A method for low-oxidation self-reduction cold pressing treatment of deoxidized sludge
By employing a closed-loop drying process, biaxial shearing dissociation activation, cold pressing, and low-temperature curing, the problems of metal oxidation loss and high equipment investment in deoxidation sludge treatment have been solved. This method achieves efficient, energy-saving, and environmentally friendly deoxidation sludge treatment, applicable to DRI production lines of various sizes, and improves metal recovery rate and metallurgical performance.
Patent Information
- Application Number
- CN202611174349.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-04
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies for treating deoxidized sludge suffer from severe metal oxidation and loss, low resource recovery, high equipment investment, high operation and maintenance costs, and low smelting efficiency, and cannot reliably provide an efficient, energy-saving, and environmentally friendly method for treating deoxidized sludge.
Indirect drying and dispersing are carried out using a closed jacketed drying cylinder, metal particle dissociation and activation are carried out using a biaxial shearing dissociation and activation machine, composite binder is added and condensate is sprayed in for homogenization and humidification, wet blocks are prepared using a high-pressure roller cold pressing molding machine, and solidification is carried out in a micro-inert low-temperature waste heat kiln. Finally, high-strength self-reducing cold blocks are formed by screening through a single-layer vibrating screen.
It improves the processing efficiency of deoxidized sludge, reduces processing costs, minimizes the loss of valuable elements, and achieves efficient, energy-saving, and environmentally friendly deoxidized sludge treatment. It is suitable for DRI production lines of various sizes and enhances metal recovery rate and metallurgical performance.
Smart Images

Figure CN123105937A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to a short-process, harmless, and high-value-added treatment method for high-moisture, high-metal-activity deoxidized sludge produced from the sedimentation tank of a wet dust collector in a deoxidized sludge production line. The high-strength self-reducing cold-pressed briquettes prepared using this method can be directly used as qualified iron-containing raw materials in electric arc furnace steelmaking, belonging to the field of metallurgical technology. Background Technology
[0002] A large amount of dust is generated during the production of deoxidized sludge. Due to the easily oxidized and spontaneously combustible nature of deoxidized sludge dust, a wet scrubber is selected for dust removal. After wet washing and sedimentation collection, deoxidized sludge is obtained from the sedimentation tank. The measured material parameters are as follows: moisture content 20%–25%, total iron (TFe) 84.98%–87.78%, metallic iron 61.28%–78.51%, metallization rate 80%–90%, fixed residual carbon 2.91%–3.68%; impurities include only SiO2, CaO, MgO, Al2O3, S, and P, and their contents are extremely low. There are no harmful heavy metals such as zinc and lead. The slag system is simple, meeting the standards for electric arc furnace feed, and it can be used as an iron-containing raw material for electric arc furnace steelmaking. The material appears as a dense mud mass, with micron-sized deoxidized sludge DRI (Direct Reduced Iron, commonly known as sponge iron) particles completely coated with silicate ultrafine dust. Deoxidized mud powder is highly chemically active. During conventional drying, transportation, and molding processes, it is easily oxidized upon contact with air, resulting in a loss of up to 12% of metallic iron, which significantly reduces the economic value of iron-containing raw materials.
[0003] The current mainstream disposal methods in the industry have obvious flaws: 1. Deoxidized mud is simply dehydrated and sold in bulk: Only basic dehydration treatment is performed, and the silicate coating layer on the surface of DRI particles is not removed, resulting in a low melting rate in electric furnace and increased power consumption per ton of steel; at the same time, this solution lacks full-process low-oxygen protection measures, resulting in serious metal oxidation and loss, which greatly reduces its use value and has extremely low resource recovery benefits.
[0004] 2. Wet magnetic separation grading process: It requires a complete set of large-scale equipment such as slurry processing, multi-stage magnetic separation, and filter press. The initial equipment investment is high, the process flow is lengthy, and a large amount of process wastewater is generated simultaneously, resulting in high water treatment and maintenance costs. It is not economically viable for small and medium-sized DRI production lines.
[0005] 3. Disc pelletizing process: requires a pelletizing machine and multi-layer green pellet screening equipment, occupies a large area, and is extremely sensitive to fluctuations in material moisture content; during the green pellet drying stage, DRI will continue to oxidize, and additional coke powder needs to be purchased to supplement the reducing agent, which significantly increases the cost of auxiliary materials.
[0006] 4. Ordinary normal temperature cold pressing process: There is no particle dissociation and residual carbon activation process. The internal porosity of the briquettes is high, which will cause a large amount of pulverization during the electric furnace feeding process, resulting in increased smoke and dust and decreased metal yield. In addition, there is no segmented anti-oxidation system, resulting in serious metal loss and making it impossible to supply the electric furnace on a large scale and stably.
[0007] Therefore, developing a low-oxidation self-reduction cold pressing treatment method for deoxidized mud that is efficient, energy-saving, environmentally friendly, and reduces the loss of valuable elements is of great practical significance. Summary of the Invention
[0008] The purpose of this invention is to address the shortcomings of existing technologies by providing a low-oxidation self-reduction cold pressing treatment method for deoxidized sludge, thereby improving the treatment efficiency of deoxidized sludge, reducing treatment costs, and minimizing the loss of valuable elements.
