A filter coating composition for fluorescence detection and its preparation method

By using a composite of mesoporous silica and nano-barium titanate powder doped with rare earth elements, the problems of dispersion and UV aging resistance of existing filters have been solved, resulting in filters with high selective optical performance and long lifespan, suitable for in vitro diagnostics in the field of biological detection.

CN122080559APending Publication Date: 2026-05-26SHENZHEN DALU BIOTECHNOLOGY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202610259263.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-03-04
Publication Date
2026-05-26

AI Technical Summary

Technical Problem

Existing fluorescent filters suffer from poor dispersion, poor spectral selectivity, and weak resistance to ultraviolet aging, making it difficult to meet the special needs of biological detection, especially in the field of in vitro diagnostics.

Method used

A composite of mesoporous silica powder and nano-barium titanate powder, doped with rare earth elements, and combined with polymer substrate, dispersant, plasticizer and anti-UV additives, is used to prepare filters through modification, mixing and granulation and vacuum evaporation processes to improve flexibility, optical performance and weather resistance.

Benefits of technology

It achieves highly selective optical performance, effectively filters excitation light and stray light, improves detection sensitivity and accuracy, extends filter life, reduces production costs, and is suitable for large-scale production of in vitro diagnostic reagents.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122080559A_ABST
    Figure CN122080559A_ABST
Patent Text Reader

Abstract

This invention discloses a filter coating composition for fluorescence detection and its preparation method, relating to the fields of optical materials and biodetection technology. The composition is formulated by compounding optical functional powders, polymer substrates, dispersants, and additives in specific proportions, exhibiting high transmittance, narrow wavelength selectivity, excellent weather resistance and mechanical stability. It can accurately filter excitation light and stray light, improving the sensitivity and specificity of fluorescence detection. The filter coating composition and its preparation method for fluorescence detection also provide a simple, cost-effective manufacturing process suitable for large-scale production, particularly applicable to gene sequencing and immunochemistry. It addresses the problems of poor wavelength selectivity, weak stability, and high cost associated with traditional filters, making it suitable for fluorescence detection scenarios such as Alzheimer's disease biomarkers. Balancing accuracy, stability, and economy, it has broad application prospects in the field of in vitro diagnostic reagents.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the fields of optical materials and biological detection technology, specifically to a filter coating composition for fluorescence detection and its preparation method. Background Technology

[0002] Fluorescence detection technology, due to its advantages of high sensitivity, strong specificity, and ease of operation, is widely used in biomedicine, environmental monitoring, food safety, and other fields. In the early diagnosis of neurodegenerative diseases such as Alzheimer's disease, fluorescence detection is often combined with electrochemical technology to achieve accurate quantification of biomarkers such as Aβ and p-tau. As the core optical component of the fluorescence detection system, the performance of the filter directly determines the accuracy of the detection results. It needs to achieve narrow-band selectivity of "high excitation light cutoff and high emission light transmittance," while also possessing good mechanical strength and weather resistance to meet the requirements of large-scale production and long-term storage of in vitro diagnostic reagents.

[0003] In the prior art, such as the ultraviolet fluorescent filter and its preparation method disclosed in application number 201310450681.7, the technical solution is as follows: the ultraviolet fluorescent filter can be used for skin damage detection. The ultraviolet fluorescent filter includes a substrate and a (G(0.5HL0.5H)^sA) film system. The (G(0.5HL0.5H)^sA) film system is deposited on the substrate. The ultraviolet fluorescent filter has high transmittance in the range of 330nm to 400nm and is cut off in two wavelength bands: 290nm to 310nm and 410nm to 780nm. The substrate is K9 glass. The (G(0.5HL0.5H)^sA) film system is composed of multiple high refractive index film layers and low refractive index film layers. The high refractive index film layer is made of Ta2O5, and the low refractive index film layer is made of SiO2.

[0004] Traditional fluorescent filters are mostly fabricated using glass substrate coating processes, which suffer from drawbacks such as high cost, poor flexibility, and fragility. While polymer-based filters offer advantages in flexibility and ease of processing, they generally suffer from poor dispersion of optical functional powders, poor wavelength selectivity, and weak resistance to UV aging. Furthermore, the formulation design of existing filter compositions does not fully consider the specific needs of biological detection, making it difficult to match the wavelength parameters of fluorescence detection systems and limiting their application in in vitro diagnostics. Therefore, developing a highly selective, highly stable, and low-cost fluorescent filter composition is of significant practical importance.

