An ultra-thin glass substrate pixel hermetic isolation integrated MIP display packaging structure

By using a combination of ultra-thin glass substrate, black glue dam, and hermetic protective layer in the MIP display packaging structure, the problems of optical crosstalk and insufficient hermeticity are solved, the thickness and flatness requirements of the OOD display module are met, the reliability and display performance of the device are improved, and the substrate cost is reduced.

CN123124550APending Publication Date: 2026-11-17GUANGDONG XINHONGYU SEMICONDUCTOR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611350841.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-02
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Existing MIP display packaging structures have shortcomings in terms of optical crosstalk, hermeticity, and stress deformation control, making it difficult to meet the requirements of ultra-thinness and high flatness, especially in the application of OOD display modules, where traditional substrates are too thick and costly.

Method used

It adopts an ultra-thin glass substrate, combined with a thin-film wiring layer, flip-chip LED, black glue dam and hermetic protective layer. The black glue dam absorbs side light and blocks light crosstalk, and the hermetic protective layer prevents moisture intrusion, ensuring that the overall thickness of the packaging structure is less than 1mm and the flatness is within ±0.05mm.

Benefits of technology

It achieves low optical crosstalk, high airtightness and good stress control, ensuring the reliability and high display contrast of MIP display devices in long-term humid and hot environments, while reducing substrate costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124550A_ABST
    Figure CN123124550A_ABST
Patent Text Reader

Abstract

This invention relates to the field of Mini / Micro LED display packaging technology, and discloses an integrated MIP display packaging structure with hermetically sealed pixel isolation on an ultra-thin glass substrate. The structure includes an ultra-thin glass substrate, a thin-film wiring layer, exposed pads, flip-chip LEDs, a black adhesive barrier, and a hermetically sealed protective layer. The thin-film wiring layer and exposed pads are located on the same side of the substrate. The chips are bonded to the wiring layer, and the black adhesive barrier surrounds each chip. The hermetically sealed protective layer continuously covers the chips and the barrier while retaining exposed pads. The black adhesive barrier cuts off the lateral light path, reducing light crosstalk. Combined with the hermetically sealed protective layer, it isolates moisture and prevents the barrier from aging and delaminating. Together, these two elements enable the device to maintain low light decay and high contrast in humid and hot environments. With a specific ultra-thin substrate and a low-stress protective layer, the overall thickness of the device is controlled within 1 mm, and the flatness reaches ±0.05 mm, while avoiding substrate stress warping, meeting the application requirements of OOD ultra-thin display modules.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of Mini / Micro LED display packaging technology, specifically to an integrated MIP display packaging structure with hermetically isolated pixels on an ultra-thin glass substrate. Background Technology

[0002] Currently, MIP (Mini / Micro LED in Package) packaging typically uses sapphire or silicon substrates. However, these substrates are generally quite thick, often exceeding 1.2mm, and have high manufacturing costs, making it difficult to meet the modern trend of thinner and lower-cost display modules. To address this issue, the industry has begun exploring flip-chip fan-out packaging using glass substrates. However, existing glass substrate packaging solutions are mostly geared towards general semiconductor packaging or designed only for backlight applications, without being optimized for the specific needs of MIP display scenarios.

[0003] In MIP display applications, display scenarios place extremely stringent requirements on pixel-level optical isolation and long-term hermetic reliability. Traditional flip-chip packaging structures lack dedicated physical structures for pixel isolation, leading to easy lateral light propagation between adjacent pixels, causing severe optical crosstalk and significantly reducing display contrast. Furthermore, existing packaging structures have significant shortcomings in hermetic protection design. Under long-term humid and hot operating environments, moisture can easily penetrate the chip sides and electrode interfaces, causing electrochemical corrosion. Simply introducing light-shielding materials into conventional structures also faces the risk of decreased absorbance and interface delamination due to humid and hot aging, resulting in poor long-term device reliability.

[0004] Furthermore, in the assembly and application of next-generation OOD (Zero Optical Distance) ultra-thin display modules, extremely stringent limitations are imposed on the physical dimensions of the devices. The overall physical thickness of the devices must be controlled within 1 mm, and the surface flatness must be consistently within ±0.05 mm. Existing packaging technologies, when attempting to reduce substrate thickness, struggle to effectively control residual stress during encapsulation curing and subsequent film formation processes. This easily leads to warping and deformation of the ultra-thin substrate, making it impossible to achieve a balance between ultra-thinness, high flatness, and high processing yield.

[0005] Therefore, there is an urgent need for a packaging structure specifically designed for OOD ultra-thin MIP display modules to effectively solve the technical problems of severe optical crosstalk, poor long-term airtight reliability, and difficulty in controlling stress deformation in existing ultra-thin glass substrate packaging. Summary of the Invention

[0006] To address the shortcomings of existing technologies, this invention provides an integrated MIP display packaging structure with ultra-thin glass substrate and hermetically isolated pixels. The technical problem solved by this invention is that existing flip-chip packaging structures have not optimized for optical crosstalk in MIP displays, and insufficient hermetically tight protection leads to poor long-term reliability, making it difficult to meet the requirements of OOD display modules for an overall device thickness of less than 1mm and flatness control within ±0.05mm.

