Battery cell comprising a reinforced region and battery device comprising
By designing reinforced areas and support structures in the battery cell casing, the problem of insufficient durability of the battery cells under external impact is solved, achieving both strength and lightweight of the casing, and improving heat dissipation performance.
Patent Information
- Application Number
- CN202323303536.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Priority Date
- 2023-07-14
- Filing Date
- 2023-12-05
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2033-12-05
AI Technical Summary
Existing battery cells are prone to short-circuit under external impact, resulting in insufficient durability, and it is difficult to balance the strength of the casing in the pursuit of lightweighting.
A battery cell casing including a reinforced area is designed. The support area and the reinforced area are formed through the ironing process. Support rods and a reinforced cover with multiple protrusions and grooves are added to improve the strength and stability of the casing. Cooling space and thermal adhesive are provided in the battery unit to enhance overall performance.
It effectively improves the durability and heat dissipation performance of the battery cells, enhances the mechanical strength and structural stability of the casing, and reduces the risk of short circuits caused by external impacts.
Smart Images

Figure CN221861776U_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a battery cell including a reinforced region and a battery device including the battery cell. More specifically, the present disclosure relates to a battery cell and a battery device that improve the strength and stability of the battery cell and include a reinforced region. Background Art
[0002] A battery cell includes an electrode assembly and a housing that accommodates the electrode assembly. When an external impact (e.g., an impact from a vehicle collision) is transmitted to the battery cell, a short circuit may occur in the battery cell, and other events may occur due to the short circuit. In order to prevent the battery cell from being short-circuited due to an external collision, a battery cell structure that improves the durability of the battery cell is studied. Utility Model Content
[0003] A battery cell may include an electrode assembly and a shell that houses the electrode assembly. The shell is made of a can to protect the electrode assembly from external impact. The strength and weight of the shell need to be balanced. When the shell is made thinner to reduce the weight of the battery cell, the strength of the shell may be reduced. One aspect of the present disclosure is to provide a battery cell and a battery device including a reinforced area, so that the strength of the can can be effectively improved.
[0004] According to one aspect of the present disclosure, a battery cell includes: an electrode assembly; and a housing accommodating the electrode assembly. The housing includes a support region surrounding at least a portion of the electrode assembly and a reinforcement region disposed on the support region.
[0005] According to an embodiment, the supporting area may include an ironing area formed using an ironing process.
[0006] According to an embodiment, the reinforcement region may comprise at least one support rod arranged on the support region.
[0007] According to an embodiment, the reinforcement region may be disposed on the support region and include a reinforcement cover having a plurality of protrusions and a plurality of grooves.
[0008] According to an embodiment, the housing may include a wide surface, a narrow surface, and a corner portion between the wide surface and the narrow surface. The reinforcement area may be provided on at least one of the wide surface, the narrow surface, and the corner portion.
[0009] According to an embodiment of the present invention, a battery device includes: a cell assembly including a plurality of battery cells; and a housing accommodating the cell assembly. Each of the plurality of battery cells may include an electrode assembly and a housing accommodating the electrode assembly, and the housing may include a support area surrounding at least a portion of the electrode assembly and a reinforcement area disposed on the support area. The cell assembly may include a heat dissipation space located between the support areas of the plurality of battery cells.
[0010] According to an embodiment of the present invention, the support area may include an ironing area formed using an ironing process. A first thickness of the ironing area may be smaller than a second thickness of the reinforcement area.
[0011] According to embodiments herein, the reinforcement region may include at least one support rod connected to the support region.
[0012] According to embodiments herein, the reinforcement region may be connected to the support region and may include a reinforcement cover having a plurality of protrusions and a plurality of grooves.
[0013] According to an embodiment of this document, the battery device may further include: a heat dissipation member attached to the support area and located within the heat dissipation space.
[0014] According to the embodiments of the present invention, the battery device may further include: a thermal adhesive connecting the battery cell assembly and the housing.
[0015] According to an embodiment of this document, the reinforcement region may include a first protrusion extending from an outer surface of the support region in the first direction and a second protrusion extending from the outer surface of the support region in the first direction.
[0016] According to an embodiment, the reinforcement area may include a third protrusion extending from a first end of a first outer surface of the support area in a first direction and a fourth protrusion extending from a second end of a second outer surface of the support area in a second direction opposite to the first direction. The third protrusion may be located at a first end of the housing, and the fourth protrusion may be located at a second end of the housing opposite to the first end.
[0017] According to an embodiment, the reinforcement region may include a plurality of fifth protrusions extending from the first outer surface of the support region in a first direction; and a plurality of sixth protrusions extending from the second outer surface of the support region in a second direction opposite to the first direction.