[0009] To achieve the above objectives, the present invention adopts the following technical solution: A method for low-oxidation self-reducing cold pressing treatment of deoxidized sludge, the method comprising the following steps: a. The deoxidized sludge is indirectly dried and dispersed using a closed jacketed drying cylinder with an internal stirring mechanism; b. In a closed biaxial shear dissociation and activation machine, the metal particles in the dried deoxidized mud are dissociated into individual particles and the fixed residual carbon is activated at low temperature. c. Add composite binder to the dissociated and activated material and spray in condensate to perform closed-loop homogenization and moisture conditioning of the material; d. Use a high-pressure roller cold pressing machine to cold press the homogenized and moisture-conditioned material into wet blocks; e. The wet briquette is fed into a micro-inert low-temperature residual heat curing kiln for low-temperature curing; f. Use a single-layer vibrating screen to screen the solidified and cooled cold-pressed blocks.
[0010] The specific methods for indirect drying and dispersing of the deoxidized sludge in the above-mentioned low-oxidation self-reduction cold pressing treatment method are as follows: Deoxidized sludge is fed into a sealed jacketed drying cylinder through a closed feed inlet and discharged through a sealed outlet. The sealed jacketed drying cylinder includes an inner cylinder and an outer cylinder fitted around it, with a medium chamber between them. Low-temperature flue gas (165-170°C) emitted from the DRI heating furnace flows through this medium chamber, using the flue gas as a heat exchange medium to perform non-contact heating and drying of the deoxidized sludge. During the drying process, a small amount of nitrogen is continuously introduced through the air inlet of the sealed jacketed drying cylinder to control the oxygen content to ≤6%, inhibiting DRI pre-oxidation. Simultaneously, a small amount of nitrogen is introduced through the air inlet of the sealed jacketed drying cylinder to control the oxygen content to ≤6%, inhibiting DRI pre-oxidation. Excess gas is discharged through the exhaust port of the sealed jacket drying cylinder. An agitation mechanism is installed inside the sealed jacket drying cylinder. The agitation mechanism includes a rotating shaft, which is rotatably connected to the sealed jacket drying cylinder through bearings. One end of the rotating shaft is connected to an electric reduction gearbox fixed outside the sealed jacket drying cylinder. Multiple rotors are installed around the rotating shaft. A flexible iron chain is connected between the middle of each rotor and the rotating shaft. The electric reduction gearbox drives the rotating shaft, rotors, and iron chain to rotate, thereby breaking up the dense mud.
[0011] The specific methods for the low-oxidation self-reduction cold pressing treatment of deoxidized sludge described above, which involve the monomer dissociation of metal particles in the dried deoxidized sludge and the low-temperature activation of fixed residual carbon, are as follows: The dried ash formed after deoxidizing the sludge is transported to a biaxial shearing and dissociation activation machine via a negative pressure closed pipeline and a sealed feed chute. After staying in the biaxial shearing and dissociation activation machine for 13-17 minutes, it is discharged from the closed discharge port. The dissociation activation machine includes a sealed pressure-resistant housing with two parallel rotating shafts inside. Each shaft has shearing blades along its axial direction. An external drive device drives the rotating shafts and shearing blades to rotate, extruding and shearing the dried ash to peel off the silicate ultrafine dust from the surface of the DRI particles, thus achieving the dissociation of individual metal particles. The sealed pressure-resistant housing is equipped with a low-temperature heat exchange jacket. A liquid circulating medium at a temperature of 190-210℃ is introduced into the inner cavity of the low-temperature heat exchange jacket to activate the fixed residual carbon in the dried ash at a low temperature, so that the activated carbon is uniformly adsorbed and coated on the surface of the DRI particles, forming a natural antioxidant film. Nitrogen gas is continuously introduced into the cavity of the sealed pressure-resistant housing through a nitrogen inlet to control the oxygen content in the cavity at 3%-4.2%.
[0012] The specific method for the closed-loop homogenization and moisture conditioning of the material in the above-mentioned low-oxidation self-reduction cold pressing treatment method for deoxidized sludge is as follows: The dissociated and activated material is fed into a closed horizontal homogenizer, and 1.7% to 2.3% of the total mass of the material is added as a composite inorganic binder. The mixing time is 4 to 6 minutes, and condensate is sprayed in simultaneously to adjust the moisture content of the mixture to 9.8% to 10.8%.
[0013] The above-mentioned low-oxidation self-reducing cold pressing treatment method for deoxidized sludge involves cold pressing the homogenized and moisture-conditioned material into wet briquettes as follows: The homogenized and moisture-conditioned material is continuously fed into the high-pressure double-roll cold pressing machine from the sealed buffer feed hopper. The high-pressure double-roll cold pressing machine includes a fully enclosed equipment frame and a pair of high-pressure forming rollers installed in the equipment frame. The pair of high-pressure forming rollers includes two parallel rollers with their roller surfaces in contact and forming grooves. The two rollers are driven to rotate synchronously in opposite directions by a hydraulic pressure regulating assembly mounted on the equipment frame. The forming grooves directly compress the material into a dense wet block in a single compression. The wet block is discharged from the discharge sealed chute at the bottom of the equipment frame.
