Continuous pulse hybrid patterned laser powder bed light path system and method thereof

By using a continuous pulse hybrid patterned laser powder bed optical path system, the powder is preheated by continuous light and melted by microsecond pulse light, which solves the problems of laser damage and large heat-affected zone, and achieves high-precision and high-efficiency part forming.

CN121467728APending Publication Date: 2026-02-06AIR FORCE UNIV PLA

Patent Information

Application Number
CN202511738034.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2025-11-25
Publication Date
2026-02-06

AI Technical Summary

Technical Problem

In existing technologies, single-pulse laser powder bed forming carries the risk of laser damage to optical components, and the continuous light heating time is too long, resulting in a large heat-affected zone and affecting the printing accuracy of parts.

Method used

A continuous pulse hybrid patterned laser powder bed optical path system is adopted. The powder is preheated to near its melting point without melting by continuous light, and then melted by microsecond pulse light. This controls the heating time and the range of thermal radiation, thereby reducing laser loss.

Benefits of technology

It improves the forming accuracy of parts, reduces the risk of damage to optical components, and balances processing efficiency and process stability, making it suitable for industrial-grade additive manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN121467728A_ABST
    Figure CN121467728A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of 3D printing, and particularly relates to a continuous pulse mixed type patterning laser powder bed light path system and method.Laser powder is preheated to be close to a melting point but not molten through set continuous-period light emitting, the preheated laser powder is completely molten through pulse-period light emitting, and in other words, the continuous pulse mixed type patterning laser powder bed light path system and method are obtained; continuous light is only used for preheating powder for a short time, so that the powder is close to a melting point but not molten; then peak energy is rapidly provided through microsecond pulsed light, powder melting is completed instantly, in this way, the effective heating time is shortened, the heat radiation range of heating is controlled, the heating time of a system is far shorter than the heating time of traditional continuous light, melting and solidification are completed when heat is not diffused out of a preset pattern in time, and the production efficiency is greatly improved. Therefore, the fusion area is limited within the pattern range, the subsequent part forming precision is improved, and laser loss caused by too high peak power due to short time is reduced through pulse light emitting and continuous light emitting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of 3D printing technology, specifically relating to a continuous pulse hybrid patterned laser powder bed optical path system and method. Background Technology

[0002] Laser Powder Bed Fusion (LPBF) is an advanced metal 3D printing technology widely used in aerospace, medical implants, and high-end manufacturing. Its working principle involves using a high-precision laser beam to scan a pre-spread bed of metal powder layer by layer, selectively melting and solidifying the powder particles, ultimately stacking them to form complex three-dimensional solid parts. Compared to traditional point-scanning laser powder bed fusion, patterned laser powder bed forming, through process innovation, surpasses traditional methods in speed, quality, and controllability, making it particularly suitable for high-efficiency, high-precision, and low-stress industrial additive manufacturing scenarios.

[0003] In the prior art, for example, Chinese Patent Publication No. CN113226622B discloses an additive manufacturing system for two-dimensional printing using pulsed laser. This system may include providing a powder bed and guiding a sequence of shaped laser beam pulses, consisting of one or more pulses and having a flux greater than 20 kW / cm², within a defined two-dimensional region of the powder bed. This minimizes adverse laser-plasma effects during the melting and fusion of the powder within the defined two-dimensional region. Another example is Chinese Patent Publication No. CN117884656A, which discloses a surface area printing system for laser additive manufacturing. This system can achieve the melting and shaping of an entire area with a single pulse, improving processing efficiency without increasing the number of lasers.

[0004] The existing technology has the following limitations: The optical systems used in the above patents all adopt a patterned melting and solidification scheme with single-pulse light emission. However, the high peak power of the pulsed laser increases the risk of laser damage to optical devices. If the traditional continuous light emission patterned melting and solidification scheme is used, due to the reduction in peak power, the area with a large pattern requires a longer single heating time scale, which will result in a large heat-affected zone and ultimately affect the printing accuracy of the parts. Summary of the Invention

[0005] To address the aforementioned problems in the prior art, this invention provides a continuous pulse hybrid patterning laser powder bed optical path system and method, which solves the problems of reduced printing accuracy due to excessively long continuous light heating timescale and laser loss caused by short pulse light emission and excessively high peak power during the patterning process of laser powder bed powder.

