An evaluation method for stress state of tunnel inverted arch and side wall joint area based on crack width inversion

By integrating measured data with numerical simulation technology, a non-contact stress diagnosis system was constructed, which solved the problem that existing technologies could not assess the stress state of completed tunnels. This enabled accurate assessment and risk identification of tunnel structures, reduced assessment costs, and improved the accuracy and comprehensiveness of assessment results.

CN122634690APending Publication Date: 2026-08-25CHINA CONSTR SECOND ENG BUREAU LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202610450304.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-04-08
Publication Date
2026-08-25

AI Technical Summary

Technical Problem

Existing technologies make it difficult to assess the stress state of tunnels that have been built but have not been pre-embedded with sensors, and existing crack assessment methods lack quantitative relationships, making it impossible to detect hidden structural damage in a timely manner.

Method used

By integrating on-site measured data and numerical simulation technology, a non-contact stress diagnosis system is constructed. The initial model is corrected using ground-penetrating radar, the true stress state of the structure is inverted, and the stiffness reduction coefficient is quantified by combining multi-dimensional crack characteristics to simulate the load migration process and realize the inversion of the internal stress state.

Benefits of technology

It enables quantitative assessment of the stress state of in-service tunnels, identifies local bearing capacity and the risk of chain failure, provides accurate safety data support, reduces assessment costs, and improves the accuracy and comprehensiveness of assessment results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN122634690A_ABST
    Figure CN122634690A_ABST
Patent Text Reader

Abstract

The application relates to a kind of evaluation methods of stress state of tunnel inverted arch and side wall junction area based on crack width inversion, and relates to the technical field of tunnel engineering monitoring, comprising: S1, collecting initial design parameters and field measured data of tunnel portal section, constructing quasi-real full-face stress initial benchmark model, and synchronously obtaining multi-dimensional crack feature data set of junction area;S2, defining local damage index based on multi-dimensional crack feature data set, and mapping to generate equivalent stiffness reduction coefficient of junction area element;S3, by simulating internal force redistribution process, the real stress state of junction area and the internal force variation increment of whole ring structure are inverted;S4, combined with the stress state and internal force variation increment inverted, execute local bearing capacity checking and global derived risk assessment, output structure safety state classification and corresponding engineering intervention suggestion, solve the problem that the cost is high in prior art due to the dependence on pre-embedded sensor, and the problem that post-stress evaluation cannot be carried out on in-service tunnel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of tunnel engineering monitoring technology, specifically to an assessment method for the stress state of the junction area between the tunnel invert and sidewall based on crack width inversion. Background Technology

[0002] The junction area between the tunnel invert and the sidewall (arch foot) is a critical area for structural stress. Especially under shallow burial and fractured surrounding rock conditions, this area bears large bending moments and axial forces, and is prone to cracks, which directly affect the safety of the tunnel structure. Therefore, accurately assessing the stress state of this area is of great significance to ensuring the long-term safe operation of the tunnel.

[0003] Currently, monitoring the stress state of tunnel structures mainly relies on pre-embedded sensing devices, such as rebar gauges and strain gauges. This method directly measures the internal forces of the structure by deploying sensors before the lining is poured. However, this monitoring method has obvious limitations: First, the sensors and their installation and data acquisition systems are costly, making it difficult to promote their application in small and medium-sized tunnels or temporary projects; second, it is only applicable to newly built tunnels. For existing tunnels that have been built but have not pre-embedded sensors, it is impossible to conduct post-construction internal force monitoring, resulting in a large number of existing tunnels lacking effective stress state assessment methods.

[0004] In addition, existing crack assessment methods mostly remain at the superficial level of judging whether the width exceeds the limit, lacking technical means to establish a quantitative relationship between apparent cracks and structural internal forces, making it difficult to detect hidden structural damage in a timely manner. Summary of the Invention

[0005] This invention provides a method for assessing the stress state of the junction zone between the tunnel invert and sidewall based on crack width inversion. By integrating field measurement data and numerical simulation technology, a non-contact tunnel stress diagnosis system is constructed. First, the initial design model is corrected using ground-penetrating radar and strength testing to establish a "quasi-realistic" stress reference surface. Then, the cross-sectional stiffness reduction coefficient is quantified using apparent multidimensional crack characteristics, and based on the internal force redistribution principle of statically indeterminate structures, the load migration process from the damaged area to the surrounding area is simulated, thereby inverting the true residual internal force of the structure. This scheme solves the problems of high cost and inability to perform post-failure stress assessment of in-service tunnels due to reliance on pre-embedded sensors in existing technologies by inversely inferring the internal stress state from apparent defects. It can not only quantitatively determine local bearing capacity but also identify the risk of cascading failures across the entire ring, providing accurate data support for proactive safety prevention of tunnels.

