A forming device and manufacturing method for counterweight pipes for marine aquaculture cages
By using the rotation of the adjusting ring and the diverting ring in the marine aquaculture cage counterweight pipe forming device to control the flow of materials in the inner and outer layers and form an interlocking structure, the problems of low bonding strength between the inner and outer layers and single density adjustment are solved, and the flexibility of bonding strength and density adjustment is realized.
Patent Information
- Application Number
- CN202611473092.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-21
- Publication Date
- 2026-11-17
AI Technical Summary
The existing counterweight pipes for marine aquaculture cages have low bonding strength between the inner and outer layers during the molding process, and the density adjustment method is limited, making it difficult to meet the requirements for normal sag and counterweight of the netting.
The forming device, consisting of a mold shell, shaft core, and interlayer bushing arranged coaxially, controls the flow channels and proportions of materials in the inner and outer layers by adjusting the relative rotation of the ring sleeve and the diversion ring sleeve, forming an inner and outer layer interlocking structure, improving the bonding strength, and adjusting the density by adjusting the angle of the annular connecting area.
It improves the bonding strength between the inner and outer layers, makes density adjustment more flexible, and meets the counterweight requirements of different aquaculture conditions in different sea areas.
Smart Images

Figure CN123104011A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of pipe forming technology, and more specifically, to a device for forming counterweight pipes for marine aquaculture cages, and also to a method for manufacturing counterweight pipes using the device. Background Technology
[0002] Marine aquaculture cages typically require counterweight structures to maintain the netting's proper hanging and unfolding in the water, and counterweight tubing is one commonly used form of counterweight. Counterweight tubing consists of an inner layer and an outer layer. The inner layer serves as the counterweight and has a higher density, while the outer layer provides protection. During the extrusion molding process of the counterweight tubing, the large proportion of counterweight material in the inner layer leads to a relatively large difference in physical properties between the inner and outer layer materials, resulting in a relatively low connection strength at the interface between the inner and outer layers.
[0003] Furthermore, the density of the counterweight tubing is critical. Excessive density will result in excessive downward counterweight to the mesh, causing tension on the mesh of the gabion; insufficient density will affect the counterweight effect, preventing the mesh from hanging properly. In existing double-layer feeding molding dies, the adjustment of the material ratio between the inner and outer layers is typically achieved by adjusting the pressure of both materials, a relatively simple adjustment method. Summary of the Invention
[0004] The purpose of this invention is to overcome the shortcomings of the prior art and provide a device for forming counterweight pipes for marine aquaculture cages and a method for manufacturing counterweight pipes. During the forming process of the counterweight pipes, the joint between the inner layer material and the outer layer material can form an interlocking structure, thereby improving the strength performance of the joint between the two.
[0005] To achieve the above objectives, the present invention adopts the following technical solution:
[0006] A device for forming counterweight pipes for marine aquaculture cages includes a mold shell, a shaft core, and a sandwich bushing arranged coaxially. The shaft core is located on the inner circumference of the mold shell, and the sandwich bushing is sleeved between the shaft core and the mold shell. An annular inner material channel is formed between the outer circumference of the shaft core and the inner circumference of the sandwich bushing, and an annular outer material channel is formed between the outer circumference of the sandwich bushing and the inner circumference of the mold shell. The sandwich bushing has a tapered portion on its output side that tapers towards the output end, and the end of the tapered portion has an end face. A diversion ring is installed on the inner circumference of the tapered portion. The diversion ring includes a plurality of guide strips arranged in an annular array and an extended ring integrally connected to the inner circumference of each guide strip. A flow guiding interval is formed between adjacent flow guiding strips; the output side of the interlayer bushing is provided with an adjusting ring sleeve that is coaxially engaged with the flow dividing ring sleeve. Multiple flow guiding strips are integrally connected to the inner circumference of the adjusting ring sleeve. The number of flow guiding strips is the same as that of flow guiding strips and they correspond one-to-one. A flow guiding interval is formed between adjacent flow guiding strips. A flow guiding channel is opened in each flow guiding strip. The flow guiding intervals 1 and 2 are axially connected to form an inner layer interval for the flow of inner layer material. The flow guiding channel forms an outer layer interval. The outer layer interval and the inner layer interval are distributed circumferentially to form an annular transition section sandwiched between the outer layer material channel and the inner layer material channel.
