Three-dimensional memory and preparation method thereof

By adopting a three-dimensional structure memory memory, it is optimized to a longitudinal electrode layer, and the performance problems caused by the reduction of the area of ​​the traditional two-dimensional memory is solved, and the mask process steps are reduced, achieving more efficient storage performance and cost reduction.

CN118946162AActive Publication Date: 2024-11-12GTA SEMICON CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411435695.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-15
Publication Date
2024-11-12
Estimated Expiration
2044-10-15

AI Technical Summary

Technical Problem

The reduction in the storage unit area of ​​traditional two-dimensional memory leads to a degradation of storage performance, and the photocoat process is complex, increasing production costs.

Method used

Using the preparation method of three-dimensional memory, by forming a semiconductor substrate, memory layer and electrode layer, it is optimized to a longitudinal structure, reducing the area of ​​the memory cell and reducing the mask process steps.

Benefits of technology

Improves storage performance, saves the area of ​​storage cells, reduces production costs, and avoids the impact of the performance reduction of the effective area of ​​the storage layer and the electrode layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118946162A_ABST
    Figure CN118946162A_ABST
Patent Text Reader

Abstract

The invention provides a three-dimensional memory and a preparation method thereof. The upper electrode layer and the lower electrode layer are optimized into the left electrode layer and the right electrode layer, a traditional transverse storage unit is optimized into the longitudinal storage unit, the effective area of a single storage unit is increased, the area of the single storage unit can be smaller, and the occupied area of the storage unit is saved; the storage performance can be improved by increasing the effective area of the device, and the operation efficiency and reliability of the device are optimized and improved. Due to the arrangement of the longitudinal storage unit, even if the first main connection structure in contact with the first electrode layer has a bulge, the deposition and phase change performance of the storage layer cannot be influenced; and when the second electrode layer is formed, the problem of etching through the storage layer does not exist, so that the performance of the storage unit can be prevented from being influenced. And only two contact hole photomask processes are needed, one contact hole photomask process is saved, and the production cost can be effectively reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a three-dimensional memory and a preparation method thereof. Background Art

[0002] New memory devices such as phase change memory (PRAM) or ferroelectric memory (FeRAM) are devices that integrate memory cells in the back-end of the line (BEOL). The storage performance of a memory cell is proportional to the effective area of ​​the storage layer and electrode layer in the memory cell.

[0003] The storage unit of the traditional two-dimensional (2D) memory is composed of an upper and lower electrode layer and a storage layer in the middle. The upper and lower electrode layers and the storage layer are deposited and grown layer by layer by atomic layer deposition (ALD). The storage layer is formed by phase change materials or ferroelectric materials. However, as the semiconductor process shrinks, the storage unit area of ​​the traditional two-dimensional memory becomes smaller, which further reduces the effective area of ​​the storage layer and the electrode layer, thereby affecting the storage performance of the memory; and the preparation of the connection structure connecting the upper and lower electrode layers of the storage unit requires multiple mask processes, resulting in increased production costs. Summary of the invention

[0004] The technical problem to be solved by the present invention is to provide a three-dimensional memory and a preparation method thereof, which can save the occupied area of ​​the storage unit and increase the effective area of ​​the device, thereby improving the storage performance, and can save the mask process and reduce the production cost.

[0005] In order to solve the above problems, the present invention provides a method for preparing a three-dimensional memory, the method comprising the following steps: forming a semiconductor substrate, the semiconductor substrate comprising a substrate, a first dielectric layer covering the surface of the substrate, a first main connection structure penetrating the first dielectric layer along a second direction and arranged at intervals along the first direction, and a first electrode layer formed on the surface of the first dielectric layer and in one-to-one contact with the first main connection structure, wherein the first direction is parallel to the substrate surface, and the second direction is perpendicular to the substrate surface; forming a storage layer and a second electrode layer, the storage layer at least covers a side wall of the first electrode layer and has an extension extending to the surface of the first dielectric layer, the second electrode layer covers the storage layer, and the maximum thickness of the second electrode layer in the second direction is greater than the thickness of the first electrode layer, wherein the first electrode layer, the storage layer, and the second electrode layer constitute a storage unit of the three-dimensional memory; forming a second dielectric layer, the second dielectric layer covers the first dielectric layer and all the storage units; and forming a second main connection structure, the second main connection structure penetrating the second dielectric layer along the second direction and in contact with the second electrode layer.

[0006] In some embodiments, the first main connection structure and the second main connection structure are made of a first metal material, the first electrode layer and the second electrode layer are made of a second metal material, and the first metal material and the second metal material are different.

[0007] In some embodiments, the material of the storage layer is a ferroelectric material or a phase change material, the materials of the first dielectric layer and the second dielectric layer are both oxide materials, the materials of the first main connection structure and the second main connection structure are both metal tungsten, and the materials of the first electrode layer and the second electrode layer are the same and are both selected from one of aluminum, copper, or aluminum-copper alloy.

[0008] In some embodiments, the steps of forming a semiconductor substrate specifically include: providing a substrate, having the first dielectric layer formed on the surface of the substrate, having first contact holes formed in the first dielectric layer, which penetrate the first dielectric layer along the second direction and are arranged at intervals along the first direction; filling the first contact hole with a first metal material to form the first main connection structure; depositing a second metal material and patterning it to form the first electrode layer on the surface of the first dielectric layer, which is in one-to-one contact with the first main connection structure.