[0006] A method for assessing the stress state of the junction zone between the tunnel invert and sidewall based on crack width inversion includes the following steps:

[0007] S1, collect the initial design parameters and field measured data of the tunnel portal section, construct a near-realistic full-section stress initial benchmark model, and simultaneously obtain the multi-dimensional crack feature dataset of the junction area;

[0008] S2, based on the multidimensional crack feature dataset, defines the local damage index and maps it to generate the equivalent stiffness reduction coefficient of the junction zone element;

[0009] S3, the equivalent stiffness reduction factor is imported into the initial benchmark model, and the actual stress state of the junction area and the internal force variation increment of the whole ring structure are inverted by simulating the internal force redistribution process.

[0010] S4 combines the inverted stress state and internal force variation increments to perform local bearing capacity verification and global derivative risk assessment, outputting structural safety status classification and corresponding engineering intervention suggestions.

[0011] Furthermore, the specific process of constructing the initial baseline model and collecting the crack dataset in step S1 includes:

[0012] S11, extract the geometric dimensions, material strength and surrounding rock grade parameters of the tunnel design stage, and construct an idealized load-structure initial model;

[0013] S12, using non-destructive testing methods to obtain the measured thickness of the lining in the junction area and the actual strength of the concrete, the geometric and material properties of the initial model are corrected to form a quasi-real reference surface;

[0014] S13 extracts multidimensional features of apparent cracks in the junction area through on-site monitoring, including crack width, extension length, distribution density and orientation, and structures them into an inversion input dataset.

[0015] Furthermore, the parameter correction of the initial model in step S12 specifically includes correcting the unit cross-sectional dimensions of the model using the actual lining thickness detected by ground-penetrating radar, and correcting the elastic modulus of the model using the concrete strength detected by rebound method or ultrasonic method, so that the reference model can reflect the true structural stiffness after construction deviation.

[0016] Furthermore, in step S2, the process of processing the equivalent stiffness reduction factor includes:

[0017] S21. Based on the logical correlation rule between crack width and effective compression zone height of the section, the section damage depth after the concrete tension zone exits the work is deduced.

[0018] S22 uses crack extension length, distribution density and orientation as correction operators to perform logical compensation on damage depth and defines a damage index that comprehensively reflects the degree of cross-sectional weakening.

[0019] S23, through analytical methods or a preset multi-condition parameter database, maps the damage index to the ratio of the actual bending stiffness of the section to the quasi-true initial stiffness, thus generating a local equivalent stiffness reduction coefficient.

[0020] Furthermore, the definition logic of the damage index is as follows: the maximum crack width is used as the core basis for quantitative damage. When the crack direction tends to be perpendicular to the direction of the principal stress of the lining, or the crack distribution density exceeds the preset threshold, the damage index is increased by the penalty coefficient to simulate the superimposed destructive effect of multidimensional cracks on structural integrity.

[0021] Furthermore, in step S3, the internal force redistribution process specifically includes:

[0022] S31, the generated equivalent stiffness reduction coefficient is assigned to the corresponding junction element in the quasi-real benchmark model, while keeping the stiffness properties of the remaining non-cracked regions and the external load boundary unchanged.

[0023] S32, based on the degree of stiffness reduction, triggers the corresponding reanalysis strategy, and simulates the process of load transfer from the severely damaged junction area to the surrounding hard nodes through finite element calculation;

[0024] S33 extracts the inversion bending moment and inversion axial force of the junction zone under equilibrium state, as well as the internal force migration increment of adjacent nodes.

[0025] Furthermore, the reanalysis strategy specifically includes:

[0026] The equivalent stiffness reduction factor is within the preset mild damage range, and the redistribution trend is quickly obtained using the linear reanalysis method;

[0027] If the reduction factor is lower than the preset severe damage threshold, the algorithm will automatically switch to a convergence algorithm with a nonlinear iterative mechanism until the residual internal force field that meets the equilibrium condition is calculated.

[0028] Furthermore, in step S4, performing a comprehensive evaluation and outputting recommendations includes:

[0029] S41, use the inverted real internal forces to perform local residual bearing capacity verification of the junction area, and calculate the structural safety factor under the current state;

[0030] S42, assess whether the increase in internal force migration at adjacent nodes leads to the risk of overload damage in other intact areas, and determine whether there is a chain reaction of structural damage.