[0007] To address the above problems, the present invention provides the following technical solution: This invention provides an ultra-thin glass substrate pixel hermetically isolated integrated MIP display packaging structure, comprising: Ultra-thin glass substrate; The thin-film wiring layer and the exposed pads are both formed on the same surface of the ultrathin glass substrate. The thin-film wiring layer includes copper traces and a plurality of chip bonding pads electrically connected to the copper traces. The exposed pads are electrically connected to the thin-film wiring layer. Multiple flip-chip LEDs, each of which is electrically connected to the thin-film wiring layer via a corresponding chip bonding pad; A black vinyl barrier is provided, which surrounds each of the flip-chip LEDs. An airtight protective layer continuously covers the plurality of flip-chip LEDs and the black adhesive barrier. The airtight protective layer has uncovered opening areas, and the exposed pads are located within the opening areas. The exposed pads have electrical connection surfaces, and the electrical connection surfaces remain exposed.

[0008] Preferably, the ultrathin glass substrate is made of alkali aluminosilicate glass, and the surface roughness Ra of the ultrathin glass substrate is less than 2 nm; The thickness of the ultrathin glass substrate is 0.15 to 0.25 mm, and the coefficient of thermal expansion of the ultrathin glass substrate is 3.0 to 4.0 ppm / ℃.

[0009] Preferably, the linewidth of the copper traces in the thin-film wiring layer is no greater than 10 μm, and the line spacing of the copper traces is no greater than 10 μm.

[0010] Preferably, the plurality of flip-chip LEDs includes a red flip-chip LED, a green flip-chip LED, and a blue flip-chip LED, wherein the red flip-chip LED is made of AlGaInP material, and the green and blue flip-chip LEDs are made of InGaN material; The multiple flip-chip LEDs are respectively fixed to the corresponding chip bonding pads by AuSn eutectic bonding.

[0011] Preferably, the width of the black glue barrier is 15 to 30 μm, and the height of the black glue barrier is the same as the height of the plurality of flip-chip LEDs; The black dam uses negative carbon black photoresist, in which carbon black nanoparticles are uniformly dispersed. The verticality of the sidewall of the black dam is not less than 85 degrees, and the light absorption rate of the black dam is not less than 95%.

[0012] Preferably, the hermetic protective layer is a silicon nitride monolayer inorganic film or an aluminum oxide monolayer inorganic film deposited using a PECVD process, and the thickness of the hermetic protective layer is 1 to 2 μm.

[0013] Preferably, the airtight protective layer is an Al2O3 / SiO2 stacked structure deposited using the ALD process, and the total thickness of the Al2O3 / SiO2 stacked structure is 100 to 300 nm. The Al2O3 / SiO2 stacked structure includes multiple stacked cycles, each of which consists of a layer of Al2O3 and a layer of SiO2 deposited sequentially. The multiple stacked cycles are arranged sequentially along the thickness direction of the hermetic protective layer and continuously cover the upper surface and sides of the multiple flip-chip LEDs and the black adhesive dam.

[0014] Preferably, in each of the stacking cycles, the thickness of the single Al2O3 layer is 5 to 15 nm, and the thickness of the single SiO2 layer is 5 to 15 nm; The number of stacking cycles is 5 to 20.

[0015] Preferably, three flip-chip LEDs constitute one display pixel, and the black adhesive barrier is in the shape of a rectangular ring, used to absorb the lateral light emitted by the flip-chip LEDs and block the lateral light from propagating to adjacent display pixels to prevent optical crosstalk.

[0016] Preferably, the overall thickness of the ultra-thin glass substrate pixel hermetically isolated integrated MIP display packaging structure is less than 1 mm, and the flatness of the ultra-thin glass substrate pixel hermetically isolated integrated MIP display packaging structure is controlled within ±0.05 mm.

[0017] This invention provides an ultra-thin glass substrate pixel hermetically isolated integrated MIP display packaging structure. It has the following advantages: 1. This invention achieves physical synergy between pixel isolation and moisture protection by setting a black adhesive barrier surrounding the flip-chip LED and an airtight protective layer that continuously covers the chip and the barrier. The black adhesive barrier absorbs the light emitted laterally from the chip to cut off the light propagation path between adjacent pixels, thereby reducing light crosstalk. The airtight protective layer prevents moisture from entering the chip electrode interface while avoiding interface delamination or light absorption rate attenuation of the black adhesive barrier in a humid and hot environment. This combined structure enables the packaged device to maintain low light decay and high display contrast simultaneously under long-term humid and hot aging conditions.

[0018] 2. This invention uses an ultra-thin glass substrate with a thickness of 0.15 to 0.25 mm and a coefficient of thermal expansion of 3.0 to 4.0 ppm / ℃, combined with a flip-chip structure with eutectic bonding. This design reduces the thickness of conventional substrates while maintaining stress balance during the encapsulation and curing process. This design successfully controls the overall physical thickness of the MIP packaged device to within 1 mm, meeting the assembly limits of OOD display modules, and stabilizing the flatness of the device within ±0.05 mm, ensuring the consistency of height difference when adjacent modules are mounted and spliced.

