Gravity activated display including patterned microcell array

By designing a gravity-driven display suitable for banknotes, using micro-unit arrays and translucent sealing layers, the problem of unsuitable size and construction in the prior art is solved, and a thin, soft and power-free safety mark is realized for banknotes. Anti-counterfeiting verification.

CN119032015APending Publication Date: 2024-11-26E INK CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202380033300.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2022-05-04
Filing Date
2023-04-28
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing gravity-driven dynamic safety devices lack detailed descriptions in their construction and manufacturing, and their size is not suitable for incorporation into paper money and cannot be effectively used in anti-counterfeiting measures.

Method used

A gravity-driven display suitable for bonding into banknotes is designed, using a micro-unit array containing a mixture of reflective particles and hydrocarbon solvents with a density greater than 7 g/cm2 and sealed by a translucent sealing layer, using micro-imprint or The photolithography method can generate verification signals by gravity driving without the need for power.

Benefits of technology

A very thin and soft safety mark is achieved, able to remain strong under harsh conditions, suitable for anti-counterfeiting verification of items such as banknotes, and increases safety and reliability due to the power-free design.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119032015A_ABST
    Figure CN119032015A_ABST
Patent Text Reader

Abstract

The gravity-driven display system is suitable for use as a security mark, for example, incorporated into banknotes. The device can be made very thin and soft, but sufficiently strong, to withstand harsh conditions of banknotes in general circulation. Because the displays are gravity driven, they do not require power or circuitry. Gravity driven displays may be fabricated using microimprint or photolithography, and may be filled and sealed using roll-to-roll technology. The microcells may also be patterned to provide a customized design, such as an official seal.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Related Applications

[0002] This application claims priority to U.S. Provisional Patent Application No. 63 / 338,156, filed on May 4, 2022. The entire contents of any patent, published application, or other published work cited herein are incorporated herein by reference.

[0003] background

[0004] Contemporary banknotes include many technical features to make it difficult for criminals to copy the currency. Although this feature significantly increases the cost of the printing process, it also deters counterfeiters and increases public confidence in the notes that will be exchanged for value. Banknotes in many countries include features such as intaglio printing, watermarks, transparent windows, security ribbons, and micro-printing. Depending on the value of the banknote, more expensive features such as holograms and RFID circuits may be justified to prevent illegal copying. Of course, this security feature is also useful in the verification of other items such as documents, artworks, clothing, sports memorabilia, historical documents, and software packaging.

[0005] One feature considered a high-tech authenticity mark is a so-called gravity-driven dynamic security device. This device can be driven by the user, i.e., the holder of the bill, by simply flipping the device, which then generates some verification signals. The verification signature can be optical or auditory, and because the device is gravity-driven, no additional power source is required. U.S. Patent No. 10,921,579 ("579 Patent") describes many optical devices that can be used for a gravity-driven dynamic security device, which includes Janus particles, differential density particles (heavy and buoyant), differential density fluids, and rolling balls in a capsule. The '579 patent does not provide detailed details about the construction of this device, but describes the final product and possible benefits. For example, the sedimentation display example of the '579 patent suggests that dense particles are included in a colored fluid, and these dense particles are included in one or more containers. However, the nature of the container, the method of making such a container, and the method of filling such a container with a sedimentation mixture are not provided. In addition, the final size of the security device described in the '579 patent is not suitable for incorporation into, for example, banknotes.

[0006] Overview

[0007] Improved gravity-driven dynamic security devices are described herein, such as gravity-driven dynamic security devices suitable for incorporation into banknotes. In one aspect, the gravity-driven display includes an array of microcells, each microcell having walls, a bottom, and a top opening, wherein the bottom of each microcell is light-transmissive; a first mixture comprising reflective particles having a density greater than 7 grams per cubic centimeter, a hydrocarbon solvent, and a first soluble dye, wherein the first mixture is disposed in at least some of the microcells in the array; and a light-transmissive sealing layer that seals the first mixture in at least some of the microcells. In one embodiment, the gravity-driven display further includes a first light-transmissive substrate coupled to the array of microcells. In one embodiment, the gravity-driven display further includes a second light-transmissive substrate coupled to the light-transmissive sealing layer. In one embodiment, the gravity-driven display does not include any light-transmissive substrate having a conductivity greater than 1×10 4 Ohm cm layer. In one embodiment, the gravity-driven display is less than 1 mm thick. In one embodiment, the gravity-driven display is less than 200 μm thick. In one embodiment, the gravity-driven display further comprises a second mixture comprising reflective particles, a hydrocarbon solvent, and a second soluble dye, wherein the second mixture is disposed in at least some microcells, and the at least some microcells are different from at least some microcells in which the first mixture is disposed. In one embodiment, the first and second soluble dyes are of different colors. In one embodiment, the reflective particles include silver, tungsten, gold, platinum, nickel, copper, tin, zinc, or indium. In one embodiment, the longest dimension of the reflective particles is 5 μm to 25 μm. In one embodiment, the reflective particles are metal flakes or metal whiskers. In one embodiment, the first soluble dye comprises anthraquinone, phthalocyanine, naphthalene, indole, imidazole, or thioindigo compounds. In one embodiment, the hydrocarbon solvent comprises aliphatic molecules having a molecular weight of 100 g / mol to 300 g / mol. In one embodiment, the microcell walls and bottoms comprise acrylates, vinyl ethers, or epoxides. In one embodiment, the sealing layer comprises polyvinyl alcohol, polyvinyl pyrrolidone, polyurethane, polyisobutylene or acrylate. In one embodiment, the first mixture further comprises a surfactant. In one embodiment, the first mixture comprises 5-15% of a surfactant (surfactant weight / mixture weight), 20-50% of reflective particles (particle weight / mixture weight) and 1-8% of a soluble dye (soluble dye weight / mixture weight), the balance being a hydrocarbon solvent.

