A method, apparatus, equipment and storage medium for adapting corrosion protection materials for hardware fittings.

By constructing an atomic model of the hardware interface and performing molecular dynamics simulations, key corrosion control factors were obtained, solving the problem of the lack of microscopic mechanisms in the design of hardware protective materials in salt lake environments. This enabled precise adaptation of protective materials and improved the service reliability and protective effect of hardware.

CN123120073APending Publication Date: 2026-11-17HAIXI POWER SUPPLY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611512089.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-28
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing technologies cannot effectively reveal the atomic-level reaction mechanism of the hardware interface in the complex brine environment of salt lakes. This results in a lack of targeted guidance on the microscopic mechanism in the design of protective materials, making them unsuitable for the harsh working conditions of multi-factor coupling in high-altitude salt lakes. Consequently, protective materials fail quickly and have short replacement cycles.

Method used

By constructing an atomic model of the zinc plating layer/steel substrate-electrolyte interface and using ReaxFF reactive force field molecular dynamics simulation, atomic trajectory data is generated to obtain dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion. The ion diffusion coefficient and reaction energy barrier are calculated, the contribution weight of each ion is statistically analyzed, and the mapping relationship between environment, material, and lifetime is established to generate a selection scheme for protective materials adapted to different corrosion levels.

Benefits of technology

It achieves precise matching of protective materials with the highly corrosive working conditions of salt lakes, solves the problem of blind selection of protective materials in existing technologies, and improves the service reliability and protective effect of fittings.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123120073A_ABST
    Figure CN123120073A_ABST
Patent Text Reader

Abstract

This application provides a method, apparatus, equipment, and storage medium for adapting corrosion protection materials for metal fittings. The method includes: obtaining the composition of the zinc plating layer and steel substrate of the metal fittings, as well as the types and concentrations of chloride, magnesium, and sulfate ions in the salt lake environment; constructing an atomic model of the zinc plating layer / steel substrate-electrolyte interface based on this, and performing ReaxFF molecular dynamics simulation to generate atomic trajectory data; obtaining dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion from the data, calculating the ion diffusion coefficient and reaction energy barrier, statistically analyzing the contribution weight of each ion to extract key corrosion control factors; establishing an environment-material-lifetime mapping relationship, and generating a selection scheme for protective materials adapted to different corrosion levels. This application reveals the corrosion mechanism of complex brine ions in salt lakes at the atomic scale and extracts key control factors, solving the problem of blind selection of protective materials and achieving precise adaptation of protective materials to the highly corrosive conditions of salt lakes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This application belongs to the field of metal fitting corrosion protection, and in particular relates to a method, apparatus, equipment and storage medium for adapting metal fitting corrosion protection materials. Background Technology

[0002] As crucial components responsible for mechanical connections, electrical transitions, and load transfer, the reliability of overhead transmission line fittings directly impacts the long-term safe operation of the entire line. Transmission lines are typically exposed to complex natural environments such as high humidity, high salt spray, industrial pollution, and fluctuating temperatures, making fittings highly susceptible to various forms of corrosion damage. This can lead to increased contact resistance, decreased mechanical strength, and even fracture failure, seriously threatening line operational safety. Particularly in high-altitude salt lake regions, line fittings are subjected to multiple environmental stresses, including high salt deposits, strong ultraviolet radiation, alternating wet and dry conditions, and drastic diurnal temperature variations. These stresses make them prone to plating thinning, localized corrosion, coating deterioration, and connection failure, further inducing a decline in mechanical performance and deterioration of electrical contact.

[0003] Currently, a comprehensive technical system has been established for corrosion prevention and maintenance management of transmission line fittings, encompassing corrosion mechanism testing and the development of protective materials. In the areas of corrosion mechanism and material protection, researchers have analyzed the corrosion behavior of metallic materials through salt spray tests and electrochemical measurements, developing a series of anti-corrosion coatings such as epoxy zinc-rich coatings, polyurethane coatings, and fluorocarbon coatings, providing diverse material options for basic fitting protection. However, existing corrosion mechanism research largely remains at the level of macroscopic electrochemistry and apparent phenomena, lacking sufficient understanding of the atomic-level reactions of salt lake composite brine ions at the fitting interface, the passivation film destruction, and the ion diffusion mechanism. The design of protective materials lacks targeted guidance based on microscopic mechanisms, leading to rapid failure and poor environmental adaptability of conventional protection systems under multi-factor coupled environments.

[0004] In their research on existing technologies, the inventors discovered that the above-mentioned technical solutions analyze corrosion behavior through macroscopic electrochemistry and apparent phenomena, and select protective materials based on conventional environmental experience. However, due to insufficient understanding of the atomic-level reactions of salt lake composite brine ions at the hardware interface, the destruction of passivation films, and the ion diffusion mechanism, the design of protective materials lacks targeted guidance based on microscopic mechanisms. This makes them unsuitable for the harsh working conditions of multi-factor coupling in high-altitude salt lakes, resulting in rapid protection failure and short replacement cycles. Summary of the Invention

[0005] The purpose of this application is to overcome the deficiencies in the prior art and provide a method, apparatus, equipment and storage medium for adapting corrosion protection materials for hardware.

[0006] This application provides a method for adapting corrosion protection materials for hardware, including:

[0007] Material properties are obtained from the fittings, including the composition of the galvanized layer and the steel substrate;

[0008] Environmental parameters are obtained from the salt lake environment, including the types and concentrations of chloride ions, magnesium ions, and sulfate ions.

[0009] Based on the material properties and environmental parameters, an atomic model of the zinc plating layer / steel substrate-electrolyte interface was constructed.

[0010] Perform ReaxFF reactive force field molecular dynamics simulations on the atomic model to generate atomic trajectory data;

[0011] Dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion are obtained from the atomic trajectory data.

[0012] Calculate the ion diffusion coefficient and reaction energy barrier based on the dynamic process parameters.

[0013] Based on the ion diffusion coefficient and the reaction energy barrier, the contribution weight of each ion is calculated, and the key corrosion control factors are extracted.

[0014] Based on the aforementioned key corrosion control factors, an environment-material-lifetime mapping relationship is established;

[0015] Based on the mapping relationship, a selection scheme for protective materials adapted to different corrosion levels is generated.

[0016] Optionally, an atomic model of the zinc plating / steel substrate-electrolyte interface is constructed, including:

[0017] The atomic model is subjected to a dry-wet cycle condition, which includes a dry phase and a wet phase.