[0019] 3. This invention addresses the processing challenges of stress deformation in ultra-thin glass substrates by limiting the hermetic protective layer to a 1-2 μm PECVD inorganic monolayer film or a 100-300 nm ALD alternating laminate film. This specific combination of film thickness and process can block the continuous penetration of water vapor and provide water vapor barrier performance, while avoiding warping of the ultra-thin substrate caused by excessive film thickness or excessive residual stress. This ensures deformation control and processing yield of the overall structure while improving the hermetic reliability of the device. Attached Figure Description

[0020] Figure 1 This is a cross-sectional schematic diagram of the ultra-thin glass substrate pixel hermetically isolated integrated MIP display packaging structure of the present invention; Figure 2 This is a schematic diagram of the fabrication process of the MIP packaged device of the present invention; Figure 3 This is a schematic diagram of the black vinyl dam planar layout and pixel isolation of the present invention; Figure 4 The diagram shows the full coverage and synergistic effect verification of the airtight protective layer of the present invention, wherein (a) is a schematic diagram of the full coverage structure of the airtight protective layer, and (b) is a verification diagram of the synergistic effect between the black rubber dam and the airtight protective layer. Figure 5The figures show a comparison of the performance of the Al2O3 / SiO2 stacked structure and the PECVD silicon nitride monolayer film, as well as the thickness, flatness, and processing yield of the ultrathin glass substrate. (a) is a performance comparison of the 200nm Al2O3 / SiO2 stacked structure and the 1.5μm PECVD silicon nitride monolayer film, and (b) is a comparison of the flatness and processing yield corresponding to different ultrathin glass substrate thicknesses.

[0021] Among them, 1. Ultra-thin glass substrate; 2. Thin film wiring layer; 21. Copper trace; 22. Chip bonding pad; 31. Red flip-chip LED chip; 32. Green flip-chip LED chip; 33. Blue flip-chip LED chip; 4. Black glue barrier; 5. Hermetic protective layer; 6. Exposed pad. Detailed Implementation

[0022] The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of the present invention, and not all embodiments. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present invention.

[0023] See attached document Figure 1 The present invention provides an integrated MIP display packaging structure with ultra-thin glass substrate pixel hermetic isolation. The structure mainly includes an ultra-thin glass substrate 1, a thin film wiring layer 2, a flip-chip LED chip, a black glue barrier 4, a hermetic protective layer 5, and exposed solder pads 6.

[0024] In this design, both the thin-film wiring layer 2 and the exposed pads 6 are formed on the same surface of the ultra-thin glass substrate 1. The thin-film wiring layer 2 includes copper traces 21 and chip bonding pads 22 electrically connected to the copper traces 21. The flip-chip LED is electrically connected to the thin-film wiring layer 2 via the chip bonding pads 22. The exposed pads 6 are electrically connected to the thin-film wiring layer 2 and are used to bring out the electrical connection terminals of the thin-film wiring layer 2. A black adhesive barrier 4 surrounds each flip-chip LED to form pixel-level optical isolation. A hermetic protective layer 5 continuously covers the flip-chip LED and the black adhesive barrier 4. The exposed pads 6 are located in the opening areas not covered by the hermetic protective layer 5, and their electrical connection surfaces remain exposed to allow the MIP (Mini / Micro LED in Package) packaged devices to be electrically connected to the external PCB driver substrate. The overall thickness of the MIP packaged device is <1mm, excluding the external PCB driving substrate. Under preferred implementation conditions, the flatness is controlled within ±0.05mm, making it suitable for 0OD (Zero Optical Distance) ultra-thin MIP display modules.

[0025] Specifically, the thickness of the ultrathin glass substrate 1 is limited to 0.1–0.3 mm, and the coefficient of thermal expansion is 3–5 ppm / ℃, preferably 3.0–4.0 ppm / ℃. In a preferred embodiment, the ultrathin glass substrate 1 is made of alkali aluminosilicate glass with a surface roughness Ra < 2 nm. Engineering tests show that the thickness of the ultrathin glass substrate 1 simultaneously affects the overall thickness of the MIP packaged device, the processing yield and flatness, as well as the warpage of the ultrathin glass substrate 1.

[0026] When the thickness of the ultrathin glass substrate 1 is 0.1 mm, the measured overall thickness of the completed MIP packaged device is approximately 0.72 mm, the flatness is approximately ±0.06 mm, the warpage is approximately 0.05 mm, and the processing yield is approximately 88%. This thickness allows the MIP packaged device to maintain a relatively small overall thickness, but the processing brittleness of the ultrathin glass substrate 1 increases significantly, and the flatness cannot be stably controlled within ±0.05 mm. Therefore, 0.1 mm is considered the lower limit of the thickness range of the ultrathin glass substrate 1 and is not regarded as the preferred thickness.