[0008] In another aspect, a gravity-driven display includes an array of microcells, each microcell having walls, a bottom, and a top opening, wherein the bottom of each microcell is light-transmissive; a first mixture comprising reflective particles having a density less than 0.5 g / cm3, a hydrocarbon solvent, and a first soluble dye, wherein the first mixture is disposed in at least some of the microcells in the array, and a light-transmissive sealing layer that seals the first mixture in at least some of the microcells. In one embodiment, the reflective particles include silicon dioxide, zirconium oxide, or aluminum oxide. In one embodiment, the gravity-driven display does not include any particles having a conductivity greater than 1×10 4 Ohm cm layer.

[0009] In another aspect, a magnetic gravity driven display comprises an array of microcells, each microcell having a wall, a bottom, and a top opening, wherein the bottom of each microcell is light transmissive, a first mixture comprising magnetic particles having a density greater than 4 g / cm3, a hydrocarbon solvent, and a first soluble dye, wherein the first mixture is disposed in at least some of the microcells in the array, and a light transmissive sealing layer that seals the first mixture in at least some of the microcells. In one embodiment, the magnetic particles comprise nickel, iron, manganese, or oxides thereof. In one embodiment, the magnetic gravity driven display does not include any material having a conductivity greater than 1×10 4 Ohm cm layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1A The diagram illustrates a cross-sectional side view of a gravity-driven display in a first stable state, wherein a high density of reflective particles have settled to the bottom of a plurality of microlocations, thereby allowing an observer to observe the color of a hydrocarbon solvent containing a compatible dye from above.

[0012] Figure 1B Illustration Description Flip Figure 1A The instant effect of the gravity-driven display.

[0013] Figure 1C The diagram illustrates an intermediate state of high density reflective particles as they settle from the top surface to the bottom surface due to the differential density of the reflective particles compared to the hydrocarbon solvent.

[0014] Figure 1D The diagram illustrates a gravity-driven display in a second stable state, wherein the high density of reflective particles has settled back to the bottom of the plurality of microcells, wherein Figure 1D The bottom surface corresponds to Figure 1A top surface.

[0015] Figure 2The diagram illustrates a cross-sectional side view of an alternative embodiment in which some of the microlocations contain a first mixture containing a first dye, some of the microlocations are empty, and some of the microlocations contain a second mixture containing a second dye.

[0016] Figure 3 An exemplary top view of a gravity-driven display is illustrated in which some microcells contain a first mixture containing a first dye, some microcells are empty, and some microcells contain a second mixture containing a second dye.

[0017] Figure 4 A method of manufacturing a microcell for use in the present invention using a roll-to-roll method is shown.

[0018] Figure 5A and 5B DETAILED DESCRIPTION Microcells of a gravity-driven display system are fabricated using photolithographic exposure through a photomask coated with a conductor film of a thermosetting precursor.

[0019] Figure 5C and 5D An alternative embodiment is described in detail in which microcells for a gravity-driven display are fabricated using photolithography. Figure 5C and 5D In the embodiment, a combination of top and bottom exposure is used, allowing the walls in one lateral direction to be cured by exposure through the top photomask, and the walls in the other lateral direction to be cured by bottom exposure through the light-transmitting substrate.

[0020] Figures 6A-6D Illustrated are the steps for filling and sealing a microcell array to be used in a gravity-driven display.

[0021] Figure 7 is a microscopic image of a layer of microcells filled with a mixture comprising a blue dye. The cells are sealed with a light-transmitting sealing layer comprising polyisobutylene.

[0022] Figures 8A-8D An alternative embodiment of a gravity driven display is illustrated, which includes a cover film having a base color and a logo cutout. When the base color is matched to the color of a hydrocarbon solvent containing a compatible dye, the logo is invisible in a default state ( Figure 8B ). However, when the device is turned over, the high-density reflective particles are allowed to settle on the cover side, and when the device is turned over a second time, the logo will briefly "appear" because the high-density reflective particles have moved to the surface adjacent to the cover film ( Figure 8C ). Over time, the high-density reflective particles will return to their initial positions and the logo will disappear ( Fig.8D ).

[0023] describe

[0024] Improved gravity-driven display systems are described herein that are suitable for use as security markings, such as for incorporation into banknotes. Gravity-driven display devices can be made very thin and flexible, but strong enough to withstand the harsh conditions of banknotes in general circulation. Because the displays are gravity-driven, they do not require power or circuitry. Gravity-driven displays can be manufactured using micro-embossing or photolithography, and can be filled and sealed using roll-to-roll technology. Microcells can also be patterned to provide customized designs, such as official seals.