[0018] During the drying stage, the number of water molecules in the atomic model is reduced and the ion mobility is decreased.

[0019] During the wetting phase, the number of water molecules and ion mobility in the atomic model are restored.

[0020] Optionally, among the dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion obtained from the atomic trajectory data, the dynamic process parameters of ion competitive adsorption obtained from the atomic trajectory data include:

[0021] The drying stage and the wetting stage are distinguished based on the time markers in the atomic trajectory data;

[0022] In the drying stage and the wetting stage, the occupancy rate of adsorption sites, adsorption residence time and desorption rate of chloride ions, magnesium ions and sulfate ions on the zinc plating layer surface are statistically analyzed respectively.

[0023] By comparing the adsorption site occupancy, adsorption residence time, and desorption rate between the drying stage and the wetting stage, the adsorption hysteresis effect under alternating dry and wet conditions is obtained.

[0024] Optionally, the ion diffusion coefficient is calculated, including:

[0025] Based on the atomic trajectory data, calculate the mean square displacement curve of each ion throughout the entire wet-dry cycle;

[0026] The mean square displacement curve is divided into several segments according to the time intervals of the drying stage and the wetting stage.

[0027] Linear fitting was performed on the mean square displacement curve of each segment to obtain the drying diffusion coefficient and the wetting diffusion coefficient.

[0028] Based on the time proportions of the drying stage and the wetting stage in the total cycle, the drying diffusion coefficient and the wetting diffusion coefficient are weighted and averaged to obtain the equivalent diffusion coefficient.

[0029] Optionally, the statistical contribution weighting of each ion includes:

[0030] The average interaction energy between the magnesium ion and the chloride ion, and the average interaction energy between the magnesium ion and the sulfate ion are calculated from the atomic trajectory data.

[0031] The average interaction energy is added as a correction term to the calculation of the contribution weight of each ion, so that the contribution weight of the magnesium ion is dynamically adjusted according to its cooperative adsorption strength with the chloride ion.

[0032] Optionally, the extraction of key corrosion control factors includes:

[0033] The adsorption stability parameters of magnesium ions on the zinc coating surface are extracted from the dynamic process parameters. The adsorption stability parameters include the average residence time of magnesium ions on the zinc oxide surface, the coordination number of magnesium ions with surface hydroxyl groups, and the probability of the formation of ion pairs between magnesium ions and chloride ions.

[0034] The adsorption stability parameter, along with the ion diffusion coefficient and the reaction barrier, are considered as key corrosion control factors.

[0035] Optionally, generate a selection scheme for protective materials adapted to different corrosion levels, including:

[0036] The ion type with the largest contribution weight was identified from the key corrosion control factors and determined as the dominant ion;

[0037] When the dominant ion is the chloride ion, the recommended selection scheme is an epoxy zinc-rich coating;

[0038] When the dominant ion is magnesium ion, the recommended selection scheme is fluorocarbon coating;

[0039] When the dominant ion is the sulfate ion, the recommended selection scheme is a polyurethane coating;

[0040] Adjust the coating thickness and application process according to the corrosion level.

[0041] This application also provides a fitting device for corrosion protection materials for hardware, including:

[0042] The acquisition module acquires material properties from the fittings, including the composition of the galvanized layer and the steel substrate;

[0043] The parameter module obtains environmental parameters from the salt lake environment, including the types and concentrations of chloride ions, magnesium ions, and sulfate ions.

[0044] The model module constructs an atomic model of the galvanized layer / steel substrate-electrolyte interface based on the material properties and environmental parameters.

[0045] The simulation module performs ReaxFF reactive force field molecular dynamics simulations on the atomic model to generate atomic trajectory data;

[0046] The process module obtains dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion from the atomic trajectory data;

[0047] The calculation module calculates the ion diffusion coefficient and reaction energy barrier based on the dynamic process parameters.

[0048] The factor module calculates the contribution weight of each ion based on the ion diffusion coefficient and the reaction energy barrier, and extracts key corrosion control factors.

[0049] The mapping module establishes an environment-material-lifetime mapping relationship based on the aforementioned key corrosion control factors;

[0050] The selection module generates a selection scheme for protective materials adapted to different corrosion levels based on the mapping relationship.

[0051] This application also provides an electronic device, including a memory and a processor, wherein the memory stores a computer program, and the processor executes the computer program to implement the method described above.

[0052] This application also provides a computer-readable storage medium having a computer program stored thereon, which, when executed in a computer, causes the computer to perform the above-described method.

[0053] The beneficial effects of this application are:

[0054] This application provides a method for adapting corrosion protection materials for metal fittings, comprising: obtaining material characteristics from the metal fittings, the material characteristics including the composition of the galvanized layer and the steel substrate; obtaining environmental parameters from the salt lake environment, the environmental parameters including the types and concentrations of chloride ions, magnesium ions, and sulfate ions; constructing an atomic model of the galvanized layer / steel substrate-electrolyte interface based on the material characteristics and the environmental parameters; performing ReaxFF reactive force field molecular dynamics simulation on the atomic model to generate atomic trajectory data; obtaining dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion from the atomic trajectory data; calculating the ion diffusion coefficient and reaction energy barrier based on the dynamic process parameters; calculating the contribution weight of each ion based on the ion diffusion coefficient and the reaction energy barrier, and extracting key corrosion control factors; establishing an environment-material-lifetime mapping relationship based on the key corrosion control factors; and generating a selection scheme for protective materials adapted to different corrosion levels based on the mapping relationship. This application reveals the corrosion mechanism of complex brine ions in salt lakes at the atomic scale and extracts key corrosion control factors, solving the problem of blind selection of protective materials due to insufficient understanding of corrosion mechanisms in existing technologies, and achieving precise matching of protective materials with the highly corrosive working conditions of salt lakes. Attached Figure Description

[0055] Figure 1 This is a schematic diagram of the process for adapting corrosion protection materials for hardware in this application;

[0056] Figure 2 This is a schematic diagram of the fitting corrosion protection material adaptation system for the hardware in this application;

[0057] Figure 3 This is a schematic diagram of the fitting corrosion protection material adapter for the hardware in this application. Detailed Implementation

[0058] Exemplary embodiments of the present disclosure will now be provided in more detail with reference to the accompanying drawings. While exemplary embodiments of the present disclosure are shown in the drawings, it is to be understood that the various forms of disclosure should not be limited to the embodiments set forth in this application. Rather, the embodiments are provided so that this disclosure will be thorough and complete, and will fully convey the scope of the disclosure to those skilled in the art.

