Angle-sensitive quantum dot short-wave infrared photoelectric detector
By designing an angle-sensitive grating structure in the short-wave infrared photodetector, the light absorption efficiency at a specific angle and polarization direction is improved, the problem of low absorption efficiency in the existing technology is solved, and an efficient photoelectric detection effect is achieved.
Patent Information
- Application Number
- CN202323276258.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-30
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2033-11-30
AI Technical Summary
It is difficult for existing short-wave infrared photodetectors to selectively enhance the light absorption of specific wavelengths and specific polarization directions under large oblique incident angles, and their absorption efficiency is low, making it impossible to effectively improve detection sensitivity.
Design an angle-sensitive quantum dot short-wave infrared photodetector, which uses an electrode layer, a quantum dot layer and a grating structure layer connected in sequence. The grating structure layer has a continuous sub-wavelength period and includes equidistant low-refractive index substrate units and high-refractive index units. Rate filling unit, by adjusting the period, depth and filling factor of the grating structure, optimize for specific oblique incident angles, polarization directions and wavelengths to improve light absorption efficiency.
It achieves high-efficiency absorption of specific wavelength light in the SWIR band at specific angles and polarization directions, with an absorption efficiency of 96%, meeting the application needs of short-wave infrared photodetectors under special circumstances.
Smart Images

Figure CN221812096U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of photoelectric detectors, in particular to an angle-sensitive quantum dot short-wave infrared photoelectric detector. Background Art
[0002] Short-wave infrared (SWIR) (λ = 1 ~ 3μm) photoelectric detection technology has great application needs in geological exploration, biological imaging, communications, medical diagnosis and health monitoring. The key component of multi-spectral photoelectric detection is to realize dozens or even hundreds of narrow-band photodetectors covering the detection spectrum, so that multiple narrow-band spectra covering the detection spectrum can be optically responded to at the same time, greatly improving the recognition accuracy of the detected object. The working principle of the photodetector is based on the photoelectric effect. Under the action of the electric field, free electrons and holes move in the semiconductor and form a current to realize the function of detecting light signals. However, due to the limitation of the carrier diffusion length, the thickness of the quantum dot layer is mostly around 200nm. At the same time, due to the low absorption coefficient of quantum dots, such a quantum dot film layer thickness will greatly restrict the light absorption capacity of the quantum dot layer, thereby weakening the responsivity and detection rate of the photodetector. To this end, a possible strategy to overcome the low absorption capacity of quantum dot-based photodetectors is to concentrate the light energy in a quantum dot layer of limited thickness and enhance the light absorption efficiency through an optical strategy. Therefore, when selectively detecting multiple spectral bands in the SWIR region at the same time, there is still a fundamental challenge of low detection sensitivity caused by the low absorption coefficient and mobility of colloidal quantum dots. Existing methods are difficult to significantly improve the light absorption rate at large oblique incident angles and to provide a general design solution that can take into account multiple wavelengths in the SWIR band.
[0003] The existing short-wave infrared photodetectors have the following problems: they cannot selectively enhance the absorption of SWIR light of a specific wavelength and a specific polarization direction under conditions of large oblique incidence angles, and their absorption efficiency still has a lot of room for improvement. Utility Model Content
[0004] The technical problem to be solved by the utility model is to provide an angle-sensitive quantum dot short-wave infrared photoelectric detector in view of the above problems.
[0005] The utility model solves the above technical problems by adopting a technical solution: providing an angle-sensitive quantum dot short-wave infrared photoelectric detector for specific absorption at a specific oblique incident angle, a specific polarization direction, and a specific wavelength, comprising an electrode layer, a quantum dot layer, a grating structure layer, and a substrate layer connected in sequence, wherein the grating structure layer has a continuous sub-wavelength period, and the grating structure layer is composed of units arranged in a sub-wavelength period, and the units include equidistant low-refractive-index substrate units and high-refractive-index filling units;
[0006] In each sub-wavelength period, the grating period p is 500-2000nm, the depth d is 400-600nm, and the filling factor ff is 0.5-0.9; the specific oblique incident angle includes at least one of 20° to 65°, the specific polarization direction includes at least one of TE polarization direction and TM polarization direction, and the specific wavelength includes at least one of 1000nm to 2000nm.
[0007] Furthermore, it is preferred that the material of the quantum dot layer includes at least one of PbS, InP, or a perovskite material; and / or the material of the substrate layer includes at least one of a silica substrate, a silicon substrate, a silicon-based CMOS driver chip, and a TFT driver chip, the material of the low refractive index substrate unit includes at least one of a silica substrate, a silicon substrate, a silicon-based CMOS driver chip, and a TFT driver chip, the filling material of the high refractive index filling unit includes at least one of PbS, InP, or a perovskite material; and / or the material of the electrode layer includes at least one of Al, Ag, Au, and indium tin oxide.
[0008] Further, preferably, the depth d of the grating structure layer is 540.0 nm, the period p is 608.1 nm, the filling factor ff is 0.5169, and the grating structure layer is configured for specific absorption of 1310 nm TE polarization at an incident angle of 45°.
[0009] Further, preferably, the depth d of the grating structure layer is 600 nm, the period p is 1216.7 nm, the filling factor ff is 0.5332, and the grating structure layer is configured for specific absorption of 1310 nm TM polarization at an incident angle of 45°.
