Step tailing discarding type beneficiation method for high-magnification semi-oxide silicon-calcium collophanite

Through the cascade tailing process and multi-stage separation processing, the problem of beneficiation of high-aluminum, high-iron, low-grade silica-calcium colloidal phosphate ore has been solved, efficient concentrate separation and low-cost production have been achieved, and the quality and efficiency of phosphoric acid production have been improved. .

CN118807960APending Publication Date: 2024-10-22BLUESTAR LEHIGH ENG INST CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202410976164.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-10-22

AI Technical Summary

Technical Problem

When existing technology processes high-aluminum, high-iron, low-grade silica-calcium collophosphate ore, the traditional process suffers from fine grinding fineness, fine concentrate particle size, high concentrate ore dressing costs, difficulty in approval of tailings ponds, poor selectivity of chemicals, P2O5 The problem of low recovery rate leads to poor physical properties and reduced quality during the production of phosphoric acid.

Method used

The cascade tailing process is adopted, through two-stage crushing, photoelectric screening, heavy media screening, spiral chute gravity separation and positive flotation process, combined with fine crushing, grinding and slurry processing, using photoelectric separation, X-ray light separation, wireless Press the third product cyclone and ultra-limit spiral chute, add inhibitors to reduce impurity content, and achieve deep tailings and concentrate separation.

Benefits of technology

It effectively reduces the cost of mineral processing and equipment load, improves the grade and quality of phosphate concentrate, reduces the grade of tailings, reduces the cost of subsequent processing and environmental pollution, and improves the efficiency and product quality of phosphoric acid production.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to a step tailing discarding type beneficiation method for high-power semi-oxide silicon-calcium collophanite, and belongs to the technical field of mineral processing. The method comprises the following steps: crushing and screening raw ores, feeding the oversize ores into a photoelectric separator, and feeding the undersize ores into a dense medium operation receiving bin; fine concentrates in the photoelectric separation operation are fed to a dense medium operation receiving bin after being crushed; oversize materials obtained through screening are fed to dense medium operation, and undersize materials are fed to a spiral chute reselection operation stock bin; dense medium operation concentrate and materials in a spiral chute gravity separation operation stock bin are subjected to ore grinding and then fed into a spiral chute for tailing discarding, and spiral chute concentrate and tailings are obtained; the spiral chute tailings are subjected to size mixing and then are subjected to direct flotation to obtain direct flotation concentrate; and the spiral chute operation concentrate and the direct flotation operation concentrate are mixed to obtain final concentrate. According to the method, the subsequent ore grinding and flotation cost is effectively reduced, water is saved, all wastewater is recycled, and the treatment cost is low. The method has the advantages of being stable in beneficiation technological process, good in separation effect, low in iron and aluminum sesquioxide content of concentrate products and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of mineral processing, and in particular relates to a step-by-step tailings discarding process for high-sesquioxide calcium-silicon collophanite. Background Art

[0002] In my country, phosphate resources are mainly concentrated in Yunnan, Guizhou, Sichuan, Hunan, Hubei and other places, mainly sedimentary phosphorite, among which medium and low-grade collophanite is the main one. Some low-grade siliceous collophanites contain high levels of aluminum and iron sesquioxides (R2O3). In the traditional wet production of phosphoric acid, there are clear requirements for iron and aluminum sesquioxides: the sesquioxide content of Class I phosphate concentrate shall not exceed 2.5%; the sesquioxide content of Class II phosphate concentrate shall not exceed 3.0%. The content of iron and aluminum oxides in phosphate ore is often expressed as R2O3 (R represents Fe and Al, that is, Fe2O3+Al2O3). Iron and aluminum not only interfere with the growth of calcium sulfate crystals, but also cause phosphoric acid to form sludge. Phosphate ore reacts with acid to generate water-insoluble complex phosphates, which will cause a large loss of P2O5 when precipitated or removed with gypsum. The resulting complex phosphates of iron and aluminum have fine crystals, which not only increase the viscosity of the solution and slurry, but also easily clog the pores of the filter cloth and filter cake. The phosphates of iron and aluminum will also bring difficulties to post-processing such as the concentration and drying of phosphoric acid or ammonium phosphate slurry, and lead to poor product properties and quality degradation. Therefore, in order to reduce the impact on the wet phosphoric acid and acid fertilizer production process, it is necessary to reduce the content of iron and aluminum sesquioxides in the phosphate concentrate as much as possible.