[0009] In some embodiments, the step of depositing and patterning the second metal material specifically includes: depositing a second metal material layer on the surface of the first dielectric layer; forming a patterned first protective layer on the surface of the second metal material layer; etching the second metal material layer using the patterned first protective layer as a mask and the first dielectric layer as an etching stop layer to form the first electrode layer that is in one-to-one contact with the first main connection structure, and the first protective layer is retained and covers the surface of the first electrode layer.

[0010] In some embodiments, the steps of forming the storage layer and the second electrode layer specifically include: depositing a storage material to form a storage material layer covering the first dielectric layer and all of the first electrode layers; depositing a second metal material to form a second electrode material layer covering the storage material layer, wherein the maximum thickness of the second electrode material layer in the second direction is greater than the thickness of the first electrode layer; forming a patterned second protective layer on the surface of the second electrode material layer, wherein the patterned second protective layer can at least block a side wall of the first electrode layer and a portion of the first dielectric layer corresponding to the side wall; etching the second electrode material layer and the storage material layer using the patterned second protective layer as a mask and the first dielectric layer as an etching stop layer, etching the remaining storage material layer to form the storage layer, etching the remaining second electrode material layer to form the second electrode layer, and retaining and covering the surface of the second electrode layer.

[0011] In some embodiments, the patterned second protection layer can also shield the corresponding area of ​​the top surface of the first electrode layer; the storage layer also covers the top surface of the first electrode layer, and the second electrode layer completely covers the storage layer.

[0012] In some embodiments, the step of forming the second dielectric layer includes: forming an etching barrier layer, the etching barrier layer covers the first dielectric layer and all the storage units, and the second dielectric layer covers the etching barrier layer; the step of forming the second main connection structure specifically includes: using the etching barrier layer as an etching stop layer, etching in the second dielectric layer to form a second contact hole exposing the second electrode layer; depositing a first metal material and planarizing it to form the second main connection structure in the second contact hole.

[0013] In some embodiments, the top surface of the second main connection structure is flush with the top surface of the second dielectric layer; and the orthographic projection of the second main connection structure on the first dielectric layer is within the range of the orthographic projection of the extension portion on the first dielectric layer.

[0014] In some embodiments, the step of forming the second main connection structure includes: depositing a second metal material and patterning it to form a metal structure on the surface of the second dielectric layer that is in one-to-one contact with the second main connection structure.

[0015] In some embodiments, the first main connection structure and the second main connection structure are made of a first metal material, the first electrode layer, the second electrode layer and the metal structure are made of a second metal material, and the first metal material is different from the second metal material.

[0016] In some embodiments, a first auxiliary connection structure is formed while forming the first main connection structure, the first auxiliary connection structure penetrates the first dielectric layer along the second direction and is spaced apart from the first main connection structure; a second auxiliary connection structure is formed while forming the second main connection structure, the second auxiliary connection structure penetrates the second dielectric layer along the second direction and contacts the first auxiliary connection structure; wherein one of the metal structures is also in contact with an adjacent second auxiliary connection structure.

[0017] In order to solve the above problems, the present invention also provides a three-dimensional memory, comprising: a substrate; a first dielectric layer, covering the surface of the substrate; a first main connection structure, penetrating the first dielectric layer along a second direction and arranged at intervals along the first direction, wherein the first direction is parallel to the substrate surface and the second direction is perpendicular to the substrate surface; a first electrode layer, formed on the surface of the first dielectric layer and in one-to-one contact with the first main connection structure; a storage layer, covering at least one side wall of the first electrode layer and having an extension extending to the surface of the first dielectric layer; a second electrode layer, covering the storage layer, and the maximum thickness of the second electrode layer in the second direction is greater than the thickness of the first electrode layer, wherein the first electrode layer, the storage layer, and the second electrode layer constitute storage units of the three-dimensional memory; a second dielectric layer, covering the first dielectric layer and all the storage units; and a second main connection structure, penetrating the second dielectric layer along the second direction and in contact with the second electrode layer.

[0018] In some embodiments, the first main connection structure and the second main connection structure are made of a first metal material, the first electrode layer and the second electrode layer are made of a second metal material, and the first metal material and the second metal material are different.

[0019] In some embodiments, the material of the storage layer is a ferroelectric material or a phase change material, the materials of the first dielectric layer and the second dielectric layer are both oxide materials, the materials of the first main connection structure and the second main connection structure are both metal tungsten, and the materials of the first electrode layer and the second electrode layer are the same and are both selected from one of aluminum, copper, or aluminum-copper alloy.

[0020] In some embodiments, the three-dimensional memory further includes: a metal structure formed on the surface of the second dielectric layer and in one-to-one contact with the second main connection structure, wherein the metal structure is made of the same material as the second electrode layer and different from the material of the second main connection structure.

[0021] In some embodiments, the three-dimensional memory also includes: a first auxiliary connection structure, which is formed by the same process as the first main connection structure, the first auxiliary connection structure penetrates the first dielectric layer along the second direction, and is spaced apart from the first main connection structure in the first direction; a second auxiliary connection structure, which is formed by the same process as the second main connection structure, the second auxiliary connection structure penetrates the second dielectric layer along the second direction and contacts the first auxiliary connection structure; wherein one of the metal structures is also in contact with an adjacent second auxiliary connection structure.

