Integrally die-cast metal single plate and method of manufacturing the same

By using integrated die-casting technology, the problems of long production cycle and unstable quality in aluminum single-panel curtain wall manufacturing have been solved, realizing efficient, low-carbon and environmentally friendly aluminum single-panel manufacturing, improving the product's impact resistance, wind pressure resistance and aesthetics, and reducing errors and scrap rate.

CN122257550APending Publication Date: 2026-06-23SICHUAN GOME TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610394263.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-03-28
Publication Date
2026-06-23

AI Technical Summary

Technical Problem

The existing aluminum single-panel curtain wall manufacturing process has a long production cycle and many production steps, which poses risks of welding stress concentration and desoldering, unstable assembly quality, large geometric dimensional errors, poor surface flatness, poor interchangeability, and large material waste.

Method used

Employing integrated die-casting technology, the plate surface, ribs, side edges, and connectors are integrally formed using a large vacuum die-casting machine. Combined with laser trimming and spraying, a cross-distributed rib structure is created, eliminating the need for welding.

Benefits of technology

It significantly shortens the production cycle, improves the flatness and consistency of products, enhances impact resistance and wind pressure resistance, reduces errors and scrap rates, and improves aesthetics and environmental friendliness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122257550A_ABST
    Figure CN122257550A_ABST
Patent Text Reader

Abstract

The application discloses an integrally die-casting metal single plate and a manufacturing method thereof. The metal single plate comprises a plate surface, the back surface of the plate surface is provided with ribs, the peripheral edge of the plate surface is provided with a side wall bent to the back surface, and a connecting piece is arranged on the peripheral side wall. The plate surface, the ribs, the side wall and the connecting piece are integrally die-cast. The application solves the problems of long processing and production period, many production links, unstable assembly quality, large geometric dimension error, poor surface flatness, poor interchangeability and large material loss of the existing metal single plate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of building curtain wall technology, specifically to an integral die-cast metal panel and its manufacturing method. Background Technology

[0002] Aluminum single-panel curtain walls are a common building curtain wall panel material. Currently, the production of aluminum single-panel curtain walls requires purchasing aluminum sheets from manufacturers (aluminum sheet manufacturers purchase aluminum ingots, heat them to 500-600°C to soften them, and repeatedly roll them through a hot rolling mill to press them into thicker sheets, which are then cold-rolled into thinner sheets). The sheets are then cut, bent, and framed, with ribs welded to the back of the aluminum single-panel and connectors welded around the perimeter. This process has a long production cycle, many production steps, stress concentration during rib and connector welding, a risk of weld failure, unstable assembly quality, large geometric dimensional errors, poor weld surface flatness, poor interchangeability, and approximately 5% scrap aluminum is generated. Summary of the Invention

[0003] To address the shortcomings of existing technologies, this invention provides an integral die-cast metal veneer and its manufacturing method, thereby solving the problems of long processing and production cycles, numerous production steps, unstable assembly quality, large geometric dimensional errors, poor surface flatness, poor interchangeability, and high material loss in existing metal veneer manufacturing processes.

[0004] On one hand, the present invention provides an integral die-cast metal single plate, including a plate surface, ribs distributed on the back side of the plate surface, side edges bent towards the back side of the plate surface, and connecting parts provided on the side edges around the perimeter. The plate surface, ribs, side edges and connecting parts are integrally die-cast.

[0005] Furthermore, the ribs on the back side of the plate are distributed in a crisscross pattern.

[0006] Furthermore, the ribs on the back of the plate are arranged in a crisscross pattern to form a rectangular grid.

[0007] Furthermore, the ribs on the back of the plate are arranged longitudinally and diagonally to form a parallelogram grid.

[0008] Furthermore, the metal panel is made of aluminum.

[0009] Furthermore, the connector is an L-shaped connector, with one side of the L-shaped connector connected to the side wall edge, and the other side of the L-shaped connector bent outward and provided with a connection hole.

