Method and system for measuring surface microstructure of wick

Through image processing and data analysis technology, combined with scanning electron microscope and Nano Measurer software, the problem of low accuracy of traditional measurement methods is solved, high-precision measurement and analysis of the microstructure of the liquid absorbent core surface is realized, the processing technology is optimized, and the microstructure is improved Forming quality.

CN118887189APending Publication Date: 2024-11-01XIAMEN UNIV
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202410972265.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The traditional microstructure measurement method for surface microstructures of liquid absorbent cores has problems such as low measurement accuracy, low efficiency and high cost, and it is difficult to accurately evaluate the microstructure forming quality.

Method used

Image processing and data analysis technology are used to obtain microstructure images through scanning electron microscopy, and combined with Nano Measurer software and data processing software, the microstructure size data is automatically marked and analyzed to achieve high-precision microstructure measurement and analysis.

Benefits of technology

It improves the accuracy and efficiency of microstructure measurement on the surface of the liquid absorbent core, and can efficiently obtain the size distribution information of the micro particle size, help optimize the processing technology and improve the microstructure forming quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118887189A_ABST
    Figure CN118887189A_ABST
Patent Text Reader

Abstract

The invention relates to a method and system for measuring the surface microstructure of a wick, and the method comprises the steps: selecting a plurality of groups of wick samples with the same processing technology and different processing parameters, and obtaining a local image, containing the microstructure, of the surface of each group of wick samples; importing the local images of each group of wick samples into statistical analysis software, setting a scale, a marking line and a particle serial number, and performing marking statistics on the microstructures of the same type on the local images to obtain size data and a size distribution diagram of all marked microstructures; the size data of all the marked microstructures are analyzed and processed, the influence of different process parameters under the same machining process on the forming quality of the microstructures is analyzed, the accuracy and efficiency of size distribution measurement of the microstructures on the surface of the wick are improved, and important reference is provided for design and manufacturing of heat pipes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of heat pipe wick processing and manufacturing, in particular to a wick surface microstructure measurement method and system. Background Art

[0002] As an efficient heat transfer device, heat pipes are widely used in electronic equipment, aerospace technology, energy systems and other fields. As one of the core components of heat pipes, the design and manufacture of the internal microstructure of the wick is crucial to the heat transfer performance and stability of the heat pipe. Due to processing problems, the surface formation of the wick has a certain randomness, but relevant studies have shown that the size distribution of its surface microstructure directly affects the capillary suction performance and heat transfer performance of the heat pipe.

[0003] Traditional methods for measuring the size distribution of microstructures on the surface of wicks are mainly based on microscopic observation and traditional measuring tools, and rely on complex and tedious manual operations. They have problems such as low measurement accuracy, low measurement efficiency, large number of samples, and high processing costs. In order to address these challenges, it is urgent to seek advanced measurement technologies and methods to improve the accuracy and reliability of wick surface microstructure measurements. Summary of the invention

[0004] The main purpose of the present invention is to overcome the above-mentioned defects in the prior art and to provide a method and system for measuring the surface microstructure of a liquid-wick, which can achieve efficient and accurate measurement based on image processing and data analysis.

[0005] The present invention adopts the following technical solution:

[0006] A method for measuring the surface microstructure of a liquid wick, comprising:

[0007] Select multiple groups of wick samples with the same processing technology and different processing parameters, and obtain local images including microstructures on the surface of each group of wick samples;

[0008] Importing the local image of each group of wick samples into statistical analysis software, setting the scale, marking line and particle serial number, marking and counting the microstructures of the same type on the local image, and obtaining the size data and size distribution diagram of all marked microstructures;

[0009] The dimension data of all marked microstructures are analyzed and processed to analyze the influence of different process parameters under the same processing technology on the forming quality of the microstructures.

[0010] The processing technology is one or more of sintering, chemical treatment, electrolysis, 3D printing or extrusion forming; the microstructure is one or more of micropores, micropits, microgrooves or microconvexities.

[0011] The size of the microstructure is micrometer or nanometer; a local image of the surface of the wick sample containing the microstructure is obtained by scanning electron microscopy, the nanometer-scale microstructure corresponds to a shooting scale of 1nm-200nm, and the micrometer-scale microstructure corresponds to a shooting scale of 1μm-200μm.

[0012] In the statistical analysis software, the scale range corresponding to the nano-scale microstructure is 1nm-200nm, and the scale range corresponding to the micro-scale microstructure is 1μm-200μm.