[0003] At present, for high-aluminum, high-iron, low-grade calcareous colloidal phosphate, the conventional process flow is the direct-reverse flotation process and the pre-de-sludge-double-reverse flotation process. The direct-reverse flotation process has the disadvantages of fine grinding fineness, fine concentrate product particle size, difficult concentrate transportation and dehydration operations, and high concentrate dressing costs. In addition, the direct-reverse flotation process must rely on tailings ponds to operate normally, and it is difficult for new phosphate mines to approve tailings ponds. The pre-de-sludge-double-reverse flotation process has the disadvantages of poor reagent selectivity, the process is greatly affected by ore slime, serious P2O5 loss in de-sludge operation, and low final concentrate P2O5 recovery rate. At present, as the grade of mined phosphate ore is getting lower and lower, if the flotation process is directly used, the grinding cost, dehydration cost and flotation cost are getting higher and higher. If the degree of dissociation of useful minerals and gangue minerals is used, the cascade pre-selection and tailings discarding process is used for low-grade phosphate ore before flotation, the dressing cost and equipment load can be greatly reduced. Summary of the invention

[0004] The purpose of the present invention is to address the deficiencies of the prior art and to propose a more reasonable and efficient cascade tailings removal process for high-quasi-oxide calcium-silicon collophanite, which is a silicate, carbonate, iron-containing and aluminum-containing gangue minerals in the collophanite.

[0005] In order to achieve the purpose of the present invention, the present invention adopts the following technical solutions: The present invention is a step-by-step tailings disposal process for high-sesquioxide calcium-silicon collophanite, which is characterized by the following steps: (1) The raw ore is crushed in two stages, and the crushed material is fed to the photoelectric screening operation. The material above the screen is fed to the photoelectric screening operation, and the material below the screen is fed to the heavy medium operation receiving bin; (2) The concentrate from the photoelectric separation operation is fed into the fine crushing equipment for further crushing, and the crushed material is fed into the receiving bin for the heavy medium operation; (3) Heavy medium operation: The material in the receiving silo is fed to the heavy medium screening operation, the material on the screen is fed to the heavy medium operation, and the material under the screen is fed to the heavy medium operation. The material is fed to the spiral chute gravity separation operation silo; (4) The heavy medium concentrate and the material in the spiral chute gravity separation silo are fed to the grinding operation, and the ground ore is fed to the spiral chute operation for further tailings discarding to obtain the spiral chute concentrate and tailings; (5) After slurry adjustment, the spiral chute tailings are fed into the direct flotation operation to obtain the direct flotation concentrate; (6) The spiral chute concentrate and the direct flotation concentrate are combined to obtain the final concentrate; The ore composition of high-semioxide type collophanite is: P2O5 grade is 15.0%~30.0%, MgO mass content is 1.0%~6.0%, SiO2 mass content is 11.1%~36.5%, Al2O3 mass content is 1.0%~8.8%, and Fe2O3 mass content is 0.5%~6.0%.

[0006] The method of the present invention has a further preferred technical solution: the two-stage crushing operation of the raw ore in step (1) and / or (2) adopts a jaw crusher and a cone crusher, the photoelectric separation operation is mainly suitable for phosphate ore with a particle size of 8 to 50 mm, and the photoelectric separation equipment adopts an X-ray optical separator or a color separator.

[0007] The method of the present invention has a further preferred technical solution: in step (3), the fine crushing operation adopts a high-pressure roller mill, an impact crusher or an impact crusher, the heavy medium operation is suitable for phosphate ore with a particle size of 1 to 10 mm, and the heavy medium operation adopts a pressureless three-product cyclone.

