Method for preparing 2, 5-furandicarboxylic acid through continuous reaction of biomass sugar
By using a homogeneous metal salt catalyst and a co-oxidant on biomass sugar to carry out dehydration and oxidation reactions, the problem of low yield and purity in the continuous reaction of biomass sugar to prepare 2,5-furandicarboxylic acid is solved, and hydrogen bromide is reduced. Used to achieve efficient and low-cost FDCA preparation.
Patent Information
- Application Number
- CN202410679518.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-29
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-05-29
AI Technical Summary
In the existing technology, when 2,5-furandicarboxylic acid is prepared from biomass sugar through continuous reaction, the yield and purity of the product are low, and the use of hydrogen bromide in the oxidation reaction will cause equipment corrosion.
A homogeneous metal salt catalyst is used to perform a dehydration reaction on biomass sugar to generate 5-hydroxymethylfurfural, and then a co-oxidant and acetic acid are added to perform an oxidation reaction under the action of the oxidation catalyst to separate 2,5-furandicarboxylic acid and reduce or Avoid the use of hydrogen bromide.
It improves the yield and purity of FDCA, reduces the risk of equipment corrosion, and improves production efficiency and cost-effectiveness.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of 2,5-furandicarboxylic acid preparation, and in particular to a method for preparing 2,5-furandicarboxylic acid by continuous reaction of biomass sugar. Background Art
[0002] The development of biodegradable plastics is urgent. Among them, PEF (polyethylene furanoate), a substitute for PET, has attracted much attention due to its excellent heat resistance and barrier properties. However, its industrialization is currently still restricted by the high price of the biomass-based monomer 2,5-furandicarboxylic acid (FDCA).
[0003] In the preparation of FDCA, fructose is dehydrated to generate 5-hydroxymethylfurfural (HMF), and HMF is then oxidized to FDCA, which is a common route. However, fructose is currently expensive, and some biomass sugars with large output and low price are more suitable as raw materials for large-scale industrial production of FDCA, for example: glucose isomerization to obtain fructose, fructose is then dehydrated to generate HMF, and then further oxidized to prepare FDCA.
[0004] Lewis acid generally has a good catalytic effect on the conversion of biomass sugar into HMF, but HMF has poor stability and is prone to hydrolysis in a high-temperature acidic aqueous phase to produce byproducts such as levulinic acid. In addition, it may also undergo dehydration condensation to form humin under high-temperature reaction conditions. The occurrence of these side reactions causes the purity of the HMF obtained by the reaction to be low. If a continuous reaction method is adopted (i.e., after the dehydration reaction is completed, the product HMF is not separated and purified, and the oxidation reaction is directly carried out), the byproducts contained in the dehydration reaction product will affect the subsequent oxidation reaction, resulting in a low yield and purity of FDCA prepared from biomass sugar. For example, in patent CN115028608A, the intermediate product HMF is not separated and purified, and FDCA is directly prepared from glucose, with a yield of only 44.1%. Summary of the invention
[0005] In order to solve the technical problem that the yield and purity of the product FDCA are low when FDCA is prepared by continuous reaction of biomass sugar, the present invention provides a method for preparing 2,5-furandicarboxylic acid by continuous reaction of biomass sugar. The method can improve the yield and product purity of FDCA prepared by continuous reaction of biomass sugar, and at the same time reduce or even avoid the use of hydrogen bromide in the oxidation reaction, thereby reducing the corrosion of hydrogen bromide to equipment.
[0006] The specific technical scheme of the present invention is: A method for preparing 2,5-furandicarboxylic acid by continuous reaction of biomass sugars, comprising the following steps: Under the action of a homogeneous metal salt catalyst, biomass sugar is used as a raw material to undergo a dehydration reaction to generate 5-hydroxymethylfurfural, and a co-oxidant and acetic acid are added to the dehydration reaction liquid obtained after the reaction is completed. The co-oxidant is one or more of acetaldehyde, triacetaldehyde and methyl ethyl ketone. Under the action of an oxidation catalyst, an oxidation reaction is carried out in an oxidizing gas atmosphere, and then 2,5-furandicarboxylic acid is separated.