[0010] Further, preferably, the depth d of the grating structure layer is 531.3 nm, the period p is 1836.2 nm, the filling factor ff is 0.9, and the grating structure layer is configured for specific absorption of 1550 nm TE polarization at an incident angle of 65°.
[0011] Further, preferably, the depth d of the grating structure layer is 436.9 nm, the period p is 1976.6 nm, the filling factor ff is 0.9, and the grating structure layer is configured for specific absorption of 1550 nm TM polarization at an incident angle of 65°.
[0012] The utility model also provides a method for preparing an angle-sensitive quantum dot short-wave infrared photoelectric detector, comprising the following steps:
[0013] S1, using electron beam to etch a hard template with target grating structure parameters; using the hard template to prepare a soft template with a target grating inverse structure;
[0014] S2, nano-imprinting the soft film plate and the substrate coated with the imprinting glue on the surface, forming a grating structure on the imprinting glue, and demoulding after curing;
[0015] S3, using O2 to etch the imprinted glue on the surface of the substrate, and after the bottom of the groove is exposed, switching to SF6 to etch the substrate, etching away the imprinted glue on the surface of the substrate, and at the same time etching the target grating structure on the substrate, to obtain a substrate layer and a low-refractive-index substrate unit with a grating structure formed on the surface of the substrate layer;
[0016] S4, repeating the steps of spin coating a filling material solution of a high refractive index filling unit, exchanging ligands and cleaning in the grooves between the low refractive index substrate units to form a grating structure layer; repeating the steps of spin coating a quantum dot layer material solution, exchanging ligands and cleaning on the surface of the grating structure layer to form a quantum dot layer on the surface of the grating structure layer;
[0017] S5. An electrode layer is manufactured by evaporating or magnetron sputtering electrode materials on the surface of the quantum dot layer to obtain an angle-sensitive quantum dot short-wave infrared photodetector.
[0018] Further, preferably, in step S1, using electron beam to etch a hard template with target grating structure parameters comprises the following steps:
[0019] S10, select a silicon dioxide wafer or a silicon wafer as a substrate, wash it and set it aside;
[0020] S11, spin coating a layer of polymethyl methacrylate photoresist on the surface of the silicon dioxide substrate and drying;
[0021] S12, using electron beam etching technology to perform overlay and mosaic exposure, irradiating the electron beam onto the photoresist to form a pattern of the target grating structure;
[0022] S13, further etching using inductively coupled plasma;
[0023] S14, removing the photoresist, cleaning and drying, and preparing a hard template with target grating structure parameters;
[0024] The preparation of a soft template having a target grating anti-structure includes:
[0025] S15. Take PDMS base liquid and curing agent in proportion and mix them evenly, such as the mass ratio of PDMS base liquid to curing agent is (8-12):1, such as 8:1, 9:1, 10:1, 11:1, 12:1, etc., without specific limitation. The two are mixed evenly to obtain PDMS prepolymer liquid, which can then be put into a vacuum pump to evacuate and remove bubbles for standby use; the PDMS base liquid and curing agent selected in the utility model are both commercially available preparations, such as 184 type silicone resin elastic base liquid is used for PDMS base liquid, and 184 type silicone resin elastic curing agent is used for curing agent. The manufacturers and batch numbers of the two are Nanjing Pengpai New Material Technology Co., Ltd. and H052J4D100, respectively. Of course, the PDMS base liquid and curing agent can also use similar products with the same efficacy, which will not be repeated here.
[0026] S16, weigh VDT-731, SIT7900, M23534, stir thoroughly to obtain a mixed solution; in a specific embodiment, the input amounts of the three are 3.4g, 0.1g, and 0.1ml, respectively. After stirring, add HMS-501 in an amount of 1g, and stir thoroughly to obtain a PDMS nanoscale mixed solution; VDT-731, SIT7900, M23534, and HMS-501 selected in the utility model are all commercially available preparations, and the manufacturers and batch numbers of the four are Nanjing Pengpai New Materials Technology Co., Ltd. and PP220215-003, respectively. Of course, the above reagents can also use similar products with the same efficacy, which will not be repeated here.
[0027] S17, spin-coating the mixed solution on the surface of the hard template with the nano-grating structure, and then spin-coating the PDMS prepolymer solution, curing, and demolding to obtain a soft template with the target grating inverse structure.
[0028] Furthermore, preferably in step S4, the filling material solution of the high refractive index filling unit and the quantum dot layer material solution are the same solution, which specifically includes the following steps: filling the grooves of the grating structure on the surface of the silica gel with the quantum dot layer material solution to form a quantum dot film; then using TBAI / methanol solution to perform ligand replacement on the quantum dot film formed by the above spin coating; then using a cleaning agent to clean it; repeating the above spin coating solution, ligand exchange and cleaning until the target thickness is reached.
[0029] Further, preferably in step S1, the hard template material is selected from a silicon dioxide-based material or a silicon wafer;
[0030] In step S2, the substrate includes at least one of a silicon dioxide substrate, a silicon substrate, a silicon-based CMOS driver chip, and a TFT driver chip;
[0031] In step S4, the filling material of the high refractive index filling unit includes at least one of PbS, ZnSe, InP, CdSe or perovskite materials; the quantum dot layer material includes at least one of PbS, ZnSe, InP, CdSe or perovskite materials;
[0032] In step S5, the electrode material includes at least one of Al, Ag, Au and indium tin oxide.
