Forming device and method for a dihedral multi-dip skin type part

By using a skin stretching and deep drawing device, combined with an upper pressing device and a rotating support arm, the problems of low forming efficiency and poor quality of anisotropic multi-depression skin parts have been solved, and high-quality anisotropic multi-depression skin parts processing has been achieved.

CN122626010APending Publication Date: 2026-08-25SHENYANG AIRCRAFT CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610780614.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-06-02
Publication Date
2026-08-25

AI Technical Summary

Technical Problem

Existing technologies are insufficient for efficiently processing anisotropic, multi-depressed skin-like parts, resulting in low forming efficiency, poor precision and quality. Furthermore, traditional methods lead to poor surface quality, requiring extensive manual finishing.

Method used

Using a skin stretching and drawing forming device and a deep drawing forming device, combined with an upper pressing device, a rotating support arm and a positioning plate, anisotropic multi-depressed skin parts are produced by skin stretching and deep drawing forming methods. Holes are drilled using a drill jig and surface features are trimmed.

Benefits of technology

It improves the forming quality of anisotropic multi-depression skin parts, reduces manual finishing time, and improves production efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122626010A_ABST
    Figure CN122626010A_ABST
Patent Text Reader

Abstract

The application discloses a kind of forming device and method of dissimilar direction multi-drawing skin class parts;The device includes skin stretch forming device and skin drawing forming device;Skin stretch forming device has drawing lower die, upper pressing device, rotating support arm, square drawing plate, special-shaped drawing cover plate and multiple drill jig, for forming drawing feature;Skin drawing forming device has drawing lower die, blank holder guide column, positioning plate, drawing upper die and pneumatic column, for forming convex feature;The method comprises: first, through skin stretch forming device, stretch and press drawing feature, drill positioning hole and fixing hole, and use square drawing plate to knock and trim;Then, through skin drawing forming device, after locating, drawing forming convex feature of part.The application combines skin stretch and drawing process, solves the problem of forming difficulty of dissimilar direction multi-drawing skin class parts, and improves forming precision and efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention belongs to the field of aluminum alloy sheet metal processing technology for aircraft, specifically relating to a forming device and method for anisotropic multi-depressed skin-like parts. Background Technology

[0002] Aluminum alloy skins are common external components of aircraft. Due to installation requirements, some areas require recessed or convex surface features on the skin. Traditional stretch forming methods can process skin parts with single or simple hyperbolic curvatures. However, if the skin surface has irregular shapes, stretch forming cannot produce such parts, requiring methods like drop hammer forming or manual finishing. Drop hammer forming or manual finishing results in poor surface quality, requiring significant time for finishing to meet delivery requirements. Compared to stretch forming, it cannot achieve the same surface quality as stretch forming in a single operation. Summary of the Invention

[0003] The purpose of this invention is to provide a forming apparatus and method for anisotropic multi-depression skin parts, in order to overcome the problems of low efficiency, insufficient precision and quality of existing processing methods.

[0004] To achieve the above objectives, the present invention employs the following technical solution: A forming apparatus for anisotropic multi-depression skin-like parts includes a skin stretching forming apparatus and a skin deep drawing forming apparatus. The skin stretching and forming apparatus includes: The lower die for drawing is machined according to the actual shape of the part, and no part is machined at the position corresponding to the protruding features of the part; An upper pressing device is installed on the upper part of the lower drawing die and is used to move downward during the stretching process to create the recessed features on the part; The rotating support arm has one end hinged to the side of the lower die and the other end fitted with a recessed plate. A recessed cover plate is installed on the surface of the lower drawing die and covers the position corresponding to the protruding feature of the part. After installation, the surrounding surface of the lower drawing die is flush and smooth. Drill jig I and drill jig II are installed on both sides of the lower drawing die and are used to drill positioning holes; Drill jigs III and IV are installed inside the recessed feature position on the surface of the lower die and are used to drill fixing holes; The skin deep drawing forming apparatus includes: The lower drawing die has a profile surface that is adapted to the shape of the part only in the area corresponding to the protruding feature of the part. The profile surface is provided with a convex surface for forming the protruding feature, and the part with the recessed feature extends out of the skin deep drawing forming device. A blank holder guide post is provided at the lower part of the drawing die to guide the blank holder to move up and down. Positioning plate I is installed on the side of the upper surface of the drawing die with the shaped surface machined, and is used to position the end of the part; Positioning plate II is installed on the other side of the non-shaped end of the lower drawing die to support the recessed feature portion, and the end is machined with a groove that can be locked onto the edge of the recessed feature. A drawing upper die is installed above the drawing lower die, and a pressure die is provided at its lower part. The lower surface of the pressure die is adapted to the profile surface processed on the drawing lower die, and a concave surface corresponding to the convex surface is provided. The pneumatic columns of the upper drawing die are located on both sides of the upper drawing die and connected to the lower drawing die.