[0006] The objective of this invention can be achieved through the following technical solution: a continuous pulse hybrid patterned laser powder bed optical path system, comprising a computer module, a power supply module, a hybrid laser emitter, a homogenization and shaping module, a pattern modulation module, a scanning module, and a forming cylinder. The computer module controls the power module to output power through a set control program, and controls the hybrid laser with the power output. The hybrid laser emits light periodically in sequence to generate a beam; The homogenization and shaping module adjusts the beam generated by the hybrid laser into a rectangular uniform spot; The computer module slices the three-dimensional structure to be printed, divides the slices according to the size of the rectangular light spot, and sends the divided graphics to the pattern modulation module in sequence. A uniform rectangular light spot is modulated into a patterned light spot by a pattern modulation module, and then the light spot is moved by a scanning module to a designated position on the processing table for processing.

[0007] Preferably, the power module includes two independent logic paths; The logic path one includes a delay signal generator one, a continuous wave modulation module and a power amplifier one, which are connected in sequence by electrical connection. The second logic path includes a second delay signal generator, a second continuous wave modulation module, and a second power amplifier unit, which are connected in sequence.

[0008] Preferably, the operating logic of the power module is as follows: Delay signal generator one and delay signal generator two periodically send control signals in sequence. The signal sent by delay signal generator one enters the continuous wave modulation module and continuously outputs a high level. The signal sent by delay signal generator two enters the microsecond pulse modulation module two and intermittently outputs a pulse high level. The continuous high level enters the power amplification unit one, and the pulse high level enters the power amplification unit two.

[0009] Preferably, the output of the hybrid laser in a single cycle is used only for the melting and solidification of a single pattern, and the output of the laser in a continuous cycle is used to preheat the laser powder to the melting point but not to melt it, while the output of the laser in a pulse cycle is used to completely melt the preheated laser powder.

[0010] A continuous pulse hybrid patterned laser powder bed optical path method includes the following steps: S1: Set the thickness and rectangular segmentation size of the 3D structure slice to be processed, control the computer module to slice it, segment the single layer after slicing, and plan the scanning path; S2: Based on the thickness and size after segmentation, and combined with the material characteristics of the powder to be printed and the laser characteristics, calculate the power and duration of continuous light emission, the power, duration and number of pulsed light emission, and the laser characteristics including emission wavelength and wall insertion efficiency. S3: Determine the interval time based on the sum of the continuous light emission time and the pulse light emission time, as well as the power supply modulation capability and the response capability of the scanning module. Determine the power supply adjustment frequency based on the interval time and the sum of the time, and control the pattern switching frequency of the pattern modulation module and the motion frequency of the scanning module to be consistent with the adjustment frequency. S4: The power module modulates the output power waveform according to the parameters in step S3, and supplies the hybrid laser to emit light periodically in sequence. The hybrid laser is modulated into a uniform rectangular spot by the homogenization and shaping module, and the size of the rectangular spot is controlled to be consistent with the rectangular segmentation size. S5: The computer module sends the segmented pattern to the pattern modulation module, and the rectangular light spot is modulated to form a high-power patterned light spot; S6: High-power patterned light spots move on the processing table via the scanning module and are scanned and stitched together to complete single-layer printing; S7: The processing table descends one layer, the powder is re-spread, and the processing is carried out again according to the preset scanning path. Repeat steps S6 and S7 to complete the processing of the entire part.

[0011] Preferably, in S3, determining the adjustment frequency includes: The total time for calibrating continuous light emission time and pulsed light emission time is: and interval time The processing cycle T for a single pattern is determined as follows: ; The adjustment frequency f of the power module is determined based on the later stage of the processing. .

[0012] Preferably, the material properties include the specific heat capacity, thermal conductivity, diffusivity, and density of the printing powder.

[0013] Preferably, in S7, the layer thickness of the processing table descending one layer is the slice thickness.

[0014] The beneficial effects of this invention are as follows: This system uses continuous periodic light emission to preheat the laser powder to near its melting point without melting it, while pulsed periodic light emission ensures complete melting of the preheated powder. In other words, continuous light is used only for short-term preheating, bringing the powder temperature close to its melting point without melting it. Subsequently, microsecond pulsed light rapidly provides peak energy, instantly melting the powder. This not only shortens the effective heating time but also controls the range of thermal radiation. Because the system's heating time is much shorter than that of traditional continuous light (continuous "low-temperature heating"), the heat does not have time to diffuse beyond the preset pattern before melting and solidification, thus limiting the melting area to within the pattern range. This improves the forming accuracy of subsequent parts and reduces laser loss caused by excessively high peak power due to short durations, achieved through pulsed and continuous light emission. Attached Figure Description

[0015] To facilitate understanding by those skilled in the art, the present invention will be further described below with reference to the accompanying drawings.