[0018] According to an embodiment, the reinforcement region may include: a seventh protrusion including an insertion portion; and an eighth protrusion in which a groove for receiving the insertion portion is formed. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] The above and other aspects, features and advantages of the present disclosure will be more clearly understood through the following detailed description in conjunction with the accompanying drawings:
[0020] Figure 1 is an exploded perspective view of a battery cell according to an embodiment;
[0021] Figure 2A , Figure 2B and Figure 2C is a view for illustrating an upper cover assembly according to an embodiment;
[0022] FIG. 3A to FIG. 3Fis a view for illustrating an assembling process of an upper cover assembly and an electrode assembly according to an embodiment;
[0023] 4A to 4F is a view for illustrating an assembly process of an electrode assembly, a jelly roll bag, and a can according to an embodiment;
[0024] Figure 5A and Figure 5B is a diagram showing a squeeze test of a square battery cell;
[0025] Figure 6 is a diagram showing a manufacturing process of a battery cell according to an embodiment;
[0026] Fig. 7A and Figure 7B is a view showing an impact extrusion process according to an embodiment;
[0027] Fig. 8A and Figure 8B is a diagram illustrating an ironing process according to an embodiment;
[0028] 9A to 9E is a view showing a can to which an ironing process is applied according to various embodiments;
[0029] FIG. 10A to FIG. 10F is a view showing a tank including a support rod according to various embodiments;
[0030] FIG. 11A to FIG. 11E is a view showing a can including a reinforced cover according to various embodiments;
[0031] Fig. 12A is a top view of a battery device according to an embodiment;
[0032] Fig. 12B is along Fig. 12A The cross-sectional view of the C-C' line;
[0033] Fig.13 is a top view of a battery device according to an embodiment;
[0034] Fig.14 is a top view of a battery cell according to an embodiment;
[0035] Fig.15A is a top view of a battery cell according to an embodiment;
[0036] Fig. 15B is a perspective view of a battery cell assembly according to an embodiment. DETAILED DESCRIPTION
[0037] Embodiments of the present disclosure will be described more fully below with reference to the accompanying drawings, and embodiments are shown, in which like symbols represent like elements throughout the drawings. However, the embodiments of the claims may be implemented in a variety of different forms and are not limited to the embodiments described herein. The examples given herein are non-limiting and are merely examples among other possible examples.
[0038] Figure 1 is an exploded perspective view of a battery cell according to an embodiment.
[0039] Reference Figure 1, the battery cell 100 may be a square battery cell. Square battery cells are widely used in the power system of electric vehicles. Square battery cells can be stacked together in a rectangular shape, allowing for more efficient use of space. Square battery cells are generally rectangular and have a higher power density than cylindrical battery cells. Square battery cells also provide better performance in cold weather and are less damaged by vibration. However, square battery cells may be more expensive to manufacture than cylindrical battery cells. In addition, square battery cells are less likely to fail due to vibration or movement. Due to the space optimization of the rectangular shape of the square battery cell, the square battery cell can deliver more power than the cylindrical battery cell. The square battery cell 100 includes a rectangular can 104, which can be formed of steel, aluminum, aluminum alloy, plastic, or other metal with sufficient structural strength. The can 104 can be manufactured according to a variety of different methods including deep drawing or impact extrusion. The method for manufacturing the can 104 can be combined with wall ironing to achieve the final geometry, thickness, and tolerance. The can 104 can be wrapped with a cell covering tape. The jelly roll 106 includes a stacked anode, a cathode and a separator. The jelly roll (electrode assembly) 106 is wound, and the jelly roll (electrode assembly) 106 is configured to have a structure with a long sheet cathode and a long sheet anode coated with an active material. At the same time, the stacked electrode assembly has a structure in which the separator is arranged between the cathode and the anode, or has a structure in which a plurality of cathodes and anodes with predetermined sizes are stacked sequentially and the separator is arranged between each cathode and anode. Compared with the sheet electrode assembly, the jelly roll (electrode assembly) 106 is easy to manufacture and has a high unit mass and energy density. In some batteries, one or more jelly rolls 106 are inserted into the can 104. Each jelly roll (electrode assembly) 106 is included in a polymer jelly roll bag 108 sealed inside the can 104. Each jelly roll 106 includes a cathode foil 112 formed of aluminum. The aluminum foil is coated with an electrode slurry. The first operation of electrode manufacturing is the slurry mixing process, which combines the active raw materials with binders, solvents and additives. The anode slurry and the cathode slurry should undergo this mixing process separately. The viscosity, density, solid content and other measurable properties of the slurry affect the battery quality and electrode uniformity. For example, when the solvent content is high, a slurry with a faster drying rate, a higher solid content, low-speed performance and low viscosity is generated. Then, the cathode slurry is applied to the aluminum foil and dried. A slot die coater is a method of coating a foil in which the slurry is diffused through a slit gap on a moving foil receiving the tension on a roller. In some embodiments, this can be done simultaneously on both sides of the foil. This production method enables high-speed production while achieving accuracy in coating thickness. The drying process can be incorporated into continuous coating. The drying process should achieve three purposes: diffusion of binders, sedimentation of particles and evaporation of solvents.Air flotation is a method of drying the slurry on the foil. The uniformity of the electrode coating and the drying process affects the safety, consistency and life cycle of the square battery cell 100. The electrode should undergo a calendering process to control the electrode porosity and twist by compressing the coated electrode sheet to a uniform thickness and density. Each jelly roll 106 includes an anode foil 110 formed of a copper foil. The anode foil 110 is arranged similarly to the cathode foil 112. Each jelly roll 106 may include a cathode connector (not shown) that forms an electrical connection between the inner end portion of the cathode foil 112 and the cathode terminal 128. Each jelly roll 106 may include an anode connector (not shown) that forms an electrical connection between the inner end portion of the anode foil 110 and the anode terminal 126. Each jelly roll 106 may include a cathode connector mask (e.g. Figure 3C Cathode connector mask 118 in.