[0022] The above technical solution optimizes the traditional horizontal storage unit into a vertical storage unit by optimizing the upper and lower electrode layers into left and right electrode layers, and increases the effective area of ​​a single storage unit, so that the area of ​​a single storage unit can be smaller, thereby saving the occupied area of ​​the storage unit; the increase in the effective area of ​​the device can improve the storage performance, optimize and improve the operation efficiency and reliability of the device. Moreover, the arrangement of the vertical storage unit makes it possible to form a first main connection structure when the first main connection structure in contact with the first electrode layer is formed, even if there is a protrusion in the first main connection structure, it will not affect the deposition and phase change performance of the storage layer, thereby avoiding affecting the performance of the storage unit; and when the second electrode layer is formed, there is no problem of etching through the storage layer, thereby further avoiding affecting the performance of the storage unit. Moreover, only two contact hole mask processes are required, saving one contact hole mask process, which can effectively reduce the production cost. The present invention solves the problem in the prior art that as the semiconductor process is miniaturized, the area of ​​the storage layer and the electrode layer of the storage unit becomes smaller, resulting in a reduction in the effective area of ​​the storage layer and the electrode layer, thereby affecting the storage performance of the memory, and saves the mask process, which can effectively reduce the production cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments of the present invention are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0024] Figure 1 It is a schematic diagram of the device structure of a memory in the prior art; Figure 2 A schematic diagram of the steps of a method for preparing a three-dimensional memory according to an embodiment of the present invention; Figure 3~Figure 6 A schematic diagram of a device structure of a semiconductor substrate provided by an embodiment of the present invention; Figure 7~Figure 10 A schematic diagram of a device structure for forming a storage layer and a second electrode layer according to an embodiment of the present invention; Fig.11 A schematic diagram of a device structure for forming a second dielectric layer according to an embodiment of the present invention; Figure 12~Figure 13 A schematic diagram of a device structure for forming a second main connection structure according to an embodiment of the present invention; Fig.14 FIG. 1 is a schematic diagram of a device structure for forming a metal structure according to an embodiment of the present invention. DETAILED DESCRIPTION

[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0026] See also Figure 1 , which is a schematic diagram of the device structure of a memory in the prior art. Figure 1 As shown, the existing memory includes: a supporting layer 10, a first dielectric layer 111 formed on the supporting layer 10, a first connecting structure 121 formed in the first dielectric layer 111, a second dielectric layer 112 formed on the first dielectric layer 111, a first conductive structure 131 formed in the second dielectric layer 112 and in contact with the first connecting structure 121, a second connecting structure 122 formed in the second dielectric layer 112 and in contact with the first conductive structure 131, a storage unit 14 formed on the second dielectric layer 112 and in contact with the second connecting structure 122, a third dielectric layer 113 covering the second dielectric layer 112 and covering the storage unit 14, a third connecting structure 123 formed in the third dielectric layer 113 and in contact with the storage unit 14, and a second conductive structure 132 formed on the surface of the third dielectric layer 113 and in contact with the third connecting structure 123. The storage unit 14 is composed of a lower electrode layer, a middle storage layer and an upper electrode layer. The support layer 10 can be a substrate, the first dielectric layer 111, the second dielectric layer 112, and the third dielectric layer 113 can be corresponding dielectric layers, and the first conductive structure 131 and the second conductive structure 132 can be corresponding metal structures.

[0027] The storage performance of the memory cell 14 is proportional to the effective area of ​​the memory layer and the electrode layer. However, as the semiconductor process is miniaturized, the area of ​​the memory layer and the electrode layer is reduced, resulting in a reduction in the effective area of ​​the memory layer and the electrode layer, thereby affecting the storage performance of the memory. At the same time, when preparing the existing memory, the preparation of the first connection structure 121, the second connection structure 122, and the third connection structure 123 requires three photomask processes, resulting in an increase in production costs.

[0028] In order to solve the problem in the prior art that as the semiconductor process is miniaturized, the area of ​​the storage layer and the electrode layer of the storage unit becomes smaller, resulting in a reduction in the effective area of ​​the storage layer and the electrode layer, thereby affecting the storage performance of the memory, the present invention provides a three-dimensional (3D) structured three-dimensional memory and a preparation method thereof, which can save the occupied area of ​​the storage unit and increase the effective area of ​​the device, thereby improving the storage performance, optimizing and improving the operating efficiency and reliability of the device, and can save the mask process and reduce the production cost.

[0029] An embodiment of the present invention provides a method for preparing a three-dimensional memory.

[0030] Please also read Figure 2~Figure 14 ,in, Figure 2 A schematic diagram of the steps of a method for preparing a three-dimensional memory according to an embodiment of the present invention; Figure 3~Figure 6 A schematic diagram of a device structure of a semiconductor substrate provided by an embodiment of the present invention; Figure 7~Figure 10 A schematic diagram of a device structure for forming a storage layer and a second electrode layer according to an embodiment of the present invention; Fig.11 A schematic diagram of a device structure for forming a second dielectric layer according to an embodiment of the present invention; Figure 12~Figure 13 A schematic diagram of a device structure for forming a second main connection structure according to an embodiment of the present invention; Fig.14 FIG. 1 is a schematic diagram of a device structure for forming a metal structure according to an embodiment of the present invention.