[0014] The above-mentioned low-oxidation self-reducing cold pressing treatment method for deoxidized mud involves the following method for low-temperature curing of wet pressed blocks: The wet briquette is laid flat and fed into a micro-inertia low-temperature waste heat curing kiln. The curing heat source is used to heat and cure the wet briquette. A nitrogen micro-inertia gas supply system continuously introduces a small amount of nitrogen into the micro-inertia low-temperature waste heat curing kiln to maintain a low-oxygen environment. The curing temperature is 135-165℃, and the curing time is 60-70 minutes.
[0015] The specific method for sieving the solidified and cooled cold-pressed blocks after the above-mentioned low-oxidation self-reduction cold-pressing treatment method for deoxidized mud is as follows: After solidification and cooling, the cold-pressed blocks are screened by a single-layer vibrating screen. The cold-pressed blocks with qualified particle size on the screen are transported to the finished cold-pressed block storage silo, and then directly sent to the electric arc furnace steelmaking workshop through the electric arc furnace steelmaking feeding system. All the crushed powder under the screen is returned to the closed horizontal homogenizing mixer to participate in the molding again.
[0016] In the above-mentioned low-oxidation self-reduction cold pressing treatment method for deoxidized mud, all the water vapor contained in the gas discharged from the exhaust port of the sealed jacket drying cylinder is condensed and recovered to the condensate recycling system for storage. When the material is subjected to sealed homogenization and humidification, the condensate sprayed into the material is provided by the condensate recycling system.
[0017] In the above-mentioned low-oxidation self-reducing cold pressing treatment method for deoxidized mud, the composite inorganic binder is composed of bentonite, light magnesium oxide, and lignin calcium.
[0018] In the above-mentioned low-oxidation self-reduction cold pressing treatment method for deoxidized mud, the curing heat source is entirely reused from the low-temperature waste heat flue gas after heat exchange in the closed jacket drying cylinder. The low-temperature waste heat flue gas is transported to the micro-inert low-temperature waste heat curing kiln through the waste heat circulation pipeline.
[0019] This invention abandons the traditional wet magnetic separation and disc pelletizing process, and only sets up six processes: drying, dissociation and activation, mixing, cold pressing, solidification and screening. At the same time, it sets up a dual anti-oxidation system of low oxygen inert atmosphere and granular carbon protective layer, which not only improves the treatment efficiency of deoxidized sludge and reduces the treatment cost, but also reduces the loss of valuable elements. Attached Figure Description
[0020] The present invention will now be described in further detail with reference to the accompanying drawings and specific embodiments.
[0021] Figure 1 This is the overall process flow diagram of the present invention; Figure 2 This is a schematic diagram of the structure of a sealed jacketed drying cylinder; Figure 3 This is a schematic diagram of the structure of a biaxial shear dissociation activation machine; Figure 4 This is a schematic diagram of the structure of a high-pressure double-roll cold pressing machine.
[0022] The following are the labels in the diagram: 1. Deoxidized sludge storage silo; 2. Sealed jacketed drying cylinder; 3. Deionization and activation machine; 4. Sealed horizontal homogenizing mixer; 5. High-pressure roller cold pressing molding machine; 6. Micro-inertia low-temperature waste heat curing kiln; 7. Single-layer vibrating screen; 8. Cold-pressed block storage silo; 9. Feeding system; 10. Waste heat circulation pipeline; 11. Nitrogen micro-inertia gas supply system; 12. Condensate circulation and recovery system; 13. Automatic control unit; 14. Tail gas flow regulating valve; 15. Support base; 16. Electro-reduction integrated machine; 17. Rotary. 18. Shaft; 19. Rotor; 20. Chain; 21. Outer cylinder; 22. Inner cylinder; 23. Feed inlet; 24. Discharge outlet; 25. DRI heating furnace; 26. Heating furnace chimney; 27. Drying gas pipeline; 28. Medium chamber; 29. Exhaust fan; 30. Drying cylinder chimney; 31. Ash discharge pool; 32. Drying gas flow regulating valve; 33. Shut-off valve; 34. Blind flange; 35. Sealed discharge port; 36. Sealed pressure-resistant casing; 37. Shear blades; 38. Low-temperature heat exchange jacket; 49. Nitrogen inlet port; 40. Feed sealing chute; 41. Discharge sealing chute; 42. Equipment frame; 43. Hydraulic pressure regulating assembly; 44. Paired high-pressure forming rollers; 45. Ellipsoidal forming groove; 46. Sealed buffer feed hopper. Detailed Implementation
[0023] This invention addresses the shortcomings of existing technologies by providing a low-oxidation self-reducing cold pressing treatment method for deoxidized sludge. This method mainly solves the following problems: 1. Dense mud clumps are formed, and DRI particles are coated with silicate dust, resulting in low melting rate and high power consumption per ton of steel in electric furnace smelting. 2. DRI fine powder has high activity and is easily oxidized throughout the conventional processing, resulting in a large loss of valuable iron. 3. The deoxidized sludge contains 2.91% to 3.68% residual carbon that is not activated and utilized, requiring the electric furnace to purchase additional carbon raisers and reducing agents, resulting in high auxiliary material costs; 4. Traditional sorting and disc pelletizing equipment require large investments and are complicated to operate and maintain, resulting in an imbalance between input and output for deoxidized sludge production lines of various sizes; 5. Conventional molding products have insufficient strength, and the electric furnace feed causes severe pulverization, making them unsuitable as high-quality iron-containing raw materials for long-term stability.