[0007] Furthermore, the adjusting ring sleeve can rotate axially relative to the diverting ring sleeve; when the first guide strip and the second guide strip are directly opposite each other, the channel of the inner layer spacer is fully opened; when the first guide strip and the second guide strip are misaligned, the first guide spacer and the second guide spacer block each other, causing the channel of the inner layer spacer to narrow.
[0008] Furthermore, the mold shell includes a front mold shell and a rear mold shell that are axially connected to each other. An installation ring is sleeved between the front mold shell and the rear mold shell. The inner circumference of the installation ring forms part of the outer layer material channel. An adjustment ring is coaxially installed on the inner circumference of the installation ring. The outer circumference of the adjustment ring and the inner circumference of the installation ring form an outer layer flow channel that communicates with the outer layer material channel.
[0009] 4. The counterweight pipe forming device according to claim 3, wherein the adjusting ring sleeve and the mounting ring sleeve are fixedly connected by a plurality of connecting ribs to support the adjusting ring sleeve.
[0010] 5. The counterweight pipe forming device according to claim 1, characterized in that the end of the second guide bar facing the input side is closed, the outer periphery of the adjusting ring sleeve near the input side is provided with an inlet portion communicating with the guide channel, and the end of the second guide bar facing the output side is provided with an outlet portion communicating with the guide channel.
[0011] Furthermore, an inclined guide portion is formed on the inner side of the inlet portion.
[0012] Furthermore, one end of the extension ring extends into the inner circumference of the interlayer bushing, and the other end extends out of the interlayer bushing toward the output side. The outer circumferential dimension of the extension ring is adapted to the inner circumferential dimension of the adjusting ring sleeve, and the adjusting ring sleeve is fitted onto the outer circumference of the portion of the extension ring that extends out of the interlayer bushing.
[0013] Furthermore, one end of the first guide bar is flush with the end face of the tapered portion; the outer periphery of the extended ring body is spaced apart from the inner periphery of the interlayer bushing, and an inner flow channel for the inner layer material to flow is formed between the inner periphery of the interlayer bushing, the outer periphery of the extended ring body, and two adjacent first guide bars.
[0014] The present invention also provides a method for manufacturing counterweight pipe, using the counterweight pipe forming device as described above, comprising the following steps: supplying inner layer material through the inner layer material channel, supplying outer layer material through the outer layer material channel, outputting the inner layer material through an inner layer interval formed by the first and second flow guides, and outputting the outer layer material through an outer layer interval formed by the flow guides, so that the inner layer material and the outer layer material form a circumferentially spaced interlocking structure at the annular transition section, and forming a counterweight pipe with interlocking inner and outer layers by extrusion molding.
[0015] Furthermore, by rotating and adjusting the relative angle between the adjusting ring and the diverting ring, the first guide strip and the second guide strip are aligned or misaligned, thereby adjusting the channel size of the inner layer partition and thus adjusting the ratio of the inner layer material to the outer layer material.
[0016] In summary, the present invention has the following beneficial effects:
[0017] By setting an annular connecting area between the outer and inner material channels, the annular connecting area includes an outer layer spacer and an inner layer spacer that are spaced apart circumferentially. The outer layer material is output through the outer layer spacer and the inner layer material is output through the inner layer spacer, so that the inner and outer layer materials form a circumferentially spaced interlocking structure in the bonding area. The inner and outer layers no longer rely solely on material bonding, which can improve the bonding strength performance of the double-layer materials.
