Electrochromic device and preparation method thereof
By adopting a composite structure of porous inorganic solid oxide film layer and liquid electrolyte in electrochromic devices, the problem of low ion conductivity in inorganic electrochromic devices is solved, and faster discoloration conversion rate and reduced liquid leakage risk is achieved. , suitable for applications in the display and automotive fields.
Patent Information
- Application Number
- CN202411287430.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-13
- Publication Date
- 2024-11-01
AI Technical Summary
The ion conductor layer materials commonly used in inorganic electrochromic devices have a low ion conductivity at room temperature, resulting in a slower transformation rate of transparent chromics, which limits its application in display and automobile fields. At the same time, liquid electrolytes have the risk of liquid leakage and flammability. Not suitable for direct use in electrochromic devices.
The composite structure of the porous inorganic solid oxide film layer and the liquid electrolyte is used as the electrolyte layer. The honeycomb-like porous structure is prepared by PS template method, photolithography, chemical corrosion and metal film anodization methods, and the liquid electrolyte is filled to improve the ionic conductivity. And reduce the risk of liquid leakage through sealing treatment.
It improves the discoloration transition rate of electrochromic devices, reduces the risk of liquid leakage of liquid electrolytes, enhances the stability and safety of electrochromic devices, and is suitable for applications in display and automobile fields.
Abstract
Description
Technical Field
[0001] The invention relates to the field of electrochromism, in particular to an electrochromism device and a preparation method thereof. Background Art
[0002] Electrochromic devices can actively adjust the transmittance of visible light by applying a small external voltage, and can achieve active transition between transparent and colored states. They can be used to control the light intensity in closed systems such as indoors or in cars, thereby improving indoor comfort and reducing energy consumption of lighting and temperature control systems.
[0003] Electrochromic devices usually include the following components in sequence: a transparent substrate, a first transparent conductive layer on the surface of the transparent substrate, an electrochromic layer, an ion conductor layer, an ion storage layer, and a second transparent conductive layer. The ion conductor layer is also called an electrolyte layer, which has the function of storing and transmitting conductive ions. Electrochromic devices are usually divided into organic and inorganic electrochromic devices, among which inorganic electrochromic devices have the most application prospects due to their stability and safety. However, the ion conductor layer materials commonly used in inorganic electrochromic devices have low room temperature ion conductivity and a slow transparent coloring conversion rate, which limits their application in fields such as display and automobiles. Liquid electrolytes have high ionic conductivity, but there are risks such as leakage and flammability, and are not suitable for direct use in electrochromic devices.
[0004] There are many factors that affect the electrochromic transition rate, and the ionic conductivity of the electrolyte layer is a key factor. To address this problem, the present invention provides a novel electrochromic device structure that can specifically solve the problem of low ionic conductivity of the electrolyte layer. Summary of the invention
[0005] The purpose of the present invention is to provide an electrochromic device to solve the problem of slow color change rate of the electrochromic device and reduce the risk of liquid electrolyte leakage; in addition, the present invention provides an embodiment to illustrate the preparation method of the electrochromic device structure.
[0006] In order to achieve the above object, the present invention adopts the following technical solutions: An electrochromic device comprises the following functional film layers: a transparent substrate, a first transparent conductive layer, an electrochromic electrode layer, a composite electrolyte layer, an ion storage layer and a second transparent conductive layer sequentially prepared on a surface of one side of the transparent substrate; The composite electrolyte layer is a film layer arranged on the surface of one side of the electrochromic electrode layer, and its structure is a composite structure of a porous inorganic solid oxide film layer and a liquid electrolyte, wherein the porous inorganic solid film layer is a porous inorganic oxide film layer including Al2O3, Ta2O5, and Nb2O5, and the film layer thickness is between 100-500nm, wherein the porous pore size is between 10-1000nm, and the liquid electrolyte is filled in the pores of the porous inorganic oxide film layer.
[0007] In the electrochromic device structure, the transparent substrate can be glass or an organic flexible substrate such as PET, PMMA, PC and CPI.
[0008] The first and second transparent conductive layers can be conductive materials that can achieve transparency and conduct electrons, such as indium oxide, tin oxide, indium-doped tin oxide, zinc oxide, aluminum-doped zinc oxide, fluorine-doped tin oxide, and metal grids. The first transparent conductive layer and the second transparent conductive layer can be prepared by chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, spin coating, medium frequency magnetron sputtering method, and direct current magnetron sputtering method.
