Display panel, display device and preparation method
By arranging metal isolation pillars and grooves in the transition area of the OLED display panel, the water and oxygen path problem caused by the opening of the light-emitting layer is solved, the protection against GDSH is enhanced, and the packaging effect and the overall performance of the display panel are improved.
Patent Information
- Application Number
- CN202411154798.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-10-22
AI Technical Summary
When the OLED display panel is equipped with cameras, sensors and other devices, the openings in the light-emitting layer are exposed, forming water and oxygen paths, causing the black spot (GDSH) problem on the display panel.
Set metal isolation pillars surrounding the opening area in the transition area of the display panel, and dig grooves in the inorganic layer to form grooves. The metal isolation pillars and grooves are used to increase the blocking distance of the light-emitting layer and delay water and oxygen from breaking through the packaging layer. speed.
It effectively enhances the GDSH protection ability of the display panel, improves the packaging effect, extends the packaging distance, reduces the speed of water and oxygen breakthrough, and improves the overall performance of the display panel.
Smart Images

Figure CN118829286A_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to the field of display technology, and in particular to a display panel, a display device, and a manufacturing method thereof. Background Art
[0002] As users pursue a high screen-to-body ratio, there is usually a need to punch holes in the display area of OLED display panels to facilitate the installation of devices such as cameras and sensors. As a result, the light-emitting layer in the display panel is exposed at the location of the holes in the display area, which easily forms a water-oxygen path and causes black spots (Growing Dark Spot at HIAA, abbreviated as GDSH) at the edges of the holes in the display panel. Summary of the invention
[0003] In view of this, an object of the present disclosure is to provide a display panel, a display device and a manufacturing method thereof.
[0004] Based on the above purpose, the present disclosure provides a display panel, the display panel having a display area, an opening area and a transition area; the transition area is located between the opening area and the display area;
[0005] The display panel comprises a substrate layer, and an inorganic layer and a light-emitting layer arranged in sequence in a direction away from the substrate layer;
[0006] The transition region includes a metal isolation column surrounding the opening region, and the metal isolation column is located between the inorganic layer and the light-emitting layer;
[0007] The inorganic layer includes a groove that cooperates with the metal isolation column to block the light-emitting layer; wherein,
[0008] The light-emitting layer includes a first light-emitting sublayer and a second light-emitting sublayer blocked from the first light-emitting sublayer, the first light-emitting sublayer is located on the side of the metal isolation column away from the substrate layer; in the direction perpendicular to the substrate layer, the height difference between the first light-emitting sublayer and the second light-emitting sublayer is not less than the height of the metal isolation column.
[0009] Based on the same inventive concept, an embodiment of the present disclosure further provides a method for preparing a display panel, wherein the display panel has a display area, an opening area, and a transition area; the transition area is located between the opening area and the display area; the preparation method comprises:
[0010] providing a substrate layer;
[0011] forming an inorganic layer on the substrate layer, and grooving the inorganic layer to obtain a groove;
[0012] forming a metal isolation layer on the inorganic layer; the metal isolation layer covers at least one of the two side walls of the groove;
[0013] forming a protective layer on the metal isolation layer outside the groove;
[0014] Etching the metal isolation layer to form a metal isolation column; wherein the metal isolation column is located in the transition area and surrounds the opening area;
[0015] A light-emitting layer is formed on the protective layer and in the groove; wherein,
[0016] The light-emitting layer includes a first light-emitting sublayer and a second light-emitting sublayer blocked from the first light-emitting sublayer, the first light-emitting sublayer is located on the side of the metal isolation column away from the substrate layer; in the direction perpendicular to the substrate layer, the height difference between the first light-emitting sublayer and the second light-emitting sublayer is not less than the height of the metal isolation column.
[0017] Based on the same inventive concept, an embodiment of the present disclosure further provides a display device, comprising a display panel as described in any one of the above.