[0018] By adjusting the relative axial rotation of the ring sleeve and the diversion ring sleeve, the guide strip one and the guide strip two can be aligned or misaligned, thereby controlling the size of the channel in the inner layer partition. This allows for fine-tuning of the ratio of inner layer material to outer layer material in the annular connection area, and thus adjusting the density of the counterweight pipe. Moreover, this adjustment can be achieved simply by rotation, making the ratio adjustment of the two materials in the intermediate transition layer more flexible. Attached Figure Description
[0019] Figure 1 This is a schematic cross-sectional view of the counterweight tube forming device in this embodiment;
[0020] Figure 2 for Figure 1 A magnified view of part A in the middle;
[0021] Figure 3 This is a cross-sectional view of the counterweight tube forming device in this embodiment;
[0022] Figure 4 This is a schematic diagram of the mating structure between the adjusting ring and the diversion ring in this embodiment;
[0023] Figure 5 This is a three-dimensional structural diagram of the adjusting ring and the diversion ring in this embodiment;
[0024] Figure 6 This is a schematic diagram of the cross-sectional structure of the extrusion channel of the counterweight tube forming device in this embodiment.
[0025] Reference numerals: Mold shell 1; Front mold shell 101; Rear mold shell 102; Shaft core 2; Interlayer bushing 3; Conical part 31; End face 32; Inner layer material channel 4; Outer layer material channel 5; Adjusting ring sleeve 6; Guide bar II 61; Guide interval II 62; Inlet part 63; Inclined guide part 64; Guide channel 65; Outlet part 66; Outer layer flow channel part 67; Mounting ring sleeve 7; Dividing ring sleeve 8; Guide bar I 81; Guide interval I 82; Extension ring body 83; Inner layer flow channel part 84; Annular connecting area 9. Detailed Implementation
[0026] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0027] Example 1
[0028] This embodiment discloses a forming device for counterweight pipes of aquaculture net cages, referring to... Figure 1As shown, the device includes a mold shell 1, a shaft core 2, and a sandwich bushing 3, all three being coaxially mounted. The shaft core 2 is located on the inner circumference of the mold shell 1, and the sandwich bushing 3 is fitted between the mold shell 1 and the shaft core 2. An annular inner material channel 4 is formed between the shaft core 2 and the inner circumference of the sandwich bushing 3; an annular outer material channel 5 is formed between the outer circumference of the sandwich bushing 3 and the inner circumference of the mold shell 1. The inner material channel 4 and the outer material channel 5 are used for the flow of internal and external materials, respectively, forming a double-layer structure during the extrusion molding process.
[0029] Reference Figure 1 , 4 As shown, a tapered portion 31 is integrally formed on the side of the jacketed bushing 3 facing the output end. The outer periphery of the tapered portion 31 tapers towards the output end, and the material can be guided through the tapered portion 31. Furthermore, an end face 32 is formed at the end of the tapered portion 31.
[0030] Reference Figure 1 and Figure 3 As shown, the mold shell 1 includes a front mold shell 101 and a rear mold shell 102. An installation ring 7 is installed in the inner cavity of the mold shell 1. The installation ring 7 is sleeved between the front mold shell 101 and the rear mold shell 102, which serves to connect the front and rear mold shells to each other. During installation, the front mold shell 101 and the rear mold shell 102 are respectively sleeved with the installation ring 7. After installation, the inner circumference of the installation ring 7 serves as part of the outer layer material channel 5, and the materials of both the inner and outer layers flow through the inner circumference of the installation ring 7.
[0031] In this embodiment, the mounting ring 7 is located on one side of the output direction of the interlayer bushing 3 and is connected to the interlayer bushing 3. The material flowing out from the inner and outer peripheries of the interlayer bushing 3 can flow through the mounting ring 7.
[0032] Reference Figure 2 As shown, the adjusting ring 6 and the diverting ring 8 are installed at the end of the output side of the interlayer bushing 3, serving to divert the material between the inner and outer layers. During the material flow process, an annular connecting area 9 can be formed between the outer layer material channel 5 and the inner layer material channel 4.
[0033] The annular connecting area 9 is sandwiched between the outer layer material channel 5 and the inner layer material channel 4, thereby forming a mutually interlocking structure between the outer layer material channel 5 and the inner layer material channel 4. This allows the inner and outer layers to not rely solely on the bonding of their materials, and the interlocking structure can improve the bonding strength of the two layers.