[0024] This invention includes the following steps: Step 1: Indirect drying and dispersing of deoxidized sludge is carried out using a closed jacketed drying cylinder with an internal stirring mechanism. The high-moisture, deoxygenated sludge with a moisture content of 20%–23.2% from the DRI sedimentation tank is then sealed and fed into a sealed jacketed drying cylinder 2 (see attached diagram). Figure 2 The sealed jacketed drying cylinder 2 includes an inner cylinder 21 and an outer cylinder 20 sleeved outside the inner cylinder 21, with a medium chamber 27 between them. The top of the sealed jacketed drying cylinder 2 has a feed inlet 22 and the bottom has a discharge outlet 23. The deoxidized sludge is fed into the sealed chamber through the feed inlet 22 and discharged through the discharge outlet 23. The closed-loop discharge system allows the 165-170°C low-temperature flue gas emitted from the DRI heating furnace 24 to flow through the medium chamber 27. Using the flue gas as a heat exchange medium, the deoxidized sludge undergoes non-contact heating and drying. During the drying process, a small amount of nitrogen is continuously introduced through the air inlet (not shown in the figure) of the closed-loop jacketed drying cylinder 2 to control the oxygen content to ≤6%, thus inhibiting DRI pre-oxidation. Simultaneously, excess gas is discharged through the exhaust port (not shown in the figure) of the closed-loop jacketed drying cylinder 2. All water vapor contained in the discharged gas is condensed and recovered to the condensate recycling system 12 for storage and subsequent molding and humidity conditioning. Metal oxidation loss in this process is controlled to within 1%. The closed-loop jacketed drying cylinder 2 is equipped with a stirring mechanism, including a rotating shaft 17. The rotating shaft 17 is rotatably connected to the sealed jacket drying cylinder 2 via bearings. One end of the rotating shaft 17 is connected to the electric reduction and deoxidation integrated machine 16 fixed outside the sealed jacket drying cylinder 2. The electric reduction and deoxidation integrated machine 16 includes a motor and a reducer. Multiple rotors 18 are installed around the rotating shaft 17 for conveying deoxidized sludge. A flexible iron chain 19 is connected between the middle of each rotor 18 and the rotating shaft 17 for breaking up dense sludge lumps. The moisture content of the material at the drying endpoint is controlled at 7% to 8%. The low-temperature flue gas emitted from the DRI heating furnace 24 enters the medium chamber 27 through the drying gas pipeline 26. The low-temperature waste heat flue gas after heat exchange is discharged through the drying cylinder chimney 29, or it can be drawn out by the induced draft fan 28 and reused through the drying gas pipeline 26 or other pipelines.
[0025] Step 2: In a closed biaxial shearing dissociation and activation machine, the metal particles in the dried deoxidized sludge are dissociated into individual particles, and the fixed residual carbon is activated at low temperature. The dry ash formed after the deoxidized sludge is dried is transported through a negative pressure closed pipeline to a biaxial shearing dissociation activation machine 3. The dissociation activation machine 3 includes a sealed pressure-resistant housing 35, inside which are two parallel rotating shafts. The rotating shafts are rotatably connected to the sealed pressure-resistant housing 35 and are also connected to an external drive device, allowing them to rotate under the drive of the external drive device. Each rotating shaft is equipped with shearing blades 36 along its axial direction. When the two rotating shafts rotate, the shearing blades 36 compress the dry ash. The process involves shearing and peeling away the silicate ultrafine dust from the surface of DRI particles, achieving the dissociation of individual metal particles. A sealed, pressure-resistant housing 35 is equipped with a low-temperature heat exchange jacket 37, through which a liquid circulating medium at a temperature of 190–210°C is introduced. Dry ash enters through a sealed feed chute 39 at the top of the sealed, pressure-resistant housing 35 and exits through a sealed discharge port 34 at the bottom, remaining within the housing for 13–17 minutes to remove 2.91%–3.68% of the dry ash. The fixed residual carbon is activated at low temperature; nitrogen is continuously introduced into the cavity of the sealed pressure housing 35 through the nitrogen inlet port 38 to control the oxygen content in the cavity at 3% to 4.2%, maintaining a low-oxygen inert atmosphere throughout the process. The activated carbon is uniformly adsorbed and coated on the surface of DRI particles to form a natural antioxidant film, giving the final cold-pressed block self-reducing properties. Electric furnace smelting does not require a large amount of externally purchased carbonaceous reducing agent; the dry ash after dissociation and activation is discharged through the sealed discharge port 34 to obtain the dissociated and activated material.
