Electrode assembly, battery monomer, battery and electric equipment

By coating the active material layer in zones on the pole pieces of the electrode assembly, and using the space gap in the second coating area to reduce stress, the problem of breakage at the corners of the electrode assembly is solved, and the structural strength and stability are improved.

CN221861683UActive Publication Date: 2024-10-18CONTEMPORARY AMPEREX TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202322813871.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-10-19
Publication Date
2024-10-18
Estimated Expiration
2033-10-19

AI Technical Summary

Technical Problem

Existing electrode assemblies are prone to stress concentration leading to breakage at the corners of the pole pieces. In particular, the probability of breakage at the corners increases significantly after cyclic charging and discharging.

Method used

By coating the active material layer in zones on the current collector of the pole piece, a first coating area and a second coating area are set. The second coating area is located at the bend and has a thickness smaller than the first coating area. Using the second The space gap in the coating area reduces the internal stress of the pole piece, provides expansion space, and improves the structural strength.

Benefits of technology

It effectively reduces the stress of the pole piece at the bending point, improves the structural strength of the electrode assembly, reduces the risk of fracture at the bending point, and especially provides corresponding expansion space when the pole piece expands.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221861683U_ABST
    Figure CN221861683U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of batteries, and provides an electrode assembly, a battery monomer, a battery and electric equipment, the electrode assembly comprises two pole pieces which are wound or laminated and have opposite polarities, the pole pieces are wound or laminated to form a plurality of bends, each pole piece comprises a current collector and an active material layer, and the active material layer is arranged between the current collector and the active material layer. The current collector comprises a first coating area and a second coating area, the second coating area is located at the bending position, and the thickness of the active material layer coated in the second coating area is smaller than that of the active material layer of the first coating area. When the pole piece is bent due to winding or stacking arrangement, the active material layer positioned in the first coating area can be properly extended by utilizing the space gap in the second coating area, so that the stress of the pole piece at the bent part is reduced, and particularly, a corresponding expansion space is provided when the pole piece is expanded, and further, the structural strength of the electrode assembly at the bent part is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of batteries, and in particular provides an electrode assembly, a battery cell, a battery and an electrical device. Background Art

[0002] Power batteries have the advantages of high energy density and environmental friendliness. At present, power batteries are widely used in electronic devices such as mobile phones and laptops. Moreover, with the vigorous development of new energy technologies, power batteries are gradually used in hybrid vehicles, electric vehicles and energy storage systems.

[0003] Among them, the power battery includes an electrode assembly, which is formed by stacking or winding pole pieces. However, stress concentration is prone to occur at the corners of the pole pieces, resulting in fracture problems. Utility Model Content

[0004] The utility model aims to provide an electrode assembly, a battery cell, a battery and an electrical device, aiming to solve the problem that the corners of the existing electrode assembly are prone to breakage.

[0005] In order to achieve the above purpose, the technical solution adopted by the utility model is:

[0006] In the first aspect, the present application also provides an electrode assembly, comprising two pole pieces with opposite polarities that are wound or stacked, the pole pieces forming multiple bends due to the winding or stacking, the pole pieces comprising a current collector and an active material layer disposed on the current collector, the current collector comprising a first coating area and a second coating area, and the second coating area is located at the bend, and the thickness of the active material layer coated on the second coating area is less than the thickness of the active material layer on the first coating area.

[0007] Beneficial effects of the utility model: the electrode assembly provided by the utility model has a first coating area and a second coating area on the current collector on the pole piece, the thickness of the active material coating on the second coating area is less than the thickness of the active material coating in the first coating area, and the second coating area is located at the bending part. Therefore, when the pole piece is bent due to winding or stacking, the active material layer located in the first coating area can utilize the spatial gap at the second coating area to extend appropriately, thereby reducing the stress of the pole piece at the bending part, especially providing corresponding expansion space when the pole piece expands, thereby improving the structural strength of the electrode assembly at the bending part.

[0008] In one embodiment, there are a plurality of second coating regions, and the second coating regions are spaced apart from each other along the length direction of the current collector.

[0009] In one embodiment, the second coating region extends along a width direction of the current collector to separate the first coating region.

[0010] In one embodiment, the thicknesses of the active material layers coated on at least two of the second coating regions are different.

[0011] In one embodiment, the thickness of the active material layer coated on each of the second coating regions is equal.

[0012] In one embodiment, each of the second coating regions is not coated with the active material layer.

[0013] In one embodiment, the current collector has a first end surface and a second end surface that are opposite to each other, and the active material layer is provided on the first end surface and / or the second end surface.

[0014] In one embodiment, the electrode sheet is a positive electrode sheet, which includes a positive electrode collector and a positive electrode active material layer arranged on the positive electrode collector, and the positive electrode collector has a first convex surface and a first concave surface at the bending point, and a plurality of the second coating areas are formed on the first convex surface and / or the first concave surface.

[0015] In one embodiment, the electrode sheet is a negative electrode sheet, which includes a negative electrode current collector and a negative electrode active material layer arranged on the negative electrode current collector, and the negative electrode current collector has a second convex surface and a second concave surface at the bending point, and a plurality of second coating areas are formed on the second convex surface and / or the second concave surface.

[0016] In one embodiment, at the bending portion, the anode capacity of the positive electrode active material layer is greater than the cathode capacity of the negative electrode active material layer.

[0017] In one embodiment, when the thickness of the positive electrode active material layer is equal to the thickness of the negative electrode active material layer, the number of the second coating regions on the positive electrode collector is less than the number of the second coating regions on the negative electrode collector.