[0008] The method of the present invention has a further preferred technical solution: in step (4), the grinding equipment is a ball mill, a rod mill, a tower mill, or a high-pressure roller mill + a ball mill, a high-pressure roller mill + a rod mill, or a high-pressure roller mill + a tower mill.

[0009] The method of the present invention has a further preferred technical solution: in step (4), the spiral chute gravity separation operation adopts an ultra-limit spiral chute with a pitch-to-diameter ratio of 0.3-0.45, and the grinding fineness applicable to the spiral chute gravity separation is -200 mesh, which is 40-80%.

[0010] The principle of the method of the present invention is that the mineral composition of the siliceous-calcium collophosphate ore is single, mainly low-carbon fluoroapatite, a small amount of carbon apatite and apatite, and the gangue minerals are mainly divided into three parts: carbonate minerals, silicate minerals, and iron-containing minerals. The carbonate minerals are mainly dolomite and calcite, the silicate minerals are mainly quartz, aluminum silicate clay minerals, and the iron-containing minerals are mainly pyrite and hematite. The difference in density, color, texture structure and light reflectivity between useful minerals and gangue minerals is used to achieve the pre-selection and tailing of the ore. The spiral chute tailings separated by the spiral chute operation are mainly fine-grained phosphate ore. By adding a combined inhibitor in the positive flotation process, the three impurity minerals of iron, aluminum and magnesium in the original ore can be effectively suppressed to achieve the purpose of simple impurity removal.

[0011] Compared with conventional flotation process, the patent of this invention has the following advantages: (1) Based on the properties of the ore, photoelectric pre-selection, medium and spiral chute series pre-selection processes are adopted to achieve maximum tailings discarding, reduce the tailings grade and effectively reduce the subsequent grinding, flotation and dehydration costs; (2) Through the deep cascade tailings dumping process of low-grade phosphate ore, high-grade phosphate ore rough concentrate, low-grade phosphate ore rough concentrate and tailings are produced, so that the high-quality phosphate concentrate can be used for the best quality and the low-quality phosphate concentrate can be used for the best quality; (3) By adding water glass, sodium lignin sulfonate and naphthalene sulfonate formaldehyde condensate, polysaccharides and polyphenols as inhibitors of gangue minerals in the positive flotation desiliconization operation, the floating difference between useful minerals and gangue minerals is increased, and the content of three impurities of iron, aluminum and magnesium in phosphate concentrate is greatly reduced; (4) The mineral processing wastewater generated by this process only needs simple treatment before being discharged, causing little pollution to the environment. DETAILED DESCRIPTION

[0012] Example 1, Experiment 1 of the step-by-step tailings beneficiation method for high-sesquioxide calcium-silicon collophanite: (1) The raw ore is crushed by a jaw crusher and a cone crusher. The crushed material is fed to a 10mm photoelectric screening operation. The +10mm on the screen is fed to an X-ray optical separator for photoelectric screening, and the -10mm under the screen is fed to a heavy medium receiving bin; (2) The concentrate from the photoelectric separation operation is fed into the fine crushing equipment for further crushing, and the crushed material is fed into the receiving bin for the heavy medium operation; (3) The material in the receiving bin of the heavy medium operation is fed to the 1mm heavy medium screening operation, the material on the screen with +1mm is fed to the pressureless three-product cyclone for heavy medium operation, and the material under the screen with -1mm is fed to the spiral chute gravity separation operation bin; (4) Feed the heavy medium concentrate and the materials in the spiral chute gravity separation silo to the high pressure roller mill + ball mill for grinding, with a grinding fineness of -200 mesh 70%, and feed them to the ultra-limit spiral chute for further tailings removal, with a pitch-to-diameter ratio of 0.4, to obtain the spiral chute concentrate and tailings; (5) The tailings in the spiral chute are fed into the heavy tailing thickener, and the bottom flow of the thickener is fed into the direct flotation after slurry adjustment. The tailings are used as fillers after dehydration. The direct flotation process mainly removes aluminum silicate minerals, carbonates and iron-containing minerals. Sodium carbonate is used as a pH adjuster, water glass is used as a silicate mineral inhibitor, sodium lignin sulfonate is used as a carbonate inhibitor, humic acid is used as an iron-containing mineral inhibitor, and an anionic fatty acid collector is used as a collector; (6) The spiral chute concentrate and the direct flotation concentrate are combined to obtain the final concentrate.