[0040] Each square battery cell 100 may have an upper cover assembly 120 welded or otherwise bonded to the top of the can 104. The upper cover assembly 120 may include a substrate 122 attached to the can 104. The substrate 122 isolates the inside and outside of the battery cell by welding with the can 104. The substrate 122 may serve as a rigid support structure for the elements within the upper cover assembly 120. The upper cover assembly 120 may include a plurality of upper insulators 124 to insulate the substrate 122. The upper insulator 124 may prevent electrolyte leakage from the square battery cell 100. In addition, the upper insulator 124 may isolate the can 104 from the cathode foil 112 and prevent moisture and gas from penetrating from the outside of the battery cell. A portion of the upper insulator 124 may protect the current interruption device. The upper cover assembly 120 includes a cathode terminal 128 electrically connecting the inside and outside of the square battery cell 100. The upper cover assembly 120 includes an anode terminal 126 electrically connecting the inside and outside of the square battery cell 100.
[0041] The upper cover assembly 120 may include a vent 130 that allows exhaust gas from the square battery cell 100 to be discharged in a controllable direction and at a controllable pressure. The upper cover assembly 120 may include a vent guard 132 that protects the vent 130 from the inside of the square battery cell 100 to prevent the vent 130 from malfunctioning. The upper cover assembly 120 may include an overcharge safety device 134 that prevents the introduction of external current using the internal gas pressure of the square battery cell 100. The upper insulator 124 may be multi-component. In some embodiments, the side of the upper insulator 124 may be mounted on the edge of the tank 104 and the upper cover assembly 120. The electrolyte cover 138 may seal the electrolyte solution inside the square battery cell 100.
[0042] The battery cell 100 may include an insulator 136 located between the upper cover assembly 120 and the can 104 .
[0043] Herein, the electrode assembly of the battery cell 100 is described as a jelly roll 106, but the electrode assembly of the battery cell 100 is not limited to the jelly roll 106. For example, the jelly roll 106 may be replaced by a stacked electrode assembly or a Z-folded electrode assembly. According to an embodiment, the jelly roll 106 described herein may refer to an electrode assembly.
[0044] In this document, the tank 104 may be referred to as a housing.
[0045] Figure 2A , 2B 2C illustrate the construction and component functions of the upper cover assembly 120. For example, Figure 2A is an exploded perspective view of an upper cover assembly 120 according to a disclosed embodiment. Figure 2B 1 is a rear perspective view of the upper cover assembly 120 according to an embodiment of the present disclosure. Figure 1 The description of the upper cover assembly 120 can be applied to Figure 2A , 2B and the upper cover assembly of 2C.
[0046] The upper cover assembly 120 serving as a cover of the square battery cell 100 is a complex assembly including a plurality of welded assemblies. An adhesive may be used instead of welding certain components.
[0047] The prismatic battery cell 100 may include a vent 130. The vent 130 provides overpressure relief when the temperature and corresponding pressure in the prismatic battery cell 100 increases. For example, the vent 130 may be activated within a pressure range of 10 to 15 bar. The vent 130 may be laser welded to the upper cover assembly 120.
[0048] The square battery cell 100 may include a tank 104. The tank 104 may typically be formed of deep drawn aluminum or stainless steel to prevent moisture from entering the battery cell while providing diffusion resistance to organic solvents such as liquid electrolytes. The most important reason why the tank 104 is typically formed of deep drawn aluminum alloy or stainless steel is to reduce welding points to improve the mechanical strength of the tank 104. The electrolyte may be filled in the square battery cell 100. After the electrolyte is filled, the electrolyte cover 138 may be welded to the upper cover assembly 120, or a locking ball (not shown) may be pressed into the opening of the electrolyte cover 138. The battery cell may have an overcharge safety device 134 that may disconnect the current when a high internal pressure is reached in the square battery cell 100. The pressure increase is typically caused by high temperature.
