Electrolytic anode tin bar with improved structure

By designing an improved hook structure on the electrolytic anode tin rod, including threaded posts, bolts and copper sheets, the problem of the traditional tin rod being easy to swing is solved, the stability and corrosion resistance are improved, and the stability of the tin rod during processing is ensured. Stable operation.

CN221854835UActive Publication Date: 2024-10-18DONGGUAN YONGCHENG SOLDER PROD CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323351350.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-09
Publication Date
2024-10-18
Estimated Expiration
2033-12-09

AI Technical Summary

Technical Problem

The traditional electrolytic anode tin rod is easy to swing after being hung on the anode, causing the tin rod to collide and affecting production stability.

Method used

A structure-improved electrolytic anode tin rod is designed, which adopts a structure including a tin rod body and a hook. The hook includes a connecting block, a bent part, a threaded column, a bolt, a copper sheet and a corrosion-resistant paint layer, and is in contact with the anode through the bolt. The tight conductivity of the copper sheet conducts current to ensure the stable positioning of the solder rod.

Benefits of technology

It effectively prevents the tin rod from swinging during processing, improves stability and corrosion resistance, and extends the service life of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221854835U_ABST
    Figure CN221854835U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of tin bars, in particular to an electrolytic anode tin bar with an improved structure, which comprises a tin bar body and a hook, the hook comprises a connecting block and a bent part arranged on the surface of one side of the connecting block, a threaded column is arranged on the surface of one side, far away from the tin bar body, of the connecting block, and the bent part is connected with the threaded column. A threaded hole is formed in the end of the tin bar body, the threaded column is in threaded fit with the threaded hole, a plurality of bolts are arranged on the outer side, away from the tin bar body, of the bent part in a threaded mode, and the end of the thread extends to the inner side of the bent part. The tin bar has the effect that the tin bar body is not easy to swing.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of tin rods, in particular to an electrolytic anode tin rod with improved structure. Background Art

[0002] Electrolytic anode tin rod is an anode material used in electrolytic processes. It is usually made of high-purity tin metal and has good corrosion resistance and conductivity. During the electrolysis process, the tin rod on the positive electrode (i.e., anode) undergoes an oxidation reaction, releasing oxygen and tin ions, and transferring current to the negative electrode (i.e., cathode) to promote the reduction reaction of metal ions in the solution. Electrolytic anode tin rods are usually used in tin electroplating, electrochemical processing and other fields.

[0003] At present, the electrolytic anode tin rod is generally provided with a hook. During the production process, the electrolytic anode tin rod is hung on the anode of the machine using the hook, and the electrolytic anode tin rod is energized through the hook to achieve the purpose of electrolysis. However, after the traditional electrolytic anode tin rod is hung on the anode, it is unstable and easy to swing during the production process, causing the tin rod to collide. Utility Model Content

[0004] In order to prevent the tin rod from swinging easily, the utility model provides an electrolytic anode tin rod with improved structure in view of the problems of the prior art.

[0005] The utility model provides an electrolytic anode tin rod with improved structure, which adopts the following technical scheme:

[0006] A structurally improved electrolytic anode tin rod comprises a tin rod body and a hook, wherein the hook comprises a connecting block and a bending portion arranged on one side surface of the connecting block, a threaded column is arranged on the side surface of the connecting block away from the tin rod body, a threaded hole is arranged at the end of the tin rod body, the threaded column is threadedly matched with the threaded hole, a plurality of bolts are arranged on the outer thread of the bending portion away from the tin rod body, and the end of the thread extends to the inner side of the bending portion.

[0007] Preferably, a pad is provided at the end of the bolt located inside the bending portion.

[0008] Preferably, the hook is made of brass.

[0009] Preferably, a bent copper sheet is provided on the inner side of the bent portion, and the copper sheet is attached to the inner side surface of the bent portion.

[0010] Preferably, a plurality of screws are threadedly connected between the copper sheet and the bending portion.

[0011] Preferably, the outer surfaces of the connecting block and the bending portion are provided with a corrosion-resistant paint layer.

[0012] Preferably, a sealing rubber pad is provided between the connecting block and the solder rod body.

[0013] In summary, the present invention includes at least one of the following beneficial technical effects:

[0014] When the hook is hung on the anode, the operator tightens the bolt so that the pad at the end of the bolt is pressed against the anode, and the tin rod body can be positioned. In this way, the tin rod body is not easy to swing during the processing, and the stability is improved. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a schematic diagram of the overall structure of the utility model.

[0016] Figure 2 It is a side schematic diagram of the utility model.

[0017] Figure 3 It is an explosion diagram of the utility model.

[0018] Figure 4 It is a structural schematic diagram of the hook in the utility model.

[0019] In the figure: 1, solder rod body; 11, threaded hole; 2, hook; 21, connecting block; 22, bending part; 23, threaded column; 24, bolt; 241, pad; 25, copper sheet; 26, screw; 27, sealing pad; DETAILED DESCRIPTION

[0020] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0021] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, or the positions or positional relationships in which the product of the application is usually placed when in use. They are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as a limitation on the present application. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.