[0026] Step 3: Add composite binder to the dissociated and activated material and spray in condensate to perform sealed homogenization and moisture conditioning of the material. The dissociated and activated material is fed into a closed horizontal homogenizer 4, and 1.7% to 2.3% of the total mass of the material is added as a composite inorganic binder. The binder is composed of bentonite, light magnesium oxide, and lignin calcium, and does not contain high-priced organic polymers. The mixing time is 4 to 6 minutes, and the condensate stored in the condensate recycling system 12 is sprayed in simultaneously to adjust the moisture content of the mixture to 9.8% to 10.8%, matching the optimal molding range of high-pressure cold pressing. The entire process is under closed negative pressure to isolate air and avoid secondary oxidation of DRI.
[0027] Step 4: Use a high-pressure roller cold pressing machine to cold press the homogenized and moisture-conditioned material into wet blocks; The homogenized and moisture-conditioned material is continuously fed into a high-pressure double-roll cold-press forming machine 5. The high-pressure double-roll cold-press forming machine 5 includes a pair of high-pressure forming rollers 43 installed within a machine frame 41. Each pair of high-pressure forming rollers 43 consists of two parallel rollers with their surfaces in contact. The two ends of each roller are rotatably connected to the machine frame 41 via bearings. The machine frame 41 is equipped with a hydraulic pressure regulating assembly 42, which drives the two rollers to rotate synchronously in opposite directions. The surface of the pair of high-pressure forming rollers 43 has 30mm × 22mm ellipsoidal forming grooves 44. The forming hydraulic pressure is 15.5–18.5 MPa, and a single extrusion directly forms a dense wet block. The machine frame 41 is a fully enclosed structure, isolating it from atmospheric oxidation. The material enters through a sealed buffer feed hopper 45 at the top of the machine frame 41, and the wet block is discharged from a sealed discharge chute 40 at the bottom of the machine frame 41. The drop strength is ≥6 times / day. With a diameter of 0.5m, the breakage rate during transport is ≤3.5%; the entire set of equipment for disc pelletizing and multi-layer green pellet grading and screening is eliminated, shortening the molding process and reducing the initial investment in equipment.
[0028] Step 5: Send the wet pressed blocks into a micro-inert low-temperature residual heat curing kiln for low-temperature curing. The wet briquettes are laid flat and fed into the micro-inertia low-temperature waste heat curing kiln 6. The curing heat source is used to heat and cure the wet briquettes. The curing heat source is entirely reused from the low-temperature waste heat flue gas after heat exchange in the sealed jacket drying cylinder 2. The low-temperature waste heat flue gas is transported into the micro-inertia low-temperature waste heat curing kiln 6 through the waste heat circulation pipeline 10, without the need for additional fuel combustion. The nitrogen micro-inertia gas supply system 11 continuously introduces a small amount of nitrogen into the micro-inertia low-temperature waste heat curing kiln 6 to maintain a low-oxygen environment. The curing temperature is 135-165℃, and the curing time is 60-70 minutes. After curing, the compressive strength of a single cold briquette at room temperature is ≥2000N, the carbon protective layer on the particle surface is stable, the metallization rate has no significant decrease, and the pulverization rate of electric furnace feeding is extremely low.
[0029] Step 6: Use a single-layer vibrating screen to screen the solidified and cooled cold-pressed blocks. After solidification and cooling, the cold-pressed blocks are screened by a simple vibrating screener 7. The high-strength self-reducing cold-pressed blocks with qualified particle size are transported to the finished cold-pressed block storage silo 8, and then directly sent to the electric arc furnace steelmaking workshop through the electric arc furnace steelmaking feeding system 9, replacing the purchased iron blocks and iron concentrate blocks. All the crushed powder under the screen is returned to the closed horizontal homogenizing mixer 4 to participate in the molding again, with no solid waste discharged externally.
[0030] The waste heat flue gas from drying and curing is recycled and reused through the waste heat circulation pipeline 10. All condensate is recycled and used for material humidification through the condensate recovery system 12. The entire system is uniformly controlled by the PLC intelligent automatic control unit 13. There is no process wastewater discharge, achieving 100% closed-loop digestion of all components of DRI.