[0013] The ore composition of the high-sesquioxide type collophanite in the above method is P2O5 grade of 23.21%, MgO mass content of 3.52%, SiO2 mass content of 14.19%, Al2O3 mass content of 4.70%, Fe2O3 mass content of 2.25%; The P2O5 grade in the collophanite concentrate obtained by the above method is 33.45%, the MgO mass content is 0.55%, and the sesquioxide (R2O3) mass content is 2.07%.

[0014] Example 2, Experiment 2 of the step-by-step tailings beneficiation method for high-sesquioxide calcium-silicon collophanite: (1) The raw ore is crushed by a jaw crusher and a cone crusher. The crushed material is fed to a 15mm photoelectric screening operation. The +15mm on the screen is fed to an X-ray optical separator for photoelectric selection, and the -15mm under the screen is fed to a heavy medium receiving bin; (2) The concentrate from the photoelectric separation operation is fed into the fine crushing equipment for further crushing, and the crushed material is fed into the receiving bin for the heavy medium operation; (3) The material in the receiving bin of the heavy medium operation is fed to the 1mm heavy medium screening operation, the material on the screen with +1mm is fed to the pressureless three-product cyclone for heavy medium operation, and the material under the screen with -1mm is fed to the spiral chute gravity separation operation bin; (4) Feed the heavy medium concentrate and the materials in the spiral chute gravity separation silo to the high pressure roller mill + ball mill for grinding, with a grinding fineness of -200 mesh 70%, and feed them to the ultra-limit spiral chute for further tailings removal, with a pitch-to-diameter ratio of 0.4, to obtain spiral chute concentrate, middlings and tailings; (5) The tailings in the spiral chute are fed into the heavy tailing thickener, and the bottom flow of the thickener is fed into the direct flotation after slurry adjustment. The tailings are used as fillers after dehydration. The direct flotation process mainly removes aluminum silicate minerals, carbonates and iron-containing minerals. Sodium carbonate is used as a pH adjuster, water glass is used as a silicate mineral inhibitor, sodium lignin sulfonate is used as a carbonate inhibitor, humic acid is used as an iron-containing mineral inhibitor, and an anionic fatty acid collector is used as a collector; (6) The spiral chute concentrate and the flotation concentrate are combined to obtain the final concentrate.

[0015] The ore composition of the high-sesquioxide type collophanite in the above method is P2O5 grade of 23.21%, MgO mass content of 3.52%, SiO2 mass content of 14.19%, Al2O3 mass content of 4.70%, Fe2O3 mass content of 2.25%; The P2O5 grade in the collophanite concentrate obtained by the above method is 33.56%, the MgO mass content is 0.56%, and the sesquioxide (R2O3) mass content is 2.32%.

[0016] Example 3, Experiment 3 of the step-by-step tailings beneficiation method for high-sesquioxide calcium-silicon collophanite: (1) The raw ore is crushed by a jaw crusher and a cone crusher. The crushed material is fed to a 10mm photoelectric screening operation. The +10mm on the screen is fed to an X-ray optical separator for photoelectric screening, and the -10mm under the screen is fed to a heavy medium receiving bin; (2) The concentrate from the photoelectric separation operation is fed into the fine crushing equipment for further crushing, and the crushed material is fed into the receiving bin for the heavy medium operation; (3) The material in the receiving bin of the heavy medium operation is fed to the 2mm heavy medium screening operation, the material on the screen with +2mm is fed to the pressureless three-product cyclone for heavy medium operation, and the material under the screen with -2mm is fed to the spiral chute gravity separation operation bin; (4) Feed the heavy medium concentrate and the materials in the spiral chute gravity separation silo to the high pressure roller mill + ball mill for grinding, with a grinding fineness of -200 mesh 65%, and feed them to the ultra-limit spiral chute for further tailings removal, with a pitch-to-diameter ratio of 0.4, to obtain spiral chute concentrate, middlings and tailings; (5) The tailings in the spiral chute are fed into the heavy tailing thickener, and the bottom flow of the thickener is fed into the direct flotation after slurry adjustment. The tailings are used as fillers after dehydration. The direct flotation process mainly removes aluminum silicate minerals, carbonates and iron-containing minerals. Sodium carbonate is used as a pH adjuster, water glass is used as a silicate mineral inhibitor, sodium lignin sulfonate is used as a carbonate inhibitor, humic acid is used as an iron-containing mineral inhibitor, and an anionic fatty acid collector is used as a collector; (6) The spiral chute concentrate and the flotation concentrate are combined to obtain the final concentrate.