[0010] On the other hand, the present invention provides a method for manufacturing an integrally die-cast metal single plate, comprising the following steps: Step S10: The alloy ingot is melted into a liquid state; Step S20: The molten liquid alloy is injected into a special mold cavity through a large vacuum die casting machine and solidified and cooled. Step S30: The formed blank is taken out and trimmed and corrected by a trimming and correction mold; Step S40: Use blue light to inspect the blank for defects such as cracks; Step S50: Perform laser trimming on the blank; Step S60: Spray coating is applied to the blank to obtain the final product; Step S70: Conduct an overall quality inspection of the product; Step S80: Package the product.

[0011] The beneficial effects of this invention are reflected in: 1. The metal single panel is integrally die-cast, with the panel surface, ribs, side edges and connectors forming the whole, eliminating the corner assembly and welding process, thus solving the risk of production deformation; 2. The production cycle is greatly shortened, eliminating the aluminum rod production process, extrusion process, and welding process; 3. It solves the problems of poor surface flatness and aesthetics, and significantly improves the appearance; 4. The ribs intersect in a cross pattern, which significantly improves the impact resistance and wind pressure resistance while significantly reducing the thickness; 5. Due to its integral casting process, the compressive strength, yield strength, wind pressure resistance, sound insulation, and thermal insulation performance are significantly improved. 6. Due to the one-time molding process, the error of metal panels for curtain walls of the same specifications is almost zero, and the production error standard of the product is more than 100% higher than the national standard. 7. The products have good consistency and interchangeability, and almost no metal waste is generated.

[0012] 8. The production process is more low-carbon and environmentally friendly. Attached Figure Description

[0013] To more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the accompanying drawings used in the description of the specific embodiments or the prior art will be briefly introduced below. In all the drawings, similar elements or parts are generally identified by similar reference numerals. In the drawings, the elements or parts are not necessarily drawn to scale.

[0014] Figure 1 This is a schematic diagram of the structure of an integral die-cast metal single plate provided in an embodiment of the present invention; Figure 2 This is a schematic diagram of the structure of an integral die-cast metal single plate provided in another embodiment of the present invention; Figure 3A manufacturing process diagram of an integral die-cast metal single plate provided for an embodiment of the present invention.

[0015] In the attached diagram, 100 is the plate surface; 200 is the rib; 300 is the edging; 400 is the connector; and 410 is the connecting hole. Detailed Implementation

[0016] The embodiments of the technical solution of the present invention will now be described in detail with reference to the accompanying drawings. These embodiments are merely illustrative of the technical solution of the present invention and are therefore intended to limit the scope of protection of the present invention.

[0017] It should be noted that, unless otherwise stated, the technical or scientific terms used in this application should have the ordinary meaning as understood by one of ordinary skill in the art to which this invention pertains.

[0018] like Figure 1 and Figure 2 As shown, this embodiment of the invention provides an integral die-cast metal panel, including a panel 100, ribs 200 distributed on the back of the panel 100, a side edge 300 bent towards the back around the periphery of the panel 100, and a connector 400 provided on the side edge 300 around the periphery. The panel 100, ribs 200, side edge 300 and connector 400 are integrally die-cast.

[0019] In this embodiment, the plate 100 and the rib 200 are die-cast as a single unit, which improves the overall strength and eliminates the risk of welding deformation.

[0020] In a preferred embodiment, the ribs 200 on the back of the panel 100 are crisscrossed, which significantly improves the impact resistance and wind pressure resistance while significantly reducing the thickness.

[0021] Optionally, such as Figure 1 As shown, the ribs 200 on the back of the panel 100 are arranged in a crisscross pattern to form a rectangular grid.

[0022] Optionally, such as Figure 2 As shown, the ribs 200 on the back of the panel 100 are arranged longitudinally and diagonally to form a parallelogram grid.

[0023] It is understandable that the arrangement of ribs 200 is not limited to Figure 1 and Figure 2 In addition to the two methods, other intersecting shapes should also be included in the protection scope of this embodiment. For example, the ribs 200 on the back of the plate 100 are distributed in a regular hexagonal shape, and the ribs 200 on the back of the plate 100 are wavy and intersecting in both directions.

[0024] In a preferred embodiment, the metal panel is made of aluminum.

[0025] It is understood that in other embodiments, the metal panel may also be made of stainless steel or other alloys.