[0031] Example 1: A method for low-oxidation self-reducing cold pressing treatment of deoxidized sludge, comprising the following steps: (1) The deoxidized sludge is indirectly dried and dispersed using a closed jacket drying cylinder with an internal stirring mechanism: Deoxygenated sludge from the DRI sedimentation tank with a moisture content of 20%–23.2% is fed into a closed jacketed drying cylinder 2. DRI heating furnace 24 is introduced into the medium chamber 27 to produce waste heat flue gas at 165–170°C for indirect heat exchange. Inside the closed jacketed drying cylinder 2, rotors 18 and chains 19 continuously rotate to break up the sludge clumps. A trace amount of nitrogen is introduced into the closed jacketed drying cylinder 2 throughout the process to control oxygen levels to ≤6%. After drying, the moisture content of the material is controlled at 7%–8%. The water vapor generated during drying is collected in the condensate recycling system 12 for condensation and storage for later use. (2) In a closed biaxial shear dissociation and activation machine, the metal particles in the dried deoxidized mud are dissociated into individual particles and the fixed residual carbon is activated at low temperature: The dried ash is conveyed under negative pressure to the dual-axis shearing and dissociation activation machine 3. Nitrogen gas is continuously introduced through the nitrogen inlet port 38 to maintain a low-oxygen atmosphere. The shearing blades 36 squeeze and shear to peel off the silicate dust on the surface of the DRI particles, realizing the dissociation of metal particles. The low-temperature heat exchange jacket 37 controls the temperature at 200℃, and the oxygen content in the chamber is stable at 4%. The material stays in the equipment for 15 minutes, and 2.91% to 3.68% of the residual carbon in the activated material is activated. The activated carbon coats the surface of the DRI particles to form an antioxidant protective layer, so that the finished cold-pressed block has the self-reduction characteristics of electric furnace. (3) Add composite binder to the dissociated and activated material and spray in condensate to perform closed-loop homogenization and moisture conditioning of the material: The activated material is fed into a closed horizontal homogenizer 4, and 2% of the total material mass of composite binder (bentonite + light magnesium oxide + lignin calcium compound) is added. The mixture is mixed in a closed system for 5 minutes, and the condensate is simultaneously sprayed into the condensate recycling system 12 to recover the condensate and precisely control the moisture content of the mixture to 10.2%. (4) The homogenized and moisture-conditioned material is cold-pressed into wet blocks using a high-pressure double-roll cold-pressing machine: Homogeneous material is fed into a high-pressure double-roll cold pressing machine 5. The hydraulic pressure regulating assembly 42 controls the forming pressure to 17MPa. The ellipsoidal forming grooves 44 on the surface of the paired high-pressure forming rollers 43 are 30mm×22mm in size and are formed by single extrusion. The wet block is discharged from the discharge sealing chute 40 and the drop strength is ≥6 times / 0.5m. (5) The wet pressed blocks are sent into a micro-inert low-temperature residual heat curing kiln for low-temperature curing: The wet-pressed block is fed into the micro-inert low-temperature waste heat curing kiln 6, and the waste heat circulation pipeline 10 delivers low-temperature waste heat flue gas from the sealed jacket drying cylinder 2 for heating; a trace amount of nitrogen gas supplied by the nitrogen micro-inert gas supply system 11 is introduced into the kiln, the curing temperature is 150℃, and the curing is maintained for 65 minutes to obtain a high-strength self-reducing cold-pressed block with a room temperature compressive strength ≥2000N. (6) Use a single-layer vibrating screen to screen the solidified and cooled cold-pressed blocks: The solidified and cooled briquettes are screened by a single-layer vibrating screener 7. The qualified finished products are sent to the finished cold briquette storage silo 8 and directly supplied to the electric arc furnace steelmaking workshop through the electric arc furnace steelmaking feeding system 9, replacing the purchased iron blocks and iron concentrate briquettes. All the crushed powder under the screen is returned to the closed horizontal homogenizing mixer 4 for recycling and molding.
[0032] The waste heat flue gas from drying and curing is recycled through the waste heat circulation pipeline 10, and the condensate recycling system 12 provides closed-loop humidity control of water resources throughout the process. The entire system has no process wastewater and no external solid waste discharge, achieving 100% full component utilization of DRI deoxidized sludge.
[0033] In this embodiment, the entire process is automatically monitored and controlled by the PLC intelligent control unit 13. The segmented low oxygen protection combined with the carbon layer on the particle surface provides double anti-oxidation, and the metallization rate of the finished product is ≥98%.
[0034] Example 2: In step (2), the low temperature heat exchange jacket 37 controls the temperature at 190°C, the oxygen content in the cavity is stable at 3%, and the material stays in the equipment for 13 minutes; in step (4), the hydraulic pressure regulating assembly 42 regulates the molding pressure to 15.5 MPa; in step (5), the curing temperature is 135°C, and the curing is maintained for 65 minutes. The remaining process parameters are completely consistent with those in Example 1. The metallization rate retention rate of the finished product is ≥98%, and the metallurgical performance meets the standards.
[0035] Example 3: In step (2), the low temperature heat exchange jacket 37 controls the temperature at 210℃, the oxygen content in the cavity is 3-5%, and the material stays in the equipment for 15 minutes; in step (4), the hydraulic pressure regulating assembly 42 regulates the molding pressure to 18.5MPa; in step (5), the curing temperature is 165℃, and the heat preservation curing is 70 minutes. The remaining process parameters are completely consistent with those in Example 1. The compressive strength of the finished product is ≥2000N, and the pulverization rate of the electric furnace feed is less than 3%.
