A borosilicate and its preparation method

By introducing a five-membered cyclic borate ester structure into the sulfonate molecule, the problems of boron loss and complex processes in the preparation of borate sulfonates are solved, achieving efficient boron conversion and improved product performance, making it suitable as a lubricating oil additive for high power density internal combustion engines.

CN123106730APending Publication Date: 2026-11-17JIANGSU AORUN ADVANCED MATERIALS CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202611179042.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-05
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing methods for preparing borosilicate sulfonates suffer from problems such as easy loss of boron, complex processes, low boron conversion rates, and poor product performance, especially in high-power-density internal combustion engines where they lack wear resistance and thermal stability.

Method used

Boron is introduced into the sulfonate molecule structure through chemical bonds. The neutralization, carbonation, hydroxylation and boron esterification reactions are carried out in a one-pot process to form a five-membered cyclic boron ester structure, realizing the molecular-level bonding of boron and sulfonate, simplifying the preparation process and improving the boron conversion rate.

Benefits of technology

Stable binding of boron in sulfonates was achieved, significantly improving the product's abrasion resistance, detergency, and thermal stability, enhancing the uniformity and batch consistency of borosulfonates, reducing slag content, and increasing product yield.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This invention relates to the field of organometallic compound technology, specifically to a borosilicate sulfonate and its preparation method, particularly to a highly alkaline borosilicate detergent and its preparation method, as well as the use of the borosilicate sulfonate as a lubricating oil additive. This invention introduces hydroxyl groups into the sulfonate molecule using a hydroxylating agent, and then chemically bonds boron to the sulfonate molecule via a dehydration condensation reaction of the hydroxyl group and boric acid, achieving a molecular-level bond between boron and the sulfonate. This chemical bonding method ensures that each sulfonate molecule contains boron, significantly improving product uniformity and batch consistency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of organometallic compound technology, specifically to a borosilicate and its preparation method, and more particularly to a highly alkaline borosilicate detergent and its preparation method, as well as the use of the borosilicate as a lubricating oil additive. Background Technology

[0002] Sulfonates are a type of metal detergent and an essential additive in internal combustion engine oils. The alkaline portion of sulfonates neutralizes the oxyacids generated by the oxidation of lubricating oil or fuel, preventing further oxidation and condensation, thereby reducing deposit formation. Furthermore, they neutralize sulfur oxides (SO2, SO3) generated by the combustion of sulfur-containing fuels or inorganic acids such as HCl and HNO3 generated by the combustion of gasoline, thus protecting the metal surfaces of components such as cylinders from corrosion.

[0003] However, traditional sulfonate detergents have shortcomings in terms of friction reduction and anti-wear properties. With the development of modern internal combustion engines towards higher power density and higher loads, higher requirements are placed on the anti-wear properties, extreme pressure properties, and thermal stability of lubricating oils. Boron-containing additives, especially alkaline earth metal borate sulfonates, have been found to not only possess excellent anti-friction properties in lubricating oil compositions but also provide detergency, rust prevention, corrosion protection, and extreme pressure properties.

[0004] Several methods for preparing borosilicate sulfonates have been disclosed in the prior art. For example, US patent 4683126A discloses a two-step method for preparing an alkaline earth metal borate dispersion, which includes reacting an oil-soluble neutral alkaline earth metal sulfonate, an alkaline earth metal hydroxide or oxide, boric acid, water, and a diluent at 20-100°C, followed by heating to 100-200°C to remove water and part of the diluent. US patent 3480548A discloses a lubricating oil composition prepared by reacting a lubricating oil dispersion of alkaline earth metal carbonates and alkaline earth metal hydrocarbon sulfonates with a boron compound selected from boric acid, boron oxide, and aqueous alkyl esters of boric acid. As another example, US patent 4,744,920 discloses a method for obtaining a borosilicate product with high carbonate content, involving mixing a highly basic sulfonate with a borate agent at a controlled temperature to minimize foaming, separate water while retaining carbonate, and obtain a borosilicate product with a high carbonate content and an average particle size of less than 9 micrometers.

[0005] However, the above-mentioned existing technologies still have the following shortcomings: (1) Boron is mostly introduced by physical mixing, and the boron element is dispersed in the product in the form of borate or borate ions, rather than being linked to sulfonate molecules by chemical bonds, which makes it easy for boron to be lost during storage and use; (2) The preparation process is complicated and usually requires multiple steps of reaction, which is cumbersome; (3) A large amount of water needs to be added during the reaction, which leads to high energy consumption and long time for subsequent dehydration; (4) The borylation reaction efficiency is low and the boron conversion rate is not ideal; (5) The free alkali content in the product is high, which affects the cleanliness and colloidal stability of the product; (6) Some methods are prone to destroying the calcium carbonate core structure during the borylation process, which affects the product performance.

