Two-step injection blow mold for plastic water cup
Through the two-step injection blow molding of the plastic water cup, the volume of the preliminary and secondary molding parts is gradually increased, which solves the problems of molding error and uneven hot melt in the existing technology, and improves the outer surface quality and molding accuracy of the plastic water cup.
Patent Information
- Application Number
- CN202420256483.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-02
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2034-02-02
AI Technical Summary
Existing injection stretch-blow molds for plastic water cups are prone to molding errors during the production process and are difficult to adjust. They can easily cause bubbles and cracks during thermal melting, affecting the quality of the outer surface.
The two-step injection blow molding method of the plastic water cup is adopted, including the preliminary injection blow molding and the secondary injection blow molding. The volume of the preliminary molding part and the secondary molding part gradually increases. Through the preliminary and secondary blow molding, the volume of the plastic water cup is ensured to be fine-tuned. and exterior wall surface quality.
It effectively avoids bubbles and cracks caused by uneven hot melt, and improves the outer surface quality and molding accuracy of the plastic water cup.
Smart Images

Figure CN221851022U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of molds and relates to a two-step injection-blow mold for a plastic water cup. Background Art
[0002] Existing general blow molding of large plastic containers adopts extrusion blow molding and injection blow molding, and its equipment cost is high, productivity is low, and there are many scraps. The two-step injection, stretch and blow molding method can concentrate on producing bottle blanks and then make large containers, so the equipment is simple, productivity is high, and cost is low. However, in the actual production process of the existing injection, stretch and blow mold for plastic water cups, since a single mold is used to complete the injection, stretch and blow process, the volume of the molded plastic part is prone to errors, and it is difficult to adjust it in the mold after the error occurs. If the molded plastic part is melted again, it is easy to cause bubbles and cracks, and the quality of the outer surface of the plastic part is difficult to guarantee. Therefore, it is urgent to design a two-step injection blow mold for plastic water cups that can overcome the above defects.
[0003] In order to overcome the shortcomings of the prior art, people have proposed various solutions through continuous exploration. For example, a Chinese patent discloses a blow molding mold for blowing plastic hollow containers [application number: 201210470787.9], which includes a side mold, a bottom mold and a guide rod of the bottom mold assembly. The side mold includes a left mold and a right mold, wherein a plurality of exhaust holes for exhausting air to the outside and forming a local vacuum in the mold cavity are provided at the symmetry line of the mold cavity of the two side molds. Utility Model Content
[0004] The utility model aims to solve the above problems and provides a two-step injection blow mold for a plastic water cup.
[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0006] A two-step injection blow mold for a plastic water cup comprises a primary injection blow mold and a secondary injection blow mold, wherein the primary injection blow mold comprises a primary molding left mold body and a primary molding right mold body, a primary molding portion is formed between the primary molding left mold body and the primary molding right mold body, and the secondary injection blow mold comprises a secondary molding left mold body and a secondary molding right mold body, a secondary molding portion is formed between the secondary molding left mold body and the secondary molding right mold body, and the volume of the secondary molding portion is greater than that of the primary molding portion.
[0007] In the above-mentioned two-step injection blow mold for plastic water cups, the preliminary molding part includes a preliminary molding chamber located between a left preliminary molding mold body and a right preliminary molding mold body, and a preliminary injection port is connected to the top of the preliminary molding chamber.
[0008] In the above-mentioned two-step injection blow mold for plastic water cups, a water cup bottom preliminary molding piece is provided at the bottom between the preliminary molding left mold body and the preliminary molding right mold body, and the water cup bottom preliminary molding piece abuts against the preliminary molding left mold body and the preliminary molding right mold body.
[0009] In the above-mentioned two-step injection blow mold for plastic water cups, the bottom preliminary molded part of the water cup includes a bottom preliminary molded ring seat arranged at the bottom between the left preliminary mold body and the right preliminary mold body, and the bottom preliminary molded ring seat is sleeved with a first sealing sleeve.
[0010] In the above-mentioned two-step injection blow mold for plastic water cups, the secondary molding part includes a secondary molding chamber arranged between a secondary molding left mold body and a secondary molding right mold body, and a secondary injection port is connected to the top of the secondary molding chamber.