[0031] like Figure 2 As shown, the preparation method of the three-dimensional memory described in this embodiment includes the following steps: S21, forming a semiconductor substrate, the semiconductor substrate includes a substrate, a first dielectric layer covering the surface of the substrate, a first main connection structure that penetrates the first dielectric layer along the second direction and is arranged at intervals along the first direction, and a first electrode layer formed on the surface of the first dielectric layer and in one-to-one contact with the first main connection structure; S22, forming a storage layer and a second electrode layer, the storage layer at least covers a side wall of the first electrode layer and has an extension extending to the surface of the first dielectric layer, the second electrode layer covers the storage layer, and the maximum thickness of the second electrode layer in the second direction is greater than the thickness of the first electrode layer, wherein the first electrode layer, the storage layer, and the second electrode layer constitute a storage unit of the three-dimensional memory; S23, forming a second dielectric layer, the second dielectric layer covers the first dielectric layer and all the storage units; and S24, forming a second main connection structure, the second main connection structure penetrates the second dielectric layer along the second direction and is in contact with the second electrode layer.

[0032] Please refer to step S21 and Figure 6, forming a semiconductor substrate, the semiconductor substrate includes a substrate 30, a first dielectric layer 31 covering the surface of the substrate 30, first main connection structures 321 penetrating the first dielectric layer 31 along the second direction D2 and arranged at intervals along the first direction D1, and a first electrode layer 33 formed on the surface of the first dielectric layer 31 and in one-to-one contact with the first main connection structures 321. The first direction D1 is parallel to the surface of the substrate 30, and the second direction D2 is perpendicular to the surface of the substrate 30.

[0033] In this embodiment, the material of the first electrode layer 33 is different from the material of the first main connection structure 321 .

[0034] In this embodiment, the step of forming a semiconductor substrate specifically includes: (1) providing a substrate 30, wherein the first dielectric layer 31 is formed on the surface of the substrate 30, and the first dielectric layer 31 is formed with first contact holes 320 that penetrate the first dielectric layer 31 along the second direction D2 and are arranged at intervals along the first direction D1, such as Figure 3 (2) Filling the first contact hole 320 with a first metal material to form the first main connection structure 321, as shown in FIG. Figure 4 (3) Depositing and patterning a second metal material to form the first electrode layer 33 on the surface of the first dielectric layer 31 and in one-to-one contact with the first main connection structure 321, as shown in FIG. Figure 6 Specifically, the second metal material is different from the first metal material.

[0035] In this embodiment, the step of depositing and patterning the second metal material specifically includes: (31) depositing a second metal material layer 330 on the surface of the first dielectric layer 31, and forming a patterned first protective layer 38 on the surface of the second metal material layer 330, such as Figure 5 As shown; (32) using the patterned first protective layer 38 as a mask and the first dielectric layer 31 as an etching stop layer, etching the second metal material layer 330 to form the first electrode layer 33 in one-to-one contact with the first main connection structure 321, and the first protective layer 38 is retained and covers the surface of the first electrode layer 33, as shown Figure 6 The second metal material layer 330 can be deposited and grown by atomic layer deposition (Atomic Layer Deposition, ALD for short).

[0036] In this embodiment, the material of the first dielectric layer 31 may be an oxide (OX) material, such as silicon oxide (SiO). The material of the first main connection structure 321 may be metal tungsten; the material of the first electrode layer 33 is selected from one of aluminum, copper, or aluminum-copper alloy, preferably aluminum-copper alloy. Among them, aluminum-copper alloy is relatively hard, generally composed of 97% aluminum and 3% copper. Aluminum-copper alloy has similar chemical properties to metal aluminum, is light and has high tensile strength, and can replace expensive copper wire. The material of the first protective layer 38 may be nitride oxide, such as silicon oxynitride (SiON).

[0037] In this embodiment, a gate structure 39 is further formed on the surface of the substrate 30, the first dielectric layer 31 further covers the gate structure 39, and the first main connection structure 321 is arranged on both sides of the gate structure 39 along the first direction D1. The gate structure 39 includes a polysilicon gate 391, a gate oxide layer 392 located below the polysilicon gate 391, and a sidewall 393 located on the sidewall of the polysilicon gate 391. Figure 3 shown.

[0038] In this embodiment, the top surface of the first main connection structure 321 is flush with the top surface of the first dielectric layer 31 .

[0039] In this embodiment, the first electrode layer 33 is in one-to-one contact with the first main connection structure 321 , and a plurality of first electrode layers 33 are disposed on the surface of the first dielectric layer 31 at intervals.

[0040] Please refer to step S22 and Fig.10 , forming a storage layer 41 and a second electrode layer 42, the storage layer 41 at least covers one side wall of the first electrode layer 33 and has an extension portion 411 extending to the surface of the first dielectric layer 31; the second electrode layer 42 covers the storage layer 41, and the maximum thickness H2 of the second electrode layer 42 in the second direction D2 is greater than the thickness H1 of the first electrode layer 33; wherein the first electrode layer 33, the storage layer 41, and the second electrode layer 42 constitute a storage unit of the three-dimensional memory.