[0022] The utility model embodiment discloses an electrolytic anode tin rod with improved structure, such as Figure 1-4 As shown, it includes a tin rod body 1 and a hook 2. The hook 2 is located at the top of the tin rod body 1. The hook 2 includes a connecting block 21 and a bending portion 22 integrally formed on one side surface of the connecting block 21. When hanging the tin rod body 1, the hook 2 is hung on the anode, and electricity is supplied to the tin rod body 1 through the hook 2.

[0023] In addition, a threaded column 23 is integrally formed on the surface of the connecting block 21 on one side away from the tin rod body 1, and a threaded hole 11 is opened at the top end of the tin rod body 1. The threaded column 23 is threadedly matched with the threaded hole 11. When the tin rod body 1 is about to be completely consumed, a small section of the tin rod body 1 that remains is unscrewed from the threaded column 23, and then replaced with a new tin rod body 1 for re-electrolysis, and the removed tin rod body 1 is re-melted and cast into a new tin rod body 1. In addition, a plurality of bolts 24 are threadedly connected to the outer side surface of one end of the bending portion 22 away from the tin rod body 1, and one end of the bolt 24 is threadedly penetrated through the bending portion 22 and extends to the inner side of the bending portion 22. When the hook 2 is hung on the anode, the operator tightens the bolt 24 so that the end of the bolt 24 is pressed against the anode, and the tin rod body 1 can be positioned. In this way, the tin rod body 1 is not easy to swing during the processing. In addition, a pad 241 is welded to the end of the bolt 24 located on the inner side of the bending portion 22, and the pad 241 can increase the contact area between the end of the bolt 24 and the anode, thereby increasing the friction.

[0024] In addition, the hook 2 is made of brass, which is an alloy composed of copper and zinc, and has better electrical conductivity than ordinary metals. In addition, a bent copper sheet 25 is provided on the inner side of the bent portion 22, and the copper sheet 25 is attached to the inner side of the bent portion 22. The copper sheet 25 is made of pure copper, which has stronger oxidation resistance than brass, and has better electrical conductivity, and can better conduct current from the anode to the hook 2. In addition, a plurality of screws 26 are threadedly connected between the copper sheet 25 and the bent portion 22. After the copper sheet 25 is damaged, the screws 26 can be unscrewed to conveniently replace the copper sheet 25. In addition, the outer surface of the connecting block 21 and the bent portion 22 is provided with a corrosion-resistant paint layer, and the corrosion-resistant paint can be one of epoxy paint, peroxide paint, and phenolic paint. The corrosion-resistant paint can prevent liquid from splashing onto the hook 2 during the production process, causing corrosion to the hook 2. In addition, a sealing rubber pad 27 is provided between the connecting block 21 and the solder rod body 1 , and the sealing rubber pad 27 can improve the sealing between the connecting block 21 and the solder rod body 1 , and prevent liquid from penetrating into between the connecting block 21 and the solder rod body 1 .

[0025] The implementation principle of the structurally improved electrolytic anode tin rod of the utility model embodiment is as follows: when the hook 2 is hung on the anode, the operator tightens the bolt 24 so that the pad 241 at the end of the bolt 24 is pressed against the anode, and the tin rod body 1 can be positioned, so that the tin rod body 1 is not easy to swing during the processing, thereby improving stability.

[0026] The above is only a preferred embodiment of the utility model, and does not limit the utility model in any form. Although the utility model is disclosed as a preferred embodiment as above, it is not used to limit the utility model. Any technician familiar with this profession can make some changes or modifications to equivalent embodiments of equivalent changes by using the technical content disclosed above without departing from the scope of the technical solution of the utility model. However, any simple modification, equivalent change and modification made to the above embodiments according to the technology of the utility model, which does not depart from the content of the technical solution of the utility model, belongs to the scope of the technical solution of the utility model.

Claims

1. An electrolytic anode tin rod with improved structure, Features: The invention comprises a tin rod body (1) and a hook (2), wherein the hook (2) comprises a connecting block (21) and a bending portion (22) arranged on a side surface of the connecting block (21), a threaded column (23) is arranged on a side surface of the connecting block (21) away from the tin rod body (1), a threaded hole (11) is arranged at the end of the tin rod body (1), the threaded column (23) is threadedly matched with the threaded hole (11), and a plurality of bolts (24) are arranged on the outer side of the bending portion (22) away from the tin rod body (1), and the end of the thread extends to the inner side of the bending portion (22).

2. The electrolytic anode tin rod with improved structure according to claim 1, Features: A pad (241) is provided at the end of the bolt (24) located inside the bent portion (22).

3. The electrolytic anode tin rod with improved structure according to claim 1, Features: The hook (2) is made of brass.

4. The electrolytic anode tin rod with improved structure according to claim 3, Features: A bent copper sheet (25) is provided inside the bent portion (22), and the copper sheet (25) is attached to the inner side surface of the bent portion (22).

5. The electrolytic anode tin rod with improved structure according to claim 4, Features: A plurality of screws (26) are threadedly connected between the copper sheet (25) and the bent portion (22).

6. The electrolytic anode tin rod with improved structure according to claim 1, Features: The outer surfaces of the connecting block (21) and the bent portion (22) are provided with a corrosion-resistant paint layer.

7. The electrolytic anode tin rod with improved structure according to claim 1, Features: A sealing rubber pad (27) is provided between the connecting block (21) and the solder rod body (1).