[0005] Furthermore, the gap between the recessed plate and the lower forming die is determined according to the sheet thickness: when the sheet thickness is ≤1mm, the gap is the part thickness -0.1mm; when the sheet thickness is >1mm and ≤3mm, the gap is the part thickness -0.2mm; when 3mm < sheet thickness ≤6mm, the gap is the part thickness -0.25mm.

[0006] Furthermore, the upper pressing device includes an upper connecting plate and a forming block. The upper connecting plate is used to be fixedly connected to the upper pressing beam of the skin stretching machine. The forming block is fixed to the lower part of the upper connecting plate. The lower surface of the forming block is adapted to the surface shape of the part and has a protrusion corresponding to the recessed feature.

[0007] Furthermore, drill jig I and drill jig II are located at opposite ends of the length direction of the lower forming die, and the line connecting their centers coincides with the length axis of the lower forming die.

[0008] A method for forming anisotropic multi-depression skin-like parts includes the following steps: Step 1: Skin stretching and shaping: Install the skin stretching and forming device on the worktable of the skin stretching machine, use the jaws of the skin stretching machine to clamp both ends of the aluminum alloy sheet, place the bottom of the sheet on the upper surface of the stretching die, and stretch and form until the gap between the sheet and the stretching die is no greater than the preset value. The upper pressure device is installed on the upper pressure beam of the skin stretching machine and moved above the lower forming die. The upper pressure beam is moved downward to make the upper pressure device close with the lower forming die and to provide downward pressure to press out the depression feature on the surface of the part. After pressing, use drill jig I and drill jig II to drill positioning holes, then cut off the excess sheet material held by the jaws of the skin stretching machine, and then drill fixing holes through drill jig III and drill jig IV. Use positioning pins to fix the sheet material on the lower stretching die. Flip and rotate the support arm to move the recessed plate above the lower forming die, so that the recessed plate fits into the pressed recessed feature. Tap down around the recessed plate to adjust it until the recessed plate and the sheet are completely horizontal and tightly fitted, so that the amount of recessed springback does not exceed the preset tolerance. After adjustment, pull out the positioning pin and remove the sheet from the lower forming die. The second step is the deep drawing and forming of the skin: Install the skin deep drawing forming device on the hydraulic press, so that the upper deep drawing die is fixedly connected to the upper worktable of the hydraulic press, and the lower deep drawing die is fixed on the lower worktable of the hydraulic press; Place the part formed in the first step on the blank holder of the drawing die, and use locating pins to position the two locating holes drilled in the first step with locating plate I and locating plate II on the drawing die. The hydraulic press slide moves downward, causing the upper and lower drawing dies to close. After pressure is maintained, the slide moves upward, the upper drawing die opens, and the part is removed, completing the forming of the raised features on the part and obtaining the processed anisotropic multi-depressed skin part.

[0009] Furthermore, in the first step, the aluminum alloy sheet is quenched and formed within 20 minutes after quenching; during the stretching process, lubricating oil is applied to the surface of the lower forming die.

[0010] Furthermore, in the first step, after the upper pressing device and the lower forming die are fully closed, a pressure of no more than 5 tons is applied for 30-50 seconds.

