Bullet train coupler fatigue crack ultrasonic detection test block and detection method thereof
By designing a multi-functional ultrasonic detection test block for fatigue cracks of EMU couplings, the problems of difficulty in carrying the test blocks and low detection accuracy in the prior art are solved, and zero deviation adjustment, refractive angle measurement and sensitivity adjustment are achieved, and detection is improved. The accuracy and consistency of the results avoid misjudgment of circumferential fatigue cracks at the right angle position of the coupling annular belt near the top.
Patent Information
- Application Number
- CN202410963696.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-18
- Publication Date
- 2024-11-26
AI Technical Summary
In the prior art, the fatigue crack detection of the annular belt of the EMU coupling near the top of the top has the problem that the test block is not easy to carry and the detection accuracy is low. The non-machining method makes the test block groove depth difficult to measure, which affects the detection results. Consistency and accuracy.
An ultrasonic detection test block for fatigue cracks of EMU coupling is designed, including a probe test adjustment area and a detection simulation area. The probe test adjustment area is used to measure the zero deviation and refractive angle of the detection equipment, and the detection simulation area is used to train detectors to confirm cracks. The reflected wave position and waveform enable multi-function debugging and simulation detection of the test block through arc surfaces, test grooves, transverse holes, tooth root reflectors and detection grooves.
It provides zero deviation adjustment, probe front edge length and refractive angle testing functions of ultrasonic flaw detectors, ensures consistency of flaw detection sensitivity, reduces the risk of misjudgment, improves the accuracy and consistency of detection results, and avoids the coupling annular belt belt Misjudgment of circumferential fatigue cracks on the right angle position on the top side.
Smart Images

Figure CN119023818A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of detection equipment, and in particular to an ultrasonic detection test block for fatigue cracks of a motor vehicle coupling and a detection method thereof. Background Art
[0002] There is a ring belt with a wall thickness of 5.35mm and a width of 5mm between the inner teeth and the top of the EMU coupling. After long-term use of the coupling, the right-angle position of the ring belt near the top is prone to circumferential fatigue cracks. This area is small and inside the coupling. Without disassembling the coupling, magnetic particle inspection, penetrant inspection, and radiographic inspection cannot detect fatigue cracks in this area. Ultrasonic inspection is generally used.
[0003] In the prior art, a comparison test block for ultrasonic flaw detection is made at a right angle to the top side of the annular belt, using non-mechanical processing methods such as laser and electric spark. The advantage is that the shape and surface state of the test block are completely consistent with the coupling, but the disadvantage is that a coupling needs to be lost, and the price of the coupling is relatively high, resulting in an increase in production costs. In addition, when non-mechanical processing methods are used for grooving, the groove depths of different test blocks are difficult to effectively measure, resulting in poor consistency between the test blocks.
[0004] When performing ultrasonic flaw detection on the coupling, it is also necessary to debug the ultrasonic flaw detector, such as testing the front length and refraction angle of the probe, testing the system zero bias, and debugging the sensitivity. In the prior art, such debugging relies on the CSK-IA test block. Therefore, two test blocks are required for crack detection on the annular belt of the coupling in the prior art. Since the test blocks are heavy, they are not easy to carry.
[0005] In addition, for the defect judgment during ultrasonic testing at the right angle position of the top side of the coupling annular belt, the existing technology generally adopts the method of comparing the defect wave height with the artificial groove wave height of the physical comparison test block. The depth of the artificial groove affects the detection sensitivity, and the depth of the groove is a matter of opinion. The crack wave judgment is affected, and there is a situation where the detection result is not accurate. In addition, there is no existing technical support for whether the echo that appears at the depth position of the non-artificial groove is judged as a crack wave, which is easy to misjudge. Therefore, there is an urgent need for an ultrasonic test block for fatigue cracks of a motor vehicle coupling and a detection method thereof to solve the problem that when two test blocks are used for coupling crack flaw detection in the existing technology, the test blocks are not easy to carry and the accuracy of the flaw detection results is low. Summary of the invention
[0006] The object of the present invention is to provide a test block for ultrasonic detection of fatigue cracks in a motor vehicle coupling and a detection method thereof, so as to solve the problems raised in the above-mentioned background technology.
