Method and system for repairing short circuit failure in liquid metal battery

The Lorentz force is generated through heating and electromagnetic effects, which solves the problem of short circuit inside the liquid metal battery, realizes self-healing of the electrode interface, and extends the service life of the battery.

CN119069841APending Publication Date: 2024-12-03HUAZHONG UNIV OF SCI & TECH +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411201226.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

Liquid metal batteries may form solid intermetallic compounds at high discharge depths, resulting in contact with positive and negative electrodes and internal short circuits. The existing technology lacks effective repair methods, which makes the battery unable to heal on its own.

Method used

The liquid metal battery is heated to the working temperature, and a Lorentz force is generated by the preset non-parallel charging current and external magnetic field under the electromagnetic effect, driving the discharge product to separate from the metal negative electrode, realizing self-healing of the electrode interface.

Benefits of technology

By adjusting the charging current and magnetic field strength, the discharge product can be effectively driven away from the negative electrode, restored the electrode interface, realize the self-healing of the liquid metal battery, and extend the battery service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069841A_ABST
    Figure CN119069841A_ABST
Patent Text Reader

Abstract

The invention discloses a method and a system for repairing an internal short circuit failure of a liquid metal battery, and belongs to the technical field of energy storage batteries, the method comprises the following steps: heating the liquid metal battery with the internal short circuit failure to a working temperature and keeping the working temperature; providing a preset external magnetic field covering the battery while providing a preset charging current for the liquid metal battery, and generating a preset Lorentz force under an electromagnetic effect; and a discharge product in the liquid metal battery is separated from the metal negative electrode under the action of the preset Lorentz force. The liquid metal battery with internal short circuit failure is heated to the working temperature and kept, the liquid metal battery is charged, due to the fact that the contact area between a battery discharge product and a negative electrode is large, and the current density at the contact position is very large, a magnetic field with certain intensity is applied at the moment; when the liquid metal battery is charged, a strong Lorentz force and moment can be generated in the liquid metal battery, so that a discharge product can be effectively driven to be separated from a negative electrode and recovered to a positive electrode area, and the self-healing process of an electrode interface is completed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of energy storage batteries, and more specifically, relates to a method and system for repairing short circuit failure in a liquid metal battery. Background Art

[0002] Liquid metal batteries are seen as a competitive option in the field of large-scale static energy storage. Its structure consists of three layers of immiscible liquids: the upper layer is the negative electrode metal, the middle layer is the inorganic molten salt electrolyte (also serving as a diaphragm), and the lower layer is the positive electrode metal gold. Liquid metal batteries completely avoid the irreversible changes in the electrode structure and the side reactions between the electrode and the electrolyte. In theory, they have an extremely long cycle life; the electrolyte is non-flammable and has inherent safety characteristics; the raw materials are widely available, the reserves are abundant, and the energy storage cost is low. However, despite the advantages of long life, high safety, and low cost, liquid metal batteries have a certain probability of internal short circuit failure during service.

[0003] This is because when the liquid metal battery is at a higher depth of discharge (or when the concentration polarization is large), a high melting point, solid intermetallic compound (such as Li3Bi, Li3Sb, etc.) will form at the positive electrode interface. Taking the Li||Bi system as an example, the uneven growth of solid Li3Bi may cause the positive and negative electrodes to contact, resulting in an internal circuit. Since Li3Bi is an electronic conductor, when the positive and negative electrodes contact, the charging current flows directly from the positive electrode through the solid Li3Bi to the negative electrode, and does not pass through the electrolyte with very low conductivity. At this time, the charging voltage is basically 0V. Since no electrochemical reaction can occur, solid Li3Bi cannot be de-lithiated and converted into a liquid Li-Bi alloy during the charging process. That is, once an internal short circuit occurs, the battery cannot heal itself.

[0004] Therefore, it is of great significance to propose a new method to repair the electrode interface of a short-circuited liquid metal battery so that it can work normally again. Summary of the invention

[0005] In view of the above defects or improvement needs of the prior art, the present invention provides a method and system for repairing short-circuit failure in a liquid metal battery, the purpose of which is to solve the technical problem in the prior art of lacking a method for repairing a short-circuited liquid metal battery.

