Pen tip iridium particle point iridium welding positioning device and processing method
By using a device consisting of a base platform, uprights, a load-bearing mechanism, a thinning mechanism, and a positioning mechanism, combined with transparent syrup and a laser emitter, the positioning and offset problems in the iridium granule welding process were solved, achieving low-cost and high-efficiency iridium granule welding.
Patent Information
- Application Number
- CN202610706096.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-05-21
- Publication Date
- 2026-06-26
AI Technical Summary
Existing welding techniques are difficult to effectively fix and precisely weld extremely small iridium nibs to pen tips, and are costly, prone to tip misalignment and damage to the clamping structure, resulting in low yield.
An apparatus comprising a base platform, uprights, a load-bearing mechanism, a thinning mechanism, and a positioning mechanism is used to solidify iridium particles using transparent syrup, combined with a laser emitter and a cooling fan, to achieve the positioning and welding of the iridium particles.
This method achieves stable positioning of iridium granules and low-cost welding, avoiding welding misalignment and damage to the clamping structure, and improving the yield.
Smart Images

Figure CN122274423A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the technical field of welding positioning equipment, specifically to a welding positioning device and processing method for iridium dots on pen tips. Background Technology
[0002] Soldering iridium tips into fountain pen nibs is a relatively high-end processing technique used to improve the smoothness and wear resistance of fountain pen nibs, and it is a commonly used processing method. Existing welding processes typically employ microscope-assisted welding methods. However, due to the extremely small size of iridium beads and the high temperature requirements during welding, tweezers or direct contact are usually used for welding, followed by grinding. But these methods easily cause the pen tip to detach from the iridium bead. Furthermore, the small size of the iridium bead makes clamping and fixing extremely difficult. If not fixed, the iridium bead may slip off the pen tip at an angle during welding, resulting in a scrapped pen tip and a low yield. If a micro-clamping device is used for assistance, the clamping structure is easily damaged during welding. Moreover, the laser welding operation field of view is extremely small, making it prone to displacement. In addition, the cost is too high, significantly exceeding the requirements of steel plate manufacturing. Summary of the Invention
[0003] In order to solve the above-mentioned problems in the existing technology, the present invention aims to provide a simple structure, with a good operating range, low cost and effective iridium tip welding positioning device and processing method for iridium tip positioning welding of pen tip.
[0004] The technical solution adopted in this invention is as follows: A positioning device for welding iridium nib beads, characterized in that: it includes a base platform and a support rod supported on the base platform, the support rod is provided with a bearing mechanism for bearing iridium nib beads for welding, and the support rod is also provided with a thinning mechanism for treating the exposed position of the iridium nib beads on the bearing mechanism. The supporting mechanism includes a connecting ring fixed to the middle of the upright, and a supporting circular plate is circumferentially connected to the inner side of the connecting ring to support the curing liquid; a laser emitter is provided on the side of the upright away from the foundation platform, and the laser emitter is fixed to one side of the iridium support surface of the supporting circular plate of the upright by a fixing clamp connected by fixing bolts.
[0005] In one embodiment, the supporting circular plate is provided with a plurality of heat-dissipating fins arranged in a rectangular array on the side near the base platform, and a cooling fan is provided between the heat-dissipating fins and the base platform, the cooling fan being connected to the upright by a movable ring.
[0006] In one embodiment, the base platform is also provided with a liquid extraction pipe, which is supported by a mechanical support arm on one side of the upright. The liquid extraction pipe has an L-shaped bend structure, with a soft rubber flared mouth at one end and an output pipe connected to the other end. A replenishment pipe is provided at the end of the liquid extraction pipe near the rubber flared mouth, and the replenishment pipe enters one part of the liquid extraction pipe and passes through the bend of the liquid extraction pipe.
[0007] In one embodiment, the end of the replenishment tube near the extraction tube is inserted into the cavity of a port adjacent to the extraction tube.