[0016] Figure 1 This is a system structure block diagram of the optical path system of the present invention; Figure 2 This is a waveform diagram of the high-level pulse output of the hybrid laser of the present invention; Figure 3 The output power waveform of the power supply module of the optical path system of this invention is shown in the figure. Figure 4 The diagram shows the continuous high-level and continuous pulse high-level waveforms of the power supply module of the optical path system of this invention. Detailed Implementation

[0017] To further illustrate the technical means and effects of the present invention in achieving its intended purpose, the following detailed description of the specific implementation methods, structures, features, and effects of the present invention, in conjunction with the accompanying drawings and preferred embodiments, is provided.

[0018] Please see Figures 1-4 This embodiment provides a continuous pulse hybrid patterned laser powder bed optical path system, which includes a computer module, a power supply module, a hybrid laser, a homogenization and shaping module, a pattern modulation module, a scanning module, and a forming cylinder. The computer module controls the power module to output power through a set control program, and uses the power output to control the hybrid laser. The power supply module includes two independent logic paths. Logic path one includes a delay signal generator, a continuous wave modulation module, and a power amplifier unit connected in sequence. Logic path two includes a delay signal generator and a continuous wave modulation module and a power amplifier unit connected in sequence. The working logic of the power module is as follows: Delay signal generator one and delay signal generator two periodically emit control signals in sequence. The computer controls delay signal generator one (output signal one) and delay signal generator two (output signal two), with a timing deviation ≤10ns. Then, delay signal generator one emits signal one into the continuous wave modulation module, continuously outputting a high level. Delay signal generator two emits signal two into the microsecond pulse modulation module two, intermittently outputting a pulse high level. The continuous high level enters power amplifier unit one, and the pulse high level enters power amplifier unit two. Please refer to [link to relevant documentation]. Figure 4 The waveforms of continuous high level and continuous pulse high level of the power supply module are given. The hybrid-emitting laser generates a beam by sequentially and periodically emitting light. Within a single cycle, the emitted light is used only for melting a single pattern. Continuous periodic emission preheats the laser powder to near its melting point without melting it. Pulsed periodic emission completely melts the preheated laser powder. (See also...) Figure 2 The waveform of the high-level pulse output of the hybrid laser is given. Among them, the core function of continuous periodic light emission is to "preheat the powder to near its melting point but not melt it", in order to avoid splashing caused by the subsequent pulse light requiring too much energy; The homogenization and shaping module modulates the beam generated by the mixed-emit laser into a rectangular uniform spot. The homogenization and shaping module is configured as an illumination system, a microlens array, and a rectangular aperture. The computer module slices the 3D structure to be printed, dividing the slices according to the size of the rectangular light spot. The segmented graphics are then sent to the pattern modulation module in sequence. Specifically, the computer module is equipped with professional LPBF slicing software (such as Magics or Materialise Insight), imports the 3D model to be processed (STL format), and slices it layer by layer according to the set slice thickness. During the slicing process, the "automatic support structure generation" function is enabled, and for areas with a droop angle ≤45°, the support type is selected as "tree support" to reduce material waste. An "adaptive mesh segmentation algorithm" is used to perform non-overlapping segmentation of single-layer slices according to the size of the rectangular light spot (if the edge area is less than one rectangle size, it is automatically adjusted to a smaller rectangle to avoid energy unevenness caused by light spot trimming). The scanning path is selected as "spiral path" to reduce galvanometer vibration error caused by abrupt changes in scanning direction, while also reducing heat accumulation between adjacent scanning lines.