[0025] The term "filled" in relation to a microcell (or multiple microcells) means that the mixture is present in the microcell (or multiple microcells). This does not necessarily mean that the entire volume of the microcell is occupied by the formulation. In other words, the term "filled" in relation to a microcell (or multiple microcells) includes the concept of a partially filled microcell (or multiple microcells) as well as a completely "filled" microcell (or multiple microcells). Similarly, filling a microcell (or multiple microcells) means adding the formulation to the microcell (or multiple microcells). This does not necessarily mean that a sufficient amount of the formulation is added to the microcell to occupy its entire volume. For example, a microcell may be "filled" with a mixture, but leaving a small amount of volume compared to the microcell, so that a sealing layer occupies a small portion of the microcell, for example, as Figure 1A shown.

[0026] Figures 1A-1D An overview of a gravity-driven display 10 is shown. The display comprises a plurality of microcells 11, each of which comprises a wall 12 and a bottom 13. The microcells 11 may be arranged in a square, honeycomb, circular, etc. The microcells are typically micro-embossed from a thermosetting material, however, as described below, they may also be produced by photolithography. Figures 1A-1D In the gravity-driven display 10, each microcell 11 is filled with a mixture containing a dyed hydrocarbon solvent 14 and high-density reflective particles 15. The hydrocarbon solvent can be a branched or straight-chain hydrocarbon, or a combination thereof. For example, the hydrocarbon solvent contains aliphatic molecules with a molecular weight of 100 g / mol to 300 g / mol. Suitable hydrocarbon solvents include Series (Exxon Mobil) and octane, nonane, decane and dodecane, which can be purchased from chemical suppliers such as Sigma Aldrich. Generally, the density of the reflective particles is greater than 7 grams per cubic centimeter, for example, greater than 8 grams per cubic centimeter, for example, greater than 10 grams per cubic centimeter, and the longest dimension is 5 μm to 25 μm, for example, the longest dimension is 10 μm to 20 μm. The reflective particles can be metal flakes or metal whiskers, such as silver powder D1 (Ames Goldsmith, South Glens Falls, NY) or precipitated silver flakes (Sigma Aldrich, Milwaukee, WI). Other high-density reflective materials such as tungsten, gold, platinum, nickel, copper, tin, zinc or indium can also be used. High-density alloys such as brass and bronze can also be used. Flake brass and bronze can be purchased from Wieland Chase (Montpelier, Ohio) or process suppliers such as Advanced Metallics (https: / / www.advancedmetallics.com / ). In some cases, a dispersant or surfactant may be added to the mixture to reduce agglomeration between the metal flakes. For example, the hydrocarbon mixture may additionally contain Surfactant (Lubrizol, Corp., Wickliffe, OH) or Surfactant (Sigma Aldrich). Other dispersants can be chemically adsorbed onto the surface of the metal, such as the surface of a charged species, i.e., polyvinyl pyrrolidone. In some embodiments, the metal particles / flakes are coated with compatible molecules that help the metal particles / flakes remain distributed, such as polyvinyl alcohol, polyurethane, fatty acids.

[0027] The light-transmitting sealing layer 16 can be composed of, for example, polyvinyl alcohol, polyvinyl pyrrolidone, polyurethane, polyisobutylene, acrylate, polyethylene, polyurethane, polycaprolactone or polysiloxane. Although the gravity-driven display 10 can be implemented with only filled microcells 11 and a light-transmitting sealing layer 16, the gravity-driven display generally also includes a first light-transmitting substrate 17 and a second light-transmitting substrate 18. The light-transmitting substrates 17 and 18 can be composed of any suitable light-transmitting film, but films with excellent sealing properties such as polyethylene, for example polyethylene terephthalate (PET) are preferred. Other suitable light-transmitting substrates may include films made of acrylate, methacrylate, polyvinyl pyrrolidone or polystyrene. Although in Figures 1A-1D It is not shown, but the gravity-driven display 10 may include an additional optically clear adhesive layer between the light-transmitting substrates 17, 18 and the microcells 11 and / or the light-transmitting sealing layer.

[0028] The total thickness of the gravity-driven display 10 can be 1 mm or thinner, such as 800 μm or thinner, such as 500 μm or thinner, such as 250 μm or thinner. For example, the thickness of the gravity-driven display 10 can be 100 μm to 1 mm, such as 200 μm to 800 μm, such as 300 μm to 600 μm. Because the gravity-driven display 10 is so thin, the gravity-driven display 10 is very soft and can be used like a ribbon to be incorporated into, for example, security documents and banknotes. When integrated into security documents and banknotes, this thin structure does not reduce appearance or performance. In addition, because the gravity-driven display 10 is so thin, when the gravity-driven display 10 is integrated into a security document or banknote, the user may not be able to feel any changes in texture. In some cases, the gravity-driven display 10 may be held in place by other structures, which may include adhesives, wires, tapes, staples, or the gravity-driven display 10 may be pressed between protective transparent layers that extend outwardly along the edges of the gravity-driven display 10. Suitable protective (barrier) layers include polyvinyl films, polyethylene films such as PET, polyimide films, and polyacrylate films. It is also possible that the gravity-driven display 10 may be secured directly to a security document or other object using an adhesive layer that may contain, for example, polyisobutylene, acrylic acid, polyethylene glycol, or silicone.

