A Three-Dimensional Quantification Method for Cracks in Harbor Infrastructure Based on FBG Strain and Ultrasonic Fusion
By using FBG strain and ultrasonic fusion technology, the problem of three-dimensional quantification of cracks in port infrastructure has been solved. It has achieved synchronous and accurate quantification of crack width and depth, reduced false alarm rate and data drift, and improved quantification accuracy and environmental adaptability.
Patent Information
- Application Number
- CN202611592705.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-15
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies cannot simultaneously acquire crack width and depth, surface width is prone to underestimating the true crack width, point monitoring has blind spots, and data drift has a high false alarm rate in marine environments.
The method of FBG strain and ultrasound fusion is adopted. By acquiring surface strain data and internal ultrasonic response data, the FBG width is corrected by the kurtosis coefficient, and the crack activity is determined by combining the coefficient of variation of multiple consecutive measurements. Adaptive compensation is performed in a high humidity and large temperature difference environment to fit the three-dimensional spatial morphology of the crack.
It achieves simultaneous and accurate quantification of crack width and depth, reduces false alarm rate, enhances early warning reliability, suppresses data drift, and improves quantification accuracy and environmental adaptability.
Smart Images

Figure CN123118928A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of structural health monitoring technology, and in particular to a three-dimensional quantification method for cracks in harbor infrastructure based on the fusion of FBG strain and ultrasound. Background Technology
[0002] Harbor terminals, breakwaters, and other infrastructure are exposed to harsh marine environments characterized by high salinity, high humidity, and high wave impact, making reinforced concrete structures highly susceptible to cracking. The width, depth, and spatial propagation pattern of cracks are key indicators for evaluating structural safety and remaining lifespan. Without accurate quantification of the three-dimensional dimensions of cracks, it is difficult to promptly assess the degree of structural deterioration and formulate maintenance plans, potentially leading to structural failure. Current technologies, particularly traditional crack gauges, are essentially point-based measuring devices that can only measure the opening displacement of known cracks at the sensor's installation location. They cannot detect or locate randomly emerging, unknown cracks on the structure, resulting in significant monitoring blind spots. Furthermore, they typically only provide displacement data in a single direction, failing to reconstruct the actual morphology of cracks in three-dimensional space. They can only be installed on the structural surface, rendering them ineffective in detecting internal crack development. Especially in the harsh environment of harbors with high salt spray and high humidity, traditional electrical crack gauges suffer from fundamental limitations such as short lifespan and severe data drift.
[0003] In recent years, there have been relevant studies and public reports on the combination of fiber Bragg grating (FBG) strain sensors and ultrasonic guided wave technology for structural health monitoring. For example, existing literature has proposed an "intelligent identification method for fatigue cracks in spacecraft structures based on fiber gratings and ultrasonic guided waves," which also adopts the technical approach of combining passive monitoring by fiber optic sensing with active detection by ultrasonic guided waves. In addition, research has also been published on the use of a hybrid system of FBG and piezoelectric ceramics for ultrasonic guided wave detection. However, the above-mentioned existing solutions only combine FBG and ultrasonic technology at a shallow physical superposition level of "separate acquisition and independent output," and have not achieved deep fusion and cross-correction of the two types of heterogeneous sensing data at the physical mechanism level. Specifically, FBG strain sensors can only sense the average strain field of the structural surface. The crack width obtained by inferring the crack width through strain is greatly affected by crack depth, stress concentration at the tip, and non-uniform deformation of concrete. When the crack depth is large or multiple microcracks coexist, the surface strain response often seriously underestimates the opening degree of the actual crack. Although ultrasonic guided wave technology is sensitive to internal depth, existing methods have failed to utilize ultrasonic depth information and waveform distortion characteristics to specifically correct the surface width measured by FBG. Furthermore, the existing scheme does not introduce an online discrimination mechanism for the dynamic activity of cracks, and cannot distinguish between stable cracks and active propagating cracks, resulting in high false alarm and false alarm rates. It also lacks adaptive compensation methods for marine high humidity and large temperature difference environments, resulting in serious drift of measurement data and environmental disturbances being easily misjudged as structural damage.