[0018] In a second aspect, an embodiment of the present application further provides a battery cell, comprising the electrode assembly described above.

[0019] In a third aspect, an embodiment of the present application further provides a battery, comprising the battery cell described above.

[0020] In a fourth aspect, an embodiment of the present application further provides an electrical device, comprising the battery described above.

[0021] It can be understood that the beneficial effects of the second, third and fourth aspects mentioned above can be found in the relevant description of the first aspect mentioned above, and will not be repeated here. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0023] Figure 1 A schematic diagram of the structure of an electrical device provided in an embodiment of the utility model;

[0024] Figure 2 An exploded view of a battery provided in an embodiment of the utility model;

[0025] Figure 3 An exploded view of a battery cell provided in an embodiment of the utility model;

[0026] Figure 4 A cross-sectional view of an electrode assembly provided in an embodiment of the utility model;

[0027] Figure 5 A cross-sectional view of a pole piece provided in Embodiment 1 of the present utility model;

[0028] Figure 6 A cross-sectional view of a pole piece provided in Embodiment 2 of the present utility model;

[0029] Figure 7 A cross-sectional view of a pole piece provided in Embodiment 3 of the present utility model;

[0030] Figure 8 A cross-sectional view of a pole piece provided in Embodiment 4 of the present utility model;

[0031] Fig. 9 A top view of the current collector of the pole piece provided in the fifth embodiment of the utility model;

[0032] Fig.10 A top view of the current collector of the pole piece provided in Example 6 of the utility model;

[0033] Fig.11 This is a top view of the current collector of the pole piece provided in Example 7 of the utility model.

[0034] Among them, the reference numerals in the figure are:

[0035] 10000, electrical equipment; 1000, controller; 2000, motor;

[0036] 3000, battery; 3002, battery box; 30021, first part; 30022, second part;

[0037] 3001, battery cell; 30011, housing; 30012, end cover; 30013, electrode terminal;

[0038] 100, electrode assembly; 10, pole piece; 11, current collector; 12, active material layer; 11a, first coating area; 11b, second coating area; 10a, positive pole piece; 10b, negative pole piece;

[0039] 111, first end surface; 112, second end surface; 1111, first convex surface; 1112, first concave surface; 1121, second convex surface; 1122, second concave surface;

[0040] The width direction W of the current collector; the length direction L of the current collector; the thickness H of the active material coating. DETAILED DESCRIPTION

[0041] The embodiments of the present invention are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements having the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limiting the present invention.

[0042] In the description of the present invention, it should be understood that the terms "length", "width", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship, are based on the orientation or position relationship shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0043] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present utility model, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0044] In the present invention, unless otherwise clearly specified and limited, the terms "install", "connect", "connect", "fix" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0045] The electrode assembly is composed of a positive electrode sheet, a negative electrode sheet and a separator. The positive electrode sheet includes a positive current collector and a positive electrode active material coated on the positive current collector, and the negative electrode sheet includes a negative current collector and a negative electrode active material coated on the negative current collector. Generally, there are two winding methods for electrode assemblies: one is to wind the positive electrode sheet, the negative electrode sheet and the separator into a roll; the other is to stack the positive electrode sheet, the negative electrode sheet and the separator layer by layer in a stacking manner. Regardless of the above forming method, the positive and negative electrode sheets in the electrode assembly will form multiple bends. However, at the bends, the stress of the electrode sheet is relatively large and it is easy to break. In particular, after the electrode assembly is cyclically charged and discharged, the probability of the electrode sheet breaking at the bend is greatly increased.

[0046] In view of this, the present application provides an electrode assembly, which divides the coating area of ​​the current collector of the electrode piece, specifically into a first coating area and a second coating area, wherein the second coating area is located at the position where the electrode piece is bent, and the thickness of the active material coating on the second coating area is less than the thickness of the active material coating on the first coating area. In this way, at the bending part, the relatively thin characteristic of the active material coating on the second coating area can be utilized to reserve a certain space, thereby reducing the internal stress of the electrode piece, thereby improving the problem that the electrode piece is prone to breakage at the bending part.

[0047] A battery cell includes an electrode assembly and an electrolyte. The electrode assembly is composed of a positive electrode sheet, a negative electrode sheet and a separator. A battery cell mainly works by the movement of metal ions between the positive electrode sheet and the negative electrode sheet. The positive electrode sheet includes a positive electrode collector and a positive electrode active material layer. The positive electrode active material layer is coated on the surface of the positive electrode collector. The current collector not coated with the positive electrode active material layer protrudes from the current collector coated with the positive electrode active material layer. The current collector not coated with the positive electrode active material layer is stacked as a positive electrode tab. For the convenience of description, the term "tab" is used to refer to the positive electrode tab and / or the negative electrode tab.

[0048] In the present application, battery cells include but are not limited to lithium-ion secondary battery cells, lithium-ion primary battery cells, lithium-sulfur battery cells, sodium-lithium-ion battery cells, sodium-ion battery cells or magnesium-ion battery cells. Battery cells can be cylindrical, flat, rectangular or other shapes. Battery cells are generally divided into three types according to the packaging method: cylindrical battery cells, square battery cells and soft-pack battery cells.