[0049] According to an embodiment, the cathode terminal 128 may be provided in plurality. For example, the cathode terminal 128 may include a first cathode terminal 128a and a second cathode terminal 128b, at least a portion of the first cathode terminal 128a is exposed to the outside of the battery cell 100, and the second cathode terminal 128b is connected to the cathode foil (e.g. Figure 1 The second cathode terminal 128b may be electrically connected to the first cathode terminal 128a. For example, a portion of the second cathode terminal 128b may contact the first cathode terminal 128a.
[0050] According to an embodiment, the anode terminal 126 may be provided in plurality. For example, the anode terminal 126 may include a first anode terminal 126a and a second anode terminal 126b, wherein at least a portion of the first anode terminal 126a is exposed to the outside of the battery cell 100, and the second anode terminal 126b is connected to the anode foil (e.g. Figure 1 The second anode terminal 126b may be electrically connected to the first anode terminal 126a. For example, a portion of the second anode terminal 126b may contact the first anode terminal 126a.
[0051] Figures 3A to 3F 3 is a view showing an assembly process of an upper cover assembly and an electrode assembly according to an embodiment. The battery cell manufacturing process 300 may include an assembly process of an upper cover assembly 120 and a jelly roll 106 .
[0052] Reference Figure 3A , a sealing tape 106a may be attached to the jelly roll 106. According to an embodiment, the sealing tape 106a may cover at least a portion of the jelly roll 106. According to an embodiment, the sealing tape 106a may seal a portion of the jelly roll 106.
[0053] Reference Figure 3B , the jelly roll 106 can be connected to the upper cover assembly 120. For example, a connection assembly for connecting the jelly roll 106 and the upper cover assembly 120 can be prepared. The upper cover assembly 120 can be tightly attached to the jelly roll 106 using the connection assembly. For example, the cathode terminal 128 of the upper cover assembly 120 can be connected to the cathode foil 112 of the jelly roll 106, and the anode terminal 126 of the upper cover assembly can be connected to the anode foil 110 of the jelly roll 106. The cathode terminal 128 can be welded to the cathode foil 112, and the anode terminal 126 can be welded (e.g., ultrasonically welded) to the anode foil 110.
[0054] Reference Figure 3C, at least a portion of the cathode terminal 128 may be masked. For example, the cathode connector mask 118 may be provided to cover a portion of the cathode terminal 128. The cathode connector mask 118 may protect the cathode terminal 128. Although not shown, the description of the mask of the cathode terminal 128 may also be applied to the anode terminal 126.
[0055] Reference Figure 3D and / or Figure 3E , the tape may be attached to at least a portion of the cathode terminal 128 and the anode terminal 126. For example, the battery cell 100 may include welding tapes 118a, 118b, 118c, and 118d attached to at least a portion of the cathode terminal 128, the anode terminal 126, the cathode foil 112, and / or the anode foil 110. According to an embodiment, the welding tapes 118a, 118b, 118c, and 118d may be attached to at least a portion of the joint portion of the cathode terminal 128, the anode terminal 126, the cathode foil 112, and / or the anode foil 110. Since the joint portion is covered by the welding tapes 118a, 118b, 118c, and 118d, the cathode terminal 128 and the anode terminal 126 may be protected.
[0056] Reference Figure 3F , the anode foil 110 connected to the anode terminal 126 may be folded. For example, when the upper cover assembly 120 is disposed on the jelly roll 106, at least a portion of the anode foil 110 may be folded. Although not shown, when the upper cover assembly 120 is placed on the jelly roll 106, the cathode foil 112 may also be folded.
[0057] Figures 4A to 4F 4 is a diagram showing an assembly process of an electrode assembly, a jelly roll bag, and a can. The battery cell manufacturing process 400 may include an assembly process of a jelly roll 106 , a jelly roll bag 108 , and a can 104 .
[0058] Reference Figure 4A , the insulator 136 may be mounted on the battery cell 100. For example, the insulator 136 may be disposed between the can 104 and the upper cover assembly 120.
[0059] Reference Figure 4B , a jelly roll bag 108 may be prepared. The jelly roll bag 108 may cover at least a portion (e.g., a side surface) of the jelly roll 106. The jelly roll 106 may be surrounded by the jelly roll bag 108. The jelly roll bag 108 may protect the jelly roll 106 from external impact. Figure 4B , a structure in which the jelly roll bag 108 is disposed on both side surfaces of the jelly roll 106 is shown, but the structure of the jelly roll bag 108 is not limited thereto. For example, according to an embodiment, the jelly roll bag 108 may be formed to cover four side surfaces of the jelly roll 106.