[0017] The ore composition of the high-sesquioxide type collophanite in the above method is 25.21% P2O5, 1.51% MgO, 13.22% SiO2, 3.55% Al2O3 and 1.89% Fe2O3; The P2O5 grade in the collophanite concentrate obtained by the above method is 33.61%, the MgO mass content is 0.40%, and the sesquioxide (R2O3) mass content is 2.22%.

[0018] Example 4, Experiment 4 of the step-by-step tailings beneficiation method for high-sesquioxide calcium-silicon collophanite: (1) The raw ore is crushed by a jaw crusher and a cone crusher. The crushed material is fed to a 15mm photoelectric screening operation. The +15mm on the screen is fed to an X-ray optical separator for photoelectric selection, and the -15mm under the screen is fed to a heavy medium receiving bin; (2) The concentrate from the photoelectric separation operation is fed into the fine crushing equipment for further crushing, and the crushed material is fed into the receiving bin for the heavy medium operation; (3) The material in the receiving bin of the heavy medium operation is fed to the 2mm heavy medium screening operation, the material on the screen with +2mm is fed to the pressureless three-product cyclone for heavy medium operation, and the material under the screen with -2mm is fed to the spiral chute gravity separation operation bin; (4) Feed the heavy medium concentrate and the materials in the spiral chute gravity separation silo to the high pressure roller mill + ball mill for grinding, with a grinding fineness of -200 mesh 65%, and feed them to the ultra-limit spiral chute for further tailings removal, with a pitch-to-diameter ratio of 0.4, to obtain spiral chute concentrate, middlings and tailings; (5) The tailings in the spiral chute are fed into the heavy tailing thickener, and the bottom flow of the thickener is fed into the direct flotation after slurry adjustment. The tailings are used as fillers after dehydration. The direct flotation process mainly removes aluminum silicate minerals, carbonates and iron-containing minerals. Sodium carbonate is used as a pH adjuster, water glass is used as a silicate mineral inhibitor, sodium lignin sulfonate is used as a carbonate inhibitor, humic acid is used as an iron-containing mineral inhibitor, and an anionic fatty acid collector is used as a collector; (6) The spiral chute concentrate and the direct flotation concentrate are combined to obtain the final concentrate.

[0019] The ore composition of the high-sesquioxide type collophanite in the above method is 25.21% P2O5, 1.51% MgO, 13.22% SiO2, 3.55% Al2O3 and 1.89% Fe2O3; The P2O5 grade of the collophanite concentrate obtained by the above method is 33.35%, the MgO mass content is 0.44%, and the sesquioxide (R2O3) mass content is 2.15%.

[0020] Example 5, a comparative experiment on the step-by-step tailings discarding process for high-sesquioxide calcareous collophosphate: The following table compares the costs of the process of the present invention with those of the conventional forward and reverse flotation process and the double reverse flotation process: .