[0007] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a test block for fatigue crack ultrasonic detection of a motor vehicle coupling, comprising a test block body, the test block body comprising a probe test adjustment area and a detection simulation area; the probe test adjustment area comprises an arc surface, a test groove and a transverse hole, wherein the arc surface is used to measure the zero bias of the detection equipment, the incident point and the front length of the detection probe; the test groove is used to measure the refraction angle of the probe; the transverse hole is used to adjust the flaw detection sensitivity of the detection equipment; the detection simulation area comprises a tooth root reflector, a tooth root reflector groove and a detection groove, wherein the shape of the tooth root reflector is adapted to the shape of the component where the crack occurs, and is used to simulate the fixed wave of the tooth root reflector; the tooth root reflector groove is used to train detection personnel to confirm the probe position when the fixed wave at the tooth root is the maximum reflected wave; the detection groove is used to train detection personnel to confirm the position and waveform of the fatigue crack reflection wave and the position of the fixed wave of the tooth root reflector.
[0008] Preferably, the arc surface is convex upward along the end of the test block body to form a quarter sector arc surface, and the arc radius is 20 mm.
[0009] Preferably, a probe detection surface is provided on the side of the test block body away from the arc surface, and the probe detection surface is connected to the horizontal edge of the fan-shaped arc surface; the groove directions of the test groove, the tooth root reflector groove and the detection groove are all perpendicular to the probe detection surface, and the groove depths are all 1±0.1mm.
[0010] Preferably, the length of the test groove is 40 mm, and the horizontal distance between the groove position of the test groove and the end of the arc surface is 20 mm.
[0011] Preferably, the opening diameter of the transverse hole is Φ2mm, and the transverse hole and the detection groove are arranged parallel to the same side, the opening length of the transverse hole and the groove length of the detection groove are both 20mm, and the horizontal distance between the opening center of the transverse hole and the end of the arc surface is 35mm.
[0012] Preferably, the tooth root reflector is recessed inward along the block to form a groove with a groove wall perpendicular to the groove top, which is used to simulate a right-angle component structure at 90° where the crack occurs. The bottom of the groove of the tooth root reflector is parallel to the detection surface of the probe, and the vertical distance between the two is 5mm. The tooth root reflector is 30mm long, 20mm wide, and 10mm thick. The opposite side of the groove of the tooth root reflector is provided with a detection groove.
[0013] Preferably, a tooth root reflector groove is provided on the extension line of the tooth root reflector, which is used to train the inspection personnel to confirm the probe position when the maximum reflected wave at a right angle formed by the inner tooth root and the inner wall of the shell appears. The groove length of the tooth root reflector groove is 20mm, and the groove direction of the tooth root reflector groove is on the same straight line as the direction of the tooth root reflector, and the distance between the two is 20mm.
[0014] Preferably, the starting point of the test groove, the center of the transverse hole, the tooth root reflector, the tooth root reflector groove and the starting point of the detection groove are respectively located in the same plane, all the grooves and transverse holes are perpendicular to the end face of the test block, and the horizontal distance between the tooth root reflector groove and the detection groove is 5mm; the block of the test block body located on the detection groove side is provided with an arc chamfer, and the radius of the chamfer is 1-45mm.
[0015] The present invention also provides a method for ultrasonic testing using a motor vehicle coupling fatigue crack ultrasonic testing block, comprising the following steps: S1. Select a digital ultrasonic flaw detector, choose a dual-crystal shear wave probe with a frequency of 4-5MHz, a refraction angle of K0.7-K0.8, and a front length of less than or equal to 10mm, and connect the probe to the ultrasonic flaw detector with a probe cable; use the curved surface and test grooves of the test block to adjust the zero bias of the ultrasonic flaw detector, and measure the probe front length and the probe refraction angle; after completing the measurement of the instrument zero bias, probe front length and refraction angle, use the horizontal hole of the test block to adjust the instrument ultrasonic detection sensitivity to complete the instrument and probe debugging before the test; S2. After the instrument and probe are debugged before the test, the probe is used to simulate the flaw detection of the test block's test simulation area and the detection echo is recorded; the detection echo includes the tooth root reflector groove echo and the simulated crack echo; S3. Use the debugged flaw detector and probe to inspect the coupling to be inspected; during the inspection process, when the inspection echo matches the groove echo of the tooth root reflector, it is confirmed that the inspection position is located at the location where the crack of the coupling occurs; when the inspection echo matches the simulated crack echo, the crack defect is determined.