[0013] The particle serial number is located on the marking line or on both sides of the marking line, and the marked serial number is displayed in combination with the color setting.

[0014] The size data of all the marked microstructures are analyzed and processed using data processing software, and the data processing software is one or more of Origin, GraphPad Prism, and SPSS.

[0015] The analysis and processing of the dimension data includes one or more of average value calculation, statistical analysis, curve fitting, statistical charts, and variance analysis.

[0016] The reference data of the forming quality include one or more of the maximum pore size, the minimum pore size, and the average pore size.

[0017] It also includes determining the optimal processing parameters of the processing technology according to the coupling relationship between the forming quality, the process parameters and the microstructure size.

[0018] A liquid wick surface microstructure measurement system, comprising:

[0019] The image acquisition device selects a plurality of groups of wick samples with the same processing technology and different processing parameters, and obtains a local image including a microstructure on the surface of each group of wick samples;

[0020] A size statistical marking device is provided with a scale, a marking line and a particle serial number in advance, and performs marking statistics on microstructures of the same type on the local image to obtain size data and a size distribution diagram of all marked microstructures;

[0021] The data analysis device analyzes and processes the size data of all marked microstructures, and analyzes the influence of different process parameters under the same processing technology on the forming quality of the microstructures.

[0022] It can be seen from the above description of the present invention that, compared with the prior art, the present invention has the following beneficial effects:

[0023] The present invention utilizes digital image processing technology and advanced computer-aided design tools to achieve digital measurement and high-precision analysis of the surface microstructure of the wick, which can not only automatically control the measurement process, but also improve the measurement accuracy and achieve efficient measurement of more samples.

[0024] The present invention adopts a scanning electron microscope, Nano Measurer software and data processing software to realize micro surface structure measurement, covering a size range of 1nm-100μm, meeting the measurement requirements for tiny particle sizes, and can efficiently and accurately obtain the micro structure size distribution information on the surface of the liquid absorbent core, so as to make a reasonable evaluation of the micro structure forming quality.

[0025] The present invention analyzes the statistical pore size through data processing software to achieve a comparative study on the microstructure forming quality under different processing technologies, which is helpful for in-depth research and optimization of the influence of processing technology in the field of microstructure preparation. Compared with the intuitive evaluation based on SEM images in traditional research, it provides important technical support for improving the microstructure forming quality and provides comprehensive data theoretical support for optimizing the processing technology.

[0026] The method of the present invention has wide applicability, and the processing technology includes but is not limited to sintering, chemical treatment, electrolysis, 3D printing, extrusion molding and other methods. It can be applied to the preparation process of different liquid-absorbing cores and has a wide range of applications. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 is a flow chart of the method of the present invention;

[0028] Figure 2 Partial image of the wick manufactured by 3D printing with a laser scanning power of 120W;

[0029] Figure 3 Schematic diagram of using Nano Measurer software to quantify the number and size of local wick micropores for 120W processed samples;

[0030] Figure 4 Schematic diagram of the 80W sample using Origin software to mathematically process the aperture data;

[0031] Figure 5 Schematic diagram of the 120W sample using Origin software to mathematically process the aperture data;

[0032] Figure 6 Comparison results of Gaussian fitting curves of pore size distribution of 120W sample and 80W sample.

[0033] The present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. DETAILED DESCRIPTION

[0034] The present invention is further described below through specific implementation modes.

[0035] See also Figure 1 , a method for measuring the surface microstructure of a liquid wick comprises the following steps:

[0036] 1) Select multiple groups of wick samples with the same processing technology and different processing parameters, and obtain local images including microstructures on the surface of each group of wick samples.

[0037] The wick sample was taken from the wick for heat pipe, which was manufactured using certain processing parameters. After cleaning and drying, it was sealed and stored. The wick sample was fixed to the scanning electron microscope sample stage using double-sided tape, and then observed by scanning electron microscope. A representative local image containing microstructure distribution was taken on the surface of the wick manufactured by each set of processing parameters. For microstructure gaps with too large an order of magnitude difference, different scales were set to obtain clear local images. The shooting areas under different processing parameter groups should be the same.

[0038] In the present invention, the processing technology of the liquid absorbent core is one or more of sintering, chemical treatment, electrolysis, 3D printing or extrusion forming. The microstructure on the surface of the liquid absorbent core includes one or more of micropores, micropits, microgrooves or microconvexities.