[0007] The present invention adopts a continuous reaction method to prepare FDCA, and the dehydration reaction product HMF is not separated and purified before the oxidation reaction, which can improve production efficiency and reduce the cost of HMF separation and purification. In order to solve the problem of low yield and purity of FDCA when the continuous reaction method is adopted, the present invention uses a specific co-oxidant, which undergoes an oxidation reaction with HMF, HMF is converted into FDCA, and the co-oxidant is converted into acetic acid, which can reduce the impact of by-products in the dehydration reaction process on the final product and promote the oxidation reaction of HMF→FDCA, thereby reducing or even avoiding the use of hydrogen bromide in the oxidation reaction to reduce equipment corrosion, and achieving a higher FDCA yield and purity.
[0008] The three co-oxidants (acetaldehyde, trimeraldehyde, and methyl ethyl ketone) used in the present invention can effectively reduce the impact of by-products in the dehydration reaction process on the final product and promote the oxidation reaction of HMF→FDCA. In addition, the product after participating in the oxidation reaction is acetic acid, which is easy to separate from FDCA. When acetic acid is used as a reaction solvent, it does not need to be separated from the reaction solvent, thereby not complicating the separation and purification process of the product.
[0009] Preferably, the method specifically comprises the following steps: (1) preparing a mixed solution containing biomass sugar, a homogeneous metal salt catalyst, an organic bromide and water, and then performing a dehydration reaction to obtain a dehydrated reaction solution; (2) adding a co-oxidant and a portion of acetic acid to the dehydration reaction solution, and mixing to obtain a primary solution; (3) adding an oxidation catalyst and another portion of acetic acid to a reaction vessel, raising the temperature to an oxidation reaction temperature, adding the initial solution to the reaction vessel under an oxidizing gas atmosphere, performing an oxidation reaction, and then separating 2,5-furandicarboxylic acid.
[0010] Preferably, the biomass sugar includes one or more of glucose, high fructose syrup, mannose, galactose, sucrose, maltose and lactose.
[0011] Furthermore, the biomass sugar is one or more of glucose, sucrose and high fructose syrup with a fructose content of 42-90% in the solid components.
[0012] Preferably, the homogeneous metal salt catalyst includes one or more of chromium salts, aluminum salts, nickel salts, iron salts, tin salts and cobalt salts.
[0013] The above homogeneous metal salt catalyst can effectively catalyze the conversion of biomass sugar into HMF, and when it remains in the dehydration reaction liquid, it will not have too great an adverse effect on the subsequent oxidation reaction. Therefore, after the dehydration reaction is completed, the subsequent oxidation reaction can be directly carried out without separation from the reaction system.
[0014] Furthermore, the homogeneous metal salt catalyst includes one or more of tetravalent chromium salts, trivalent aluminum salts, divalent nickel salts, trivalent iron salts, divalent tin salts and divalent cobalt salts.
[0015] Preferably, the organic bromide comprises one or more of choline bromide, bromide-containing quaternary ammonium salts and bromide-containing imidazole ionic liquids.
[0016] Further, the organic bromide includes one or more of choline bromide, tetramethylammonium bromide, tetraethylammonium bromide, tetrapropylammonium bromide, tetrabutylammonium bromide, 1-ethyl-3-methylimidazolium bromide, 1-butyl-3-methylimidazolium bromide, 1-hexyl-3-methylimidazolium bromide, 1-octyl-3-methylimidazolium bromide and 1-butyl-2,3-dimethylimidazolium bromide.
[0017] Preferably, the mass ratio of the homogeneous metal salt catalyst to the biomass sugar is 0.02-0.5:1; the temperature of the dehydration reaction is 100-150°C, and the time is 20min-5h.
[0018] Furthermore, the dehydration reaction is carried out at a temperature of 110 to 140° C. and for a time of 1 to 4 hours.
[0019] Preferably, the mass ratio of the biomass sugar to the organic bromide is 1:0.5-10.
[0020] Preferably, the oxidation catalyst includes a main catalyst, or a main catalyst and a co-catalyst; the co-catalyst contains cobalt and manganese elements; the co-catalyst contains at least one of iron, zirconium, zinc, copper and nickel elements.
[0021] Furthermore, the main catalyst includes a divalent cobalt salt and a divalent manganese salt; the co-catalyst includes one or more of a trivalent iron salt, a tetravalent zirconium salt, a divalent copper salt, a divalent zinc salt and a divalent nickel salt.
[0022] Furthermore, the oxidation catalyst is a metal salt homogeneous catalyst.
[0023] Furthermore, the metal salt homogeneous catalyst includes one or more of acetate, halide, carbonate, sulfate, nitrate and phosphate.