[0031] S43 integrates local safety factors and global derived risk indicators to construct an assessment matrix, outputting the structural safety status level and corresponding monitoring or reinforcement recommendations.

[0032] Furthermore, the judgment rules for global derivative risk assessment include: comparing the newly added internal force values ​​in the arch crown and arch waist areas after the redistribution of internal forces with the ultimate resistance of the material in that area. If the newly added internal forces cause the originally safe area to enter a plastic state or exceed the extreme value of bearing capacity, then it is determined that there is a high risk of "internal force transfer type failure".

[0033] Furthermore, the linkage rules between structural safety status classification and engineering intervention include: dividing the safety status into four risk levels from 1 to 4; where level 1 corresponds to normal monitoring, level 2 corresponds to increased monitoring frequency, level 3 corresponds to load-limited operation or local grouting reinforcement, and level 4 corresponds to emergency support reinforcement or replacement lining, so as to achieve proactive safety prevention based on the inversion results.

[0034] The beneficial effects of the above-described technical solutions provided in the embodiments of the present invention include at least the following:

[0035] 1. Traditional assessments rely on pressure cells or strain gauges embedded during the construction phase. For tunnels that are already in operation and have not been equipped with sensors, only qualitative assessments can be performed. This solution reverse-engineers the internal stress through apparent crack data, solving the problem of missing stress state monitoring in in-service tunnels. Moreover, it does not require structural damage, thus reducing assessment costs.

[0036] 2. Existing technologies are mostly based on ideal design drawings for modeling, ignoring construction deviations (such as lining thinning and concrete strength fluctuations). This solution corrects the initial parameters of the model through non-destructive testing methods such as ground-penetrating radar, ensuring the objectivity of the mechanical calculation base and making the evaluation results closer to the actual engineering situation.

[0037] 3. This scheme utilizes the principle of internal force redistribution in statically indeterminate structures, which can not only calculate the residual bearing capacity at the defect site, but also quantitatively identify the "secondary risks" of load transfer to areas such as the arch crown and arch waist caused by local weakening, thereby achieving advanced and accurate pre-control of the risk of overall tunnel collapse.

[0038] Other features and advantages of the invention will be set forth in the description which follows, and will be apparent in part from the description, or may be learned by practicing the invention. The objects and other advantages of the invention may be realized and obtained by means of the structures particularly pointed out in the written description, claims, and drawings.

[0039] The technical solution of the present invention will be further described in detail below with reference to the accompanying drawings and embodiments. Attached Figure Description

[0040] The accompanying drawings are provided to further illustrate the invention and form part of the specification. They are used in conjunction with embodiments of the invention to explain the invention and do not constitute a limitation thereof. In the drawings:

[0041] Figure 1This is a flowchart of the stress state assessment method for the junction area between the tunnel invert and the sidewall, as disclosed in an embodiment of the present invention.

[0042] Figure 2 for Figure 1 The flowchart of step S1 in the process;

[0043] Figure 3 for Figure 1 The flowchart of step S2 in the process;

[0044] Figure 4 for Figure 1 The flowchart of step S3 in the process;

[0045] Figure 5 for Figure 1 The flowchart of step S4 in the process. Detailed Implementation

[0046] Exemplary embodiments of the present disclosure will now be described in more detail with reference to the accompanying drawings. While exemplary embodiments of the present disclosure are shown in the drawings, it should be understood that the present disclosure may be implemented in various forms and should not be limited to the embodiments set forth herein. Rather, these embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the disclosure to those skilled in the art.

[0047] like Figure 1-5 As shown, this embodiment of the invention provides an assessment method for the stress state of the junction area between the tunnel invert and the sidewall based on crack width inversion. It mainly targets the quantitative stress assessment of cracks caused by severe eccentric compression in the junction area (arch foot) between the tunnel invert and the sidewall under conditions of ultra-shallow burial (such as burial depth 0~20m) and strongly weathered soft surrounding rock (such as strongly weathered sandy slate).

[0048] In this embodiment, the core logic of step S1 lies in eliminating the "distortion" between the theoretical design value and the actual construction value through the fusion of multi-source data, thereby providing a high-precision digital physical foundation for subsequent stress inversion. The specific implementation process is as follows:

[0049] S11, Construct an idealized load-structure initial model.

[0050] First, geometric parameters and engineering environmental parameters are extracted from the tunnel design data.

[0051] In this embodiment, for the D-shaped cross-section of the target tunnel portal section, the design thickness of the secondary lining, the design strength of the concrete, and the reinforcement configuration parameters are obtained.