[0029] In from Figures 1A to 1D The function of the gravity-driven display 10 is illustrated in the transition of Figures 1A to 1D In all figures in , gravity (G) is toward the bottom of the page. Figure 1A As shown, the gravity-driven display starts in a stable display state. Figure 1A As shown, an observer viewing from above will see the color of the dyed hydrocarbon solvent 14 because all of the intermediate layers are light transmissive. To drive the display, the user will flip the gravity-driven display 10, as shown in FIG. Figure 1B As shown, the observer will then briefly see the color of the high-density reflective particles 15 that are present on the (now) top viewing surface. In other words, because both the light-transmitting sealing layer 16 and the light-transmitting substrate 18 are light-transmitting, the user sees light reflected from the high-density reflective particles 15. Figure 1C As shown, shortly after the gravity-driven display 10 is flipped over, the high-density reflective particles 15 will begin to settle under the action of gravity and move toward the (now) bottom of the gravity-driven display 10. Over time, the high-density reflective particles 15 will settle onto the (now) bottom substrate 17, and the user will see the color of the dyed hydrocarbon solvent 14, which is consistent with the color of the dyed hydrocarbon solvent 14. Figure 1AThe initial view in FIG. 1 is very similar, if not identical. For the avoidance of doubt, it is not necessary to include a conductive layer, such as a metal foil, carbon paste, a conductive ceramic such as ITO, or a layer having a thickness greater than 1×10 4 Some other layer with an electrical conductivity of ohm-cm. However, a gravity-driven display 10 that includes one or more conductive layers can be prepared. In some embodiments, the gravity-driven display 10 can include high-density reflective particles 15 that are charged and move in a sufficient electric field, or are magnetic and can be driven by a magnetic field, or some combination of electric charge, magnetic charge, and gravity drive. Suitable magnetic, ferromagnetic, or antiferromagnetic particles can include high-density reflective particles 15 that include nickel, iron, iron oxide, manganese oxide, or lanthanum manganese oxide, and such particles can be doped with charge carriers or other materials to increase or decrease the magnetic or ferromagnetic response.

[0030] The amount of time between flipping the gravity-driven display 10 and the high-density reflective particles 15 returning to the bottom can be modified by including a free polymer or rheology modifier in the dyed hydrocarbon solvent 14. In some embodiments, the time between flipping the gravity-driven display 10 and the high-density reflective particles 15 returning to the bottom will be greater than 0.5 seconds, such as greater than 1 second, such as greater than 2 seconds, such as greater than 3 seconds, such as greater than 4 seconds. In some embodiments, the time between flipping the gravity-driven display 10 and the high-density reflective particles 15 returning to the bottom will be less than 20 seconds, such as less than 15 seconds, such as less than 10 seconds, such as less than 5 seconds. For example, the time between flipping the gravity-driven display 10 and the high-density reflective particles 15 returning to the bottom can be 1-10 seconds, such as 2-8 seconds, such as 3-6 seconds. The viscosity of the dyed hydrocarbon solvent 14 may be greater than 0.8 cSt at 25°C, greater than 1.0 cSt at 25°C, greater than 1.2 cSt at 25°C, greater than 1.4 cSt at 25°C, greater than 1.6 cSt at 25°C.

[0031] like Figure 2As shown, the patterned gravity-driven display 30 may include one or more microcells 31A containing a first dyed hydrocarbon solvent 34A and one or more microcells 31B containing a second dyed hydrocarbon solvent 34B. The patterned gravity-driven display 30 may also include one or more empty microcells 31C, which are not gravity-switched. Alternatively, the empty microcells 31C may be filled with hydrocarbon solvents without high-density reflective particles 15. Filling the non-switching microcells 31C may help seal the surrounding microcells 31A / 31B with a light-transmitting sealing layer 16. Filling the non-switching microcells 31C may also facilitate index matching across the interface of the patterned gravity-driven display 20, for example, if the user needs to view through the patterned gravity-driven display 20, for example, to observe additional security markings. In some embodiments, the non-switching microcell 31C may also include a third dye or a first or second dye or some combination thereof. However, because there are no high-density reflective particles 15, the dyed hydrocarbon solvent is always visible in the non-switching microcell 31C.

[0032] Any dye that is soluble in a hydrocarbon solvent is suitable for incorporation into the gravity-driven display 10, including the patterned gravity-driven display 20. Such dyes may include anthraquinone, phthalocyanine, naphthalene, indole, imidazole, or thioindigo compounds. Suitable dyes include so-called solvent dyes, such as Solvent Blue 89HF, Solvent Green M HF, Solvent Violet RS HF, Solvent Red 175HF, and Solvent Red IK HF, all available from Abbey Color (Philadelphia, PA). Thus, the dyed hydrocarbon solvent used in the present invention may include red, orange, yellow, green, blue, indigo, or violet. The color saturation of the dyed hydrocarbon solvent will depend on the amount of dye added to the hydrocarbon solvent. Suitable saturation can be achieved with as little as 0.5% soluble dye (weight of dye / weight of hydrocarbon mixture including high-density reflective particles 15), however the dyed hydrocarbon mixture generally contains 1-8% soluble dye, for example 2-5% soluble dye. In some embodiments, the hydrocarbon mixture may additionally contain a surfactant, such as Surfactant (Lubrizol, Corp., Wickliffe, OH) or Surfactant (Sigma Aldrich). In some embodiments, the dyed hydrocarbon mixture comprises 5-15% surfactant (surfactant weight / mixture weight), 20-50% reflective particles (particle weight / mixture weight), and 1-8% soluble dye (soluble dye weight / mixture weight), with the balance being hydrocarbon solvent.