[0004] In summary, although the technical concept of fusing FBG and ultrasound has been proposed, there are still no effective technical solutions disclosed, such as how to dynamically correct the FBG surface width using the kurtosis coefficient of the ultrasonic envelope to solve the problem of width underestimation, how to determine crack activity based on the coefficient of variation of multiple consecutive measurements to reduce false alarm rate, how to construct an adaptive temperature and humidity compensation mechanism for the high humidity and large temperature difference environment of the ocean to suppress data drift, and how to use the opening angle measured by the cross-shaped FBG as a directional constraint to fit the three-dimensional spatial morphology of the crack, so as to realize the simultaneous and accurate quantification of crack width, depth and three-dimensional orientation in the marine environment. Summary of the Invention
[0005] To address the problems of existing technologies being unable to simultaneously acquire crack width and depth, easily underestimating the true crack width, having blind spots in point monitoring, and high false alarm rates due to data drift in marine environments, this invention provides a three-dimensional quantification method for cracks in harbor infrastructure based on FBG strain and ultrasonic fusion.
[0006] The technical solution adopted by this invention to solve its technical problem is: a three-dimensional quantification method for cracks in harbor infrastructure based on FBG strain and ultrasonic fusion. Preferably, the method includes: S1: acquiring strain data from a strain sensing array arranged on the surface of the structure under test, and ultrasonic response data from an ultrasonic sensing array arranged inside the structure; S2: determining whether the crack triggering condition is met based on the change characteristics of the strain data, and determining the surface opening width and initial position of the crack based on the response differences of each sensor in the strain sensing array when triggered; S3: in response to the triggering, exciting the ultrasonic sensing array to emit ultrasonic guided waves and receiving its response signal, extracting waveform feature parameters characterizing the crack morphology from the response signal, and inverting the internal depth information of the crack; S4: inputting the surface opening width, the internal depth information, and the waveform feature parameters into a pre-constructed fusion correction model, and outputting the corrected true crack width and true depth; S5: based on the corrected true crack width, true depth, and their corresponding spatial coordinates, fitting and generating a three-dimensional spatial morphological representation of the crack.
[0007] Preferably, the fusion correction model includes the following empirical formula: ; ; in, This is the corrected actual width, in mm. The width of the surface opening measured by the FBG strain sensor is in mm. This is the corrected actual depth, in mm. The kurtosis coefficient of the waveform envelope is dimensionless. denoted as the average crack depth obtained by ultrasonic inversion, in mm; 0.1 is the reference width constant; and 0.3 and 0.2 are empirical indices fitted by experiments.
[0008] Preferably, the waveform characteristic parameters include the kurtosis coefficient. The received ultrasonic envelope is extracted using the following formula, and the sharpness of the four peaks of the envelope is calculated: ; in, The fourth central moment of the envelope amplitude, The second central moment of the envelope amplitude; when When >0, the crack is determined to be a single through crack; when When <0, the crack is determined to be multiple microcracks; when When the value is 0, it is determined that the crack morphology is between the two or the signal is greatly affected by noise, and it needs to be judged in combination with other characteristic parameters.
[0009] Preferably, in step S2, the method of triggering a measurement is not to trigger it only once, but to record five consecutive measurement results every two minutes after the trigger starts, and calculate the coefficient of variation of the opening width for these five measurements. The calculation formula is: ; in, The standard deviation of the five opening width values is expressed in mm. The average of five opening width values, in mm; if the coefficient of variation If the value is greater than 0.15, it indicates the crack is still active; in this case, add a 15% safety margin to the final output width value. This indicates that the crack is in a transitional state, and the average value is directly taken as the final output width value without increasing the safety margin; if If the value is less than 0.1, it indicates that the crack has stabilized, and the average value is taken directly.
[0010] Preferably, in addition to extracting the wave velocity of the L(0,1) mode wave, the response signal also extracts the arrival time difference between the second arriving F(1,1) mode wave and the first arriving L(0,1) mode wave, and defines the arrival time difference as... The unit is microseconds; when the arrival time difference Compared to the baseline arrival time difference in a healthy state When the increase exceeds 20 microseconds, it is determined that the crack depth has exceeded the thickness of the concrete protective layer, and the upper limit of the correction coefficient of the empirical formula described in S4 is adjusted from 1.3 to 1.8.