[0026] In a preferred embodiment, the connector 400 is an L-shaped connector. One side of the L-shaped connector is connected to the side edge 300, and the other side of the L-shaped connector is bent outward and provided with a connecting hole 410. The connecting hole 410 is used for connecting screws to pass through, so as to fix the metal single-panel curtain wall to the curtain wall keel.

[0027] like Figure 3 As shown in the figure, this embodiment of the invention also provides a method for manufacturing an integrally die-cast metal single plate, including the following steps: Step S10: The alloy ingot is melted into a liquid state. The alloy ingot is an aluminum alloy, and the temperature is maintained at around 660°C after melting. Step S20: The molten liquid alloy is injected into a special mold cavity through a large vacuum die casting machine for 100 seconds to form and solidify and cool. Step S30: The formed blank is taken out and trimmed and corrected by a trimming and correction mold; Step S40: Use blue light to inspect the blank for defects such as cracks; Step S50: Perform laser trimming on the blank; Step S60: Spray coating is applied to the blank to obtain the final product; Step S70: Conduct an overall quality inspection of the product; Step S80: Package the product.

[0028] The performance parameters of the one-piece die-cast aluminum panel of the present invention are compared with those of conventional aluminum panels in the following table:

[0029] Compared to conventional metal panels, the one-piece die-cast metal panel of this embodiment has at least the following advantages: 1. The metal single panel is integrally die-cast, with the panel surface 100, ribs 200, side edges 300 and connectors 400, eliminating the need for corner assembly and welding, thus solving the risk of production deformation. 2. The production cycle is greatly shortened, eliminating the aluminum rod production process, extrusion process, and welding process; 3. It solves the problems of poor surface flatness and aesthetics, and significantly improves the appearance; 4. The ribs are 200mm in diameter and intersect each other, which significantly improves the impact resistance and wind pressure resistance while significantly reducing the thickness; 5. Due to its integral casting process, the compressive strength, yield strength, wind pressure resistance, sound insulation, and thermal insulation performance are significantly improved. 6. Due to the one-time molding process, the error of metal panels for curtain walls of the same specifications is almost zero, and the production error standard of the product is more than 100% higher than the national standard. 7. The products have good consistency and interchangeability, and produce almost no metal waste. 8. The production process is more low-carbon and environmentally friendly.

[0030] In summary, this invention solves the problems of long production cycles, numerous production steps, unstable assembly quality, large geometric dimensional errors, poor surface flatness, poor interchangeability, and large material losses in existing metal veneer processing.

[0031] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, and not to limit them. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some or all of the technical features therein. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention, and they should all be covered within the scope of the claims and specification of the present invention.

Claims

1. A one-piece die-cast metal veneer, characterized in that: The plate includes a plate surface, on the back of which ribs are distributed, and a side edge that bends towards the back of the plate surface. Connectors are provided on the side edge. The plate surface, ribs, side edge, and connectors are integrally die-cast.

2. The integral die-cast metal veneer according to claim 1, characterized in that: The ribs on the back of the plate are crisscrossed.

3. The integral die-cast metal veneer according to claim 2, characterized in that: The ribs on the back of the plate are arranged in a crisscross pattern to form a rectangular grid.

4. The integral die-cast metal veneer according to claim 2, characterized in that: The ribs on the back of the plate are arranged longitudinally and diagonally to form a parallelogram grid.

5. The integral die-cast metal veneer according to claim 1, characterized in that: The metal panel is made of aluminum.

6. The integral die-cast metal veneer according to claim 1, characterized in that: The connector is an L-shaped connector, with one side of the L-shaped connector connected to the side wall edge, and the other side of the L-shaped connector bent outward and provided with a connection hole.

7. A method for manufacturing an integrally die-cast metal single plate as described in any one of claims 1-6, characterized in that, Includes the following steps: Step S10: The alloy ingot is melted into a liquid state; Step S20: The molten liquid alloy is injected into a special mold cavity through a large vacuum die casting machine and solidified and cooled. Step S30: The formed blank is taken out and trimmed and corrected by a trimming and correction mold; Step S40: Use blue light to inspect the blank for defects such as cracks; Step S50: Perform laser trimming on the blank; Step S60: Spray coating is applied to the blank to obtain the final product; Step S70: Conduct an overall quality inspection of the product; Step S80: Package the product.