[0039] The size of the microstructure is micrometer or nanometer; a local image of the surface of the wick sample containing the microstructure is obtained by a scanning electron microscope, the corresponding shooting scale of the nanometer-scale microstructure is 1nm-200nm, and the corresponding shooting scale of the micrometer-scale microstructure is 1μm-200μm.

[0040] 2) Import the local image of each group of wick samples into statistical analysis software, set the scale, marking line and particle number, mark and count the microstructures of the same type on the local image, and obtain the size data and size distribution diagram of all marked microstructures. The particle number is located on the marking line or on both sides of the marking line, and the marked number is displayed in combination with the color setting.

[0041] The statistical analysis software may be Nano Measurer software, but is not limited thereto. Convert the local image file taken by the scanning electron microscope from tif format to jpg or bmp format, then import it into the statistical analysis software, set the scale, marking line and particle number. Among them, the scale range corresponding to the nano-scale microstructure is 1nm-200nm, and the scale range corresponding to the micron-scale microstructure is 1μm-200μm. Mark and count the same type of microstructures on the electron microscope image, and view the size of the corresponding number through real-time reports.

[0042] In this step, after all targets are marked, the report is checked to obtain the microstructure size and size distribution diagram of all marks, and the size data and distribution diagram are reprocessed to make them more intuitive.

[0043] 3) Analyze and process the dimensional data of all marked microstructures, and analyze the influence of different process parameters on the microstructure forming quality under the same processing technology.

[0044] In this step, the size data of all the marked microstructures are analyzed and processed using data processing software, and the data processing software is one or more of Origin, GraphPad Prism, SPSS, etc. The size data report is exported to txt format, and then the size data is imported into the data processing software for size data analysis.

[0045] The analysis and processing of the dimension data includes one or more of average value calculation, statistical analysis, curve fitting, statistical charts, and variance analysis. The specific description is as follows:

[0046] Average calculation:

[0047] The maximum, minimum, and average values ​​of the micropore diameter, micropit diameter, microgroove width, and microconvex diameter are calculated respectively to obtain the average size of the microstructure in each group of samples (e.g. the average value of the maximum value, the average value of the minimum value, and the overall average value of each group of samples), providing a basis for subsequent data analysis.

[0048] Statistical analysis:

[0049] For different groups of samples with the same processing parameters, the size distribution, frequency, mean, standard deviation and number of microstructures per unit area were calculated, and the randomness of microstructure formation under the processing parameters was compared to avoid contingency.

[0050] Curve Fitting:

[0051] Perform Gaussian curve fitting or other appropriate curve fitting methods on the size data and distribution, analyze the size distribution characteristics, and gain an in-depth understanding of the size distribution law under certain processing parameters through fitting curves.

[0052] Statistical charts:

[0053] Based on the average value calculation, statistical analysis, and curve fitting results, the data and curves under different processing parameters are integrated into the same chart to intuitively show the differences in the size and quantity of microstructure features under different processing parameters, helping to understand and compare the data more intuitively.

[0054] ANOVA:

[0055] Variance analysis was performed on the dimensional data and the number of microstructures between different processing parameter groups to determine which processing parameters have a significant impact on the microstructure forming quality, so as to optimize the processing parameters and improve the forming quality.

[0056] In the present invention, the reference data of the forming quality include one or more of the maximum pore size, the minimum pore size, and the average pore size. That is, the forming quality of the absorbent core is evaluated according to one or more of the maximum pore size, the minimum pore size, or the average pore size. By analyzing these reference data, the forming quality of the absorbent core can be comprehensively evaluated. For example, smaller pore size variation and uniform pore size distribution usually indicate higher forming quality, and when the average pore size is small and the number of microstructures is large, the absorbent core often shows excellent heat and mass transfer performance.

[0057] The present invention also includes determining the optimal processing parameters of the processing technology according to the coupling relationship between the forming quality, the process parameters and the microstructure size. For example, the processing parameters corresponding to the liquid-absorbing core with the best forming quality are used as the optimal processing parameters of the processing technology. According to the forming conditions of the microstructure under the different processing parameter combinations of different processing technologies, the influence of different processing technologies on the forming quality is judged, and the optimal processing parameters of the processing technology corresponding to the optimal forming quality are obtained. The specific method includes: the processing technology A has three design parameters a1, a2, and a3, and the processing technology B has three design parameters b1, b2, and b3. Through statistical analysis of the microstructure forming conditions under the processing parameter combinations of a1b1, a1b2, a1b3, a2b1, a2b2, a2b3, a3b1, a3b2, and a3b3, the influence of processes A and B on the forming quality, the mutual influence between processes A and B, and the process A and B parameter groups that can obtain the optimal forming quality can be obtained.

