A process for the preparation of a low-aldehyde polyether polyol
By combining aminosilane-modified adsorbents with silicate adsorbents during the purification process of polyether polyols, chemical and physical adsorption of aldehydes was achieved, solving the problem of difficulty in reducing aldehyde content and odor in existing technologies, and producing polyether polyols with ultra-low aldehyde content.
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- CNOOC & SHELL PETROCHEMICAL CO LTD
- Filing Date
- 2026-05-08
- Publication Date
- 2026-06-30
AI Technical Summary
Existing technologies are insufficient to effectively reduce the aldehyde content and odor in polyether polyols, especially since propionaldehyde residue is relatively high. Existing methods, such as improving raw material quality, optimizing production processes, and purification methods, have limited effectiveness.
In the purification process of polyether polyols, an aminosilane-modified adsorbent is added. The aldehydes are adsorbed onto the solid adsorbent by the chemical adsorption reaction between amino and aldehyde groups, and then removed by filtration. Combined with the physical adsorption of silicate adsorbents, the aldehydes are completely removed.
Polyether polyols with ultra-low aldehyde content were prepared, with a total aldehyde content of ≤3ppm, especially a propionaldehyde content of ≤0.56ppm, which significantly reduced the aldehyde content and odor of the product, and improved the product purity and aldehyde removal efficiency.