[0034] Moreover, in this embodiment, the cross-section of the annular connecting area 9 forms an annularly spaced structure, that is, it is divided into several regions in the circumferential direction, specifically divided into an outer layer spacer and an inner layer spacer; wherein, the outer layer spacer is connected to the outer layer material channel 5; the inner layer spacer is connected to the inner layer material channel 4. During the extrusion molding process, the materials of the inner and outer layers can form an annularly spaced interlocking structure in the spaced groove.
[0035] Reference Figure 4 and Figure 5 As shown, the adjusting ring 6 is coaxially mounted on the inner circumference of the mounting ring 7, forming an outer flow channel 67 between the adjusting ring 6 and the mounting ring 7. The outer flow channel 67 communicates with the outer material channel 5, and most of the material in the outer material channel 5 flows through the outer flow channel 67. The adjusting ring 6 and the mounting ring 7 are fixedly connected by several connecting ribs, which can support the adjusting ring 6. Several guide strips 61 are integrally connected to the inner circumference of the adjusting ring 6. The guide strips 61 are arranged in a ring array, and an axial guide interval 62 is formed between adjacent guide strips 61. A guide channel 65 is opened in the guide strip 61. The end of the guide strip 61 facing the input side is closed, and an inlet 63 is opened at the end of the outer circumference of the adjusting ring 6 near the input side; an outlet 66 is opened at the end of the guide strip 61 facing the output side. Furthermore, an inclined guide section 64 is formed on the inner side of the inlet section 63, which allows the outer material to pass smoothly through the inlet section 63, reducing dead zones in the flow.
[0036] Reference Figure 4 and Figure 5 As shown, the flow-diverting ring 8 is installed on the inner circumference of the conical portion 31 of the sandwich bushing 3. The flow-diverting ring 8 includes a plurality of flow guide strips 81 and an extension ring 83, wherein the extension ring 83 is fixedly connected to the inner circumference of each flow guide strip 81 and is integrally formed with the flow guide strip 81; the flow guide strips 81 are arranged in a ring array, and the number of flow guide strips 81 corresponds one-to-one with the number of flow guide strips 61, with one end of each flow guide strip 81 flush with the end face 32 of the conical portion 31. Moreover, the outer circumference of the extension ring 83 and the inner circumference of the sandwich bushing 3 are spaced apart, forming a flow channel between the inner circumference of the sandwich bushing 3, the outer circumference of the extension ring 83, and two adjacent flow guide strips 81, which serves as the inner flow channel portion 84. The inner circumference of the extension ring 83 is flush with the inner circumference of the flow guide strips 81. Furthermore, one end of the extension ring 83 extends into the inner circumference of the interlayer bushing 3, while the other end extends out of the interlayer bushing 3 towards the output side. The outer circumferential dimensions of the extension ring 83 are adapted to the inner circumference of the adjusting ring 6, allowing the adjusting ring 6 to be fitted onto the outer circumference of the portion of the extension ring 83 extending out of the interlayer bushing 3. After both are fitted together, the second flow guide gap 62 and the first flow guide gap 82 can be interconnected in the axial direction, forming a channel for the flow of inner layer materials.
[0037] Reference Figure 6 As shown, in the cross-sectional direction, the extrusion channel of the pipe is divided into an outer flow channel section 67, an inner flow channel section 84, and a central annular connecting area 9. The cross-sectional spaces of the outer flow channel section 67 and the inner flow channel section 84 cannot be adjusted. In the annular connecting area 9, by adjusting the deflection angles of the adjusting ring 6 and the diverting ring 8, the partially misaligned state of the first guide bar 81 and the second guide bar 61 can be controlled, thereby controlling the channel of the inner spacer section formed by the second guide bar 62 and the first guide bar 82; the guide channel 65 serves as the outer spacer section.