[0005] In view of this, in-depth research was conducted on the above issues, which led to the creation of this case. Summary of the Invention

[0006] The purpose of this invention is to provide a filter coating composition for fluorescence detection and its preparation method, so as to solve the problems of poor dispersibility, poor band selectivity and weak UV aging resistance mentioned in the background art.

[0007] To achieve the above objectives, the present invention provides the following technical solution: A filter coating composition for fluorescence detection, comprising optical functional powder, polymer substrate, dispersant, plasticizer, and UV-resistant additive, wherein the filter coating composition comprises, by weight, 25-40 parts of optical functional powder, 50-65 parts of polymer substrate, 2-5 parts of dispersant, 1-3 parts of plasticizer, and 0.5-2 parts of UV-resistant additive, wherein the optical functional powder is a compound of mesoporous silica powder and nano-barium titanate powder, wherein the mesoporous silica powder is doped with rare earth elements, and the mass ratio of mesoporous silica powder to nano-barium titanate powder is (3-5):1, wherein the rare earth elements are Eu³⁺ or Tb³⁺, and the doping amount of rare earth elements is 0.8%-1.5% of the mass of the mesoporous silica powder.

[0008] Preferably, the polymer substrate is a blend of one or more of polycarbonate (PC), polymethyl methacrylate (PMMA), or cyclic olefin copolymer (COC).

[0009] Using the above technical solutions, the polymer substrates of polycarbonate (PC) / polymethyl methacrylate (PMMA) / cyclic olefin copolymer (COC) alone or in blends, compared with glass substrates, have improved filter flexibility, reduced breakage rate, and the blended substrates are suitable for different processing scenarios. The temperature resistance range is expanded to -40℃ to 120℃, making them suitable for long-term operation of fluorescence detection equipment. The cyclic olefin copolymer (COC) has advantages such as low birefringence, high transmittance, and chemical corrosion resistance, making it suitable for applications of biological detection reagents.

[0010] Preferably, the dispersant is a silane coupling agent KH-550 or KH-570, the plasticizer is dioctyl phthalate (DOP) or tributyl citrate (TBC), and the UV-resistant additive is nano zinc oxide or benzotriazole UV absorber UV-327.

[0011] Using the above technical solution, the silane coupling agent KH-550 / KH-570 dispersant improves the dispersion uniformity of optical functional powders, the dioctyl phthalate (DOP) / tributyl citrate (TBC) plasticizer increases the filter forming rate, and the nano zinc oxide / UV-327 anti-ultraviolet additive extends the aging resistance and lifespan of the filter.

[0012] Preferably, the pore size of the mesoporous silica powder is 5-20 nm, and the specific surface area of ​​the mesoporous silica powder is ≥300 m² / g, the particle size of the nano barium titanate powder is 20-50 nm, and the purity of the nano barium titanate powder is ≥99.5%.

[0013] By adopting the above technical solutions, mesoporous silica powder with a pore size of 5-20nm and a specific surface area of ​​≥300m² / g exhibits improved fluorescence enhancement, while nano-barium titanate powder with a particle size of 20-50nm and a purity of ≥99.5% improves the accuracy of the filtering band, ensuring the accuracy of the detection signal.

[0014] Preferably, the filter prepared by the filter coating composition is used to filter excitation light and stray light in the fluorescence detection system, with an applicable excitation wavelength range of 365-488nm and an emission wavelength range of 520-650nm.

[0015] Using the above technical solution, the filter is adapted to excitation wavelengths of 365-488nm and emission wavelengths of 520-650nm, improving stray light filtration efficiency, accurately matching the fluorescence detection system, improving detection sensitivity, and avoiding interference of excitation light with detection results.

[0016] Preferably, the fluorescence detection system is an electrochemical-fluorescence combined detection system for Alzheimer's disease biomarkers Aβ and p-tau.

[0017] By adopting the above technical solution, an electrochemical-fluorescence joint detection system for Alzheimer's disease biomarkers Aβ and p-tau is specifically adapted, which improves the detection specificity, accurately filters out interfering wavelengths in the system, improves the accuracy of detection results, and meets the needs of precise detection in in vitro diagnostics.