[0011] In the above-mentioned two-step injection blow mold for plastic water cups, a water cup bottom secondary molded piece is provided at the bottom between the secondary molded left mold body and the secondary molded right mold body, and the water cup bottom secondary molded piece abuts against the secondary molded left mold body and the secondary molded right mold body.
[0012] In the above-mentioned two-step injection blow mold for plastic water cups, the bottom secondary molded part of the water cup includes a bottom secondary molded ring seat arranged at the bottom between the left secondary molded mold body and the right secondary molded mold body, and a second sealing sleeve is sleeved on the bottom secondary molded ring seat.
[0013] In the above-mentioned two-step injection blow mold for plastic water cups, the volume of the primary molding chamber is smaller than the volume of the secondary molding chamber, the height of the primary injection port is the same as the height of the secondary injection port, and the inner diameter of the primary injection port is smaller than the inner diameter of the secondary injection port.
[0014] In the above-mentioned two-step injection blow mold for the plastic water cup, the height of the bottom primary molding ring seat is smaller than the height of the bottom secondary molding ring seat, and the outer diameter of the bottom primary molding ring seat is smaller than the outer diameter of the bottom secondary molding ring seat.
[0015] In the above-mentioned two-step injection blow mold for plastic water cups, the outer diameter of the first sealing sleeve is smaller than the outer diameter of the second sealing sleeve.
[0016] Compared with the existing technology, the advantages of the utility model are:
[0017] In the blow molding process of the utility model, the primary molding left mold body and the primary molding right mold body are first closely matched, and the molten material is injected from the injection port of the primary injection blow mold. The primary molding part is used for primary molding, and the material is preliminarily blow-molded by cooperating with the blow molding machine to form a primary embryo. After the primary blow molding, the primary embryo is taken out and placed between the secondary molding left mold body and the secondary molding right mold body. At this time, the secondary molding left mold body and the secondary molding right mold body are closely matched so that the primary embryo is located in the secondary molding part, and the primary embryo is subjected to secondary blow molding. The volume of the secondary molding part is larger than that of the primary molding part. In the secondary blow molding process, the volume of the plastic water cup can be finely adjusted and increased. The two-step injection blowing method is adopted to avoid bubbles and cracks on the outer wall of the plastic water cup due to multiple non-uniform hot melting, thereby greatly improving the outer surface quality of the plastic water cup.
[0018] Other advantages, objectives and features of the present invention will be embodied in part through the following description, and in part will be understood by those skilled in the art through research and practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a schematic diagram of the structure of the preliminary injection blow mold.
[0020] Figure 2 It is a schematic diagram of the structure of the initial forming right mold.
[0021] Figure 3 It is a schematic cross-sectional view of the preliminary injection blow mold.
[0022] Figure 4 It is a structural schematic diagram of a secondary injection blow mold.
[0023] Figure 5 It is a schematic diagram of the structure of the left secondary molding mold.
[0024] Figure 6 It is a cross-sectional schematic diagram of a secondary injection blow mold.
[0025] In the figure: preliminary injection blow mold 1, secondary injection blow mold 2, preliminary molding left mold body 3, preliminary molding right mold body 4, preliminary molding part 5, secondary molding left mold body 6, secondary molding right mold body 7, secondary molding part 8, preliminary molding chamber 9, preliminary injection port 10, preliminary molding part 11 of water cup bottom, preliminary molding ring seat 12 of bottom, first sealing sleeve 13, secondary molding chamber 14, secondary injection port 15, secondary molding part 16 of water cup bottom, secondary molding ring seat 17 of bottom, second sealing sleeve 18. DETAILED DESCRIPTION
[0026] The utility model is further described below in conjunction with the accompanying drawings.
[0027] like Figure 1-6As shown, a two-step injection blow mold for a plastic water cup includes a primary injection blow mold 1 and a secondary injection blow mold 2, wherein the primary injection blow mold 1 includes a primary molding left mold body 3 and a primary molding right mold body 4, and a primary molding portion 5 is formed between the primary molding left mold body 3 and the primary molding right mold body 4, and the secondary injection blow mold 2 includes a secondary molding left mold body 6 and a secondary molding right mold body 7, and a secondary molding portion 8 is formed between the secondary molding left mold body 6 and the secondary molding right mold body 7, and the volume of the secondary molding portion 8 is greater than the volume of the primary molding portion 5.