[0006] Therefore, developing a boronized sulfonate with simple process, high boron conversion rate, and excellent product performance through chemical bonding, and its preparation method, has important industrial application value. Summary of the Invention

[0007] To address the shortcomings of the prior art, this invention provides a boron sulfonate and its preparation method. The aim is to solve the following technical problems: introducing boron into the sulfonate molecular structure through chemical bonds, achieving molecular-level bonding between boron and sulfonate; simplifying the preparation process and reducing operational steps; improving the efficiency of the boronizing reaction and boron conversion rate; improving the product's detergency, abrasion resistance, and thermal stability; reducing the slag content in the product and increasing product yield.

[0008] Therefore, the present invention provides the following technical solution.

[0009] The first aspect of the present invention provides a borosilicate sulfonate molecule containing a benzene ring sulfonic acid ortho-five-membered cyclic borosilicate covalent structure having the following general formula: R-C6H2(SO3M)-(OBO); Wherein, M is selected from at least one alkaline earth metal element; the parent nucleus group R is a C8-C30 alkyl group; -OBO- is connected to two adjacent carbon atoms on the benzene ring through oxygen atoms to form a five-membered cyclic borate ester structure.

[0010] This borate sulfonate product uses an alkaline earth metal salt of alkylphenyl sulfonate as the parent core. The hydroxyl group at the ortho carbon position of the sulfonic acid group on the benzene ring is connected to the hydroxyl group. The ortho dihydroxyl group dehydrates and closes the ring with the boric acid molecule to form a stable five-membered cyclic borate ester structure. The boron atom is embedded in the organic molecular skeleton of the sulfonate ester through BOC covalent bond, rather than physical doping.

[0011] In a preferred embodiment of the present invention, the borosulfonate is obtained by dehydration and cyclization of alkylbenzene sulfonate with ortho-hydroxy-substituted benzene ring sulfonate and boric acid to form a five-membered cyclic boroester, wherein the boron atom is embedded in the organic molecular skeleton of the sulfonate through a BOC covalent bond.

[0012] In a preferred embodiment of the present invention, the total base value of the borosilicate is 200-500 mg KOH / g, and the boron content is 0.5-5.0 wt%, preferably 1-4 wt%.

[0013] In a preferred embodiment of the present invention, M is selected from at least one of calcium, magnesium or barium; and R is a C12-C24 straight-chain or branched alkyl group.

[0014] In a preferred embodiment of the present invention, in the sulfonate containing hydroxyl groups, the hydroxyl group is located ortho to the sulfonic acid group, and after dehydration condensation with boric acid, a five-membered ring borate ester structure is formed. The five-membered ring structure, due to its low ring strain and high thermodynamic stability, endows the product with superior thermal stability and wear resistance.

[0015] A second aspect of the present invention provides a method for preparing borosilicate sulfonate as described above, comprising the following steps: S1: Add organic solvent, long-chain alkylbenzene sulfonic acid, heavy alkylbenzene sulfonic acid, low-carbon alcohol and base oil into a reaction vessel and mix. Then carry out a neutralization reaction at 40-80°C for 0.5-3 hours to obtain reaction mixture I. S2: Add alkaline earth metal oxides and water in batches to the obtained reaction mixture I, and pass carbon dioxide to carry out a carbonation reaction, controlling the free alkalinity to reach 200-400 mg KOH / g, to obtain reaction mixture II; S3: Add a hydroxylating agent to the obtained reaction mixture II and carry out a hydroxylation reaction at 50-100°C for 1-4 hours to introduce hydroxyl groups into the sulfonate molecules to obtain reaction mixture III; S4: Add boric acid to the obtained reaction mixture III and carry out a dehydration condensation reaction at 70-150°C for 2-8 hours to obtain reaction mixture IV; S5: The obtained reaction mixture IV is subjected to de-alcoholization and dehydration, centrifugation to remove residue, and distillation to remove solvent, to obtain the borosulfonate product.

[0016] In a preferred embodiment of the present invention, in step S1, the components by weight percentage are: 30-55% organic solvent, 5-10% long-chain alkylbenzene sulfonic acid, 5-10% heavy alkylbenzene sulfonic acid, 1-8% low-carbon alcohol, and the balance being base oil.

[0017] In a preferred embodiment of the present invention, in step S1, the organic solvent is a C6-C12 aromatic solvent or alkane solvent, such as benzene, toluene, xylene, n-hexane, n-heptane, cyclohexane, or any suitable organic solvent in the art.

[0018] In a preferred embodiment of the present invention, in step S1, the long-chain alkylbenzene sulfonic acid refers to an alkylbenzene sulfonic acid with an alkyl carbon chain length of C16 to C24, such as 4-pentadecanylbenzene sulfonic acid, 4-hexadecylbenzene sulfonic acid or 4-heptadecylbenzene sulfonic acid.