[0033] like Figure 3As shown, because certain microcells can be filled with a specific mixture of dyed hydrocarbon solvents, patterns can be produced in a patterned gravity-driven display 20. Using a slot coater with an adjustable feed channel, using only preferential microcell filling before sealing, various lines, shapes, logos, etc. can be produced in the microcell array, as discussed below. In other embodiments not shown in the figure, individual microcell segments can also be combined, wherein each individual segment is filled with a differently dyed hydrocarbon fluid to produce patterns in a gravity-driven display. Microcell arrays with different microcell widths or depths can also be used to produce patterns that can be used as additional indications of authenticity. For example, a microcell with a depth twice the depth of other microcells may take longer to return to a stable state after a gravity-driven display is flipped. Alternatively, a microcell with a depth half the depth of other microcells may not reach a saturated color state when in a stable state because the high-density reflective particles are partially visible when they are located at the bottom of the shallower microcells.

[0034] In another embodiment not shown in the figure, the high density reflective particles can be replaced by floating reflective particles, which rise to the surface when the gravity-driven display is flipped over. Figures 1A-1D In the case where the reflective particles are shown falling due to gravity, the reflective particles in this embodiment will rise to the viewing surface. Thus, the stable default color of the gravity driven display will generally be white or some other reflective color, and when the display is flipped over, the color of the dyed hydrocarbon solvent will be seen until the floating reflective particles rise to the viewing surface. (e.g., Figure 1B will represent the default state, and the instantaneous flipped state will be represented by Figure 1A ) Suitable buoyant reflective particles generally have a density of less than 0.5 g / cm3 and may include silica, zirconia, or alumina. Suitable buoyant particles may be obtained from Polysciences, Inc. (Warrington, PA).

[0035] exist Figures 8A-8DIn another embodiment illustrated, a gravity-driven display 10 or a patterned gravity-driven display 20 can be combined with a graphic cover 85 to produce a gravity-driven cover display 80, which hides a portion of the display from the observer. The graphic cover 85 is generally a thin film, which can be composed of a light-transmitting film such as PET, whereby a pattern such as a company logo or identification number is printed on the film, for example, by screen printing or inkjet printing. In other embodiments, the graphic cover 85 can be physically cut from a colored film to partially hide the gravity-driven display below from the observer. The desired pattern can be a positive film, which means that the pattern itself is printed on the film, or is made of a cut sheet adhered to the film. The desired pattern can be a negative film, which means that everything except the pattern is printed on the film, or the shape of the pattern is cut from the colored film. The printed portion or the cut colored film can be color-matched with the color of the reflective particles, or color-matched with a soluble dye. It should be understood that an optically transparent adhesive layer (not shown) will generally be used to bond the graphic cover 85 to the display below. In addition, despite Fig. 8A Only one graphic overlay 85 is shown, but the second graphic overlay ( Fig. 8A ) is applied to the bottom of the display, thereby allowing the gravity-driven cover display 80 to change appearance with each flip, which is simple and clear. In addition, the first and second graphic cover layers can include the same pattern or different patterns.

[0036] The gravity driven cover display 80 mechanism is Figures 8B to 8D Described in detail in Figures 8B to 8D is a top view of the device. Figure 8B As shown, a logo 90 ("LOGO") is printed as a negative on a graphic cover layer 85, which is made of a transparent film. The area around the logo 90 is color matched to match the dyed hydrocarbon solvent 14. As a result, when the gravity-driven cover display 80 is viewed from above, the logo 90 is not visible because the area around the logo 90 is the same color as the dyed hydrocarbon solvent. ( Figure 8B and 8D The logo 90 in the figure is shaded slightly darker for easier understanding. In actual practice, the logo 90 is virtually invisible to the untrained eye.) To verify the authenticity of the item to which the gravity-driven overlay display 80 is attached, the user will flip the gravity-driven overlay display 80, wait for a period of time, and then

[0037] Techniques for constructing microcells. Microcells can be formed in a batch process or in a continuous roll-to-roll process, as disclosed in U.S. Pat. No. 6,933,098. The latter provides a continuous, low-cost, high-throughput manufacturing technology for making compartments for use in a variety of applications including gravity-driven displays. Figure 4 As shown, micro-unit arrays suitable for use in the present invention can be produced using micro-embossing. The male mold 20 can be placed above the web 24, such as Figure 4 21, or placed under the web 24 (not shown); however, alternative arrangements are possible. See U.S. Pat. No. 7,715,088, which is incorporated herein by reference in its entirety. The conductive substrate can be constructed by forming a conductor film 21 on a polymer substrate, which becomes the backing of the device. A composition 22 comprising a thermoplastic, a thermosetting substance, or a precursor thereof is then applied to the conductor film. The thermoplastic or thermosetting precursor layer is embossed by a positive mold in the form of a roller, plate, or belt at a temperature above the glass transition temperature of the thermoplastic or thermosetting precursor layer.

[0038] The thermoplastic or thermosetting precursors used to prepare the micro-units can be multifunctional acrylates or methacrylates, vinyl ethers, epoxides and their oligomers or polymers, etc. The combination of multifunctional epoxides and multifunctional acrylates is also very useful for achieving the desired physical and mechanical properties. Crosslinkable oligomers such as urethane acrylates or polyester acrylates that impart flexibility can be added to improve the flexural resistance of the imprinted micro-units. The composition can contain polymers, oligomers, monomers and additives or only oligomers, monomers and additives. The glass transition temperature (or T g ) is usually in the range of about -70°C to about 150°C, preferably about -20°C to about 50°C. The micro-embossing method is generally carried out at a temperature above T g A heated male mold or a heated housing substrate against which the mold is pressed can be used to control the micro-embossing temperature and pressure.