[0018] A method for preparing a filter coating composition for fluorescence detection, the method comprising the following steps: Step 1, Modification of optical functional powder: Mesoporous silica powder is dispersed in anhydrous ethanol and ultrasonically dispersed for 10 min to form a suspension. Rare earth nitrate solution is added, and the pH is adjusted to 8-9. The mixture is stirred at a constant temperature of 50-60℃ for 2-3 h. After stirring, the mixture is centrifuged, washed, and dried to obtain rare earth-doped mesoporous silica powder. The rare earth-doped mesoporous silica powder is mixed with nano barium titanate powder, and after adding a dispersant, it is ultrasonically dispersed for 30-40 min to obtain modified optical functional powder. Step 2, mixing and granulation: Add the polymer matrix, modified optical functional powder, plasticizer, and UV-resistant additive to a high-speed mixer and mix at a speed of 1000-1500 r / min for 15-20 min. Then, granulate the mixture through a twin-screw extruder at an extrusion temperature of 180-220℃ to obtain filter masterbatch. Step 3, molding and coating: The filter masterbatch obtained in step 2 is dried and injection molded to obtain the filter substrate with a thickness of 0.3-1.0 mm. A layer of silicon dioxide antireflection film with a thickness of 50-100 nm is vacuum evaporated on the surface of the substrate to obtain the finished filter.

[0019] Preferably, the rare earth nitrate solution in step one is europium nitrate solution or terbium nitrate solution with a concentration of 0.1-0.2 mol / L, and the pH is adjusted by adding ammonia. The washing after stirring is performed with anhydrous ethanol 3-4 times, the drying temperature is 80℃, and the vacuum drying time is 12h.

[0020] Using the above technical solution, a 0.1-0.2 mol / L europium nitrate / terbium nitrate solution is used to improve the uniformity of rare earth doping. Ammonia water is used to adjust the pH and anhydrous ethanol is used for washing to improve the purity of the powder. The powder is then vacuum dried at 80℃ for 12 hours to avoid powder agglomeration and ensure consistency in subsequent processing.

[0021] Preferably, in step two, the twin-screw extruder includes a first extrusion zone, a second extrusion zone, and a third extrusion zone, with the temperature of the first extrusion zone being 180°C, the temperature of the second extrusion zone being 200°C, and the temperature of the third extrusion zone being 220°C.

[0022] By adopting the above technical solution, the twin-screw extruder has three-stage temperature control, which improves the uniformity of material melting, avoids the degradation of polymer substrates by segmented temperature control, improves the stability of optical performance of filters, and reduces transmittance fluctuations.

[0023] Preferably, in step three, the filter masterbatch obtained in step two is dried by forced air at 80°C for 4 hours, the injection molding temperature is 200-230°C, the mold temperature is 50-60°C, the vacuum degree of vacuum evaporation is 1×10⁻³-5×10⁻³Pa, and the evaporation temperature is 100-150°C.

[0024] Using the above technical solution, drying at 80℃ for 4 hours reduces the moisture content of the filter masterbatch and the bubble rate during injection molding. The injection molding temperature of 200-230℃ combined with the mold temperature of 50-60℃ improves the flatness of the substrate. The vacuum degree of 1×10⁻³-5×10⁻³Pa and the evaporation temperature of 100-150℃ improve the adhesion of the silica antireflective film and reduce the film peeling rate.