[0016] As a preferred embodiment, when adjusting the zero bias of the ultrasonic flaw detector, measuring the front length of the probe and the refraction angle of the probe in S1, the probe is moved to find the maximum echo of the arc surface to adjust the zero bias of the instrument so that the sound path of the arc surface is displayed as 20 mm. At this time, a ruler is used to measure the distance X1 from the front end of the probe to the edge of the test block body, and the front length of the shear wave probe X2 = 20-X1, that is, the instrument zero bias and the front length X2 test of the probe are completed; and when measuring the refraction angle of the probe, the probe is moved to the test groove, and the maximum reflected wave of the test groove is found, and a ruler is used to measure the length X3 between the end of the arc surface and the front end of the probe, and the refraction angle of the probe is calculated using the probe refraction angle formula β = tg-1 ((X3+X2-20) / Y), and the refraction angle is entered into the instrument parameter column; wherein Y is the vertical distance between the test groove and the probe detection surface; When adjusting the ultrasonic detection sensitivity of the instrument, move the probe to the position where the probe detection surface corresponds to the horizontal hole, find the maximum reflected wave of the horizontal hole, adjust its amplitude to 80% of the full height of the instrument and then set the gain to 20dB, which is used as the ultrasonic detection sensitivity of fatigue cracks of the EMU coupling; When the probe is used to simulate flaw detection on the detection simulation area of the test block in S2, the probe is used to perform root reflector groove detection exercises on the detection simulation area of the test block to confirm the position of the probe when the maximum reflection wave of the tooth root appears. After completion, further detection exercises are performed on the detection groove to confirm the detection groove reflection wave position and waveform and non-crack fixed wave position; during actual detection, the echo confirmed as a crack must meet any one of the following two conditions: (1) The horizontal position of the reflection wave is located at the detection groove position, the display depth is consistent with the detection groove echo display depth, the reflection wave amplitude is greater than or equal to 40% of the full height of the instrument and there is no other echo before the groove echo depth; (2) Echoes appear at other positions with a smaller echo depth than the detection groove, the echo amplitude at the detection groove depth position reaches 80% or more, and the maximum amplitude of the echo at the detection groove depth position is 20 dB or more higher than the maximum amplitude of the echo at other positions.
[0017] Beneficial effects: 1. The test block provided by the present invention has the zero bias adjustment of the ultrasonic flaw detector, the front length of the probe, the refraction angle test function and the flaw detection sensitivity adjustment function of the ultrasonic flaw detector, and the flaw detection sensitivity between the test blocks of the same model is consistent.
[0018] 2. The test block provided by the present invention is provided with a tooth root reflector simulating that the root of the inner tooth of the coupling forms a 90° right angle with the top inner wall, a tooth root reflector groove for training testers to confirm that the root of the inner tooth of the coupling forms a 90° right angle with the top inner wall, and a test groove for simulating the occurrence of circumferential fatigue cracks at a right angle position on the top side of the annular belt of the coupling, so as to provide basic training conditions for flaw detectors.
[0019] 3. The use of the test block provided by the present invention can eliminate the error in identifying the tooth root reflector during the refraction angle test of the short focal length, dual crystal, and shear wave probe. For the refraction angle test of the oblique probe with a refraction angle of less than 60°, the prior art uses a Φ50mm reflector test at a burial depth of 70mm on the CSK-IA test block. It is found that when the dual crystal oblique probe with a frequency of 4-5MHz, a refraction angle of K0.7-K0.8, and a focal length of 10mm is placed in the specified position, 3 echoes will appear on the instrument screen at the same time. If the operator sets the gate of the ultrasonic flaw detector too wide, the instrument will read the highest wave signal according to its own logic, which will increase the shear wave refraction angle test result by about 9°. If the detection system is set according to this refraction angle, the crack depth and horizontal position at the right angle position of the top side of the coupling annular belt will deviate, which will affect the defect judgment and cause the risk of misjudgment. When using the test block and detection method provided by the present invention, when the shear wave probe refraction angle is tested using the test groove, there is only a single reflected wave on the instrument screen, and the risk of using the prior art test will not occur.