[0038] During the rotation adjustment process, the channel ratio of the outer and inner layer spacers changes, thereby allowing for fine-tuning of the proportions of the inner and outer layer materials. Specifically, by increasing the flow channel of the inner layer spacer, the proportion of the inner layer material in the annular connection zone 9 can be increased, thus increasing the overall density of the pipe; conversely, by decreasing the flow channel of the inner layer spacer, the proportion of the inner layer material in the annular connection zone 9 can be reduced, thus decreasing the overall density of the pipe.
[0039] In this embodiment, there are two ways to adjust the relative rotation of the adjusting ring 6 and the diversion ring 8. In the first way, the adjusting ring 6 is in a fixed state, and the interlayer bushing 3 can be axially rotated for adjustment. By rotating the angle of the interlayer bushing 3, the relative position of the adjusting ring 6 and the diversion ring 8 can be adjusted. In the second way, the interlayer bushing 3 is in a fixed state, and the adjusting ring 6 can be rotated for adjustment. When it is necessary to adjust the density, the adjusting ring 6 is loosened, and then the adjusting ring 6 is rotated for adjustment to an appropriate angle, thereby adjusting the relative position of the adjusting ring 6 and the diversion ring 8. After adjustment, the adjusting ring 6 is locked and fixed again.
[0040] Example 2
[0041] This embodiment discloses a method for manufacturing counterweight pipes using the above-mentioned counterweight pipe forming device, for producing counterweight pipes for aquaculture net cages, including inner layer material preparation, co-extrusion molding and post-processing steps.
[0042] Step S11, raw material pretreatment.
[0043] The high-density filler material is placed in an oven and dried at 80-125℃ for 2-5 hours until its moisture content drops below 0.08%. The dried filler material and surface treatment agent are then added to a high-speed mixer and mixed at 90-100℃ and 500-800 rpm for 6-8 minutes to obtain a surface-activated filler material. The filler material can be selected from materials with a specific gravity of 4.0-4.5 and a particle size D50 of 2-4 μm; the surface treatment agent can be selected from silane coupling agent KH-550, etc.
[0044] Step S12, premixing.
[0045] Weigh the following components by weight: 20-80 parts of resin material, 20-80 parts of surface-activated filler material obtained in step S11, 0.5-1 part of antioxidant 1010 (hindered phenol), 0.5-1 part of antioxidant 168 (phosphite), 1-5 parts of zinc stearate, and 1-5 parts of color masterbatch. Put all the above components into a high-speed mixer and mix for 5-10 minutes at 90-100℃ and 600-800rpm to obtain a premix with uniform color and fully adsorbed additives.
[0046] Step S13: Melt blending and granulation.
[0047] The premixed material is fed into a co-rotating parallel twin-screw extruder for granulation. The extruder screw diameter is 50-65 mm, with a length-to-diameter ratio of 33-40:1. The screw is equipped with a combination of high-shear and kneading blocks. The temperature settings for each section of the extruder from the feed port to the die head are as follows: Zone 1 165-220℃, Zone 2 175-220℃, Zone 3 185-210℃, Zone 4 190-210℃, Zone 5 190-210℃, and Die Head 195-230℃; the screw speed is 200-320 rpm. Vacuum degassing is initiated after the melting section, maintaining the vacuum level at -0.08 to -0.02 MPa. After melting, mixing, and degassing, the melt is extruded into strips through a multi-hole die. After cooling in a water bath, pelletizing by a pelletizer, and sieving to remove long strips and debris, high-density counterweight masterbatch is obtained. The masterbatch appears dense and has a uniform color; its density, as tested, can reach 2.0-2.5 g / cm³.
[0048] Step S21, Equipment preparation.
[0049] A single-screw extruder (length-to-diameter ratio 30-33:1) is used as the outer extruder for processing resin; an SJ-75 / 33 high-torque single-screw extruder (length-to-diameter ratio 30-33:1) is used as the inner extruder for processing high-density counterweight masterbatch.
[0050] Step S22, co-extrusion molding.