[0011] Furthermore, using a crane, the lower and upper drawing dies are placed in the closed state on the lower worktable or shims, ensuring that the die shank of the upper drawing die is aligned with the die shank hole of the hydraulic press slider. The hydraulic press is then started to slide the slider downwards, allowing the die shank to enter the die shank hole and lock it in place. A test blank with the same thickness as the sheet metal used in the first step is placed on the lower worktable. This test blank has not been pre-formed. The test blank is placed on the blank holder of the lower drawing die, and the upper drawing die is moved downwards by the hydraulic press slider to close with the lower drawing die. The test blank is used to adjust the die closing gap. Apply lubricant to the surface of the lower drawing die, set the hydraulic press pressure and the initial drawing test depth, drive the slide to descend and close the die, hold the pressure, then move the slide upward and open the die. Remove the test blank and observe whether wrinkles or cracks appear. Based on the material flow of the test blank, manually trim the edges of the test blank and remove any areas where material flow is obstructed. If wrinkles appear, increase the pressure of the blank holder. If cracks appear, decrease the pressure of the blank holder or apply lubricant to the surface of the lower drawing die and the blank holder. For unbroken test blanks, after manual smoothing, the drawing depth is increased and the drawing test is continued; for broken test blanks, the test blanks are recut according to the trimmed contour and then tested; through multiple tests and gradually increasing the drawing depth, until the final forming state is achieved when the upper and lower drawing dies are fully closed, the test adjustment is completed.

[0012] Furthermore, in the second step, when installing the lower drawing die and the upper drawing die, it is determined whether to add shims on the lower worktable based on the closed height of the lower drawing die and the slide stroke of the hydraulic press; if shims are required, the shims are evenly placed on the lower worktable at preset intervals according to the outer dimensions of the lower drawing die to ensure left-right symmetry. Compared with the prior art, the present invention has the following technical features: This invention addresses the high surface quality requirements of anisotropic multi-depression skin parts, especially when the depression directions are inconsistent, by adding local feature processing methods. The new forming device can effectively improve the forming quality of anisotropic multi-depression skin parts, reduce manual finishing time, and improve product quality and production efficiency. Attached Figure Description

[0013] Figure 1 This is a schematic diagram of an anisotropic, multi-depressed skin-like part; Figure 2 This is a schematic diagram of the process flow of the method of the present invention; Figure 3 This is a schematic diagram of the upper and lower die structures for drawing. Figure 4 This is a schematic diagram of a rotating support arm structure; Figure 5 This is a top view of the lower die of the forming die; Figure 6 This is a side view of the sunken plate; Figure 7 Top view of the lower and upper dies for deep drawing; Figure 8 Side views of the lower and upper dies for deep drawing; Figure 9 This is a side view of the guide post of the pressure ring. Detailed Implementation

[0014] This invention provides a forming apparatus and method for anisotropic multi-depressed skin-like parts. The recessed portion is formed using skin stretching and an auxiliary pressing device, followed by deep drawing to complete the anisotropic feature processing. See also... Figure 1 The anisotropic multi-depression skin parts involved in this solution refer to aluminum alloy sheet metal components with irregular depression and protrusion features on the skin surface, and the depression features and protrusion features have opposite orientations or inconsistent distribution directions.

[0015] See Figure 2 and Figure 3 The present invention provides a forming apparatus for anisotropic multi-depressed skin parts, comprising two parts: a skin stretching forming apparatus and a skin deep drawing forming apparatus.

[0016] The skin stretching and forming device includes a lower stretching die 1, an upper pressing device 2, a rotating support arm 3, a recessed plate 4, a recessed cover plate 5, drill jigs I 6, II 7, III 8, and IV 9, wherein: The surface of the lower forming die 1 is machined according to the actual shape of the part. The raised features on the part surface are not machined in the lower forming die 1; that is, no cavity is machined on the surface of the lower forming die 1 at the position corresponding to the raised feature of the part, and this position remains flat or empty. A recessed cover plate 5 is installed on the surface of the lower forming die 1, covering the position on the lower forming die 1 corresponding to the raised feature of the part. After the recessed cover plate 5 is installed, the surrounding surface of the lower forming die 1 is flush and smooth. An upper pressing device 2 is installed on the upper part of the lower forming die 1. The upper pressing device 2 includes an upper connecting plate and a forming block. The upper connecting plate is fixedly connected to the upper pressure beam of the skin stretching machine. The forming block is fixed to the lower part of the upper connecting plate. The lower surface of the forming block is adapted to the surface shape of the part and has protrusions corresponding to the recessed features. The upper pressing device 2 moves downward during the stretching process, forming the recessed features on the part. Figure 1 The lower part of the component has a square recess (for easy subsequent finishing); a rotating support arm 3 is installed on the side of the lower forming die 1, one end of which is hinged to the side of the lower forming die 1 via a pivot, allowing for 0°-180° rotation in space; the other end of the rotating support arm 3 is bolted to a recessed plate 4, the lower surface shape of which matches the shape of the recessed feature pressed by the upper pressing device 2, and is used to cover the recessed feature after it has been pressed and formed, allowing for secondary finishing of areas that spring back. Considering the springback factor of the sheet metal, the gap between the recessed plate 4 and the lower forming die 1 is determined according to the following formula to facilitate the proper correction of the recessed feature: When the sheet metal thickness is ≤1mm, the gap is the part thickness -0.1mm; when the sheet metal thickness is >1mm and ≤3mm, the gap is the part thickness -0.2mm; when 3mm < sheet metal thickness ≤6mm, the gap is the part thickness -0.25mm.