[0009] The electrochromic electrode layer can be a cathode electrochromic material such as tungsten oxide, molybdenum oxide, and corresponding tungsten oxide and molybdenum oxide doped with different transition metals. The electrochromic electrode layer can be prepared by chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, magnetron sputtering method, reactive magnetron sputtering and the like.
[0010] The composite electrolyte layer is a film layer arranged on the surface of one side of the electrochromic electrode layer, and its structure is a composite structure of a porous inorganic solid film layer and a liquid electrolyte, wherein the porous inorganic film layer is a porous inorganic oxide film layer including Al2O3, Ta2O5, and Nb2O5, and the film layer thickness is between 100-500nm, wherein the porous pore size is between 10-1000nm, and the liquid electrolyte is filled in the pores of the porous inorganic oxide film layer.
[0011] The porous inorganic oxide film layer in the composite electrolyte layer can be prepared by PS template method, using photolithography, chemical etching and anodic oxidation of metal film.
[0012] The liquid electrolyte can be a lithium salt solution, such as lithium hexafluorophosphate (LiPF6), lithium tetrafluoroborate (LiBF4), lithium hexafluoroarsenate (LiAsF6), lithium perchlorate (LiClO4), lithium bis(trifluoromethanesulfonyl)imide, etc., as well as a solution of a salt that can transport metal ions, such as a sodium salt, an aluminum salt, a magnesium salt, etc., wherein the solvent can be non-aqueous ethylene carbonate (EC), propylene carbonate (PC), diethyl carbonate (DEC), dimethyl carbonate (DMC), ethyl methyl carbonate (EMC), etc. and their mixed solvents.
[0013] The ion storage layer can be an anode electrochromic material such as nickel oxide, lithium-doped nickel oxide, tungsten-doped nickel oxide, and lithium- and tungsten-doped nickel oxide, wherein the ion storage electrode layer can be prepared by chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, magnetron sputtering, reactive magnetron sputtering and the like.
[0014] The electrochromic device of the present invention is prepared by the following method: (1) A clean transparent substrate is used as the first substrate to prepare a first substrate film layer, wherein the first substrate can be a glass or plastic substrate such as PET. If it is glass, it is preferably float glass, and its thickness is 0.1-10 mm. The specific process includes the following: (a) firstly, a silicon oxide film is prepared on the first substrate, the film thickness is 10-100 nm, wherein the silicon oxide film has a barrier layer protection function, and the specific preparation method can be chemical vapor deposition, medium frequency magnetron sputtering, radio frequency magnetron sputtering and medium frequency reactive magnetron sputtering; (b) On a first substrate prepared with a silicon oxide thin film, a first transparent conductive layer is prepared on the surface of the silicon oxide side, and the film thickness is 50-300nm. The first transparent conductive layer can be a conductor material that can achieve transparency and conduct electrons, such as ITO, AZO, FTO and metal grid. The preparation method can be chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, spin coating, medium frequency magnetron sputtering method and direct current magnetron sputtering method.
[0015] (c) preparing an electrochromic electrode layer on the surface of the first transparent conductive layer on the first substrate, wherein the film thickness is 50-500 nm, wherein the electrochromic electrode layer can be prepared by chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, magnetron sputtering method, reactive magnetron sputtering and the like; (d) preparing an inorganic oxide film layer with a honeycomb porous structure on the surface of the electrochromic electrode layer of the first substrate, wherein the inorganic oxide can be a metal oxide film layer such as aluminum oxide, tantalum oxide, niobium oxide, etc., the thickness of the oxide film layer is between 100-500nm, wherein the porous pore size is between 10-1000nm, wherein the porous inorganic oxide film layer can be prepared by PS template method, photolithography, chemical etching and anodization of metal film and the like; (e) applying an electrolyte droplet onto the porous inorganic oxide film layer on the first substrate to form a composite electrolyte film layer having a composite structure of porous oxide and electrolyte; (2) Take a second clean transparent substrate as the second substrate, wherein the second substrate can be glass or a plastic substrate such as PET. If it is glass, it is preferably float glass, and its thickness is 0.1-10 mm. The second substrate and the first substrate can be made of the same material or different materials. The thickness of the second substrate and the first substrate can be the same or different. Prepare a second substrate film layer on the surface of the second substrate. Specifically, it includes the following processes: (a) preparing a second transparent conductive layer on the surface of the second substrate; the second transparent conductive layer can be a material that can achieve transparent conductivity, such as ITO, AZO, FTO and metal grid, wherein the film thickness is 50-300nm, and the preparation method can be chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, spin coating, medium frequency magnetron sputtering and direct current magnetron sputtering.