[0025] Compared with the prior art, the beneficial effects of the present invention are: the filter coating composition for fluorescence detection and its preparation method, 1. Excellent optical performance ensures accurate fluorescence detection: Through the composite design of "rare earth element (Eu³⁺ / Tb³⁺) doped mesoporous silica powder and nano barium titanate powder (mass ratio 3-5:1)," a highly selective optical system is constructed. The filter has a cutoff rate of ≥99% for 365-488nm excitation light, which can effectively block the excitation light from entering the detection optical path. The transmittance of ≥99% for 520-650nm emission light ensures efficient transmission of target fluorescence signal. The narrow band selective design makes the stray light filtering rate ≤0.1%, which improves the fluorescence detection sensitivity. It is especially suitable for the electrochemical-fluorescence joint detection of Alzheimer's disease biomarkers Aβ and p-tau, effectively eliminating interference signals and improving the accuracy of detection results. 2. Strong environmental and mechanical stability, suitable for long-term use: The formula adds nano zinc oxide or benzotriazole UV-327 anti-ultraviolet additives, combined with dioctyl phthalate (DOP) or tributyl citrate (TBC) plasticizers, forming a double stabilizing protection. After being placed under accelerated aging conditions of 50℃ and 85% relative humidity for 6 months, the transmittance of emitted light of the filter decreases by ≤2%, the excitation light cutoff decreases by ≤1%, and the optical performance does not deteriorate significantly. The polymer substrate and optical functional powder work together to make the filter flexural strength ≥50MPa and impact strength ≥20kJ / m². The mechanical strength meets the requirements of large-scale processing and long-term storage of in vitro diagnostic reagents, and the breakage rate is reduced from 20% of traditional glass filters to ≤0.1%.

[0026] 3. Simple and efficient preparation process, reducing production costs and barriers to entry: The integrated process of "optical functional powder modification → mixing and granulation → injection molding → vacuum evaporation" is adopted: ultrasonic dispersion ensures uniform powder dispersion, twin-screw three-stage temperature-controlled extrusion achieves full melting of materials, injection molding quickly prepares 0.3-1.0mm thick substrates, and finally vacuum evaporation deposits a 50-100nm silica antireflective film, which improves production efficiency by 150% and eliminates the need for expensive glass processing equipment, reducing production costs by 30%-50%, making it suitable for large-scale production by small and medium-sized enterprises and lowering the application threshold for high-selectivity filters. Attached Figure Description

[0027] Figure 1 This is the absorption curve of the 1% DMF dye solution of the present invention at 400-650 nm. Figure 2 This is a transmittance curve of the 562nm long-wavelength pass coating of the present invention; Figure 3 This is a lensless fluorescence imaging image of the sensor with the fluorescent coating of the present invention. Detailed Implementation

[0028] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0029] Please see Figure 1-3 The present invention provides a technical solution: A filter coating composition for fluorescence detection, comprising optical functional powder, polymer substrate, dispersant, plasticizer, and UV-resistant additive, wherein the filter coating composition comprises, by weight, 25-40 parts of optical functional powder, 50-65 parts of polymer substrate, 2-5 parts of dispersant, 1-3 parts of plasticizer, and 0.5-2 parts of UV-resistant additive, wherein the optical functional powder is a compound of mesoporous silica powder and nano-barium titanate powder, wherein the mesoporous silica powder is doped with rare earth elements, and the mass ratio of mesoporous silica powder to nano-barium titanate powder is (3-5):1, the rare earth elements are Eu³⁺ or Tb³⁺, and the doping amount of rare earth elements is 0.8%-1.5% of the mass of mesoporous silica powder.

[0030] The polymer substrate is a blend of one or more of polycarbonate (PC), polymethyl methacrylate (PMMA), or cyclic olefin copolymer (COC). Compared with glass substrates, the polymer substrates of polycarbonate (PC), polymethyl methacrylate (PMMA), and cyclic olefin copolymer (COC) alone or in blend form offer improved filter flexibility and reduced breakage rate. The blended substrates are suitable for different processing scenarios and have an expanded temperature resistance range of -40℃ to 120℃, making them suitable for long-term operation of fluorescence detection equipment. Cyclic olefin copolymer (COC) has advantages such as low birefringence, high transmittance, and resistance to chemical corrosion, making it suitable for applications in biological detection reagents.

[0031] The dispersant is silane coupling agent KH-550 or KH-570, the plasticizer is dioctyl phthalate (DOP) or tributyl citrate (TBC), and the UV absorber is nano zinc oxide or benzotriazole UV absorber UV-327. The silane coupling agent KH-550 / KH-570 dispersant improves the uniformity of optical functional powder dispersion. The dioctyl phthalate (DOP) / tributyl citrate (TBC) plasticizer improves the filter forming rate. The nano zinc oxide / UV-327 UV absorber extends the aging resistance and lifespan of the filter.

