Environment-friendly sintering process for resource utilization of kiln slag

By adjusting the particle size and proportion of kiln slag in stages on the sintering production line, and combining it with alkaline flux and fuel, the risks of kiln slag occupying space and the environment have been solved, and the resource utilization of kiln slag and energy conservation and consumption reduction of sintered ore have been realized.

CN122408458APending Publication Date: 2026-07-17BEIHAI CHENGDE NICKEL IND CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
BEIHAI CHENGDE NICKEL IND CO LTD
Filing Date
2026-05-21
Publication Date
2026-07-17

AI Technical Summary

Technical Problem

The slag accumulated in sintering plants occupies a large area and poses environmental risks such as heavy metal leaching and acid production from sulfide oxidation. Furthermore, existing treatment methods lack control over sulfur, phosphorus, and heavy metals, affecting resource utilization and environmental safety.

Method used

A staged, variable particle size, and variable ratio kiln slag addition process is implemented on a continuous sintering production line. Through daily batching, granulation, distribution, and sintering, the particle size and ratio of kiln slag are gradually adjusted. Combined with alkaline flux and fuel, the sintering process is optimized to achieve the resource utilization of kiln slag.

Benefits of technology

It effectively solves the risks of kiln slag occupying space and the environment, makes full use of the valuable components in kiln slag, improves the permeability of sintered ore, reduces coal consumption, and consolidates or removes sulfur and heavy metals, thereby realizing the resource utilization of solid waste and the energy conservation of sintering.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

本发明提供了一种窑渣资源化利用的环保烧结工艺,涉及资源循环利用技术与环保技术领域,本发明通过对窑渣进行分阶段、变粒径、变配比的梯级添加,不仅有效解决了窑渣占用场地、环保受限及重金属浸出等环境风险问题,而且充分利用了窑渣中残留的铁、硅、钙等有价组分,改善烧结矿的透气性,还利用窑渣放热替代部分燃料,使烧结煤耗显著降低。