[0039] like Figure 4As shown, demoulding during or after the precursor layer hardens to reveal the array of microunits 23. The hardening of the precursor layer can be completed by cooling, solvent evaporation, radiation crosslinking, thermal crosslinking or moisture crosslinking. If the curing of the thermosetting precursor is completed by ultraviolet radiation, the ultraviolet rays can be radiated from the bottom or top of the web to the transparent conductor film, as shown in the two figures. Alternatively, a UV lamp can be placed in the mold. In this case, the mold must be transparent so that the ultraviolet light is radiated to the thermosetting precursor layer through the pre-patterned positive mold. The positive mold can be prepared by any suitable method, such as a diamond turning method or a photoresist method, and then etching or electroplating. The master template for the positive mold can be manufactured by any suitable method, such as electroplating. Using electroplating, a thin layer (generally 200 mm) of a seed metal such as chrome inconel is used. ) sputtered glass substrate. The mold is then coated with a photoresist layer and exposed to ultraviolet light. A mask is placed between the ultraviolet light and the photoresist layer. The exposed areas of the photoresist become hardened. The unexposed areas are then removed by washing with a suitable solvent. The remaining hardened photoresist is dried and sputtered again with a thin layer of seed metal. The master is then ready for electroforming. The general material for electroforming is nickel cobalt. Alternatively, the master can be made of nickel by electroforming or chemical nickel deposition. The bottom of the mold is generally about 50 to 400 microns. The master can also be made using other microengineering techniques, including electron beam writing, dry etching, chemical etching, laser writing or laser interference, as described in "Replication techniques for micro-optics", SPIE Proc. Vol. 3099, pp. 76-82 (1997). Alternatively, the mold can be made using plastic, ceramic or metal by photomechanical processing.

[0040] Before applying the UV-curable resin composition, the mold can be treated with a release agent to help the demoulding process. The UV-curable resin can be degassed before distribution and can optionally contain a solvent. The solvent (if present) evaporates easily. The UV-curable resin is distributed on the male mold by any suitable means, such as coating, dipping, pouring, etc. The distributor can be mobile or fixed. The conductor film is covered with the UV-curable resin. If necessary, pressure can be applied to ensure that the appropriate combination between the resin and the plastic and the thickness of the bottom of the micro-unit are controlled. Lamination rollers, vacuum molding, pressure devices or any other similar means can be used to apply pressure. If the male mold is metallic and opaque, the plastic substrate is generally transparent to the actinic radiation used to cure the resin. On the contrary, the male mold can be transparent, and the plastic substrate can be opaque to actinic radiation. In order to realize that the molded features are well transferred to the transfer sheet, the conductor film needs to have good adhesion to the UV-curable resin, and the UV-curable resin should have good release properties for the mold surface.

[0041] Photolithography. Microcells can also be made using photolithography. Photolithography methods for making microcell arrays are Figure 5A and 5B The diagram in the figure shows the following. Figure 5A and 5B As shown, the microcell array 40 can be prepared by exposing a radiation-curable material 41a applied to a conductor electrode film 42 by known methods to ultraviolet light (or alternatively to other forms of radiation, electron beams, etc.) through a mask 46 to form walls 41b corresponding to the image projected through the mask 46. The base conductor film 42 is preferably mounted on a supporting substrate base web 43, which can include a plastic material.

[0042] exist Figure 5A In the photomask 46 in FIG. 4 , dark squares 44 represent opaque areas of the mask 46, and the spaces between the dark squares represent transparent areas 45 of the mask 46. The ultraviolet radiation reaches the radiation-curable material 41a through the transparent areas 45. The exposure is preferably performed directly on the radiation-curable material 41a, that is, the ultraviolet light does not pass through the substrate 43 or the base conductor 42 (top exposure). For this reason, neither the substrate 43 nor the conductor 42 need to be transparent to the ultraviolet light or other radiation wavelength used.

[0043] like Figure 5BAs shown, the exposed areas 41b become hardened, and then the unexposed areas (protected by the opaque areas 44 of the mask 46) are removed by a suitable solvent or developer to form micro-units 47. The solvent or developer is selected from those commonly used to dissolve radiation-curable materials or reduce the viscosity of radiation-curable materials, such as methyl ethyl ketone (MEK), toluene, acetone, isopropyl alcohol, etc. The preparation of the micro-units can be similarly accomplished by placing a photomask under the conductor film / substrate support web, and in this case, the UV light is radiated through the photomask from the bottom, and the substrate needs to be transparent to the radiation.

[0044] Imagewise exposure. Another alternative method for preparing the microunit array of the present invention by imagewise exposure is Figure 5C and 5D When opaque conductor lines are used, the conductor lines can be used as a photomask for exposure from the bottom. Additional exposure from the top through a second photomask with opaque lines perpendicular to the conductor lines forms durable microcell walls. Figure 5C The diagram illustrates the use of the top and bottom exposure principles to manufacture the microcell array 50 of the present invention. The base conductor film 52 is opaque and line patterned. The radiation-curable material 51a coated on the base conductor 52 and the substrate 53 is exposed from the bottom through the conductor line pattern 52 used as a first photomask. A second exposure is performed from the "top" side through a second photomask 56 having a line pattern perpendicular to the conductor lines 52. The spaces 55 between the lines 54 are substantially transparent to ultraviolet light. In this process, the wall material 51b is cured from the bottom up in a lateral orientation and from the top down in a vertical direction, connecting to form an integral microcell 57. As shown in FIG. Figure 5D As shown, the unexposed areas are then removed by a solvent or developer as described above to reveal the microelements 57.