[0041] In this embodiment, the steps of forming the storage layer 41 and the second electrode layer 42 specifically include: (1) depositing a storage material to form a storage material layer 410 covering the first dielectric layer 31 and all of the first electrode layer 33, such as Figure 7 (2) depositing a second metal material to form a second electrode material layer 420 covering the storage material layer 410, wherein the maximum thickness H2 of the second electrode material layer 420 in the second direction D2 is greater than the thickness H1 of the first electrode layer 33; Figure 8(3) A patterned second protective layer 43 is formed on the surface of the second electrode material layer 420, and the patterned second protective layer 43 can at least shield a side wall of the first electrode layer 33 and a portion of the first dielectric layer 31 corresponding to the side wall, as shown in FIG. Fig. 9 (4) Using the patterned second protective layer 43 as a mask and the first dielectric layer 31 as an etching stop layer, the second electrode material layer 420 and the storage material layer 410 are etched, the remaining storage material layer 410 is etched to form the storage layer 41, and the remaining second electrode material layer 420 is etched to form the second electrode layer 42, and the second protective layer 43 is retained and covers the surface of the second electrode layer 42, as shown in FIG. Fig.10 shown.

[0042] In this embodiment, the patterned second protective layer 43 can also shield the corresponding area of ​​the top surface of the first electrode layer 33; the storage layer 41 also covers the top surface of the first electrode layer 33; and the second electrode layer 42 completely covers the storage layer 41. Specifically, when the first electrode layer 33 has the first protective layer 38 on the top surface, the storage layer 41 completely covers the top surface of the first protective layer 38 located on the top surface of the first electrode layer 33.

[0043] In some embodiments, the storage material layer 410 may be deposited and grown by maskless atomic layer deposition (ALD). The material of the storage layer 41 is a ferroelectric material or a phase change material. The material of the second protection layer 43 may be nitride oxide, such as silicon oxynitride (SiON).

[0044] In this embodiment, the second electrode layer 42 and the first electrode layer 33 are arranged in pairs, and together with the intermediate storage layer 41, form a vertical storage unit (along the direction D2 shown in the figure), which can save the occupied area of ​​the storage unit and increase the effective area of ​​the device. The arrangement of the vertical storage unit in this embodiment makes it possible to avoid the problem of etching through the storage layer when forming the second main connection structure 361 (upper contact hole process), thereby further avoiding affecting the performance of the storage unit. And compared with Figure 1 In the conventional method, there are three dielectric layers and three contact hole (VIA) mask processes. In this embodiment, only two dielectric layers and two contact hole (VIA) mask processes are required, thereby saving one contact hole mask process and effectively reducing production costs.

[0045] In this embodiment, a plurality of storage units are formed and distributed at intervals, and adjacent storage units are separated by a second dielectric layer 35 formed subsequently.

[0046] Please refer to step S23 and Fig.11, forming a second dielectric layer 35, wherein the second dielectric layer 35 covers the first dielectric layer 31 and all the storage units.

[0047] The material of the second dielectric layer 35 may be the same as that of the first dielectric layer 31 , both of which are oxide (OX) materials, for example, both are silicon oxide (SiO).

[0048] Please refer to step S24 and Fig.13 , forming a second main connection structure 361 , wherein the second main connection structure 361 penetrates the second dielectric layer 35 along the second direction D2 and contacts the second electrode layer 42 .

[0049] In this embodiment, the material of the second main connection structure 361 can be the same as that of the first main connection structure 321 , such as metal tungsten. The material of the second main connection structure 361 is different from that of the first electrode layer 33 and the second electrode layer 42 .

[0050] In this embodiment, the top surface of the second main connection structure 361 is flush with the top surface of the second dielectric layer 35. The orthographic projection of the second main connection structure 361 on the first dielectric layer 31 is within the range of the orthographic projection of the extension portion 411 on the first dielectric layer 31.

[0051] In this embodiment, the step of forming the second dielectric layer 35 includes: forming an etching stop layer 50, wherein the etching stop layer 50 covers the first dielectric layer 31 and all the storage layer units, and the second dielectric layer 35 covers the etching stop layer 50. Accordingly, the step of forming the second main connection structure 361 specifically includes: (1) using the etching stop layer 50 as an etching stop layer, etching in the second dielectric layer 35 to form a second contact hole 350 exposing the second electrode layer 42, such as Fig.12 (2) depositing a first metal material and planarizing it to form the second main connection structure 361 in the second contact hole 350, as shown in FIG. Fig.13 shown.

[0052] like Fig.14 As shown, in this embodiment, the step of forming the second main connection structure 361 includes: depositing a second metal material and patterning it to form a metal structure 37 in one-to-one contact with the second main connection structure 361 on the surface of the second dielectric layer 35. The metal structure 37 is made of the same material as the first electrode layer 33 and is different from the material of the second main connection structure 361. The metal structure 37 serves as a lead-out structure or a pad.

[0053] In this embodiment, a first auxiliary connection structure 322 is formed while forming the first main connection structure 321. The first auxiliary connection structure 322 penetrates the first dielectric layer 31 along the second direction D2 and is spaced apart from the first main connection structure 321 in the first direction D1. A second auxiliary connection structure 362 is formed while forming the second main connection structure 361. The second auxiliary connection structure 362 penetrates the second dielectric layer 35 along the second direction D2 and contacts the first auxiliary connection structure 322. One of the metal structures 37 is also in contact with the adjacent second auxiliary connection structure 362, such as Fig.14 shown.