[0018] From the above, it can be seen that the present disclosure provides a display panel, a display device and a preparation method, wherein the display panel has a display area, an opening area and a transition area between the opening area and the display area; the transition area includes a metal isolation column surrounding the opening area; the display panel includes a substrate layer and an inorganic layer and a light-emitting layer arranged in sequence in a direction away from the substrate layer; the metal isolation column is located between the inorganic layer and the light-emitting layer; the inorganic layer includes a groove that cooperates with the metal isolation column to block the light-emitting layer; wherein the height difference between the light-emitting layer located on the side of the metal isolation column away from the substrate layer and the light-emitting layer blocked by it is not less than the height of the metal isolation column. Such a technical solution digs a groove in the inorganic layer to obtain a groove, and uses the metal isolation column and the groove to increase the blocking distance of the light-emitting layer, thereby slowing down the speed at which water and oxygen break through the encapsulation layer, improving the encapsulation effect, and enhancing the GDSH protection capability of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the technical solutions in the present disclosure or related technologies, the drawings required for use in the embodiments or related technical descriptions are briefly introduced below. Obviously, the drawings described below are only embodiments of the present disclosure. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0020] Figure 1 A schematic diagram showing the structure of a display panel provided by a related technical solution is shown;
[0021] Figure 2 A scanning electron microscope image showing a partial structure of a display panel provided by a related technical solution;
[0022] Figure 3A A partial structural schematic diagram of a display panel provided by an embodiment of the present disclosure is shown;
[0023] Figure 3B A partial structural schematic diagram of another display panel provided by an embodiment of the present disclosure is shown;
[0024] Figure 4 Show Figure 3A Schematic diagram of the cross-sectional structure of line AA in FIG.
[0025] Figure 5A to Figure 5J A schematic diagram of a manufacturing process of a display panel provided by an embodiment of the present disclosure is shown. DETAILED DESCRIPTION
[0026] In order to make the objectives, technical solutions and advantages of the present disclosure more clearly understood, the present disclosure is further described in detail below in combination with specific embodiments and with reference to the accompanying drawings.
[0027] It should be noted that, unless otherwise defined, the technical terms or scientific terms used in the embodiments of the present disclosure should be understood by people with ordinary skills in the field to which the present disclosure belongs. The "first", "second" and similar words used in the embodiments of the present disclosure do not indicate any order, quantity or importance, but are only used to distinguish different components. "Including" or "comprising" and similar words mean that the elements or objects appearing before the word cover the elements or objects listed after the word and their equivalents, without excluding other elements or objects. "Connect" or "connected" and similar words are not limited to physical or mechanical connections, but can include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.
[0028] Figure 1 FIG. 1 is a schematic diagram showing the structure of a display panel 100 provided by a related technical solution. Figure 1 As shown, the OLED display panel 100 has a display area 101 (Active Area, referred to as AA area), an opening area 103 and a transition area 102; the display area 101 surrounds the opening area 103; the transition area 102 is located between the opening area 103 and the display area 101. During the manufacturing process, an opening needs to be opened in the display area 101 to form the opening area 103. In this process, the light-emitting layer (Electro-Luminescence, referred to as EL) is cut off, which easily forms a water-oxygen path and causes the display panel to generate GDSH.
[0029] In order to block the formation of water-oxygen paths, the solutions in the related art usually set isolation columns at the periphery of the opening area 103 to block the continuity of the light-emitting layer. Figure 2 A scanning electron microscope image showing a partial structure of a display panel provided by a related technical solution. Figure 2 The transition area of the display panel includes a light-emitting layer, an isolation column 202 and an inorganic layer 203; wherein the isolation column 202 is located between the light-emitting layer and the inorganic layer 203. Furthermore, the isolation column 202 blocks the light-emitting layer into a first light-emitting layer 2011 and a second light-emitting layer 2012, blocks the continuity of the organic material in the light-emitting layer between the opening area and the display area to block the water-oxygen path, thereby preventing water-oxygen from penetrating into the display area through the light-emitting layer to cause GDSH.
[0030] In some embodiments, the metal isolation column is the most common isolation column structure because it can be prepared in the same layer as the source and drain, and does not require additional masks, processes, equipment, etc. It should be noted that the height of the metal isolation column is strongly related to the blocking distance of the light-emitting layer and the height of the metal isolation column. The maximum blocking distance is usually about 700nm (similar to the height of the source and drain). Considering that the light-emitting material climbs up the side slope l' of the metal isolation column, the actual blocking distance will be smaller. Figure 2 It can be seen that the first light-emitting layer 2011 is located on the side of the metal isolation column 202 away from the inorganic layer 203; the second light-emitting layer 2012 is located on the partial slope of the inorganic layer 203 and the metal isolation column 202. The actual blocking distance between the two is much smaller than the height of the metal isolation column, which further leads to a limited packaging distance between the two and a short packaging structure. Water and oxygen can easily break through the short-distance packaging structure to form a water-oxygen passage, and then GDSH occurs.