[0045] After the microcells are fabricated, they are filled with a suitable mixture of a dyed hydrocarbon solvent and high density reflective particles. The microcell array 60 may be prepared by any of the methods described above. Figures 6A-6D As shown in the cross section of FIG. 6 , microcell walls 61 extend upward from a light-transmitting substrate 63 to form an open cell. Optionally, the microcell may include a primer layer 62 to passivate the bottom of the microcell to prevent high-density reflective particles from adhering to the cell bottom and / or walls.

[0046] Next, the microcells are filled with a dyed hydrocarbon mixture 64 that includes high-density reflective particles 65. In some embodiments, the dyed hydrocarbon mixture 64 that includes high-density reflective particles 65 will be sonicated prior to filling the microcells to produce a consistent mixture of high-density reflective particles 65 in the dyed hydrocarbon mixture 64. In some embodiments not shown in the figures, a desired amount of high-density reflective particles 65 is distributed among the microcells, and the dyed hydrocarbon mixture 64 is then filled into each microcell. In some embodiments, gentle agitation helps fill the microcells with high-density reflective particles 65. Filling can be accomplished with a pipette, a gravity-filled dispenser, or a rubber roller. Figure 6B As shown, different microcells may include different dyed hydrocarbon mixtures, as described above with respect to Figure 2 and 3 Microcells 60 are preferably partially filled to prevent overflow and inadvertent mixing of differently colored hydrocarbon mixtures.

[0047] Various techniques can be used to fill the microcells. In some embodiments, when a large number of adjacent microcells are to be filled with the same mixture, a doctor blade can be used to fill the microcells to the depth of the microcell wall 61. In other embodiments, a slot die with positionable channels can be used to simultaneously fill multiple types of dyed hydrocarbon mixtures. In still other embodiments, when different mixtures are to be filled into various nearby microcells, an inkjet-type microinjection can be used to fill the microcells. In still other embodiments, a microneedle array or a pipette can be used to fill the microcell array with the dyed hydrocarbon mixture in the correct order.

[0048] like Figure 6C As shown, after filling, the microcells are sealed by applying a polymer 66 that becomes a light-transmitting sealing layer. The light-transmitting sealing material may include polyvinyl alcohol, polyvinyl pyrrolidone, polyurethane, polyisobutylene, or acrylate. In some embodiments, the sealing process may involve exposure to heat, dry hot air, or ultraviolet radiation. In most embodiments, the polymer 66 will be compatible with the mixture 64, but will not be dissolved by hydrocarbon fluids. Therefore, the final microcell structure is almost leak-proof and can withstand flexing without delamination of the light-transmitting sealing layer.

[0049] After filling the microcells 60, the sealed array can be laminated to a top light-transmitting substrate 67 using a thin layer of optically clear adhesive (OCA) 68. The light-transmitting substrate 67 can be a polyethylene film. Figures 6A-6DIt is not shown, but another OCA layer may be used to add a bottom transparent substrate to the opposite side of the microcell array. In addition, the edges of the microcell array 60 may be sealed with a polymer such as polyurethane to prevent leakage of hydrocarbon fluids. In an alternative embodiment, the filled and sealed microcell array may be encapsulated and sealed with a polyethylene film preform, and the edges may be sealed with heat or by laser clamping.

[0050] Example 1 - Gravity-driven display with silver flakes

[0051] The microcell layer was prepared by microembossing polyethylene terephthalate (PET) as described above. A dyed hydrocarbon mixture was prepared by adding 30 grams of 10 μm silver flakes (Sigma Aldrich) to 140 mL of Isopar E along with 5 mL of Solsperse 19000 (Lubrizol) and 3 grams of Solvent Blue 89HF (Abbey Color). The mixture was sonicated for 10 minutes and then dispensed into the microcells with a pipette, and the residual dyed hydrocarbon mixture was removed from the top of the microcells with a rubber spatula. The filled microcells were coated with a light-transmitting sealing material consisting of 1 part (by weight) polyurethane (HD2125; Hauthaway Corp.) to four parts polyvinyl alcohol (Z410; Mitsubishi Chemical) to 2 parts deionized water. An 8 mil (0.21032 mm) thick wet coating of the sealing material was applied to the top of the filled microcells, and the coated sealing material was then dried to produce a light-transmitting sealing layer. Figure 7 Microscope view showing the filled and sealed microcell layer. The microcell walls (72) are covered by the polyurethane sealing layer (74) through which some silver flake particles (75) are visible. Figure 7 As shown, after the gravity-driven display has been placed, it appears blue when viewed from above. If the gravity-driven display is turned over, the new viewing surface is instantly shiny due to the reflective silver particles at the viewing surface. The shiny surface quickly begins to fade and returns to its original blue color after three seconds.