[0036] The advantages of this invention are: 1. Lightweight manufacturing process, compatible with all sizes of DRI production lines. Abandoning the high-investment, long-process solutions of wet magnetic separation and disc pelletizing, this method only sets up six processes: drying, dissociation and activation, mixing, cold pressing, curing, and screening. The number of supporting equipment is reduced by 45%, and the initial equipment investment is only 36% of that of wet separation and 55% of that of disc pelletizing. Large, medium and small DRI production lines can be implemented at low cost.
[0037] 2. Dual antioxidant system significantly improves metal recovery rate. The drying, activation, mixing, and curing processes are carried out in stages by introducing trace amounts of nitrogen to create a low-oxygen, sealed environment. At the same time, the residual carbon activated at low temperature forms a carbon protective layer on the surface of DRI particles, which doubles the barrier against air oxidation and ensures a stable metallization rate retention of ≥98%. Compared with the 10% to 12% metal loss of traditional open processes, a large amount of valuable iron can be recovered every year, increasing the effective iron content of the electric furnace raw materials.
[0038] 3. Utilize virgin residual carbon on-site to reduce the cost of auxiliary materials for electric furnaces. The integrated dual-axis shearing equipment simultaneously completes dust dissociation and residual carbon activation, making full use of the 2.91% to 3.68% carbon resources inherent in the deoxidized mud. The cold-pressed blocks can be fed into the electric furnace to provide reducing carbon, significantly reducing the procurement expenditure of steelmaking carbonizers and reducing agents.
[0039] 4. The entire process of waste heat and water resources is in a closed loop, resulting in low operating costs. The drying and curing processes reuse the DRI heating furnace 24 to discharge low-temperature waste heat, eliminating the need for additional natural gas or coal consumption; all drying condensate is stored in the condensate recycling system 12 for reuse, eliminating the need to purchase production water externally, and significantly reducing energy and water consumption per ton of ash processed.
[0040] 5. The finished product has excellent metallurgical properties and can be directly powered by a furnace for stable production. After curing, the cold-pressed blocks have high compressive strength, less pulverization during material transfer and electric furnace feeding, low smelting dust emissions, and improved metal yield. They can replace expensive purchased iron blocks and iron concentrate briquettes for a long time, continuously reducing the raw material procurement cost of electric furnaces.
[0041] 6. Clean closed-loop production with outstanding environmental advantages: The entire system is sealed under negative pressure, eliminating secondary dust generation. Waste heat and condensate are internally circulated, and there is no discharge of process wastewater or tailings solid waste; relying on native carbon to replace purchased carbon auxiliary materials reduces carbon emissions and complies with metallurgical clean production control standards.
Claims
1. A method for low-oxidation self-reducing cold pressing treatment of deoxidized sludge, characterized in that, The method includes the following steps: a. The deoxidized sludge is indirectly dried and dispersed using a closed jacketed drying cylinder with an internal stirring mechanism; b. In a closed biaxial shear dissociation and activation machine, the metal particles in the dried deoxidized mud are dissociated into individual particles and the fixed residual carbon is activated at low temperature. c. Add composite binder to the dissociated and activated material and spray in condensate to perform closed-loop homogenization and moisture conditioning of the material; d. Use a high-pressure roller cold pressing machine to cold press the homogenized and moisture-conditioned material into wet blocks; e. The wet briquette is fed into a micro-inert low-temperature residual heat curing kiln for low-temperature curing; f. Use a single-layer vibrating screen to screen the solidified and cooled cold-pressed blocks.
2. The method for low-oxidation self-reduction cold pressing treatment of deoxidized sludge according to claim 1, characterized in that, The specific method for indirect drying and dispersing of deoxidized sludge is as follows: The deoxidized sludge is fed into the sealed jacketed drying cylinder (2) through the feed inlet (22) and discharged through the discharge outlet (23). The sealed jacketed drying cylinder (2) includes an inner cylinder (21) and an outer cylinder (20) sleeved outside the inner cylinder (21). A medium chamber (27) is provided between the two, so that the low-temperature flue gas of 165-170°C emitted from the DRI heating furnace (24) flows through the medium chamber (27). The flue gas is used as a heat exchange medium to heat and dry the deoxidized sludge without contact. During the drying process, a small amount of nitrogen is continuously introduced through the air inlet of the sealed jacketed drying cylinder (2) to control the oxygen content ≤6% and inhibit DRI pre-oxidation. At the same time, the nitrogen is introduced through the air inlet of the sealed jacketed drying cylinder (2). Excess gas is discharged through the exhaust port; an agitation mechanism is provided inside the sealed jacket drying cylinder (2), the agitation mechanism includes a rotating shaft (17), the rotating shaft (17) is rotatably connected to the sealed jacket drying cylinder (2) through a bearing, one end of the rotating shaft (17) is connected to the electric reduction integrated machine (16) fixed outside the sealed jacket drying cylinder (2), multiple rotors (18) are installed around the rotating shaft (17), and a flexible iron chain (19) is connected between the middle of each rotor (18) and the rotating shaft (17). The rotating shaft (17), rotors (18) and iron chain (19) are driven to rotate by the electric reduction integrated machine (16) to break up the dense mud.