[0033] The implementation of the utility model has at least the following beneficial effects: by adjusting the characteristic parameters of the grating, the utility model makes the grating period p of the grating structure be 500-2000nm, the depth d be 400-600nm, and the filling factor ff be 0.5-0.9, thereby achieving high-efficiency absorption of specific wavelength light (1000nm-2000nm) in the SWIR band in a specific polarization direction (TE polarization direction, TM polarization direction) under a specific angle (20°-65°) of oblique incidence, and the absorption efficiency is as high as 96%, meeting the application requirements of short-wave infrared photoelectric detectors in special circumstances. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0035] Figure 1 It is a three-dimensional structural schematic diagram of the angle-sensitive quantum dot short-wave infrared photoelectric detector in the utility model;
[0036] Figure 2 It is a structural schematic diagram of the grating structure layer in the utility model;
[0037] Figure 3 It is a structural side view of the quantum dot layer and the grating structure layer in the utility model;
[0038] Figure 4 This is a schematic diagram of the structure of a photoelectric detector with an equal amount of quantum dots in a planar structure used for comparison in the present invention;
[0039] Figure 5 It is a comparison diagram of the absorption spectra of the angle-sensitive quantum dot short-wave infrared photodetector in Example 1 of the present utility model and the planar device structure with an equal amount of quantum dots under 1310nm TE polarized 45° light incidence;
[0040] Figure 6This is a comparison diagram of the absorption spectra of the angle-sensitive quantum dot short-wave infrared photodetector in Example 1 of the present utility model at 1310nm TE polarization 45°, 30° and 60° light incidence;
[0041] Figure 7 It is a comparison diagram of the absorption spectra of the angle-sensitive quantum dot short-wave infrared photodetector in Example 2 of the present utility model and the planar device structure with an equal amount of quantum dots under the incidence of 1310nmTM polarized 45° light;
[0042] Figure 8 This is a comparison diagram of the absorption spectra of the angle-sensitive quantum dot short-wave infrared photodetector in Example 2 of the present utility model when incident with 1310nmTM light polarized at 45°, 30° and 60°;
[0043] Fig. 9 It is the absorption spectrum of the angle-sensitive quantum dot short-wave infrared photodetector and the equivalent quantum dot planar device structure under 1550nm TE polarization 65° light incidence in Example 3 of the present utility model;
[0044] Fig.10 It is the absorption spectrum of the angle-sensitive quantum dot short-wave infrared photodetector in Example 3 of the present utility model and the planar device structure with equal amount of quantum dots at 1550nm TE polarization 65°, 50°, 80° light incidence;
[0045] Fig.11 It is the absorption spectrum of the angle-sensitive quantum dot short-wave infrared photodetector and the equivalent quantum dot planar device structure under 1550nmTM polarized 65° light incidence in Example 4 of the present utility model;
[0046] Fig.12 It is the absorption spectrum of the angle-sensitive quantum dot short-wave infrared photodetector in Example 4 of the present utility model and the planar device structure of the equivalent quantum dot at 1550nmTM polarized 65°, 50°, 80° light incidence;
[0047] Fig.13 It is a schematic flow chart of a method for preparing an angle-sensitive quantum dot short-wave infrared photoelectric detector of the utility model;
[0048] Fig.14 It is a schematic diagram of the process of making a soft template with a target grating anti-structure in the method for preparing the angle-sensitive quantum dot short-wave infrared photoelectric detector of the utility model;
[0049] Fig.15 It is a schematic diagram of the process of etching to obtain a grating structure layer having a grating structure in the method for preparing the angle-sensitive quantum dot short-wave infrared photoelectric detector of the utility model. DETAILED DESCRIPTION
[0050] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0051] An angle-sensitive quantum dot short-wave infrared photodetector for absorption at specific oblique incident angles, specific polarization directions, and specific wavelengths, such as Figure 1-Figure 3As shown, it includes an electrode layer 3, a quantum dot layer 1, a grating structure layer 2 and a substrate layer 4 connected in sequence, and the grating structure layer 2 has a continuous sub-wavelength period, and the grating structure layer 2 is composed of units arranged according to the sub-wavelength period, and the unit includes an equidistant low-refractive index substrate unit 21 and a high-refractive index filling unit 22; in each sub-wavelength period, the grating period p is 500-2000nm, each grating period p is equal to the sum of the grating spacing and the grating width w, the depth d is 400-600nm, the filling factor ff is 0.5-0.9, and the filling factor ff=w / p; if the grating depth is controlled to be 400nm, 436.9nm, 440nm, 460nm, 480nm, 500nm, 520nm, 550nm, nm, 600nm, etc., without specific limitation; such as controlling the grating period to be 500nm, 550nm, 608.1nm, 610nm, 650nm, 700nm, 750nm, 800nm, 900nm, 1000nm, 1100nm, 1200nm, 1300nm, 1400nm, 1500nm, 1600nm, 1700nm, 1800nm, 1900nm, 1950nm, 1976.6nm and 2000nm, etc., without specific limitation; such as controlling the filling factor ff to be 0.5, 0.5169, 0.52, 0.55, 0.6, 0.65, 0.70, 0.75, 0.85, 0.88, 0.9, etc., without specific limitation. The specific oblique incident angle includes at least one of 20° to 65°, such as an incident angle of 20°, 25°, 30°, 40°, 45°, 50°, 55°, 60°, 65°, etc., without specific limitation; the specific polarization direction includes at least one of a TE polarization direction and a TM polarization direction, and the specific wavelength includes at least one of 1000 to 2000nm, such as a wavelength of 1000nm, 1100nm, 1200nm, 1300nm, 1310nm, 1330nm, 1350nm, 1380nm, 1400nm, 1430, 1450nm, 1480nm, 1500nm, 1550nm, 1600nm, 1700nm, 1800nm, 1900n, 2000nm, etc., without specific limitation. In the utility model, the geometric dimensions of the grating for a specific wavelength and a specific polarization state under a specific angle of oblique incidence are reversely designed, and the optimal geometric dimensions of the grating are found, and its characteristic parameters are d, p, and ff. The grating structure layer 2 is designed according to the characteristic parameters to achieve high-efficiency absorption of SWIR with a specific angle of oblique incidence, a specific wavelength, and a specific polarization. The light absorption spectrum confirms that the angle-sensitive quantum dot short-wave infrared photodetector designed by the utility model can improve the spectral absorption efficiency.