[0024] Furthermore, the molar ratio between the cobalt element and the manganese element in the main catalyst is 1:0.015-0.15.
[0025] Furthermore, calculated on the basis of metal elements, the molar ratio between the main catalyst and the co-catalyst is 1:0.07-0.10.
[0026] Preferably, the mass ratio of the co-oxidant to the biomass sugar is 0.2-1.5:1, more preferably 0.4-1.1:1.
[0027] In the process of preparing HMF by biomass sugar reaction, side reactions are prone to produce humins, resulting in low purity of HMF in the dehydration reaction liquid. By increasing the amount of co-oxidant added, it is helpful to reduce the influence of HMF purity on the yield and purity of FDCA to a greater extent. However, when the amount of co-oxidant added is too large, it will cause excessive oxidation reaction and generate by-products. The present invention, on the basis of introducing a co-oxidant, can further improve the yield and purity of the product prepared by the continuous reaction of biomass sugar to FDCA by controlling the mass ratio between the co-oxidant and the biomass sugar within the above range.
[0028] Preferably, the content of the oxidation catalyst in terms of metal element in the total mass of the dehydration reaction liquid, the co-oxidant, the acetic acid and the oxidation catalyst is 1000 to 6000 ppm; the temperature of the oxidation reaction is 120 to 200° C., and the time is 10 min to 1 h.
[0029] Furthermore, the temperature of the oxidation reaction is 130-180°C.
[0030] Preferably, the oxidizing gas is air, or a mixture of air and CO2; the pressure of the oxidizing gas atmosphere is 0.4-5 MPa.
[0031] Furthermore, the oxidizing gas is a mixed gas of air and CO2 in a volume ratio of 1:0.125-4, and a further preferred volume ratio is 1:0.15-2.
[0032] Preferably, the method for separating 2,5-furandicarboxylic acid is crystallization.
[0033] Preferably, in step (1), among the biomass sugar, organic bromide and water, the mass proportion of the biomass sugar is 30-60%.
[0034] As the biomass sugar concentration increases, the purity of the dehydration reaction product HMF decreases, which in turn causes the subsequent oxidation reaction product FDCA yield and purity to decrease. The present invention can reduce the influence of HMF purity on FDCA yield and purity by using a co-oxidant during the oxidation reaction, thereby making it possible to reduce the magnitude of the decrease in FDCA yield and purity when the biomass sugar concentration increases, thereby achieving a relatively high FDCA yield and purity at a higher biomass sugar concentration.
[0035] Preferably, in step (2), during the preparation of the initial solution, the mass ratio of the dehydration reaction solution to the portion of acetic acid is 1:3 to 10, more preferably 1:4 to 8.
[0036] Compared with the prior art, the present invention has the following advantages: (1) The present invention can achieve a higher yield and purity of the product FDCA in the process of preparing 2,5-furandicarboxylic acid by continuous reaction of biomass sugar, and the reaction raw material can use low-priced biomass sugar such as glucose, which gives the continuous reaction method a better industrial application prospect, is conducive to reducing production costs and improving production efficiency; (2) The present invention can reduce or even avoid the use of hydrogen bromide during the oxidation reaction while ensuring the yield and purity of FDCA, thereby reducing corrosion to equipment. DETAILED DESCRIPTION
[0037] The present invention will be further described below in conjunction with the embodiments.
[0038] Overall embodiment A method for preparing 2,5-furandicarboxylic acid by continuous reaction of biomass sugars, comprising the following steps: Under the action of a homogeneous metal salt catalyst, biomass sugar is used as a raw material to undergo a dehydration reaction to generate 5-hydroxymethylfurfural, and a co-oxidant and acetic acid are added to the dehydration reaction liquid obtained after the reaction is completed. The co-oxidant is one or more of acetaldehyde, triacetaldehyde and methyl ethyl ketone. Under the action of an oxidation catalyst, an oxidation reaction is carried out in an oxidizing gas atmosphere, and then 2,5-furandicarboxylic acid is separated.