[0011] Preferably, the FBG strain sensors in the strain sensing array are arranged in a cross pattern, with a first FBG strain sensor parallel to the predicted crack direction and a second FBG strain sensor perpendicular to the predicted crack direction simultaneously attached at each measuring point; let the strain in the parallel direction be... The strain in the vertical direction is Then the opening angle of the crack Calculate using the following formula: ; in For strain in the parallel direction, Strain in the vertical direction. The opening angle of the crack; the opening angle of the crack As a directional constraint when fitting space curves in S5.
[0012] Preferably, a self-check and compensation step is included between S3 and S4: synchronously collecting ambient temperature. and relative humidity The ambient temperature, measured in degrees Celsius, was collected synchronously. The unit is a percentage; when the condition is met... >90% or the absolute value of the temperature change At temperatures above 2 degrees Celsius, compensation values are obtained in real time using reference sensors deployed in unloaded locations. The strain data from the FBG strain sensor in the strain sensing array and the ultrasonic response data from the ultrasonic sensing array are compensated and calibrated respectively, so that both sets of data return to the reference state, and then step S4 is executed; wherein, the temperature change amount This represents the difference between the current ambient temperature and the initial ambient temperature.
[0013] Preferably, the empirical formula in the fusion correction model is a set of coefficient tables corresponding to the structural location type where the crack is located. The coefficient tables include three sets of independent coefficients for the beam area, the pile area, and the panel area. Each set of coefficients is pre-calibrated by conducting destructive tests on the corresponding type of specimens and fitting the data. During use, the operator manually selects the current structural location type and calls the corresponding coefficients to participate in the calculation.
[0014] The beneficial effects of this invention are as follows: By substituting the surface opening width measured by FBG and the crack depth obtained by ultrasonic inversion into the empirical formula for kurtosis coefficient correction, the problem of a single sensor being unable to simultaneously acquire crack width and depth is solved, thus avoiding an underestimation of the true crack extent by the surface width. The introduction of the kurtosis coefficient of the ultrasonic envelope distinguishes between single through-cracks and multiple microcracks, and the correction coefficient is dynamically adjusted accordingly, significantly improving the quantification accuracy under different crack morphologies. The use of the coefficient of variation from multiple consecutive measurements to determine crack activity proactively adds a safety margin, enhancing the reliability of early warning. Combined with environmental temperature and humidity self-checking and real-time compensation from reference sensors, data drift in high-humidity and large-temperature-difference marine environments is effectively suppressed, reducing the false alarm rate. Fifth, the opening angle measured by the cross-shaped FBG can constrain spatial curve fitting, and can also output manual verification prompts when the number of sensors is insufficient, balancing the flexibility of automated monitoring and on-site verification. Attached Figure Description
[0015] To more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are merely exemplary, and those skilled in the art can derive other embodiments based on the provided drawings without creative effort.
[0016] Figure 1 This is a flowchart of the optimal embodiment of the method for three-dimensional quantification of cracks in harbor infrastructure based on the fusion of FBG strain and ultrasound of the present invention; Figure 2 This is a diagram illustrating the calculation steps of the fusion correction model for the three-dimensional quantification method of cracks in harbor infrastructure based on the fusion of FBG strain and ultrasound in this invention. Figure 3 This invention presents a three-dimensional quantification method for cracks in harbor infrastructure based on the fusion of FBG strain and ultrasound, with step-by-step diagrams illustrating crack activity identification and temperature and humidity compensation. Detailed Implementation
[0017] The technical solutions of the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.
[0018] Example 1 like Figure 1 As shown, this invention is a three-dimensional quantification method for cracks in harbor infrastructure based on the fusion of FBG strain and ultrasound, including the following: S1: Acquire strain data from a strain sensor array arranged on the surface of the structure under test, and ultrasonic response data from an ultrasonic sensor array arranged inside the structure. In areas of the concrete surface prone to cracking, specifically along the longitudinal centerline at the bottom of the crossbeam span, a row of FBG strain sensors is installed. The center-to-center distance between adjacent FBG strain sensors is 1 meter. The FBG strain sensors are wavelength-modulated fiber optic grating sensors with a center wavelength range of 1525nm to 1565nm, providing a strain measurement accuracy of ±1 microstrain and a range of ±5000 microstrain. Epoxy resin adhesive is used to firmly bond the sensors to the cleaned concrete surface, ensuring reliable strain transmission.