[0058] Based on this, the present invention also proposes a system for measuring the surface microstructure of a liquid wick, comprising:

[0059] The image acquisition device selects a plurality of groups of wick samples with the same processing technology and different processing parameters, and obtains a local image including a microstructure on the surface of each group of wick samples.

[0060] The size statistical marking device pre-sets the scale, marking line and particle serial number, and performs marking statistics on the microstructures of the same type on the local image to obtain the size data and size distribution diagram of all marked microstructures. The size statistical marking device includes statistical analysis software, such as Nano Measurer software, but is not limited thereto.

[0061] The data analysis device analyzes and processes the size data of all marked microstructures, and analyzes the influence of different process parameters under the same processing technology on the microstructure forming quality. The data analysis device includes the above-mentioned data processing software, which is one or more of Origin, GraphPad Prism, SPSS, etc.

[0062] The system of the present invention uses a graphics acquisition device to implement step 1) of the above-mentioned method for measuring the surface microstructure of a liquid-absorbing core, and uses a size statistical marking device to implement the above-mentioned step 2).

[0063] Application Examples

[0064] The absorbent cores manufactured by selective laser sintering 3D printing technology have the same structure design. The only processing parameter that differs between different experimental groups is the laser power. 316L stainless steel metal powder is used as the printing raw material. The laser scanning power is set to 80W and 120W respectively, and three samples are processed at each power. The 3D printed absorbent cores are washed with deionized water, dried at 80℃, and sealed for storage.

[0065] Use a scanning electron microscope to observe and record images. The scanning electron microscope model used in this embodiment is ZEISS SUPRA55SAPPHIRE, with a resolution of 0.8nm@15KV; 1.6nm@1KV and a magnification of 12 to 1,000,000 times. Use double-sided tape to fix the wick to the scanning electron microscope sample stage. Follow the standard scanning electron microscope procedure and take a picture of the central area of ​​the wick at a scale of 200μm. Take a picture of a relatively uniform distribution of microstructures. Six samples are taken at the same position. The local images are as follows: Figure 2 shown.

[0066] The scanning electron microscope image file was converted from tif format to jpg format using the image format conversion tool, and then imported into the Nano Measurer software. The scale was set to 200um, and the particle number was on the marking line. The marking line and the number text were both white. Then, the maximum pore size of the microporous structure on the SEM image was marked one by one. The number of marks must be greater than 10. The marking process is as follows: Figure 3 As shown, by checking the report, you can get the particle size bar distribution diagram and all single marked target sizes. Under the same scanning power, 34 holes are marked for each of the three samples, and then the lowest value and the highest value are removed, that is, the aperture data for the same power is 100. After marking, the report is exported to txt format, and the data is used for processing in Origin software. The average and variance of all maximum aperture data of the three samples under the same scanning power are calculated, and Gaussian curves are used to fit all aperture data of the same sample. The curves of different samples are placed in the same chart for comparative analysis.

[0067] Scanning electron microscopy showed that the pore size of the 3D printed wick is relatively uniform, the micropores are neatly arranged, the distance between each pore is roughly the same, and a small amount of particles are attached to the surface. In this example, the pore size range is about 350-440um at 80W, the average pore size is 388.46um, and the pore size distribution Gaussian fitting image is as follows Figure 4As shown; the aperture range at 120W is about 360-460um, the average aperture is about 404.81um, and the aperture distribution Gaussian fitting image is as follows Figure 5 As shown; the comparison of the two power Gaussian fitting curves is Figure 6 As shown in the figure, the pore size range under 80W is mainly concentrated around 385um, and the pore size distribution under 120W is uniform. Relatively speaking, the number of large pores in 120W is obviously more than that in 80W, and the number of small pores accounts for a small proportion. The pore size greater than 400um accounts for 54% in 120W and 25% in 80W; the average pore size of the 120W absorbent core is about 4.2% higher than that of 80W. From the comprehensive analysis of the data, it can be inferred that in order to obtain a 3D printed absorbent core with a larger pore size, a scanning power of 120W should be selected. When optimizing the scanning power processing parameter, set the scanning power to 100W and 140W and repeat the above steps, compare the pore size data between different groups, until the absorbent core with ideal pore size distribution is obtained, and the above steps can also be referred to when optimizing other parameters such as scanning speed and absorbent core structure parameters.