[0039] As a specific implementation, the method specifically includes the following steps: (1) preparing a mixed solution containing biomass sugar, a homogeneous metal salt catalyst, an organic bromide and water, and then performing a dehydration reaction to obtain a dehydrated reaction solution; Optionally, the organic bromide comprises one or more of choline bromide, bromide-containing quaternary ammonium salts and bromide-containing imidazole ionic liquids, the mass ratio of the biomass sugar to the organic bromide is 1:0.5-10; among the biomass sugar, the organic bromide and water, the mass ratio of the biomass sugar is 30-60%; (2) adding a co-oxidant and a portion of acetic acid to the dehydration reaction solution, and mixing to obtain a primary solution; Optionally, the mass ratio between the dehydration reaction liquid and the portion of acetic acid is 1:3-10; (3) adding an oxidation catalyst and another portion of acetic acid to a reaction vessel, raising the temperature to an oxidation reaction temperature, adding the initial solution to the reaction vessel under an oxidizing gas atmosphere, performing an oxidation reaction, and then separating 2,5-furandicarboxylic acid.
[0040] As a specific embodiment, the biomass sugar includes one or more of glucose, high fructose syrup, mannose, galactose, sucrose, maltose and lactose.
[0041] As a specific embodiment, the homogeneous metal salt catalyst includes one or more of chromium salts, aluminum salts, nickel salts, iron salts, tin salts and cobalt salts; the mass ratio between the homogeneous metal salt catalyst and biomass sugar is 0.02-0.5:1; the temperature of the dehydration reaction is 100-150°C, and the time is 20min-5h.
[0042] As a specific embodiment, the oxidation catalyst includes a main catalyst, or includes a main catalyst and a co-catalyst; the co-catalyst contains cobalt and manganese elements; the co-catalyst contains at least one of iron, zirconium, zinc, copper and nickel elements; the molar ratio between the cobalt element and the manganese element in the main catalyst is 1:0.015~0.15; in terms of metal elements, the molar ratio between the main catalyst and the co-catalyst is 1:0.07~0.10.
[0043] As a specific implementation manner, the mass ratio between the co-oxidant and the biomass sugar is 0.2-1.5:0.05-0.6:1; in the total mass of the dehydration reaction liquid, the co-oxidant, acetic acid and the oxidation catalyst, the content of the oxidation catalyst in terms of metal elements is 1000-6000 ppm; the temperature of the oxidation reaction is 120-200°C, and the time is 10min-1h.
[0044] As a specific implementation manner, the oxidizing gas is air, or a mixed gas of air and CO2 in a volume ratio of 1:0.125-4; the pressure of the oxidizing gas atmosphere is 0.4-5 MPa.
[0045] As a specific embodiment, the method for separating 2,5-furandicarboxylic acid is crystallization. Specific embodiments The present invention is described below by specific examples. It should be understood that these examples are only used to illustrate the present invention and are not used to limit the scope of the present invention. Without departing from the spirit and scope of the inventive concept, changes and advantages that can be thought of by those skilled in the art are included in the present invention, and the attached claims and any equivalents thereof are the protection scope of the present invention.
[0047] Unless otherwise defined, all technical terms and scientific terms used in the present invention have the same meanings as those commonly understood by ordinary technicians in the field to which the present disclosure belongs. Unless otherwise specified, the raw materials and equipment used in the present invention are conventional raw materials and equipment in the field and can be obtained from conventional commercial channels; unless otherwise specified, the methods used in the present invention are conventional methods in the field.
[0048] The detection and analysis methods used in the following examples are as follows: (1) High performance liquid chromatography detection method for each component: Biomass sugar: The instrument is Agilent 1260, the chromatographic column model is Hi-Plex H, the column temperature is 65°C, the differential detector is used, the mobile phase is 5 mM sulfuric acid aqueous solution, and the flow rate is 0.4 mL / min.
[0049] HMF: The instrument was Agilent 1260, the column model was Eclipse XDB-C18, the column temperature was 40°C, the detector was UV, the mobile phase was a mixture of methanol and water in a volume ratio of 9:1, the flow rate was 1 mL / min, and the detection wavelength was 283 nm.
[0050] FDCA: The instrument was Agilent 1260, the chromatographic column model was Eclipse XDB-C18, the column temperature was 35°C, the detector was UV, the mobile phase was a mixture of trifluoroacetic acid aqueous solution (mass fraction 0.1%) and methanol in a volume ratio of 2:3, the flow rate was 1 mL / min, and the detection wavelength was 260 nm.
[0051] (2) Calculation formula for biomass sugar and HMF conversion rate: Biomass sugar conversion rate = molar amount of converted biomass sugar / molar amount of added biomass sugar × 100%; HMF conversion rate = molar amount of converted HMF / molar amount of HMF in the added fructose dehydration reaction solution × 100%.