[0006] To achieve the above object, according to one aspect of the present invention, a method for repairing short circuit failure in a liquid metal battery is provided, comprising:

[0007] S1: heating the liquid metal battery with internal short circuit failure to the operating temperature and maintaining the temperature, wherein the metal positive electrode in the liquid metal battery is connected to the metal negative electrode through the discharge product, resulting in a short circuit;

[0008] S2: providing a preset charging current for the liquid metal battery and providing a preset external magnetic field covering the liquid metal battery, so as to generate a preset Lorentz force acting on the inside of the liquid metal battery under the electromagnetic effect; the directions of the preset charging current and the preset external magnetic field are not parallel;

[0009] S3: Under the action of the preset Lorentz force, the preset Lorentz force causes the discharge product inside the liquid metal battery to separate from the metal negative electrode, thereby achieving self-healing of the liquid metal battery.

[0010] In one embodiment, the intensity and direction of the preset charging current are adjustable.

[0011] In one embodiment, the current intensity of the preset charging current corresponds to an adjustment range of 10 to 2000 mA / cm 2 .

[0012] In one of the embodiments, the strength and direction of the preset external magnetic field are adjustable.

[0013] In one of the embodiments, the magnetic field strength of the preset external magnetic field has an adjustment range of 0.001 to 2T.

[0014] In one embodiment, when the preset Lorentz force is generated, the current density at the contact position between the discharge product and the metal negative electrode is dozens of times the current density during normal charge and discharge.

[0015] In one embodiment, the metal positive electrode includes: one of metal bismuth, antimony, tellurium, tin, lead and alloys thereof.

[0016] In one embodiment, the metal negative electrode includes: one of metal lithium, metal sodium, metal potassium, metal magnesium, and metal calcium.

[0017] In one embodiment, the electrolyte in the liquid metal battery includes a metal halide salt mixture.

[0018] According to another aspect of the present invention, a repair system for short circuit failure in a liquid metal battery is provided, comprising:

[0019] A heating device, used to heat the liquid metal battery that has failed due to internal short circuit to the operating temperature;

[0020] A battery testing device, used to provide a preset charging current for the liquid metal battery;

[0021] An external magnetic field device, used for providing a preset external magnetic field covering the liquid metal battery while the battery testing device provides the preset charging current to the liquid metal battery, so as to generate a preset Lorentz force acting on the inside of the liquid metal battery under the electromagnetic effect;

[0022] Among them, the directions of the preset charging current and the preset external magnetic field are non-parallel; under the action of the preset Lorentz force, the preset Lorentz force causes the discharge products inside the liquid metal battery to separate from the metal negative electrode, thereby achieving self-healing of the liquid metal battery.

[0023] In general, the above technical solutions conceived by the present invention can achieve the following beneficial effects compared with the prior art:

[0024] (1) The present invention provides a method for repairing a liquid metal battery that has failed due to an internal short circuit. The method comprises heating the liquid metal battery that has failed due to an internal short circuit to an operating temperature and maintaining the temperature. The liquid metal battery is also charged. Since the contact area between the discharge product of the battery and the negative electrode is large and the current density at the contact point is very large, a magnetic field of a certain intensity is applied at this time, which will generate a strong Lorentz force and torque inside the liquid metal battery, which can effectively drive the discharge product to break contact with the negative electrode and return to the positive electrode area, thereby completing the self-healing process of the electrode interface.

[0025] (2) This solution adjusts the intensity and direction of the Lorentz force by adjusting the intensity and direction of the preset charging current, thereby causing the discharge product to separate from the metal negative electrode and achieving internal short circuit self-healing of the liquid metal battery.

[0026] (3) This solution can flexibly and quickly adjust the intensity and direction of the Lorentz force by adjusting the preset charging current and the intensity and direction of the preset external magnetic field, thereby prompting the discharge product to quickly separate from the metal negative electrode and achieving internal short-circuit self-healing of the liquid metal battery.