[0019] In a preferred embodiment of the present invention, in step S1, the heavy alkylbenzene sulfonic acid is a high-boiling-point byproduct of the production of dodecylbenzene, a raw material for detergents. Heavy alkylbenzene has a very complex composition, being a mixture of various long-chain alkylbenzenes, with its alkyl chains primarily branched and typically having C14 to C18 or higher carbon atoms. Furthermore, it may also contain more complex components such as dialkylbenzenes. For example, "linear heavy alkylbenzene sulfonic acid" with CAS number 68584-22-5.

[0020] In a preferred embodiment of the present invention, in step S1, the lower alcohol is a C1-C4 monohydric alcohol, such as methanol, ethanol, isopropanol, n-butanol, etc.

[0021] In a preferred embodiment of the present invention, in step S2, the alkaline earth metal oxide is at least one of calcium oxide, magnesium oxide or barium oxide; the amount of alkaline earth metal oxide added is 2-8% of the mass of reaction mixture I.

[0022] In a preferred embodiment of the present invention, in step S2, the carbonation reaction is carried out in 2-4 batches with alkaline earth metal oxide and water, with each batch containing 1-4% alkaline earth metal oxide and 0.5-1.5% water.

[0023] In a preferred embodiment of the present invention, in step S3, the hydroxylating agent is selected from at least one of ethylene oxide, propylene oxide, ethylene glycol, glycerol, and diethanolamine.

[0024] In a preferred embodiment of the present invention, in step S3, the amount of the hydroxylating agent added is 2-10% of the mass of reaction mixture II.

[0025] In a preferred embodiment of the present invention, in step S3, the hydroxylation reaction is carried out in the presence of an alkaline catalyst, wherein the alkaline catalyst is selected from at least one of sodium hydroxide, potassium hydroxide, and triethylamine.

[0026] In a preferred embodiment of the present invention, the amount of alkaline catalyst added is 0.1-1% of the mass of the hydroxylating agent.

[0027] In a preferred embodiment of the present invention, in step S4, the molar ratio of the reaction mixture III to boric acid is 1:(0.5-3).

[0028] In a preferred embodiment of the present invention, in step S4, the dehydration condensation reaction is carried out under azeotropic dehydration conditions, and a dehydrating agent is used to continuously remove the water generated in the reaction; the dehydrating agent is selected from at least one of toluene, xylene, and cyclohexane.

[0029] In a preferred embodiment of the present invention, in step S4, the dehydration condensation reaction is carried out in the presence of a catalyst selected from at least one of p-toluenesulfonic acid, sulfuric acid, and phosphoric acid.

[0030] In a preferred embodiment of the present invention, the amount of catalyst added is 0.1-1% of the mass of boric acid.

[0031] In a preferred embodiment of the present invention, in step S5, the temperature for de-alcoholization and dehydration is 120-200°C; the speed for centrifugal slag removal is 3000-8000 rpm, and the time is 10-60 minutes.

[0032] A third aspect of the invention provides the use of borosilicates as described above or borosilicates prepared according to the preparation method described above as lubricating oil additives in the preparation of lubricating oils.

[0033] By employing the above technical solution, the present invention has at least the following advantages: (1) Boron is introduced through chemical bonding: In this invention, hydroxyl groups are introduced into the sulfonate molecule through a hydroxylating agent, and then boron is chemically bonded to the sulfonate molecule in the form of borate ester bonds (BOC) through the dehydration condensation reaction of the hydroxyl groups and boric acid, thus achieving molecular-level bonding between boron and sulfonate. This chemical bonding method ensures that each sulfonate molecule contains boron, and the uniformity and batch consistency of the product are significantly improved.

[0034] (2) Stable boron content: Since boron is chemically bonded to the sulfonate molecular skeleton, it is not easily lost during storage and use, resulting in excellent stability of the boron content in the product. At the same time, the boron esterification reaction is carried out under azeotropic dehydration or in the presence of a catalyst, and the reaction equilibrium shifts towards the product, so that the boron conversion rate can reach more than 85%.

[0035] (3) Simplified process: The present invention uses a one-pot method to continuously carry out neutralization, carbonation, hydroxylation and borate esterification reactions without intermediate separation and purification steps, which is simple to operate and suitable for industrial production.

[0036] (4) Significantly improved anti-wear performance: Chemically bonded borate ester groups can more effectively release boron at the friction interface, forming a boundary lubrication film with anti-wear and extreme pressure properties.

[0037] (5) Excellent product performance: The borosilicate salt prepared by this invention has a high total base number (200-500 mgKOH / g) and a suitable boron content (0.5-5.0 wt%), and also has excellent detergency, antioxidant properties, anti-wear properties and extreme pressure properties. The product has good colloidal stability and dispersibility in lubricating oil, low slag content (≤0.5 wt%), and high yield (≥90%).