[0016] (b) preparing an ion storage layer on the second transparent conductive layer of the second substrate, wherein the thickness of the ion storage layer is 50-500 nm, wherein the preparation method of the ion storage layer can be chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, magnetron sputtering method, reactive magnetron sputtering, etc.; (c) coating a gel-type ion-conducting electrolyte layer on the surface of the ion storage layer on the second substrate, wherein the gel-type ion-conducting electrolyte is a commonly used gel-type electrolyte in this field and has the function of bonding the membrane layers on both sides, wherein the gel-type ion-conducting electrolyte layer has a thickness of 100-1000 nm and can be prepared by spin coating, scraping coating, etc.; (3) The composite electrolyte membrane layer side of the first substrate membrane layer and the gel-type ion electrolyte layer side of the second substrate membrane layer are tightly attached together, pressed together, and sealed.
[0017] The advantages of the present invention are: the problem of low ion conductivity of the solid ion conductor layer is improved by introducing an electrolyte, and the risk of leakage is reduced by fixing and encapsulating the electrolyte in a honeycomb porous structure. DETAILED DESCRIPTION Example
[0018] The present invention provides an electrochromic device, comprising the following functional film layers: a first transparent substrate, a first transparent conductive layer, an electrochromic electrode layer, a composite electrolyte layer, an ion storage layer, a second transparent conductive layer and a second substrate layer sequentially prepared on the surface of one side of the transparent substrate, wherein the composite electrolyte layer is a film layer arranged on the surface of one side of the electrochromic electrode layer, and its structure is a composite structure of a porous inorganic solid film layer and a liquid electrolyte, wherein the porous inorganic film layer is a porous inorganic oxide film layer including Al2O3, Ta2O5, and Nb2O5, and the film layer thickness is between 100-500nm, wherein the porous pore size is between 10-1000nm, and the liquid electrolyte is filled in the pores of the porous inorganic oxide film layer.
[0019] The liquid electrolyte can be a lithium salt solution, including lithium hexafluorophosphate (LiPF6), lithium tetrafluoroborate (LiBF4), lithium hexafluoroarsenate (LiAsF6), lithium perchlorate (LiClO4), lithium bis(trifluoromethanesulfonyl)imide, etc., as well as solutions of salts that can transport metal ions, such as sodium salts, aluminum salts, and magnesium salts, wherein the solvent is non-aqueous ethylene carbonate (EC), propylene carbonate (PC), diethyl carbonate (DEC), dimethyl carbonate (DMC), ethyl methyl carbonate (EMC) and their mixed solvents.
[0020] The transparent substrate may be glass or an organic flexible substrate such as PET, PMMA, PC, and CPI, and the transparent conductive layer material on one side of the substrate may be a material that can achieve transparent conductivity, such as ITO, AZO, FTO, and a metal grid; The electrochromic layer is a cathode electrochromic material such as WO3, MoO3, etc., and the ion storage layer is an anode electrochromic material such as NiO, LixNiOy, etc. Example
[0021] The present invention provides a method for preparing an electrochromic device, comprising the following steps: (1) Using glass as the substrate, a layer of SiO2 film with a thickness of 10-100 nm is first prepared on a clean glass substrate by reactive sputtering; (2) An ITO transparent conductive film layer was prepared on the surface of the glass substrate with silicon oxide film by magnetron sputtering, and the film layer thickness was 300 nm; (3) A cathode electrochromic layer WO3 film was prepared on the ITO surface by reactive sputtering, and the film thickness was 300 nm; (4) A single-layer PS template layer was prepared on the surface of the WO3 film layer by a doctor blade method. The particle size of the PS beads was 300 nm. After the template layer was dried, an aluminum oxide film was prepared on the PS template layer by a sol-gel method. The film thickness was about 150 nm. After the preparation was completed, it was calcined in a high-temperature furnace at 400 degrees Celsius for 30-60 minutes to remove the PS template layer. The obtained aluminum oxide film layer had a honeycomb porous structure. The pore size of the aluminum oxide film layer was 100-300 nm, the spatial distance was 100-120 nm, and the pore depth of the film was 140-150 nm. (5) applying electrolyte droplets on the porous alumina membrane layer to form a composite electrolyte membrane layer having a composite structure of porous alumina and electrolyte; (6) Take a second clean glass and prepare a 300 nm thick ITO film layer on its surface; (7) Preparing a NiO film layer on the ITO film layer on the glass surface, with a film thickness of 300 nm; (8) coating a gel ion conductor layer on the surface of the NiO film layer prepared in step (7); (9) Laminating the second piece of glass prepared with ITO and NiO film layers with the functional layer prepared with the first transparent conductive layer, the cathode electrochromic layer WO3 and the composite electrolyte layer. Specifically, the surface of the NiO film layer on the second piece of glass is tightly attached to the surface of the composite electrolyte film layer on the first piece of glass, and the two are pressed and sealed. Example