[0008] In one embodiment, the liquid extraction tube is provided with a plurality of arrayed rotating inclined plates on the periphery of the inner cavity where the liquid replenishment tube is located, and the end of the rotating inclined plate near the liquid extraction tube is inserted into the inner cavity of the port of the liquid extraction tube.
[0009] In one embodiment, a positioning mechanism is provided on one side of the supporting circular plate. The positioning mechanism includes a clamping roller, and a pressing tile is provided at the end of the clamping roller. The pressing tile has an arc-shaped buckle structure. Extension rods are provided at both ends of the pressing tile. The extension rods have an L-shaped bending rod structure. Two sets of extension rods are interlocked on both sides of the clamping roller. A clamping bolt is provided in the middle of the extension rod. The clamping bolt passes through and is rotatably connected to the extension rod. The end of the clamping bolt abuts against the arc surface of the clamping roller away from the pressing tile. A rotating component is provided in the middle of the clamping roller to rotate the intersection angle between the axis of the clamping roller and the base platform.
[0010] In one embodiment, the rotating component includes a swing ring, the clamping roller is inserted into and rotatably connected to the inner cavity of the swing ring, the swing ring has a rotating shaft at both ends, the rotating shaft has a lifting block in the middle, the rotating shaft passes through and is rotatably connected to the lifting block, a sliding block is provided between the lifting block and the base platform, the sliding block abuts against the base platform, a lifting guide rod is provided on the sliding block, the lifting guide rod passes through and is slidably connected to the lifting block, and a thrust spring is provided between the lifting block and the lifting guide rod, which is penetrated by the lifting guide rod.
[0011] In one embodiment, the end of the clamping roller away from the pressing tile is further provided with a rotating wheel to drive the clamping roller to rotate on the swing ring.
[0012] In one embodiment, a sliding rod is provided in the middle of the sliding block. The sliding rod passes through and is slidably connected to the sliding block. The axis of the sliding rod is oriented towards the direction of movement from the positioning mechanism to the bearing mechanism. Both ends of the sliding rod are supported on the base platform by support blocks.
[0013] In one embodiment, a method for welding iridium dots to the iridium tip is also included, the specific implementation method of which is as follows: S1. After the curing liquid is placed on the carrier plate, the iridium granules are then placed on the surface of the carrier plate and in contact with the carrier plate. S2. Utilizing the solidification ability of liquids to transform them into solids; S3. Grind the solid surface formed by the solidified liquid to expose the iridium particles; S4. Support the pen tip on the iridium tip, start the laser emitter to weld, and use vaporization or combustion to remove some of the solidified liquid, causing the iridium tip to detach from the support of the bearing plate. S5. After welding is completed, remove the bearing circular plate from the connecting ring, then reinstall it and wait for the subsequent welding process.
[0014] The beneficial effects of this invention are as follows: The purpose of this invention is to provide a simple structure, a good operating range, low cost, and an effective method for positioning and welding iridium tips in fountain pens, as well as a method for processing such welding. The operator first installs the pen tip between the pressing tile and the clamping roller, and after the pen tip is exposed, rotates the clamping bolt to push it into the clamping roller. As the clamping bolt is continuously pushed into the clamping roller, it pushes the extension rod to move relative to the clamping roller, causing the pressing tile to continuously approach the clamping roller to clamp and fix the pen tip, and then the welding preparation work can be carried out. Next, the supporting circular plate is placed in the inner ring of the connecting ring for connection. The curing liquid, preferably transparent syrup, is then placed inside the syrup. After that, the cooling fan is activated to blow the heat-dissipating fins of the three mechanical support arms to quickly dissipate heat and solidify the solid block. At this point, the block can be ground by the thinning mechanism. After the rubber flared end of the suction tube is attached to the solid block using a mechanical support arm, the soft structure of the rubber flared end ensures complete contact with the surface up to