[0038] (6) Integrity of the core structure: The present invention avoids the destruction of the calcium carbonate core during the hydroxylation and borate esterification process, resulting in a product with good filterability and excellent colloidal stability.

[0039] The above description is merely an overview of the technical solution of the present invention. In order to better understand the technical means of the present invention and to implement it in accordance with the contents of the specification, the preferred embodiments of the present invention are described in detail below. Detailed Implementation

[0040] To make the technical means, creative features, achieved objectives, and effects of this invention readily understandable, the technical solutions in the embodiments of this invention will be clearly and completely described below in conjunction with the embodiments of this invention. Obviously, the described embodiments are merely some embodiments of this invention, and not all embodiments. Based on the embodiments of this invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this invention.

[0041] Example 1: Calcium borosulfonate and its preparation The preparation steps of calcium borosulfonate in this embodiment are as follows: S1: By weight percentage, 45% n-hexane and long-chain alkylbenzene sulfonic acid (C 16 Alkylbenzenesulfonic acid) 8%, heavy alkylbenzenesulfonic acid (C 20 -C 24 8% alkylbenzene sulfonic acid, 4% isopropanol, and the balance base oil 150SN were added to the reactor and stirred at 65°C for 2 hours to carry out the neutralization reaction, yielding reaction mixture I.

[0042] S2: Carbonation reaction is carried out in two steps to the obtained reaction mixture I: First, 2% by mass of calcium oxide and 0.8% by mass of reaction mixture I are added, and CO2 is introduced until the free alkalinity reaches 100 mg KOH / g; Second, 2% by mass of calcium oxide and 0.8% by mass of reaction mixture I are added again, and CO2 is introduced until the free alkalinity reaches 300 mg KOH / g, to obtain reaction mixture II.

[0043] S3: Add ethylene oxide (6% of the mass of reaction mixture II) and sodium hydroxide (0.5% of the mass of reaction mixture II) to the obtained reaction mixture II, and react at 70°C for 2.5 hours to introduce hydroxyl groups into the sulfonate molecules, thus obtaining reaction mixture III.

[0044] S4: Add boric acid to the resulting reaction mixture III at a molar ratio of 1:2, followed by toluene (0.6% of the boric acid mass). Heat to 130°C and stir for 5 hours to carry out the dehydration condensation reaction. During the reaction, continuously remove the generated water using a water separator to obtain reaction mixture IV.

[0045] S5: The resulting reaction mixture IV was heated to 165°C to remove alcohol and water, then centrifuged at 5000 rpm for 30 minutes to remove residue, and the solvent was removed by distillation to obtain calcium borate sulfonate product.

[0046] Product structure confirmation: Infrared spectroscopy analysis was performed on the obtained product at 1340 cm⁻¹. -1 The characteristic absorption peak of the BOC bond appears at this location; 11 B NMR spectra showed a characteristic signal of borate ester at a chemical shift of 20 ppm, confirming the formation of BOC bonds.

[0047] Example 2: Calcium borosulfonate and its preparation The preparation steps of calcium borosulfonate in this embodiment are as follows: S1: By weight percentage, 30% toluene and long-chain alkylbenzene sulfonic acid (C 18 Alkylbenzenesulfonic acid) 10%, heavy alkylbenzenesulfonic acid (C 22 -C 26 5% alkylbenzene sulfonic acid, 8% n-butanol, and the balance base oil 500SN were added to a reaction vessel and stirred at 60°C for 1.5 hours to carry out a neutralization reaction, yielding reaction mixture I.

[0048] S2: Carbonation reaction is carried out in two steps to the obtained reaction mixture I: First, 1.5% by mass of calcium oxide and 0.6% by mass of reaction mixture I are added, and CO2 is introduced until the free alkalinity reaches 80 mg KOH / g; Second, 1.5% by mass of calcium oxide and 0.6% by mass of reaction mixture I are added again, and CO2 is introduced until the free alkalinity reaches 280 mg KOH / g, to obtain reaction mixture II.

[0049] S3: Add glycerol (10% of the mass of reaction mixture II) and triethylamine (1% of the mass of reaction mixture II) to the obtained reaction mixture II, and react at 80°C for 2 hours to introduce hydroxyl groups into the sulfonate molecules, thus obtaining reaction mixture III.

[0050] S4: Add boric acid to the obtained reaction mixture III at a molar ratio of 1:3, then add xylene (1% of the mass of boric acid), heat to 120°C, and stir for 4 hours to carry out the dehydration condensation reaction. During the reaction, continuously remove the generated water using a water separator to obtain reaction mixture IV.

[0051] S5: The resulting reaction mixture IV was heated to 160°C to remove alcohol and water, then centrifuged at 5000 rpm for 30 minutes to remove residue, and the solvent was removed by distillation to obtain calcium borate sulfonate product.