[0052] In some embodiments, the material of the quantum dot layer 1 includes at least one of PbS, InP or a perovskite material, and the filling material of the high refractive index filling unit 22 includes at least one of PbS, InP or a perovskite material. The material of the high refractive index filling unit 22 and the material of the quantum dot layer 1 may be the same or different. For ease of preparation, it is preferred that the materials of the two are the same. The above materials all have a high refractive index. And / or, the material of the substrate layer 4 includes at least one of a silicon dioxide substrate, a silicon substrate, a silicon-based CMOS driver chip and a TFT driver chip, and the material of the low-refractive index substrate unit 21 includes at least one of a silicon dioxide substrate, a silicon substrate, a silicon-based CMOS driver chip and a TFT driver chip. The material of the substrate layer 4 and the material of the low-refractive index substrate unit 21 may be the same or different. For the convenience of preparation, it is preferred that the materials of the two are the same. For example, the substrate layer 4 selects a silicon dioxide substrate, and etching is performed on the surface of the silicon dioxide substrate. The bottom plane area of the silicon dioxide substrate forms the substrate layer 4, and the remaining convex part of the surface etched forms the low-refractive index substrate unit 21. The above materials have the properties of semiconductor materials, and have good photoelectric properties in the visible light and infrared spectrum ranges, and are also highly sensitive to infrared light, so that the photodetector can cope with a wide spectral range, has high integration, good stability, and relatively mature manufacturing technology; the refractive index of the above materials is lower than the refractive index of the quantum dot layer 1; and / or, the material of the electrode layer 3 includes at least one of Al, Ag, Au and indium tin oxide. In the present invention, the thickness of the quantum dot layer 1, the grating structure layer 2 and the electrode layer 3 are consistent with or equal to the thickness of the quantum dot layer 1, the substrate and the electrode layer 3 of the existing short-wave infrared photodetector. In some specific embodiments, the thickness of the quantum dot layer 1 is controlled to be 90-300nm, such as 90nm, 100nm, 110nm, 120nm, 130nm, 140nm, 150nm, 160nm, 180nm, 200nm, 250nm, 290nm, 300nm, etc., without specific limitation. Figure 2 As shown, the electrode layer 3 is made of Au, the quantum dot layer 1 is made of PbS, and the grating structure layer is made of silicon dioxide.
[0053] By comparing light with different polarization directions, transverse electric field (TE) and transverse magnetic field (TM), it was found that the traditional planar device structure cannot distinguish different polarized lights. Different polarized lights and different incident angles are incident on the planar device and their absorption is basically the same. The angle-sensitive quantum dot short-wave infrared photodetector of the utility model can effectively distinguish and detect specific wavelengths (1310nm~1550nm) of SWIR band with specific polarization directions (TE polarization direction, TM polarization direction) under specific angles (45°~65°) of oblique incidence.
[0054] Example 1
[0055] An angle-sensitive quantum dot short-wave infrared photodetector, comprising an electrode layer 3, a quantum dot layer 1, a grating structure layer 2 and a substrate layer 4 connected in sequence, wherein the material of the quantum dot layer 1 is PbS, wherein the thickness of the quantum dot layer 1 is 200 nm, the low-refractive-index substrate unit 21 in the grating structure layer 2 is made of silicon dioxide, the high-refractive-index filling unit 22 is made of PbS, the substrate layer 4 is made of silicon dioxide, and the material of the electrode layer 3 is indium tin oxide; the depth d of the grating structure layer is 540.0 nm, the period p is 608.1 nm, the filling factor ff is 0.5169, and the grating structure layer is configured for specific absorption of 1310 nm TE polarization at an incident angle of 45°, and the absorption spectrum is as follows: Figure 5 As shown by the solid line, under the incident light source of the target, the total light absorption reaches 96.24% of the total incident light. Another photodetector with a planar structure made of the same amount of quantum dots is used for comparison. A more common planar structure is used, such as Figure 4 As shown, it includes an indium tin oxide electrode layer 3, a PbS quantum dot layer 1, and a silicon dioxide substrate layer 4, wherein the amount of PbS in the quantum dot layer is the same as the amount of PbS in this embodiment (the amount of PbS in the quantum dot layer is added to the amount of PbS in the high refractive index filling unit). When TE polarized light with a wavelength of 1310nm is incident at 45°, the absorption spectrum is as shown in FIG. Figure 5 As shown by the dotted line, its absorption rate is 22.31%. This control group illustrates that the dielectric grating short-wave infrared photoelectric detector of this embodiment has a significant improvement in light absorption efficiency.