directly above the iridium granule. Then, liquid, such as water, is introduced through the replenishment tube into the suction tube. The liquid contacts the solid block and melts its surface. Simultaneously, the fused liquid is extracted through the output tube. The liquid flows through the end of the suction tube into the cavity of the fixed block, accumulating within the tube until it passes through a corner. During extraction through the output tube, a rotating inclined plate guides the liquid flow and rotates, accelerating the dissolution of the solid block. The replenishment tube is then stopped, but the extraction through the output tube continues. The suction tube is then detached from the solid block surface to observe the treatment effect. If the iridium granule is exposed, the above operation is repeated multiple times until it is exposed. Once exposed, the thinning mechanism can be removed from the area for welding. Microscopes or other tools can be used for assistance if necessary. After the sliding block slides along the sliding rod, the rotating shaft is rotated and the lifting block is pressed down to suppress the thrust spring and guide the movement of the lifting guide rod until the pen tip at the end of the clamping roller contacts the exposed iridium granule on the surface of the bearing circular plate. The fixing clamp is then activated to weld the steel pen tip. Before welding, the solid block fixes the iridium granule to prevent it from deviating. It also does not obstruct the welding process. During welding, the high temperature melts the solid block, causing the iridium granule to detach and adhere to the pen tip. Then, the rotating wheel is rotated to drive the clamping roller to rotate. At the same time, the position of the laser emitter is adjusted and the laser emitter is used to supplement the welding around the perimeter, thus completing the welding. Afterward, the transparent syrup on the surface of the bearing circular plate is treated, and preparations for the next welding can begin.
[0015] The device has a simple structure and uses the physical deformation of solid blocks for fixation. It also solves the problems of high temperature and welding misalignment during the welding process. The angled pen tip does not affect the welding field of view of the laser emitter. It has good practicality and economy, which is beneficial to the promotion and use of the equipment. Attached Figure Description
[0016] The present invention will now be described in further detail with reference to the accompanying drawings and specific implementation methods.
[0017] Figure 1 This is a three-dimensional structural schematic diagram of the present invention; Figure 2 This is a three-dimensional structural diagram of the supporting mechanism of the present invention; Figure 3 This is a three-dimensional structural diagram of the thinning mechanism of the present invention; Figure 4 This is a three-dimensional cross-sectional structural diagram of the thinning mechanism of the present invention; Figure 5 This is a three-dimensional structural diagram of the positioning mechanism of the present invention; Figure 6 This is a three-dimensional structural diagram of the positioning mechanism of the present invention.
[0018] Figure Descriptions: 1. Base platform; 11. Upright pole; 12. Fixing clamp; 121. Laser emitter; 13. Fixing bolt; 2. Thinning mechanism; 21. Mechanical support arm; 221. Output pipe; 22. Liquid extraction pipe; 222. Rubber flare; 223. Rotating inclined plate; 23. Liquid replenishment pipe; 3. Bearing mechanism; 31. Bearing circular plate; 32. Connecting ring; 33. Heat dissipation fins; 34. Movable ring; 35. Cooling fan; 4. Positioning mechanism; 41. Sliding rod; 411. Support block; 42. Lifting block; 421. Lifting guide rod; 422. Sliding block; 43. Thrust spring; 44. Swinging ring; 441. Rotating shaft; 45. Clamping roller; 451. Rotating wheel; 46. Pressing tile; 461. Extension rod; 462. Clamping bolt. Detailed Implementation
[0019] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only for explaining the invention and are not intended to limit the invention; that is, the described embodiments are merely some embodiments of the invention, and not all embodiments. The components of the embodiments of the invention described and shown in the accompanying drawings can generally be arranged and designed in various different configurations.
[0020] Therefore, the following detailed description of the embodiments of the invention provided in the accompanying drawings is not intended to limit the scope of the claimed invention, but merely to illustrate selected embodiments of the invention. All other embodiments obtained by those skilled in the art based on the embodiments of the invention without inventive effort are within the scope of protection of the invention.