[0027] (4) In this solution, when the preset Lorentz force is generated, the current density at the contact position between the discharge product and the metal negative electrode is dozens of times the current density during normal charge and discharge. Since the contact area between the battery discharge product and the negative electrode is large, the current density at the contact point is very large, which may be dozens of times the normal charge and discharge current density, and a large torque will be generated, causing the product to separate from the negative electrode. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 The first embodiment of the present invention provides a flow chart of a method for repairing short-circuit failure in a liquid metal battery;

[0029] Figure 2 This is a schematic diagram of the mechanism of repairing a short-circuited liquid metal battery by applying an external magnetic field provided in Example 1 of the present invention;

[0030] Figure 3 is a cross-sectional photograph of a liquid metal with an internal short circuit provided in Example 1 of the present invention;

[0031] Figure 4 It is a schematic diagram of an experimental device corresponding to a liquid metal battery internal short circuit failure repair system provided in Example 2 of the present invention;

[0032] Figure 5 is a charge and discharge curve diagram of the process of repairing a short-circuited liquid metal battery provided in Example 2 of the present invention;

[0033] Figure 6 It is a comparison diagram of the discharge curves before short circuit and after external magnetic field repair provided by Example 2 of the present invention. DETAILED DESCRIPTION

[0034] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0035] Example 1

[0036] like Figure 1 As shown, this embodiment provides a method for repairing an internal short circuit failure of a liquid metal battery, characterized in that it includes: S1: heating the liquid metal battery with internal short circuit failure to the operating temperature and maintaining it, so that the metal positive electrode in the liquid metal battery is connected to the metal negative electrode through the discharge product to cause a short circuit; S2: providing a preset charging current to the liquid metal battery while providing a preset external magnetic field covering the liquid metal battery, and generating a preset Lorentz force acting on the inside of the liquid metal battery under the electromagnetic effect; the directions of the preset charging current and the preset external magnetic field are not parallel; S3: under the action of the preset Lorentz force, the preset Lorentz force causes the discharge product inside the liquid metal battery to separate from the metal negative electrode, thereby realizing self-healing of the liquid metal battery.

[0037] It should be understood that although Figure 1 The steps in the flowchart are shown in sequence as indicated by the arrows, but these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified in this document, there is no strict order restriction for the execution of these steps, and these steps can be executed in other orders. Moreover, Figure 1At least part of the steps may include multiple sub-steps or multiple stages. These sub-steps or stages are not necessarily executed at the same time, but can be executed at different times. The execution order of these sub-steps or stages is not necessarily sequential, but can be executed in turn or alternately with other steps or at least part of the sub-steps or stages of other steps.

[0038] like Figure 2 The mechanism of repairing short-circuited liquid metal batteries by applying an external magnetic field is explained. Figure 2 Part (a) is a schematic diagram of a liquid metal battery with internal short circuit failure. Figure 2 Part (b) is a schematic diagram of a liquid metal battery with a repaired internal short circuit. The Lorentz force F (and its torque) generated by the interaction between the charging current I and the magnetic induction intensity B breaks the contact between the positive and negative electrodes. At this time, the charging current can only pass through the molten salt electrolyte, causing the electrochemical reaction to begin, and the positive electrode gradually transforms into a full liquid phase state at a low discharge depth. Under the action of the surface tension of the liquid, the electrode completes the self-healing process.

[0039] As an optional implementation, the intensity and direction of the preset charging current are adjustable.

[0040] As an optional implementation, the current intensity of the preset charging current corresponds to an adjustment range of 10 to 2000 mA / cm 2 .

[0041] As an optional implementation, the strength and direction of the preset external magnetic field are adjustable.

[0042] As an optional implementation, the adjustment range of the magnetic field strength of the preset external magnetic field is 0.001-2T.

[0043] As an optional implementation manner, when the preset Lorentz force is generated, the current density at the contact position between the discharge product and the metal negative electrode is several dozen times the current density during normal charge and discharge.

[0044] The present invention is further described in detail below with reference to specific cases.

[0045] Example 1: (1) For a short-circuited liquid metal battery (the negative electrode is metal lithium, the electrolyte is LiCl-KCl eutectic salt, the positive electrode is metal bismuth, and the operating temperature is 450°C); (2) Place the battery in a heating furnace, heat it to the operating temperature, connect it to a battery tester, and apply 200 mA cm -2 The current density is 250 mT; at the same time, a horizontal magnetic field of 250 mT is applied through the Helmholtz coil to complete the repair of the short-circuited liquid metal battery.

[0046] Example 2: (1) For a short-circuited liquid metal battery (the negative electrode is metal lithium, the electrolyte is LiCl-LiBr-KBr eutectic salt, the positive electrode is metal bismuth, and the operating temperature is 420°C); (2) Place the battery in a heating furnace, heat it to the operating temperature, connect it to a battery tester, and apply 300 mA cm -2 At the same time, a 200mT horizontal magnetic field is applied through the Helmholtz coil to complete the repair of the short-circuited liquid metal battery.