[0059] This application provides a method for adapting corrosion protection materials for hardware, which is applied in the field of corrosion protection for power transmission lines.

[0060] This application addresses the technical challenges of unclear corrosion mechanisms and blind selection of protection systems for transmission line fittings in highly corrosive environments. The method includes:

[0061] This application achieves precise control over the entire process of transmission line fittings in highly corrosive areas, from protective design to operation and maintenance, through the coordinated operation of four modules: microscopic mechanism analysis and protective material adaptation, multi-factor aging evaluation and lifespan prediction, spatial electric field sensing and corrosion status identification, and multi-dimensional risk classification and differentiated decision-making. The corrosion mechanism and protective material adaptation module serves as the fundamental parameter source for the entire method, providing mechanistic basis and quantitative benchmarks for lifespan assessment and material selection. The spatial electric field corrosion sensing and status identification module provides real-time on-site corrosion status data for risk classification. The corrosion risk classification and operation and maintenance decision-making module is the core of the entire method, receiving multi-source data and transforming it into executable operation and maintenance instructions. The closed-loop optimization module is the mechanism that ensures continuous adaptation and iterative improvement of accuracy in complex field environments. Collaboration is achieved through data interaction at each layer.

[0062] Please refer to Figure 1 and Figure 2 As shown, the method for adapting a metal fitting corrosion protection material according to this application includes:

[0063] S101. Obtain material properties from the fittings, the material properties including the composition of the galvanized layer and the steel substrate.

[0064] First, it is necessary to clarify the material composition of the hardware to be protected.

[0065] The material properties of hardware are the intrinsic cause of its corrosion reaction, which determines the chemical nature of its interaction with the external environment.

[0066] For example, typical overhead transmission line fittings have a hot-dip galvanized layer on the surface and a steel substrate inside.

[0067] Therefore, the material properties that need to be obtained should at least include the composition of the steel base material that constitutes the main body of the hardware, as well as the chemical composition of the zinc plating layer that plays a major protective role, which is usually iron (Fe) and zinc (Zn) and their oxides.

[0068] S102. Obtain environmental parameters from the salt lake environment, including the types and concentrations of chloride ions, magnesium ions, and sulfate ions.

[0069] It is also necessary to clarify the service environment of the hardware, that is, the external corrosion driving force.

[0070] The corrosion of the interface between the zinc plating layer and the steel substrate of hardware in the highly corrosive environment of salt lake is essentially a continuous electrochemical reaction process involving competitive adsorption of multiple ions, rupture of the passivation film, anodic dissolution of the substrate, and diffusion of products, accompanied by the synergistic acceleration effect of characteristic ions of salt lake.

[0071] The process can be divided into three stages:

[0072] The first stage is the interfacial adsorption and enrichment stage. Chloride ions, sulfate ions, magnesium ions, etc. in the brine of the salt lake accumulate in the thin liquid film on the surface of the hardware under the action of alternating dry and wet conditions. They are adsorbed onto the surface of zinc oxide or zinc hydroxide passivation film by electrostatic and van der Waals forces. Among them, chloride ions have a small radius and strong penetrability, and preferentially occupy the defect sites of the passivation film. Magnesium ions enhance the ion adsorption stability by changing the interfacial hydration structure. The two produce a synergistic acceleration effect.

[0073] The second stage is the passivation film destruction stage. Adsorbed corrosive ions diffuse into the passivation film lattice, inducing zinc-oxygen bond polarization, bond length elongation until breakage. Local damage to the passivation film forms pitting corrosion initiation sources. The process is controlled by interfacial chemical reactions, and the reaction energy barrier directly determines the corrosion initiation rate.

[0074] The third stage is the substrate dissolution and diffusion stage. The zinc or iron substrate exposed at the passivation film damage site undergoes an anodic dissolution reaction. The generated metal ions diffuse towards the solution side, while corrosion products are deposited on the surface to form a secondary product layer. The ion diffusion rate and the density of the product layer together determine the corrosion propagation rate.

[0075] Salt lake environments are typically highly corrosive, and their environmental parameters are crucial in determining corrosion rates and mechanisms. The necessary environmental parameters should include at least the types and concentrations of the most representative corrosive ions in the salt lake brine, such as chloride ions (Cl). - ), magnesium ions (Mg 2+ ) and sulfate ions (SO4) 2- The types and concentrations of the aforementioned ions directly affect their adsorption, reaction, and diffusion behavior on the surface of hardware.

[0076] For example, chloride ions have a small radius and strong penetrability, making them more likely to occupy defect sites in the passivation film; magnesium ions, on the other hand, enhance the stability of ion adsorption by changing the interfacial hydration structure and produce a synergistic acceleration effect with chloride ions.

[0077] S103. Based on the material properties and environmental parameters, construct an atomic model of the zinc plating layer / steel substrate-electrolyte interface.

[0078] Please refer to Figure 2 As shown, after clarifying the hardware materials and environmental parameters, it is necessary to construct an atomic-scale model that can realistically reproduce the service conditions.

[0079] Typical brine ions from salt lakes, including chloride, magnesium, and sulfate ions, were selected and combined with the metal fitting substrate, including iron, zinc, and their oxides, to construct an atomic model of the zinc plating layer / steel substrate-electrolyte interface. In this model, ion concentration and temperature parameters can be adjusted to reproduce the service environment of the salt lake.

[0080] For example, different ion concentration gradients can be set to simulate the concentration effect of thin liquid films during alternating wet and dry processes, or different temperatures can be set to simulate the effect of diurnal temperature differences on reaction kinetics.

[0081] When constructing an atomic model of the galvanized layer / steel substrate-electrolyte interface, a wet-dry alternating cycle condition can be applied to the atomic model.

[0082] The alternating dry and wet cycle includes a dry phase and a wet phase.

[0083] During the drying stage, the number of water molecules in the atomic model is reduced and the ion mobility is decreased.

[0084] During the wetting phase, the number of water molecules and ion mobility in the atomic model are restored. This allows for a more realistic reproduction of the natural environment of alternating wet and dry conditions in the salt lake region.

[0085] S104. Perform ReaxFF reactive force field molecular dynamics simulation on the atomic model to generate atomic trajectory data.

[0086] After constructing the atomic model, advanced computational methods are needed to simulate its dynamic evolution process.

[0087] Molecular dynamics methods based on the ReaxFF reactive force field can quantitatively describe the chemical reactions in the corrosion process at the atomic scale. The core of the ReaxFF reactive force field lies in its ability to describe the breaking and formation of chemical bonds through continuous changes in bond order, thereby simulating real chemical reaction processes.