[0017] Two drill jigs, III8 and IV9, are installed inside the recessed feature position on the surface of the lower forming die 1 to guide the drill bit to drill fixing holes in the sheet metal during finishing. Two drill jigs, I6 and II7, are installed on both sides of the lower forming die 1 to drill positioning holes for the parts. The position of the two drill jigs should take into account the shape of the parts. They need to be selected along the length direction of the parts and set on the axis. That is, drill jigs I6 and II7 are located at the two ends of the length direction of the lower forming die 1, and the line connecting their centers coincides with the length axis of the lower forming die 1, which facilitates the positioning of the next process.

[0018] Skin deep drawing equipment is used to process raised features on parts, such as... Figure 1 The upper part is shown in the figure; wherein the raised features and the recessed features are opposite in direction; the skin deep drawing forming device includes a lower drawing die 10, a blank holder guide post 11, a positioning plate I12, a positioning plate II13, an upper drawing die 14, and a pneumatic column 15 for the upper drawing die, wherein: The lower drawing die 10 is made of 45# steel or a material of equivalent strength, such as... Figure 7 As shown; the upper surface of the lower drawing die 10 is machined with a profile that matches the shape of the part only in the area corresponding to the protruding feature of the part, which serves to support the part; while the part with the recessed feature extends out of the skin deep drawing forming device; a blank holder ring is provided on the lower drawing die 10, and a blank holder ring guide post 11 is installed at the lower part of the lower drawing die 10. The blank holder ring guide post 11 passes through the blank holder ring and guides the blank holder ring to move up and down; a convex surface is provided on the profile corresponding to the protruding feature. This convex surface pushes the sheet metal upward during the deep drawing process and cooperates with the upper drawing die 14 to form the protruding feature of the part; a positioning plate I12 is installed on the side of the upper surface of the lower drawing die 10 with the profile, which is used to position the end of the part. Positioning; a positioning plate II13 is installed on the non-profiled end of the other side. The positioning plate II13 supports the recessed feature and has a groove at its end that can be locked onto the edge of the recessed feature; a drawing upper die 14 is installed on the lower drawing die 10 and is connected to the upper worktable of the hydraulic press; a pressure die is provided at the lower part of the drawing upper die 14. The lower surface of the pressure die is adapted to the profiled surface machined on the lower drawing die 10 and has a concave surface corresponding to the convex surface; retractable pneumatic columns 15 are provided on both sides of the drawing upper die 14 and connected to the lower drawing die 10; the drawing upper die 14 is connected to the upper worktable of the hydraulic press to facilitate the upper worktable to apply downward pressure; when pressure is applied, the pneumatic columns 15 retract to create the convex feature on the surface of the part.

[0019] Based on the above technical solutions, the present invention further provides a forming method for anisotropic multi-depression skin-like parts, comprising: The first step is to stretch and shape the skin.

[0020] The skin stretching and forming device is installed on the worktable of the skin stretching machine, and the lower stretching die 1 is fixed on the worktable of the skin stretching machine; the two ends of the aluminum alloy sheet are clamped by the jaws of the skin stretching machine, and the bottom of the sheet is placed on the upper surface of the lower stretching die 1.

[0021] The cut aluminum alloy sheet is stretched and formed using a skin stretching machine. To ensure the sheet fits the mold after stretching, the aluminum alloy sheet is quenched and formed within 20 minutes after quenching. During the forming process, lubricating oil is applied to the surface of the lower forming die 1 to improve the stretching of the sheet during the forming process and reduce the friction between the part surface and the tooling. When the gap between the stretched sheet and the lower forming die 1 is no more than 0.5mm, the movement of the jaws on both sides of the skin stretching machine is stopped, and the tension is kept constant.