[0052] Simultaneously, based on the geological survey report, the surrounding rock grade and physical and mechanical properties (such as the elastic resistance coefficient of strongly weathered slate) are determined. Using finite element software, a full-section beam element or solid element model is established based on the "load-structure" model. Vertical pressure and lateral earth pressure of the full soil column are applied to form an idealized stress benchmark.

[0053] S12, Correction and construction of the quasi-true reference surface.

[0054] Due to objective deviations such as uneven lining thickness and discrete concrete strength during on-site construction, this step involves parametric correction of the ideal model in S11 by introducing non-destructive testing data. This includes: lining geometry correction, material stiffness correction, and contact state correction.

[0055] Lining geometry correction: Ground-penetrating radar is used to continuously scan the junction area between the invert arch and the sidewall to obtain the true thickness profile inside the lining. If the measured thickness is 480mm (design thickness is 500mm), the cross-sectional geometric properties of the corresponding element in the finite element model are updated in real time.

[0056] Material stiffness correction: The compressive strength of concrete in the junction area is determined by the rebound method or the combined ultrasonic rebound method. The actual elastic modulus of concrete is calculated based on the measured strength. If the measured strength only reaches 90% of the design strength, the material elastic properties of the model unit are adjusted down accordingly.

[0057] Contact state correction: Based on the results of ground-penetrating radar detection, if a void is found between the back of the lining and the surrounding rock, the elastic support (simulating the surrounding rock constraint) in this area is logically set to "failure" in the model, thereby constructing a "quasi-realistic" calculation reference surface that is close to the engineering entity.

[0058] S13, Collection of multi-dimensional crack feature dataset in the junction area.

[0059] While constructing the near-realistic model, quantitative data on surface defects in the junction area are collected, including visual identification and contact-based precision monitoring.

[0060] Visual recognition acquisition: High-resolution industrial cameras or drone inspection systems are used to capture images of the junction area. Cracks are identified through digital image processing technology. The acquisition indicators include not only the maximum crack width, but also the total length of the cracks, the number of cracks per unit area (distribution density), and the angle between the cracks and the tunnel axis (direction).

[0061] Contact-based precision monitoring: Crack gauges are deployed at key stress points to monitor the dynamic opening and closing width of cracks under different environmental loads (such as water level changes) in real time. Finally, the above parameters such as width, length, density, and orientation are encapsulated into a structured feature dataset, which serves as the input source for calculating the damage index in the subsequent S2 step.

[0062] In this embodiment, the core principle of step S2 lies in establishing the conversion logic between "apparent damage" and "structural internal mechanical properties," quantifying the visible multidimensional crack features into stiffness degradation factors that can be identified by the computational model. The specific implementation process is as follows:

[0063] S21, establish the logical conversion relationship between apparent cracks and cross-sectional damage depth.

[0064] This step is based on the "plane section assumption" and "reinforcement strain compatibility logic" in mechanics, and uses the crack width to inversely deduce the offset of the neutral axis of the section and the change in the height of the effective compression zone. Specifically, when cracks occur at the junction of the tunnel invert and the sidewall, the concrete on the tension side of the section gradually withdraws from its function, resulting in a decrease in the effective moment of inertia of the section. The larger the crack width, the more severe the offset of the compression zone of the neutral axis of the section.

[0065] Specifically, based on the maximum crack width collected, the calculation logic for the damage depth of the cross section is set. When the crack width reaches a certain critical value, it is logically determined that the concrete in the tension zone has completely failed, and the strain increment of the tensile steel is converted into a quantitative basis for the height degradation of the compression zone of the cross section.

[0066] S22 defines the local damage index and introduces a correction operator.

[0067] To comprehensively reflect the weakening effect of cracks on structural integrity, this step not only considers the "opening degree" of cracks but also uses a damage index to comprehensively weight multidimensional characteristics, including:

[0068] Length correction logic: A crack length correction operator is introduced. If a crack runs across the entire junction section, its damage to the continuity of the section is much greater than that of a local short crack. In implementation, the crack depth is amplified by setting a length threshold.

[0069] Distribution density and orientation correction: A distribution density correction coefficient is introduced. If multiple parallel cracks appear within a unit length, the area is judged to have "diffuse damage". The accelerated degradation of the overall stiffness of the cross section is simulated by increasing the weighting value of the damage index. At the same time, if the crack orientation is parallel to the tunnel axis (i.e. perpendicular to the direction of the principal tensile stress), a higher damage weight is assigned.

[0070] S23 generates the equivalent stiffness reduction factor.