[0054] The memory cell of the three-dimensional memory prepared in this embodiment optimizes the upper and lower electrode layers into left and right electrode layers to realize the transformation of the traditional lateral memory cell (Cell) (such as Figure 1 The storage unit 14 shown in the figure is optimized as a longitudinal storage unit (along the direction D2 shown in the figure). The effective area of ​​a single storage unit is increased, and a smaller area (Footprint) of a single storage unit can be achieved to save the occupied area of ​​the storage unit. The increase in the effective area of ​​the device can improve the storage performance and optimize the operation efficiency and reliability of the device. In addition, the arrangement of the longitudinal storage unit in this embodiment makes it possible to form a first main connection structure 321 (lower contact hole process) when forming the first main connection structure 321 (lower contact hole process). Even if the lower contact hole process causes a protrusion in the first main connection structure 321 in contact with the first electrode layer 33 (left electrode layer shown in the figure), it will not affect the deposition and phase change performance of the storage layer 41, thereby avoiding affecting the performance of the storage unit. And when the second main connection structure 361 (upper contact hole process) is formed, there is no problem of etching through the storage layer 41, thereby further avoiding affecting the performance of the storage unit. And compared to Figure 1 In the conventional method, there are three dielectric layers and three contact holes (VIA) mask processes. This embodiment only requires two dielectric layers and two contact holes (VIA) mask processes, saving one contact hole mask process, which can effectively reduce production costs. This embodiment solves the problem in the prior art that as the semiconductor process shrinks, the area of ​​the storage layer and the electrode layer of the storage unit becomes smaller, resulting in a reduction in the effective area of ​​the storage layer and the electrode layer, thereby affecting the storage performance of the memory, and saves the mask process, which can effectively reduce production costs.

[0055] Based on the same inventive concept, the present invention also provides a three-dimensional memory prepared by the above method of the present invention.

[0056] See also Figure 3~Figure 14The three-dimensional memory of this embodiment includes: a substrate 30, a first dielectric layer 31, a first main connection structure 321, a first electrode layer 33, a storage layer 41, a second electrode layer 42, a second dielectric layer 35 and a second main connection structure 361. The first electrode layer 33, the storage layer 41 and the second electrode layer 42 constitute a storage unit of the three-dimensional memory.

[0057] In this embodiment, the first main connection structure 321 and the second main connection structure 361 are made of a first metal material, the first electrode layer 33 and the second electrode layer 42 are made of a second metal material, and the first metal material is different from the second metal material.

[0058] Specifically, the first dielectric layer 31 covers the surface of the substrate 30. The material of the first dielectric layer 31 may be an oxide (OX) material, such as silicon oxide (SiO).

[0059] Specifically, the first main connection structures 321 penetrate the first dielectric layer 31 along the second direction D2 and are arranged at intervals along the first direction D1. The first direction D1 is parallel to the surface of the substrate 30, and the second direction D2 is perpendicular to the surface of the substrate 30. The material of the first main connection structure 321 is metal tungsten. The top surface of the first main connection structure 321 is flush with the top surface of the first dielectric layer 31.

[0060] Specifically, the first electrode layer 33 is formed on the surface of the first dielectric layer 31 and is in one-to-one contact with the first main connection structure 321. A plurality of first electrode layers 33 are arranged at intervals on the surface of the first dielectric layer 31. The material of the first electrode layer 33 is selected from one of aluminum, copper, or aluminum-copper alloy, preferably aluminum-copper alloy.

[0061] Specifically, the storage layer 41 covers a side wall of the first electrode layer 33 and has an extension portion 411 extending to the surface of the first dielectric layer 31. The storage layer 41 also covers the top surface of the first electrode layer 33. Specifically, the storage layer 41 includes an extension portion 411 extending to the surface of the first dielectric layer 31, a first covering portion 412 covering a side wall of the first electrode layer 33, and a second covering portion 413 covering the top surface of the first electrode layer 33, as shown in FIG. Fig.10 The material of the storage layer 41 is a ferroelectric material or a phase change material.

[0062] Specifically, the second electrode layer 42 covers the storage layer 41, and the maximum thickness H2 of the second electrode layer 42 in the second direction D2 is greater than the thickness H1 of the first electrode layer 33. Specifically, the second electrode layer 42 completely covers the storage layer 41. The first electrode layer 33, the storage layer 41, and the second electrode layer 42 are arranged along the first direction D1 to form a longitudinal storage unit of the three-dimensional memory. The material of the second electrode layer 42 is selected from one of aluminum, copper, or aluminum-copper alloy, preferably aluminum-copper alloy.

[0063] Specifically, the second dielectric layer 35 covers the first dielectric layer 31 and all the storage units. The material of the second dielectric layer 35 can be the same as that of the first dielectric layer 31, both of which are oxide (OX) materials, such as silicon oxide (SiO).

[0064] Specifically, the second main connection structure 361 penetrates the second dielectric layer 35 along the second direction D2 and contacts the second electrode layer 42. The material of the second main connection structure 361 may be metal tungsten.

[0065] In this embodiment, the top surface of the second main connection structure 361 is flush with the top surface of the second dielectric layer 35. The orthographic projection of the second main connection structure 361 on the first dielectric layer 31 is within the range of the orthographic projection of the extension portion 411 on the first dielectric layer 31.

[0066] In this embodiment, a gate structure 39 is further formed on the surface of the substrate 30, the first dielectric layer 31 further covers the gate structure 39, and the first main connection structure 321 is disposed along the first direction D1 on both sides of the gate structure 39. The gate structure 39 includes a polysilicon gate 391, a gate oxide layer 392 located below the polysilicon gate 391, and a sidewall 393 located on the sidewall of the polysilicon gate 391.