[0088] In the simulation, the total potential energy of the system is composed of bond energy, valence angle energy, torsional energy, van der Waals interaction, and Coulomb interaction, and its mathematical expression is:

[0089]

[0090] in, This represents the total potential energy of the entire molecular simulation system. For bond energy terms, For valence angle energy terms, For the torsional angular energy term, For van der Waals interaction energy, It is the Coulomb electrostatic interaction energy.

[0091] The bond order is calculated from the interatomic spacing. When the bond order is below the threshold, chemical bond breakage is determined, thereby quantitatively describing the dynamic process of bond-breaking reaction in the passivation film.

[0092] By performing ReaxFF reactive force field molecular dynamics simulations on the atomic model, the position, velocity, and force information of all atoms in the system at each moment can be obtained, i.e., atomic trajectory data.

[0093] S105. Obtain dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion from the atomic trajectory data.

[0094] The simulated atomic trajectory data contains all the microscopic information of the corrosion process, and key process parameters need to be extracted from it.

[0095] The following dynamic process parameters need to be tracked and obtained:

[0096] The first step is the ion competition adsorption process, that is, how chloride ions, magnesium ions, and sulfate ions compete for adsorption sites on the surface of the hardware;

[0097] Secondly, there is the passivation film bond breaking process, that is, how adsorbed corrosive ions induce zinc-oxygen bonds to polarize, elongate, and eventually break.

[0098] Finally, there is the diffusion process of corrosion products, that is, how metal ions generated after the matrix dissolves diffuse into the solution.

[0099] The aforementioned dynamic process parameters collectively depict the complete picture of corrosion from its inception to its development.

[0100] When obtaining the dynamic process parameters of ion competitive adsorption from the atomic trajectory data, the drying stage and the wetting stage can be distinguished based on the time markers in the atomic trajectory data. In the drying stage and the wetting stage, the occupancy rate of adsorption sites, adsorption residence time, and desorption rate of chloride ions, magnesium ions, and sulfate ions on the zinc plating layer surface are statistically analyzed.

[0101] Then, the adsorption site occupancy, adsorption residence time, and desorption rate of the drying stage and the wetting stage are compared to obtain the adsorption hysteresis effect under alternating dry and wet conditions.

[0102] S106. Calculate the ion diffusion coefficient and reaction energy barrier based on the dynamic process parameters.

[0103] After obtaining the dynamic process parameters, they need to be quantified into specific physicochemical parameters in order to evaluate the kinetic and thermodynamic properties of corrosion.

[0104] For example, the ion diffusion coefficient can be derived from atomic trajectory data using Einstein relations.

[0105] Specifically, the mean square displacement (MSD) of the ions is first calculated using the following formula:

[0106]

[0107] in, For molecular dynamics simulation time, For the first The target ions are in The spatial position vector at a given time. For the first The target ions at the initial time of the simulation Spatial position vector.

[0108] Then, the diffusion coefficient is calculated using Einstein's relation. :

[0109]

[0110] The formula establishes a quantitative mapping between the microscopic motion of ions and the macroscopic diffusion coefficient. The larger the diffusion coefficient, the stronger the ability of ions to penetrate into the interface and the higher the corrosion propagation rate.

[0111] Furthermore, the reaction energy barrier can be calculated using the Arrhenius equation.

[0112] Interfacial reaction rate constant With temperature Satisfying the Arrhenius equation:

[0113]

[0114] in, The activation energy is calculated from the energy difference of the reaction path simulated by ReaxFF. Pre-exponential factor, It is a natural constant. is the molar gas constant.

[0115] Both increased temperature and decreased activation energy lead to an exponential increase in reaction rate, mathematically demonstrating the accelerating effect of high-temperature environment and highly active ion system on corrosion.

[0116] When calculating the ion diffusion coefficient, the mean square displacement curve of each ion throughout the entire dry-wet cycle can be calculated based on the atomic trajectory data. The mean square displacement curve is divided into several segments according to the time intervals of the drying and wetting stages. Linear fitting is performed on the mean square displacement curve of each segment to obtain the drying diffusion coefficient and the wetting diffusion coefficient. Based on the time proportions of the drying and wetting stages in the total cycle, a weighted average of the drying diffusion coefficient and the wetting diffusion coefficient is performed to obtain the equivalent diffusion coefficient.

[0117] S107. Based on the ion diffusion coefficient and the reaction energy barrier, calculate the contribution weight of each ion and extract the key corrosion control factors.

[0118] After calculating the various parameters, the role of different ions in the corrosion process is quantitatively evaluated.

[0119] By statistically analyzing parameters such as mean square displacement and interaction energy, the contribution weight of different ions to the corrosion process can be clearly determined.

[0120] For example, the diffusion coefficients of chloride, magnesium, and sulfate ions can be compared, as well as the energy barriers of the reactions they each initiate, to determine which ion is the dominant factor in accelerating corrosion.

[0121] The above analysis can extract key corrosion control factors, such as the strength of the synergistic accelerating effect of magnesium and chloride ions, or whether the diffusion rate of a certain ion is a bottleneck for the corrosion rate, providing a data basis for the functional design of protective materials.

[0122] When calculating the contribution weight of each ion, the average interaction energy between the magnesium ion and the chloride ion, and the average interaction energy between the magnesium ion and the sulfate ion, can be calculated from the atomic trajectory data. The average interaction energy is then added as a correction term to the calculation of the contribution weight of each ion, so that the contribution weight of the magnesium ion is dynamically adjusted according to its cooperative adsorption strength with the chloride ion.

[0123] When extracting key corrosion control factors, the adsorption stability parameter of magnesium ions on the zinc plating surface can be extracted from the dynamic process parameters. The adsorption stability parameter includes the average residence time of magnesium ions on the zinc oxide surface, the coordination number of magnesium ions with surface hydroxyl groups, and the probability of forming ion pairs between magnesium ions and chloride ions. This adsorption stability parameter, along with the ion diffusion coefficient and the reaction barrier, is considered as a key corrosion control factor.

[0124] S108. Based on the aforementioned key corrosion control factors, establish a mapping relationship between environment, materials, and lifespan.

[0125] After extracting the key corrosion control factors, a mathematical model is established to predict the service life of materials under specific environments, aiming to construct a quantitative relationship between environmental parameters, material properties and service life.