[0052] Example 2 - Gravity-driven display with bronze foil

[0053] The microcell layer was prepared by microembossing polyethylene terephthalate (PET) as described above. A dyed hydrocarbon mixture was prepared by adding 15 grams of 50 μm bronze metal flakes (Bravo Bronze, Lebanon, Tennessee) to 140 mL of Isopar E along with 5 mL of Solsperse 19000 (Lubrizol) and 3 grams of Solvent Blue 89HF (Abbey Color). The mixture was sonicated for 10 minutes and then dispensed into the microcells with a pipette, and the residual dyed hydrocarbon mixture was removed from the top of the microcells with a rubber spatula. The filled microcells were coated with a light-transmitting sealant consisting of 1 part (by weight) polyurethane (HD2125; Hauthaway Corp.) to four parts polyvinyl alcohol (Z410; Mitsubishi Chemical) to 2 parts deionized water. An 8 mil (0.21032 mm) thick wet coating of sealant material is applied on top of the filled microcells, and the applied sealant material is subsequently dried to produce a light-transmitting sealant layer. If the gravity-driven display is turned over, the new viewing surface instantly turns yellow and shiny due to the reflective bronze particles at the viewing surface. The shiny surface quickly begins to fade and returns to its original blue color after five seconds. For 140 ml E A subsequent sample was prepared using 1 gram of SolventBlue 89HF, which had a lighter blue base color, and a clear transition from shiny yellow to green to blue after the device was turned over.

[0054] It is obvious to those skilled in the art that various changes and modifications may be made to the specific embodiments of the present invention described above without departing from the scope of the present invention. Therefore, the entire contents of the above description should be interpreted in an illustrative rather than a restrictive sense.

Claims

1. A gravity-driven display (10, 30, 80), wherein include: An array of microcells (11), each microcell (11) having a wall (12), a bottom (13) and a top opening, wherein the bottom (13) of each microcell is light-transmissive; a first mixture comprising reflective particles (15) having a density greater than 7 g / cm3, a hydrocarbon solvent (14), and a first soluble dye, wherein the first mixture is disposed in at least some of the microlocations (11) in the array; and A light-transmitting sealing layer (16) seals the first mixture in at least some of the microcells (11).

2. The gravity-driven display of claim 1, wherein the reflective particles (15) comprise silver, tungsten, gold, platinum, nickel, copper, tin, zinc, indium or a bronze alloy.

3. A gravity-driven display as described in claim 1 or 2, wherein the first mixture comprises 5-15% surfactant (surfactant weight / mixture weight), 20-50% reflective particles (particle weight / mixture weight) and 1-8% soluble dye (soluble dye weight / mixture weight), and the balance is hydrocarbon solvent.

4. A gravity-driven display (10, 30, 80), wherein include: An array of microcells (11), each microcell (11) having a wall (12), a bottom (13) and a top opening, wherein the bottom (13) of each microcell is light-transmissive; a first mixture comprising reflective particles (15) having a density less than 0.5 g / cm3, a hydrocarbon solvent (14), and a first soluble dye, wherein the first mixture is disposed in at least some of the microlocations (11) in the array; and A light-transmitting sealing layer (16) seals the first mixture in at least some of the microcells (11).

5. The gravity-driven display of claim 4, wherein the reflective particles (15) comprise silicon dioxide, zirconium oxide or aluminum oxide.

6. The gravity-driven display of any one of claims 1 to 5, further comprising a first light-transmitting substrate (17) coupled to the array of microcells (11), and optionally a second light-transmitting substrate (18) coupled to the light-transmitting sealing layer (16).

7. The gravity-driven display of any one of claims 1 to 5, wherein the gravity-driven display does not include any material with an electrical conductivity greater than 1×10 4 Ohm cm layer.

8. The gravity driven display of any one of claims 1 to 5, wherein the gravity driven display is less than 1 mm thick, optionally less than 200 μm thick.

9. A gravity driven display as claimed in any preceding claim further comprising a graphic overlay (85) which conceals a portion of the gravity driven display from a viewer and is colour matched to the reflective particles (15) or to a soluble dye.

10. A gravity-driven display as claimed in any one of claims 1 to 5, further comprising a second mixture (34B) comprising reflective particles (15), a hydrocarbon solvent (14) and a second soluble dye, wherein the second mixture (34B) is arranged in at least some of the microcells (31B), and the at least some of the microcells (31B) are different from at least some of the microcells (31A) in which the first mixture (34A) is arranged.

11. The gravity driven display of claim 10, wherein the first and second soluble dyes are different colors.

12. The gravity-driven display of any one of claims 1-5, wherein the longest dimension of the reflective particles (15) is 5 μm to 25 μm.

13. The gravity driven display of any one of claims 1 to 5, wherein the hydrocarbon solvent (14) comprises aliphatic molecules having a molecular weight of 100 g / mol to 300 g / mol.

14. The gravity-driven display of any one of claims 1 to 5, wherein the microcell walls (12) and base (13) comprise acrylates, vinyl ethers or epoxides, and the sealing layer (16) comprises polyvinyl alcohol, polyvinyl pyrrolidone, polyurethane, polyisobutylene or acrylates.

15. The gravity-driven display of any one of claims 1 to 5, wherein the first mixture further comprises a surfactant.

Citation Information

Patent Citations

  • Image presentation and micro-optic security system

    CN101379423A

  • Image arrays for security devices and methods of manufacture thereof

    GB201510072D0

  • Security devices and methods of manufacture thereof

    GB201510073D0

  • Electrophoretic display and novel process for its manufacture

    US20020131152A1

  • Plastic cards with high density particles

    US20150041546A1