[0067] In this embodiment, the material of the storage layer 41 is a ferroelectric material or a phase change material; the materials of the first dielectric layer 31 and the second dielectric layer 35 are both oxide materials; the material of the first main connection structure 321 and the second main connection structure 361 is metal tungsten; the material of the first electrode layer 33 and the second electrode layer 42 is the same, and both are selected from one of aluminum, copper, or aluminum-copper alloy, preferably aluminum-copper alloy.

[0068] In this embodiment, the three-dimensional memory further includes: a first protective layer 38 covering the surface of the first electrode layer 33; and a second protective layer 43 covering the surface of the second electrode layer 42. The materials of the first protective layer 38 and the second protective layer 43 can be nitride oxide, such as silicon oxynitride (SiON).

[0069] In this embodiment, the three-dimensional memory further includes: a metal structure 37; the metal structure 37 is formed on the surface of the second dielectric layer 35 and is in one-to-one contact with the second main connection structure 361. The metal structure 37 serves as a lead-out structure or a pad. The metal structure 37 is made of the same material as the first electrode layer 33, and is different from the material of the second main connection structure 361.

[0070] In this embodiment, the three-dimensional memory further includes: a first auxiliary connection structure 322, the first auxiliary connection structure 322 and the first main connection structure 321 are formed by the same process, the first auxiliary connection structure 322 penetrates the first dielectric layer 31 along the second direction D2, and is spaced apart from the first main connection structure 321 in the first direction D1. A second auxiliary connection structure 362, the second auxiliary connection structure 362 and the second main connection structure 361 are formed by the same process, the second auxiliary connection structure 362 penetrates the second dielectric layer 35 along the second direction D2 and contacts the first auxiliary connection structure 322. One of the metal structures 37 is also in contact with the adjacent second auxiliary connection structure 362, such as Fig.14 shown.

[0071] In the above description, the description of well-known components and technologies is omitted to avoid unnecessary confusion of the concept of the present invention. In the above embodiments, each embodiment focuses on the differences from other embodiments, and the same / similar parts between the embodiments can be referred to each other.

[0072] It should be noted that, in this article, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply that there is any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that the process, method, article or equipment including a series of elements not only include those elements, but also include other elements not clearly listed, or also include elements inherent to such process, method, article or equipment. In the absence of more restrictions, there is a sentence "also includes a ..." The elements limited do not exclude the existence of other identical elements in the process, method, article or equipment including the elements. In addition, the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict.

[0073] The above description is only a preferred embodiment of the present invention and is not intended to limit the protection scope of the present invention. It should be noted that a person skilled in the art may make several improvements and modifications without departing from the principle of the present invention, and these improvements and modifications shall also be regarded as the protection scope of the present invention.

Claims

1. A method for preparing a three-dimensional memory, It is characterized in that The method comprises the following steps: forming a semiconductor substrate, the semiconductor substrate comprising a substrate, a first dielectric layer covering the surface of the substrate, a first main connection structure penetrating the first dielectric layer along a second direction and arranged at intervals along the first direction, and a first electrode layer formed on the surface of the first dielectric layer and in one-to-one contact with the first main connection structure, wherein the first direction is parallel to the substrate surface, and the second direction is perpendicular to the substrate surface; forming a storage layer and a second electrode layer, wherein the storage layer at least covers a side wall of the first electrode layer and has an extension extending to the surface of the first dielectric layer, the second electrode layer covers the storage layer, and the maximum thickness of the second electrode layer in the second direction is greater than the thickness of the first electrode layer, wherein the first electrode layer, the storage layer, and the second electrode layer constitute storage units of the three-dimensional memory; forming a second dielectric layer, wherein the second dielectric layer covers the first dielectric layer and all the storage units; and forming a second main connection structure, wherein the second main connection structure penetrates the second dielectric layer along the second direction and is in contact with the second electrode layer.

2. The method according to claim 1, It is characterized in that The first main connection structure and the second main connection structure are made of a first metal material, the first electrode layer and the second electrode layer are made of a second metal material, and the first metal material is different from the second metal material.

3. The method according to claim 1, It is characterized in that The material of the storage layer is ferroelectric material or phase change material, the materials of the first dielectric layer and the second dielectric layer are both oxide materials, the materials of the first main connection structure and the second main connection structure are both metal tungsten, and the materials of the first electrode layer and the second electrode layer are the same and are both selected from one of aluminum, copper, or aluminum-copper alloy.

4. The method according to claim 1, It is characterized in that The steps of forming a semiconductor substrate specifically include: providing a substrate, the first dielectric layer being formed on the surface of the substrate, the first dielectric layer having first contact holes formed in the first dielectric layer and penetrating the first dielectric layer along the second direction and arranged at intervals along the first direction; filling the first contact hole with a first metal material to form the first main connection structure; depositing a second metal material and patterning it to form the first electrode layer on the surface of the first dielectric layer, which is in one-to-one contact with the first main connection structure.

5. The method according to claim 4, It is characterized in that The steps of depositing and patterning the second metal material specifically include: depositing a second metal material layer on the surface of the first dielectric layer; forming a patterned first protective layer on the surface of the second metal material layer; etching the second metal material layer using the patterned first protective layer as a mask and the first dielectric layer as an etching stop layer to form the first electrode layer that is in one-to-one contact with the first main connection structure, and the first protective layer is retained and covers the surface of the first electrode layer.