[0031] In view of this, an embodiment of the present disclosure provides a display panel, in which grooves are dug in an inorganic layer to obtain grooves, and metal isolation columns and grooves are used to increase the blocking distance of the light-emitting layer, thereby slowing down the speed at which water and oxygen break through the encapsulation layer, improving the encapsulation effect, and enhancing the GDSH protection capability of the display panel.
[0032] Figure 3A A partial structural schematic diagram of a display panel 300 provided in an embodiment of the present disclosure is shown. Figure 3B FIG. 2 is a partial structural diagram of another display panel provided by an embodiment of the present disclosure. Figure 3A and Figure 3B As shown, the display panel 300 includes a display area 301, an opening area 303, and a transition area 302 therebetween. The transition area 302 is provided with a metal isolation column 304 and a groove 305. It should be noted that the number of the metal isolation column 304 can be one (eg, Figure 3AIn some embodiments, each metal isolation column 304 may be provided with a matching groove 305, or some of the metal isolation columns 304 may be selected to provide a matching groove 305, which is not limited in the embodiment of the present disclosure. Providing multiple metal isolation columns 304 helps to increase the packaging effect.
[0033] Combine the following Figure 3A and Figure 3B The structure and position of the groove 305 are exemplarily described.
[0034] In some embodiments, Figure 3A As shown, the groove 305 is disposed inside the metal isolation column 304 . For example, the metal isolation column 304 is divided into a first metal isolation column 3041 and a second metal isolation column 3042 by the groove 305 .
[0035] In some alternative embodiments, such as Figure 3B As shown, the groove 305 is disposed on at least one of the two sides of the metal isolation column 304 , for example, a side of the metal isolation column 304 close to the opening area 303 or a side of the metal isolation column 304 far from the opening area 303 .
[0036] In some embodiments, Figure 3A As shown, the groove 305 can be a continuous structure, such as a ring. In some alternative embodiments, such as Figure 3B As shown, the grooves 305 may be a discontinuous structure, for example, arranged intermittently around the opening area 303 .
[0037] Figure 4 Show Figure 3A Schematic diagram of the cross-sectional structure of the AA line in FIG. Figure 4 As shown, the transition region of the display panel includes a substrate layer 401, and the substrate layer 401 is sequentially provided with an inorganic layer 402, a metal isolation column 403, a protective layer 404, a light-emitting layer 405, and an encapsulation layer 406. Further, the inorganic layer 402 includes a groove 4021. The orthographic projection of the groove 4021 on the substrate layer 401 and the orthographic projection of the metal isolation column 403 on the substrate layer 401 partially overlap (as shown in FIG. Figure 4 shown) or adjacent ( Figure 4 402 is not shown in the figure). The protective layer 404 is located on the side of the metal isolation column 403 away from the substrate layer 401. In this way, the groove 4021 can effectively extend the height difference of the metal isolation column 403 in the height direction, and the blocking distance of the blocked light-emitting layer 405 is much greater than the blocking distance of the metal isolation column 403 alone, thereby increasing the packaging distance, delaying the speed of water and oxygen in the light-emitting layer near the opening area breaking through the packaging layer, and enhancing the packaging effect.
[0038] For example, the height of the metal spacer 403 is 700 nm, and the depth of the groove 4021 can be 1300 nm; then considering the slopes of the metal spacer 403 and the groove 4021, the blocking distance of the light-emitting layer 405 is not less than 2000 nm. Compared with the blocking distance of the metal spacer 403, the way in which the metal spacer 403 and the groove 4021 cooperate with each other greatly increases the blocking distance.
[0039] It should be noted that the depth of the groove 4021 does not exceed the thickness of the inorganic layer 402, and the present disclosure does not specifically limit the depth of the groove 4021. It should be understood that the greater the depth of the groove 4021, the more helpful it is to increase the blocking distance.
[0040] In some embodiments, the protective layer 404 is located at a distance from the center line of the groove 4021 ( Figure 4 The distance L1 between the metal isolation column 403 and the dotted line in the figure is less than the distance L2 between the boundary of the metal isolation column 403 close to the substrate layer and the center line of the groove 4021. In this way, the protective layer 404 can effectively block the side slope of the metal isolation column 403, avoiding the possibility of the light-emitting material climbing up the side slope of the metal isolation column 403 during the formation of the light-emitting layer 405, and ensuring that the light-emitting layer 405 is located on the side of the protective layer 404 away from the substrate layer 401 and in the groove 4021. Figure 4 It can be seen that this approach greatly increases the blocking distance of the encapsulation layer 406 and helps to improve the blocking effect.