[0021] The following is combined Figure 1-6 The present invention describes a specific embodiment of an iridium tip welding positioning device, comprising a base platform 1 and a support rod 11 supported on the base platform 1. The support rod 11 is provided with a bearing mechanism 3 for bearing the iridium tip for welding. The iridium tip is a ball that needs to be welded to the pen tip. It has high hardness and very small size. If necessary, a microscope or other means can be used to assist in observing the welding. This is prior art and will not be described in detail. The support rod 11 is also provided with a thinning mechanism 2 for processing the exposed position of the iridium tip on the bearing mechanism 3. The supporting mechanism 3 includes a connecting ring 32 fixed to the middle of the upright 11. A supporting circular plate 31 is circumferentially connected to the inner side of the connecting ring 32. It can be fixed by screwing in or snapping, forming a shallow supporting recess to hold the curing liquid. Specifically, the curing liquid is fixed by a specific method, preferably a transparent syrup, or something similar, which can be fixed by cooling and subsequently melted by a liquid such as water. Specifically, the transparent syrup has high hardness after curing, can dissolve in water, is transparent, and easily positions the iridium particles. Furthermore, after high-temperature welding, it easily dissolves or carbonizes and detaches from the supporting circular plate 31. A laser emitter 121 is provided on the side of the rod 11 away from the base platform 1. Specifically, the laser emitter 121 is a traditional auxiliary means of pen tip welding. It mainly uses laser to heat the contact part between the pen tip and the iridium tip, melting the pen tip and covering the iridium tip for connection. This is an existing technology that can achieve similar welding effects. The laser emitter 121 is fixed to one side of the iridium tip support surface on the bearing circular plate 31 of the upright rod 11 by a fixing clip 12 connected to the fixing bolt 13. This facilitates the adjustment of the position or height of the laser emitter 121. The fixing clip 12, together with the fixing bolt 13, can achieve the fixing function. It is a universal clamping structure.
[0022] Specifically, the supporting circular plate 31 has several heat-dissipating fins 33 arranged in a rectangular array on the side near the base platform 1 to assist in dissipating heat from the transparent syrup. A cooling fan 35 is provided between the heat-dissipating fins 33 and the base platform 1 to assist in dissipating heat. The cooling fan 35 is connected to the upright 11 by a movable ring 34.
[0023] Specifically, a liquid extraction pipe 22 is also provided on the base platform 1. The liquid extraction pipe 22 is supported on one side of the upright 11 by a mechanical support arm 21. The mechanical support arm 21 mainly supports the liquid extraction pipe 22 through connecting rods or support structures, which is existing technology. It can usually achieve movable support for the support, such as rotation adjustment, height adjustment or position positioning, etc. It can achieve the above functions, so it will not be described in detail. The liquid extraction pipe 22 has an L-shaped bend structure. One end of the liquid extraction pipe 22 is provided with a soft rubber flared mouth 222, and the other end is connected to an output pipe 221 for extracting liquid. It can be connected to a liquid extraction structure such as a liquid pump for assistance. The end of the liquid extraction pipe 22 near the rubber flared mouth 222 is provided with a replenishment pipe 23 for replenishing liquid. It can be connected to a replenishment structure such as a replenishment pump for assistance. Specifically, the liquid pump and the replenishment pump mainly realize the extraction or replenishment of liquid, which is existing technology. It can assist in achieving the above functions. The replenishment pipe 23 enters one part of the liquid extraction pipe 22 and passes through the bend of the liquid extraction pipe 22.
[0024] Specifically, the end of the replenishing tube 23 near the extraction tube 22 is inserted into the cavity of the port of the extraction tube 22, so that there is room for movement between the liquid and the transparent syrup solid, thereby improving the dissolution efficiency.
[0025] Specifically, the liquid extraction tube 22 has several arrayed rotating inclined plates 223 arranged around the inner cavity of the liquid replenishment tube 23. The end of the rotating inclined plate 223 near the liquid extraction tube 22 is inserted into the inner cavity of the liquid extraction tube 22 near the port. During liquid extraction, the liquid is rotated to improve the dissolution efficiency.