[0019] A uniform rectangular light spot is modulated into a patterned light spot by a pattern modulation module. The light spot is then moved by a scanning module to a designated position on the processing table for processing. The scanning module is configured as a dual-mirror and a translation stage, and the combination of the two realizes the moving scanning function. When scanning a small area, the light spot is driven to move by the dual-mirror. When scanning a large area, the dual-mirror is responsible for local scanning, and the translation stage is responsible for overall displacement. Gaps caused by displacement errors are eliminated by splicing overlapping areas. In traditional substrate manufacturing, the continuous light patterning process requires prolonged heating (seconds or sub-seconds) to melt a large area of ​​powder. Heat can diffuse beyond the pre-set pattern via thermal conduction, leading to an enlarged molten area (i.e., an excessively large heat-affected zone) and ultimately reduced part dimensional accuracy. This solution addresses this by using continuous light output to preheat the laser powder to near its melting point without melting it, and pulsed light output to completely melt the preheated powder. In other words, continuous light is used only for short-term preheating, bringing the powder temperature close to its melting point without melting it. Subsequently, microsecond pulsed light rapidly provides peak energy, instantly melting the powder. This not only shortens the effective heating time but also controls the range of heat radiation. Because the system's heating time is much shorter than that of traditional continuous light (continuous "low-temperature heating"), heat does not have time to diffuse beyond the pre-set pattern before melting and solidification, thus limiting the molten area within the pattern and improving the subsequent part forming accuracy.

[0020] Furthermore, in traditional single-pulse patterning, extremely high pulse peak power (usually above kilowatts) is required to melt the powder in a short time. Strong light can easily cause aging and damage to optical components (such as lenses and modulators) in the optical path system, shortening their service life. This solution preheats the powder with continuous light, so that the powder is close to a molten state. At this time, the pulse hook only needs to provide a lower peak power to complete the melting. By reducing the power requirement of the pulse light peak, the energy impact on the optical components is reduced. Moreover, by using continuous light and pulse light to work in a time-division manner (light is emitted sequentially in a single cycle), the instantaneous high power caused by energy superposition is avoided, further reducing the risk of damage to the optical components and extending their service life.

[0021] This embodiment provides a continuous pulse hybrid patterned laser powder bed optical path method, including the following steps: S1: Set the thickness and rectangular segmentation size of the 3D structure slice to be processed, control the computer module to slice it, segment the single layer after slicing, and plan the scanning path; S2: Based on the thickness and size after segmentation, combined with the material properties of the powder to be printed and the laser properties, calculate the continuous light output power and continuous light output time, pulse light output power, pulse light output time and pulse number, laser properties including emission wavelength and wall insertion efficiency, and material properties including specific heat capacity, thermal conductivity, diffusivity and density of the printing powder. S3: Based on the sum of continuous light emission time and pulsed light emission time And determine the interval time based on the power modulation capability and the response capability of the scanning module. The power supply regulation frequency is determined based on the interval time and the total time. Specifically, this includes time based on total time. and interval time The processing cycle T for a single pattern is determined by the power supply regulation frequency: ; The adjustment frequency f of the power module is determined based on the processing cycle. ; And control the pattern switching frequency of the pattern modulation module and the motion frequency of the scanning module to keep them consistent with the adjustment frequency; S4: The power module modulates the output power waveform according to the parameters in step S3. Please refer to the output power waveform diagram. Figure 3 The mixed-emitting laser is supplied with light in a sequential and periodic manner. The mixed-emitting laser is modulated into a uniform rectangular spot by a homogenization and shaping module, and the size of the rectangular spot is controlled to be consistent with the size of the rectangular segmentation. S5: The computer module sends the segmented pattern to the pattern modulation module, and the rectangular light spot is modulated to form a high-power patterned light spot; S6: High-power patterned light spots move on the processing table via the scanning module and are scanned and stitched together to complete single-layer printing; S7: The processing table descends one layer. The thickness of the descending layer is set according to the slice thickness. Powder is re-spread, and processing is performed again according to the preset scanning path. Steps S6 and S7 are repeated to complete the processing of the entire part.

[0022] This method significantly reduces the risk of damage to optical components while ensuring high precision and high mechanical properties of printed parts, and balances processing efficiency and process stability, making it suitable for the large-scale and high-reliability requirements of industrial additive manufacturing.

[0023] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention in any way. Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art can make some modifications or alterations to the above-disclosed technical content to create equivalent embodiments without departing from the scope of the present invention. Any simple modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present invention without departing from the scope of the present invention shall still fall within the scope of the present invention.