[0041] For example, reference Fig.5I As shown, the light-emitting layer 505 includes a first light-emitting sublayer 5051 and a second light-emitting sublayer 5052 that blocks the first light-emitting sublayer 5051, wherein the first light-emitting sublayer 5051 is located on the side of the protective layer away from the substrate layer, and the second light-emitting sublayer 5052 is located in the groove of the inorganic layer. Fig.5I It can be seen that the second luminescent sublayer 5052 only has a climbing phenomenon on the side wall of the groove, and there is no luminescent layer at the side wall of the metal isolation column. In other words, in the direction perpendicular to the substrate layer, the height difference H1 between the first luminescent sublayer 5051 and the second luminescent sublayer 5052 is greater than the height H2 of the metal isolation column. It can be seen that based on the cooperation of the metal isolation column and the groove, the blocking distance l between the luminescent sublayers (i.e., the distance between the end of the first luminescent sublayer 5051 and the end of the second luminescent sublayer 5052 adjacent thereto) is greatly improved, which helps to improve the blocking effect and enhance the GDSH protection capability.
[0042] In some embodiments, Figure 4 As shown, the material of the protection layer 404 may be at least one of SiO 2 , SiNx and polyimide.
[0043] In some alternative embodiments, reference Fig. 5F As shown, the material of the protection layer 504 ′ can be metal. It should be noted that the protection layer 504 ′ can be prepared by the same preparation method as the metal isolation column 403 .
[0044] In some embodiments, Figure 4 As shown, the metal isolation column 403 includes a second metal layer 4032 and a first metal layer 4031 and a third metal layer 4033 located on both sides of the second metal layer 4032. Optionally, the first metal layer 4031 and the third metal layer 4033 have different etching selectivities from the second metal layer 4032, for example, the second metal layer 4032 can be etched by dry etching and anode wet etching; the first metal layer 4031 and the third metal layer 4033 can only be etched by dry etching. With such a configuration, the third metal layer 4033 protrudes toward the center line of the groove 4021 relative to the second metal layer 4032, so that the protective layer 404 protrudes from the side wall of the metal isolation column 403, thereby helping to prevent the light-emitting layer 405 from not being formed on the side wall of the metal isolation column 403.
[0045] Optionally, the material of the first metal layer 4031 and the third metal layer 4033 may be titanium, and the material of the second metal layer 4032 may be aluminum. Here, in addition to the above-mentioned function of controlling the position of the light-emitting layer 403, the arrangement of the first metal layer 4031 and the third metal layer 4033 also helps to prevent the second metal layer 4032 from warping.
[0046] Since cameras and sensors are usually placed in the opening area, and function buttons such as the smart island can also be set, these processes and operations can easily cause the edge of the opening area to be impacted, causing the light-emitting layer 405 to separate from the adjacent film layer. The setting of the groove 4021 can not only increase the packaging distance and improve the packaging effect, but also the groove can alleviate the separation effect of the impact force on the light-emitting layer 405, improve the crack resistance of the inorganic layer 402, and better improve the hole strength. The metal isolation column 403 and the groove 4021 play the role of a crack dam, and there is no need to specially set up a crack dam, achieving the technical effect of saving space.
[0047] Since the groove increases the distance in the height direction of the metal isolation column, the film formation of the encapsulation layer 406 is more uniform, the stress of the film layer is small, and the risk of cracks is smaller. At the same time, the larger the distance, the smaller the impact of the protruding part of the metal isolation column 403 on the exposure, the more sufficient the exposure of the pixel definition layer (PDL), and the risk of residual glue on the side wall of the metal isolation column 403 is smaller.
[0048] The disclosed embodiments also provide a method for preparing the aforementioned display panel. Figure 5A to Figure 5JThe following is a schematic diagram of the manufacturing process of a display panel provided by an embodiment of the present disclosure. Figure 5A to Figure 5J A method for preparing a display panel provided in an embodiment of the present disclosure is introduced.
[0049] like Figure 5A to Figure 5J As shown, the method for preparing the display panel includes:
[0050] Provide a substrate layer 501 such as Figure 5A It should be noted that the substrate layer 501 can be a flexible layer or a rigid layer, which is not limited in the present disclosure.