[0020] 4. The defect confirmation method provided by the present invention can avoid the risk of misjudgment of circumferential fatigue cracks in ultrasonic testing at the right angle between the inner cylindrical surface and the top of the coupling. The present invention's approach to defect judgment is: "During actual testing, the echo confirmed as a crack must meet any one of the following two conditions: (1) The horizontal position of the reflected wave is located at the detection groove position, the displayed depth is consistent with the detection groove echo display depth, the reflected wave amplitude is greater than or equal to 40% of the full height of the instrument, and there is no other echo before the groove echo depth; (2) Echoes appear at other positions that are smaller than the detection groove echo depth, the echo amplitude at the detection groove depth position reaches 80% or more, and the maximum amplitude of the echo at the detection groove depth position is 20dB or more higher than the maximum amplitude of the echo at other positions." This can effectively avoid the misjudgment of crack defects by inspectors due to knife marks or other unexpected factors generated during the manufacturing process of the coupling. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 This is a schematic diagram of the structure of the test block for fatigue cracks of a motor vehicle coupling according to the present embodiment; Figure 2 It is a top view of the test block for fatigue crack ultrasonic detection of the motor vehicle coupling of this embodiment. DETAILED DESCRIPTION
[0022] The technical solution of the present invention is described in detail below with reference to the accompanying drawings, but the protection scope of the present invention is not limited to the embodiments.
[0023] Example: Figure 1-Figure 2As shown: This embodiment provides a fatigue crack ultrasonic detection test block for a motor vehicle coupling, including a test block body, which includes a probe test adjustment area and a detection simulation area; the probe test adjustment area includes an arc surface, a test groove A and a transverse hole B, wherein the arc surface is used to measure the zero bias of the detection equipment, the incident point of the detection probe and the front length; the test groove A is used to measure the refraction angle of the probe; the transverse hole B is used to adjust the flaw detection sensitivity of the detection equipment; the detection simulation area includes a tooth root reflector C1, a tooth root reflector groove C2 and a detection groove D, wherein the shape of the tooth root reflector C1 is adapted to the shape of the component where the crack occurs, and is used to simulate the tooth root reflector fixed wave; the tooth root reflector groove C2 is used to train detection personnel to confirm the probe position when the fixed wave at the tooth root is the maximum reflected wave; the detection groove D is used to train detection personnel to confirm the fatigue crack reflection wave position and waveform and the tooth root reflector fixed wave position.
[0024] The arc surface of this embodiment is convex upward along the end of the test block body to form a quarter sector arc surface, and the arc radius is 20 mm.
[0025] In this embodiment, a probe detection surface E is provided on the block body on one side away from the arc surface, and the probe detection surface is connected to the horizontal side of the sector arc surface; the groove directions of the test groove, the tooth root reflector groove and the test groove are all perpendicular to the probe detection surface, and the groove depth is 1±0.1mm. The groove length of the test groove A is 40mm, and the horizontal distance between the groove position of the test groove and the end of the arc surface is 20mm.
[0026] In addition, the opening diameter of the transverse hole B in this embodiment is Φ2mm, and the transverse hole B is arranged parallel to the detection groove D on the same side, the opening length of the transverse hole and the opening length of the detection groove are both 20mm, and the horizontal distance between the opening center of the transverse hole and the end of the arc surface is 35mm. The tooth root reflector C1 is concave inward along the block to form a groove with a groove wall perpendicular to the groove top, which is used to simulate the right-angle component structure of 90° at the crack occurrence site. The groove bottom of the tooth root reflector C1 is parallel to the probe detection surface E, and the vertical distance between the two is 5mm. The tooth root reflector C1 is 30mm long, 20mm wide, and 10mm thick; the opposite side of the groove of the tooth root reflector C1 is provided with a detection groove D.
[0027] Furthermore, a tooth root reflector groove C2 is provided on the extended line of the tooth root reflector C1, which is used to train the inspection personnel to confirm the probe position when the maximum reflected wave at a right angle formed by the inner tooth root and the inner wall of the shell appears. The groove length of the tooth root reflector groove C2 is 20 mm, and the groove direction of the tooth root reflector groove C2 is on the same straight line as the direction of the tooth root reflector C1, and the distance between the two is 20 mm.