[0049] The embodiment of the present application provides a battery cell 3001 using the above electrode assembly 100 as a power source, which can be applied to electric devices 10000 such as vehicles, mobile phones, portable devices, laptops, ships, spacecraft, and electric tools. Among them, the vehicle can be a fuel vehicle, a gas vehicle, or a new energy vehicle, and the new energy vehicle can be a pure electric vehicle, a hybrid vehicle, or an extended-range vehicle, etc.; the spacecraft includes airplanes, rockets, space shuttles, and spacecrafts, etc.; the electric toys include fixed or mobile electric toys, such as game consoles, electric car toys, electric ship toys, electric airplane toys, etc.; the electric tools include metal cutting electric tools, grinding electric tools, assembly electric tools, and iron electric tools, such as electric drills, electric grinders, electric wrenches, electric screwdrivers, electric hammers, impact drills, concrete vibrators, and electric planers, etc.

[0050] The battery cell 3001 described in the embodiment of the present application is not limited to the electrical equipment 10000 described above, but can also be applied to all devices using the battery cell 3001. However, for the sake of simplicity, the following embodiments are described using electric vehicles as an example.

[0051] For example, see Figure 1 , the figure is a schematic diagram of the structure of a vehicle according to an embodiment of the present application. The vehicle may be a fuel vehicle, a gas vehicle or a new energy vehicle. The new energy vehicle may be a pure electric vehicle, a hybrid vehicle or an extended-range vehicle, etc. A battery 3000, a controller 1000 and a motor 2000 may be arranged inside the vehicle, and the controller 1000 is used to control the battery 3000 to supply power to the motor 2000. For example, a battery 3000 may be arranged at the bottom, front or rear of the vehicle. The battery 3000 may be used to power the vehicle. For example, the battery 3000 may be used as an operating power source for the vehicle, for the circuit system of the vehicle, for example, for the working power requirements during the start-up, navigation and operation of the vehicle. In another embodiment of the present application, the battery 3000 may not only be used as an operating power source for the vehicle, but also as a driving power source for the vehicle, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle.

[0052] The battery 3000 mentioned in the embodiment of the present application refers to a single physical module including one or more battery cells 3001 to provide higher voltage and capacity. Figure 2, the battery 3000 may include multiple battery cells 3001. The number of battery cells 3001 and the connection between the battery cells 3001 can be set according to demand to meet different power requirements. Specifically, multiple battery cells 3001 can be connected in series, in parallel, or in mixed connection. Mixed connection refers to a mixture of series connection and parallel connection so that the battery 3000 has a larger capacity or power. Optionally, multiple battery cells 3001 can be connected in series, in parallel, or in mixed connection to form a battery 3000 module, and multiple battery 3000 modules can be connected in series, in parallel, or in mixed connection to form a battery 3000. In other words, multiple battery cells can directly form a battery 3000, or they can first form a battery module, and then the battery module can form a battery 3000.

[0053] The battery 3000 also includes a battery case 3002, and the battery case 3002 has a storage space inside, and multiple battery cells are stored in the storage space. As shown in the figure, the battery case 3002 may include two parts, which are respectively referred to as the first part 30021 and the second part 30022. Please refer to Figure and Figure, which is a first part 30021 of a battery case 3002. The first part 30021 and the second part 30022 can be connected by snapping, bonding, etc. to form a storage space. Multiple battery cells are connected in parallel, series, or mixed and placed in the box formed by connecting the first part 30021 and the second part 30022. Among them, the shapes of the first part 30021 and the second part 30022 can be determined according to the shape formed by the combination of multiple battery cells.

[0054] The battery case 3002 is used to protect at least one battery cell, thereby reducing the impact of liquid or other foreign matter outside the battery 3000 on the charging or discharging of at least one battery cell. The battery cell may be cylindrical, flat, rectangular or other shapes, etc., which are not limited in the present embodiment. The packaging methods of the battery cell include but are not limited to cylindrical battery cells, square battery cells and soft-pack battery cells, etc., which are not specifically limited in the present embodiment.

[0055] In addition, the battery 3000 may also include other structures, which are not described one by one here. For example, the battery 3000 may also include a busbar. The busbar is used to achieve electrical connection between multiple battery cells, such as parallel connection, series connection or mixed connection between multiple battery cells. Specifically, the busbar can achieve electrical connection between battery cells by connecting the electrode terminals of the battery cells. Further, the busbar can be fixedly connected to the electrode terminals of the battery cells by welding. Optionally, the busbar may include a conductive mechanism, and the electric energy generated by the multiple battery cells can be further led out through the battery case 3002 through the conductive mechanism.

[0056] Each battery cell 3001 may be a lithium-ion battery cell, a lithium-sulfur battery cell, a sodium-ion battery cell or a magnesium-ion battery cell, but is not limited thereto. The battery cell 3001 may be cylindrical, flat, rectangular or in other shapes.

[0057] Please refer to Figure 3 , Figure 3 The schematic diagram of the decomposition structure of a battery cell 3001 provided in some embodiments of the present application. The battery cell 3001 refers to the smallest unit that constitutes the battery 3000. Figure 3 The battery cell 3001 includes a shell 30011, an end cover 30012, an electrode assembly 100, an electrode terminal 30013 and other functional components.