[0047] Example 3: (1) For a short-circuited liquid metal battery (the negative electrode is metallic lithium, the electrolyte is LiF-LiCl-LiBr eutectic salt, the positive electrode is antimony-tin alloy, and the operating temperature is 500°C); (2) Place the battery in a heating furnace, heat it to the operating temperature, connect it to a battery tester, and apply 500 mA cm -2 At the same time, a 150mT horizontal magnetic field is applied through the Helmholtz coil to complete the repair of the short-circuited liquid metal battery.

[0048] Example 4: (1) For a short-circuited liquid metal battery (the negative electrode is metallic lithium, the electrolyte is LiCl-KCl-CsCl eutectic salt, the positive electrode is bismuth-tin alloy, and the operating temperature is 300°C); (2) Place the battery in a heating furnace, heat it to the operating temperature, connect it to a battery tester, and apply 200 mA cm -2 current density; at the same time, a high temperature resistant permanent magnet (such as a samarium cobalt magnet) is used to apply a magnetic field of a certain strength, thereby completing the repair of the short-circuited liquid metal battery.

[0049] Example 5: (1) For a short-circuited liquid metal battery (the negative electrode is sodium potassium alloy, the electrolyte is 1M sodium perchlorate dissolved in DME / FEC solvent, the positive electrode is gallium indium tin alloy, and the operating temperature is room temperature); (2) Place the battery in a heating furnace, heat it to the operating temperature, connect it to a battery tester, and apply 200 mA cm -2 current density; at the same time, a permanent magnet (such as a NdFeB magnet) is used to apply a magnetic field of a certain strength to complete the repair of the short-circuited liquid metal battery.

[0050] As an optional embodiment, the metal positive electrode includes: one of metal bismuth, antimony, tellurium, tin, lead and alloys thereof.

[0051] As an optional embodiment, the metal negative electrode includes: one of metal lithium, metal sodium, metal potassium, metal magnesium, and metal calcium.

[0052] As an optional embodiment, the electrolyte in the liquid metal battery includes a metal halide salt mixture, such as LiF-LiCl, LiF-LiCl-LiBr, LiF-LiCl-LiI, LiCl-KCl, LiCl-NaCl-KCl, LiCl-LiBr-KBr, LiCl-KCl-CsCl, LiBr-KBr-CsBr, etc.

[0053] like Figure 3 The picture shows a cross-section of a liquid metal with an internal short circuit. For example, the negative electrode is lithium metal, the electrolyte is LiCl-KCl eutectic salt, the positive electrode is bismuth metal, and the operating temperature of the battery is 450°C. Due to the uneven deposition of the intermetallic compound (Li3Bi), the positive and negative electrodes come into contact, and the electrodes cannot heal themselves during charging.

[0054] Example 2

[0055] This embodiment provides a repair system for a liquid metal battery with an internal short circuit failure, comprising: a heating device, a battery testing device, and an external magnetic field device. The heating device is used to heat the liquid metal battery with an internal short circuit failure to the operating temperature, and may be a heating furnace; the battery testing device is used to provide a preset charging current for the liquid metal battery; the external magnetic field device is used to provide a preset external magnetic field covering the liquid metal battery while the battery testing device provides the preset charging current for the liquid metal battery, and to generate a preset Lorentz force acting on the inside of the liquid metal battery under the electromagnetic effect. Among them, the directions of the preset charging current and the preset external magnetic field are not parallel; under the action of the preset Lorentz force, the preset Lorentz force causes the discharge products inside the liquid metal battery to separate from the metal negative electrode, thereby achieving self-healing of the liquid metal battery.

[0056] like Figure 4 The figure shows the liquid metal battery test and the external magnetic field device. The liquid metal battery is placed in a pit furnace and heated to the operating temperature. Its leads extend out of the furnace and are connected to the battery tester. A horizontal, uniform, and adjustable magnetic field is applied through the Helmholtz coil.