[0051] Next, an inorganic layer 502 is formed on the substrate layer 501, and a groove 5021 is obtained by digging a groove in the inorganic layer 502. Figure 5B As shown. Optionally, the inorganic layer 502 may be grooved using laser cutting technology. Optionally, the inorganic layer 502 may be a chemical vapor deposition (CVD) film layer.
[0052] It should be noted that the groove 5021 can be a continuous groove surrounding the opening area, or can be an alternately arranged groove, which is not limited in the present disclosure. Here, compared with the alternate groove, the continuous groove has a better effect on preventing GDSH.
[0053] In some embodiments, the depth of the groove 5021 does not exceed the thickness of the inorganic layer, and can be 200nm, 500nm, 700nm, 900nm, 1300nm, 1400nm, 1450nm, etc., which is not limited in this article.
[0054] Then, a metal isolation layer 503 is formed on the inorganic layer 502; the metal isolation layer 503 covers at least one of the two side walls of the groove. Figure 5C Here, whether the metal isolation layer 503 covers one side or both sides of the groove determines the relative position relationship between the subsequent metal isolation column and the groove. For example, if the metal isolation layer 503 covers one side of the groove, the metal isolation column is located on the side of the groove close to the opening area or the side far from the opening area. For another example, if the metal isolation layer 503 covers both sides of the groove, the groove divides the metal isolation column into Figure 3A The two parts are shown.
[0055] In some embodiments, the metal isolation layer 503 includes a first metal layer 5031, a second metal layer 5032, and a third metal layer 5033, which are sequentially arranged on the side of the inorganic layer 502 away from the substrate layer 501. Optionally, the metal isolation layer 503 can be manufactured at the same time as the source and drain layers are manufactured, and the specific manufacturing process is not limited. This method does not require additional manufacturing processes and does not require a separate mask, saving costs.
[0056] Optionally, the materials of the first metal layer 5031 and the third metal layer 5033 have different etching selectivities from the material of the second metal layer 5032. For example, the materials of the first metal layer 5031 and the third metal layer 5033 may be titanium, and the material of the second metal layer 5032 may be aluminum.
[0057] Next, a protective layer 504 is formed on the metal isolation layer 503 outside the groove. Figure 5D shown.
[0058] In some embodiments, the protective layer 504 may be an inorganic material layer, such as SiO2, SiN x , or it can be an organic material layer, such as polyimide (PI for short).
[0059] It should be noted that the boundary of the protection layer 504 exceeds the boundary of the groove, but does not fall on the slope of the metal isolation layer 503. Such a structure can effectively prevent the subsequent light-emitting layer material from climbing the slope of the metal isolation column.
[0060] Then, the first metal layer 5031, the second metal layer 5032 and the third metal layer 5033 are etched to expose the inorganic layer at the bottom of the groove, the second metal layer 5032 and the third metal layer 5033 located in the direction of the sidewall of the groove. Figure 5E Here, the first metal layer 5031, the second metal layer 5032 and the third metal layer 5033 can be etched simultaneously by dry etching.
[0061] Next, the second metal layer 5032 in the direction of the exposed groove sidewall is etched by anode wet etching to form a metal isolation column. Figure 5G Here, the metal isolation column is located in the transition area and surrounds the opening area.
[0062] from Figure 5E and Figure 5G As can be seen from the elliptical dashed box, the protective layer 504 can protect the metal isolation layer 503 during the previous etching step, but cannot protect the second metal layer 5032 during the anode wet etching. Therefore, the ends of the protective layer 504 and the third metal layer 503 protrude from the second metal layer, effectively shielding the slope of the second metal layer 5032.
[0063] In some alternative embodiments, such as Fig. 5F As shown, the protective layer 504' can replace the protective layer 504. Here, the material and preparation method of the protective layer 504' are the same as those of the metal isolation layer 503, and the present disclosure does not limit this.
[0064] Exemplarily, the protection layer 504' includes a fourth metal layer and a fifth metal layer. Specifically, the fourth metal layer and the fifth metal layer are sequentially formed on the metal isolation layer 503. The material of at least one of the fourth metal layer and the fifth metal layer has a different etching selectivity from the material of the second metal layer 5032. Figure 5H As shown, the fourth metal layer and the second metal layer 5032 are further etched by anode wet etching to obtain metal isolation columns.
[0065] It should be noted that the height of the metal isolation column can be 700 nm.