[0126] For example, a function can be established based on simulation results. Its inputs are environmental parameters such as ambient temperature and ion concentration, as well as material parameters such as zinc plating thickness and coating type. The output is the expected lifespan of the material under the corresponding environment.

[0127] In addition to the atomic-scale mechanism based on ReaxFF simulations, a more comprehensive mapping relationship can be established through multi-factor coupled accelerated aging tests. The aging of anti-corrosion coatings under the coupled effects of ultraviolet irradiation in salt lakes, salt spray deposition, and temperature cycling is a cross-scale deterioration process involving photo-oxidative degradation, ion penetration corrosion, and thermal stress fatigue.

[0128] Photo-oxidative degradation refers to the process where ultraviolet photons with energy higher than the carbon-carbon and carbon-hydrogen bonds of the coating resin molecules trigger free radical chain reactions, generating polar groups such as carbonyl and hydroxyl groups, leading to polymer chain breakage and a decrease in crosslinking density.

[0129] Water and ions in the salt spray further accelerate the hydrolysis reaction, producing a synergistic degradation effect with ultraviolet light. The photo-oxidative degradation of the coating follows first-order reaction kinetics, with a carbonyl index... With aging time The changes satisfy:

[0130]

[0131] in, for carbonyl index at time, The initial carbonyl index, The limiting carbonyl index, The constant of the photo-oxidative degradation rate of the coating is determined by both UV intensity and temperature. This refers to the aging time.

[0132] The formula quantitatively describes the monotonic evolution of chemical structural damage over time.

[0133] Resin degradation leads to an increase in the free volume and porosity within the coating, allowing corrosive ions to penetrate along the pores to the coating / substrate interface. Thermal stress generated by temperature cycling accelerates pore expansion and interfacial delamination, forming precursors to coating blistering and peeling.

[0134] In the early stages of degradation, the porosity of the coating is... It satisfies a positive linear correlation with the carbonyl index:

[0135]

[0136] in, The current porosity of the coating. The initial porosity, This is a proportionality coefficient, determined by the intrinsic properties of the coating material. The current carbonyl index, This is the initial carbonyl index.

[0137] Increased coating porosity and interfacial delamination together lead to a decline in shielding performance, a decrease in the low-frequency modulus of the electrochemical impedance spectroscopy, and ultimately, macroscopic shielding failure. The impedance follows a negative exponential relationship with porosity; the higher the porosity, the more ion permeation pathways there are, and the lower the impedance.

[0138]

[0139] in, for The low-frequency impedance modulus of the lower coating layer The initial low-frequency impedance modulus of the new coating. The porosity influence coefficient is... This represents the porosity of the coating.

[0140] By conducting accelerated aging tests with multiple coupled factors, the performance degradation patterns of typical protection systems can be tested, and a life prediction model can be established.

[0141] A multi-factor composite cyclic test system was constructed, including strong ultraviolet irradiation, salt spray deposition, high and low temperature shock, and alternating dry and wet conditions. Accelerated aging tests were conducted on typical coatings such as epoxy zinc-rich coating, polyurethane coating, and fluorocarbon coating, as well as hot-dip galvanized steel substrates, to reproduce the multi-field synergistic aging effect of salt lake.

[0142] Fourier transform infrared spectroscopy and X-ray photoelectron spectroscopy were used to track the degradation of functional groups and changes in crosslinking density of the coating resin, and the mechanical property degradation of the hardware substrate was tested simultaneously to obtain comprehensive degradation data including chemical structure, microstructure and macroscopic properties.

[0143] A comprehensive evaluation index for aging degree is established by integrating multi-dimensional performance parameters based on the entropy weight method.

[0144] The formula for calculating the comprehensive aging evaluation index is:

[0145]

[0146] in, The comprehensive aging index is defined by the following values: arrive The larger the value, the more severe the aging. For the first The weight of each performance indicator For the first Current value of the indicator As the initial value, This is the failure threshold.

[0147] By fitting data, a mapping equation is constructed between environmental stress intensity, aging degree, and remaining service life, enabling quantitative prediction of the service life of the protection system. The remaining service life prediction formula is:

[0148]

[0149] in, To predict remaining lifespan, Designed for lifespan under standard conditions. This is the correction factor for environmental corrosion intensity.

[0150] S109. Based on the mapping relationship, generate a selection scheme for protective materials that are suitable for different corrosion levels.

[0151] Based on the established environment-material-lifetime mapping relationship, the optimal protective material selection scheme can be provided for working conditions with different corrosion levels.

[0152] For example, in one specific embodiment, based on the corrosion control factor output by ReaxFF simulation, the following selection mapping can be established:

[0153] When the contribution weight of magnesium ions is ≥0.3 and the diffusion coefficient of chloride ions is ≥1.5×10 -9 When the flow rate is m² / s, it indicates that the synergistic acceleration effect of magnesium ions and chloride ions is significant. Conventional epoxy zinc-rich coatings fail quickly, and fluorocarbon coatings with stronger resistance to ion penetration should be selected.

[0154] When the contribution weight of magnesium ions is between 0.1 and 0.3, a polyurethane coating can be used, and the thickness of the zinc plating layer can be appropriately increased to ≥85μm;

[0155] When the contribution weight of magnesium ions is less than 0.1, the epoxy zinc-rich coating can meet the protection requirements.

[0156] The above thresholds are jointly calibrated by ReaxFF simulation results and multi-factor coupled aging test data, and can be dynamically adjusted according to on-site environmental parameters.

[0157] When generating a selection scheme for protective materials adapted to different corrosion levels, the ion type with the highest contributing weight from the key corrosion control factors can be identified as the dominant ion. When the dominant ion is chloride, the selection scheme recommends an epoxy zinc-rich coating. When the dominant ion is magnesium, the selection scheme recommends a fluorocarbon coating. When the dominant ion is sulfate, the selection scheme recommends a polyurethane coating. The coating thickness and application process are adjusted according to the corrosion level.

[0158] The corrosion rate of the zinc coating simulated by ReaxFF can be compared and verified with the measured thinning rate of the zinc coating in a multi-factor coupled accelerated aging test. Under the same environmental parameters, the relative deviation between the simulated and measured values ​​is less than 20%, and the two values ​​show the same trend with a high correlation coefficient. Greater than 0.90. The verification confirms that the ReaxFF simulation method can effectively predict the corrosion behavior of hardware in a salt lake environment, providing a reliable mechanistic basis for the selection of protective materials.

[0159] The method can also work in conjunction with a space electric field corrosion sensing and state recognition module.