[0058] The end cap 30012 refers to a component that covers the opening of the shell 30011 to isolate the internal environment of the battery cell 3001 from the external environment. Without limitation, the shape of the end cap 30012 can be adapted to the shape of the shell 30011 to match the shell 30011. Optionally, the end cap 30012 can be made of a material with a certain hardness and strength (such as aluminum alloy), so that the end cap 30012 is not easily deformed when squeezed and collided, so that the battery cell 3001 can have a higher structural strength and the safety performance can also be improved. Functional components such as electrode terminals 30013 can be provided on the end cap 30012. The electrode terminal 30013 can be used to connect with the electrode assembly 100 to output or input the electrical energy of the battery cell. In some embodiments, the end cap 30012 can also be provided with a pressure relief mechanism for releasing the internal pressure when the internal pressure or temperature of the battery cell 3001 reaches a threshold. The material of the end cap 30012 can also be various, such as copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc., which is not particularly limited in the present embodiment. In some embodiments, an insulating member can be provided inside the end cap 30012, and the insulating member can be used to isolate the electrical connection components in the housing 30011 from the end cap 30012 to reduce the risk of short circuit. Exemplarily, the insulating member can be plastic, rubber, etc.

[0059] The shell 30011 is a component used to cooperate with the end cap 30012 to form the internal environment of the battery cell 3001, wherein the formed internal environment can be used to accommodate the electrode assembly 100, the electrolyte and other components. The shell 30011 and the end cap 30012 can be independent components, and an opening can be set on the shell 30011, and the end cap 30012 is made to cover the opening at the opening to form the internal environment of the battery cell. Without limitation, the end cap 30012 and the shell 30011 can also be integrated. Specifically, the end cap 30012 and the shell 30011 can form a common connection surface before other components are put into the shell, and when it is necessary to encapsulate the interior of the shell 30011, the end cap 30012 is made to cover the shell 30011. The shell 30011 can be of various shapes and sizes, such as a rectangular parallelepiped, a cylindrical shape, a hexagonal prism, etc. Specifically, the shape of the shell 30011 can be determined according to the specific shape and size of the electrode assembly. The shell 30011 can be made of a variety of materials, such as copper, iron, aluminum, stainless steel, aluminum alloy, plastic, etc., and the embodiments of the present application do not impose any special restrictions on this.

[0060] The electrode assembly 100 is a component in the battery cell 3001 where an electrochemical reaction occurs. One or more electrode assemblies 100 may be included in the housing 30011. The electrode assembly 100 is mainly formed by winding a positive electrode sheet and a negative electrode sheet, and a separator is usually provided between the positive electrode sheet and the negative electrode sheet. The parts of the positive electrode sheet and the negative electrode sheet with active materials constitute the main body of the electrode assembly, and the parts of the positive electrode sheet and the negative electrode sheet without active materials each constitute a tab. The positive tab and the negative tab may be located together at one end of the main body or at both ends of the main body respectively. During the charge and discharge process of the battery, the positive active material and the negative active material react with the electrolyte, and the tabs connect the electrode terminals to form a current loop.

[0061] Combined with reference Figures 4 to 11 , Figure 4 A schematic diagram of the structure of an electrode assembly 100 provided in some embodiments of the present application; Figures 5 to 8 A cross-sectional view of a pole piece provided for some embodiments of the present application; Figures 9 to 11 A top view of a current collector provided for some embodiments of the present application.

[0062] In a first aspect, the present application provides an electrode assembly 100, comprising two types of pole pieces 10 with opposite polarities which are wound or stacked, the pole pieces 10 forming multiple bends due to the winding or stacking, the pole pieces 10 comprising a current collector 11 and an active material layer 12 disposed on the current collector 11, the current collector 11 comprising a first coating area 11a and a second coating area 11b, and the second coating area 11b is located at the bend, and a thickness H of the active material layer 12 coated on the second coating area 11b is less than a thickness H of the active material layer 12 of the first coating area 11a.

[0063] It can be understood that the two pole pieces 10 with opposite polarities are respectively a positive pole piece 10a and a negative pole piece 10b. Among them, the positive pole piece 10a includes a positive current collector and a positive active material layer, and the negative pole piece 10b includes a negative current collector and a negative active material layer. The different active material layers 12 are formed on the corresponding current collector 11 in ways including but not limited to spraying, coating, etc. Taking lithium-ion batteries as an example, the material of the positive current collector may be aluminum, and the positive active material may be lithium cobalt oxide, lithium iron phosphate, ternary lithium or lithium manganese oxide, etc. The material of the negative current collector may be copper, and the negative active material may be carbon or silicon, etc.

[0064] At the same time, the electrode assembly 100 is divided into a wound electrode assembly and a stacked electrode assembly. Regardless of the forming method, the pole piece 10 in the electrode assembly 100 has multiple bends due to winding or stacking. For example, the pole piece 10 of the wound electrode assembly is wound from the inside to the outside in circles. Under the action of gravity, the wound electrode assembly is relatively flat, and the bends are concentrated in the two arc-shaped transition sections protruding outward of the electrode assembly 100; while the pole piece 10 of the stacked electrode assembly is stacked from bottom to top in sequence, so the bend occurs at the position where the pole piece 10 of the stacked electrode assembly needs to be stacked in reverse, that is, the connection between each adjacent pole piece 10 on both sides.

[0065] The first coating area 11a and the second coating area 11b both refer to the surface area of ​​the current collector 11 for coating the active material layer 12. The difference is that the second coating area 11b is only located at the bending part of the pole piece 10, and the first coating area 11a can be located at the bending part of the pole piece 10, or at other positions on the pole piece 10 except the bending part, or at the bending part and other positions of the pole piece 10, etc.