[0071] This step transforms the qualitative damage index into a quantitative stiffness reduction parameter for subsequent model stiffness resetting. A multi-condition database lookup method is used, which involves simulating cracking conditions of different depths and widths using finite element analysis software to generate a multi-dimensional comparison database of "crack characteristics-stiffness degradation". In the actual assessment, based on the dataset collected in S13, the equivalent stiffness reduction coefficient that best fits the actual on-site conditions is automatically retrieved and interpolated.

[0072] Step S2 uses the multidimensional crack characteristics (width, length, density, and orientation) collected on-site as input variables and utilizes the tensile stiffening effect and the degradation principle of the effective compression zone of the cross section to construct a multidimensional damage assessment system. Its core working logic is as follows: First, the core indicator of "crack width" is transformed into "the degradation amount of the compression zone height of the cross section" using the plane section assumption to establish the basic value of damage; then, correction operators such as length, density, and orientation are introduced, and the basic damage is corrected through weighted logic to form a comprehensive damage index that can fully characterize the degree of structural weakening; finally, the damage index is quantitatively mapped to the equivalent stiffness reduction factor of the cross section through analytical calculation or a preset finite element parameter database.

[0073] This process not only overcomes the limitations of traditional methods that rely solely on width for qualitative evaluation, but also quantifies the actual weakening effect of complex crack clusters on the bending stiffness of the tunnel arch foot through the correction logic of multiple embodiments, providing a calculable data foundation for subsequent accurate simulation of internal force redistribution.

[0074] The core logic of step S3 is to utilize the load transfer characteristics of statically indeterminate structures to simulate the "stress reorganization" that occurs after local damage to the structure, thereby achieving the reverse solution of the actual stress state at the junction of the invert arch and the sidewall. The specific implementation process is as follows:

[0075] S31, Resetting the local stiffness properties of the model and mapping the elements.

[0076] This step involves precisely injecting the stiffness reduction characteristics quantified in the aforementioned steps into a quasi-realistic benchmark model, thereby constructing a non-homogeneous structure calculation system with damage awareness. Specifically, the geometric units (i.e., the junction units between the invert arch and the sidewall) corresponding to the locations of cracks in the tunnel are first identified in the model, and the bending stiffness properties of these specific units are modified according to a preset reduction ratio.

[0077] It should be noted that, considering the possible differences in the stress environment of the left and right arch feet of the tunnel, if the measured data shows that the cracks on one side are more serious, the stiffness of the unit on that side will be adjusted to a higher degree. For parts such as the arch crown and arch waist where no cracks are found, their original stiffness will be strictly maintained, so as to truly reproduce the mechanical state of "local cracking of defects and overall structural adjustment" in the model.

[0078] 3.2 Simulation and calculation strategy for redistribution of internal forces in structures.

[0079] After completing the local stiffness reduction treatment, this step, while maintaining the original external water and soil pressure load unchanged, initiates the structural equilibrium weight analysis program, including:

[0080] Linear reanalysis strategy: If the stiffness reduction in the junction area is within a slight range, the system quickly calculates the trend of moment redistribution due to the "softening" of the arch foot through a linear solver;

[0081] Nonlinear iterative strategy: If the damage in the junction area is severe enough to cause the local area to enter the material plastic stage, a nonlinear iterative mechanism is used for in-depth simulation. This process can capture the dynamic trajectory of the load spontaneously migrating from the severely damaged arch foot to the more rigid arch waist, invert arch and other areas, until the internal force field and displacement field of the whole ring structure reach a new equilibrium point in mechanical sense.

[0082] 3.3, Extraction of internal forces from inversion and verification of mechanical equilibrium.

[0083] After the model reaches reequilibrium, the system extracts key stress indicators from the calculation results as evaluation criteria, including:

[0084] Core parameter inversion: The key is to extract the inversion bending moment, inversion axial force and inversion shear force of the junction section. These parameters truly reflect the actual load share that this part can bear after taking crack damage into account.

[0085] Related node monitoring: Simultaneously extract the changes in internal forces in adjacent areas (such as the waist of the arch and the center of the inverted arch) and the deformation displacement increment of the entire ring. Through logical verification, verify the balance relationship of the total internal forces of the entire ring to ensure that the inverted force data has a solid physical support and eliminate the interference of calculation fluctuations.

[0086] This step uses the stiffness degradation parameters obtained in the previous stage as a physical disturbance source, which is applied to the established quasi-realistic benchmark model, thereby breaking the original mechanical equilibrium state. Its core working logic is to use the natural law of spontaneous distribution of internal forces in statically indeterminate structures according to stiffness ratio to simulate the "unloading" process of tunnel lining after arch foot cracking and weakening of bending stiffness. That is, the excess load originally borne by the junction area is logically transferred to the surrounding intact nodes.