[0160] The spatial electric field corrosion sensing and status recognition module relies on an UAV-borne d-dot electric field sensor to collect spatial electric field signals around the hardware in a non-contact manner. Through signal preprocessing, feature extraction and intelligent recognition algorithms, it determines the type and severity of corrosion defects in the hardware and outputs quantitative results of corrosion status.

[0161] The essence of the spatial electric field distortion caused by corrosion defects in hardware is the reconstruction of the electrostatic field distribution due to changes in conductor boundary conditions and surface dielectric parameters, based on the Poisson equation for the electrostatic field. Under normal conditions, hardware is an equipotential conductor with a smooth surface, uniform plating, and a symmetrical electric field distribution with regular waveforms in the surrounding space. When corrosion occurs, the zinc plating layer thins, local pits alter the conductor's geometric boundaries, and the corrosion product layer and coating damage areas change the surface dielectric constant and conductivity distribution, leading to changes in the original electric field boundary conditions.

[0162] The electric field lines at the defect are distorted, the local electric field is enhanced, and the amplitude, waveform, and spectral characteristics of the spatial electric field change regularly accordingly. The more severe the defect, the greater the degree of distortion.

[0163] The governing equation for the electrostatic field is:

[0164]

[0165] in, For the Laplace operator, Potential, space charge density, is the dielectric constant of the medium.

[0166] The surface of the fittings is subject to the first type of boundary condition. That is, the operating voltage.

[0167] When the surface of the hardware has a depth of When corrosion defects occur, the boundary conditions are perturbed. The perturbation method can be used to derive the electric field distortion increment at a point in space under small defect conditions. With defect depth Approximately satisfies a linear positive correlation:

[0168]

[0169] in, This is the increment of electric field distortion. This is the geometric influence coefficient, which is related to the detection distance and the shape of the fitting. This represents the depth of localized corrosion defects.

[0170] This establishes a quantitative mapping basis between the degree of corrosion and the characteristic quantities of the electric field.

[0171] For signal acquisition and preprocessing, a d-dot electric field sensor is mounted on a drone to collect the spatial electric field signal around the fittings along the inspection route, and noise reduction and standardization are performed. During dynamic acquisition, the drone flies at a constant speed along a preset route, the sensor maintains a set detection distance from the fittings, and simultaneously collects the time-domain waveform of the spatial electric field and environmental parameters such as temperature and humidity, and locates and marks the position of the fittings.

[0172] The signal denoising uses a wavelet threshold denoising algorithm to suppress electromagnetic interference and motion noise. The algorithm is as follows:

[0173]

[0174] in, The original electric field signal sequence after denoising. The original input signal, and These are wavelet transform and its inverse transform, respectively. For soft thresholding function, noise threshold Determined adaptively based on noise variance.

[0175] Normalization uses Z-score standardization to eliminate the influence of sensor channel differences and flight distance fluctuations.

[0176]

[0177] in, The output signal is standardized to Z-score. The mean of the signal. This represents the standard deviation of the signal.

[0178] In terms of feature extraction and state recognition, electric field-sensitive features are extracted from multiple dimensions to train an intelligent recognition model and output the type and severity of corrosion defects.

[0179] The construction of a multi-dimensional feature pool includes four types of feature parameters.

[0180] Time-domain waveform characteristics include peak value, RMS value, kurtosis, and waveform factor.

[0181] The formula for calculating the peak value is:

[0182]

[0183] in, For the standardized space electric field signal The instantaneous values ​​at each sampling point represent, physically, the extreme values ​​of the electric field peaks caused by corrosion pits. The formula for calculating the effective value is as follows: ,in This represents the total number of sampling points for a single signal segment. For the first The signal at each sampling point has the physical meaning of the overall signal energy level, which changes monotonically as the coating thins.

[0184] The formula for calculating kurtosis is:

[0185]

[0186] in, The total number of sampling points. For the first Each sampling point signal, The average value of the electric field signal sampling in the aforementioned segment is... The standard deviation of the electric field signal sampling in the aforementioned segment has the physical meaning of waveform sharpness and sensitivity to localized corrosion.

[0187] The formula for calculating the waveform factor is:

[0188]

[0189] in, The effective value of the signal. The total number of sampling points. The sampling point signal has the physical meaning of waveform morphology characteristics, reflecting the degree of distortion.

[0190] Frequency domain characteristics include fundamental amplitude, harmonic proportion, and spectral centroid.

[0191] The formula for calculating the fundamental amplitude is:

[0192]

[0193] in, The result is the Fourier transform. Represents frequency, The corresponding frequency component amplitude has the physical meaning of the amplitude of the main component of the power frequency electric field.

[0194] The formula for calculating the harmonic ratio is:

[0195]

[0196] in, for The amplitude of a subharmonic wave is, in physical terms, a measure of waveform distortion caused by non-uniformity of the surface medium.

[0197] The formula for calculating the centroid of the spectrum is:

[0198]

[0199] The physical meaning is the degree of shift in the frequency band where energy is concentrated.

[0200] The time-frequency domain feature is the wavelet packet energy entropy, calculated using the following formula:

[0201]

[0202] in, This is the wavelet packet decomposition layer index. This refers to the sub-band node index of the layer. For the first Layer The proportion of energy of each child node to the total energy of the entire signal, the feature measure is the energy distribution complexity of the erosion state in the time-frequency plane.

[0203] The nonlinear characteristic is approximate entropy, and the calculation formula is:

[0204]

[0205] in:

[0206]

[0207] in, To embed the dimension of the pattern, reconstruct the phase space parameters. A similarity threshold is used to determine whether two pattern vectors are similar. The total length of the signal sequence. For template vector matching count, count the matches with the first... The number of vectors similar to each template This is the mean of the logarithms of the pattern matching probabilities.

[0208] The more irregular the corrosion morphology, the higher the signal complexity and the greater the approximate entropy.

[0209] Sensitive feature screening uses the mutual information method to select the feature subset that is most correlated with the corrosion state, eliminating redundant features.

[0210] The formula for calculating mutual information is:

[0211]

[0212] in, For the first Dimensional candidate electric field characteristics, For the discrete variable of corrosion state category label, The joint probability of features and labels. For feature edge probabilities, This represents the edge probability of the label.

[0213] For each candidate feature Calculate its correlation with corrosion status label Mutual information, retain Feature composition subset ,in The threshold for mutual information filtering.