[0022] Install the upper pressure device 2 on the upper pressure beam of the skin stretching machine and move it above the lower forming die 1; move the upper pressure beam downward so that the upper pressure device 2 and the lower forming die 1 close together and apply downward pressure. After the upper pressure device 2 and the lower forming die 1 are fully closed, continue to apply pressure of no more than 5 tons for 30-50 seconds to complete the pressing of the depression feature on the surface of the part.

[0023] After the depression feature is pressed, the upper pressing device 2 is opened, and two positioning holes are drilled manually using a pneumatic drill with drill jigs I6 and II7. After this process, the lower forming die 1 is hoisted from the workbench of the skin stretching machine to a platform on the ground. The excess sheet metal held by the jaws of the skin stretching machine is cut off using a cutting saw. At the same time, fixing holes for the next step of finishing are drilled using a pneumatic drill with drill jigs III8 and IV9. The sheet metal is fixed to the lower forming die 1 using positioning pins through the fixing holes. Then, the rotating support arm 3 is flipped to move the depression plate 4 above the lower forming die 1, so that the depression plate 4 fits into the depression feature pressed in the stretching process. The depression plate 4 is then hammered downwards around the depression plate 4 with an aluminum hammer until the depression plate 4 is completely horizontal and tightly fitted to the sheet metal, achieving a depression springback of no more than 0.5mm. After finishing, the positioning pins are removed, and the sheet metal is removed from the lower forming die 1.

[0024] The second step is deep drawing and forming of the skin.

[0025] (1) Installation and pressure testing of the skin deep drawing forming device.

[0026] The skin deep drawing forming device is installed on a hydraulic press, so that the upper drawing die 14 is fixedly connected to the upper worktable of the hydraulic press, and the lower drawing die 10 is fixed on the lower worktable of the hydraulic press.

[0027] Based on the closed height of the lower drawing die 10 and the stroke of the hydraulic press slide, determine whether to add shims to the lower worktable. If shims are needed, place them evenly on the lower worktable every 150-250mm according to the outer dimensions of the lower drawing die 10, ensuring left-right symmetry. Use a crane to place the lower drawing die 10 and the upper drawing die 14 in the closed state on the lower worktable or shims and adjust their positions to ensure that the die shank (the columnar structure connected to the die shank hole of the slide block) of the upper drawing die 14 is aligned with the die shank hole of the hydraulic press slide block. Start the hydraulic press and slide the slide block downwards so that the die shank of the upper drawing die 14 enters the die shank hole of the slide block. Manually lock the die shank hole to clamp and fix the upper drawing die 14 on the slide block.

[0028] Place a test blank with the same thickness as the sheet metal used in the first step on the lower worktable. This test blank has not been pre-formed. Place the test blank on the blank holder of the lower drawing die 10, ensuring that the perimeter allowance is uniform. Drive the upper drawing die 14 downward by the hydraulic press slider to close the die with the lower drawing die 10. Use the test blank to adjust the die closing gap to ensure that the upper drawing die 14 and the lower drawing die 10 are aligned. This operation is not necessary for dies with guides or pre-retained sheet metal blanks. Apply lubricant to the surface of the lower drawing die 10 with a brush, but do not apply the lubricant to the upper drawing die 14.

[0029] Set the hydraulic press pressure and the initial drawing test depth; drive the slide block downward to close the upper drawing die 14 and the lower drawing die 10. After holding the pressure for more than 6 seconds, the slide block moves upward and the upper drawing die 14 opens; take out the test blank and observe the drawing forming condition to see if wrinkles or cracks appear.

[0030] Adjust the deep drawing test conditions. Based on the material flow of the test blank, manually trim the edges of the test blank and remove any areas where material flow is obstructed. If wrinkles appear, increase the pressure of the blank holder. If cracks appear, reduce the pressure of the blank holder or apply lubricant to the surface of the lower drawing die 10 and the blank holder. For uncracked test blanks, manually smooth out wrinkles and increase the drawing depth to continue the deep drawing test. For cracked test blanks, re-cut the test blank according to the trimmed contour and perform the test. Through multiple tests and gradually increasing the drawing depth, until the final forming state is achieved when the upper drawing die 14 and the lower drawing die 10 are fully closed, the test adjustment is completed.

[0031] (2) Formal deep drawing.