[0060] Reference Figure 4C , the insulator 108a may be attached to the jelly roll 106. According to an embodiment, in a state where the jelly roll bag 108 is unfolded, the insulator 108a may be attached to a lower portion of the jelly roll 106. The insulator 108a may be referred to as a lower insulator.
[0061] Reference Figure 4D , at least some components of the battery cell 100 may be taped. For example, the battery cell 100 may include the upper cover assembly 120, the can 104, and / or at least one first tape 108b attached to the insulator 136 and / or a second tape 108c attached to the lower portion of the jelly roll bag 108 along the side of the insulator 136.
[0062] Reference Figure 4E , jelly roll 106 can be inserted into jar 104. Jelly roll 106 and / or jelly roll bag 108 can be inserted into jar 104.
[0063] According to an embodiment, the battery cell manufacturing process 400 may include a wetting process of the jelly roll 106. For example, the jelly roll 106 may be initially wetted with an electrolyte delivered by an electrolyte injection port. For example, a partial vacuum may be formed in the square battery cell 100, and a predetermined amount of electrolyte may be injected through the electrolyte injection port. The partial vacuum may improve the distribution and wetting of all layers within the jelly roll 106. Wetting all layers within the jelly roll 106 may require a rolling or rotating method to enhance the wetting effect.
[0064] According to an embodiment, the battery cell manufacturing process 400 may include a quality inspection process for an initial wetting process, such as checking the weight of the square battery cell 100 immediately after charging. For example, a second electrolyte charging operation of charging the electrolyte to achieve a desired weight may be applied to the battery cell. According to an embodiment, the battery cell manufacturing process 400 may include a pre-forming process of charging the square battery cell 100 and discharging the gas.
[0065] Reference Figure 4F , the electrolyte injection port can be sealed. For example, the electrolyte cover 138 can be inserted into the electrolyte injection port.
[0066] Figure 5A and Figure 5B is a diagram showing a crush test of a square battery cell.
[0067] For example, Figure 5A A battery cell 100 and a vertical compression test tool 500 are shown. As an example, it can be selectively applied Figure 5A The vertical squeeze test tool 500 is shown in FIG. Figure 5AThe positional relationship between the prismatic battery cell 100 and the vertical crush test tool 500 during the vertical crush test is shown.
[0068] Figure 5B A first squeeze test direction (eg, vertical squeeze test direction) 502, a second squeeze test direction (eg, narrow vertical squeeze test direction) 504, and a third squeeze test direction (eg, horizontal squeeze test direction) 506 are shown, in which the squeeze strength of the battery cell 100 can be evaluated according to various standards.
[0069] In an embodiment, the battery cell 100 can be subjected to pressure or force in a first extrusion test direction 502, a second vertical extrusion test direction 504, and / or a third extrusion test direction 506 using a vertical extrusion test tool 500, and the extrusion strength is evaluated. For example, the requirements for extrusion strength in the "UL Standard for Safety Batteries for Electric Vehicles, UL 2580, Third Edition, April 1, 2020" are disclosed as follows. "These standards evaluate the ability of energy storage components to safely withstand simulated abuse conditions and prevent abuse from causing harm to personnel." UN ECE R100 Rev2 is an important regulation of the United Nations (UN) in Europe. The regulation specifies all tests that should be performed on lithium batteries installed on four-wheel electric vehicles for transporting people or goods on M and N roads using electric traction. Two of these standards include mechanical integrity tests to verify the tolerance of rechargeable energy storage systems (REESS) to contact loads that may occur during vehicle collisions. In the positive or negative direction or in both directions, a compression of 100KN is carried out using a compression plate with a radius of 75mm and a mechanical shock test of a maximum of 28G for 80 milliseconds depending on the vehicle class. The mechanical shock test is generally carried out on a sled test machine.
[0070] Figure 6 is a view for illustrating the impact extrusion process of forming a shell of a square battery cell according to an embodiment. For example, Figure 6 Five stages of the impact extrusion manufacturing process for converting an aluminum block 600 into the can 104 of the prismatic battery cell 100 are shown.
[0071] The first stage is an aluminum block 600. The aluminum block 600 may be extruded and transformed into a first workpiece 602.
[0072] The first workpiece 602 may be stretched into the second workpiece 604 by ironing. At least a portion of the second workpiece 604 may be cut and transformed into the third workpiece 606. The third workpiece 606 may be trimmed and polished to reach the final state of the can 104. For example, unintended protrusions formed on the surface of the third workpiece 606 may be removed. The first workpiece 602, the second workpiece 604, and the third workpiece 606 may be formed in the process of processing the aluminum block 600 into the can 104. In an embodiment, the first workpiece 602, the second workpiece 604, and the third workpiece 606 may be referred to as a first level, a second level, and a third level, respectively.