[0028] At the same time, the starting point of the test groove A of this embodiment, the center of the hole B, the tooth root reflector C1, the tooth root reflector groove C2 and the starting point of the detection groove D are respectively located in the same plane, all the grooves and the directions of the transverse holes are perpendicular to the end face of the test block, and the horizontal distance between the tooth root reflector groove C2 and the detection groove D is 5mm; the block of the test block body located on the detection groove side is provided with an arc chamfer, and the radius of the chamfer is 1-45mm.
[0029] The detection method of the EMU coupling fatigue crack ultrasonic detection test block of this embodiment is carried out according to the following steps: S1. First, select a digital ultrasonic flaw detector, a dual crystal shear wave probe with a frequency of 4-5MHz, a refraction angle of K0.7-K0.8, and a front length of less than or equal to 10mm, and connect the probe to the ultrasonic flaw detector with a probe line; when debugging the ultrasonic flaw detector, apply coupling agent to the probe detection surface of the test block, place the probe in the position corresponding to the arc surface, and then move the probe. When the maximum echo of the R20 arc surface is found, the zero bias of the flaw detector can be adjusted to make the arc surface sound path display 20mm. At this time, use a ruler to measure the distance X1 from the front end of the probe to the edge of the end of the arc surface, and the front length X2 of the shear wave probe = 20-X1, that is, the instrument zero bias and probe front length X2 test are completed.
[0030] S10. Then measure the refraction angle of the probe. Move the probe to find the maximum reflected wave of the test groove A which is 20mm horizontally away from the end of the arc surface. Use a ruler to measure the distance X3 between the front end of the probe and the test groove A. Use the probe refraction angle formula β=tg-1((X3+X2-20) / Y)to calculate the refraction angle of the probe, and enter the refraction angle into the instrument parameter column to complete the measurement of the instrument refraction angle. Where Y is the vertical distance between the test groove and the probe detection surface.
[0031] S11. Then move the flaw detector probe toward the horizontal hole to find the maximum reflected wave of the horizontal hole B, and adjust its amplitude to 80% of the full height of the flaw detector and then increase the gain by 20 dB as the ultrasonic detection sensitivity of fatigue cracks of the EMU coupling to complete the instrument and probe debugging before the test; S2. After the instrument and probe debugging before the test is completed, the probe is used to perform the tooth root reflector groove C2 test exercise on the test simulation area of the test block to confirm the position of the probe when the maximum reflection wave of the tooth root appears. After completion, further test the test groove D to confirm the position and waveform of the test groove reflection wave and the non-crack fixed wave position. During the actual test, the echo confirmed as a crack must meet any one of the following two conditions: (1) The horizontal position of the reflection wave is located at the test groove position, the display depth is consistent with the display depth of the test groove echo, the reflection wave amplitude is greater than or equal to 40% of the full height of the instrument, and there is no other echo before the groove echo depth; (2) Echoes appear at other positions with a smaller echo depth than the test groove, the echo amplitude at the test groove depth position reaches 80% or more, and the maximum amplitude of the echo at the test groove depth position is 20dB or more higher than the maximum amplitude of the echo at other positions.
[0032] S3. Use the debugged flaw detector and probe to inspect the coupling to be inspected; when it is confirmed that a defect needs to be measured during the inspection process, keep the probe direction unchanged under the flaw detection sensitivity, and move the probe along one side of the circumferential direction. When the defect wave amplitude is equal to the noise wave amplitude, the probe width center is one end point of the defect indication length. Then, move the probe in the opposite circumferential direction to find the other end point of the defect. The arc length between the two end points is the defect indication length. In addition, during the flaw detection scanning of the coupling, it should be ensured that the maximum echo amplitude of the tooth root in the entire circle of the coupling is basically consistent to avoid defect omission due to reduced flaw detection sensitivity.