[0087] Through this process, this solution not only accurately inverts the current actual stress state (bending moment, axial force) of the junction area, but more importantly, it quantifies the disturbance intensity of local defects on the entire ring structure system by identifying the migration trajectory of internal forces throughout the ring. This step plays a crucial role in the overall process, transforming surface crack phenomena into internal force values, providing core mechanical evidence for subsequent assessment of potential damage transfer risks and structural classification early warning.

[0088] In this embodiment, the core logic of step S4 lies in using the real mechanical parameters obtained from the inversion to perform a "physical examination and grading" of the structure. This not only focuses on the residual strength of the damaged areas but also on the risk of secondary disasters caused by the transfer of internal forces. The specific implementation process is as follows:

[0089] 4.1 Verification of the local residual bearing capacity of the junction area between the invert arch and the side wall.

[0090] This step quantifies the local safety margin of the junction zone by comparing the inverted internal forces with the actual resistance of the damaged section. Specifically, the inverted bending moment and inverted axial force extracted in step S3 are substituted into the section strength calculation model after stiffness reduction correction.

[0091] Considering that the section has been reduced in the compression zone due to cracking, this embodiment uses the reduced effective geometric parameters to recalculate the ultimate bearing capacity of the section under eccentric compression. If the combination point of the true bending moment and axial force obtained by inversion approaches or exceeds the strength envelope of the material, it is determined that the local position is on the edge of instability. The local safety factor of the part is obtained by calculating the ratio of the ultimate resistance to the inverted load effect.

[0092] 4.2 Risk Derivative Assessment of the Full Ring Structure of the Tunnel

[0093] This step focuses on investigating the risk of "overloading" in the surrounding area caused by the "unloading" of the arch foot, reflecting the principle of overall structural assessment. It retrieves the internal force migration increments of adjacent key nodes (such as the arch crown, arch waist, and invert center) retrieved in step S3 and superimposes them onto the initial stress state of that part.

[0094] Regarding the determination of cascading failure, even if no cracks have yet appeared in the crown area, if the inversion calculation shows that the increase in the crown bending moment exceeds a specific threshold (such as 85%) of its design bearing capacity due to the weakening of the arch foot stiffness, then logically it is determined that the structure is at risk of "internal force transfer type failure", that is, local cracking may induce overall collapse.

[0095] 4.3 Structural safety status classification and early warning recommendations output.

[0096] Based on the aforementioned local and global quantitative indicators, this step outputs the final engineering instructions through an analysis matrix, establishing a multi-indicator decision matrix that includes crack width, local safety factor, and derived risk level, dividing the safety status into four early warning levels, where:

[0097] Level 1 (Normal): The local safety factor is sufficient, and the internal force transfer is slight. It is recommended to maintain routine monitoring.

[0098] Level 2 (Note): The safety factor has decreased, and it is recommended to increase the frequency of crack monitoring;

[0099] Level 3 (Warning): The local bearing capacity is close to the limit or there is significant overload in the surrounding area. It is recommended to take measures such as load-limited operation, local grouting at the arch foot, or anchor reinforcement.

[0100] Level 4 (Danger): The inverted internal force exceeds the limit, or there is a clear risk of chain reaction damage. Logically, this directly triggers an emergency warning. It is recommended to take mandatory measures such as arch reinforcement, replacement lining, or emergency support.

[0101] This step accurately calculates the true local safety factor of the weak link, the junction area (arch foot), by coupling the inverted internal forces with the properties of the damaged section. Then, using the full-ring internal force migration data, the overload risk in areas such as the arch crown and arch waist caused by local weakening is dynamically investigated, thereby identifying potential cascading damage paths.

[0102] This process transforms previously isolated crack monitoring data into mechanical safety indicators with engineering guidance, ensuring that the assessment results not only cover the survival status of the affected areas but also predict the collapse tendency of the overall structure. By establishing a tiered early warning mechanism, this solution provides logical decision support for tunnel operation and maintenance, moving from "passive repair" to "active intervention," ensuring the safe and controlled operation of tunnel structures in ultra-shallow buried fractured surrounding rock environments.

[0103] The tunnel stress assessment method proposed in this invention is based on the mechanical logic chain of "digital benchmark correction, damage mapping and internal force redistribution inversion". First, by introducing ground-penetrating radar thickness measurement and rebound strength detection, random deviations such as lining thinning and strength fluctuations generated during construction are incorporated into the initial model to construct a "quasi-real benchmark surface" that can objectively reflect the current state of the project, thus solving the pain point of inaccurate assessment benchmark.