[0068] In summary, the present invention combines scanning electron microscopy (SEM) technology with Nano Measurer software and data processing software, and can observe the characteristics of the number of microstructures and pore size distribution on the surface of the wick. When exploring the processing technology of the wick and the relationship between the characteristics, the microstructure characteristics under different processing technologies can be scientifically analyzed according to data processing, and it has broad application prospects.

[0069] The above is only a specific implementation of the present invention, but the design concept of the present invention is not limited thereto. Any non-substantial changes to the present invention using this concept shall be deemed as an infringement of the protection scope of the present invention.

Claims

1. A method for measuring the surface microstructure of a liquid wick, It is characterized in that include: Select multiple groups of wick samples with the same processing technology and different processing parameters, and obtain local images including microstructures on the surface of each group of wick samples; Importing the local image of each group of wick samples into statistical analysis software, setting the scale, marking line and particle serial number, marking and counting the microstructures of the same type on the local image, and obtaining the size data and size distribution diagram of all marked microstructures; The dimension data of all marked microstructures are analyzed and processed to analyze the influence of different process parameters under the same processing technology on the forming quality of the microstructures.

2. A method for measuring the surface microstructure of a liquid wick as claimed in claim 1, Features: The processing technology is one or more of sintering, chemical treatment, electrolysis, 3D printing or extrusion forming; the microstructure is one or more of micropores, micropits, microgrooves or microconvexities.

3. A method for measuring the surface microstructure of a liquid wick as claimed in claim 1, Features: The size of the microstructure is micrometer or nanometer; a local image of the surface of the wick sample containing the microstructure is obtained by scanning electron microscopy, the nanometer-scale microstructure corresponds to a shooting scale of 1nm-200nm, and the micrometer-scale microstructure corresponds to a shooting scale of 1μm-200μm.

4. A method for measuring the surface microstructure of a liquid wick as claimed in claim 3, Features: In the statistical analysis software, the scale range corresponding to the nano-scale microstructure is 1nm-200nm, and the scale range corresponding to the micro-scale microstructure is 1μm-200μm.

5. A method for measuring the surface microstructure of a liquid wick as claimed in claim 1, Features: The particle serial number is located on the marking line or on both sides of the marking line, and the marked serial number is displayed in combination with the color setting.

6. A method for measuring the surface microstructure of a liquid wick as claimed in claim 1, Features: The size data of all the marked microstructures are analyzed and processed using data processing software, and the data processing software is one or more of Origin, GraphPadPrism, and SPSS.

7. A method for measuring the surface microstructure of a liquid wick as claimed in claim 1, Features: The analysis and processing of the dimension data includes one or more of average value calculation, statistical analysis, curve fitting, statistical charts, and variance analysis.

8. A method for measuring the surface microstructure of a liquid wick as claimed in claim 1, Features: The reference data of the forming quality include one or more of the maximum pore size, the minimum pore size, and the average pore size.

9. A method for measuring the surface microstructure of a liquid wick as claimed in claim 1, Features: It also includes determining the optimal processing parameters of the processing technology according to the coupling relationship between the forming quality, the process parameters and the microstructure size.

10. A system for measuring the surface microstructure of a liquid wick. Features: include The image acquisition device selects a plurality of groups of wick samples with the same processing technology and different processing parameters, and obtains a local image including a microstructure on the surface of each group of wick samples; A size statistical marking device is provided with a scale, a marking line and a particle serial number in advance, and performs marking statistics on microstructures of the same type on the local image to obtain size data and a size distribution diagram of all marked microstructures; The data analysis device analyzes and processes the size data of all marked microstructures, and analyzes the influence of different process parameters under the same processing technology on the forming quality of the microstructures.

Citation Information

Patent Citations

  • Method for classified machining of surface microstructures through four-axis linkage laser milling machine

    CN117182316A

  • Image-Based Assay Using Intelligent Monitoring Structures

    US20210181086A1

  • Particle Size Statistical Method of Granular Minerals of Shale

    US20240077401A1