[0032] The part formed in the first step is placed on the pressure ring of the lower drawing die 10. The two positioning holes drilled in the first step are positioned with the positioning plates I12 and II13 on the lower drawing die 10 to ensure that the positioning references of the two are consistent. According to the pressure and drawing depth determined after the test pressure adjustment, the hydraulic press slide is driven to move down, so that the upper drawing die 14 and the lower drawing die 10 are closed. After holding the pressure, the slide moves up, the upper drawing die 14 is opened, the part is taken out, and the forming of the protruding features on the part is completed, and the processed anisotropic multi-depression skin part is obtained.

[0033] The above embodiments are only used to illustrate the technical solutions of this application, and are not intended to limit them. Although this application has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of this application, and should all be included within the protection scope of this application.

Claims

1. A forming apparatus for anisotropic multi-depression skin-like parts, characterized in that, Including skin stretching forming equipment and skin deep drawing forming equipment; The skin stretching and forming apparatus includes: The lower die (1) is formed by drawing, and its surface is processed according to the actual shape of the part, but no part is processed at the position corresponding to the protruding feature of the part; The upper pressing device (2) is installed on the upper part of the lower drawing die (1) and is used to move downward during the stretch forming process to create the recessed features on the part; A rotating support arm (3) is hinged at one end to the side of the pull-shaped lower mold (1) and a recessed plate (4) is installed at the other end. A recessed cover plate (5) is installed on the surface of the lower drawing die (1) and covers the position corresponding to the protruding feature of the part. After installation, the surrounding surface of the lower drawing die (1) is flush and smooth. Drill jig I (6) and drill jig II (7) are installed on both sides of the lower die (1) and are used to drill positioning holes; Drill jigs III (8) and IV (9) are installed inside the recessed feature position on the surface of the lower die (1) and are used to drill a fixing hole; The skin deep drawing forming apparatus includes: The lower drawing die (10) has a profile surface that is adapted to the shape of the part only in the area corresponding to the protruding feature of the part. The profile surface is provided with a convex surface for forming the protruding feature, and the part with the recessed feature is extended outside the skin deep drawing forming device. A blank holder guide post (11) is provided at the lower part of the drawing die (10) to guide the blank holder to move up and down; Positioning plate I (12) is installed on the side of the upper surface of the drawing die (10) where the profile is machined, and is used to position the end of the part; Positioning plate II (13) is installed on the other side of the non-shaped end of the lower drawing die (10) to support the recessed feature part, and the end is machined with a groove that can be stuck on the edge of the recessed feature. The upper drawing die (14) is installed above the lower drawing die (10), and a pressure die is provided at its lower part. The lower surface of the pressure die is adapted to the profile surface processed on the lower drawing die (10), and a concave surface corresponding to the convex surface is provided. The pneumatic column (15) of the upper drawing die is disposed on both sides of the upper drawing die (14) and connected to the lower drawing die (10).

2. The forming apparatus for anisotropic multi-depression skin-like parts according to claim 1, characterized in that, The gap between the recessed plate (4) and the lower forming die (1) is determined according to the thickness of the sheet material: when the sheet material thickness is ≤1mm, the gap is the part thickness -0.1mm; when the sheet material thickness is >1mm and ≤3mm, the gap is the part thickness -0.2mm; when 3mm < sheet material thickness ≤6mm, the gap is the part thickness -0.25mm.

3. The forming apparatus for anisotropic multi-depression skin-like parts according to claim 1, characterized in that, The upper pressing device (2) includes an upper connecting plate and a forming block. The upper connecting plate is used to be fixedly connected to the upper pressing beam of the skin stretching machine. The forming block is fixed to the lower part of the upper connecting plate. The lower surface of the forming block is adapted to the surface shape of the part and has a protrusion corresponding to the recessed feature.

4. The forming apparatus for anisotropic multi-depression skin-like parts according to claim 1, characterized in that, The drill jig I (6) and drill jig II (7) are located at the two ends of the length direction of the lower drawing die (1), and the line connecting their centers coincides with the length direction axis of the lower drawing die (1).