[0033] Working principle: The ultrasonic test block for fatigue crack detection of the EMU coupling of the present invention adopts R20 arc surface and 1mm deep groove calibration detection system to prevent the misjudgment of reflected wave when the refraction angle of short focal length dual crystal oblique probe is tested by the existing technology; Ф2×20 transverse hole is used to adjust the flaw detection sensitivity to ensure the consistency of flaw detection sensitivity adjustment between test blocks of the same model; a 90° tooth root reflector groove C2 formed by the inner tooth root and the inner wall of the shell is made for training test personnel to confirm, so that the flaw detection personnel can clearly know the front end position of the probe when the reflected wave appears; a 1×20mm detection groove D is made to simulate the circumferential fatigue crack at the right angle between the inner circular surface and the top, so that the flaw detection personnel can clearly know the position and waveform of the groove reflection wave and the non-crack fixed wave position; and the detection method provided stipulates the judgment method of the defect wave to prevent misjudgment.
[0034] As above, although the present invention has been shown and described with reference to specific preferred embodiments, it should not be construed as limiting the present invention itself. Various changes may be made to it in form and detail without departing from the spirit and scope of the present invention as defined in the appended claims.
Claims
1. A test block for fatigue cracks of a motor vehicle coupling, comprising a test block body, characterized in that: The test block body includes a probe test adjustment area and a detection simulation area; the probe test adjustment area includes an arc surface, a test groove and a transverse hole, wherein the arc surface is used to measure the zero bias of the detection equipment, the incident point and the front length of the detection probe; the test groove is used to measure the refraction angle of the probe; the transverse hole is used to adjust the flaw detection sensitivity of the detection equipment; the detection simulation area includes a tooth root reflector, a tooth root reflector groove and a detection groove, wherein the shape of the tooth root reflector is adapted to the shape of the component where the crack occurs, and is used to simulate the fixed wave of the tooth root reflector; the tooth root reflector groove is used to train detection personnel to confirm the probe position when the fixed wave at the tooth root is the maximum reflected wave; the detection groove is used to train detection personnel to confirm the position and waveform of the fatigue crack reflection wave and the position of the fixed wave of the tooth root reflector.
2. The ultrasonic testing block for fatigue cracks of a motor vehicle coupling according to claim 1 is characterized in that: The arc surface is convex upward along the end of the test block body to form a quarter sector arc surface, and the arc radius is 20 mm.
3. The ultrasonic testing block for fatigue cracks of a motor vehicle coupling according to claim 1 is characterized in that: A probe detection surface is provided on the side of the test block body away from the arc surface, and the probe detection surface is connected to the horizontal edge of the fan-shaped arc surface; the groove directions of the test groove, the tooth root reflector groove and the detection groove are all perpendicular to the probe detection surface, and the groove depths are all 1±0.1mm.
4. The ultrasonic testing block for fatigue cracks of a motor vehicle coupling according to claim 2 is characterized in that: The length of the test groove is 40 mm, and the horizontal distance between the groove position of the test groove and the end of the arc surface is 20 mm.
5. The ultrasonic testing block for fatigue cracks of a motor vehicle coupling according to claim 2 is characterized in that: The opening diameter of the transverse hole is Φ2mm, and the transverse hole and the detection groove are arranged parallel to the same side, the opening length of the transverse hole and the groove length of the detection groove are both 20mm, and the horizontal distance between the opening center of the transverse hole and the end of the arc surface is 35mm.
6. The ultrasonic testing block for fatigue cracks of a motor vehicle coupling according to claim 3 is characterized in that: The tooth root reflector is recessed inward along the block to form a groove with a groove wall perpendicular to the groove top, which is used to simulate a right-angle component structure with a 90° angle at the crack occurrence site. The groove bottom of the tooth root reflector is parallel to the probe detection surface, and the vertical distance between the two is 5mm. The tooth root reflector is 30mm long, 20mm wide, and 10mm thick. The detection groove is provided on the opposite side of the tooth root reflector groove.
7. The ultrasonic testing block for fatigue cracks of a motor vehicle coupling according to claim 3 is characterized in that: A tooth root reflector groove is provided on the extension line of the tooth root reflector, which is used to train detection personnel to confirm the probe position when the maximum reflected wave at a right angle formed by the inner tooth root and the inner wall of the shell appears. The groove length of the tooth root reflector groove is 20mm, and the groove direction of the tooth root reflector groove is on the same straight line as the direction of the tooth root reflector, and the distance between the two is 20mm.