[0066] Then, a light emitting layer 505 is formed on the protective layer 504 and in the groove. Fig.5I As shown. The light-emitting layer 505 is blocked by the groove into a first light-emitting sublayer 5051 and a second light-emitting sublayer 5052. The first light-emitting sublayer 5051 is located on the side of the protective layer 504 away from the substrate layer, and the second light-emitting sublayer 5052 is located in the groove. Optionally, the light-emitting layer 505 is formed by evaporation. The height of the metal isolation column is 700nm, and the depth of the groove is 1300nm, then the blocking distance l between the two light-emitting sublayers is not less than 2000nm.
[0067] Finally, a packaging layer 506 is formed. Figure 5J It should be noted that the encapsulation layer 506 covers the light emitting layer 505 and the metal isolation column and the sidewall of the groove. Optionally, the encapsulation layer 506 can be a CVD layer.
[0068] The above-mentioned preparation embodiment is used to prepare the corresponding display panel in any of the above-mentioned embodiments, and has the beneficial effects of the corresponding display panel embodiment, which will not be described in detail here.
[0069] The present disclosure also provides a display panel. Figure 1 The display panel has a display area 101, an opening area 103 and a transition area 102; the transition area 102 is located between the opening area 103 and the display area 101; Figure 4 As shown, the display panel includes a substrate layer 401 and an inorganic layer 402 and a light-emitting layer 405 arranged in sequence in a direction away from the substrate layer; the transition area includes a metal isolation column 403 surrounding the opening area, and the metal isolation column is located between the inorganic layer 402 and the light-emitting layer 405; the inorganic layer 402 includes a groove 4021 that cooperates with the metal isolation column 403 to block the light-emitting layer 405. Fig.5IAs shown, the light-emitting layer includes a first light-emitting sublayer 5051 and a second light-emitting sublayer 5052 blocked with the first light-emitting sublayer 5051, and the first light-emitting sublayer 5051 is located on the side of the metal isolation column away from the substrate layer; in the direction perpendicular to the substrate layer, the height difference H1 between the first light-emitting sublayer and the second light-emitting sublayer is not less than the height H2 of the metal isolation column.
[0070] This technical solution solves the technical problem of short blocking distance caused by insufficient height of metal isolation columns by adding grooves in the inorganic layer, thereby increasing the blocking distance between light-emitting sub-layers, thereby increasing the packaging distance, slowing down the speed at which water and oxygen break through the packaging layer, increasing the packaging effect, and effectively preventing GDSH.
[0071] In some embodiments, the orthographic projection of the groove on the substrate layer and the orthographic projection of the metal isolation column on the substrate layer are adjacent to or partially overlapped (refer to Fig.5I ). Such a design can ensure that the groove effectively increases the distance in the lateral direction of the metal isolation column, providing a guarantee for extending the blocking distance of the light-emitting layer.
[0072] In some embodiments, Figure 4 and Fig.5I As shown, the display panel further includes protective layers 404 and 504, and the protective layers 404 and 504 are located between the metal isolation column 403 and the first light-emitting sublayer 5051. The protective layer 404 can play a protective role in the process of forming the metal isolation column 403 and the subsequent etching process.
[0073] In some embodiments, Figure 4 As shown, the distance L1 between the protective layer 404 and the center line of the groove 4021 is smaller than the distance L2 between the boundary of the metal isolation column 403 close to the substrate layer 401 and the center line of the groove 4021. The protective layer 404 blocks the sidewalls of the metal isolation column 403, which helps the material of the light-emitting layer to climb the sidewalls of the metal isolation column 403.
[0074] In some embodiments, the material of the protection layer is selected from at least one of SiO 2 , SiNx, metal, and polyimide.
[0075] In some embodiments, the groove 305 is located near the metal isolation column 304 (refer to Figure 3B ) or a side away from the opening area 303. In some embodiments, reference Figure 3A The metal isolation column 304 is disposed on a side ( 3042 ) of the groove 305 away from the hole area 303 and a side ( 3041 ) of the groove 305 close to the opening area 303 .
[0076] In some embodiments, the groove is a continuous groove surrounding the opening area (see Figure 3A ) or discontinuous groove (reference Figure 3B).