[0019] Simultaneously, an ultrasonic sensor array is welded every 2 meters along the axis of the corresponding reinforcing steel bars inside the concrete. The ultrasonic sensor array uses lead zirconate titanate piezoelectric ceramic transducers with a center frequency of 75kHz, a resonant impedance of no more than 100 ohms, and a transmission voltage of ±50 volts. Before welding, a metallic luster is polished onto the surface of the reinforcing steel bars. Low-temperature solder is used to weld and fix the transducer leads to the reinforcing steel bars, and the weld points are sealed with epoxy resin to prevent electrochemical corrosion in the marine environment.
[0020] To further improve the ability to identify crack spatial morphology, two FBG strain sensors are installed at each measuring point in a cross-shaped arrangement. Specifically, at the center of each measuring point, the first FBG strain sensor is first installed with its axis parallel to the predicted crack direction, i.e., parallel to the axis of the beam. Then, the second FBG strain sensor is installed with its axis perpendicular to the predicted crack direction, i.e., perpendicular to the axis of the beam. Let the strain in the parallel direction be... The strain in the vertical direction is Then the opening angle of the crack Calculate using the following formula: ; in, The strain is perpendicular to the predicted crack direction, dimensionless, and the unit is microstrain; The strain is parallel to the predicted crack direction, dimensionless, and the unit is microstrain; The crack opening angle is expressed in degrees, ranging from 0 to 90 degrees. When the temperature is close to 0 degrees, it indicates that the crack is basically perpendicular to the monitoring direction; when When the angle approaches 90 degrees, it indicates that the crack is essentially parallel to the monitoring direction. This opening angle... This will be used as a directional constraint in the subsequent S5 to make the fitted crack space curve more consistent with the actual mechanical morphology.
[0021] All FBG strain sensors and ultrasonic sensor arrays continuously acquire data, with sampling frequencies set to 100Hz and 1MHz, respectively.
[0022] S2: Based on the variation characteristics of the strain data, determine whether the crack triggering condition has been met, and upon triggering, determine the surface opening width and initial position of the crack based on the response differences of each sensor in the strain sensing array. The system triggers a complete crack measurement when the strain change rate of three consecutive FBG strain sensors all exceeds 5%. The formula for calculating the strain change rate is: ; in, For the rate of change of strain, The strain value at the current moment. The strain value at the previous moment is taken as the average strain value within 10 seconds before triggering, in order to eliminate the influence of instantaneous noise.
[0023] After triggering, the strain differential meter of the FBG strain sensor is first used to calculate the crack center location, surface opening width, and surface opening width. The calculation method is as follows: At the triggering moment, measure the strain values of all FBG strain sensors and subtract their initial strain values under healthy structural conditions to obtain the strain difference. The sensor location with the largest strain difference is taken as the crack center location. Surface opening width. The calculation formula is: ; in, The strain difference is dimensionless. In this embodiment, the effective sensing length of the FBG strain sensor is... =5mm, The unit is mm.
[0024] like Figure 3 As shown, to improve the reliability of crack activity assessment, instead of measuring only once after triggering, five consecutive measurements are recorded every two minutes from the start of triggering. These measurements are recorded as follows: , , , , All values are in mm. Calculate the coefficient of variation for these 5 opening width values. The calculation formula is as follows: ; in, The coefficient of variation is dimensionless. The standard deviation of the five opening width values is expressed in mm. The calculation formula is as follows: ; The average of 5 opening width values, in mm, is calculated using the following formula: ; If the coefficient of variation A value >0.15 indicates that the crack is still in an active propagation state, and the crack width is continuously changing. To prevent underestimating the crack width, a 15% safety margin is added to the final output width value; that is, the final width is the average of five measurements multiplied by 1.15. If the coefficient of variation... If the coefficient of variation is less than 0.1, it indicates that the crack has stabilized and the width variation is very small. Therefore, the average of the five measurements is taken as the final width output. If the coefficient of variation... If the value is between 0.1 and 0.15, the average value is taken directly without increasing the safety margin.