[0032] Mesoporous silica powder has a pore size of 5-20 nm and a specific surface area ≥300 m² / g. Barium titanate nanoparticles have a particle size of 20-50 nm and a purity ≥99.5%. Mesoporous silica powder with a pore size of 5-20 nm and a specific surface area ≥300 m² / g exhibits improved fluorescence enhancement, while barium titanate nanoparticles with a particle size of 20-50 nm and a purity ≥99.5% offer improved filtering band precision, ensuring accurate detection signals.

[0033] The filter, prepared from the filter coating composition, is used to filter excitation and stray light in the fluorescence detection system. It is suitable for excitation wavelengths of 365-488 nm and emission wavelengths of 520-650 nm. The fluorescence detection system is an electrochemical-fluorescence co-detection system for Alzheimer's disease biomarkers Aβ and p-tau. The filter is adapted to excitation wavelengths of 365-488 nm and emission wavelengths of 520-650 nm, improving stray light filtration efficiency, accurately matching the fluorescence detection system, increasing detection sensitivity, avoiding interference from excitation light, and specifically adapting to the electrochemical-fluorescence co-detection system for Alzheimer's disease biomarkers Aβ and p-tau. This improves detection specificity, accurately filters interfering wavelengths in the system, and enhances the accuracy of detection results, meeting the needs of precise in vitro diagnostic testing.

[0034] A method for preparing a filter coating composition for fluorescence detection, comprising the following steps: Step 1, Modification of optical functional powder: Mesoporous silica powder is dispersed in anhydrous ethanol and ultrasonically dispersed for 10 min to form a suspension. Rare earth nitrate solution is added, and the pH is adjusted to 8-9. The mixture is stirred at a constant temperature of 50-60℃ for 2-3 h. After stirring, the mixture is centrifuged, washed, and dried to obtain rare earth-doped mesoporous silica powder. The rare earth-doped mesoporous silica powder is mixed with nano barium titanate powder, and after adding a dispersant, it is ultrasonically dispersed for 30-40 min to obtain modified optical functional powder. Step 2, mixing and granulation: Add the polymer matrix, modified optical functional powder, plasticizer, and UV-resistant additive to a high-speed mixer and mix at a speed of 1000-1500 r / min for 15-20 min. Then, granulate the mixture through a twin-screw extruder at an extrusion temperature of 180-220℃ to obtain filter masterbatch. Step 3, molding and coating: The filter masterbatch obtained in step 2 is dried and injection molded to obtain the filter substrate with a thickness of 0.3-1.0 mm. A layer of silicon dioxide antireflection film with a thickness of 50-100 nm is vacuum evaporated on the surface of the substrate to obtain the finished filter.

[0035] In step one, the rare earth nitrate solution is either europium nitrate or terbium nitrate solution with a concentration of 0.1-0.2 mol / L. The pH is adjusted by adding ammonia. After stirring, the mixture is washed 3-4 times with anhydrous ethanol. The drying temperature is 80℃, and the vacuum drying time is 12 hours. In step two, the twin-screw extruder includes a first extrusion zone, a second extrusion zone, and a third extrusion zone. The temperature of the first extrusion zone is 180℃, the temperature of the second extrusion zone is 200℃, and the temperature of the third extrusion zone is 220℃. In step three, the filter masterbatch obtained in step two is dried by forced air at 80℃ for 4 hours. The injection molding temperature is 200-230℃, the mold temperature is 50-60℃, the vacuum degree of vacuum evaporation is 1×10⁻³-5×10⁻³ Pa, and the evaporation temperature is 100- At 150℃, a 0.1-0.2mol / L europium nitrate / terbium nitrate solution was used to improve the uniformity of rare earth doping. Ammonia was used to adjust the pH, and anhydrous ethanol was used for washing to improve powder purity. Vacuum drying at 80℃ for 12 hours prevented powder agglomeration and ensured consistency in subsequent processing. Three-stage temperature control in a twin-screw extruder improved the uniformity of material melting. Segmented temperature control prevented degradation of the polymer substrate, improving the stability of the filter's optical performance and reducing transmittance fluctuations. Blow-drying at 80℃ for 4 hours reduced the moisture content of the filter masterbatch and decreased the bubble rate during injection molding. An injection temperature of 200-230℃ combined with a mold temperature of 50-60℃ improved substrate flatness. A vacuum of 1×10⁻³-5×10⁻³Pa and a vapor deposition temperature of 100-150℃ improved the adhesion of the silica antireflective film and reduced film peeling rate.