[0073] exist Figure 6 In the embodiment of the present invention, the can 104 made of aluminum is described, but the material of the can 104 is not limited thereto. For example, the can 104 may include other metals (eg, titanium).
[0074] Fig. 7A and Figure 7B is a view for illustrating the impact extrusion process according to an embodiment. For example, Fig. 7A and Figure 7B Two cross sections of the impact extrusion process are shown. Aluminum block 600 can be placed between mandrel 700 and drive wedge 702. Typically using a pneumatic or hydraulic press, drive wedge 702 can be moved in the direction of the arrow until it reaches Figure 7B When the driving wedge 702 reaches Figure 7B When in the position shown, the aluminum block 600 can be formed into a workpiece (e.g. Figure 6 The first workpiece 602 in the embodiment of the present invention is used to produce the can 104 of the square battery cell 100. The size and shape of the mandrel 700 and / or the driving wedge 702 can be selectively designed. For example, the length of the mandrel 700 can be changed according to the final shape of the square battery cell 100.
[0075] Fig. 8A and Figure 8B is a diagram for illustrating an ironing process according to an embodiment.
[0076] In an embodiment, the can 104 can be further formed by ironing after the impact extrusion process. Fig. 7A and 7B The second workpiece 604 manufactured by the impact extrusion process is further subjected to an ironing process.
[0077] The ironing process may refer to using the iron 800 to iron the first workpiece (eg, Figure 7B The process of applying pressure to the first workpiece 602 in the second workpiece 604a to change the shape of the first workpiece 602. For example, the thickness of at least a portion of the second workpieces 604a and 604b may be different from the thickness of the first workpiece 602.
[0078] The iron 800 can apply pressure to the can 104 to stretch the material in a given direction, thereby producing a thinner, larger, and more uniform can 104. In an embodiment, the inner mold 806 can be disposed inside the can 104, and the iron 800 can apply pressure to the can 104 outside the can 104. The second workpiece 604b shows the unironed portion of the square battery can 104. Fig. 8A and Figure 8B , the iron 800 can be moved from the lower portion of the can 104 to the upper portion. The iron 800 can deform the can 104 by lifting the material of the second workpieces 604a and 604b. For example, the iron 800 can produce an ironed portion of the square battery can 104 shown in the second workpiece 604b. The thickness and / or shape of at least a portion of the can 104 can be deformed during the ironing process.
[0079] 9A to 9E is a view of a can for illustrating application of an ironing process according to various embodiments. The strength and / or rigidity of the can 104 of the battery cell 100 may be improved using an ironing (eg, wall ironing) process. 9A to 9E The tank 104 can be used Fig. 8A and Figure 8B The ironing process is used to manufacture the can 104. Figure 1 The battery cell 100.
[0080] Reference 9A to 9E , the tank 104 may include at least one of the ironing regions 910a, 910b, and 910c and the reinforcement regions 1010a, 1010b, and 1010c. The thickness of the ironing regions 910a, 910b, and 910c may be different from the thickness of the reinforcement regions 1010a, 1010b, and 1010c. For example, the second thickness w2 of the second reinforcement region 1010b may be greater than the first thickness w1 of the second ironing region 910b.
[0081] Reference Fig. 9A and Fig. 9B , the tank 104 may include a first ironing area 910a formed by three irons 800 equally spaced apart on a vertical side surface of the tank 104. For example, the tank 104 may include at least one ironing area 910a in a vertical direction.
[0082] For example, when the iron 800 moves upward and downward or moves from the lower part to the upper part, the iron 800 may form an ironing area 910a on the surface of the tank 104. Other portions of the tank 104 where the ironing area 910a is not formed may be referred to as a reinforcement area 1010a. Fig. 9B), the can 104 may include four reinforcement areas 1010a and three vertical ironing areas 910a having a thickness thinner than the reinforcement areas 1010a. In an embodiment, the thickness of the vertical ironing areas 910a may be substantially the same as the normal thickness of the can 104 of the square battery cell formed by the currently known impact extrusion process. Therefore, the thickness of the reinforcement area (e.g., the first reinforcement area 1010a) may be greater than the thickness of the can 104 of the square battery cell 100. In an embodiment, the first reinforcement area 1010a may be referred to as a vertical rail or rail portion.
[0083] According to an embodiment, the tank 104 may include a Fig. 11C wide surface 1020c) and narrow surface (e.g. Fig. 11C The reinforced areas 1010a, 1010b, and 1010c may be disposed or formed on at least one of the wide surface 1020c, the narrow surface 1020d, and the corner.