[0022] Another method for preparing an electrochromic device provided by the present invention comprises the following steps: (1) Using glass as the substrate, a layer of SiO2 film with a thickness of 10-100 nm is first prepared on a clean glass substrate by reactive sputtering; (2) An ITO transparent conductive film layer was prepared on the surface of the glass substrate with silicon oxide film by magnetron sputtering, and the film layer thickness was 300 nm; (3) A cathode electrochromic layer WO3 film was prepared on the ITO surface by reactive sputtering, and the film thickness was 300 nm; (4) using magnetron sputtering to prepare a layer of aluminum film on the surface of the WO3 film in step (3), with a thickness of 500-1000 nm; (5) The aluminum film was treated with a secondary anodization method at 0.3 mol·L -1Anodic oxidation was performed in a H2C2O4 aqueous solution at a constant DC voltage of 40V and a temperature of 5°C. The film layer except the metal aluminum was controlled not to contact the solution. After the reaction was completed, it was repeatedly rinsed with deionized water to clean the residual H2C2O4 aqueous solution and dried naturally to obtain a porous aluminum oxide film with a pore size of 100-200nm and a space distance of about 100nm. The film pore depth was 100-500nm. (6) applying electrolyte droplets on the porous alumina membrane layer to form a composite electrolyte membrane layer having a composite structure of porous alumina and electrolyte; (7) Take a second clean glass and prepare a 300 nm thick ITO film layer on its surface; (8) Preparing a NiO film layer on the ITO film layer on the glass surface, with a film thickness of 300 nm; (9) coating a gel ion conductor layer on the surface of the NiO film layer prepared in step (7); (10) The second glass with ITO and NiO film layers is placed on the glass with the first transparent conductive layer and cathode electrochromic layer WO3 And the functional layer of the composite electrolyte layer is pressed, specifically, one side surface of the NiO film layer of the second glass is tightly attached to one side surface of the composite electrolyte film layer of the first glass, pressed, and sealed.
Claims
1. An electrochromic device, comprising a transparent substrate, a first transparent conductive layer, an electrochromic electrode layer, a composite electrolyte layer, an ion storage layer, and a second transparent conductive layer sequentially prepared on a surface of one side of the transparent substrate, characterized in that: The composite electrolyte layer is a film layer arranged on the surface of the electrochromic layer, and its structure is a composite structure of a porous inorganic solid film layer and a liquid electrolyte, wherein the porous inorganic film layer is a porous inorganic oxide film layer including Al2O3, Ta2O5, and Nb2O5, and the film layer thickness is between 100-500nm, wherein the porous pore size is between 10-1000nm, and the liquid electrolyte is filled in the pores of the porous inorganic oxide film layer.
2. An electrochromic device according to claim 1, characterized in that: The liquid electrolyte is a lithium salt solution, including one or a combination of lithium hexafluorophosphate LiPF6, lithium tetrafluoroborate LiBF4, lithium hexafluoroarsenate LiAsF6, lithium perchlorate LiClO4, and lithium bis(trifluoromethanesulfonyl)imide; the liquid electrolyte is also a solution of a salt that can transport metal ions, including sodium salt, aluminum salt, and magnesium salt; the solvent of the liquid electrolyte is one or a mixed solvent of non-aqueous ethylene carbonate EC, propylene carbonate PC, diethyl carbonate DEC, dimethyl carbonate DMC, and ethyl methyl carbonate EMC.
3. An electrochromic device according to claim 1 or 2, characterized in that: The transparent substrate includes glass, PET, PMMA, PC and CPI organic flexible substrates.
4. An electrochromic device according to claim 1-2, characterized in that: The first transparent conductive layer and the second transparent conductive layer are made of ITO, AZO, FTO and metal grid, which are conductive materials that are transparent and capable of conducting electrons.