Claims

1. A step-by-step tailings beneficiation method for high-sesquioxide calcium-silicon collophanite, characterized in that: The steps of this method are as follows: (1) The raw ore is crushed in two stages, and the crushed material is fed to the photoelectric screening operation. The material above the screen is fed to the photoelectric screening operation, and the material below the screen is fed to the heavy medium operation receiving bin; (2) The concentrate from the photoelectric separation operation is fed into the fine crushing equipment for further crushing, and the crushed material is fed into the heavy medium operation receiving bin; (3) The material in the heavy medium operation receiving bin is fed into the heavy medium screening operation, and the material on the screen is fed into the heavy medium operation, and the material under the screen is fed into the heavy medium operation. The material is fed to the spiral chute gravity separation operation silo; (4) The heavy medium concentrate and the material in the spiral chute gravity separation silo are fed to the grinding operation, and the ground ore is fed to the spiral chute operation for further tailings discarding to obtain the spiral chute concentrate and tailings; (5) After slurry adjustment, the spiral chute tailings are fed into the direct flotation operation to obtain the direct flotation concentrate; (6) The spiral chute concentrate and the direct flotation concentrate are combined to obtain the final concentrate; The ore composition of high-semioxide type collophanite is: P2O5 grade is 15.0%~30.0%, MgO mass content is 1.0%~6.0%, SiO2 mass content is 11.1%~36.5%, Al2O3 mass content is 1.0%~8.8%, and Fe2O3 mass content is 0.5%~6.0%.

2. The ore dressing method according to claim 1, characterized in that: In step (1) and / or (2), the two-stage crushing operation of the raw ore adopts a jaw crusher and a cone crusher, the particle size of the phosphate material in the photoelectric separation operation is 8-50 mm, and the photoelectric separation equipment adopts an X-ray optical sorter or a color sorter.

3. The ore dressing method according to claim 1, characterized in that: In step (3), the fine crushing operation adopts a high pressure roller mill, an impact crusher or an impact crusher, the particle size of the phosphate material in the heavy medium operation is 1-10 mm, and the heavy medium operation adopts a pressureless three-product cyclone.

4. The ore dressing method according to claim 1, characterized in that: In step (4), the grinding equipment is a ball mill, a rod mill, a tower mill, or a high pressure roller mill + a ball mill, a high pressure roller mill + a rod mill, or a high pressure roller mill + a tower mill.

5. The ore dressing method according to claim 1, characterized in that: In step (4), the spiral chute gravity separation operation adopts an ultra-limit spiral chute with a pitch-to-diameter ratio of 0.3-0.45, and the grinding fineness of the spiral chute gravity separation is -200 mesh and is 40-80%.

6. The ore dressing method according to claim 1, characterized in that: The ground ore is fed into the spiral chute, which includes roughing, cleaning or scavenging. When the mud content of the ground slurry is greater than 20% (-0.038mm), a cyclone desludging operation is added before the re-selection operation.

7. The ore dressing method according to claim 1, characterized in that: The spiral chute concentrate is processed in two ways according to the grade and particle size distribution. One is to use it as concentrate directly, and the other is to feed it to a high-frequency screen. The concentrate on the screen is used as gravity concentrate, and the concentrate under the screen is fed to the positive flotation operation.

8. The ore dressing method according to claim 1, characterized in that: Before the spiral chute tailings are fed into the direct flotation operation, they must first be fed into the thickener. The overflow of the thickener returns to the direct flotation return water sedimentation tank, and the underflow of the thickener is fed into the direct flotation operation. The spiral chute tailings can be re-grinded or directly fed into the direct flotation process according to the dissociation situation. The tower mill or ball mill is used for re-grinding. The direct flotation process mainly removes carbonate minerals, aluminosilicate minerals and iron-containing minerals.

9. The ore dressing method according to claim 8, characterized in that: In the positive flotation process, sodium carbonate is used as a pH adjuster, water glass is used as an inhibitor of silicate minerals, sodium lignin sulfonate and naphthalene sulfonate formaldehyde condensate are used as inhibitors of carbonate minerals, polysaccharides and polyphenols are used as inhibitors of iron-containing minerals, and fatty acid soap organic matter is used as a collector.

Citation Information

Cited By

  • Green and efficient beneficiation method for silico-calcareous phosphorite