[0027] When the thickness of the ultrathin glass substrate 1 is 0.2mm, the measured overall thickness of the packaged MIP device is approximately 0.82mm, the flatness is approximately ±0.03mm, the warpage is approximately 0.02mm, and the processing yield is approximately 96%. When the thickness of the ultrathin glass substrate 1 is 0.3mm, the measured overall thickness of the packaged MIP device is approximately 0.92mm, the flatness is approximately ±0.02mm, the warpage is approximately 0.01mm, and the processing yield is approximately 98%. The processing stability is relatively high, but the overall thickness of the MIP device is close to the thickness limit of 1mm.

[0028] Considering the overall thickness, processing yield, and flatness of the MIP packaged device, the thickness of the ultra-thin glass substrate 1 is preferably 0.15–0.25 mm. In the preferred embodiment using a 0.25 mm ultra-thin glass substrate 1, the measured overall thickness of the packaged MIP device is approximately 0.85 mm, and the flatness is approximately ±0.04 mm. The above experimental results show that controlling the thickness of the ultra-thin glass substrate 1 within the preferred range of 0.15–0.25 mm achieves a good balance between the thinness of the MIP packaged device, processing yield, and flatness.

[0029] See attached document Figure 2 The thin-film wiring layer 2, formed on the same surface of the ultra-thin glass substrate 1, includes copper traces 21 and chip bonding pads 22 electrically connected to the copper traces 21. Exposed pads 6 are also formed on this surface and electrically connected to the thin-film wiring layer 2. The line width / spacing of the copper traces 21 is ≤10μm, preferably 8μm in width and 8μm in spacing.

[0030] In the fabrication of MIP packaged devices, a thin-film wiring layer 2, chip bonding pads 22, and exposed pads 6 are first formed on an ultra-thin glass substrate 1. Then, a flip-chip LED is fixed to the chip bonding pads 22 via AuSn eutectic bonding. Next, a black adhesive barrier 4 is formed around the flip-chip LED. Subsequently, a hermetic protective layer 5 is formed using PECVD (Plasma-Enhanced Chemical Vapor Deposition) or ALD (Atomic Layer Deposition) processes, ensuring that the electrical connection surfaces of the exposed pads 6 remain exposed, thus completing the MIP packaged device packaging. The deposition and patterning of the thin-film wiring layer 2, chip bonding pads 22, and exposed pads 6 can be achieved by those skilled in the art through sputtering or electroplating combined with photolithography processes. These metal deposition and patterning processes are well-known technologies in the field and will not be elaborated upon here.

[0031] The flip-chip LEDs include three colors: R, G, and B, and are fixed to the chip bonding pads 22 via eutectic bonding. Specifically, the red flip-chip LED 31 is made of AlGaInP material, while the green and blue flip-chip LEDs 32 and 33 are made of InGaN material. Each flip-chip LED has a length and width of 30–100 μm, for example, a flip-chip LED with a length of 80 μm and a width of 50 μm. Each pixel contains three flip-chip LEDs (R, G, and B). In one specific embodiment, the chip spacing between the three flip-chip LEDs (R, G, and B) within the same pixel is 120 μm. The pixel spacing of the OOD ultra-thin MIP display module is P0.4–P1.0, where P0.6 indicates a center-to-center distance of 600 μm between adjacent pixel units. The chip spacing determines the arrangement of the three flip-chip LEDs (R, G, and B) within a single pixel, and the pixel spacing determines the arrangement between adjacent pixel units.

[0032] Eutectic bonding uses an AuSn alloy, with the bonding temperature controlled between 280 and 300°C. For the AuSn eutectic bonding and alignment of flip-chip LEDs, those skilled in the art can complete the process using conventional flip-chip die bonding equipment. The temperature control and chip alignment process for AuSn eutectic bonding are well-known technologies in the field and will not be elaborated upon here. The AuSn eutectic bonding of the flip-chip LEDs is completed before the black adhesive dam 4 is formed.

[0033] See attached document Figure 3 , Figure 3Taking a 3×3 pixel array as an example, the positional relationship between the vinyl dam 4 and the flip-chip LEDs is illustrated. Each pixel includes three flip-chip LEDs: R, G, and B. The vinyl dam 4 is a rectangular ring surrounding each flip-chip LED, used to absorb the lateral light emitted from the flip-chip LEDs and block the lateral light from propagating to adjacent pixels, thus preventing optical crosstalk. The width of the vinyl dam 4 is 15–30 μm, preferably 20 μm; the height of the vinyl dam 4 is the same as the height of the flip-chip LEDs, preferably 60 μm.

[0034] The black dam 4 uses a negative carbon black photoresist with a viscosity of 500–2000 cP. After the flip-chip LED completes AuSn eutectic bonding, a negative carbon black photoresist layer is formed on the side of the ultrathin glass substrate 1 where the flip-chip LED is located. This layer is then exposed and developed using 365nm ultraviolet light to form the black dam 4. The negative carbon black photoresist uniformly disperses carbon black nanoparticles with a particle size of 15–25 nm, preferably 20 nm, and a content of 10–20 wt%, preferably 15 wt%. The coating thickness, exposure dose, and development time of the negative carbon black photoresist can be adjusted by those skilled in the art using conventional photolithography parameters to adapt the target height of the black dam 4 and the negative carbon black photoresist material system. Such photolithography parameter matching is a well-known technique in the field and will not be elaborated upon here.

