Solid-liquid gold sheet

Through the design of solid liquid gold sheets, the combination of a skeleton layer with high thermal conductivity and a liquid gold layer, combined with a strong adhesion structure and plating fixation, solves the problem of liquid metal scattering and achieves efficient heat dissipation and convenient installation and disassembly.

CN221860945UActive Publication Date: 2024-10-18李强
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323388901.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-12
Publication Date
2024-10-18
Estimated Expiration
2033-12-12

AI Technical Summary

Technical Problem

The existing liquid metal heat dissipation medium is easily scattered or leaked during use, causing damage to the computer and making installation and disassembly inconvenient.

Method used

A solid liquid gold sheet is designed, including a skeleton layer, a liquid gold layer and a thin film layer. The liquid gold layer is solid at room temperature and liquid at high temperatures. It adheres to the skeleton layer and is fixed through a strong adhesion structure and plating to avoid scattering and keep it outside. Covered with plastic film to facilitate installation and removal.

Benefits of technology

It achieves efficient heat dissipation while avoiding computer malfunctions caused by liquid gold scattering. The installation and disassembly process is simple, and it is easy to package and transport at room temperature.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221860945U_ABST
    Figure CN221860945U_ABST
Patent Text Reader

Abstract

The utility model belongs to the technical field of computer heat dissipation accessories, and relates to a solid and liquid gold sheet, which comprises a framework layer, a liquid gold layer and a thin film layer, the framework layer is sheet metal, the liquid gold layer is fixed on the outer side of the framework layer to form a thin plating layer, the melting point of the liquid gold layer is 40-80 DEG C, and the thin film layer is made of metal. The liquid gold layer is in a solid state and is integrated with the framework layer in a room temperature state, the liquid gold layer is in a liquid state and is attached to the framework layer in a high temperature state, and the thin film layer is fixed on the outer side of the liquid gold layer in a peelable mode. The solid-liquid gold sheet provided by the utility model can prevent liquid metal from scattering, and has the advantages of simple structure and convenience in use.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of computer heat dissipation accessories and relates to a solid liquid gold sheet. Background Art

[0002] At present, the main methods of heat dissipation for computer CPU (central processing unit) and GPU (graphics processing unit) on the market are air cooling, liquid cooling and semiconductor cooling. In order to quickly transfer heat between the radiator and the CPU and GPU, a layer of thermal grease is usually added, which is the mainstream first type of heat transfer medium. In addition to thermal grease, there are also thermal pads and phase change sheets, which are the second type of heat transfer medium. Liquid metal belongs to the third type of heat transfer medium. Among these heat transfer media, liquid metal has the strongest thermal conductivity, which can reach 137w / mK. Although liquid metal is a good conductor of electricity, it is in a liquid state and is easy to scatter or leak during use, causing damage to the computer. Utility Model Content

[0003] In view of the deficiencies in the prior art, the utility model provides a solid liquid gold sheet, which can prevent the liquid metal from scattering and has the advantages of simple structure and convenient use.

[0004] In order to solve the above technical problems, the purpose of the utility model is achieved through the following technical solutions:

[0005] A solid liquid gold sheet comprises a skeleton layer, a liquid gold layer and a thin film layer, wherein the skeleton layer is a sheet of metal, the liquid gold layer is fixed on the outer side of the skeleton layer to form a thin coating, the melting point of the liquid gold layer is 40-80°C, the liquid gold layer is solid at room temperature and forms an integral structure with the skeleton layer, and the liquid gold layer is liquid and attached to the skeleton layer at high temperature, and the thin film layer is peelably fixed on the outer side of the liquid gold layer.

[0006] In the above-mentioned solid liquid gold sheet, the skeleton layer is made of metal with high thermal conductivity, preferably, the skeleton layer is a copper sheet; preferably, the liquid gold layer is a tin-bismuth alloy or a gallium-based liquid alloy, more preferably, the liquid gold layer is a tin-bismuth alloy; preferably, the film layer is plastic.

[0007] In the above-mentioned solid liquid gold sheet, the liquid gold layer is fixed by electroplating, chemical plating or other methods.

[0008] In the above-mentioned solid liquid gold sheet, the liquid gold layer and the skeleton layer may have different thicknesses according to the product specifications, so that the liquid gold layer can be stably attached to the skeleton layer. Preferably, the thickness of the liquid gold layer is less than 1 mm.

[0009] In the above-mentioned solid liquid gold sheet, preferably, the melting point of the liquid gold layer is 50-55°C.

[0010] In the above-mentioned solid liquid gold sheet, strong adhesion structures are provided on both side surfaces of the skeleton layer.