8. The ultrasonic testing block for fatigue cracks of a motor vehicle coupling according to claim 6 is characterized in that: The starting point of the test groove, the center of the transverse hole, the tooth root reflector, the tooth root reflector groove and the starting point of the detection groove are respectively located in the same plane, all the grooves and transverse holes are perpendicular to the end face of the test block, and the horizontal distance between the tooth root reflector groove and the detection groove is 5mm; the block of the test block body located on the detection groove side is provided with an arc chamfer, and the arc radius of the chamfer is 1-45mm.
9. The ultrasonic detection method of a motor vehicle coupling fatigue crack ultrasonic detection test block according to any one of claims 1 to 8, characterized in that: The detection steps include: S1. Select a digital ultrasonic flaw detector, choose a dual-crystal shear wave probe with a frequency of 4-5MHz, a refraction angle of K0.7-K0.8, and a front length of less than or equal to 10mm, and connect the probe to the ultrasonic flaw detector with a probe cable; use the curved surface and test grooves of the test block to adjust the zero bias of the ultrasonic flaw detector, and measure the probe front length and the probe refraction angle; after completing the measurement of the instrument zero bias, probe front length and refraction angle, use the horizontal hole of the test block to adjust the instrument ultrasonic detection sensitivity to complete the instrument and probe debugging before the test; S2. After the instrument and probe are debugged before the test, the probe is used to simulate the flaw detection of the detection simulation area of the test block, and the detection echo is recorded; wherein the detection echo includes the tooth root reflector groove echo and the simulated crack echo; S3. Use the debugged flaw detector and probe to inspect the coupling to be inspected; during the inspection process, when the inspection echo matches the groove echo of the tooth root reflector, it is confirmed that the inspection position is located at the location where the crack of the coupling occurs; when the inspection echo matches the simulated crack echo, the crack defect is determined.
10. The ultrasonic testing method for a fatigue crack ultrasonic testing block of a motor vehicle coupling according to claim 9 is characterized in that: When adjusting the zero bias of the ultrasonic flaw detector, measuring the front length of the probe and the refraction angle of the probe in S1, move the probe to find the maximum echo of the arc surface to adjust the zero bias of the instrument so that the sound path of the arc surface is displayed as 20mm. At this time, use a ruler to measure the distance X1 from the front end of the probe to the edge of the test block body, and the front length of the shear wave probe X2 = 20-X1, that is, the instrument zero bias and probe front length X2 tests are completed; and when measuring the refraction angle of the probe, move the probe to the test groove, and then find the maximum reflected wave of the test groove, and use a ruler to measure the length X3 between the end of the arc surface and the front end of the probe, and use the probe refraction angle formula β = tg-1 ((X3+X2-20) / Y) to calculate the refraction angle of the probe, and enter the refraction angle into the instrument parameter column; where Y is the vertical distance between the test groove and the probe detection surface; When adjusting the sensitivity of ultrasonic testing of the instrument, move the probe to the position where the probe testing surface corresponds to the horizontal hole, find the maximum reflected wave of the horizontal hole, adjust its amplitude to 80% of the full height of the instrument and then set the gain to 20dB, which is used as the ultrasonic testing sensitivity of fatigue cracks of the EMU coupling; When the probe is used to simulate flaw detection on the detection simulation area of the test block in S2, the probe is used to perform root reflector groove detection exercises on the detection simulation area of the test block to confirm the position of the probe when the maximum reflection wave of the tooth root appears. After completion, further detection exercises are performed on the detection groove to confirm the detection groove reflection wave position and waveform and non-crack fixed wave position; during actual detection, the echo confirmed as a crack must meet any one of the following two conditions: (1) The horizontal position of the reflection wave is located at the detection groove position, the display depth is consistent with the detection groove echo display depth, the reflection wave amplitude is greater than or equal to 40% of the full height of the instrument and there is no other echo before the groove echo depth; (2) Echoes appear at other positions with a smaller echo depth than the detection groove, the echo amplitude at the detection groove depth position reaches 80% or more, and the maximum amplitude of the echo at the detection groove depth position is 20 dB or more higher than the maximum amplitude of the echo at other positions.