[0056] For comparison, the target incident angle is adjusted from 45° to 30°. The absorption spectrum of the short-wave infrared photoelectric detector of this embodiment is as follows: Figure 6 As shown, the light absorption efficiency is 44.75%; the target incident angle is adjusted from 45° to 60°, and under the 60° oblique incident wavelength of 1310nm TE polarized light energy, the absorption spectrum is as follows Figure 6As shown, the light absorption efficiency is 29.15%. This control group illustrates that the dielectric grating short-wave infrared photodetector of this embodiment has an angle-sensitive characteristic.
[0057] In summary, when the wavelength of light is 1310nm, the light absorption efficiency of this embodiment under 45° oblique incident TE polarized light is 2.16 times that of 30° TE polarized incident light, and 3.30 times that of 60° TE polarized incident light; and it is 4.31 times that of the planar structure with an equal amount of quantum dots at a wavelength of 1310nm and 45° TE polarized incident light; comparing the absorption spectra under different conditions, the angle-sensitive quantum dot short-wave infrared photodetector of the utility model can form a narrow and long absorption line only when the incident light is 45° obliquely with a wavelength of 1310nm TE polarized light.
[0058] Example 2
[0059] An angle-sensitive quantum dot short-wave infrared photodetector comprises an electrode layer 3, a quantum dot layer 1, a grating structure layer 2 and a substrate layer 4 connected in sequence, wherein the material of the quantum dot layer 1 is PbS, wherein the thickness of the quantum dot layer 1 is 200 nm, the low-refractive-index substrate unit 21 in the grating structure layer 2 is made of silicon dioxide, the high-refractive-index filling unit 22 is made of PbS, the substrate layer 4 is made of silicon dioxide, and the material of the electrode layer 3 is indium tin oxide; the depth d of the grating structure layer is 600 nm, the period p is 1216.7 nm, the filling factor ff is 0.5332, and the grating structure layer is configured for specific absorption of 1310 nmTM polarization at an incident angle of 45°, and the absorption spectrum is as follows: Figure 7 As shown by the solid line, under the incident light source of the target, the total light absorption reaches 77.1% of the total incident light. Another photodetector with a planar structure made of the same amount of quantum dots is used for comparison. A more common planar structure is used, such as Figure 4 As shown, it includes an indium tin oxide electrode layer 3, a PbS quantum dot layer 1, and a silicon dioxide substrate layer 4, wherein the amount of PbS in the quantum dot layer is the same as that in the present embodiment (the amount of PbS in the quantum dot layer is added to the amount of PbS in the high refractive index filling unit). When TM polarized light with a wavelength of 1310 nm is incident at 45°, the absorption spectrum is as follows: Figure 7 As shown by the dotted line, the absorption rate is 22.18%. This control group illustrates that the dielectric grating short-wave infrared photoelectric detector of this embodiment has a significant improvement in light absorption efficiency.
[0060] As a comparison, the target incident angle is adjusted from 45° to 30°. The absorption spectrum of the short-wave infrared photoelectric detector of this embodiment is as follows: Figure 8As shown, the light absorption efficiency is 41.9%; as a comparison, the target incident angle is adjusted from 45° to 60°, and the short-wave infrared photoelectric detector of this embodiment is illuminated by 60° oblique incident wavelength 1310nmTM polarized light energy, and the absorption spectrum is as shown in Figure 8 As shown, the light absorption efficiency is 47.4%. This control group illustrates that the dielectric grating short-wave infrared photodetector of this embodiment has an angle-sensitive characteristic.
[0061] In summary, at a wavelength of 1310nm, the light absorption efficiency of this embodiment under 45° oblique incident TM polarized light is 1.84 times that of 30° TM polarized light, and 1.63 times that of 60° TM polarized light; and 3.48 times that of the same quantum dot planar structure under 45° TM polarized light of wavelength 1310nm. Comparing the absorption spectra under different conditions, the angle-sensitive quantum dot short-wave infrared photodetector of the utility model can only form a narrow and long absorption line under 45° oblique incident TM polarized light with a wavelength of 1310nm.