[0011] Furthermore, in the above-mentioned solid liquid gold sheet, the strong adhesion structure includes a plurality of through-hole structures penetrating the skeleton layer along the thickness direction. The liquid gold layer cannot pass through the through-hole structure when it is in liquid state. The through-hole is a small hole structure and may have different pore sizes depending on the material of the liquid gold. The pore size selection criteria are: the surface tension of the liquid gold can prevent it from passing through the through-hole of the pore size.

[0012] Furthermore, in the above-mentioned solid liquid gold sheet, the strong adhesion structure includes a plurality of blind hole structures arranged on both sides of the skeleton layer. Preferably, the hole depth of the blind hole is not more than one third of the thickness of the skeleton layer.

[0013] Furthermore, in the above-mentioned solid liquid gold sheet, the strong adhesion structure includes foamed copper, and the liquid gold layer is attached to the foamed copper.

[0014] In the above-mentioned solid liquid gold sheet, the solid liquid gold sheet is placed between the heat sink and the processor, and the processor includes a computer CPU and a GPU.

[0015] Compared with the prior art, the utility model has the following beneficial effects:

[0016] 1. The utility model provides a solid liquid gold sheet, which attaches liquid metal to a metal frame in the form of a coating, and is placed between the radiator and the processor when in use. When the computer is in use, the temperature of the processor will rise to the melting point of the liquid gold, and the liquid gold will melt, thereby filling the gap between the heat sink and the processor and driving out the air in the gap. Since the thermal conductivity of liquid gold and copper is very high, the entire liquid gold sheet can also achieve a very good heat dissipation effect. At the same time, when in use, the liquid gold will adhere to the frame layer and will not scatter into the computer, thereby avoiding computer failure.

[0017] 2. The utility model can be placed directly between the radiator and the processor when in use, and is very convenient to install. At the same time, as long as the computer is kept at room temperature when disassembling, the liquid gold sheet exists in a solid form and can be easily disassembled. In addition, the utility model is also covered with a plastic film on the outer layer, which can further protect the liquid gold sheet and facilitate packaging and transportation.

[0018] 3. The utility model fixes the liquid gold layer to the skeleton layer by plating, so that the liquid gold layer can be more firmly attached before use; the utility model further arranges a variety of strong attachment structures, so that the liquid gold layer can be more firmly attached to the skeleton layer in the liquid state to prevent it from scattering. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic diagram of the structure of Embodiment 1 of the present utility model;

[0020] Figure 2 It is a structural schematic diagram of Embodiment 2 of the present utility model;

[0021] Figure 3 It is a structural schematic diagram of Embodiment 3 of the present utility model;

[0022] Figure numerals: 1. skeleton layer; 2. liquid gold layer; 3. thin film layer; 4. through hole structure; 5. blind hole structure. DETAILED DESCRIPTION

[0023] The present invention will be further described below with reference to the accompanying drawings. Figure 1-3 :

[0024] Example 1

[0025] Compare with Figure 1 A solid liquid gold sheet comprises a skeleton layer 1, a liquid gold layer 2 and a thin film layer 3, wherein the skeleton layer 1 is a sheet metal, the liquid gold layer 2 is fixed to the outer side of the skeleton layer 1 to form a thin coating, the melting point of the liquid gold layer 2 is 40-80°C, the liquid gold layer 2 is solid at room temperature and is an integral structure with the skeleton layer 1, and the liquid gold layer 2 is liquid at high temperature and is attached to the skeleton layer 1, and the thin film layer 3 is peelably fixed to the outer side of the liquid gold layer 2.

[0026] When in use, first tear off the film layer 3, and then place the liquid gold sheet between the radiator and the processor. When the computer is in use, the temperature of the processor will rise to the melting point of the liquid gold, and the liquid gold will melt, thereby filling the gap between the heat sink and the processor, driving out the air in the gap, and forming a highly efficient heat dissipation structure. At the same time, the liquid gold will adhere to the skeleton layer 1 and will not scatter into the inside of the computer and cause computer malfunction. When the computer is finished using, the liquid gold sheet cools down and returns to a solid state.

[0027] In this embodiment, the skeleton layer 1 is made of metal with high thermal conductivity, preferably, the skeleton layer 1 is a copper sheet; preferably, the liquid gold layer 2 is a tin-bismuth alloy or a gallium-based liquid alloy, more preferably, the liquid gold layer 2 is a tin-bismuth alloy; preferably, the thin film layer 3 is plastic.