[0025] S3: In response to the trigger, the ultrasonic sensing array is excited to emit ultrasonic guided waves and its response signal is received. Waveform feature parameters characterizing the crack morphology are extracted from the response signal, and the internal depth information of the crack is inverted. Simultaneously with the trigger measurement, an L(0,1) mode ultrasonic guided wave with a center frequency of 75 kHz is emitted by the ultrasonic sensor array. The L(0,1) mode is the longitudinal mode of ultrasonic guided waves, characterized by non-dispersion, stable propagation speed, and sensitivity to cracks. The emitted waveform uses a 5-cycle sinusoidal pulse modulated by a Hanning window, with an excitation voltage of ±50 volts. The ultrasonic sensor array at the receiving end acquires the guided wave signal, with a sampling frequency of 2.5 MHz and a recording length of 500 microseconds.
[0026] The received guided wave signal is processed by a bandpass filter with a passband of 50kHz to 100kHz. Then, the signal envelope is extracted. The envelope is calculated by performing a Hilbert transform on the original signal and then calculating the magnitude of the transformed signal. Three characteristic parameters are extracted from the envelope: wave velocity, amplitude attenuation, and kurtosis coefficient of the waveform envelope. .
[0027] The formula for calculating the wave speed is: ; in, Wave speed, measured in meters per second; The straight-line distance between the transmitting transducer and the receiving transducer is expressed in meters. The time difference between the time of transmission and the time of receiving the peak of mode L(0,1) is the flight time, expressed in seconds.
[0028] The formula for calculating the amplitude attenuation is: ; in, For amplitude attenuation, The maximum amplitude of the received wave. The reference amplitude of the transmitted wave. The unit is decibel.
[0029] Kurtosis coefficient The following formula is used to describe the sharpness of the received waveform envelope, i.e., the steepness of its distribution pattern: ; in, The fourth central moment of the envelope amplitude, This is the second-order central moment of the envelope amplitude. The formula for calculating the central moment is: ; ; in, For the first on the envelope The amplitude of each sampling point The average value of the envelope amplitude. The total number of sampling points. This is the dimensionless kurtosis coefficient, with a baseline value of 0 corresponding to a normal distribution. Those skilled in the art will understand that for a Gaussian distribution, ... It equals 0; for a more angular distribution, For a more flattened distribution, the result is positive; It is a negative value.
[0030] when When >0, the crack is determined to be a single through crack; when When <0, the crack is determined to be multiple microcracks; when When the value is 0, it is determined that the crack morphology is between the two or that the signal is greatly affected by noise, and other characteristic parameters need to be considered for comprehensive judgment. The physical principle is as follows: a single through crack scatters ultrasonic guided waves more concentratedly, and the received wave envelope shows a sharp single-peak shape with a large kurtosis coefficient; multiple microcracks cause multiple scattering and mode conversion of guided waves, and the received wave envelope is broadened and flattened with a smaller kurtosis coefficient.
[0031] Simultaneously, the average depth of the crack was inverted using wave velocity attenuation data. The inversion method involves pre-establishing a calibration curve between crack depth and wave velocity attenuation. Concrete specimens with pre-cast cracks of different depths are used to measure the corresponding ultrasonic guided wave velocity attenuation. The linear relationship between depth and attenuation is then obtained using the least squares method. ; in, This represents the wave velocity attenuation value, in dB. This is the attenuation coefficient, expressed in dB / mm. This is a calibration constant, in mm. The unit is mm. Specifically, in this embodiment, when the wave velocity attenuation is 3dB, the calibration curve is given. The value is 20mm; when the wave velocity attenuates to 6dB, The value is 40mm; when the wave velocity attenuation is 9dB, It is 60mm.
[0032] To further determine whether the crack has exceeded the thickness of the concrete cover, this embodiment also extracts the arrival time difference between the second arriving F(1,1) mode wave and the first arriving L(0,1) mode wave. The unit is microseconds. The F(1,1) mode is the bending mode in ultrasonic guided waves, which is more sensitive to changes in crack depth. Time difference with baseline arrival under structural health conditions Comparison. Benchmark This is obtained through a single measurement when the structure is not cracked, for example: when The crack depth was determined to exceed the thickness of the concrete cover. The thickness of the concrete protective layer. for Group velocity of modal waves.