6. The method according to claim 1, It is characterized in that The steps of forming the storage layer and the second electrode layer specifically include: depositing a storage material to form a storage material layer covering the first dielectric layer and all the first electrode layers; depositing a second metal material to form a second electrode material layer covering the storage material layer, wherein the maximum thickness of the second electrode material layer in the second direction is greater than the thickness of the first electrode layer; forming a patterned second protective layer on the surface of the second electrode material layer, wherein the patterned second protective layer can at least shield a side wall of the first electrode layer and a portion of the first dielectric layer corresponding to the side wall; etching the second electrode material layer and the storage material layer using the patterned second protective layer as a mask and the first dielectric layer as an etching stop layer, etching the remaining storage material layer to form the storage layer, etching the remaining second electrode material layer to form the second electrode layer, and retaining and covering the surface of the second electrode layer.

7. The method according to claim 6, It is characterized in that The patterned second protection layer can also shield the corresponding area of ​​the top surface of the first electrode layer; the storage layer also covers the top surface of the first electrode layer, and the second electrode layer completely covers the storage layer.

8. The method according to claim 1, It is characterized in that The step of forming the second dielectric layer includes: forming an etching barrier layer, the etching barrier layer covers the first dielectric layer and all the storage units, and the second dielectric layer covers the etching barrier layer; the step of forming the second main connection structure specifically includes: using the etching barrier layer as an etching stop layer, etching in the second dielectric layer to form a second contact hole exposing the second electrode layer; depositing a first metal material and planarizing it to form the second main connection structure in the second contact hole.

9. The method according to claim 1, It is characterized in that The top surface of the second main connection structure is flush with the top surface of the second dielectric layer; the orthographic projection of the second main connection structure on the first dielectric layer is located within the range of the orthographic projection of the extension portion on the first dielectric layer.

10. The method according to claim 1, It is characterized in that The step of forming the second main connection structure includes: depositing a second metal material and patterning it to form a metal structure on the surface of the second dielectric layer that is in one-to-one contact with the second main connection structure.

11. The method according to claim 10, It is characterized in that The first main connection structure and the second main connection structure are made of a first metal material, the first electrode layer, the second electrode layer and the metal structure are made of a second metal material, and the first metal material is different from the second metal material.

12. The method according to claim 10, It is characterized in that A first auxiliary connection structure is formed while the first main connection structure is formed, the first auxiliary connection structure penetrates the first dielectric layer along the second direction and is spaced apart from the first main connection structure; a second auxiliary connection structure is formed while the second main connection structure is formed, the second auxiliary connection structure penetrates the second dielectric layer along the second direction and is in contact with the first auxiliary connection structure; wherein one of the metal structures is also in contact with an adjacent second auxiliary connection structure.

13. A three-dimensional memory, It is characterized in that include: substrate; A first dielectric layer, covering the surface of the substrate; A first main connection structure penetrates the first dielectric layer along a second direction and is arranged at intervals along the first direction, wherein the first direction is parallel to the substrate surface and the second direction is perpendicular to the substrate surface; a first electrode layer is formed on the surface of the first dielectric layer and is in one-to-one contact with the first main connection structure; a storage layer covers at least one side wall of the first electrode layer and has an extension extending to the surface of the first dielectric layer; a second electrode layer covers the storage layer, and the maximum thickness of the second electrode layer in the second direction is greater than the thickness of the first electrode layer, wherein the first electrode layer, the storage layer, and the second electrode layer constitute storage units of the three-dimensional memory; a second dielectric layer covers the first dielectric layer and all the storage units; and a second main connection structure penetrates the second dielectric layer along the second direction and is in contact with the second electrode layer.

14. The three-dimensional memory according to claim 13, It is characterized in that The first main connection structure and the second main connection structure are made of a first metal material, the first electrode layer and the second electrode layer are made of a second metal material, and the first metal material is different from the second metal material.

15. The three-dimensional memory according to claim 13, It is characterized in that The material of the storage layer is ferroelectric material or phase change material, the materials of the first dielectric layer and the second dielectric layer are both oxide materials, the materials of the first main connection structure and the second main connection structure are both metal tungsten, and the materials of the first electrode layer and the second electrode layer are the same and are both selected from one of aluminum, copper, or aluminum-copper alloy.

16. The three-dimensional memory according to claim 13, It is characterized in that Also includes: A metal structure is formed on the surface of the second dielectric layer and is in one-to-one contact with the second main connection structure. The metal structure is made of the same material as the second electrode layer and different from the material of the second main connection structure.

17. The three-dimensional memory according to claim 16, It is characterized in that Also includes: a first auxiliary connection structure, formed by the same process as the first main connection structure, the first auxiliary connection structure penetrating the first dielectric layer along the second direction and spaced apart from the first main connection structure in the first direction; a second auxiliary connection structure, formed by the same process as the second main connection structure, the second auxiliary connection structure penetrating the second dielectric layer along the second direction and contacting the first auxiliary connection structure; One of the metal structures is also in contact with the adjacent second auxiliary connection structure.

Citation Information

Patent Citations

  • Phase change memory structure containing sandwich-type electrodes and producing method thereof

    CN103427022A

  • Resistive random access memory

    CN111430537A

  • Ferroelectric memory and manufacturing method

    JP1998056149A