[0028] In this embodiment, during the blow molding process, the primary molding left mold body 3 and the primary molding right mold body 4 are first closely matched, and the molten material is injected from the injection port of the primary injection blow mold 1. The primary molding part 5 is used for preliminary molding, and the material is preliminarily blow-molded by cooperating with the blow molding machine to form a primary embryo. After the preliminary blow molding, the primary embryo is taken out and placed between the secondary molding left mold body 6 and the secondary molding right mold body 7. At this time, the secondary molding left mold body 6 and the secondary molding right mold body 7 are closely matched so that the primary embryo is located in the secondary molding part 8, and the primary embryo is subjected to secondary blow molding. The volume of the secondary molding part 8 is larger than that of the primary molding part 5. During the secondary blow molding process, the volume of the plastic water cup can be fine-tuned and increased. The two-step injection blowing method is adopted to avoid bubbles and cracks on the outer wall of the plastic water cup due to multiple uneven hot melts, thereby greatly improving the outer surface quality of the plastic water cup.
[0029] Combination Figure 1-3 As shown, the preliminary molding part 5 includes a preliminary molding chamber 9 located between a preliminary molding left mold body 3 and a preliminary molding right mold body 4 , and a preliminary injection port 10 is connected to the top of the preliminary molding chamber 9 .
[0030] Specifically, during the primary blow molding process, the molten material is injected into the primary molding chamber 9 through the primary injection port 10, and the primary blow molding is performed in cooperation with the blow molding machine to form a primary embryo.
[0031] A water cup bottom preliminary forming piece 11 is provided at the bottom between the preliminary forming left mold body 3 and the preliminary forming right mold body 4 , and the water cup bottom preliminary forming piece 11 abuts against the preliminary forming left mold body 3 and the preliminary forming right mold body 4 .
[0032] In this embodiment, the preliminary molded part 11 of the bottom of the water cup is used to assist in molding the bottom structure of the preliminary blank during the preliminary blow molding process.
[0033] Combination Figure 1-3 As shown, the preliminary molding part 11 of the bottom of the water cup includes a preliminary molding ring seat 12 arranged at the bottom between the preliminary molding left mold body 3 and the preliminary molding right mold body 4, and a first sealing sleeve 13 is sleeved on the bottom preliminary molding ring seat 12.
[0034] In this embodiment, the bottom preliminary molding ring seat 12 is used to assist in molding the bottom structure of the preform during the preliminary blow molding process, and the first sealing sleeve 13 is sleeved on the bottom preliminary molding ring seat 12 to achieve the purpose of sealing and leak-proofing.
[0035] Combination Figure 3-6 As shown, the secondary molding part 8 includes a secondary molding chamber 14 disposed between the secondary molding left mold body 6 and the secondary molding right mold body 7 , and a secondary injection port 15 is connected to the top of the secondary molding chamber 14 .
[0036] In this embodiment, during the secondary blow molding process, the molded embryo is placed in the secondary molding chamber 14, and the secondary blow molding is performed by the blow molding machine in conjunction with the secondary injection port 15. The volume of the secondary molding chamber 14 is larger than the volume of the primary molding chamber 9. During the secondary blow molding process, the volume of the plastic water cup can be fine-tuned and increased. The two-step injection blowing method is adopted to avoid bubbles and cracks on the outer wall of the plastic water cup caused by multiple uneven hot melts, thereby greatly improving the outer surface quality of the plastic water cup.
[0037] Combination Figure 3-6 As shown, a water cup bottom secondary molding piece 16 is provided at the bottom between the secondary molding left mold body 6 and the secondary molding right mold body 7 , and the water cup bottom secondary molding piece 16 abuts against the secondary molding left mold body 6 and the secondary molding right mold body 7 .
[0038] In this embodiment, the secondary molded part 16 of the bottom of the water cup is used to assist in molding the bottom structure of the plastic part during the secondary blow molding process.
