Continuous current switch for superconducting electromagnets

By using magnet continuous current switches of low-temperature and high-temperature superconducting materials in series in superconducting magnets, the problems of long ramp-up time and large thermal load of superconducting magnets in the existing technology are solved, and efficient ramp-up and cooling are achieved. Cooling time and helium losses are reduced.

CN118786771APending Publication Date: 2024-10-15KONINKLIJKE PHILIPS NV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202380019035.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-01-27
Filing Date
2023-01-26
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

Existing superconducting magnets take a long time to ramp up, and the cooling process will cause helium to evaporate and increase the temperature, which increases the heat load of the magnet.

Method used

A magnet continuous current switch using low-temperature superconducting material (lts segment) and high-temperature superconducting material (hts segment) in series is used. The hts segment has high resistance in the superconducting state, reducing heat dissipation, and effectively passing through heaters and thermal switches. Take the heat away and increase your ramp speed.

Benefits of technology

Rapid ramp heating and cooling at high voltage is achieved, reducing the heat load on the magnet, shortening the cooling time, and reducing helium loss.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118786771A_ABST
    Figure CN118786771A_ABST
Patent Text Reader

Abstract

A persistent current switch (10) for a superconducting magnet, the persistent current switch comprising a length of superconducting wire having an electrical connection port (16) at its end and a heater (13) for supplying heat to the superconducting wire. The section of superconducting wire comprises an LTS section (11) made of a low-temperature superconducting material and an HTS section (12) made of a high-temperature superconducting material. Preferably, two LTS sub-segments (11) and one HTS segment (12) are electrically connected in series in an alternating manner.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a magnet continuous current switch for a superconducting magnet. The superconducting magnet is formed as an electromagnet having a magnet winding of a superconducting material. When current is introduced into the magnet winding and the magnet winding is cooled below the superconducting critical temperature of the magnet winding material, the current continues to flow through the winding and generates a continuous magnetic field.

[0002] M. Wilson explains continuous mode operation of superconducting magnets in Section 11.2 of his book Superconducting Magnets (Oxford University Press, 1983, ISBN 0-19-854805-2).

[0003] Continuous mode operation of a superconducting magnet is achieved by connecting a superconducting switch in series with a superconducting magnetic field generating coil. The switch comprises an electrical switch in the form of a switchable electrical connector and having a length of superconducting wire wound on a support structure in such a way that it does not contribute to the magnetic field of the magnet. In continuous operation, the switch carries the entire magnet current. Heating the switch to a temperature above the superconducting transition temperature causes the switch to become resistive. A power supply connected in parallel with the switch can then be used to vary the current in the magnetic field generating coil. Background Art

[0004] Such a magnetic continuous current switch is known from the international application WO 2019 / 096567.

[0005] The magnet continuous current switch known from international application WO2015 / 096567 has a section of superconducting wire which is part of the magnet winding. That is, part of the winding of the superconducting magnetic field generating coil is circuitized to operate as the superconducting wire of the magnet continuous current switch.

[0006] A magnetic continuous current switch made of a high-temperature superconductor is known from European patent application EP 4 024 415. Summary of the invention

[0007] It is an object of the present invention to provide a magnet persistence current switch which enables the time required for ramping up of a superconducting magnet to be reduced.

[0008] This object is achieved by a magnet continuous current switch for a superconducting magnet, the magnet continuous current switch comprising:

[0009] a length of superconducting wire having an electrical connection port at an end of the length of superconducting wire,

[0010] A heater for supplying heat to the section of superconducting wire, wherein:

[0011] The section of superconducting wire includes an lts section of low-temperature superconducting material and an hts section of high-temperature superconducting material.