[0077] In some embodiments, the number of metal spacers is one or more; at least one of the plurality of metal spacers is provided with a matching groove. Exemplarily, each metal spacer has a matching groove on one side close to the opening area. Exemplarily, half of the metal spacers close to the opening area among the plurality of metal spacers are provided with matching grooves. Such a technical approach helps to reduce the adverse effects of water and oxygen on the display area. Here, the specific setting method of the groove is as described above and will not be repeated.
[0078] In some embodiments, Figure 4 As shown, the metal isolation column 403 includes a second metal layer 4032 and a first metal layer 4031 and a third metal layer 4033 located on both sides of the second metal layer 4032; wherein the etching selectivity of the first metal layer 4031 and the third metal layer 4033 is different from that of the second metal layer 4032. This method helps to expose the side of the second metal layer while retaining the end of the third metal layer 4033, which plays a role in supporting the protective layer 404.
[0079] Based on the same inventive concept, corresponding to any of the above embodiments, the present disclosure further provides a method for preparing a display panel. Here, the display panel has a display area, an opening area and a transition area; the transition area is located between the opening area and the display area.
[0080] like Figure 5A to Figure 5J As shown, the preparation method comprises:
[0081] Providing a substrate layer 501;
[0082] An inorganic layer 502 is formed on the substrate layer 501, and a groove 5021 is obtained by digging a groove in the inorganic layer 502;
[0083] A metal isolation layer 503 is formed on the inorganic layer 502; the metal isolation layer 503 covers at least one of the two sidewalls of the groove;
[0084] forming a protection layer 504 on the metal isolation layer 503 outside the groove;
[0085] Etching the metal isolation layer 503 to form a metal isolation column; wherein the metal isolation column is located in the transition area and surrounds the opening area;
[0086] A light emitting layer 505 is formed on the protective layer 504 and in the groove; wherein,
[0087] like Fig.5IAs shown, the light-emitting layer 505 includes a first light-emitting sublayer 5051 and a second light-emitting sublayer 5052 blocked with the first light-emitting sublayer 5051, and the first light-emitting sublayer 5051 is located on the side of the metal isolation column away from the substrate layer 501; in the direction perpendicular to the substrate layer 501, the height difference between the first light-emitting sublayer 5051 and the second light-emitting sublayer 5052 is not less than the height of the metal isolation column.
[0088] In some embodiments, Figure 5E to Figure 5H As shown, the metal isolation layer 503 includes a second metal layer 5032 and a first metal layer 5031 and a third metal layer 5032 located on both sides of the second metal layer 5032; etching the metal isolation layer to form a metal isolation column includes:
[0089] Performing dry etching on the first metal layer 5031, the second metal layer 5032, and the third metal layer 5033;
[0090] The dry-etched second metal layer 5032 is wet-etched to obtain a metal isolation column.
[0091] In some embodiments, the material of the protection layer 504' is metal; the step of forming the protection layer 504' on the metal isolation layer includes:
[0092] A fourth metal layer and a fifth metal layer are sequentially formed on the metal isolation layer; the etching selectivity of at least one of the fourth metal layer and the fifth metal layer is different from that of the second metal layer.
[0093] In some embodiments, an encapsulation layer 506 is formed on the light emitting layer 505 , the grooves, and the sidewalls of the metal isolation pillars.
[0094] In some embodiments, the light emitting layer is deposited by evaporation; and / or the encapsulation layer is deposited by chemical vapor deposition.
[0095] Based on the same inventive concept, corresponding to the display panel described in any of the above embodiments, the present disclosure further provides a display device including any of the above display panels. The display device has the beneficial effects of the corresponding display panel embodiments, which will not be described in detail here.
[0096] Those skilled in the art should understand that the discussion of any of the above embodiments is merely illustrative and is not intended to imply that the scope of the present disclosure (including the claims) is limited to these examples. Based on the concept of the present disclosure, the technical features in the above embodiments or different embodiments may be combined, the steps may be implemented in any order, and there are many other variations of the different aspects of the embodiments of the present disclosure as described above, which are not provided in detail for the sake of simplicity.
[0097] Although the present disclosure has been described in conjunction with specific embodiments of the present disclosure, many replacements, modifications and variations of these embodiments will be apparent to those skilled in the art from the foregoing description. For example, other memory architectures (e.g., dynamic RAM (DRAM)) may use the embodiments discussed.
[0098] The embodiments of the present disclosure are intended to cover all such substitutions, modifications and variations that fall within the broad scope of the appended claims. Therefore, any omissions, modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the embodiments of the present disclosure should be included in the scope of protection of the present disclosure.