[0039] The water cup bottom secondary molding part 16 comprises a bottom secondary molding ring seat 17 arranged at the bottom between the secondary molding left mold body 6 and the secondary molding right mold body 7 , and a second sealing sleeve 18 is sleeved on the bottom secondary molding ring seat 17 .
[0040] In this embodiment, the bottom secondary molding ring seat 17 is used to assist in the bottom structure of the molded plastic part during the secondary blow molding process, and finally determines the shape and size of the bottom structure of the molded plastic part. The second sealing sleeve 18 is sleeved on the bottom secondary molding ring seat 17 to achieve the purpose of sealing and leak prevention.
[0041] Combination Figure 1-6 As shown, the volume of the primary molding chamber 9 is smaller than the volume of the secondary molding chamber 14 , the height of the primary injection port 10 is the same as the height of the secondary injection port 15 , and the inner diameter of the primary injection port 10 is smaller than the inner diameter of the secondary injection port 15 .
[0042] In this embodiment, the volume of the primary molding chamber 9 is smaller than the volume of the secondary molding chamber 14, and the inner diameter of the primary injection port 10 is smaller than the inner diameter of the secondary injection port 15. During the secondary blow molding process, the volume of the plastic water cup can be fine-tuned and increased. The two-step injection blowing method is adopted to avoid bubbles and cracks on the outer wall of the plastic water cup caused by multiple uneven hot melts, thereby greatly improving the outer surface quality of the plastic water cup.
[0043] Combination Figure 1-6 As shown, the height of the bottom primary molding ring seat 12 is smaller than the height of the bottom secondary molding ring seat 17 , and the outer diameter of the bottom primary molding ring seat 12 is smaller than the outer diameter of the bottom secondary molding ring seat 17 .
[0044] In this embodiment, the height of the bottom preliminary molding ring seat 12 is smaller than the height of the bottom secondary molding ring seat 17, and the outer diameter of the bottom preliminary molding ring seat 12 is smaller than the outer diameter of the bottom secondary molding ring seat 17. During the secondary blow molding process, the bottom structure of the plastic water cup can be fine-tuned and increased to ensure the accuracy of the molding of the bottom structure of the plastic part.
[0045] Combination Figure 1-6 As shown, the outer diameter of the first sealing sleeve 13 is smaller than the outer diameter of the second sealing sleeve 18 .
[0046] In this embodiment, the outer diameter of the first sealing ferrule 13 is smaller than the outer diameter of the second sealing ferrule 18 , so as to be able to sleeve the bottom primary molding ring seat 12 and the bottom secondary molding ring seat 17 of different widths.
[0047] The working principle of the utility model is:
[0048] During the blow molding process, the primary left mold body 3 and the primary right mold body 4 are first closely matched. During the primary blow molding process, the molten material is injected into the primary molding chamber 9 through the primary injection port 10, and the blow molding machine is used for primary blow molding to form a primary embryo. During the secondary blow molding process, the molded primary embryo is placed in the secondary molding chamber 14, and the blow molding machine is used for secondary blow molding with the secondary injection port 15. The volume of the secondary molding chamber 14 is larger than the volume of the primary molding chamber 9. During the secondary blow molding process, the volume of the plastic water cup can be fine-tuned and increased. The two-step injection blowing method is used to avoid bubbles and cracks on the outer wall of the plastic water cup due to multiple uneven hot melts, thereby greatly improving the outer surface quality of the plastic water cup.
[0049] The height of the preliminary molding chamber 9 is 224.5mm, the height of the bottom preliminary molding ring seat 12 is 47mm, the outer diameter of the bottom preliminary molding ring seat 12 is 69.7mm, the outer diameter of the first sealing sleeve 13 is 83.7mm, the diameter of the preliminary injection port 10 is 81.5mm, the height of the secondary molding chamber 14 is 246.4mm, the outer diameter of the bottom secondary molding ring seat 17 is 73.6mm, the height is 48.1mm, and the outer diameter of the second sealing sleeve 18 is 87.6mm.
[0050] The specific embodiments described herein are merely examples of the spirit of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in similar ways without departing from the spirit of the present invention.