3. The method for low-oxidation self-reduction cold pressing treatment of deoxidized sludge according to claim 2, characterized in that, The specific method for monomer dissociation of metal particles in dried deoxidized sludge and low-temperature activation of fixed residual carbon is as follows: The dry ash formed after the deoxidized mud is dried is transported to the biaxial shearing dissociation activation machine (3) through a negative pressure closed pipe and a feed sealed chute (39). After staying in the biaxial shearing dissociation activation machine (3) for 13 to 17 minutes, it is discharged from the closed discharge port (34). The dissociation activation machine (3) includes a closed pressure-resistant housing (35). The closed pressure-resistant housing (35) has two parallel rotating shafts inside. Each rotating shaft has shearing blades (36) along its axial direction. An external drive device drives the rotating shafts and shearing blades (36) to rotate, extruding and shearing the dry ash, peeling off the silicate ultrafine dust on the surface of DRI particles, and realizing the dissociation of metal particles. The closed pressure-resistant housing (35) is equipped with a low-temperature heat exchange jacket (37). The inner cavity of the low-temperature heat exchange jacket (37) is circulated with a liquid circulating medium at a temperature of 190 to 210°C to activate the fixed residual carbon in the dry ash at low temperature, so that the activated carbon is uniformly adsorbed and coated on the surface of DRI particles to form a natural antioxidant film. Nitrogen gas is continuously introduced into the cavity of the sealed pressure-resistant housing (35) through the nitrogen gas inlet port (38) to control the oxygen content in the cavity at 3% to 4.2%.
4. The method for low-oxidation self-reducing cold pressing treatment of deoxidized sludge according to claim 3, characterized in that, The specific method for achieving closed-loop homogenization and moisture conditioning of materials is as follows: The dissociated and activated material is fed into a closed horizontal homogenizer (4), and 1.7% to 2.3% of the total mass of the material is added as a composite inorganic binder. The mixing time is 4 to 6 minutes, and condensate is sprayed in simultaneously to adjust the moisture content of the mixture to 9.8% to 10.8%.
5. The method for low-oxidation self-reduction cold pressing treatment of deoxidized sludge according to claim 4, characterized in that, The method for cold-pressing homogenized and moisture-conditioned materials into wet blocks is as follows: The homogenized and humidified material is continuously fed into the high-pressure double-roll cold pressing machine (5) from the closed buffer feed hopper (45). The high-pressure double-roll cold pressing machine (5) includes a fully enclosed equipment frame (41) and a pair of high-pressure forming rollers (43) installed in the equipment frame (41). The pair of high-pressure forming rollers (43) includes two parallel rollers with their roller surfaces in contact and forming grooves (44) are provided. The two rollers are driven to rotate synchronously in opposite directions by the hydraulic pressure regulating assembly (42) mounted on the equipment frame (41). The material is directly squeezed by the forming grooves (44) to form a dense wet block. The wet block is discharged from the discharge sealing chute (40) at the bottom of the equipment frame (41).
6. The method for low-oxidation self-reducing cold pressing treatment of deoxidized sludge according to claim 5, characterized in that, The method for low-temperature curing of wet-pressed blocks is as follows: The wet briquette is laid flat and sent into the micro-inert low-temperature residual heat curing kiln (6). The wet briquette is heated and cured using the curing heat source. The nitrogen micro-inert gas supply system (11) continuously introduces a small amount of nitrogen into the micro-inert low-temperature residual heat curing kiln (6) to maintain a low oxygen environment. The curing temperature is 135-165℃ and the curing time is 60-70 minutes.
7. The method for low-oxidation self-reducing cold pressing treatment of deoxidized sludge according to claim 6, characterized in that, The specific method for sieving the cold-pressed blocks after curing and cooling is as follows: After solidification and cooling, the cold-pressed blocks are screened by a single-layer vibrating screen (7). The cold-pressed blocks with qualified particle size on the screen are transported to the finished cold-pressed block storage silo (8) and then directly sent to the electric arc furnace steelmaking workshop through the electric arc furnace steelmaking feeding system (9). All the crushed powder under the screen is returned to the closed horizontal homogenizing mixer (4) to participate in the molding again.
8. The method for low-oxidation self-reduction cold pressing treatment of deoxidized sludge according to claim 7, characterized in that, All water vapor contained in the gas discharged from the exhaust port of the sealed jacket drying cylinder (2) is condensed and recovered to the condensate recycling system (12) for storage. When the material is subjected to sealed homogenization and humidification, the condensate sprayed into the material is provided by the condensate recycling system (12).
9. The method for low-oxidation self-reducing cold pressing treatment of deoxidized sludge according to claim 8, characterized in that, The composite inorganic binder is composed of bentonite, light magnesium oxide, and lignin calcium.
10. The method for low-oxidation self-reducing cold pressing treatment of deoxidized sludge according to claim 9, characterized in that, The curing heat source is entirely reused from the low-temperature waste heat flue gas after heat exchange in the closed jacket drying cylinder (2). The low-temperature waste heat flue gas is transported to the micro-inert low-temperature waste heat curing kiln (6) through the waste heat circulation pipeline.