[0052] (3) When glucose, mannose, fructose syrup or galactose is used as raw material, the yield calculation formula of HMF and FDCA is: HMF yield = molar amount of HMF produced / molar amount of biomass sugar added × 100%; FDCA yield = molar amount of FDCA produced / molar amount of HMF fed into the oxidation reactor × HMF yield.
[0053] (4) When sucrose, maltose or lactose is used as the raw material, the yield of HMF and FDCA is calculated as follows: HMF yield = molar amount of HMF generated / (molar amount of biomass sugar added × 2) × 100%; FDCA yield = molar amount of FDCA produced / molar amount of HMF fed into the oxidation reactor × HMF yield.
[0054] The above-mentioned “molar amount of converted biomass sugar”, “molar amount of produced HMF” and “molar amount of produced FDCA” were measured by high performance liquid chromatography.
[0055] Examples 1 to 8: Effect of the Selection of Organic Bromide on the Reaction 2,5-furandicarboxylic acid was prepared by continuous reaction of glucose, the steps are as follows: S1: Glucose → 5-Hydroxymethylfurfural: A certain amount of glucose, 500 g of organic bromide, 100 g of water and a certain amount of homogeneous metal salt catalyst were added to a 2 L reactor, stirring was started, the temperature was raised to the dehydration reaction temperature, and the reaction was carried out for a certain time to obtain a dehydration reaction liquid. Samples were taken, and the HPLC was used for detection, and the yield of 5-hydroxymethylfurfural was calculated.
[0056] S2: 5-Hydroxymethylfurfural → 2,5-furandicarboxylic acid: A certain amount of co-oxidant is added to the dehydration reaction liquid, and then mixed with a certain amount of acetic acid to obtain a preliminary solution. 6000g of acetic acid and a certain amount of oxidation catalyst are added to a 20L reactor. After heating to the oxidation reaction temperature, 6000g of the preliminary solution (feed rate is 60g / min, time is 100min) is passed under an oxidizing gas atmosphere to perform an oxidation reaction to generate 2,5-furandicarboxylic acid. After the reaction is completed, 2,5-furandicarboxylic acid is separated by crystallization, detected by high performance liquid chromatography, and the fructose conversion rate and the purity and yield of 2,5-furandicarboxylic acid are calculated. It has been measured that the glucose conversion rates in Examples 1 to 8 are all >99.9%.
[0057] The detailed design of the preparation process in Examples 1 to 8, as well as the calculated results of the product purity and yield are shown in Tables 1 and 2.
[0058] Table 1 Preparation process details and experimental results of Examples 1 to 4 1Glucose mass fraction: refers to the mass proportion of glucose in glucose, organic bromide and water in step S1, that is, glucose mass fraction = glucose mass / (glucose mass+organic bromide mass+water mass)×100%; the "glucose mass fraction" in the tables below has the same meaning.
[0059] 2 Added amount: refers to the mass of glucose added in step S1; the “added amount” in the following tables has the same meaning.
[0060] 3 Dehydration reaction liquid: acetic acid (m:m): "Acetic acid" here refers to the acetic acid added when preparing the "initial solution"; the "dehydration reaction liquid: acetic acid (m:m)" in the following tables has the same meaning.
[0061] 4 Oxidation reaction temperature and time: The oxidation reaction time here is counted from the time the initial solution is added; the "oxidation reaction temperature and time" in the tables below have the same meaning.
[0062] Table 2 Preparation process details and experimental results of Examples 5 to 8 By analyzing Examples 1 to 8, the following conclusions can be drawn: Under the condition that the reaction is ensured to proceed fully (glucose conversion rate>99.9%), compared with other organic bromides, when choline bromide or tetraethylammonium bromide is used, the HMF yield can be increased, thereby improving the purity and yield of the final product FDCA.
[0063] Examples 9-15: Effects of different dehydration catalysts (homogeneous metal salt catalysts) on the reaction In Examples 9 to 15, the steps of preparing 2,5-furandicarboxylic acid by continuous reaction of glucose are the same as those in Examples 1 to 8. It has been measured that the glucose conversion rates of Examples 9 to 15 are all greater than 99.9%.
[0064] The detailed design of the preparation process in Examples 9 to 15, as well as the calculated results of the product purity and yield are shown in Tables 3 and 4.