[0051] The temperature gradient settings for the outer extruder from the feeding section to the die connector are: 150-170℃, 170-190℃, 185-200℃, 195-200℃, 200-220℃. For the inner extruder, to ensure sufficient plasticization of high-viscosity materials, the temperature settings are slightly higher: 160-170℃, 180-190℃, 200-220℃, 205-210℃, 210-220℃. The co-extrusion die temperature is uniformly set at 190-205℃. First, start both extruders separately. After preheating and plasticizing the material at a low speed (e.g., 10-20 rpm), gradually increase the speed. By adjusting the screw speeds of both extruders, control the output ratio of the inner and outer layers to achieve the required wall thickness. The extruded tube blank is introduced into a vacuum sizing chamber, with the inner diameter of the sizing sleeve set to the outer diameter of the target tube. The vacuum level is maintained between -0.07 and -0.03 MPa. The shaped tube blank then enters a spray cooling water bath for cooling. The fully cooled tube is then drawn out by a traction machine at a constant speed.
[0052] During the co-extrusion molding process, the inner layer material is output through the channel (i.e., the inner layer interval section) formed by the inner layer material channel 4, the inner layer flow channel 84, the first flow guide interval 82, and the second flow guide interval 62. The outer layer material is output through the outer layer material channel 5, the outer layer flow channel 67, the inlet 63, the flow guide channel 65 (i.e., the outer layer interval section), and the outlet 66. The inner and outer layer materials form a circumferentially spaced interlocking structure at the annular connecting area 9, thus forming a counterweight pipe with interlocking inner and outer layers. When it is necessary to adjust the density of the counterweight pipe, the relative angle between the adjusting ring 6 and the diverting ring 8 is adjusted to increase or decrease the channel of the inner layer interval section. By fine-tuning the ratio of the inner layer material to the outer layer material in the annular connecting area 9, the overall density of the pipe can be adjusted to meet the counterweight requirements of different aquaculture conditions.
[0053] Step S23, post-processing.
[0054] After the pipe has cooled and formed, a CNC drilling machine is used to drill a through hole with a diameter of 5-30mm every 50-400mm along the axial direction of the cut pipe. This hole is used for later fixing of the mesh. Coolant is used during drilling to ensure that the hole wall is smooth and burr-free. The formed counterweight pipe has an outer layer of plastic round pipe with an outer diameter of DN32-800mm and a wall thickness of 10-73mm. Different wall thicknesses of plastic protective layers can be designed according to the requirements of different sea areas. The inner counterweight layer is a composite layer with a thickness of 5.5-50mm. The filling ratio is adjusted according to the required counterweight weight, and appropriate filling materials and addition ratios are selected.
[0055] The above description is merely a preferred embodiment of the present invention. The scope of protection of the present invention is not limited to the above embodiments. All technical solutions falling within the scope of the present invention's concept are within the scope of protection of the present invention. It should be noted that for those skilled in the art, any improvements and modifications made without departing from the principles of the present invention should also be considered within the scope of protection of the present invention.
Claims
1. A molding device for counterweight pipes of marine aquaculture cages, comprising a mold shell (1), a shaft core (2), and a sandwich bushing (3) coaxially arranged, wherein the shaft core (2) is located on the inner circumference of the mold shell (1), the sandwich bushing (3) is sleeved between the shaft core (2) and the mold shell (1), an annular inner material channel (4) is formed between the outer circumference of the shaft core (2) and the inner circumference of the sandwich bushing (3), and an annular outer material channel (5) is formed between the outer circumference of the sandwich bushing (3) and the inner circumference of the mold shell (1), characterized in that, The sandwich bushing (3) has a tapered portion (31) on the side facing the output end, which tapers towards the output end. The end of the tapered portion (31) has an end face (32). A diverter ring (8) is installed on the inner circumference of the tapered portion (31). The diverter ring (8) includes a plurality of guide strips (81) arranged in a ring array and an extension ring (83) integrally connected to the inner circumference of each guide strip (81). A guide interval (82) is formed between adjacent guide strips (81). The output side of the sandwich bushing (3) has an adjusting ring (6) that is coaxially fitted with the diverter ring (8). The inner circumference of the adjusting ring (6) is integrally connected to the diverter ring (8). Multiple guide strips (61) are connected, and the number of guide strips (61) is the same as that of guide strips (81) and they correspond one-to-one. A guide interval (62) is formed between adjacent guide strips (61), and a guide channel (65) is opened in each guide strip (61). The guide interval (82) and the guide interval (62) are axially connected to form an inner layer interval for the flow of inner layer material. The guide channel (65) forms an outer layer interval. The outer layer interval and the inner layer interval are distributed circumferentially to form an annular transition section (9) sandwiched between the outer layer material channel (5) and the inner layer material channel (4).