[0035] Within the aforementioned material range and molding conditions, the verticality of the sidewalls of the molded black rubber dam 4 is ≥85°, and the light absorption rate is ≥95%, preferably 96%. Tests show that after setting the black rubber dam 4, the light crosstalk between adjacent pixels is reduced by more than 70%, and the contrast ratio of the 0OD ultra-thin MIP display module is increased from 2500:1 to 4500:1.

[0036] See attached document Figure 4 , Figure 4 a. Taking the red flip-chip LED 31 as an example, the full-coverage structure of the hermetic protective layer 5 is shown. Figure 4 The bar chart in section b represents the light decay of MIP packaged devices with different protection structures after aging at 85°C and 85%RH for 1000 hours, and the broken line represents the corresponding display contrast. The hermetic protective layer 5 is disposed on the outside of the flip-chip LED and the black adhesive barrier 4, continuously covering the upper surface and sides of the flip-chip LED and the black adhesive barrier 4, except for the opening area corresponding to the exposed pad 6. The hermetic protective layer 5 forms an opening in the area corresponding to the exposed pad 6, keeping the electrical connection surface of the exposed pad 6 exposed for electrical connection between the MIP packaged device and the external PCB driver substrate.

[0037] When forming the hermetic protective layer 5, a mask can be applied to the area corresponding to the exposed pads 6 before deposition, allowing the hermetic protective layer 5 to selectively cover areas other than the exposed pads 6; alternatively, the hermetic protective layer 5 can be deposited first, and then patterned mask removal can be performed on the area corresponding to the exposed pads 6, exposing the electrical connection surface of the exposed pads 6. In this invention, the hermetic protective layer 5 can be fabricated using the following two process routes: Route 1 is the PECVD airtight protective layer 5 scheme, which takes into account both airtight performance and manufacturing cost.

[0038] The hermetic protective layer 5 is formed by PECVD deposition and is a single-layer inorganic film of silicon nitride or aluminum oxide with a thickness limited to 1–2 μm. The PECVD process parameters are limited to: RF power 100–300 W, deposition temperature 150–300 °C, deposition rate 50–200 nm / min, and the refractive index of silicon nitride after film deposition is 1.9–2.1, while that of aluminum oxide is 1.6–1.7. The thickness of the hermetic protective layer 5 affects both the moisture barrier capability and the warpage of the ultrathin glass substrate 1.

[0039] The following is a comparative test of film thickness using silicon nitride hermetic protective layer 5 as an example. The water vapor transmission rate of samples with different film thicknesses was measured, and each sample was subjected to an aging test at 85℃ and 85%RH for 1000 hours: When the membrane thickness is 0.5 μm, the water vapor permeability is 0.08 g / (m²). 2 The light decay after aging is 12% (day); when the film thickness is 1μm, the water vapor permeability is 0.008g / (m²). 2 The light decay after aging is 4% (day); when the film thickness is 1.5 μm, the water vapor permeability is 0.005 g / (m²). 2 The light decay after aging is 2.8% (day); when the film thickness is 2μm, the water vapor permeability is 0.003g / (m²). 2 The light decay after aging is 2.5% when the film thickness increases to 3 μm; however, the light decay after aging is 2.3% when the film thickness increases to 3 μm, but the PECVD deposition stress increases, and the warpage of the ultrathin glass substrate 1 increases from about 0.02 mm to 0.08 mm. Here, 1 μm and 2 μm correspond to the lower and upper limits of the thickness range of the silicon nitride hermetic protective layer 5, respectively, and 0.5 μm and 3 μm are used as comparative thicknesses outside the thickness range of the silicon nitride hermetic protective layer 5.

[0040] The above results indicate that when the thickness of the silicon nitride hermetic protective layer 5 formed by the PECVD process is controlled within 1–2 μm, the water vapor permeability is less than 0.01 g / (m²). 2 (day), while no significant increase in warping was observed as seen in the 3μm comparison sample. In a preferred embodiment, the hermetic protective layer 5 is a silicon nitride film with a thickness of 1.5μm.

[0041] Route 2 is the ALD stacked airtight protective layer 5 scheme, which mainly considers reducing the thickness of the airtight protective layer 5, improving the conformal coverage of complex surfaces, and long-term airtight reliability.

[0042] See attached document Figure 5 , Figure 5 The first two performance indicators in 'a' correspond to the left vertical axis, and the last three performance indicators correspond to the right vertical axis. Figure 5 In section b, the solid line represents flatness, the dashed line represents processing yield, and the two vertical dashed lines between 0.15 and 0.25 mm represent the preferred range for the thickness of the ultra-thin glass substrate. The hermetic protective layer 5 is an Al2O3 / SiO2 stacked structure deposited by the ALD process. The thickness of a single Al2O3 layer is 5–15 nm, preferably 10 nm; the thickness of a single SiO2 layer is 5–15 nm, preferably 10 nm; and the number of stacking cycles is 5–20. Each stacking cycle consists of a sequentially deposited Al2O3 layer and a SiO2 layer, and the stacking cycles are arranged sequentially along the thickness direction of the hermetic protective layer 5, continuously covering the upper surface and sides of the flip-chip LED chip and the black adhesive dam 4.