[0066] Furthermore, the thickness H of the active material layer 12 on the second coating area 11 b is smaller than the thickness H of the active material layer 12 on the first coating area 11 a . Here, the thickness H of the active material layer 12 refers to the coating thickness or plating thickness of the active material layer 12 on the current collector 11 .

[0067] It should be noted that the first coating area 11a and the second coating area 11b are divided based on the thickness H of the active material layer 12 coated thereon. That is, the thickness H of the active material layer 12 coated on the first coating area 11a is the same or substantially the same, while the thickness H of the active material layer 12 coated on the second coating area 11b is thinner, so as to distinguish them. Optionally, there may be no active material layer 12 on the second coating area 11b, that is, the second coating area 11b is a blank uncoated area.

[0068] And, on a current collector 11 of a certain width and a certain length, the sum of the lengths of the coating areas is equal to the length of the current collector 11. The width of the first coating area 11a should be the same as the width of the current collector 11, and the active material layer 12 is completely covered in the first coating area 11a, that is, the width of the active material layer 12 is the same as the width of the first coating area 11a, to meet a higher energy density.

[0069] The width of the second coating area 11b can be equal to the width of the current current collector 11 or less than the width of the current current collector 11. Therefore, in terms of position distribution, when the width of the second coating area 11b is equal to the width of the current current collector 11, the second coating area 11b separates the first coating area 11a, so that the first coating area 11a is discontinuous; or, when the width of the second coating area 11b is less than the width of the current current collector 11, the first coating area 11a is continuous, and the second coating area 11b is surrounded by the first coating area 11a.

[0070] The electrode assembly 100 provided by the utility model has a first coating area 11a and a second coating area 11b on the current collector 11 on the pole piece 10, the thickness of the active material coating on the second coating area 11b is less than the thickness of the active material coating on the first coating area 11a, and the second coating area 11b is located at the bending part. Therefore, when the pole piece 10 is bent due to winding or stacking, the active material layer 12 located in the first coating area 11a can utilize the space gap at the second coating area 11b to extend appropriately, thereby reducing the stress of the pole piece 10 at the bending part, especially providing corresponding expansion space when the pole piece 10 expands, thereby improving the structural strength of the electrode assembly 100 at the bending part.

[0071] Please refer to Figures 5 to 8 In some embodiments, there are multiple second coating regions 11 b , and the second coating regions 11 b are spaced apart from each other along the length direction of the current collector 11 .

[0072] It can be understood that the length direction L of the current collector 11 is the extension direction of the current collector 11, and the area between the two second coating areas 11b is the first coating area 11a. After the active material layer 12 is coated on the corresponding coating area, the surface of the active material layer 12 is undulating, so that at the bend of the pole piece 10, the groove or groove-like structure formed on the active material layer 12 provides a certain expansion space for the active material to expand and reduce internal stress.

[0073] When the number of windings or stackings is large, the bending area and bending degree of the electrode assembly 100 are large. Therefore, it is necessary to increase the number of second coating areas 11 b to further reduce the internal stress of the electrode sheet 10 at the bending part.

[0074] Furthermore, the spacing between the second coating areas 11 b is the length of the active material layer 12 coated therebetween. Therefore, the spacing between the second coating areas 11 b can be adjusted according to the usage requirements of different scenarios.

[0075] Optionally, in the length direction L of the current collector 11, the second coating regions 11b are spaced apart at equal intervals. This situation is applicable to the electrode assembly 100 bent by the stacking process, and the bending degree and bending amplitude of each bent portion of the electrode sheet 10 are substantially the same.

[0076] Optionally, in the length direction L of the current collector 11, the spacing between each second coating area 11b first increases and then decreases, and the second coating area 11b with larger spacing is closer to the bending corner (the corner is the actual position where the pole piece 10 is bent). This situation is applicable to the bent electrode assembly 100 of the winding process, especially the pole piece 10 of the inner layer of the winding, the bending degree and amplitude of the pole piece 10 are greater than the pole piece 10 wound on the outer layer, thus providing a larger reserved space for the expansion of the active material.

[0077] Please refer to Figures 9 to 11 In some embodiments, the second coating region 11 b extends along the width direction W of the current collector 11 to separate the first coating region 11 a .

[0078] The width direction W of the current collector 11 is perpendicular to the length direction L of the current collector 11 , and the extension direction of the second coating region 11 b is perpendicular to the length direction L of the current collector 11 .

[0079] It can be understood that when the pole piece 10 is wound or stacked, the outer edge side of the pole piece 10 of the bottom layer or inner circle needs to be aligned or basically aligned with the outer edge side of the pole piece 10 of the upper layer or outer circle. Therefore, the current collector 11 of the pole piece 10 is folded in half with respect to its own width direction. In this way, the extension direction of the second coating area 11b is parallel or basically parallel to the symmetry axis of the bent pole piece 10. Then, the expansion direction of the active material is consistent or basically consistent with the space formed by the coating thickness difference on the active material layer 12, which is more conducive to reducing the stress concentration inside the active material.

[0080] Please refer to Figure 5 In one embodiment, the thickness H of the active material layer 12 coated on at least two second coating regions 11 b is different.

[0081] It can be understood that in each second coating area 11 b , the thickness H of the active material layer 12 coated on at least two second coating areas 11 b is different.

[0082] The second coating areas 11 b at different positions are coated with active material layers 12 of different thicknesses to adapt to the bending requirements of the electrode sheet 10 .