[0033] S4: Input the surface opening width, the internal depth information and the waveform feature parameters into the pre-built fusion correction model, and output the corrected crack true width and true depth; like Figure 2 As shown, the surface opening width obtained by S2 The average crack depth obtained from S3 and kurtosis coefficient Substitute the following empirical formula for correction: ; ; in, The corrected actual width, in mm; The width of the surface opening measured by the FBG strain sensor is in mm. This is the corrected actual depth, in mm; The kurtosis coefficient of the waveform envelope is dimensionless. 0.1 is the average crack depth obtained by ultrasonic inversion, in mm; 0.1 is the reference width constant, in mm, representing a reference value for the width of a typical crack opening; 0.3 and 0.2 are empirical indices obtained by fitting through failure tests of a large number of specimens with different crack morphologies, and are dimensionless.
[0034] The calibration process for the above empirical formula is as follows: Ten sets of concrete specimens were prepared, each set containing two types of crack morphologies: single through cracks and multiple microcracks. The crack widths ranged from 0.05 mm to 0.5 mm, and the depths ranged from 10 mm to 80 mm. FBG strain gauges were attached to the surface of the specimens for measurement. Measurement using ultrasonic guided waves and The true width and depth are obtained by direct measurement after cutting. Nonlinear regression fitting yields coefficients of 0.3 and 0.2, along with a baseline width constant of 0.1 mm, and a coefficient of determination. A value greater than 0.95 indicates that the formula has high prediction accuracy.
[0035] For cases where the crack depth exceeds the thickness of the concrete cover, the upper limit of the coefficient in the formula is adjusted from 1.3 to 1.8. This is because when the crack depth exceeds the cover, the bond between the steel reinforcement and the concrete deteriorates more severely, and the representativeness of the surface width to the true width further decreases, so it is necessary to increase the upper limit of the correction.
[0036] Between S3 and S4, this embodiment also performs a self-check and compensation step. The system synchronously collects the ambient temperature. and relative humidity The ambient temperature was collected simultaneously in degrees Celsius. The units are percentages. The temperature sensor is a PT100 platinum resistance thermometer, and the humidity sensor is a capacitive humidity sensor. Initial ambient temperature. and initial relative humidity Recorded during system installation.
[0037] When relative humidity Greater than 90% or the absolute value of the temperature change Compensation is activated when the temperature exceeds 2 degrees Celsius. Compensation values are acquired in real time using reference sensors deployed in unloaded locations. The reference sensor is identical in model to the working sensor, but it is mounted in a location unaffected by structural forces and only senses environmental changes. All strain changes or ultrasonic time-of-flight variations measured by the reference sensor are attributed to environmental factors, denoted as . For FBG strain sensors, the compensated strain value is equal to the original measured strain value minus... : For ultrasonic sensor arrays, the compensated flight time is equal to the original measurement flight time minus... : After both sets of data have returned to the baseline state, the correction calculation in S4 is then performed. The baseline state is defined as temperature. relative humidity The sensor response at that time.
[0038] S5: Based on the corrected true width and true depth of the crack and its corresponding spatial coordinates, a three-dimensional spatial morphological representation of the crack is fitted and generated. The corrected crack width ,depth The spatial coordinates of each sensor are projected onto the same three-dimensional coordinate system. The spatial coordinates of the sensors are obtained by pre-measuring the three-dimensional coordinates of each sensor installation point, with an accuracy of ±1mm. The origin of the coordinate system can be set to the lower left corner of the monitoring area, with the X-axis along the length of the beam, the Y-axis along the width of the beam, and the Z-axis along the depth.