[0043] The total thickness of the Al2O3 / SiO2 stack structure is determined by multiplying the sum of the thicknesses of the Al2O3 and SiO2 layers within a single stack cycle by the number of stack cycles. The total thickness is controlled within the range of 100–300 nm by carefully selecting the individual layer thickness and the number of stack cycles. The thickness of the individual Al2O3 layer, the thickness of the individual SiO2 layer, and the number of stack cycles must simultaneously meet the aforementioned total thickness requirement; not all values ​​within these parameter ranges can be combined. Within the parameter combinations that satisfy the total thickness requirement, the corresponding water vapor barrier performance is obtained by adjusting the individual layer thickness and the number of stack cycles.

[0044] In a preferred embodiment, the Al2O3 monolayer thickness is 10 nm, the SiO2 monolayer thickness is 10 nm, the number of stacking periods is 10, the total thickness is 200 nm, and the measured water vapor permeability is 0.003 g / (m²). 2 (day). The deposition temperature for the ALD process is set to 80–200°C, preferably 150°C. In contrast, the PECVD hermetic protective layer 5 uses a 1.5 μm thick silicon nitride monolayer film, and the deposition temperature is 250°C.

[0045] In the sidewall region of a 0.3mm × 0.3mm MIP package, the local aspect ratio is approximately 2:1. For this sidewall and step region, the ALD process utilizes self-confined surface reaction to form a conformal film layer. The sidewall film thickness uniformity of the Al2O3 / SiO2 stack structure is approximately ±3%, while the sidewall film thickness uniformity of the PECVD silicon nitride monolayer is approximately ±15%. Therefore, the Al2O3 / SiO2 stack structure can reduce the risk of localized hermetically weak areas due to insufficient step coverage in complex three-dimensional structures.

[0046] Although the total thickness of the aforementioned Al2O3 / SiO2 stacked structure is only about 200 nm, significantly smaller than the 1.5 μm thickness of a PECVD silicon nitride monolayer film, its water vapor permeability is 0.003 g / (m²). 2 (day), lower than 0.005 g / (m²) of PECVD silicon nitride monolayer films. 2 (day). The film layer formed by the ALD process has high density. After alternating Al2O3 and SiO2 layers, the microscopic defects in different film layers are staggered, making it difficult to form a continuous water vapor diffusion channel along the thickness direction of the airtight protective layer 5. At the same time, the multilayer interface blocks water vapor diffusion and prolongs the effective diffusion path of water vapor through the airtight protective layer 5. Therefore, the Al2O3 / SiO2 stacked structure can achieve a low water vapor permeability with a relatively small total thickness.

[0047] Under the deposition conditions of this embodiment, the compressive stress generated by the Al2O3 layer and the tensile stress generated by the SiO2 layer are partially offset after alternating stacking. Simultaneously, the ALD deposition temperature is lower than the comparative PECVD deposition temperature, reducing the warpage of the ultrathin glass substrate 1 from approximately 0.02 mm to approximately 0.01 mm, a reduction of approximately 50%. The interfacial adhesion strength between the Al2O3 / SiO2 stack structure and the black adhesive dam 4 is 5.2 MPa, while the interfacial adhesion strength between the PECVD silicon nitride monolayer film and the black adhesive dam 4 is 4.2 MPa, representing an improvement of approximately 24%. The conformal deposition of the ALD process improves the contact integrity between the Al2O3 / SiO2 stack structure and the surface of the black adhesive dam 4, thereby enhancing the interfacial bonding stability between the two.

[0048] After aging for 1000 hours at 85℃ and 85%RH, the MIP packaged device with the above-mentioned 200nm Al2O3 / SiO2 stacked structure has a light decay of 2.2%, while the MIP packaged device with the 1.5μm silicon nitride hermetic protective layer 5 has a light decay of 2.8%.

[0049] Further comparison of the thickness parameters of the Al2O3 / SiO2 stacked structure revealed that when the thickness of both the single-layer Al2O3 and single-layer SiO2 was 15 nm and the number of stacking periods was 20, the total thickness of the Al2O3 / SiO2 stacked structure was 600 nm, and the water vapor permeability decreased to 0.001 g / (m²). 2 (day). Although the single-layer thickness and stacking period number in this parameter combination are in the range of 5-15 nm and 5-20 periods respectively, the resulting total thickness of 600 nm exceeds the total thickness range of 100-300 nm, and therefore is used as comparative data outside the total thickness range. Although further increasing the total thickness of the Al2O3 / SiO2 stack structure can further reduce water vapor permeability, the ALD deposition time increases accordingly.