[0062] Example 3
[0063] An angle-sensitive quantum dot short-wave infrared photodetector, comprising an electrode layer 3, a quantum dot layer 1, a grating structure layer 2 and a substrate layer 4 connected in sequence, wherein the material of the quantum dot layer 1 is PbS, wherein the thickness of the quantum dot layer 1 is 200 nm, the low-refractive-index substrate unit 21 in the grating structure layer 2 is made of silicon dioxide, the high-refractive-index filling unit 22 is made of PbS, the substrate layer 4 is made of silicon dioxide, and the material of the electrode layer 3 is indium tin oxide; the depth d of the grating structure layer is 531.3 nm, the period p is 1836.2 nm, the filling factor ff is 0.9, the grating structure layer is configured for specific absorption at an incident angle of 65° and 1550 nm TE polarization, and the absorption spectrum is as follows Fig. 9 As shown by the solid line, under the incident light source of the target, the total light absorption reaches 36.87% of the total incident light. Another photodetector with a planar structure made of the same amount of quantum dots is used for comparison. A more common planar structure is used, such as Figure 4 As shown, it includes an indium tin oxide electrode layer 3, a PbS quantum dot layer 1, and a silicon dioxide substrate layer 4, wherein the amount of PbS in the quantum dot layer is the same as that in the present embodiment (the amount of PbS in the quantum dot layer is added to the amount of PbS in the high refractive index filling unit). When TE polarized light with a wavelength of 1550nm is incident at an angle of 65°, the absorption spectrum is as follows: Fig. 9 As shown by the dotted line, its absorption rate is 0.06%. This control group illustrates that the dielectric grating short-wave infrared photoelectric detector of this embodiment has a significant improvement in light absorption efficiency.
[0064] As a comparison, the target incident angle of 65° is adjusted to 50°. The absorption spectrum of the short-wave infrared photoelectric detector of this embodiment is as follows: Fig.10 As shown, the light absorption efficiency is 0.12%. The target incident angle is adjusted from 65° to 80°. The short-wave infrared photoelectric detector of this embodiment is illuminated by TE polarized light energy with an incident wavelength of 1550nm at an angle of 80°. The absorption spectrum is as shown in FIG. Fig.10 As shown, the light absorption efficiency is 0.04%. This control group illustrates that the dielectric grating short-wave infrared photodetector of this embodiment has an angle-sensitive characteristic.
[0065] In summary, at a light wavelength of 1550nm, the light absorption efficiency of this embodiment under 65° oblique incident TE polarized light is 307.25 times that of 50° TE polarized light, and 921.75 times that of 80° TE polarized light; and it is 614.5 times that of the planar structure with an equal amount of quantum dots at a wavelength of 1550nm and 65° TE polarized incident light; comparing the absorption spectra under different conditions, the angle-sensitive quantum dot short-wave infrared photodetector of the utility model can form a narrow and long absorption line only when the incident light is 65° obliquely with a wavelength of 1550nm TE polarized light.
[0066] Example 4
[0067] An angle-sensitive quantum dot short-wave infrared photodetector, comprising an electrode layer 3, a quantum dot layer 1, a grating structure layer 2 and a substrate layer 4 connected in sequence, wherein the material of the quantum dot layer 1 is PbS, wherein the thickness of the quantum dot layer 1 is 200 nm, the low-refractive-index substrate unit 21 in the grating structure layer 2 is made of silicon dioxide, the high-refractive-index filling unit 22 is made of PbS, the substrate layer 4 is made of silicon dioxide, and the material of the electrode layer 3 is indium tin oxide; the depth d of the grating structure layer is 436.9 nm, the period p is 1976.6 nm, the filling factor ff is 0.9, the grating structure layer is configured for specific absorption at an incident angle of 65° and 1550 nm TM polarization, and the absorption spectrum is as follows Fig.11 As shown by the solid line, under the incident light source, the total light absorption reaches 13.67% of the total incident light. Another photodetector with the same amount of quantum dots is made into a planar structure for comparison. A more common planar structure is used, such as Figure 4 As shown, it includes an indium tin oxide electrode layer 3, a PbS quantum dot layer 1, and a silicon dioxide substrate layer 4, wherein the amount of PbS in the quantum dot layer is the same as that of the present embodiment (the amount of PbS in the quantum dot layer is added to the amount of PbS in the high refractive index filling unit). When TM polarized light with a wavelength of 1550nm is incident at an angle of 65°, the absorption spectrum is as follows: Fig.11As shown by the dotted line, its absorption rate is 0.15%. This control group illustrates that the dielectric grating short-wave infrared photodetector of this embodiment has a significant improvement in light absorption efficiency.
[0068] As a comparison, the target incident angle of 65° is adjusted to 50°. The absorption spectrum of the short-wave infrared photoelectric detector of this embodiment is as follows when the incident light with a wavelength of 1550nmTM is irradiated at an oblique angle of 50°. Fig.12 As shown, the light absorption efficiency is 0.2%; as a comparison, the target incident angle is adjusted from 65° to 80°, and the short-wave infrared photoelectric detector of this embodiment is illuminated by 80° oblique incident wavelength 1550nmTM polarized light energy, and the absorption spectrum is as shown in Fig.12 As shown, the light absorption efficiency is 0.3%. This control group illustrates that the dielectric grating short-wave infrared photodetector of this embodiment has an angle-sensitive characteristic.
[0069] In summary, at a wavelength of 1550nm, the light absorption efficiency of this embodiment under 65° oblique incident TM polarized light is 68.35 times that of 50° TM polarized light, and 45.57 times that of 80° TM polarized light; and 91.1 times that of the same quantum dot planar structure at 1550nm 65° TM polarized light. Comparing the absorption spectra under different conditions, the angle-sensitive quantum dot short-wave infrared photodetector of the utility model can only form a narrow and long absorption line under 65° oblique incident TM polarized light with a wavelength of 1550nm.