[0026] Beneficially, a positioning mechanism 4 is provided on one side of the supporting circular plate 31. The positioning mechanism 4 includes a clamping roller 45, and a pressing tile 46 is provided at the end of the clamping roller 45. The pressing tile 46 has an arc-shaped buckle structure. Extension rods 461 are provided at both ends of the pressing tile 46. The extension rods 461 have an L-shaped bent rod structure. Two sets of extension rods 461 are interlocked on both sides of the clamping roller 45. A clamping bolt 462 is provided in the middle of the extension rod 461. The clamping bolt 462 passes through and is rotatably connected to the extension rod 461. The end of the clamping bolt 462 abuts against the arc surface of the clamping roller 45 away from the pressing tile 46. A rotating part is provided in the middle of the clamping roller 45 for rotating the clamping roller 45. The angle of intersection between the axis and the base platform 1 is beneficial. The rotating component includes a swing ring 44, a clamping roller 45 that passes through and is rotatably connected to the inner cavity of the swing ring 44, a rotating shaft 441 at both ends of the swing ring 44, a lifting block 42 in the middle of the rotating shaft 441, the rotating shaft 441 passing through and rotatably connected to the lifting block 42, a sliding block 422 between the lifting block 42 and the base platform 1, the sliding block 422 abutting against the base platform 1, a lifting guide rod 421 on the sliding block 422, the lifting guide rod 421 passing through and slidably connected to the lifting block 42, and a thrust spring 43 that is passed through the lifting guide rod 421 between the lifting block 42 and the lifting guide rod 421.
[0027] Beneficially, the end of the clamping roller 45 away from the pressing tile 46 is also provided with a rotating wheel 451 to drive the clamping roller 45 to rotate on the swing ring 44.
[0028] Beneficially, a sliding rod 41 is provided in the middle of the sliding block 422. The sliding rod 41 passes through and is slidably connected to the sliding block 422. The axis of the sliding rod 41 is oriented towards the direction of moving from the positioning mechanism 4 to the bearing mechanism 3. Both ends of the sliding rod 41 are supported on the base platform 1 by the support blocks 411.
[0029] Also beneficial is a method for welding iridium dots to the iridium tip of a pen, the specific implementation method of which is shown below: S1. After the curing liquid is placed on the bearing circular plate 31, the iridium particles are then placed on the surface of the bearing circular plate 31 and in contact with the bearing circular plate 31. Since the iridium particles have a large unit mass, they will sink into the curing liquid to the surface of the bearing circular plate 31, creating a space for subsequent grinding. S2. Utilizing the solidification ability of liquids to turn them into solids, such as by cooling; S3. Grind the solid surface formed by the solidified liquid to expose the iridium tip. Only a very small part of the tip needs to be welded. S4. Support the pen tip on the iridium granule, activate the laser emitter 121 to perform welding, and eliminate part of the solidified liquid by vaporization or combustion, so that the iridium granule is detached from the support of the bearing plate 31. S5. After welding is completed, remove the bearing circular plate 31 from the connecting ring 32, then reinstall it and wait for the subsequent welding process.