[0083] Optionally, the thickness H of the active material layer 12 coated on each second coating area 11b is different, and in the length direction L of the current collector 11, the thickness H of the active material layer 12 on each second coating area 11b decreases first and then increases, and the thinnest part of the active material layer 12 is located at or close to the bending part of the pole piece 10. In this way, the stress is most concentrated at the symmetric axis with the largest bending degree, and reducing the active material at this place can provide more reserved space. At the same time, the thickness H of the active material layer 12 away from the bending symmetry gradually increases, firstly, the bending degree and amplitude are weakened, and secondly, the total mass of the active material is increased to a certain extent, thereby improving the energy density of the electrode assembly 100.

[0084] Please refer to Figure 6 and Figure 7 In some embodiments, the thickness H of the active material layer 12 coated on each second coating area 11 b is equal.

[0085] It can be understood that in each second coating area 11 b , the thickness H of the active material layer 12 coated on each second coating area 11 b is the same.

[0086] The second coating area 11 b at each position is coated with an active material layer 12 of the same thickness, which is suitable for the electrode assembly 100 bent by the stacking process, and the bending degree and bending amplitude of each bent position of the electrode sheet 10 are substantially the same.

[0087] Please refer to Figure 7 In one embodiment, each second coating region 11 b is not coated with the active material layer 12 .

[0088] It can be understood that each second coating area 11 b is not coated with the active material layer 12 , and thus each second coating area 11 b is a blank area.

[0089] Thus, the thickness H of the active material layer 12 of each second coating area 11b is zero, and the reserved space formed in the second coating area 11b is the largest, which can provide the space required for the active material at the bend to expand to the greatest extent, thereby reducing the internal stress.

[0090] Optionally, in a specific embodiment, each second coating area 11b is a blank area, the number of the second coating areas 11b is five to twenty, and each second coating area 11b is arranged at intervals along the length direction L of the current collector 11, the length of each second coating area 11b ranges from 0.01mm to 0.1mm, and the interval between two adjacent second coating areas 11b is greater than 1mm. In this way, a blank area group is formed at each bend of each pole piece 10, and the number of the second coating areas 11b can be increased or decreased according to the degree and amplitude of the bending of the current pole piece 10, and the length and spacing of each second coating area 11b can be adjusted.

[0091] It should be noted that the active material layer 12 is not coated on the corresponding second coating area 11b by using an oscillating gap coating process, that is, there is a corresponding coating gap during the coating process, and the coating gap corresponds to the corresponding second coating area 11b. In the case where the thickness H of the active material layer 12 coated on the second coating area 11b is less than the thickness H of the active material layer 12 on the first coating area 11a, an engraving or etching process is used, that is, a layer of active material layer 12 with uniform thickness is coated on the current collector 11, and then the active material layer 12 is removed at the position corresponding to the second coating area 11b, so as to achieve a thinner thickness H of the active material layer 12 in this area.

[0092] Please refer to Figure 8 In one embodiment, the current collector 11 has a first end surface 111 and a second end surface 112 that are opposite to each other, and an active material layer 12 is disposed on the first end surface 111 and / or the second end surface 112 .

[0093] It can be understood that the first end face 111 and the second end face 112 are two faces in the thickness direction of the current collector 11, and the active material layer 12 can be selectively coated on the first end face 111; or, the active material layer 12 can be coated on the second end face 112; or, the active material layer 12 can be coated on both the first end face 111 and the second end face 112.

[0094] Corresponding to the bend of the current collector 11 , the first end surface 111 may be a convex surface protruding outward due to the bend, and the second end surface 112 may be a concave surface recessed inward due to the bend; or, the first end surface 111 is a concave surface, and the second end surface 112 is a convex surface.

[0095] Optionally, an active material layer 12 is coated on both the first end surface 111 and the second end surface 112 of the current collector 11 to increase the total mass of the active material.

[0096] Please refer to Figure 4 In one embodiment, the electrode sheet 10 is a positive electrode sheet 10a, which includes a positive electrode current collector and a positive electrode active material layer disposed on the positive electrode current collector. The positive electrode current collector has a first convex surface 1111 and a first concave surface 1112 at a bending portion, and a plurality of second coating areas 11b are formed on the first convex surface 1111 and / or the first concave surface 1112.

[0097] It can be understood that the first convex surface 1111 and the first concave surface 1112 are both surfaces of the positive electrode current collector, and after being bent by force, the surface of the positive electrode current collector forms a convex surface and a concave surface. Among them, the first convex surface 1111 is a structural surface that bulges outward due to bending, and the first concave surface 1112 is a structural surface that is concave inward due to bending.

[0098] Alternatively, a positive electrode active material layer may be coated on the first convex surface 1111; or, a positive electrode active material layer may be coated on the first concave surface 1112; or, a positive electrode active material layer may be coated on both the first convex surface 1111 and the first concave surface 1112. In this way, a plurality of second coating regions 11b may be formed on the first convex surface 1111; or, a plurality of second coating regions 11b may be formed on the first concave surface 1112; or, a plurality of second coating regions 11b may be formed on both the first convex surface 1111 and the first concave surface 1112.

[0099] With such arrangement, the positive electrode plate 10a can selectively form a plurality of second coating areas 11b on the first convex surface 1111, on the first concave surface 1112, and on the first convex surface 1111 and the first concave surface 1112 at the bending portion, so that the thickness of the positive electrode active material layer is reduced on the corresponding second coating areas 11b, thereby releasing more reserved space and reducing internal stress.