[0050] Considering the thickness of the airtight protective layer 5, water vapor barrier performance, and ALD deposition efficiency, this invention controls the total thickness of the Al2O3 / SiO2 stacked structure to be between 100 and 300 nm. The measured water vapor permeability of the 200 nm Al2O3 / SiO2 stacked structure is 0.003 g / (m²). 2 •day), and as a preferred embodiment. The PECVD airtight protective layer 5 solution can be used for applications that are more sensitive to manufacturing costs, while the ALD laminated airtight protective layer 5 solution can be used for applications that have high requirements for the thickness of the airtight protective layer 5, sidewall coverage, and long-term reliability.

[0051] Furthermore, to verify the synergistic effect of the black glue dam 4 and the airtight protective layer 5, a PECVD silicon nitride film with a thickness of 1.5μm was used as the airtight protective layer 5 in the comparative test, and MIP packaged devices with different protective structures were compared and tested.

[0052] Reference Figure 4 b. A MIP packaged device without the black glue barrier 4 and the hermetic protective layer 5 was used as the baseline sample. After aging for 1000 hours at 85°C and 85%RH, the light decay of this baseline sample was 25%; due to the absence of the black glue barrier 4, there was optical crosstalk between adjacent pixels, and its display contrast ratio was 2500:1. When the black glue barrier 4 was used alone, i.e., scheme A, the black glue barrier 4 could absorb and block the lateral light emitted between adjacent pixels, and its display contrast ratio was 4500:1; however, due to the lack of the hermetic protective layer 5, moisture could penetrate the side of the flip-chip LED and the electrode interface and cause electrochemical corrosion, while also accelerating the damp heat aging of the carbon black nanoparticles in the black glue barrier 4. After aging for 1000 hours at 85°C and 85%RH, the light decay of scheme A was 15%.

[0053] When the airtight protective layer 5 is used alone, i.e. Scheme B, the airtight protective layer 5 can reduce the degree of water vapor entering the flip-chip LED chip and electrode interface. After aging for 1000 hours at 85℃ and 85%RH, the light decay is 8%; however, since the black glue barrier 4 is not set, there is still light crosstalk between adjacent pixels, and its display contrast ratio is 2500:1.

[0054] When both the black glue barrier 4 and the airtight protective layer 5 are used, i.e., scheme C, this scheme corresponds to the combined structure of the present invention that simultaneously sets the black glue barrier 4 and the airtight protective layer 5. The black glue barrier 4 absorbs and blocks the lateral light emitted between adjacent pixels. The airtight protective layer 5 continuously covers the flip-chip, the black glue barrier 4 and its interface. On the one hand, it reduces the entry of moisture into the flip-chip and electrode interface, and on the other hand, it reduces the entry of moisture into the interface between the black glue barrier 4 and the flip-chip, thereby reducing the risk of delamination at the interface and reducing the impact of the humid and hot environment on the light absorption performance of the carbon black nanoparticles in the black glue barrier 4.

[0055] After aging for 1000 hours at 85℃ and 85%RH, scheme C exhibits light decay below 3%, maintains a contrast ratio of 4500:1, and retains a light absorption rate of over 95% for the black rubber dam 4. Scheme C, under long-term humid and hot conditions, simultaneously maintains low light decay, high contrast ratio, and the light absorption performance of the black rubber dam 4. Its test results are significantly better than those of schemes A and B when using their respective protective structures alone, indicating that the black rubber dam 4 and the airtight protective layer 5 form a synergistic protective effect.

[0056] The results above show that in MIP display applications, the black vinyl barrier 4 primarily serves to isolate light at the pixel level and prevent crosstalk, while the airtight protective layer 5 primarily serves to block moisture and heat. By protecting the black vinyl barrier 4 and its interface, it maintains long-term pixel isolation performance, thus forming a functional division of labor: the black vinyl barrier 4 mainly provides internal crosstalk prevention, and the airtight protective layer 5 mainly provides external moisture and heat protection. This structure is designed to address the characteristic of different pixel units in MIP displays requiring independent light emission.

[0057] NCSP (Near Chip Scale Package) backlight packaging primarily uses a phosphor layer to cover the flip-chip LED to form a unified white light output. It does not require independent optical isolation for different pixel units, therefore the combined structure of the black adhesive dam 4 and the hermetic protective layer 5 of this invention is not used. Compared to NCSP backlight packaging, this invention uses the black adhesive dam 4 and the hermetic protective layer 5 to respectively undertake pixel-level optical isolation and moisture and heat barrier functions, forming an integrated structure of pixel-level optical isolation and hermetic protection within the MIP package device.

[0058] In one embodiment of an OOD ultra-thin MIP display module, the MIP packaged device of the present invention is assembled with an external PCB driving substrate with a thickness of 0.4 mm, and the exposed pads 6 of the MIP packaged device are connected to the corresponding electrical connection terminals on the external PCB driving substrate. The MIP packaged device uses a 0.25 mm ultra-thin glass substrate 1 and a 1.5 μm PECVD silicon nitride hermetic protective layer 5. After encapsulation, the measured overall thickness is approximately 0.85 mm. The total thickness of the OOD ultra-thin MIP display module formed after assembly with the external PCB driving substrate is approximately 1.25 mm, meeting the requirement that the total thickness is not greater than 1.5 mm. The flatness of the MIP packaged device is approximately ±0.04 mm.