[0030] Working principle of this invention: The operator first installs the pen tip between the pressing tile 46 and the clamping roller 45, and after the pen tip is exposed, rotates the clamping bolt 462 to push it into the clamping roller 45. As the end of the clamping bolt 462 is continuously pushed, it pushes the extension rod 461 to move relative to the clamping roller 45, causing the pressing tile 46 to continuously approach the clamping roller 45 to clamp and fix the pen tip, and then the welding preparation work can be carried out. Next, the supporting circular plate 31 is placed in the inner ring of the connecting ring 32 for connection. The curing liquid, preferably transparent syrup, is then placed inside the syrup. After that, the cooling fan 35 is activated to blow the heat-dissipating fins 33 of the mechanical support arm 21 to quickly dissipate heat and solidify the block. The solid block can then be ground by the thinning mechanism 2. After the rubber flared end 222 of the suction tube 22 is attached to the solid block using the mechanical support arm 21, the soft structure of the rubber flared end 222 ensures complete contact with the surface up to directly above the iridium granule. Then, liquid, such as water, is introduced through the replenishment tube 23 into the suction tube 22. The liquid contacts the solid block and melts its surface. Simultaneously, the fused liquid is extracted through the output tube 221. The liquid flows through the end of the suction tube 22 into the cavity of the fixed block, accumulating within the suction tube 22 until it passes through a corner. During extraction through the output tube 221, the rotating inclined plate 223 guides the liquid flow and rotates, accelerating the dissolution of the solid block. Then, the replenishment tube 23 stops supplying liquid, but the output tube 221 continues extraction. The suction tube 22 is then detached from the solid block surface. The processing effect is observed. If the iridium granule is exposed, the above operation is repeated multiple times until it is exposed. Then, the thinning mechanism 2 can be removed from the area for welding. If necessary, a microscope or other means can be used for assistance. After the sliding block 422 slides guided on the sliding rod 41, the rotating shaft 441 is rotated and the lifting block 42 is pressed down to suppress the thrust spring 43 and guide the movement of the lifting guide rod 421 until the pen tip at the end of the clamping roller 45 abuts against the exposed iridium granule on the surface of the bearing circular plate 31. The fixing clamp 12 is then activated to fuse the steel pen tip for welding. Before welding, the solid block fixes the iridium granule and positions it to prevent it from deviating. It will not obstruct the welding process. During welding, the high temperature melts the solid block, causing the iridium granule to detach and adhere to the pen tip. Then, the rotating wheel 451 is rotated to drive the clamping roller 45 to rotate. At the same time, the position of the laser emitter 121 is adjusted and the laser emitter 121 is used to supplement the welding of the periphery, thus completing the welding. After the transparent syrup on the surface of the bearing circular plate 31 is treated, preparations for the next welding can begin.
[0031] In the description of this invention, it should be noted that, unless otherwise explicitly specified and limited, the terms "installation," "connection," "linking," etc., should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral connection; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; and they can refer to the internal communication between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.
[0032] The above description is merely an example and illustration of the structure of the present invention. Those skilled in the art can make various modifications or additions to the specific embodiments described or use similar methods to replace them, as long as they do not deviate from the structure of the invention or exceed the scope defined in the claims, they should all fall within the protection scope of the present invention.
Claims
1. A device for positioning and welding iridium particles in a pen tip, characterized in that: Includes a base platform (1) and a support pole (11) supported on the base platform (1). The support pole (11) is provided with a bearing mechanism (3) for bearing iridium particles for welding. The support pole (11) is also provided with a thinning mechanism (2) for processing the exposed position of the iridium particles on the bearing mechanism (3). The bearing mechanism (3) includes a connecting ring (32) fixed in the middle of the upright (11), and a bearing circular plate (31) is circumferentially connected to the inner side of the connecting ring (32) to bear the curing liquid; a laser emitter (121) is provided on the side of the upright (11) away from the base platform (1), and the laser emitter (121) is fixed to one side of the iridium support surface on the bearing circular plate (31) of the upright (11) by a fixing clamp (12) connected by a fixing bolt (13).
2. The iridium tip dot welding positioning device according to claim 1, characterized in that: The supporting circular plate (31) has a number of heat-dissipating fins (33) arranged in a rectangular array on the side near the base platform (1). A cooling fan (35) is provided between the heat-dissipating fins (33) and the base platform (1). The cooling fan (35) is connected to the upright (11) by a movable ring (34).
3. The iridium tip dot welding positioning device according to claim 2, characterized in that: The base platform (1) is also provided with a liquid extraction pipe (22). The liquid extraction pipe (22) is supported by a mechanical support arm (21) on one side of the upright (11). The liquid extraction pipe (22) has an L-shaped bend structure. One end of the liquid extraction pipe (22) is provided with a soft rubber flared mouth (222), and the other end is connected to an output pipe (221). The end of the liquid extraction pipe (22) near the rubber flared mouth (222) is provided with a replenishment pipe (23). The replenishment pipe (23) enters one part of the liquid extraction pipe (22) and passes through the bend of the liquid extraction pipe (22).