[0065] Table 3 Preparation process details and experimental results of Examples 9 to 12 Table 4 Preparation process details and experimental results of Examples 13 to 15 By analyzing Examples 9 to 15, the following conclusions can be drawn: Under the condition of ensuring that the reaction is fully carried out (glucose conversion rate>99.9%), compared with several other homogeneous metal salt catalysts, when chromium salts (such as chromium bromide and chromium chloride) are used as dehydration reaction catalysts, the HMF yield can be improved, thereby improving the purity and yield of the final product FDCA.
[0066] Examples 16-21: Effect of the amount of dehydration catalyst (homogeneous metal salt catalyst) added on the reaction In Examples 16 to 21, the steps of preparing 2,5-furandicarboxylic acid by continuous reaction of glucose are the same as those in Examples 1 to 8. It has been measured that the glucose conversion rates of Examples 16 to 21 are all greater than 99.9%.
[0067] The detailed design of the preparation process in Examples 16 to 21, as well as the calculated results of the product purity and yield are shown in Table 5.
[0068] Table 5 Preparation process details and experimental results of Examples 16 to 21 By analyzing Examples 16 to 21, the following conclusions can be drawn: Under the condition that the reaction is fully carried out (glucose conversion rate>99.9%), with the increase of the amount of dehydration reaction catalyst, the yield of HMF and the purity and yield of FDCA first increase and then decrease.
[0069] Examples 22-29: Effect of the ratio of dehydration reaction liquid to acetic acid on the reaction In Examples 22 to 29, the steps of preparing 2,5-furandicarboxylic acid by continuous reaction of glucose are the same as those in Examples 1 to 8. It has been measured that the glucose conversion rates of Examples 22 to 29 are all greater than 99.9%.
[0070] The detailed design of the preparation process in Examples 22 to 29, as well as the calculated results of the product purity and yield are shown in Tables 6 and 7.
[0071] Table 6 Preparation process details and experimental results of Examples 22 to 25 Table 7 Preparation process details and experimental results of Examples 26 to 29 By analyzing Examples 22 to 29, the following conclusions can be drawn: Within a certain range, the purity of the product FDCA can be improved by increasing the mass ratio between the dehydration reaction liquid and acetic acid.
[0072] Examples 30-37: Effects of different biomass sugars on the reaction The steps for preparing 2,5-furandicarboxylic acid from biomass sugars are as follows: S1: Biomass sugar → 5-hydroxymethylfurfural: A certain amount of biomass sugar, 500g of organic bromide, 100g of water and a certain amount of homogeneous metal salt catalyst were added to a 2L reactor, stirring was started, the temperature was raised to the dehydration reaction temperature, and the reaction was carried out for a certain time to obtain a dehydration reaction liquid. Samples were taken, and the HPLC was used for detection, and the yield of 5-hydroxymethylfurfural was calculated.
[0073] S2: 5-Hydroxymethylfurfural → 2,5-furandicarboxylic acid: A certain amount of co-oxidant is added to the dehydration reaction liquid, and then mixed with a certain amount of acetic acid to obtain a preliminary solution. 6000g of acetic acid and a certain amount of oxidation catalyst are added to a 20L reactor. After heating to the oxidation reaction temperature, 6000g of the preliminary solution is passed under an oxidizing gas atmosphere (the feeding rate is 60g / min, and the time is 100min), and an oxidation reaction is carried out to generate 2,5-furandicarboxylic acid. After the reaction is completed, 2,5-furandicarboxylic acid is separated by crystallization, detected by high performance liquid chromatography, and the fructose conversion rate and the purity and yield of 2,5-furandicarboxylic acid are calculated. It has been measured that the glucose conversion rates of Examples 30 to 37 are all >99.9%.
[0074] The detailed design of the preparation process in Examples 30 to 37, as well as the calculated results of the product purity and yield are shown in Tables 8 and 9.
[0075] Table 8 Preparation process details and experimental results of Examples 30 to 33 1 Mass fraction: refers to the mass proportion of biomass sugar in biomass sugar, organic bromide and water in step S1, that is, biomass sugar mass fraction = biomass sugar mass / (biomass sugar mass + organic bromide mass + water mass) × 100%; the "mass fraction" in Table 9 has the same meaning.
[0076] 2 Added amount: refers to the mass of biomass sugar added in step S1; the “added amount” in Table 9 has the same meaning.