[0070] The utility model also provides a method for preparing an angle-sensitive quantum dot short-wave infrared photoelectric detector, such as Fig.13 As shown, the following steps are included:
[0071] S1. A hard template with target grating structure parameters is etched by electron beam. A soft template with target grating anti-structure is prepared by using the hard template. Here, the target grating anti-structure refers to a structure opposite to the target grating, and the two can be snapped together.
[0072] First, electron beam etching is used to produce a template with target grating structure parameters, including the following steps: S10, select a 15×15 mm silicon dioxide wafer or silicon wafer as a substrate and clean it; S11, spin-coat a layer of polymethyl methacrylate photoresist on the surface of the silicon dioxide substrate and dry it; S12, use electron beam etching (EBL) technology to perform overlay and mosaic exposure, irradiate the electron beam onto the photoresist to form a pattern of the target grating structure; S13, perform inductively coupled plasma (ICP) etching on the sample obtained in the third step to further enhance the dimensional accuracy of the grating structure; S14, remove the photoresist by using acetone, clean with alcohol and blow dry with nitrogen to prepare a hard template with target grating structure parameters.
[0073] The preparation of a soft template having a target grating anti-structure includes the following steps: Fig.14 As shown:
[0074] S15. Take PDMS base liquid and curing agent in proportion and mix them evenly, such as the mass ratio of PDMS base liquid to curing agent is (8-12):1, such as 8:1, 9:1, 10:1, 11:1, 12:1, etc., which is not specifically limited. The two are mixed evenly to obtain PDMS prepolymer liquid, which can then be put into a vacuum pump to evacuate and remove bubbles for standby use; the PDMS base liquid and curing agent selected in the utility model are both commercially available preparations, such as 184 type silicone resin elastic base liquid is used for PDMS base liquid, and 184 type silicone resin elastic curing agent is used for curing agent, and the manufacturer batch numbers of both are H052J4D100. Of course, the PDMS base liquid and curing agent can also use similar products with the same efficacy, which will not be repeated here.
[0075] S16, weigh VDT-731, SIT7900, M23534, stir thoroughly to obtain a mixed solution; in a specific embodiment, the input amounts of the three are 3.4g, 0.1g, and 0.1ml, respectively. After stirring, add HMS-501 in an amount of 1g, and stir thoroughly to obtain a PDMS nanoscale mixed solution; VDT-731, SIT7900, M23534, and HMS-501 selected in the utility model are all commercially available preparations, and the manufacturer's batch number is PP220215-003. Of course, the above reagents can also use similar products with the same efficacy, which will not be repeated here.
[0076] S17. Clean the hard template: Rinse the hard template with anhydrous ethanol or acetone, repeat the cleaning two to three times, and then dry the side with the target grating structure upwards, such as at a drying temperature of 70°C, to ensure the cleanliness of the hard template. Spin-coat the PDMS nanoscale mixed liquid on the surface of the hard template with the nano-grating structure, and then spin-coat the PDMS prepolymer liquid; during spin coating, the rotation speed of the spin coater can use the following parameters: 1000 rpm for 30 seconds; then heat at 85°C for 20 minutes after degassing in a vacuum pump; solidify and demold to obtain a soft template with the target grating inverse structure. The preparation of the soft template allows the subsequent repeated replication of the grating structure layer.
[0077] S2. Place the soft film plate and the substrate coated with the imprint glue on the surface into the ultraviolet nanoimprint equipment for nanoimprinting. After the imprinting is completed, use ultraviolet light to perform UV curing to form a grating structure on the imprint glue, and demold after curing; wherein the substrate includes at least one of a silicon dioxide substrate, a silicon substrate, a silicon-based CMOS driver chip and a TFT driver chip.
[0078] S3, such as Fig.15As shown, O2 is used to etch the embossed glue 20 on the surface of the substrate 10. After the bottom of the groove (the surface of the substrate 10) is exposed, SF6 is switched to etch the substrate to etch away the embossed glue 20 on the surface of the substrate 10. At the same time, the target grating structure is also etched on the substrate to obtain a substrate layer 4 and a low-refractive-index substrate unit 21 having a grating structure formed on the surface of the substrate layer 4, that is, the substrate 10 is formed into two parts, the bottom plane part is defined as the substrate layer 4, and the low-refractive-index substrate unit 21 having a grating structure layer is defined as the surface of the substrate layer 4.
[0079] S4. Repeat the steps of spin coating the filling material solution of the high refractive index filling unit, ligand exchange and cleaning in the grooves between adjacent low refractive index substrate units, so that the high refractive index material filled in all the grooves forms a high refractive index filling unit. The high refractive index filling unit and the low refractive index substrate unit together form a grating structure layer. The surface of the substrate layer 4 to the top surface of the substrate is defined as the grating structure layer; repeat the steps of spin coating the quantum dot layer material solution, ligand exchange and cleaning on the surface of the grating structure layer to form a quantum dot layer on the surface of the grating structure layer.