[0057] Figure 5The charge and discharge curves of the liquid metal battery during the short-circuit repair process are shown. Internal short-circuit failure is a key failure form of liquid metal batteries. In the past, the lack of repair methods for short-circuited liquid metal batteries restricted the service life of the battery. The method of repairing short-circuited liquid metal batteries through an external magnetic field (Lorentz force) can make the failed battery work normally again and extend the service life of the battery. When the magnetic field is not applied, the charging voltage of the battery is about 0V due to the short circuit between the positive and negative poles, and the effective capacity cannot be charged at all times; after applying a 250mT magnetic field, the contact between the positive and negative poles is broken, and the charging voltage returns to normal. After the repair is completed, the external magnetic field is removed, and the battery can still perform normal charge and discharge cycles.

[0058] Figure 6 This is a comparison of the discharge curves before short circuit and after external magnetic field repair. During the discharge process, the battery short-circuited and the voltage dropped sharply. In the subsequent charging process, the voltage was basically 0V and could not reach the normal charging voltage. After the magnetic field was applied, under the action of the Lorentz force and torque, the contact between the positive and negative electrodes was broken, the effective capacity could be charged, the charging voltage returned to normal, and the self-healing process was gradually completed. After the magnetic field was removed, the battery was able to continue the normal charge and discharge cycle.

[0059] It will be easily understood by those skilled in the art that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for repairing short circuit failure in a liquid metal battery, characterized in that: include: S1: heating the liquid metal battery with internal short circuit failure to the operating temperature and maintaining the temperature, wherein the metal positive electrode in the liquid metal battery is connected to the metal negative electrode through the discharge product, resulting in a short circuit; S2: providing a preset charging current for the liquid metal battery and providing a preset external magnetic field covering the liquid metal battery, so as to generate a preset Lorentz force acting on the inside of the liquid metal battery under the electromagnetic effect; the directions of the preset charging current and the preset external magnetic field are not parallel; S3: Under the action of the preset Lorentz force, the preset Lorentz force causes the discharge product inside the liquid metal battery to separate from the metal negative electrode, thereby achieving self-healing of the liquid metal battery.

2. The method for repairing short circuit failure in a liquid metal battery according to claim 1, characterized in that: The intensity and direction of the preset charging current are adjustable.

3. The method for repairing internal short circuit failure of a liquid metal battery according to claim 2, characterized in that: The current intensity of the preset charging current corresponds to an adjustment range of 10 to 2000 mA / cm 2 .

4. The method for repairing internal short circuit failure of a liquid metal battery according to claim 1, characterized in that: The intensity and direction of the preset external magnetic field are adjustable.

5. The method for repairing internal short circuit failure of a liquid metal battery according to claim 4, characterized in that: The magnetic field strength of the preset external magnetic field has an adjustment range of 0.001 to 2T.

6. The method for repairing internal short circuit failure of a liquid metal battery according to claim 1, characterized in that: When the preset Lorentz force is generated, the current density at the contact position between the discharge product and the metal negative electrode is several dozen times the current density during normal charge and discharge.

7. The method for repairing internal short circuit failure of a liquid metal battery according to claim 1, characterized in that: The metal positive electrode includes: one of metal bismuth, antimony, tellurium, tin, lead and alloys thereof.

8. The method for repairing internal short circuit failure of a liquid metal battery according to claim 7, characterized in that: The metal negative electrode includes: one of metal lithium, metal sodium, metal potassium, metal magnesium, and metal calcium.

9. The method for repairing internal short circuit failure of a liquid metal battery according to claim 7, characterized in that: The electrolyte in the liquid metal battery includes a metal halide salt mixture.

10. A liquid metal battery internal short circuit failure repair system, characterized in that: include: A heating device is used to heat a liquid metal battery that has failed due to an internal short circuit to an operating temperature, wherein the metal positive electrode in the liquid metal battery is connected to the metal negative electrode through the discharge product to cause a short circuit; A battery testing device, used to provide a preset charging current for the liquid metal battery; An external magnetic field device, used for providing a preset external magnetic field covering the liquid metal battery while the battery testing device provides the preset charging current to the liquid metal battery, so as to generate a preset Lorentz force acting on the inside of the liquid metal battery under the electromagnetic effect; Among them, the directions of the preset charging current and the preset external magnetic field are non-parallel; under the action of the preset Lorentz force, the preset Lorentz force causes the discharge products inside the liquid metal battery to separate from the metal negative electrode, thereby achieving self-healing of the liquid metal battery.