[0100] Please refer to Figure 4 In one embodiment, the electrode sheet 10 is a negative electrode sheet 10b, which includes a negative electrode current collector and a negative electrode active material layer disposed on the negative electrode current collector. The negative electrode current collector has a second convex surface 1121 and a second concave surface 1122 at a bending portion, and a plurality of second coating areas 11b are formed on the second convex surface 1121 and / or the second concave surface 1122.

[0101] It can be understood that the second convex surface 1121 and the second concave surface 1122 are both surfaces of the negative electrode current collector, and after being bent by force, the surface of the negative electrode current collector forms a convex surface and a concave surface. Among them, the second convex surface 1121 is a structural surface that bulges outward due to bending, and the second concave surface 1122 is a structural surface that is concave inward due to bending.

[0102] Alternatively, a negative electrode active material layer may be coated on the second convex surface 1121; or, a negative electrode active material layer may be coated on the second concave surface 1122; or, a negative electrode active material layer may be coated on both the second convex surface 1121 and the second concave surface 1122. In this way, a plurality of second coating regions 11b may be formed on the second convex surface 1121; or, a plurality of second coating regions 11b may be formed on the second concave surface 1122; or, a plurality of second coating regions 11b may be formed on both the second convex surface 1121 and the second concave surface 1122.

[0103] With such arrangement, the negative electrode plate 10b can selectively form a plurality of second coating areas 11b on the second convex surface 1121, on the second concave surface 1122, and on the second convex surface 1121 and the second concave surface 1122 at the bending portion, so that the thickness of the negative electrode active material layer is reduced on the corresponding second coating area 11b, thereby releasing more reserved space and reducing internal stress.

[0104] In a specific embodiment, taking the wound electrode assembly as an example, the positive electrode sheet 10a and the negative electrode sheet 10b are wound layer by layer from the inside to the outside, the first convex surface 1111 of the positive electrode collector corresponds to the second concave surface 1122 of the negative electrode collector, and the first concave surface 1112 of the positive electrode collector corresponds to the second convex surface 1121 of the negative electrode collector. At the same time, according to actual use needs, one or more second coating areas 11b are formed on any one or more of the first convex surface 1111, the first concave surface 1112, the second convex surface 1121, and the second concave surface 1122, so that the corresponding active material layer 12 can be thinned in thickness on the corresponding second coating area 11b.

[0105] For example, a plurality of second coating regions 11b are formed on the first convex surface 1111 of each positive electrode plate 10a at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Alternatively, a plurality of second coating regions 11b are formed on the first concave surface 1112 of each positive electrode plate 10a at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Alternatively, a plurality of second coating regions 11b are formed on both the first convex surface 1111 and the first concave surface 1112 of each positive electrode plate 10a at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region.

[0106] For example, a plurality of second coating regions 11b are formed on the second convex surface 1121 of each cathode electrode sheet 10 at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Alternatively, a plurality of second coating regions 11b are formed on the second concave surface 1122 of each cathode electrode sheet 10 at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Alternatively, a plurality of second coating regions 11b are formed on both the second convex surface 1121 and the second concave surface 1122 of each cathode electrode sheet 10 at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region.

[0107] For example, a plurality of second coating regions 11b are formed on the first convex surface 1111 of each positive electrode plate 10a at the bend, and a plurality of second coating regions 11b are formed on the second concave surface 1122 of each cathode electrode plate 10 at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Alternatively, a plurality of second coating regions 11b are formed on the first concave surface 1112 of each positive electrode plate 10a at the bend, and a plurality of second coating regions 11b are formed on the second convex surface 1121 of each cathode electrode plate 10 at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Alternatively, a plurality of second coating areas 11b are formed on the first convex surface 1111 and the first concave surface 1112 of each positive electrode plate 10a at the bend, and a plurality of second coating areas 11b are formed on the second convex surface 1121 and the second concave surface 1122 of each cathode electrode plate 10 at the bend, and each second coating area 11b is not coated with the active material layer 12, that is, is a blank area.

[0108] In one embodiment, at the bend, the anode capacity of the positive electrode active material layer is greater than the cathode capacity of the negative electrode active material layer.

[0109] In the electrode assembly 100, the ratio of the anode capacity to the cathode capacity on the opposite side is called the CB value (cell balance). Specifically, the CB value is equal to the ratio of the anode capacity per unit area to the cathode capacity per unit area, wherein the anode capacity is equal to the gram capacity of the anode active material multiplied by the anode coating weight multiplied by the loading of the anode active material; the cathode capacity is equal to the gram capacity of the cathode active material multiplied by the cathode coating weight multiplied by the loading of the cathode active material.

[0110] The essence of this is whether the lithium vacancies provided by the anode can receive the active lithium ions provided by the cathode when the battery is charged, so as to ensure that the active lithium does not precipitate at the anode. Generally, in order to reduce the risk of lithium precipitation, the CB value should be greater than 1. Therefore, the coating weight of the positive active material on the positive current collector should be greater than the coating weight of the negative active material on the negative current collector.

[0111] In one embodiment, when the thickness of the positive active material layer is equal to the thickness of the negative active material layer, the number of the second coating regions 11 b on the positive current collector is less than the number of the second coating regions 11 b on the negative current collector.

[0112] Here, the thickness of the positive active material layer on the positive current collector is equal to the thickness of the negative active material layer on the negative current collector, which means that the thickness of the positive active material layer on the first coating area 11a of the positive current collector is equal to the thickness of the negative active material layer on the first coating area 11a of the negative current collector, and the thickness of the positive active material layer on the second coating area 11b of the positive current collector is equal to the thickness of the negative active material layer on the second coating area 11b of the negative current collector. In this way, the thickness H of the active material layer 12 on the two current collectors 11 is equal.