[0080] Among them, spin coating material solution, ligand exchange and cleaning are performed as one operation. In order to obtain a quantum dot layer of the desired thickness, the utility model is operated by repeating the above steps. The filling material solution of the high refractive index filling unit and the quantum dot layer material solution are the same solution, specifically including the following steps: filling the quantum dot layer material solution in the grooves of the grating structure on the surface of the silica gel to form a quantum dot film; then using TBAI / methanol solution to perform ligand replacement on the quantum dot film formed by the above spin coating; then using a cleaning agent to clean; repeating the above spin coating solution, ligand exchange and cleaning until the target thickness is reached. Among them, the filling material of the high refractive index filling unit includes at least one of PbS, InP, or perovskite materials; the quantum dot layer material includes at least one of PbS, InP, or perovskite materials;
[0081] In a specific embodiment, taking PbS quantum dots as the filling material of the quantum dot layer and the high refractive index filling unit as an example, the spin coating solution is prepared by dissolving the PbS quantum dot material in an n-octane solution at a concentration of 50 mG / mL. The solution is first filled in the grooves of the grating structure on the silica gel surface, and then the ligand exchange process uses TBAI / methanol solution to replace the ligands of the quantum dot film formed by the above spin coating. Since the I- ions in the TBAI / methanol solution have a stronger binding energy with the PbS quantum dots, the original long-chain OA- ligands outside the PbS quantum dot material will be replaced, resulting in a decrease in the quantum dot spacing and a tighter stacking, which is beneficial to charge transfer and carrier extraction; then a cleaning agent, such as methanol, is used for cleaning; after the quantum dot film is allowed to stand and stabilize, the above spin coating solution, ligand exchange and cleaning steps are repeated; preferably, it is repeated 5-10 times to achieve the target thickness to form a grating structure layer and a quantum dot layer.
[0082] Furthermore, the cleaning agent used for cleaning is a ligand solvent, such as TBAI / methanol solution.
[0083] S5. On the surface of the quantum dot layer, an electrode material is deposited or magnetron sputtered, wherein the electrode material includes at least one of Al, Ag, Au and indium tin oxide to produce an electrode layer to obtain an angle-sensitive quantum dot short-wave infrared photodetector.
[0084] Of course, the angle-sensitive quantum dot short-wave infrared photoelectric detector of the present invention can also be prepared by other conventional preparation methods.
[0085] The utility model adjusts the characteristic parameters of the grating so that the grating period p of the grating structure is 608.1-1976.6nm, the depth d is 436.9-600nm, and the filling factor ff is 0.5169-0.9, thereby achieving high-efficiency absorption of specific wavelength light (1310nm-1550nm) in the SWIR band in a specific polarization direction (TE polarization direction, TM polarization direction) under a specific angle (45°-65°) of oblique incidence, with an absorption efficiency of up to 96%, thereby meeting the application requirements of short-wave infrared photoelectric detectors in special circumstances.
[0086] The above disclosure is only a preferred embodiment of the present invention, and certainly cannot be used to limit the scope of rights of the present invention. Ordinary technicians in this field can understand that all or part of the processes of the above embodiment and equivalent changes made according to the claims of the present invention still fall within the scope covered by the utility model.
Claims
1. An angle-sensitive quantum dot short-wave infrared photodetector, used for obtaining maximum light absorption efficiency at a specific oblique incident angle, a specific polarization direction, and a specific wavelength, characterized in that: It comprises an electrode layer, a quantum dot layer, a grating structure layer and a substrate layer connected in sequence, wherein the grating structure layer has a continuous sub-wavelength period, and the grating structure layer is composed of units arranged in a sub-wavelength period, and the units include equidistant low-refractive-index substrate units and high-refractive-index filling units; In each sub-wavelength period, the grating period p is 500~2000nm, the depth d is 400~600nm, and the filling factor ff is 0.5~0.9; The specific oblique incident angle includes at least one of 20°~65°, the specific polarization direction includes at least one of TE polarization direction and TM polarization direction, and the specific wavelength includes at least one of 1000 nm~2000 nm.
2. The angle-sensitive quantum dot short-wave infrared photodetector according to claim 1, characterized in that: The depth d of the grating structure layer is 540.0 nm, the period p is 608.1 nm, the filling factor ff is 0.5169, and the grating structure layer is configured for specific absorption of 1310 nm TE polarization at an incident angle of 45°.
3. The angle-sensitive quantum dot short-wave infrared photodetector according to claim 1, characterized in that: The depth d of the grating structure layer is 600 nm, the period p is 1216.7 nm, the filling factor ff is 0.5332, and the grating structure layer is configured for specific absorption of 1310 nm TM polarization at an incident angle of 45°.
4. The angle-sensitive quantum dot short-wave infrared photodetector according to claim 1, characterized in that: The depth d of the grating structure layer is 531.3 nm, the period p is 1836.2 nm, the filling factor ff is 0.9, and the grating structure layer is configured for specific absorption of 1550 nm TE polarization at an incident angle of 65°.
5. The angle-sensitive quantum dot short-wave infrared photodetector according to claim 1, characterized in that: The depth d of the grating structure layer is 436.9 nm, the period p is 1976.6 nm, the filling factor ff is 0.9, and the grating structure layer is configured for specific absorption of 1550 nm TM polarization at an incident angle of 65°.
6. The angle-sensitive quantum dot short-wave infrared photodetector according to claim 1, characterized in that: The substrate layer includes at least one of a silicon dioxide substrate, a silicon substrate, a silicon-based CMOS driver chip and a TFT driver chip.
7. The angle-sensitive quantum dot short-wave infrared photodetector according to claim 1, characterized in that: The low refractive index substrate unit includes at least one of a silicon dioxide substrate, a silicon substrate, a silicon-based CMOS driver chip and a TFT driver chip.