[0052] Example 3: Magnesium borosulfonate and its preparation The preparation steps of magnesium borosulfonate in this embodiment are as follows: S1: By weight percentage, 55% xylene and long-chain alkylbenzene sulfonic acid (C 20 Alkylbenzenesulfonic acid) 5%, heavy alkylbenzenesulfonic acid (C 18 -C 22 10% alkylbenzene sulfonic acid, 1% methanol, and the balance base oil 150SN were added to a reaction vessel and stirred at 50°C for 1 hour to carry out a neutralization reaction, yielding reaction mixture I.

[0053] S2: Carbonation reaction is carried out in two steps to the obtained reaction mixture I: First, 1% magnesium oxide and 0.5% water by mass of reaction mixture I are added, and CO2 is introduced until the free alkalinity reaches 70 mg KOH / g; Second, 1% magnesium oxide and 0.5% water by mass of reaction mixture I are added again, and CO2 is introduced until the free alkalinity reaches 250 mg KOH / g, to obtain reaction mixture II.

[0054] S3: Add ethylene glycol (2% of the mass of reaction mixture II) and potassium hydroxide (0.1% of the mass of reaction mixture II) to the obtained reaction mixture II, and react at 75°C for 3 hours to introduce hydroxyl groups into the sulfonate molecules, thus obtaining reaction mixture III.

[0055] S4: Add boric acid to the obtained reaction mixture III at a molar ratio of 1:0.5, followed by cyclohexane (0.1% of the boric acid mass). Heat to 100°C and stir for 6 hours to carry out the dehydration condensation reaction. During the reaction, continuously remove the generated water using a water separator to obtain reaction mixture IV.

[0056] S5: The resulting reaction mixture IV was heated to 150°C to remove alcohol and water, then centrifuged at 4000 rpm for 40 minutes to remove residue, and the solvent was removed by distillation to obtain magnesium borate sulfonate product.

[0057] Example 4: Calcium borosulfonate and its preparation In this embodiment, long-chain alkylbenzene sulfonic acid with adjacent dihydroxyl groups substituted at the ortho position of the sulfonic acid group on the benzene ring is directly used as the raw material. This raw material can be prepared by the following method: C 16 Alkylbenzene sulfonic acid was sulfonated at 110°C for 5 hours in the presence of fuming sulfuric acid, followed by hydrolysis under alkaline conditions to introduce ortho-dihydroxyl groups. After acidification, a C-type benzene ring with adjacent dihydroxyl groups substituted at the ortho-position of the sulfonic acid group was obtained. 16 Alkylbenzene sulfonic acid.

[0058] The preparation steps of calcium borosulfonate in this embodiment are as follows: S1: By weight percentage, 50% n-heptane, and long-chain alkylbenzene sulfonic acid (C) with adjacent dihydroxyl groups substituted at the ortho-position of the sulfonic acid group on the above benzene ring. 16 10% alkyl group, heavy alkylbenzene sulfonic acid (C 20 -C 24 8% alkylbenzene sulfonic acid, 4% ethanol, and the balance base oil 150SN were added to a reaction vessel and stirred at 55°C for 1.5 hours to carry out a neutralization reaction, yielding reaction mixture I.

[0059] S2: Carbonation reaction is carried out in two steps to the obtained reaction mixture I: First, 1.5% by mass of calcium oxide and 0.6% by mass of reaction mixture I are added, and CO2 is introduced until the free alkalinity reaches 90 mg KOH / g; Second, 1.5% by mass of calcium oxide and 0.6% by mass of reaction mixture I are added again, and CO2 is introduced until the free alkalinity reaches 290 mg KOH / g, to obtain reaction mixture II.

[0060] S3: Add propylene oxide (4% of the mass of reaction mixture II) and triethylamine (0.2% of the mass of reaction mixture II) to the obtained reaction mixture II, and react at 70°C for 2.5 hours to introduce hydroxyl groups into the sulfonate molecules, thus obtaining reaction mixture III.

[0061] S4: Boric acid was added to the resulting reaction mixture III at a molar ratio of 1:2, followed by toluene (0.5% of the boric acid mass) and p-toluenesulfonic acid (0.1% of the boric acid mass). The mixture was heated to 125°C and stirred for 5 hours to carry out a dehydration condensation reaction. Because the benzene ring in the reactant has adjacent dihydroxyl groups at the ortho-position of the sulfonic acid group, the dehydration condensation of boric acid with the ortho-dihydroxyl groups forms a five-membered cyclic borate ester structure (ring size BOCCCO, a total of 6 atoms, but named as a five-membered cyclic borate ester according to nomenclature rules), which has higher structural stability. During the reaction, water was continuously removed using a water separator to obtain reaction mixture IV.

[0062] S5: The resulting reaction mixture IV was heated to 160°C to remove alcohol and water, then centrifuged at 5000 rpm for 30 minutes to remove residue, and the solvent was removed by distillation to obtain calcium borate sulfonate product with a five-membered cyclic borate ester structure.