[0077] Table 9 Preparation process details and experimental results of Examples 34 to 37 By analyzing Examples 30 to 37, the following conclusions can be drawn: (1) When high fructose syrup is used as the reaction raw material, the yield of HMF and the yield and purity of FDCA can be increased by increasing the fructose content therein.
[0078] (2) Compared with several other biomass sugars, the use of high fructose syrup or sucrose can achieve higher FDCA yield and purity.
[0079] Examples 38-40: Effects of different co-oxidants on the reaction In Examples 38 to 40, the steps of preparing 2,5-furandicarboxylic acid by continuous reaction of glucose are the same as those in Examples 1 to 8. It has been measured that the glucose conversion rate and HMF conversion rate of Examples 38 to 40 are both greater than 99.9%.
[0080] The detailed design of the preparation process in Examples 38 to 40, as well as the calculated results of the product purity and yield are shown in Table 10.
[0081] Table 10 Preparation process details and experimental results of Examples 38 to 40 By analyzing Examples 38 to 40, the following conclusions can be drawn: Compared with acetaldehyde and methyl ethyl ketone, when using paraldehyde as a co-oxidant, a higher FDCA yield and purity can be achieved. This is because the co-oxidant is first oxidized in the acetic acid solvent to generate peroxides, and the peroxides will then change the valence state of the metal elements in the catalyst through oxidation, promoting the oxidation of HMF. Acetaldehyde and methyl ethyl ketone have similar structures, and the mechanism of peroxide generation from paraldehyde is different. The higher activity of paraldehyde may be because the peroxide generated by paraldehyde has higher oxidation activity than acetaldehyde and methyl ethyl ketone.
[0082] Examples 41-50: Effect of the amount of co-oxidant added on the reaction In Examples 41 to 50, the steps of preparing 2,5-furandicarboxylic acid by continuous reaction of glucose are the same as those in Examples 1 to 8. It has been measured that the glucose conversion rates of Examples 41 to 50 are all greater than 99.9%.
[0083] The detailed design of the preparation process in Examples 41 to 50, as well as the calculated results of the product purity and yield are shown in Tables 11 and 12.
[0084] Table 11 Preparation process details and experimental results of Examples 41 to 45 Table 12 Preparation process details and experimental results of Examples 46 to 50 By analyzing Examples 41 to 50, the following conclusions can be drawn: Within a certain range, the yield and purity of FDCA can be improved by increasing the amount of co-oxidant; however, when the amount of co-oxidant is too large, it will have an adverse effect on the yield and purity of FDCA. This is because: the co-oxidant can promote the reaction of HMF→FDCA and reduce the effect of HMF purity on the yield and purity of the product FDCA, but when the amount of co-oxidant is too large, it will cause excessive oxidation reaction and generate by-products.
[0085] Comparative Examples 1-2: Effect of not using a co-oxidant on the reaction 2,5-furandicarboxylic acid was prepared by continuous reaction of glucose, the steps are as follows: S1: Glucose → 5-Hydroxymethylfurfural: A certain amount of glucose, 500 g of organic bromide, 100 g of water and a certain amount of homogeneous metal salt catalyst were added to a 2 L reactor, stirring was started, the temperature was raised to the dehydration reaction temperature, and the reaction was carried out for a certain time to obtain a dehydration reaction liquid. Samples were taken, and the HPLC was used for detection, and the yield of 5-hydroxymethylfurfural was calculated.
[0086] S2: 5-Hydroxymethylfurfural → 2,5-furandicarboxylic acid: The dehydrated reaction liquid is mixed with a certain amount of acetic acid to obtain a preliminary solution. 6000g of acetic acid and a certain amount of oxidation catalyst are added to a 20L reactor, and after heating to the oxidation reaction temperature, 6000g of the preliminary solution is introduced under an oxidizing gas atmosphere (feeding rate is 60g / min, time is 100min), and an oxidation reaction is performed to generate 2,5-furandicarboxylic acid. After the reaction is completed, 2,5-furandicarboxylic acid is separated by crystallization, detected by high performance liquid chromatography, and the fructose conversion rate and the purity and yield of 2,5-furandicarboxylic acid are calculated.
[0087] The glucose conversion rate and HMF conversion rate of Comparative Examples 1 to 2 were measured to be greater than 99.9%. The detailed design of the preparation process in Comparative Examples 1 to 2, as well as the calculated results of the product purity and yield are shown in Table 13.
