reference. Furthermore, the change point of the improvement effect of the high-rate characteristics is observed from the intersection of these two auxiliary lines m1 and m2. When the liquid flow rate Q is expressed as "g (@3 min) / kPa·mm3", the change point is located at the value obtained by subtracting the liquid flow rate Qn on the negative electrode 4 side from the liquid flow rate Qp on the positive electrode 3 side. -6 ” location.

[0080] Based on the above test results, in the above embodiment, the relationship of formula (3) is derived as a more preferable numerical range. That is, it can be confirmed that “Qp-Qn≧0.66×10 -6 " is appropriate. It is speculated that in cases where the level required for high-rate characteristics is relatively gentle, by excluding "Comparative Example 1" in consideration of measurement errors, the preferred numerical range can be expanded to the range represented by the above formula (1) (Qp-Qn>0).

[0081] Furthermore, in "Example 1" to "Example 4", the liquid flow rate Qp on the positive electrode 3 side is "7.8×10 -7 "Above and "8.8×10 -6". In addition, in these "Example 1" to "Example 4", the thickness Dp of the positive electrode composite material layer 32P is in the range of "0.034 mm" or more and "0.050 mm" or less. In addition, in these "Example 1" to "Example 4", the liquid flow rate Qn on the negative electrode 4 side is in the range of "2.4×10 -6 " and above and "1.1×10 -5 " is within the range of less than "0.060 mm". The thickness Dn of the negative electrode composite material layer 32N of these "Example 1" to "Example 4" is all within the range of more than "0.060 mm" and less than "0.080 mm".

[0082] From the above, it can be confirmed that the liquid flow rate Qp and thickness Dp of the positive electrode mixture layer 32P and the liquid flow rate Qn and thickness Dn of the negative electrode mixture layer 32N shown as preferred numerical ranges in the above embodiment are appropriate.

Claims

1. A secondary battery, wherein: An electrode body is provided in which positive and negative electrode sheets are layered and wound with separators interposed therebetween. Each electrode sheet is formed by laminating an electrode composite material layer on a substrate as a current collector, and In a state where the electrode sheet is wound, when a predetermined time and pressure are applied to the electrode composite material layer, the weight of the electrolyte flowing out of the electrode composite material layer per unit pressure applied to the electrode composite material layer and per unit volume of the electrode composite material layer are used as fluidity index values ​​of the electrolyte impregnated into the electrode composite material layer. The predetermined time for causing the pressure to act on the electrode composite material layer is set to 3 minutes, When the fluidity index value of the electrolyte is expressed as "g (@3 minutes) / kPa·m3", The value obtained by subtracting the fluidity index value of the negative electrode composite material layer from the fluidity index value of the positive electrode composite material layer is 0.48×10 -6 above.

2. The secondary battery according to claim 1, wherein The fluidity index value of the positive electrode composite material layer is 7.8×10 -7 Above and 8.8×10 -6 the following.

3. The secondary battery according to claim 1, wherein The thickness of the positive electrode composite material layer is greater than or equal to 0.034 mm and less than or equal to 0.050 mm.

4. The secondary battery according to claim 1, wherein The fluidity index value of the negative electrode composite material layer is 2.4×10 -6 Above and 1.1×10 -5 the following.

5. The secondary battery according to claim 1, wherein The thickness of the negative electrode composite material layer is greater than or equal to 0.060 mm and less than or equal to 0.080 mm.

6. The secondary battery according to any one of claims 1 to 5, wherein The positive electrode composite material layer contains a conductive fibrous carbon material.