[0084] In an embodiment, a reinforced area 1010a may be formed at the corner of the can 104 of the square battery cell 100 through an ironing process. The ironing process may make the corner material of the square battery cell can 104 thicker, thereby improving the structural strength. Since the ironing process increases the thickness of the corner of the can 104, the structural strength of the can 104 may be improved.
[0085] The ironing regions 910a, 910b, and 910c may be formed on the inner surface and / or outer surface of the can 104. In an embodiment, the first ironing region 910a may be formed on the outer surface of the can 104. For example, the iron 800 and the inner mold (e.g., Figure 8B The inner mold 806 in the embodiment forms a first ironing area 910a on the outer surface of the can 104. According to an embodiment (not shown), the first ironing area 910a may be formed on the inner surface of the can 104. For example, during the ironing process, an outer mold (not shown) surrounding the outer surface of the can 104 and an iron pressing the inner surface of the can 104 may be used.
[0086] At least part of the description of the first ironing area 910a and the first reinforcement area 1010a may apply to the second ironing area 910b (eg, horizontal ironing area), the third ironing area 910c (eg, oblique ironing area), the horizontal support area 1010b and / or the oblique support area 1010c.
[0087] Reference Fig. 9C and Fig.9D , the tank 104 may include a second ironing area 910b formed by three irons 800 spaced evenly apart on the horizontal side surface of the tank 104. For example, when the iron 800 moves from left to right or from left to right, a second ironing area 910b may be formed. Fig. 9C and Fig.9D The four horizontal supporting areas 1010b shown in FIG. 1 are thinner than the three horizontal ironing areas 910b.
[0088] According to the embodiments (e.g. Fig.9E ), the tank 104 may include an oblique ironing area 910c and an oblique support area 1010c. For example, when a pair of irons 800 move parallel to each other, an oblique support area 1010c passing through the center of the tank 104 may be formed.
[0089] 9A to 9E The shape of the tank 104 shown is exemplary. For example, in the case of a structure for improving the strength of the tank 104, the number and / or shape of the ironing areas 910a, 910b and 910c and / or the reinforcing areas 1010a, 1010b and 1010c are not limited.
[0090] FIG. 10A to FIG. 10F 920a, 920b, and 920c are views for illustrating a can including support bars according to various embodiments. The strength and / or rigidity of the battery cell 100 may be improved by the support bars 920a, 920b, and 920c.
[0091] According to the embodiments (e.g. Fig. 10A and / or Fig. 10B ), the tank 104 may include four first support rods 920a. The first support rods 920a may be referred to as vertical support rods. The first support rods 920a may be disposed on the support region 1020 of the tank 104. The structural strength of the tank 104 may be improved by the first support rods 920a. For example, the support region 1020 has the shape of a common tank 104, and the thickness of the tank 104 is increased by the support rods 920, thereby improving the structural strength of the tank 104. In an embodiment, the support rods 920 may be coupled to the support region 1020 of the tank 104 using an adhesive or welding.
[0092] According to the embodiments (e.g. Fig. 10B ), the tank 104 may include a plurality of first support rods 920a welded to a support region 1020. The plurality of first support rods 920a may be arranged substantially in parallel. The support region 1020 may be an aluminum plate. In an embodiment, the support region 1020 may be referred to as a support plate. In this article, the description of the first support rod 920a may be applied to the second support rod 920b and the third support rod 920c.
[0093] According to an embodiment, the support area 1020 to which the first support rod 920a is attached may be formed integrally with the tank 104. According to an embodiment, the support area 1020 to which the first support rod 920a is attached may be formed as a separate component from the tank 104. For example, the support area 1020 may be manufactured in the shape of a support plate and welded or attached to the tank 104.
[0094] According to the embodiments (e.g. Fig. 10C ), the tank 104 may include a second support rod 920b. The second support rod 920b may be referred to as a horizontal support rod. For example, the tank 104 may include a plurality of second support rods 920b extending parallel to each other in a horizontal direction.
[0095] According to an embodiment (not shown), the tank 104 may include a first support rod 920a and a second support rod 920b. For example, the tank 104 may include a support rod having a checkerboard pattern. A support rod having a checkerboard pattern refers to a support rod having a shape that allows the first support rod 920a and the second support rod 920b to be combined or formed into one body.
[0096] According to the embodiments (e.g. FIG. 10D to FIG. 10F ), the tank 104 may include a third support rod 920c. The third support rod 920c may be referred to as a cross-type support rod. The third support rod 920c may include a plurality (e.g., two) of the third support rods arranged substantially vertically. In an embodiment, at least a portion of the third support rod 920c may be disposed on the center portion of the tank 104.
[0097] According to an embodiment, the third support bar 920c may be coupled to the support region 1020. For example, the third support bar 920c may be connected to the support region 1020 using welding.