[0063] Product structure confirmation: 11 B NMR spectra showed characteristic signals of five-membered cyclic borate esters at chemical shifts of 15-18 ppm, confirming the formation of a stable five-membered cyclic structure. 1 The 1H NMR spectrum shows that the integral ratio of aromatic hydrogens on the benzene ring is 2H (C6H2), consistent with the trisubstituted benzene ring structure; the formation of the BOC bond is shown in the infrared spectrum at 1340 cm⁻¹. -1 The characteristic absorption peaks at the location further confirmed the structure. Elemental analysis results: C 57.8 wt%, H 8.3 wt%, B 2.9 wt%, Ca 9.2 wt%, S 4.7 wt%, consistent with the expected structure.

[0064] Comparative Example 1: Calcium borosulfonate and its preparation The preparation steps of calcium borosulfonate in this embodiment are as follows: S1: By weight percentage, 45% n-hexane and long-chain alkylbenzene sulfonic acid (C 16 Alkylbenzenesulfonic acid) 8%, heavy alkylbenzenesulfonic acid (C 20 -C 24 8% alkylbenzene sulfonic acid, 4% isopropanol, and the balance base oil 150SN were added to the reactor and stirred at 65°C for 2 hours to carry out the neutralization reaction, yielding reaction mixture I.

[0065] S2: Carbonation reaction is carried out in two steps to the obtained reaction mixture I: First, 2% by mass of calcium oxide and 0.8% by mass of reaction mixture I are added, and CO2 is introduced until the free alkalinity reaches 100 mg KOH / g; Second, 2% by mass of calcium oxide and 0.8% by mass of reaction mixture I are added again, and CO2 is introduced until the free alkalinity reaches 300 mg KOH / g, to obtain reaction mixture II.

[0066] S3: Add boric acid to the obtained reaction mixture II at a molar ratio of 1:2, then add toluene (0.6% of the boric acid mass), heat to 130°C, and stir for 5 hours to carry out the dehydration condensation reaction. During the reaction, continuously remove the generated water using a water separator to obtain reaction mixture III.

[0067] S4: The resulting reaction mixture III was heated to 165°C to remove alcohol and water, then centrifuged at 5000 rpm for 30 minutes to remove residue, and the solvent was removed by distillation to obtain calcium borate sulfonate product.

[0068] Note: Due to the lack of hydroxyl groups, boric acid cannot form chemical bonds with sulfonates, and most of the boric acid is removed in subsequent treatments.

[0069] Comparative Example 2: Calcium Sulfonate and its Preparation The preparation steps of calcium sulfonate in this embodiment are as follows: S1: By weight percentage, 45% n-hexane and long-chain alkylbenzene sulfonic acid (C 16 Alkylbenzenesulfonic acid) 8%, heavy alkylbenzenesulfonic acid (C 20 -C 24 8% alkylbenzene sulfonic acid, 4% isopropanol, and the balance base oil 150SN were added to the reactor and stirred at 65°C for 2 hours to carry out the neutralization reaction, yielding reaction mixture I.

[0070] S2: Carbonation reaction is carried out in two steps to the obtained reaction mixture I: First, 2% by mass of calcium oxide and 0.8% by mass of reaction mixture I are added, and CO2 is introduced until the free alkalinity reaches 100 mg KOH / g; Second, 2% by mass of calcium oxide and 0.8% by mass of reaction mixture I are added again, and CO2 is introduced until the free alkalinity reaches 300 mg KOH / g, to obtain reaction mixture II.

[0071] S3: The resulting reaction mixture II was heated to 165°C to remove alcohol and water, then centrifuged at 5000 rpm for 30 minutes to remove residue, and the solvent was removed by distillation to obtain calcium sulfonate product.

[0072] Test Example 1: Basic Performance Testing of the Product The performance of the products from Examples 1-4 and Comparative Examples 1-2 was tested, and the results are shown in Table 1.

[0073] Table 1 Summary of product performance in each embodiment and comparative example ; As shown in Table 1, the boron content of the products in Examples 1-4 of the present invention is 2.5-3.2 wt%, and the boron conversion rate is 85-90%, which is significantly better than that of Comparative Example 1 (boron content 0.5 wt%, boron conversion rate 25%). This indicates that the present invention can effectively introduce boron into the sulfonate molecule in the form of chemical bonds by introducing hydroxyl groups through the hydroxylation step and then carrying out a dehydration condensation reaction with boric acid.