[0028] In this embodiment, the liquid gold layer 2 is fixed by electroplating, chemical plating or other methods.

[0029] According to the product specifications, the liquid gold layer 2 and the skeleton layer 1 may have different thicknesses, so that the liquid gold layer 2 can be stably attached to the skeleton layer 1. At the same time, the appropriate thickness can also ensure that the liquid gold is sufficient to fill the gap when it is in liquid state. In this embodiment, the thickness of the liquid gold layer 2 is less than 1 mm.

[0030] In this embodiment, in order to enable the liquid gold layer 2 to melt in time when in use and quickly return to a solid state at room temperature, preferably, the melting point of the liquid gold layer 2 is 50-55°C.

[0031] Example 2

[0032] Compare with Figure 2 Based on Example 1, this example further provides a strong adhesion structure on both side surfaces of the skeleton layer 1.

[0033] The strong adhesion structure includes a plurality of through-hole structures 4 that penetrate the skeleton layer 1 in the thickness direction. The liquid gold layer 2 cannot pass through the through-hole structures 4 when it is in liquid state. The through-holes are small hole structures. Depending on the material of the liquid gold, they can have different apertures. The aperture selection criteria are: the surface tension of the liquid gold can prevent it from passing through the through-holes of the aperture. The through-hole structures 4 can make the liquid gold in liquid state more firmly attached to the skeleton layer 1.

[0034] Example 3

[0035] Compare with Figure 3 Based on Example 1, this example further provides a strong adhesion structure on both side surfaces of the skeleton layer 1.

[0036] The strong adhesion structure includes a plurality of blind hole structures 5 arranged on both sides of the skeleton layer 1. Preferably, the depth of the blind hole is not more than one third of the thickness of the skeleton layer 1. The blind hole structure 5 can make the liquid gold in liquid state adhere to the skeleton layer 1 more firmly.

[0037] Example 4

[0038] On the basis of Example 1, this example further provides strong adhesion structures on both side surfaces of the skeleton layer 1 .

[0039] The strong adhesion structure includes copper foam, and the liquid gold layer 2 is attached to the copper foam. The porous structure in the copper foam forms a certain restraining effect on the liquid gold layer 2, which can further prevent it from scattering. At the same time, the copper foam will not affect its heat dissipation performance.

[0040] The above embodiments are only preferred embodiments of the present invention and are not intended to limit the protection scope of the present invention. Therefore, any equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A solid liquid gold sheet, characterized in that: The invention comprises a skeleton layer (1), a liquid gold layer (2) and a thin film layer (3), wherein the skeleton layer (1) is a sheet metal, the liquid gold layer (2) is fixed on the outer side of the skeleton layer (1) to form a thin coating, the melting point of the liquid gold layer (2) is 40-80°C, the liquid gold layer (2) is solid at room temperature and forms an integral structure with the skeleton layer (1), and the liquid gold layer (2) is liquid and adheres to the skeleton layer (1) at high temperature, and the thin film layer (3) is fixed on the outer side of the liquid gold layer (2) in a removable manner.

2. A solid liquid gold sheet according to claim 1, characterized in that: The skeleton layer (1) is a copper sheet, the liquid gold layer (2) is a tin-bismuth alloy or a gallium-based liquid alloy, and the thin film layer (3) is plastic.

3. The solid liquid gold sheet according to claim 1, characterized in that: The liquid gold layer (2) is fixed in an electroplating or chemical plating manner.

4. The solid liquid gold sheet according to claim 1, characterized in that: The thickness of the liquid gold layer (2) is less than 1 mm.

5. The solid liquid gold sheet according to claim 1, characterized in that: The melting point of the liquid gold layer (2) is 50-55°C.

6. The solid liquid gold sheet according to claim 1, characterized in that: Strong adhesion structures are provided on both side surfaces of the skeleton layer (1).

7. The solid liquid gold sheet according to claim 6, characterized in that: The strong adhesion structure comprises a plurality of through-hole structures (4) penetrating the skeleton layer (1) along the thickness direction, and the liquid gold layer (2) cannot pass through the through-hole structures (4) when it is in a liquid state.

8. The solid liquid gold sheet according to claim 6, characterized in that: The strong adhesion structure comprises a plurality of blind hole structures (5) arranged on the surfaces of both sides of the skeleton layer (1).

9. The solid liquid gold sheet according to claim 6, characterized in that: The strong adhesion structure comprises foam copper, and the liquid gold layer (2) is attached to the foam copper.

10. A solid liquid gold sheet according to any one of claims 1 to 9, characterized in that: The solid liquid gold sheet is placed between the heat sink and the processor.