[0104] Subsequently, this method utilizes the multidimensional characteristics (width, length, density, and orientation) of apparent cracks as "sensory signals" of structural performance degradation. Through preset mechanical mapping rules (such as the degradation principle of the compression zone of the cross section and the penalty operator), these signals are transformed into "equivalent stiffness reduction coefficients" that can be recognized by the computational model, thereby realizing the quantitative conversion of apparent defects into internal mechanical damage.

[0105] Finally, utilizing the natural law of the distribution of internal forces in statically indeterminate structures according to stiffness ratio, the "unloading" process of the tunnel lining after arch foot cracking and stiffness reduction is simulated. By inverting and calculating this redistributed mechanical equilibrium state, not only can the current real residual bearing capacity of the junction area be accurately extracted, but also the derivative risks in adjacent areas such as the arch crown and arch waist caused by "internal force transfer" can be identified. This assessment principle, which proceeds from the surface to the core and from local defects to the overall safety situation, enables accurate diagnosis and graded early warning of hidden risks in tunnel structures.

[0106] It should be understood that the specific order or hierarchy of steps in the disclosed process is an example of an exemplary method. Based on design preferences, it should be understood that the specific order or hierarchy of steps in the process may be rearranged without departing from the scope of this disclosure. The appended method claims provide elements of various steps in an exemplary order and are not intended to limit the scope to the specific order or hierarchy described.

[0107] In the detailed description above, various features are combined together in a single embodiment to simplify this disclosure. This approach to disclosure should not be construed as reflecting an intention that embodiments of the claimed subject matter require more features than are explicitly stated in each claim. Rather, as reflected in the appended claims, the invention is presented with fewer features than all of the features in a single disclosed embodiment. Therefore, the appended claims are hereby explicitly incorporated into the detailed description, with each claim representing a separate preferred embodiment of the invention.

[0108] Those skilled in the art will also understand that the various illustrative logic blocks, modules, circuits, and algorithm steps described in conjunction with the embodiments herein can be implemented as electronic hardware, computer software, or a combination thereof. To clearly illustrate the interchangeability between hardware and software, the various illustrative components, blocks, modules, circuits, and steps described above are generally described in terms of their functionality. Whether such functionality is implemented as hardware or software depends on the specific application and the design constraints imposed on the overall system. Those skilled in the art can implement the described functionality in alternative ways for each specific application; however, such implementation decisions should not be construed as departing from the scope of this disclosure.

[0109] The steps of the methods or algorithms described in conjunction with the embodiments herein can be directly embodied in hardware, software modules executed by a processor, or a combination thereof. The software modules can reside in RAM memory, flash memory, ROM memory, EPROM memory, EEPROM memory, registers, hard disks, removable disks, CD-ROMs, or any other form of storage medium well known in the art. An exemplary storage medium is connected to the processor, enabling the processor to read information from and write information to the storage medium. Of course, the storage medium can also be a component of the processor. The processor and storage medium can reside in an ASIC. The ASIC can reside in a user terminal. Alternatively, the processor and storage medium can exist as discrete components in the user terminal.

[0110] For software implementation, the techniques described in this application can be implemented using modules (e.g., procedures, functions, etc.) that perform the functions described in this application. This software code can be stored in memory units and executed by a processor. The memory units can be implemented within the processor or outside the processor; in the latter case, they are communicatively coupled to the processor via various means, as is well known in the art.

[0111] The foregoing description includes examples of one or more embodiments. It is certainly impossible to describe all possible combinations of components or methods in order to describe the above embodiments, but those skilled in the art will recognize that further combinations and arrangements of the various embodiments are possible. Therefore, the embodiments described herein are intended to cover all such changes, modifications, and variations that fall within the scope of the appended claims. Furthermore, the term "comprising" as used in the specification or claims is interpreted in a manner similar to the term "including," as interpreted when used as a conjunction in the claims. Additionally, the use of any term "or" in the specification of the claims is intended to mean "non-exclusive or."

Claims

1. A method for evaluating the stress state of the junction zone between the tunnel invert and sidewall based on crack width inversion, characterized in that, Includes the following steps: S1, collect the initial design parameters and field measured data of the tunnel portal section, construct a near-realistic full-section stress initial benchmark model, and simultaneously obtain the multi-dimensional crack feature dataset of the junction area; S2, based on the multidimensional crack feature dataset, defines the local damage index and maps it to generate the equivalent stiffness reduction coefficient of the junction zone element; S3, the equivalent stiffness reduction factor is imported into the initial benchmark model, and the actual stress state of the junction area and the internal force variation increment of the whole ring structure are inverted by simulating the internal force redistribution process. S4 combines the inverted stress state and internal force variation increments to perform local bearing capacity verification and global derivative risk assessment, outputting structural safety status classification and corresponding engineering intervention suggestions.

2. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 1, characterized in that, The specific process of constructing the initial baseline model and collecting the crack dataset in step S1 includes: S11, extract the geometric dimensions, material strength and surrounding rock grade parameters of the tunnel design stage, and construct an idealized load-structure initial model; S12, using non-destructive testing methods to obtain the measured thickness of the lining in the junction area and the actual strength of the concrete, the geometric and material properties of the initial model are corrected to form a quasi-real reference surface; S13 extracts multidimensional features of apparent cracks in the junction area through on-site monitoring, including crack width, extension length, distribution density and orientation, and structures them into an inversion input dataset.

3. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 2, characterized in that, The parameter correction of the initial model in step S12 specifically includes correcting the unit cross-sectional dimensions of the model using the actual lining thickness detected by ground-penetrating radar, and correcting the elastic modulus of the model using the concrete strength detected by rebound method or ultrasonic method, so that the reference model can reflect the true stiffness of the structure after construction deviation.

4. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 1, characterized in that, In step S2, the process of processing the equivalent stiffness reduction factor includes: S21. Based on the logical correlation rule between crack width and effective compression zone height of the section, the section damage depth after the concrete tension zone exits the work is deduced. S22 uses crack extension length, distribution density and orientation as correction operators to perform logical compensation on damage depth and defines a damage index that comprehensively reflects the degree of cross-sectional weakening. S23, through analytical methods or a preset multi-condition parameter database, maps the damage index to the ratio of the actual bending stiffness of the section to the quasi-true initial stiffness, thus generating a local equivalent stiffness reduction coefficient.

5. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 4, characterized in that, The definition logic of the damage index is as follows: the maximum crack width is used as the core basis for quantitative damage. When the crack direction tends to be perpendicular to the direction of the principal stress of the lining, or the crack distribution density exceeds the preset threshold, the damage index is increased by the penalty coefficient to simulate the superimposed damage effect of multidimensional cracks on the structural integrity.

6. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 1, characterized in that, In step S3, the internal force redistribution process specifically includes: S31, the generated equivalent stiffness reduction coefficient is assigned to the corresponding junction element in the quasi-real benchmark model, while keeping the stiffness properties of the remaining non-cracked regions and the external load boundary unchanged. S32, based on the degree of stiffness reduction, triggers the corresponding reanalysis strategy, and simulates the process of load transfer from the severely damaged junction area to the surrounding hard nodes through finite element calculation; S33 extracts the inversion bending moment and inversion axial force of the junction area under equilibrium state, as well as the internal force migration increment of adjacent nodes.

7. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 6, characterized in that, The reanalysis strategy specifically includes: The equivalent stiffness reduction factor is within the preset mild damage range, and the redistribution trend is quickly obtained using the linear reanalysis method; If the reduction factor is lower than the preset severe damage threshold, the algorithm will automatically switch to a convergence algorithm with a nonlinear iterative mechanism until the residual internal force field that meets the equilibrium condition is calculated.

8. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 1, characterized in that, In step S4, the comprehensive evaluation and recommendations are output, including: S41, use the inverted real internal forces to perform local residual bearing capacity verification of the junction area, and calculate the structural safety factor under the current state; S42, assess whether the increase in internal force migration at adjacent nodes leads to the risk of overload damage in other intact areas, and determine whether there is a chain reaction of structural damage. S43 integrates local safety factors and global derived risk indicators to construct an assessment matrix, outputting the structural safety status level and corresponding monitoring or reinforcement recommendations.

9. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 8, characterized in that, The judgment rules for global derivative risk assessment include: comparing the newly added internal force values ​​in the arch crown and arch waist areas after the redistribution of internal forces with the ultimate resistance of the material in that area. If the newly added internal forces cause the originally safe area to enter a plastic state or exceed the extreme value of bearing capacity, then it is determined that there is a high risk of "internal force transfer type failure".

10. The method for evaluating the stress state of the tunnel invert arch and sidewall junction area based on crack width inversion as described in claim 8, characterized in that, The linkage rules between structural safety status classification and engineering intervention include: dividing the safety status into four risk levels from 1 to 4; where level 1 corresponds to normal monitoring, level 2 corresponds to increased monitoring frequency, level 3 corresponds to load-limited operation or local grouting reinforcement, and level 4 corresponds to emergency support reinforcement or replacement lining, so as to achieve proactive safety prevention based on the inversion results.