[0012] An insight of the present invention is that the heat dissipation in a magnet continuous current switch (MPCS) during ramping up or ramping down (i.e., when current is flowing through the section of wire) is inversely proportional to the resistance (ohms) of the material of the section of wire. The HTS section of the section of wire is formed of a high temperature superconductor material, which has a very high resistance in its normal state. Therefore, when the temperature is above the critical temperature of superconductivity of the HTS section, the HTS section and the section of wire as a whole have very low heat dissipation during the ramp change of the magnet. Because only a very small amount of heat dissipated by the magnet continuous current switch needs to be taken away from the superconducting magnet, the heat dissipation of the magnet continuous current switch is taken away quickly and a high ramp speed is achieved. This high ramp speed is mainly achieved by the higher ramp voltage allowed, with almost no (heat) losses dissipated into the refrigerant system of the magnet. In conventional cases, a ramp voltage of 5V is used in most cases. The present invention enables the ramp voltage to be increased to, for example, 20V or even higher. Because the resistivity of the high temperature superconducting ceramic material is one or several orders of magnitude higher than the resistivity of the low temperature superconducting material of the lts segment, the length of the hts segment can be one or several orders of magnitude shorter than the length of the wire of the conventional MPCS. In practice, the lts segment is made of a metal (Cu) matrix or cladding that holds the low temperature superconducting material, and the resistance of the lts segment may be determined by the resistivity of the metal matrix or cladding.

[0013] In general, the MPCS of the invention is used in superconducting magnets to energize superconducting magnets and switch to continuous mode (and vice versa) to discharge these magnets. In state-of-the-art superconducting magnets (such as MRI magnets), the magnet coils are made of standard superconducting wire (also called lts - low temperature superconductor), for example NbTi and the MPCS are made of the same material. The switch is opened (= becomes normal) by heating the wire to a temperature above the critical temperature of the wire. During the energization of the magnet, the same voltage used to energize the magnet (= the inductor voltage on the magnet coil) is also applied to the MPCS in the "on" state. This causes dissipation (V 2 / R). For so-called sealed magnets (magnets not immersed in a pool of liquid helium), this dissipation leads to helium evaporation and / or temperature increase. In addition, the invention achieves a reduction in the thermal load of the low temperature (4K) structure of the magnet. This reduces the amount of helium lost when applied to magnets whose windings are cooled by immersing them in liquid helium.

[0014] According to the present invention, the MPCS comprises a section of wire of at least two different materials connected in series: one section (LTS section) is made of LTS wire, and the other section (HTS section) is made of HTS wire. HTS is a ceramic material, and its resistance is very high in a normal state. Therefore, when the MPCS is heated to a temperature higher than the critical temperature of the LTS wire and the HTS wire, the resistance of the MPCS becomes very high, and the dissipation during power-on (or discharge) becomes very low.

[0015] The hts and lts segments may be formed as a straight or twisted length of wire, or may be wound into, for example, a solenoid.

[0016] The MPCS of the present invention generally achieves the following aspects:

[0017] During energization or discharge, the losses in the magnet (except the heater) are reduced due to the MPCS. Less heat load means the magnet gets hotter less during energization (or discharge). Therefore less time is needed to cool down.

[0018] By using a magnet power supply with a higher ramp voltage, high speed ramp up and / or high speed ramp down can be used. A gradient amplifier can be used instead of a dedicated magnet power supply. This therefore reduces the ramp up / ramp down power up and discharge times. This is important for 3T sealed magnets, i.e. within the temperature window (T 自动放电 -T 开始通电 ) and the ability to automatically discharge before quenching, or have a reasonable T 自动放电 When using high-speed power-up, T 开始通电 It could be higher.

[0019] Instead of using a quench button (when using high ramp-down voltages), a fast (controlled) ramp-down is possible: a 1.5 T magnet ramps down in e.g. 5 minutes.

[0020] These and other aspects of the invention will be further elaborated with reference to the embodiments defined in the dependent claims.

[0021] In one example of the MPCS of the present invention, the hts segment is formed of a ceramic high temperature superconducting material (e.g., MgB2 or YBaCuO, or other hts cuprates), preferably without a metallic conductive matrix or coating, so that the hts segment as a whole has a high ohmic resistance in its normal state above its superconducting critical temperature. Yttrium barium copper oxide (YBCO) is a family of crystalline compounds that exhibit high temperature superconductivity; it includes the first material discovered to date that becomes superconducting at about 93K above the boiling point of liquid nitrogen (77K). Many YBCO compounds have the general formula Yba2Cu3O7x), although there are also materials with other Y:Ba:Cu ratios, such as YBa2Cu4Oy (Y124) or Y2Ba4Cu7Oy(). It is part of the more common rare earth barium copper oxide (ReBCO), in which other rare earth elements are present instead of yttrium. These materials are suitable for high temperature superconducting segments. Magnesium boride, which has a critical temperature of about 39K, can also be used in high temperature superconducting segments.