5. An electrochromic device according to claim 1 or 2, characterized in that: The electrochromic electrode layer can be tungsten oxide, molybdenum oxide, and corresponding tungsten oxide and molybdenum oxide cathode electrochromic materials doped with different transition metals.
6. An electrochromic device according to claim 5, characterized in that: The ion storage layer is nickel oxide, nickel oxide doped with metallic lithium, nickel oxide doped with tungsten, and nickel oxide doped with tungsten and lithium.
7. A method for preparing an electrochromic device as claimed in claims 1 to 6, characterized in that The following steps are involved: (1) A clean transparent substrate is used as a first substrate to prepare a first substrate film layer, wherein the first substrate can be a glass substrate or a plastic substrate such as PET. If it is glass, it is preferably float glass, and its thickness is 0.1-10 mm. Specifically, the following sub-steps are included: (a) firstly, a silicon oxide film is prepared on a first substrate, the film thickness of which is 10-100 nm, wherein the silicon oxide film has a function of a barrier protective layer, and the specific preparation method can be chemical vapor deposition, medium frequency magnetron sputtering, radio frequency magnetron sputtering, medium frequency reactive magnetron sputtering, etc.; (b) On a first substrate with a silicon oxide film, a first transparent conductive layer is prepared on the surface of the silicon oxide side, and the film thickness is 50-300 nm. The first transparent conductive layer can be a conductor material that can achieve transparency and conduct electrons, such as ITO, AZO, FTO, and a metal grid. The preparation method can be chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, spin coating, medium frequency magnetron sputtering, and DC magnetron sputtering. (c) preparing an electrochromic electrode layer on the surface of the first transparent conductive layer on the first substrate, wherein the film thickness is 50-500 nm, wherein the electrochromic electrode layer can be prepared by chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, magnetron sputtering method, reactive magnetron sputtering and the like; (d) preparing a honeycomb porous inorganic oxide film layer on the surface of the electrochromic electrode layer of the first substrate, wherein the inorganic oxide can be a metal oxide film layer such as aluminum oxide, tantalum oxide, niobium oxide, etc., and the thickness of the oxide film layer is between 100-500nm, wherein the porous pore size is between 10-1000nm, wherein the porous inorganic oxide film layer can be prepared by PS template method, photolithography, chemical etching and anodization of metal film; (e) applying an electrolyte droplet onto the porous inorganic oxide film layer on the first substrate to form a composite electrolyte film layer having a composite structure of the porous inorganic oxide and the electrolyte; (2) Take a second clean transparent substrate as the second substrate, wherein the second substrate is a glass or PET plastic substrate. If it is glass, it is preferably float glass, and its thickness is 0.1-10 mm. The second substrate and the first substrate can be made of the same material or different materials. Prepare a second substrate film layer on the surface of the second substrate, which specifically includes the following sub-steps: (a) preparing a second transparent conductive layer on the surface of the second substrate; the second transparent conductive layer is a conductive material that can achieve transparency and conduct electrons, such as ITO, AZO, FTO and metal grid, wherein the film thickness is 50-300nm, and the preparation method is chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, spin coating, medium frequency magnetron sputtering and DC magnetron sputtering; (b) preparing an ion storage layer on the second transparent conductive layer of the second substrate, wherein the thickness of the ion storage layer is 50-500 nm, wherein the ion storage layer is prepared by chemical vapor deposition, physical vapor deposition, wet chemical method, sol-gel method, magnetron sputtering method and reactive magnetron sputtering; (c) coating a gel-type ion-conducting electrolyte layer on the surface of the ion storage layer on the second substrate, wherein the gel-type ion-conducting electrolyte is a commonly used gel-type electrolyte in this field and has the function of bonding the membrane layers on both sides, wherein the gel-type ion-conducting electrolyte layer has a thickness of 100-1000 nm and is prepared by spin coating or scraping coating; (3) The composite electrolyte membrane layer side of the first substrate membrane layer and the gel-type ion electrolyte layer side of the second substrate membrane layer are tightly attached together, pressed together, and sealed.
Citation Information
Patent Citations
Preparation of porous quasi-solidus electrochromism PVB electrolyte membrane with electrostatic spinning method and preparing technology thereof
CN107422564A
High-performance solid-state electrochromic supercapacitor
CN114530337A
Electrochromic device
CN116931329A
Porous polymer film and solid electrolyte film
JP1994287336A
Manufacturing method of smart window with porous membrane
KR1020170040615A