[0036] Example 1 A filter coating composition for fluorescence detection, comprising, by weight parts: 24 parts of Eu³⁺-doped mesoporous silica powder, 6 parts of nano-barium titanate powder, 60 parts of COC substrate, 3 parts of KH-570 dispersant, 2 parts of TBC plasticizer, and 1 part of UV-327 anti-ultraviolet additive; wherein the doping amount of Eu³⁺ is 1.0% of the mass of the mesoporous silica powder.

[0037] The preparation method is as follows: Step 1: Disperse 24 parts of mesoporous silica powder in 200 mL of anhydrous ethanol and sonicate for 10 min; add 15 mL of 0.15 mol / L europium nitrate solution, adjust the pH to 8.5 with ammonia water, and stir at 55℃ for 2.5 h; centrifuge, wash, and dry to obtain Eu³⁺-doped mesoporous silica powder; mix with 6 parts of nano barium titanate powder, add 3 parts of KH-570, and sonicate at 400 W for 35 min to obtain modified optical functional powder; Step 2: Add the modified powder, 60 parts of COC base material, 2 parts of TBC, and 1 part of UV-327 to a high-speed mixer and mix at 1200 r / min for 18 min; extrude and granulate using a twin-screw extruder with extrusion temperatures of 180℃ in zone 1, 200℃ in zone 2, and 220℃ in zone 3, and a screw speed of 250 r / min.

[0038] Step 3: After drying the masterbatch at 80℃ for 4 hours, it is injection molded at 210℃ and mold temperature at 55℃ to obtain a 0.5mm thick substrate; a silica antireflective film is vacuum-deposited at a vacuum degree of 3×10⁻³Pa and a deposition temperature of 120℃ to obtain a film thickness of 80nm, thus obtaining the filter.

[0039] Example 2 A filter composition for fluorescence detection, comprising, by weight parts: 30 parts of Tb³⁺-doped mesoporous silica powder, 7.5 parts of nano-barium titanate powder, 55 parts of PMMA substrate, 4 parts of KH-550 dispersant, 2 parts of DOP plasticizer, and 1.5 parts of nano-zinc oxide UV-resistant additive; wherein the Tb³⁺ doping amount is 1.2% of the mass of the mesoporous silica powder.

[0040] The preparation method is basically the same as in Example 1, except that in step one, the rare earth nitrate solution is terbium nitrate solution with a concentration of 0.2 mol / L and pH adjusted to 9; in step three, the injection molding temperature is 220℃ and the vapor deposition film thickness is 100 nm.

[0041] Performance test results: The optical performance and stability of the filters prepared in Examples 1 and 2 were tested. The industry standard for excitation cutoff rate (488nm) is ≥98%; The industry standard for emitted light transmittance (550nm) is ≥85%; The industry standard for weather resistance (transmittance retention rate after 6 months) is ≥90%. The excitation cutoff rate (488nm) of Example 1 is 99.5%, the emitted light transmittance (550nm) is 92%, and the weather resistance (transmittance retention rate after 6 months) is 98%. The excitation cutoff rate (488nm) of Example 2 is 99.3%, the emission transmittance (550nm) is 91%, and the weather resistance (transmittance retention rate after 6 months) is 97%.

[0042] Industrial applicability:

[0043] The filter composition prepared by this invention can be mass-produced through injection molding. The finished filter can be directly integrated into devices such as fluorescence detection chips, enzyme-linked immunosorbent assay (ELISA) readers, and electrochemical-fluorescence coupled detectors. It is especially suitable for in vitro diagnostic detection of Alzheimer's disease biomarkers such as Aβ and p-tau, and has significant economic and social value.

[0044] The contents not described in detail in this specification are existing technologies known to those skilled in the art.

[0045] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1. A filter coating composition for fluorescence detection, characterized in that: The optical filter coating composition comprises optical functional powder, polymer substrate, dispersant, plasticizer, and UV-resistant additive. The optical filter coating composition, by weight, comprises: 25-40 parts optical functional powder, 50-65 parts polymer substrate, 2-5 parts dispersant, 1-3 parts plasticizer, and 0.5-2 parts UV-resistant additive. The optical functional powder is a compound of mesoporous silica powder and nano-barium titanate powder, and the mesoporous silica powder is doped with rare earth elements. The mass ratio of mesoporous silica powder to nano-barium titanate powder is (3-5):

1. The rare earth elements are Eu³⁺ or Tb³⁺, and the doping amount of the rare earth elements is 0.8%-1.5% of the mass of the mesoporous silica powder.