[0022] In one example of MPCS, the present invention is implemented as a series arrangement of two lts segments and an hts segment between the lts segments.

[0023] Drift and voltage noise of the magnet power supply may cause changes in the current flowing through the LTS segment and the HTS segment because they are connected in series. In particular, when the HTS segment is cooled to return to its superconducting state, in the final stage of the ramp change of the superconducting magnet in the transition state near the critical temperature of the HTS segment, a changing micropath that becomes superconducting may appear, and the local dissipation caused by the above-mentioned current change may offset the superconducting state. During the process of the HTS segment transitioning from its normal state to its superconducting state, the LTS segment remains in its normal (resistance) conductive state. The resistance of the LTS segment reduces the voltage noise on the HTS segment of the MPCS, thereby reducing the loss of the microchannels in the HTS segment. In practice, the ohmic resistance of the LTS segment may be determined by the resistivity of the conductive (e.g., Cu) matrix (coating or matrix) in which the low-temperature superconducting material (e.g., NbTi) is set. The HTS segment preferably does not contain any conductive material as a coating or matrix. During the cooling process at the last stage of the temperature increase process, i.e. when the MPCS is cooled, there is a moment when the HTS segment may be partially superconducting and partially in the normal state. Ceramic superconductor materials consist of a large number of grains or domains, which may have slightly different ratios of composite elements, or may have slightly different crystal structures, or may be at slightly different temperatures and different (stray) magnetic fields, so the effective superconducting critical temperature may have a distribution of varying values ​​on the HTS segment. During the recovery of the superconducting state, in the almost final stage, only a few grains or domains are still in the normal resistive state, i.e. there may be an "almost superconducting path" in which a string of grains is superconducting and one or a few grains are still in the normal state. The presence of the series LTS segment, which is still resistive, cancels out the entire voltage noise on these one or a few grains. However, in this case, the main dissipation of heat will be provided by the LTS segment in series with the HTS segment, so the final grains or domains will also be effectively cooled to below their respective superconducting critical temperature values. The voltage applied by the magnet power supply across the wire length of the MPCS is divided so that the larger contribution is on the LTS segment and at most only a small portion of the voltage is divided on the HTS segment. Therefore, there is at most very low heat dissipation on the HTS segment. Therefore, when approaching the superconducting critical temperature of the HTS material, the HTS segment can be effectively cooled by the cryogen system and stably restore its superconducting state while the LTS segment is still in its normal resistance state. Some form of conductive metallic material or metal oxide can be used as a matrix, substrate or coating to increase the uniformity of heat dissipation on the HTS segment during cooling, because the current will be transferred from the part of the ceramic high temperature superconducting material that is still in the normal conductive state to the metal or metal oxide. Since the resistance of such a metal or metal oxide of the HTS segment is much smaller than the resistance of the LTS segment, the power consumption on the HTS segment is kept low, so the time required for ramping can be shortened due to the higher ramp voltage. The HTS segment has a much higher resistance than the LTS segment in the normal state.Therefore, with the addition of a matrix / substrate / cladding, the resistance should still be much higher than that of the lts segment, but may be a compromise to make the transition to the normal state easier.

[0024] In another example of the MPCS of the present invention, a capacitor forms a parallel circuit with the electrical connection port, so that when the voltage source (usually called the magnet power supply) is ramped, the capacitor is connected in parallel with the magnet power supply. This acts as a low pass filter, i.e. as a shortcut for high frequency noise that may appear during the ramp. The capacitor short-circuits high frequency noise caused by changes in the conductivity of the high temperature superconducting section. The low pass filter avoids current fluctuations through the MPCS, which may be caused by EM field fluctuations caused by changes caused by external noise sources (such as the main power supply, passing vehicles, etc.). The magnet windings are sensitive to this and may pass voltage noise to the MPCS.

[0025] In another example of the MPCS of the present invention, a shunt conductor in series with a controllable switch forms a parallel circuit with the LTS segment and / or the HTS segment, and optionally also on the LTS segment. The controllable switch is set in its open state when the HTS segment is in its normal state and has a high ohmic resistance, i.e. during ramp up / down, the voltage is applied by the magnet power supply. During cooling, when the superconducting magnet is in continuous mode, the controllable switch is closed. The shunt conductor protects the HTS segment in the event of a quench of the superconductivity of the HTS segment, since the current will pass through the shunt conductor and the resistive LTS segment, where the energy from the HTS segment is dissipated.