[0051] Although the terms such as the primary injection blow mold 1, the secondary injection blow mold 2, the primary molding left mold body 3, the primary molding right mold body 4, the primary molding part 5, the secondary molding left mold body 6, the secondary molding right mold body 7, the secondary molding part 8, the primary molding chamber 9, the primary injection port 10, the water cup bottom primary molding part 11, the bottom primary molding ring seat 12, the first sealing ferrule 13, the secondary molding chamber 14, the secondary injection port 15, the water cup bottom secondary molding part 16, the bottom secondary molding ring seat 17, the second sealing ferrule 18 are used more frequently in this article, the possibility of using other terms is not excluded. The use of these terms is only for the purpose of more conveniently describing and explaining the essence of the utility model, and interpreting them as any additional restrictions is contrary to the spirit of the utility model.
Claims
1. A two-step injection blow mold for a plastic water cup, comprising a primary injection blow mold (1) and a secondary injection blow mold (2), characterized in that: The primary injection blow mold (1) comprises a primary molding left mold body (3) and a primary molding right mold body (4), a primary molding portion (5) is formed between the primary molding left mold body (3) and the primary molding right mold body (4), and the secondary injection blow mold (2) comprises a secondary molding left mold body (6) and a secondary molding right mold body (7), a secondary molding portion (8) is formed between the secondary molding left mold body (6) and the secondary molding right mold body (7), and the volume of the secondary molding portion (8) is greater than the volume of the primary molding portion (5).
2. The two-step injection blow mold for a plastic water cup according to claim 1, characterized in that: The preliminary molding part (5) comprises a preliminary molding chamber (9) located between a preliminary molding left mold body (3) and a preliminary molding right mold body (4), and a preliminary injection port (10) is connected to the top of the preliminary molding chamber (9).
3. The two-step injection blow mold for a plastic water cup according to claim 2, characterized in that: A water cup bottom preliminary forming piece (11) is provided at the bottom between the preliminary forming left mold body (3) and the preliminary forming right mold body (4), and the water cup bottom preliminary forming piece (11) abuts against the preliminary forming left mold body (3) and the preliminary forming right mold body (4).
4. The two-step injection blow mold for a plastic water cup according to claim 3, characterized in that: The water cup bottom preliminary molding part (11) comprises a bottom preliminary molding ring seat (12) arranged at the bottom between a preliminary molding left mold body (3) and a preliminary molding right mold body (4), and a first sealing sleeve (13) is sleeved on the bottom preliminary molding ring seat (12).
5. The two-step injection blow mold for a plastic water cup according to claim 4, characterized in that: The secondary molding part (8) comprises a secondary molding chamber (14) arranged between a secondary molding left mold body (6) and a secondary molding right mold body (7), and the top of the secondary molding chamber (14) is connected to a secondary injection port (15).
6. The two-step injection blow mold for a plastic water cup according to claim 5, characterized in that: A water cup bottom secondary molding piece (16) is provided at the bottom between the secondary molding left mold body (6) and the secondary molding right mold body (7), and the water cup bottom secondary molding piece (16) abuts against the secondary molding left mold body (6) and the secondary molding right mold body (7).
7. The two-step injection blow mold for a plastic water cup according to claim 6, characterized in that: The water cup bottom secondary molding part (16) comprises a bottom secondary molding ring seat (17) arranged at the bottom between a secondary molding left mold body (6) and a secondary molding right mold body (7), and a second sealing sleeve (18) is sleeved on the bottom secondary molding ring seat (17).
8. The two-step injection blow mold for a plastic water cup according to claim 7, characterized in that: The volume of the primary molding chamber (9) is smaller than the volume of the secondary molding chamber (14), the height of the primary injection port (10) is the same as the height of the secondary injection port (15), and the inner diameter of the primary injection port (10) is smaller than the inner diameter of the secondary injection port (15).
9. The two-step injection blow mold for a plastic water cup according to claim 8, characterized in that: The height of the bottom primary molding ring seat (12) is smaller than the height of the bottom secondary molding ring seat (17), and the outer diameter of the bottom primary molding ring seat (12) is smaller than the outer diameter of the bottom secondary molding ring seat (17).