[0059] The pixel pitch of the 0OD ultra-thin MIP display module can be selected within the range of P0.4 to P1.0 according to product specifications. In an embodiment with a pixel pitch of P0.6, the center distance between adjacent pixel units is 600μm, and the brightness of the 0OD ultra-thin MIP display module can reach 1500 nits, with a color gamut of 110% NTSC. No dead pixels were observed after 1000 hours of lighting aging test. The aforementioned flatness is beneficial for controlling the height difference between adjacent modules, and the resulting 0OD ultra-thin MIP display module can be applied to automotive displays and commercial ultra-thin displays. By using the ultra-thin glass substrate 1, the substrate cost is reduced by more than 50% compared to the sapphire substrate.

[0060] Although embodiments of the invention have been shown and described, it will be understood by those skilled in the art that various changes, modifications, substitutions and alterations can be made to these embodiments without departing from the principles and spirit of the invention, the scope of which is defined by the appended claims and their equivalents.

Claims

1.An ultra-thin glass substrate pixel airtight isolation integrated MIP display packaging structure, characterized in that, include: Ultra-thin glass substrate (1); Thin film wiring layer (2) and exposed pad (6) are formed on the same surface of the ultrathin glass substrate (1). The thin film wiring layer (2) includes copper traces (21) and a plurality of chip bonding pads (22) electrically connected to the copper traces (21). The exposed pad (6) is electrically connected to the thin film wiring layer (2). Multiple flip-chip LEDs are electrically connected to the thin-film wiring layer (2) via corresponding chip bonding pads (22); Black glue barriers (4) are arranged around each of the flip-chip LEDs; An airtight protective layer (5) continuously covers the plurality of flip-chip LEDs and the black glue dam (4). The airtight protective layer (5) has uncovered opening areas. The exposed pads (6) are located in the opening areas. The exposed pads (6) have electrical connection surfaces that remain exposed. 2.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 1, wherein, The ultrathin glass substrate (1) is made of alkali aluminosilicate glass, and the surface roughness Ra of the ultrathin glass substrate (1) is less than 2 nm. The thickness of the ultrathin glass substrate (1) is 0.15 to 0.25 mm, and the coefficient of thermal expansion of the ultrathin glass substrate (1) is 3.0 to 4.0 ppm / ℃. 3.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 1, wherein, The line width of the copper trace (21) in the thin film wiring layer (2) is no greater than 10 μm, and the line spacing of the copper trace (21) is no greater than 10 μm. 4.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 1, wherein, The plurality of flip-chip LEDs include a red flip-chip LED (31), a green flip-chip LED (32) and a blue flip-chip LED (33). The red flip-chip LED (31) is made of AlGaInP material, and the green flip-chip LED (32) and the blue flip-chip LED (33) are made of InGaN material. The multiple flip-chip LEDs are respectively fixed to the corresponding chip bonding pads (22) by AuSn eutectic bonding. 5.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 1, wherein, The width of the black rubber dam (4) is 15 to 30 μm, and the height of the black rubber dam (4) is the same as the height of the plurality of flip-chip LEDs; The black dam (4) is made of negative carbon black photoresist, and carbon black nanoparticles are uniformly dispersed in the negative carbon black photoresist. The verticality of the sidewall of the black dam (4) is not less than 85 degrees, and the light absorption rate of the black dam (4) is not less than 95%. 6.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 1, wherein, The airtight protective layer (5) is a silicon nitride monolayer inorganic film or an aluminum oxide monolayer inorganic film deposited by PECVD process, and the thickness of the airtight protective layer (5) is 1 to 2 μm. 7.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 1, wherein, The airtight protective layer (5) is an Al2O3 / SiO2 stacked structure deposited by ALD process, and the total thickness of the Al2O3 / SiO2 stacked structure is 100 to 300 nm. The Al2O3 / SiO2 stacked structure includes multiple stacked cycles, each of which consists of a layer of Al2O3 and a layer of SiO2 deposited sequentially. The multiple stacked cycles are arranged sequentially along the thickness direction of the airtight protective layer (5) and continuously cover the upper surface and side surface of the multiple flip-chip LEDs and the black glue dam (4). 8.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 7, wherein, In each of the stacking cycles, the thickness of the single Al2O3 layer is 5 to 15 nm, and the thickness of the single SiO2 layer is 5 to 15 nm; The number of stacking cycles is 5 to 20. 9.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 1, wherein, Three of the multiple flip-chip LEDs constitute a display pixel. The black rubber dam (4) is in the shape of a rectangular ring and is used to absorb the side light emitted by the flip-chip LEDs and block the side light emitted from propagating to the adjacent display pixels to form optical crosstalk. 10.The ultra-thin glass substrate pixel air-tight isolation integrated MIP display package structure of claim 1, wherein, The overall thickness of the ultra-thin glass substrate pixel hermetically isolated integrated MIP display packaging structure is less than 1mm, and the flatness of the ultra-thin glass substrate pixel hermetically isolated integrated MIP display packaging structure is controlled within ±0.05mm.