[0026] In another example of the MPCS of the present invention, a thermal switch is provided between the HTS segment and the thermal connection port. The thermal connection port establishes an entry point for a thermal path to a low-temperature (e.g., 4K) structure of the magnet, which is cooled by the magnet's cryogen system. When implemented in a superconducting magnet, the HTS segment is thermally coupled to a thermal buffer of the superconducting magnet's cryogen system via the thermal switch. During the cooling of the HTS segment, the thermal switch is closed, allowing heat to be more efficiently transferred from the HTS segment to the thermal buffer, which reduces the time required to cool the HTS segment to become a superconducting segment. In continuous mode, the thermal switch is opened to thermally insulate the HTS wire.

[0027] In another example, the LTS segment includes several LTS sub-segments, and the HTS segment includes one or several HTS sub-segments, and the LTS sub-segments and the one or several HTS sub-segments alternately form a series circuit. Therefore, the HTS sub-segments are connected in series between the LTS sub-segments. In particular, the LTS sub-segments can be wound into solenoids, which are connected in series by relatively short wires forming the HTS segments.

[0028] The present invention also relates to a superconducting magnet comprising an assembly of a superconducting magnet winding and an MPCS, wherein the superconducting wire segments comprise an lts segment of a low temperature superconducting material and an hts segment of a high temperature superconducting material. The superconducting magnet of the present invention can be ramped up at a high voltage, so that the time required for ramping up / down is shorter.

[0029] In one example of the superconducting magnet of the present invention, a cryogen system is coupled to the magnet winding assembly, and a magnet continuous current switch has a thermal connection port that is thermally coupled to a thermal buffer of the cryogen system through a thermal switch. When the thermal switch is closed, the thermal connection port thermally corresponds to the HTS segment of the MPCS. This provides a thermal path to bring heat from the HTS segment to the thermal buffer while thermally isolating the HTS segment during continuous mode operation.

[0030] In addition, the present invention relates to a method for ramping up / ramping down the superconducting magnet of the present invention. During the van der MPCS cooling process, especially when the temperature rise process is nearing the end, the thermal switch will be closed. The thermal switch can also be closed at the end of the descent process to carry away the heat generated during the descent process in a controlled manner. In one embodiment, the method for ramping up / ramping down includes controlling a controllable switch in a shunt wire. In another embodiment, the method of the present invention includes controlling a thermal switch between an HTS segment and a thermal connection port, which is thermally connected to a thermal buffer in the refrigerant system of the superconducting magnet. The control of the controllable switch and the thermal switch can be implemented independently or in combination.

[0031] With the present invention, when used in a magnetic resonance examination system, it is possible to use a gradient amplifier that can be incorporated into the magnet, since the magnet power supply can be used entirely for tilting the magnet, as well as tilting the magnet using the gradient coils. Both have the capability of high ramp speeds. See previous invention disclosure (already filed as a patent). A dedicated MPS providing high voltage is of course also possible. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] These and other aspects of the invention will be elucidated with reference to the embodiments described hereinafter and with reference to the accompanying drawings, in which:

[0033] Figure 1 and Figure 2 A schematic diagram of an MPCS incorporating the present invention is shown, the MPCS having a lts segment of a certain length of lts wire and an hts segment as a piece of hts, with a heater at the hts segment or also having a heater for the lts segment;

[0034] Figure 3 and Figure 4 shows a schematic diagram of an MPCS incorporating the present invention, the MPCS having parallel electrical switches that are closed during cooling (recovery to a superconducting state) of the hts segment; Figure 3 Only the electricity is switched to the hts segment, Figure 4 Switch to the hts segment and (part of) the lts segment; and

[0035] Figure 5 A schematic diagram of an MPCS incorporating the present invention is shown, wherein the MPCS is thermally switched to a thermal buffer to quickly cool the MPCS (particularly the hts section). DETAILED DESCRIPTION