4. The iridium tip dot welding positioning device according to claim 3, characterized in that: The end of the replenishing tube (23) near the end of the extraction tube (22) is inserted into the cavity of the port of the extraction tube (22).
5. The iridium tip dot welding positioning device according to claim 4, characterized in that: The liquid extraction tube (22) has a plurality of arrayed rotating inclined plates (223) on the periphery of the inner cavity of the liquid replenishment tube (23). The end of the rotating inclined plate (223) near the liquid extraction tube (22) is inserted into the inner cavity of the port of the liquid extraction tube (22).
6. The iridium tip dot welding positioning device according to claim 1, characterized in that: A positioning mechanism (4) is provided on one side of the bearing circular plate (31). The positioning mechanism (4) includes a clamping roller (45). The clamping roller (45) has a pressing tile (46) at its end. The pressing tile (46) has an arc-shaped buckle structure. The pressing tile (46) has extension rods (461) at both ends. The extension rods (461) have an L-shaped bent rod structure. Two sets of extension rods (461) are fastened to both sides of the clamping roller (45). The extension rods (461) have clamping bolts (462) in the middle. The clamping bolts (462) are inserted into and rotatably connected to the extension rods (461). The insertion end of the clamping bolts (462) abuts against the arc surface of the clamping roller (45) away from the pressing tile (46). The clamping roller (45) has a rotating part in the middle to rotate the intersection angle between the axis of the clamping roller (45) and the base platform (1).
7. The iridium tip dot welding positioning device according to claim 6, characterized in that: The rotating component includes a swing ring (44), and the clamping roller (45) is inserted into and rotatably connected to the inner cavity of the swing ring (44). The swing ring (44) has a rotating shaft (441) at both ends, and a lifting block (42) is provided in the middle of the rotating shaft (441). The rotating shaft (441) passes through and is rotatably connected to the lifting block (42). A sliding block (422) is provided between the lifting block (42) and the base platform (1). The sliding block (422) abuts against the base platform (1). A lifting guide rod (421) is provided on the sliding block (422). The lifting guide rod (421) passes through and is slidably connected to the lifting block (42). A thrust spring (43) is provided between the lifting block (42) and the lifting guide rod (421) and is penetrated by the lifting guide rod (421).
8. The iridium tip dot welding positioning device according to claim 7, characterized in that: The clamping roller (45) is provided with a rotating wheel (451) at the end away from the pressing tile (46) to drive the clamping roller (45) to rotate on the swing ring (44).
9. The iridium tip dot welding positioning device according to claim 7, characterized in that: The sliding block (422) is provided with a sliding rod (41) in the middle. The sliding rod (41) passes through and is slidably connected to the sliding block (422). The axis of the sliding rod (41) is oriented towards the direction of moving from the positioning mechanism (4) to the bearing mechanism (3). Both ends of the sliding rod (41) are supported on the base platform (1) by support blocks (411).
10. A method for welding iridium dots to a pen tip, using the pen tip iridium dot welding positioning device as described in any one of claims 1-9, characterized in that: The specific implementation method is as follows: S1. After placing the curing liquid onto the support circular plate (31), the iridium granules are then placed on the surface of the support circular plate (31) and in contact with the support circular plate (31); S2. Utilizing the solidification ability of liquids to transform them into solids; S3. Grind the solid surface formed by the solidified liquid to expose the iridium particles; S4. Support the pen tip on the iridium granule, start the laser emitter (121) to weld, and eliminate part of the solidified liquid by vaporization or combustion, so that the iridium granule is detached from the support of the bearing disc (31); S5. After welding is completed, remove the bearing circular plate (31) from the connecting ring (32), then reinstall it and wait for the subsequent welding process.