2. The filter coating composition for fluorescence detection according to claim 1, characterized in that: The polymer substrate is one or more blends of polycarbonate (PC), polymethyl methacrylate (PMMA), or cyclic olefin copolymer (COC).

3. The filter coating composition for fluorescence detection according to claim 1, characterized in that: The dispersant is a silane coupling agent KH-550 or KH-570, the plasticizer is dioctyl phthalate (DOP) or tributyl citrate (TBC), and the UV-resistant additive is nano zinc oxide or benzotriazole UV absorber UV-327.

4. The filter coating composition for fluorescence detection according to claim 1, characterized in that: The mesoporous silica powder has a pore size of 5-20 nm and a specific surface area of ​​≥300 m² / g. The nano barium titanate powder has a particle size of 20-50 nm and a purity of ≥99.5%.

5. The filter coating composition for fluorescence detection according to claim 1, characterized in that: The filter prepared by the filter coating composition is used to filter excitation light and stray light in the fluorescence detection system. The applicable excitation wavelength range is 365-488nm, and the emission wavelength range is 520-650nm.

6. The filter coating composition for fluorescence detection according to claim 5, characterized in that: The fluorescence detection system is an electrochemical-fluorescence combined detection system for Alzheimer's disease biomarkers Aβ and p-tau.

7. A method for preparing a filter coating composition for fluorescence detection according to any one of claims 1-6, characterized in that: The method for preparing the filter coating composition includes the following steps: Step 1, Modification of optical functional powder: Mesoporous silica powder is dispersed in anhydrous ethanol and ultrasonically dispersed for 10 min to form a suspension. Rare earth nitrate solution is added, and the pH is adjusted to 8-9. The mixture is stirred at a constant temperature of 50-60℃ for 2-3 h. After stirring, the mixture is centrifuged, washed, and dried to obtain rare earth-doped mesoporous silica powder. The rare earth-doped mesoporous silica powder is mixed with nano barium titanate powder, and after adding a dispersant, it is ultrasonically dispersed for 30-40 min to obtain modified optical functional powder. Step 2, mixing and granulation: Add the polymer matrix, modified optical functional powder, plasticizer, and UV-resistant additive to a high-speed mixer and mix at a speed of 1000-1500 r / min for 15-20 min. Then, granulate the mixture through a twin-screw extruder at an extrusion temperature of 180-220℃ to obtain filter masterbatch. Step 3, molding and coating: The filter masterbatch obtained in step 2 is dried and injection molded to obtain the filter substrate with a thickness of 0.3-1.0 mm. A layer of silicon dioxide antireflection film with a thickness of 50-100 nm is vacuum evaporated on the surface of the substrate to obtain the finished filter.

8. The method for preparing the filter coating composition for fluorescence detection according to claim 7, characterized in that: The rare earth nitrate solution in step one is europium nitrate solution or terbium nitrate solution with a concentration of 0.1-0.2 mol / L. The pH is adjusted by adding ammonia. After stirring, the solution is washed 3-4 times with anhydrous ethanol. The drying temperature is 80℃ and the vacuum drying time is 12h.

9. The method for preparing the filter coating composition for fluorescence detection according to claim 7, characterized in that: In step two, the twin-screw extruder includes a first extrusion zone, a second extrusion zone, and a third extrusion zone, with the temperature of the first extrusion zone being 180°C, the temperature of the second extrusion zone being 200°C, and the temperature of the third extrusion zone being 220°C.

10. The method for preparing the filter coating composition for fluorescence detection according to claim 7, characterized in that: In step three, the filter masterbatch obtained in step two is dried by forced air at 80°C for 4 hours. The injection molding temperature is 200-230°C, the mold temperature is 50-60°C, the vacuum degree of vacuum evaporation is 1×10⁻³-5×10⁻³Pa, and the evaporation temperature is 100-150°C.

Citation Information

Patent Citations

  • Ultraviolet fluorescent light filter and preparation method thereof