[0036] Figure 1 and Figure 2 A schematic diagram of an MPCS incorporating the present invention is shown, the MPCS having a lts segment of a certain length of lts wire and an hts segment as a piece of hts, with a heater at the hts segment or also having (one or more) heaters for the lts segment. Figure 1 and Figure 2 In the example of , the LTS segment 11 consists of two sub-segments, and the HTS segment 12 forms a series circuit between the LTS segment 11. An electrical connection port 16 is provided, to which a magnet winding (not shown) and a magnet power supply for injecting current into the magnet winding can be switchably connected. The heater 13 is placed close to the HTS segment so that when in operation, the heater 13 diffuses heat to the HTS segment as well as the LTS segment. The heater 13 is controlled by a control unit 14. When the magnet ramp temperature changes, the control unit activates the heater so that the HTS segment 12 and / or the LTS sub-segment 11 are in their normal resistance state. When the LTS sub-segment 13 and the HTS segment 12 are to be restored to the superconducting state, the control unit 14 turns off the heater because when the (one or more) heaters 13, 21 are turned off, the LTS sub-segment 13 and the HTS segment 12 are cooled by the refrigerant system of the magnet. In Figure 2 In the example of FIG. 1 , an additional heater 21 is provided near the lts subsection 21 to more efficiently distribute heat over a section of superconducting wire 11 , 12 .

[0037] Figure 3 and Figure 4 shows a schematic diagram of an MPCS incorporating the present invention, wherein electrical switches are connected in parallel and closed during cooling (recovery to a superconducting state) of the hts segment; Figure 3 Switch to hts segment only, Figure 4 Switch to the hts section and (part of) the lts section. Figure 3 In the example of , a shunt conductor with a switch is connected in parallel with the HTS segment 12. Figure 4 In the example of FIG. 4 , a shunt conductor 41 with a switch 42 is connected in parallel between the lts sub-segment and the hts segment.

[0038] Figure 5A schematic diagram of an MPCS incorporating the present invention is shown, which is thermally switched to a thermal buffer to rapidly cool the MPCS (especially the hts segment). The superconducting wires 11, 12 of a segment of MPCS 10 are thermally coupled to a thermal conductor 54 made of a material with good thermal conductivity. The thermal conductor is in thermal contact with one end of a thermal switch 51, and the other end of the thermal switch 51 is in thermal contact 52 with a thermal buffer 53. The thermal switch can be activated by a control unit 14.

Claims

1. A magnet continuous current switch (10) for a superconducting magnet, the magnet continuous current switch include: a length of superconducting wire having an electrical connection port (16) at an end of the length of superconducting wire, A heater (12, 21) for supplying heat to the section of superconducting wire, wherein: The section of superconducting wire comprises an lts section (11) of low-temperature superconducting material and an hts section (13) of high-temperature superconducting material.

2. The magnetic continuous current switch according to claim 1, in, The hts segment is formed of a ceramic high temperature superconducting material.

3. The magnetic continuous current switch according to claim 1 or 2, in, The capacitor and the electrical connection port form a parallel circuit.

4. A magnetic continuous current switch according to any one of the preceding claims, in, A shunt conductor (31, 41) connected in series with a controllable switch (32, 42) forms a parallel circuit with the lts segment and / or the hts segment.

5. A magnet continuous current switch according to any preceding claim, comprising a thermal switch between the hts segment and a thermal connection port.

6. A magnetic continuous current switch according to any one of the preceding claims, in, The lts segment includes several lts sub-segments, and the hts segment includes one or several hts sub-segments, and the lts sub-segments and the one or several hts sub-segments alternately form a series circuit.

7. A superconducting magnet comprising an assembly of magnet windings and a magnet continuous current switch according to any one of claims 1 to 4.

8. A superconducting magnet comprising an assembly of magnet windings, a cryogen system coupled to said assembly of magnet windings, and a magnet continuous current switch according to claim 5, in, The thermal connection port is thermally coupled to a thermal buffer of the refrigerant system.

9. A method for ramping the temperature of a superconducting magnet according to claim 4, include: When the hts segment is in its normal conducting state, the controllable switch controlling the shunt conductor (31, 41) is in its open state.

10. A method of ramping the temperature of a superconducting magnet according to claim 7, comprising controlling the thermal switch in its closed state during the ramp up.