5. A forming method for anisotropic multi-depression skin-like parts, characterized in that, Includes the following steps: Step 1: Skin stretching and shaping: Install the skin stretching and forming device on the worktable of the skin stretching machine, use the jaws of the skin stretching machine to clamp the two ends of the aluminum alloy sheet, place the bottom of the sheet on the upper surface of the stretching die (1), stretch and form until the gap between the sheet and the stretching die (1) is not greater than the preset value. The upper pressing device (2) is installed on the upper pressing beam of the skin stretching machine and moved above the lower forming die (1). The upper pressing beam is moved downward so that the upper pressing device (2) and the lower forming die (1) are closed and downward pressure is provided to press out the depression feature on the surface of the part. After pressing, use drill jig I (6) and drill jig II (7) to drill positioning holes, then cut off the excess sheet material of the skin stretching machine jaw clamping part, and then drill fixing holes through drill jig III (8) and drill jig IV (9), and use positioning pins to fix the sheet material on the stretching lower die (1). Rotate the support arm (3) to move the recessed plate (4) above the lower die (1) so that the recessed plate (4) fits into the pressed recessed feature. Tap down around the recessed plate (4) to adjust until the recessed plate (4) is completely horizontal and tightly fitted with the sheet material, so that the amount of recessed springback is not higher than the preset tolerance. After the adjustment is completed, pull out the positioning pin and remove the sheet material from the lower die (1). The second step is the deep drawing and forming of the skin: Install the skin deep drawing forming device on the hydraulic press, so that the deep drawing upper die (14) is fixedly connected to the upper worktable of the hydraulic press, and the deep drawing lower die (10) is fixed on the lower worktable of the hydraulic press; Place the part formed in the first step on the blank holder of the lower drawing die (10), and use the positioning pin to position the two positioning holes drilled in the first step with the positioning plate I (12) and positioning plate II (13) on the lower drawing die (10); Drive the hydraulic press slide downwards to close the upper drawing die (14) and the lower drawing die (10). After holding the pressure, the slide moves upwards, the upper drawing die (14) opens, the part is taken out, and the protruding features on the part are formed, resulting in a processed anisotropic multi-depression skin part.

6. The forming method for anisotropic multi-depression skin-like parts according to claim 5, characterized in that, In the first step, the aluminum alloy sheet is quenched and formed within 20 minutes after quenching; during the stretching process, the surface of the lower forming die (1) is coated with lubricating oil.

7. The forming method for anisotropic multi-depression skin-like parts according to claim 5, characterized in that, In the first step, after the upper pressure device (2) and the lower forming die (1) are completely closed, a pressure of no more than 5 tons is applied for 30-50 seconds.

8. The forming method for anisotropic multi-depression skin-like parts according to claim 5, characterized in that, Using a crane, place the lower drawing die (10) and the upper drawing die (14) in the closed state on the lower worktable or shims, ensuring that the die shank of the upper drawing die (14) is aligned with the die shank hole of the hydraulic press slider. Start the hydraulic press and slide the slider downwards to allow the die shank to enter the die shank hole and lock it. Place a test blank with the same thickness as the sheet metal used in the first step on the lower worktable. The test blank has not been pre-formed. Place the test blank on the pressure ring of the lower drawing die (10). Drive the upper drawing die (14) downwards and close it with the lower drawing die (10) using the hydraulic press slider. Use the test blank to adjust the mold closing gap. Apply lubricant to the surface of the lower drawing die (10), set the hydraulic press pressure and the depth of the first deep drawing test, drive the slide to move down to close the die, hold the pressure and then move the slide up to open, take out the test blank, and observe whether wrinkles or cracks appear; according to the material flow of the test blank, manually cut and trim the edge of the test blank, and remove the parts where the material flow is not smooth; if wrinkles appear, increase the pressure of the blank holder; if cracks appear, reduce the pressure of the blank holder or apply lubricant to the surface of the lower drawing die (10) and the blank holder. Unbroken test blanks are manually wrinkled and then the drawing depth is increased to continue the drawing test. Broken test blanks are recut according to the trimmed outline and then tested. Through multiple tests and gradually increasing the drawing depth, the final forming state is achieved when the upper drawing die (14) and the lower drawing die (10) are completely closed. At this time, the test adjustment is completed.

9. The forming method for anisotropic multi-depression skin-like parts according to claim 5, characterized in that, In the second step, when installing the lower drawing die (10) and the upper drawing die (14), it is determined whether to add shims on the lower worktable based on the closing height of the lower drawing die (10) and the slide stroke of the hydraulic press. If shims are needed, the shims are evenly placed on the lower worktable at preset intervals according to the outer dimensions of the lower drawing die (10) to ensure left and right symmetry.