Claims

1. A continuous pulse hybrid patterned laser powder bed optical path system, characterized in that: Includes a computer module, a power supply module, a hybrid laser, a homogenization and shaping module, a pattern modulation module, a scanning module, and a forming cylinder. The computer module controls the power module to output power through a set control program, and controls the hybrid laser with the power output. The hybrid laser emits light periodically in sequence to generate a beam; The homogenization and shaping module adjusts the beam generated by the hybrid laser into a rectangular uniform spot; The computer module slices the three-dimensional structure to be printed, divides the slices according to the size of the rectangular light spot, and sends the divided graphics to the pattern modulation module in sequence. A uniform rectangular light spot is modulated into a patterned light spot by a pattern modulation module, and then the light spot is moved by a scanning module to a designated position on the processing table for processing.

2. The continuous pulse hybrid patterned laser powder bed optical path system according to claim 1, characterized in that: The power module includes two independent logic paths; The logic path one includes a delay signal generator one, a continuous wave modulation module and a power amplifier one, which are connected in sequence by electrical connection. The second logic path includes a second delay signal generator, a second continuous wave modulation module, and a second power amplifier unit, which are connected in sequence.

3. The continuous pulse hybrid patterned laser powder bed optical path system according to claim 1, characterized in that: The operating logic of the power module is as follows: Delay signal generator one and delay signal generator two periodically send control signals in sequence. The signal sent by delay signal generator one enters the continuous wave modulation module and continuously outputs a high level. The signal sent by delay signal generator two enters the microsecond pulse modulation module two and intermittently outputs a pulse high level. The continuous high level enters the power amplification unit one, and the pulse high level enters the power amplification unit two.

4. The continuous pulse hybrid patterned laser powder bed optical path system according to claim 3, characterized in that: The output of the hybrid laser in a single cycle is used only for the melting and solidification of a single pattern, while the output in a continuous cycle is used to preheat the laser powder to its melting point without melting it, and the output in a pulse cycle is used to completely melt the preheated laser powder.

5. A continuous pulse hybrid patterned laser powder bed optical path method, applied to a continuous pulse hybrid patterned laser powder bed optical path system as described in any one of claims 1-4, characterized in that, Includes the following steps: S1: Set the thickness and rectangular segmentation size of the 3D structure slice to be processed, control the computer module to slice it, segment the single layer after slicing, and plan the scanning path; S2: Based on the thickness and size after segmentation, and combined with the material characteristics of the powder to be printed and the laser characteristics, calculate the power and duration of continuous light emission, the power, duration and number of pulsed light emission, and the laser characteristics including emission wavelength and wall insertion efficiency. S3: Determine the interval time based on the sum of the continuous light emission time and the pulse light emission time, as well as the power supply modulation capability and the response capability of the scanning module. Determine the power supply adjustment frequency based on the interval time and the sum of the time, and control the pattern switching frequency of the pattern modulation module and the motion frequency of the scanning module to be consistent with the adjustment frequency. S4: The power module modulates the output power waveform according to the parameters in step S3, and supplies the hybrid laser to emit light periodically in sequence. The hybrid laser is modulated into a uniform rectangular spot by the homogenization and shaping module, and the size of the rectangular spot is controlled to be consistent with the rectangular segmentation size. S5: The computer module sends the segmented pattern to the pattern modulation module, and the rectangular light spot is modulated to form a high-power patterned light spot; S6: High-power patterned light spots move on the processing table via the scanning module and are scanned and stitched together to complete single-layer printing; S7: The processing table descends one layer, the powder is re-spread, and the processing is carried out again according to the preset scanning path. Repeat steps S6 and S7 to complete the processing of the entire part.

6. The continuous pulse hybrid patterned laser powder bed optical path method according to claim 5, characterized in that: In S3, determining the adjustment frequency includes: The total time for calibrating continuous light emission time and pulsed light emission time is: and interval time The processing cycle T for a single pattern is determined as follows: ; The adjustment frequency f of the power module is determined based on the later stage of the processing. .

7. The continuous pulse hybrid patterned laser powder bed optical path method according to claim 6, characterized in that: The material properties include the specific heat capacity, thermal conductivity, diffusivity, and density of the printing powder.

8. The continuous pulse hybrid patterned laser powder bed optical path method according to claim 5, characterized in that: In S7, the layer thickness of the processing table descending one level is the slice thickness.

Citation Information

Patent Citations

  • Additive manufacturing system for 2D printing using pulsed lasers

    CN113226622B

  • Surface area printing system for laser additive manufacturing

    CN117884656A

Cited By

  • Method and equipment for inhibiting loss of reinforced particles in laser additive manufacturing metal matrix composite

    CN121988754A