[0039] A spatial curve was fitted to these discrete points using the least squares method. The specific fitting method is as follows: the X and Y coordinates of the discrete points were used as independent variables, and the crack width was... As the dependent variable, cubic spline interpolation was used to fit a curve showing the width variation along the crack direction. The width corresponding to the highest point of this curve was taken as the maximum crack width. The total crack length was obtained by integrating along the curve, i.e., integrating from the outermost sensor position at one end of the crack to the outermost sensor position at the other end. During the fitting process, the crack opening angle calculated in S1 was used. As a directional constraint, the tangent direction of the fitted curve should be parallel to... Maintain consistency to avoid creating a distorted curve that does not match the actual force applied.
[0040] Finally, the system outputs three-dimensional quantitative results of the cracks, including maximum width (mm), average depth (mm), total length (meters), spatial orientation (represented by the three-dimensional coordinates of the starting and ending points), and crack type (single through crack or multiple microcracks). These results are displayed on the monitoring interface as a color three-dimensional surface plot, where width is represented by color intensity and depth by contour lines.
[0041] Example 2 Comparative Experiment: To verify the improvement effect of the proposed fusion correction model on the quantitative accuracy of crack width and depth, a comparative experiment was designed in this embodiment. Ten precast concrete beam specimens from the same batch were selected, with dimensions of 150mm×200mm×1200mm, concrete strength grade C40, and protective layer thickness of 25mm. Cracks of different widths (0.05mm~0.50mm) and different depths (10mm~60mm) were precast in the mid-span region of each specimen by three-point bending loading, resulting in a total of 30 valid crack samples.
[0042] The following three methods were used to measure each group of cracks: The method of this invention: Following the complete process of Example 1, FBG strain and ultrasonic guided wave data are acquired simultaneously, and the corrected width is output after fusion correction model. and correction depth .
[0043] Pure FBG method: Utilizing only the surface strain difference value of the FBG strain sensor according to the formula... The width and depth of the surface opening cannot be obtained when calculating it.
[0044] Pure ultrasonic method: Inverting the average crack depth using only the wave velocity attenuation of ultrasonic guided waves. and with As a depth output, no FBG width correction is performed; width information cannot be obtained.
[0045] All measurement results were compared with the actual values measured directly after the specimen was cut, and the mean relative error (MRE) and standard deviation (SD) were calculated. The results are shown in Table 1.
[0046] Table 1 Comparison of the method of the present invention with the pure FBG method and the pure ultrasound method This document uses specific examples to illustrate the principles and implementation methods of this application. The descriptions of the above embodiments are only for the purpose of helping to understand the methods and core ideas of this application. The above descriptions are only preferred embodiments of this application. It should be noted that due to the limitations of written expression, while there are objectively infinite specific structures, those skilled in the art can make several improvements, modifications, or changes without departing from the principles of this application, and can also combine the above technical features in an appropriate manner. These improvements, modifications, changes, or combinations, or the direct application of the inventive concept and technical solution to other situations without modification, should all be considered within the scope of protection of this application.
Claims
1. A three-dimensional quantification method for cracks in harbor infrastructure based on FBG strain and ultrasonic fusion, characterized in that, include: S1: Acquire strain data from a strain sensor array arranged on the surface of the structure under test, and ultrasonic response data from an ultrasonic sensor array arranged inside the structure. S2: Based on the change characteristics of the strain data, determine whether the crack triggering condition has been met, and when triggered, determine the surface opening width and initial position of the crack according to the response differences of each sensor in the strain sensing array; S3: In response to the trigger, the ultrasonic sensing array is excited to emit ultrasonic guided waves and its response signal is received. Waveform feature parameters characterizing the crack morphology are extracted from the response signal, and the internal depth information of the crack is inverted. S4: Input the surface opening width, the internal depth information and the waveform feature parameters into the pre-built fusion correction model, and output the corrected crack true width and true depth; S5: Based on the corrected true width and true depth of the crack and its corresponding spatial coordinates, a three-dimensional spatial morphological representation of the crack is generated by fitting.
2. The method for three-dimensional quantification of cracks in harbor infrastructure based on FBG strain and ultrasonic fusion as described in claim 1, characterized in that, The fusion correction model includes the following empirical formula: ; ; in, This is the corrected actual width, in mm. The width of the surface opening measured by the FBG strain sensor is in mm. This is the corrected actual depth, in mm. The kurtosis coefficient of the waveform envelope is dimensionless. denoted as the average crack depth obtained by ultrasonic inversion, in mm; 0.1 is the reference width constant; and 0.3 and 0.2 are empirical indices fitted by experiments.