[0088] Table 13 Preparation process details and experimental results of comparative examples 1 to 2 By analyzing Examples 38 to 40 and Comparative Examples 1 to 2, the following conclusions can be drawn: By using a co-oxidant such as acetaldehyde, trimeraldehyde or methyl ethyl ketone, the yield and purity of FDCA can be increased while the use of hydrobromic acid can be reduced and the reaction temperature can be lowered.
[0089] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any way. Any simple modification, change and equivalent transformation made to the above embodiment based on the technical essence of the present invention still falls within the protection scope of the technical solution of the present invention.
Claims
1. A method for preparing 2,5-furandicarboxylic acid by continuous reaction of biomass sugars, characterized in that: The following steps are involved: Under the action of a homogeneous metal salt catalyst, biomass sugar is used as a raw material to undergo a dehydration reaction to generate 5-hydroxymethylfurfural, and a co-oxidant and acetic acid are added to the dehydration reaction liquid obtained after the reaction is completed. The co-oxidant is one or more of acetaldehyde, triacetaldehyde and methyl ethyl ketone. Under the action of an oxidation catalyst, an oxidation reaction is carried out in an oxidizing gas atmosphere, and then 2,5-furandicarboxylic acid is separated.
2. The method according to claim 1, characterized in that The specific steps include: (1) preparing a mixed solution containing biomass sugar, a homogeneous metal salt catalyst, an organic bromide and water, and then performing a dehydration reaction to obtain a dehydrated reaction solution; (2) adding a co-oxidant and a portion of acetic acid to the dehydration reaction solution and mixing to obtain a primary solution; (3) Adding an oxidation catalyst and another portion of acetic acid to a reaction vessel, raising the temperature to an oxidation reaction temperature, adding the initial solution to the reaction vessel under an oxidizing gas atmosphere, carrying out an oxidation reaction, and then separating 2,5-furandicarboxylic acid.
3. The method according to claim 1 or 2, characterized in that: The biomass sugars include one or more of glucose, high fructose syrup, mannose, galactose, sucrose, maltose and lactose.
4. The method according to claim 3, characterized in that The biomass sugar is one or more of glucose, sucrose and high fructose syrup with a fructose content of 42-90% in the solid components.
5. The method according to claim 1 or 2, characterized in that: The homogeneous metal salt catalyst includes one or more of chromium salts, aluminum salts, nickel salts, iron salts, tin salts and cobalt salts.
6. The method according to claim 1 or 2, characterized in that: The mass ratio between the homogeneous metal salt catalyst and the biomass sugar is 0.02-0.5:1; the temperature of the dehydration reaction is 100-150°C, and the time is 20 min-5 h.
7. The method according to claim 1 or 2, characterized in that: The oxidation catalyst includes a main catalyst, or a main catalyst and a co-catalyst; the co-catalyst contains cobalt and manganese elements; the co-catalyst contains at least one of iron, zirconium, zinc, copper and nickel elements.
8. The method according to claim 1 or 2, characterized in that: The mass ratio between the co-oxidant and the biomass sugar is 0.2-1.5:
1.
9. The method according to claim 2, characterized in that: In step (1), among the biomass sugar, organic bromide and water, the mass proportion of the biomass sugar is 30-60%.
10. The method according to claim 2, characterized in that In step (2), during the preparation of the initial solution, the mass ratio between the dehydration reaction solution and the portion of acetic acid is 1:3-10.
Citation Information
Patent Citations
Oxidation of furfural compounds
CN102459214A
Preparation method of 2, 5-furandicarboxylic acid
CN114605362A
Co-production method of 5-hydroxymethylfurfural, 5-alkanoyloxy methylfurfural and 2, 5-furandicarboxylic acid
CN115028608A
Process for producing both biobased succinic acid and 2,5-furandicarboxylic acid
WO2013033081A2
Method and system for continuously producing 5-hydroxymethylfurfural and 2,5-furandicarboxylic acid
WO2023072053A1
Cited By
Method for preparing 2, 5-furandicarboxylic acid based on waste textiles
CN122010879A
A method for preparing 2,5-furan dicarboxylic acid based on waste and old textiles
CN122010879B
Method for preparing 2,5-furandicarboxylic acid from 5-hydroxymethylfurfural by means of co-oxidation
WO2025241292A1