Claims
1. A display panel, characterized in that: The display panel comprises a display area, an opening area and a transition area; the transition area is located between the opening area and the display area; The display panel comprises a substrate layer, and an inorganic layer and a light-emitting layer arranged in sequence in a direction away from the substrate layer; The transition region includes a metal isolation column surrounding the opening region, and the metal isolation column is located between the inorganic layer and the light-emitting layer; The inorganic layer includes a groove that cooperates with the metal isolation column to block the light-emitting layer; wherein, The light-emitting layer includes a first light-emitting sublayer and a second light-emitting sublayer blocked from the first light-emitting sublayer, the first light-emitting sublayer is located on the side of the metal isolation column away from the substrate layer; in the direction perpendicular to the substrate layer, the height difference between the first light-emitting sublayer and the second light-emitting sublayer is not less than the height of the metal isolation column.
2. The display panel according to claim 1, characterized in that: The orthographic projection of the groove on the substrate layer is adjacent to or partially overlaps with the orthographic projection of the metal isolation column on the substrate layer.
3. The display panel according to claim 1, characterized in that: The invention also includes a protection layer, wherein the protection layer is located between the metal isolation column and the first light-emitting sublayer.
4. The display panel according to claim 3, characterized in that: The distance between the protection layer and the center line of the groove is smaller than the distance between the boundary of the metal isolation column close to the substrate layer and the center line of the groove.
5. The display panel according to claim 3, characterized in that: The material of the protection layer is selected from at least one of SiO2, SiNx, metal and polyimide.
6. The display panel according to claim 1, characterized in that: The groove is located on a side of the metal isolation column close to or away from the opening area; or The metal isolation column is arranged on a side of the groove away from the opening area and a side of the groove close to the opening area.
7. The display panel according to claim 1, characterized in that: The groove is a continuous groove or a discontinuous groove surrounding the opening area.
8. The display panel according to claim 1, characterized in that: The number of the metal isolation columns is one or more; at least one of the plurality of metal isolation columns is provided with a matching groove.
9. The display panel according to claim 1, characterized in that: The metal isolation column includes a second metal layer and a first metal layer and a third metal layer located on both sides of the second metal layer; wherein the etching selectivity of the first metal layer and the third metal layer is different from that of the second metal layer.
10. A method for preparing a display panel, characterized in that: The display panel has a display area, an opening area and a transition area; the transition area is located between the opening area and the display area; the preparation method includes: providing a substrate layer; forming an inorganic layer on the substrate layer, and grooving the inorganic layer to obtain a groove; forming a metal isolation layer on the inorganic layer; the metal isolation layer covers at least one of the two side walls of the groove; forming a protective layer on the metal isolation layer outside the groove; Etching the metal isolation layer to form a metal isolation column; wherein the metal isolation column is located in the transition area and surrounds the opening area; A light-emitting layer is formed on the protective layer and in the groove; wherein, The light-emitting layer includes a first light-emitting sublayer and a second light-emitting sublayer blocked from the first light-emitting sublayer, the first light-emitting sublayer is located on the side of the metal isolation column away from the substrate layer; in the direction perpendicular to the substrate layer, the height difference between the first light-emitting sublayer and the second light-emitting sublayer is not less than the height of the metal isolation column.
11. The preparation method according to claim 10, characterized in that: The metal isolation layer includes a second metal layer and a first metal layer and a third metal layer located on both sides of the second metal layer; The etching of the metal isolation layer to form a metal isolation column comprises: performing dry etching on the first metal layer, the second metal layer, and the third metal layer; The second metal layer that has been dry-etched is wet-etched to obtain the metal isolation column.
12. The preparation method according to claim 11, characterized in that: The material of the protective layer is metal; The step of forming a protective layer on the metal isolation layer comprises: A fourth metal layer and a fifth metal layer are sequentially formed on the metal isolation layer; and an etching selectivity ratio of at least one of the fourth metal layer and the fifth metal layer is different from that of the second metal layer.
13. The preparation method according to claim 10, characterized in that: An encapsulation layer is formed on the light emitting layer, the groove and the sidewalls of the metal isolation column.
14. The preparation method according to claim 13, characterized in that: The light emitting layer is deposited by evaporation; and / or the encapsulation layer is deposited by chemical vapor deposition.
15. A display device, characterized in that: The display panel comprises the display panel according to any one of claims 1 to 9.