[0074] Experimental Example 2: Boron Stability Test The products of Examples 1-4 and Comparative Examples 1-2 were dissolved in 150SN base oil (addition amount 2 wt%) and heated at 120°C for 72 hours. The changes in boron content in the oil samples before and after heating were measured, and the results are shown in Table 2. Table 2. Results of boron stability test ; As shown in Table 2, the boron retention rates of the boron sulfonate products in Examples 1-4 of this invention all reached over 93%, significantly higher than that of Comparative Example 1 (60.0%). This indicates that the boron introduced through chemical bonds (boron ester bonds) exhibits excellent stability under high-temperature storage conditions and is not easily lost. Among them, Example 4 (five-membered cyclic boron ester structure) showed the highest boron retention rate, reaching 96.7%, indicating that the cyclic structure further enhanced the stability of the boron ester bonds.

[0075] Test Example 3: Cleanliness Test The detergency of each product was evaluated using a panel coker test. Test conditions: oil temperature 100°C, panel temperature 330°C, running time 3 hours. The results are shown in Table 3.

[0076] Table 3 Cleanliness Test Results (Coking Plate Test) ; As shown in Table 3, the coking amount of the borosilicate products of Examples 1-4 of this invention is significantly lower than that of Comparative Examples 1 and 2, indicating that the borosilicates of this invention have excellent detergency. Among them, Example 4 (five-membered cyclic borosilicate ester structure) has the lowest coking amount (6.0 mg) and the best detergency. Comparative Example 2 (boron-free calcium sulfonate) has the highest coking amount (16.5 mg), indicating that the introduction of boron helps to improve the detergency of the product.

[0077] Test Example 4: Wear Resistance Test The wear resistance of each product was evaluated using a four-ball friction and wear tester. Test conditions: load 392 N, speed 1200 rpm, temperature 75°C, running time 60 minutes. The results are shown in Table 4.

[0078] Table 4. Test results of wear resistance (four-ball test) ; As shown in Table 4, the borosilicate sulfonate products of Examples 1-4 of this invention exhibit significantly better wear scar diameter and friction coefficient than Comparative Examples 1 and 2, indicating that the borosilicate sulfonates of this invention possess excellent anti-wear and friction-reducing properties. Among them, Example 4 (a five-membered cyclic borosilicate ester structure) showed the best performance, with a wear scar diameter of only 0.35 mm and a friction coefficient as low as 0.062. Comparative Examples 1 (without chemically bonded boron) and 2 (without boron) showed significantly poorer anti-wear properties, indicating that boron introduced through chemical bonds can more effectively exert its anti-wear and friction-reducing effects.

[0079] Experimental Example 5: Thermal Stability Test Thermogravimetric analysis (TGA) was used to evaluate the thermal stability of each product. The product was heated from room temperature to 600°C at a heating rate of 10°C / min under a nitrogen atmosphere. The results are shown in Table 5.

[0080] Table 5 Thermal stability test results (TGA) ; As shown in Table 5, the initial decomposition temperatures of the borosilicate sulfonate products of Examples 1-4 of this invention are all ≥290°C, significantly higher than those of Comparative Example 1 (240°C) and Comparative Example 2 (250°C), and the residual rates at 500°C are also significantly higher than those of the comparative examples. Among them, Example 4 (five-membered cyclic borosilicate ester structure) has the highest initial decomposition temperature (310°C) and the highest residual rate at 500°C (50%), indicating that the five-membered cyclic borosilicate ester structure endows the product with superior thermal stability. The above results show that the borosilicate ester structure introduced through chemical bonds significantly improves the thermal stability of the product.

[0081] Experimental Example 6: Oxidative Stability Test Differential scanning calorimetry (DSC) was used to evaluate the oxidation induction period (OIT) of each product. Test conditions: oxygen atmosphere, constant temperature of 210°C. The results are shown in Table 6.

[0082] Table 6. Oxidative Stability Test Results (DSC) ; As shown in Table 6, the oxidation induction period of the borosilicate products of Examples 1-4 of this invention is ≥46 minutes, significantly longer than that of Comparative Example 1 (28 minutes) and Comparative Example 2 (25 minutes), indicating that the borosilicates of this invention have excellent antioxidant properties. Among them, Example 4 (five-membered cyclic borosilicate ester structure) has the longest oxidation induction period (55 minutes) and the best antioxidant performance. The results show that the introduction of the borosilicate ester structure effectively improves the oxidation stability of the product.

[0083] Application Example 1: Lubricating Oil Composition The products prepared in Examples 1-4 and Comparative Examples 1-2 of this invention were added to API Group I base oil (150SN) at an addition amount of 2 wt% to formulate a lubricating oil composition. The performance indicators of this lubricating oil composition are shown in Table 7.

[0084] Table 7 Performance Indicators of Lubricating Oil Compositions ; The results in Table 7 show that, compared with Comparative Examples 1-2, the boron sulfonates prepared in Examples 1-4 of the present invention, as lubricating oil additives, can significantly improve the anti-wear properties, detergency, thermal stability and oxidation stability of base oils, and the retention rate of boron in the oil is extremely high.