2. The counterweight tube forming device according to claim 1, characterized in that, The adjusting ring (6) can rotate axially relative to the diverting ring (8); when the first guide bar (81) and the second guide bar (61) are aligned, the channel of the inner layer spacer is fully opened; when the first guide bar (81) and the second guide bar (61) are misaligned, the first guide gap (82) and the second guide gap (62) block each other, causing the channel of the inner layer spacer to shrink.
3. The counterweight tube forming device according to claim 1, characterized in that, The mold shell (1) includes a front mold shell (101) and a rear mold shell (102) that are connected to each other along the axial direction. An installation ring (7) is sleeved between the front mold shell (101) and the rear mold shell (102). The inner circumference of the installation ring (7) forms part of the outer layer material channel (5). An adjustment ring (6) is coaxially installed on the inner circumference of the installation ring (7). The outer circumference of the adjustment ring (6) and the inner circumference of the installation ring (7) form an outer layer flow channel (67) that communicates with the outer layer material channel (5).
4. The counterweight tube forming device according to claim 3, characterized in that, The adjusting ring (6) and the mounting ring (7) are fixedly connected by several connecting ribs to support the adjusting ring (6).
5. The counterweight tube forming device according to claim 1, characterized in that, The second guide bar (61) is closed at one end facing the input side, and the outer periphery of the adjusting ring (6) near the input side has an inlet (63) that communicates with the guide channel (65). The second guide bar (61) has an outlet (66) that communicates with the guide channel (65) at one end facing the output side.
6. The counterweight tube forming device according to claim 5, characterized in that, An inclined guide section (64) is formed on the inner side of the inlet (63).
7. The counterweight tube forming device according to claim 1, characterized in that, One end of the extension ring (83) extends into the inner circumference of the interlayer bushing (3), and the other end extends out of the interlayer bushing (3) toward the output side. The outer circumference of the extension ring (83) is adapted to the inner circumference of the adjusting ring (6). The adjusting ring (6) is fitted on the outer circumference of the part of the extension ring (83) that extends out of the interlayer bushing (3).
8. The counterweight tube forming device according to claim 7, characterized in that, One end of the guide bar (81) is flush with the end face (32) of the tapered part (31); the outer periphery of the extension ring (83) is spaced apart from the inner periphery of the interlayer bushing (3), and an inner flow channel (84) for the inner layer material to flow is formed between the inner periphery of the interlayer bushing (3), the outer periphery of the extension ring (83), and the two adjacent guide bars (81).
9. A method for manufacturing counterweight tubing, using the counterweight tubing forming apparatus according to any one of claims 1 to 8, characterized in that, Includes the following steps: The inner layer material is supplied through the inner layer material channel (4), and the outer layer material is supplied through the outer layer material channel (5). The inner layer material is output through the inner layer interval formed by the connection between the first flow interval (82) and the second flow interval (62), and the outer layer material is output through the outer layer interval formed by the flow channel (65). The inner layer material and the outer layer material form a circumferentially spaced interlocking structure at the annular transition section (9). The inner and outer layers are interlocked and formed into a counterweight pipe by extrusion molding.
10. The method for manufacturing counterweight pipes according to claim 9, characterized in that, By rotating and adjusting the relative angle between the adjusting ring (6) and the diverting ring (8), the first guide bar (81) and the second guide bar (61) are aligned or misaligned, thereby adjusting the channel size of the inner layer partition and thus adjusting the ratio of the inner layer material to the outer layer material.