[0113] When the number of the second coating areas 11b on the positive electrode current collector is less than the number of the second coating areas 11b on the negative electrode current collector, the total amount of the positive electrode active material coated on the positive electrode current collector is greater than the total amount of the negative electrode active material coated on the negative electrode current collector, thereby achieving a CB value greater than 1 and reducing the probability of lithium deposition at the anode.

[0114] Please refer to Figure 4 , Figure 8 and Fig.11 The present application provides a specific embodiment, the electrode assembly 100 includes a positive electrode sheet 10a and a negative electrode sheet 10b which are wound or stacked, and the positive electrode sheet 10a and the negative electrode sheet 10b are bent at multiple locations due to the winding or stacking. The positive electrode sheet 10a includes a positive electrode current collector and a positive electrode active material layer disposed on the positive electrode current collector, and the positive electrode current collector has a first convex surface 1111 and a first concave surface 1112 at the bend, and the negative electrode sheet 10b includes a negative electrode current collector and a negative electrode active material layer disposed on the negative electrode current collector, and the negative electrode current collector 11 has a second convex surface 1121 and a second concave surface 1122 at the bend. A plurality of second coating regions 11b are formed on the first convex surface 1111 of each positive electrode plate 10a at the bend, and a plurality of second coating regions 11b are formed on the second concave surface 1122 of each cathode electrode plate 10 at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Alternatively, a plurality of second coating regions 11b are formed on the first concave surface 1112 of each positive electrode plate 10a at the bend, and a plurality of second coating regions 11b are formed on the second convex surface 1121 of each cathode electrode plate 10 at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Alternatively, a plurality of second coating regions 11b are formed on the first convex surface 1111 and the first concave surface 1112 of each positive electrode sheet 10a at the bend, and a plurality of second coating regions 11b are formed on the second convex surface 1121 and the second concave surface 1122 of each cathode electrode sheet 10 at the bend, and each second coating region 11b is not coated with the active material layer 12, that is, a blank region. Also, when the thickness of the positive electrode active material layer is equal to the thickness of the negative electrode active material layer, the number of the second coating regions 11b on the positive electrode current collector is less than the number of the second coating regions 11b on the negative electrode current collector.

[0115] In a second aspect, the embodiment of the present application further provides a battery cell 3001 , comprising the above-mentioned electrode assembly 100 .

[0116] In a third aspect, an embodiment of the present application further provides a battery 3000 , comprising the above-mentioned battery cell 3001 .

[0117] In a fourth aspect, an embodiment of the present application further provides an electric device 10000, comprising the above-mentioned battery 3000.

[0118] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. An electrode assembly, comprising two pole pieces with opposite polarities which are wound or stacked, wherein the pole pieces are bent at multiple locations due to the winding or stacking, and the pole pieces comprise a current collector and an active material layer disposed on the current collector, characterized in that: The current collector includes a first coating area and a second coating area, wherein the second coating area is located at the bend, and the thickness of the active material layer coated in the second coating area is smaller than the thickness of the active material layer in the first coating area.

2. The electrode assembly according to claim 1, characterized in that: There are a plurality of second coating regions, and the second coating regions are spaced apart from each other along the length direction of the current collector.

3. The electrode assembly according to claim 1 or 2, characterized in that: The second coating region extends along a width direction of the current collector to separate the first coating region.

4. The electrode assembly according to claim 3, characterized in that: The thicknesses of the active material layers coated on at least two of the second coating regions are different.

5. The electrode assembly according to claim 3, characterized in that: The thickness of the active material layer coated on each of the second coating areas is equal.

6. The electrode assembly according to claim 5, characterized in that: Each of the second coating regions is not coated with the active material layer.

7. The electrode assembly according to claim 1, characterized in that: The current collector has a first end surface and a second end surface that are opposite to each other, and the active material layer is provided on the first end surface and / or the second end surface.

8. The electrode assembly according to claim 1, characterized in that: The electrode sheet is a positive electrode sheet, comprising a positive electrode current collector and a positive electrode active material layer disposed on the positive electrode current collector, the positive electrode current collector having a first convex surface and a first concave surface at the bending portion, and a plurality of the second coating areas are formed on the first convex surface and / or the first concave surface.

9. The electrode assembly according to claim 8, characterized in that: The electrode sheet is a negative electrode sheet, comprising a negative electrode current collector and a negative electrode active material layer disposed on the negative electrode current collector, the negative electrode current collector having a second convex surface and a second concave surface at the bending portion, and a plurality of second coating areas are formed on the second convex surface and / or the second concave surface.

10. The electrode assembly according to claim 9, characterized in that: At the bending portion, the anode capacity of the positive electrode active material layer is greater than the cathode capacity of the negative electrode active material layer.

11. The electrode assembly according to claim 10, characterized in that: When the thickness of the positive electrode active material layer is equal to the thickness of the negative electrode active material layer, the number of the second coating regions on the positive electrode collector is less than the number of the second coating regions on the negative electrode collector.

12. A battery cell, characterized in that: Comprising the electrode assembly according to any one of claims 1 to 11.

13. A battery, characterized in that: Comprising the battery cell according to claim 12.

14. An electrical equipment, characterized in that: Comprising the battery of claim 13.