[0085] The above description is merely a preferred embodiment of the present invention and is not intended to limit the present invention in any way. Although the present invention has been disclosed above with reference to preferred embodiments, it is not intended to limit the present invention. Any person skilled in the art can make some modifications or alterations to the methods and techniques disclosed above without departing from the scope of the present invention to create equivalent embodiments. Any simple modifications, equivalent changes and alterations made to the above embodiments based on the technical essence of the present invention without departing from the scope of the present invention shall still fall within the scope of the present invention.

Claims

1. A borosilicate salt, characterized in that, The borosilicate sulfonate molecule contains a covalent structure of a benzene ring sulfonic acid ortho-five-membered cyclic borosilicate ester, and has the following general formula: R-C6H2(SO3M)-(OBO); Wherein, M is selected from at least one alkaline earth metal element; the parent nucleus group R is a C8-C30 alkyl group; -OBO- is connected to two adjacent carbon atoms on the benzene ring through oxygen atoms to form a five-membered cyclic borate ester structure; The borosulfonate is obtained by dehydration condensation and ring closure of alkylbenzene sulfonate with ortho-hydroxy-substituted benzene ring sulfonate and boric acid to form a five-membered cyclic boroate ester, with boron atoms embedded in the organic molecular skeleton of the sulfonate through BOC covalent bonds; The total base value of the borosulfonate is 200-500 mg KOH / g, and the boron content is 0.5-5.0 wt%.

2. The borosilicate salt according to claim 1, characterized in that, M is selected from at least one of calcium, magnesium, or barium; R is a C12-C24 straight-chain or branched alkyl group.

3. A method for preparing borosilicate sulfonate according to claim 1 or 2, characterized in that, Includes the following steps: S1: Add organic solvent, long-chain alkylbenzene sulfonic acid, heavy alkylbenzene sulfonic acid, low-carbon alcohol and base oil into a reaction vessel and mix. Then carry out a neutralization reaction at 40-80°C for 0.5-3 hours to obtain reaction mixture I. S2: Add alkaline earth metal oxides and water in batches to the obtained reaction mixture I, and pass carbon dioxide to carry out a carbonation reaction, controlling the free alkalinity to reach 200-400 mg KOH / g, to obtain reaction mixture II; S3: Add a hydroxylating agent to the obtained reaction mixture II and carry out a hydroxylation reaction at 50-100°C for 1-4 hours to introduce hydroxyl groups into the sulfonate molecules to obtain reaction mixture III; S4: Add boric acid to the obtained reaction mixture III and carry out a dehydration condensation reaction at 70-150°C for 2-8 hours to obtain reaction mixture IV; S5: The obtained reaction mixture IV is subjected to de-alcoholization and dehydration, centrifugation to remove residue, and distillation to remove solvent, to obtain the borosulfonate product.

4. The preparation method according to claim 3, characterized in that, In step S1, the components, by weight percentage, are: 30-55% organic solvent, 5-10% long-chain alkylbenzene sulfonic acid, 5-10% heavy alkylbenzene sulfonic acid, 1-8% low-carbon alcohol, and the balance being base oil.

5. The preparation method according to claim 3, characterized in that, In step S1, the organic solvent is a C6-C12 aromatic solvent or alkane solvent; The lower alcohol is a C1-C4 monohydric alcohol.

6. The preparation method according to claim 3, characterized in that, In step S2, the alkaline earth metal oxide is at least one of calcium oxide, magnesium oxide, or barium oxide; the amount of alkaline earth metal oxide added is 2-8% of the mass of reaction mixture I.

7. The preparation method according to claim 3, characterized in that, In step S3, the hydroxylating agent is selected from at least one of ethylene oxide, propylene oxide, ethylene glycol, glycerol, and diethanolamine; The amount of the hydroxylating agent added is 2-10% of the mass of reaction mixture II.

8. The preparation method according to claim 3, characterized in that, In step S3, the hydroxylation reaction is carried out in the presence of an alkaline catalyst, wherein the alkaline catalyst is selected from at least one of sodium hydroxide, potassium hydroxide, and triethylamine; The amount of alkaline catalyst added is 0.1-1% of the mass of reaction mixture II.

9. The preparation method according to claim 3, characterized in that, In step S4, the molar ratio of reaction mixture III to boric acid is 1:(0.5-3). The dehydration condensation reaction is carried out in the presence of a catalyst, which is selected from at least one of p-toluenesulfonic acid, sulfuric acid, and phosphoric acid. The amount of catalyst added is 0.1-1% of the mass of boric acid.

10. The use of borosilicate salts according to claim 1 or 2, or borosilicate salts prepared by the preparation method according to any one of claims 3-9, as lubricating oil additives in the preparation of lubricating oils.

Citation Information

Patent Citations

  • Method for producing alkaline earth metal borate dispersions

    US4683126A

  • Borated overbased material

    US4744920A