[0214] The intelligent identification model constructs a corrosion state classifier based on the random forest algorithm. It takes a sensitive feature vector as input and outputs a classification result of the hardware corrosion state, including five categories: normal corrosion, uniform corrosion, localized corrosion, coating peeling, and connection defects. The Gini impurity calculation formula is:

[0215]

[0216] in, Gini impurity measures the degree of contamination in node samples. The smaller the value, the purer the node sample category. For corrosion category index, For the current node belonging to the category The percentage of samples.

[0217] The formula for calculating split gain is:

[0218]

[0219] in, For splitting gain, the decrease in Gini value before and after splitting is the algorithm's preferred choice. Split the largest feature with the threshold. The Gini value of the parent node before the split. This represents the total number of samples in the parent node. This represents the number of samples in the left child node after the split. This represents the number of samples in the right child node after the split. For the left child node Gini, Gini is the right child node.

[0220] Each split selection makes Biggest feature With threshold This forms a rule tree combining features and thresholds.

[0221] Features are cascaded layer by layer according to threshold inequalities, and the final leaf node outputs the posterior probability of the erosion category. The final prediction result is:

[0222]

[0223] in, Here is the input sample vector, and here is the filtered sensitive feature vector. This represents the total number of decision trees in the random forest. The average of all tree votes for the sample Belongs to the corrosion category The posterior probability, For the first The category of the tree output Posterior probability, Output the predicted corrosion category for the model. To make the probability The category corresponding to the maximum value .

[0224] The feature set construction and recognition model training of the space electric field corrosion sensing and state identification module use the material properties and morphological parameters of different corrosion stages obtained from the corrosion mechanism and protective material adaptation module as the calibration basis. The module outputs defect type and severity results, which are then input into the corrosion risk classification and operation and maintenance decision module as the core data source for defect severity indicators.

[0225] The corrosion risk classification and operation and maintenance decision-making module integrates four types of parameters: remaining material life, corrosion defect status, regional environmental corrosion intensity, and equipment operational importance. It constructs a multi-dimensional corrosion risk assessment index system, classifies risk levels, and generates corresponding differentiated protection and repair measures and operation and maintenance strategies. This module includes risk quantification assessment and classification decision generation.

[0226] In terms of risk quantification assessment, four primary indicators are set up: material aging degree weight 0.3, defect severity weight 0.4, environmental corrosion intensity weight 0.2, and equipment importance weight 0.1. Each primary indicator has a corresponding secondary quantitative indicator.

[0227] The weighted summation method is used to calculate the overall risk value. :

[0228]

[0229] in, This is the index subscript for the primary evaluation indicator. Indicates the degree of material aging. Indicates the severity of the defect. Indicates the intensity of environmental corrosion. Indicates the importance of the equipment. As the weight of the primary indicator, Quantify the score for the primary indicator and assign values. arrive .

[0230] according to The values ​​are divided into four levels: security level Warning level Alarm level Severity level .

[0231] In terms of tiered decision generation, differentiated protection and repair measures and operation and maintenance strategies are matched to different risk levels. At the safety level, routine periodic inspections are performed to maintain the existing protection system and record basic status data. At the early warning level, inspection cycles are shortened, the frequency of special spatial electric field testing is increased, hardware surfaces are cleaned and preventatively coated, remaining lifespan is reviewed, and medium- to long-term replacement plans are developed. At the alarm level, power outage maintenance plans are arranged, coating peeling areas are repaired, connections are tightened, the remaining zinc plating thickness is assessed, and hardware that does not meet requirements is added to the replacement list. At the critical level, live-line testing or power outage maintenance is immediately arranged, failed hardware is replaced, adjacent hardware is inspected in batches, the protection scheme for the area is optimized, and a protection system with a higher corrosion resistance level is upgraded.

[0232] The corrosion risk classification and operation and maintenance decision-making module simultaneously receives material remaining life parameters from the corrosion mechanism and protective material adaptation module, and defect status data from the spatial electric field corrosion sensing and condition identification module. These are then overlaid with regional environmental intensity and equipment importance parameters to achieve fusion and quantification. The output protection and repair plan utilizes the material selection library results from the corrosion mechanism and protective material adaptation module to ensure accurate matching of repair measures to the corrosion risk level. Operation and maintenance execution data is synchronously input into the execution feedback and closed-loop optimization module for closed-loop optimization.

[0233] The execution feedback and closed-loop optimization module is responsible for recording the decision execution results, comparing and evaluating the deviation of the repair effect, and triggering the optimization process when the deviation exceeds the limit, automatically correcting the corrosion status assessment index weights, risk classification thresholds and decision rule parameters.

[0234] The module enables the system to learn on its own. The more experience the system has in operation and maintenance, the more accurate its subsequent decisions will be, ultimately achieving the continuous evolution of corrosion grading standards and operation and maintenance strategies.

[0235] Regarding data recording, the execution status of each operation and maintenance decision is recorded, including hardware ID, corrosion risk level, decision measures, actual implementation measures, construction process parameters, post-repair retest data, personnel involved, and execution time.

[0236] In terms of effect evaluation, the retest data after repair were compared with the expected effect, and the repair effect deviation rate was calculated:

[0237] :

[0238] in, The expected corrosion score after repair. The overall corrosion score is based on the actual repair.

[0239] In terms of model optimization, when When the preset threshold is exceeded, the model optimization process is triggered. The execution feedback data, along with information such as the grading standard deviation and decision threshold deviation, are integrated into an optimized dataset. Based on this optimized dataset, data review is conducted, feeding back on field measured data to the mechanistic model, lifespan prediction model, and identification algorithm to correct model parameters, improve evaluation accuracy, and form a closed-loop management system encompassing detection, evaluation, decision-making, execution, and optimization.

[0240] Please refer to Figure 3 As shown, this application also provides a fitting adapter for corrosion protection materials for hardware, comprising:

[0241] The acquisition module 201 acquires material properties from the fittings, the material properties including the composition of the galvanized layer and the steel substrate;

[0242] Parameter module 202 obtains environmental parameters from the salt lake environment, including the types and concentrations of chloride ions, magnesium ions, and sulfate ions;

[0243] Model module 203 constructs an atomic model of the galvanized layer / steel substrate-electrolyte interface based on the material properties and environmental parameters.

[0244] Simulation module 204 performs ReaxFF reactive force field molecular dynamics simulation on the atomic model to generate atomic trajectory data;

[0245] Process module 205 obtains dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion from the atomic trajectory data;

[0246] The calculation module 206 calculates the ion diffusion coefficient and reaction energy barrier based on the dynamic process parameters.