3. The method for three-dimensional quantification of cracks in harbor infrastructure based on FBG strain and ultrasonic fusion as described in claim 1, characterized in that, The waveform characteristic parameters include kurtosis coefficient. The received ultrasonic envelope is extracted using the following formula, and the sharpness of the four peaks of the envelope is calculated: ; in, The fourth central moment of the envelope amplitude, The second central moment of the envelope amplitude; when When >0, the crack is determined to be a single through crack; when When <0, the crack is determined to be multiple microcracks; when When the value is 0, it is determined that the crack morphology is between the two or the signal is greatly affected by noise, and it needs to be judged in combination with other characteristic parameters.
4. The method for three-dimensional quantification of cracks in harbor infrastructure based on FBG strain and ultrasonic fusion as described in claim 1, characterized in that, After the trigger is activated, five consecutive measurements are recorded every two minutes from the start of the trigger, and the coefficient of variation of the opening width is calculated for these five measurements. The calculation formula is: ; in, The standard deviation of the five opening width values is expressed in mm. This is the average of five opening width values, in mm. If the coefficient of variation If the value is greater than 0.15, it indicates that the crack is still active. In this case, add a 15% safety margin to the final output width value. if This indicates that the crack is in a transitional state, and the average value is directly taken as the final output width value without increasing the safety margin. if If the value is less than 0.1, it indicates that the crack has stabilized, and the average value is taken directly.
5. The method for three-dimensional quantification of cracks in harbor infrastructure based on FBG strain and ultrasonic fusion as described in claim 2, characterized in that, In addition to extracting the wave velocity of the L(0,1) mode wave, the response signal also extracts the arrival time difference between the second arriving F(1,1) mode wave and the first arriving L(0,1) mode wave, and defines the arrival time difference as... The unit is microseconds; When the arrival time difference Compared to the baseline arrival time difference in a healthy state When the increase exceeds 20 microseconds, it is determined that the crack depth has exceeded the thickness of the concrete protective layer, and the upper limit of the correction coefficient of the empirical formula is adjusted from 1.3 to 1.
8.
6. The method for three-dimensional quantification of cracks in harbor infrastructure based on FBG strain and ultrasonic fusion as described in claim 1, characterized in that, The FBG strain sensors in the strain sensing array are arranged in a cross pattern, with a first FBG strain sensor parallel to the crack prediction direction and a second FBG strain sensor perpendicular to the crack prediction direction attached at each measuring point. Let the strain in the parallel direction be... The strain in the vertical direction is Then the opening angle of the crack Calculate using the following formula: ; in For strain in the parallel direction, Strain in the vertical direction. The opening angle of the crack; The opening angle of the crack As a directional constraint when fitting space curves in S5.
7. The method for three-dimensional quantification of cracks in harbor infrastructure based on FBG strain and ultrasonic fusion as described in claim 1, characterized in that, A self-check and compensation step is also included between S3 and S4: Simultaneous collection of ambient temperature and relative humidity The ambient temperature, measured in degrees Celsius, was collected synchronously. The unit is percentage; When satisfied >90% or the absolute value of the temperature change At temperatures above 2 degrees Celsius, compensation values are obtained in real time using reference sensors deployed in unloaded locations. The strain data of the FBG strain sensor in the strain sensing array and the ultrasonic response data of the ultrasonic sensing array are compensated and calibrated respectively, so that both sets of data return to the reference state, and then S4 is executed. Wherein, the temperature change This represents the difference between the current ambient temperature and the initial ambient temperature.
8. The method for three-dimensional quantification of cracks in harbor infrastructure based on FBG strain and ultrasonic fusion as described in claim 1, characterized in that, The empirical formula in the fusion correction model is a set of coefficient tables corresponding to the structural location type where the crack is located. The coefficient tables include three sets of independent coefficients for the beam area, the pile area, and the panel area. Each set of coefficients is pre-calibrated by conducting destructive tests on the corresponding type of specimens and fitting the data. During use, the operator manually selects the current structural location type and calls the corresponding coefficients to participate in the calculation.