[0247] Factor module 207 calculates the contribution weight of each ion based on the ion diffusion coefficient and the reaction energy barrier, and extracts key corrosion control factors.

[0248] The mapping module 208 establishes an environment-material-lifetime mapping relationship based on the aforementioned key corrosion control factors.

[0249] Select module 209 to generate a selection scheme for protective materials adapted to different corrosion levels based on the mapping relationship.

[0250] This application also provides an electronic device, including a memory and a processor, wherein the memory stores a computer program, and the processor executes the computer program to implement the method described above.

[0251] This application also provides a computer-readable storage medium having a computer program stored thereon, which, when executed in a computer, causes the computer to perform the above-described method.

[0252] The above embodiments are provided to enable those skilled in the art to understand and apply this application. Those skilled in the art will readily make various modifications to the above embodiments and apply the general principles described herein to other embodiments without inventive effort. Therefore, this application is not limited to the above embodiments, and any improvements and modifications made to this application based on the disclosure of this application should be within the scope of protection of this application.

Claims

1. A method for adapting corrosion-protective materials for hardware, characterized in that, include: Material properties are obtained from the fittings, including the composition of the galvanized layer and the steel substrate; Environmental parameters are obtained from the salt lake environment, including the types and concentrations of chloride ions, magnesium ions, and sulfate ions. Based on the material properties and environmental parameters, an atomic model of the zinc plating layer / steel substrate-electrolyte interface was constructed. Perform ReaxFF reactive force field molecular dynamics simulations on the atomic model to generate atomic trajectory data; Dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion are obtained from the atomic trajectory data. Calculate the ion diffusion coefficient and reaction energy barrier based on the dynamic process parameters. Based on the ion diffusion coefficient and the reaction energy barrier, the contribution weight of each ion is calculated, and the key corrosion control factors are extracted. Based on the aforementioned key corrosion control factors, an environment-material-lifetime mapping relationship is established; Based on the mapping relationship, a selection scheme for protective materials adapted to different corrosion levels is generated.

2. The method according to claim 1, characterized in that, Constructing an atomic model of the zinc plating / steel substrate-electrolyte interface, including: The atomic model is subjected to a dry-wet cycle condition, which includes a dry phase and a wet phase. During the drying stage, the number of water molecules in the atomic model is reduced and the ion mobility is decreased. During the wetting phase, the number of water molecules and ion mobility in the atomic model are restored.

3. The method according to claim 2, characterized in that, The dynamic process parameters for ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion obtained from the atomic trajectory data include: The drying stage and the wetting stage are distinguished based on the time markers in the atomic trajectory data; In the drying stage and the wetting stage, the occupancy rate of adsorption sites, adsorption residence time and desorption rate of chloride ions, magnesium ions and sulfate ions on the zinc plating layer surface are statistically analyzed respectively. By comparing the adsorption site occupancy, adsorption residence time, and desorption rate between the drying stage and the wetting stage, the adsorption hysteresis effect under alternating dry and wet conditions is obtained.

4. The method according to claim 2, characterized in that, Calculation of ion diffusion coefficient includes: Based on the atomic trajectory data, calculate the mean square displacement curve of each ion throughout the entire wet-dry cycle; The mean square displacement curve is divided into several segments according to the time intervals of the drying stage and the wetting stage. Linear fitting was performed on the mean square displacement curve of each segment to obtain the drying diffusion coefficient and the wetting diffusion coefficient. Based on the time proportions of the drying stage and the wetting stage in the total cycle, the drying diffusion coefficient and the wetting diffusion coefficient are weighted and averaged to obtain the equivalent diffusion coefficient.

5. The method according to claim 1, characterized in that, The contribution weights of each ion are statistically analyzed, including: The average interaction energy between the magnesium ion and the chloride ion, and the average interaction energy between the magnesium ion and the sulfate ion are calculated from the atomic trajectory data. The average interaction energy is added as a correction term to the calculation of the contribution weight of each ion, so that the contribution weight of the magnesium ion is dynamically adjusted according to its cooperative adsorption strength with the chloride ion.

6. The method according to claim 1, characterized in that, The extraction of key corrosion control factors includes: The adsorption stability parameters of magnesium ions on the zinc coating surface are extracted from the dynamic process parameters. The adsorption stability parameters include the average residence time of magnesium ions on the zinc oxide surface, the coordination number of magnesium ions with surface hydroxyl groups, and the probability of the formation of ion pairs between magnesium ions and chloride ions. The adsorption stability parameter, along with the ion diffusion coefficient and the reaction barrier, are considered as key corrosion control factors.

7. The method according to claim 1, characterized in that, Generate selection schemes for protective materials adapted to different corrosion levels, including: The ion type with the largest contribution weight was identified from the key corrosion control factors and determined as the dominant ion; When the dominant ion is the chloride ion, the recommended selection scheme is an epoxy zinc-rich coating; When the dominant ion is magnesium ion, the recommended selection scheme is fluorocarbon coating; When the dominant ion is the sulfate ion, the recommended selection scheme is a polyurethane coating; Adjust the coating thickness and application process according to the corrosion level.

8. A fitting adapter for corrosion protection materials in hardware, characterized in that, include: The acquisition module acquires material properties from the fittings, including the composition of the galvanized layer and the steel substrate; The parameter module obtains environmental parameters from the salt lake environment, including the types and concentrations of chloride ions, magnesium ions, and sulfate ions. The model module constructs an atomic model of the galvanized layer / steel substrate-electrolyte interface based on the material properties and environmental parameters. The simulation module performs ReaxFF reactive force field molecular dynamics simulations on the atomic model to generate atomic trajectory data; The process module obtains dynamic process parameters of ion competitive adsorption, passivation film bond breaking, and corrosion product diffusion from the atomic trajectory data; The calculation module calculates the ion diffusion coefficient and reaction energy barrier based on the dynamic process parameters. The factor module calculates the contribution weight of each ion based on the ion diffusion coefficient and the reaction energy barrier, and extracts key corrosion control factors. The mapping module establishes an environment-material-lifetime mapping relationship based on the aforementioned key corrosion control factors; The selection module generates a selection scheme for protective materials adapted to different corrosion levels based on the mapping relationship.

9. An electronic device, characterized in that, It includes a memory and a processor, wherein the memory stores a computer program, and the processor executes the computer program to implement the method as described in any one of claims 1 to 7.

10. A computer-readable storage medium, characterized in that, It stores a computer program that, when executed in a computer, causes the computer to perform the method described in any one of claims 1 to 7.