[0098] Herein, the support rod 920 is connected to the inner surface of the tank 104 and / or the support area 1020, but the position of the support rod 920 is not limited thereto. For example, in an embodiment not shown, the support rod 920 can be connected to the outer surface of the tank 104 and / or the support area 1020.
[0099] In an embodiment, the support region 1020 and / or the support rods 920a, 920b, and 920c may include aluminum. For example, the support rods 920a, 920b, and 920c may be formed of aluminum, as may the tank 104 and / or the support region 1020. In an embodiment, the support rods 920a, 920b, and 920c, the tank 104, and / or the support region 1020 may include titanium.
[0100] According to an embodiment, the support rods 920 a , 920 b , 920 c may be disposed on the inner surface and / or the outer surface of the tank 104 .
[0101] According to an embodiment, FIG. 10A to FIG. 10F At least a portion of the support rods 920a, 920b, and 920c in the embodiment may be connected to the previously described reinforcement area (e.g. 9A to 9E Used together with at least a portion of the reinforced areas 1010a, 1010b and 1010c).
[0102] FIG. 11A to FIG. 11E 2 is a view for illustrating a can including a reinforced cover according to various embodiments.
[0103] Reference FIG. 11A to FIG. 11E , the tank 104 may include a support area 1020 and a reinforcement cover 930. Fig. 10A The description of the tank 104 and / or support area 1020 in the embodiment of the present invention may be applied to FIG. 11A to FIG. 11E tank 104 and / or support area 1020.
[0104] The reinforcement covers 930a, 930b, 930c, and 930d may include a plurality of protrusions and a plurality of grooves. For example, the reinforcement covers 930a, 930b, 930c, and 930d may have a corrugated shape. According to an embodiment, the reinforcement covers 930a, 930b, 930c, and 930d may be referred to as corrugated reinforcements. According to an embodiment, the reinforcement covers 930a, 930b, 930c, and 930d may be formed using an extrusion process (e.g., Fig. 7A and 7B impact extrusion process).
[0105] The positions of the reinforcement covers 930a, 930b, 930c and 930d formed on the tank 104 may be selectively designed. Fig.11A ), the tank 104 may include a first reinforcing cover 930a arranged transversely. In an embodiment, the first reinforcing cover 930a may be formed on the inner surface of the plates 1020a and 1020b of the tank 104. The plates 1020a and 1020b of the tank 104 may include aluminum. The reinforcing cover 930 may be formed by extruding from the plates 1020a and 1020b. In an embodiment, the plates 1020a and 1020b may be at least a portion of the support area 1020 of the tank 104. For example, the plates 1020a and 1020b may be a portion of the wide surface 1020c of the tank 104 forming the tank 104. In an embodiment, the plates 1020a and 1020b may be independent components attached to the support area 1020 of the tank 104. The first reinforcing cover 930a and the second reinforcing cover 930b may be respectively disposed between the plates 1020a and 1020b connected to the tank 104.
[0106] According to an embodiment, the reinforcing cap 930 may include aluminum. Like the tank 104 or the plates 1020a and 1020b, the reinforcing cap 930 may be made of aluminum. According to an embodiment, the reinforcing cap 930 may be made of other materials, such as titanium, to increase the strength of the tank 104 or reduce the weight of the tank 104.
[0107] The shape of the tank 104 and / or the shape of the first reinforcing cover 930a may be selectively designed. Fig.11A), the first reinforcement cover 930a may extend horizontally. According to an embodiment (eg Fig. 11B ), the first reinforcement cover 930a may extend vertically.
[0108] At least a portion of the description of the first reinforcement cover 930a may be applied to the second reinforcement cover 930b, the third reinforcement cover 930c, and / or the fourth reinforcement cover 940d.
[0109] According to the embodiments (e.g. Fig. 11C ), the tank 104 may include a second reinforcement cover 930b disposed on the wide surface 1020c. The wide surface 1020c may be referred to as a relatively long side surface of the tank 104. The second reinforcement cover 930b may cover at least a portion of the wide surface 1020c of the tank 104. The second reinforcement cover 930b may prevent the wide surface 1020c of the tank 104 from being bent or damaged. According to an embodiment, the second reinforcement cover 930b may be formed in a vertical direction.
[0110] According to the embodiments (e.g. Fig.11D ), the tank 104 may include a third reinforcement cover 930c disposed on the narrow surface 1020d. The narrow surface 1020d may be referred to as a relatively short side surface of the tank 104. The third reinforcement cover 930c may cover at least a portion of the narrow surface 1020d of the tank 104. The third reinforcement cover 930c may prevent the narrow surface 1020d of the tank 104 from being bent or damaged. According to an embodiment, the third reinforcement cover 930c may be formed in a vertical direction.
[0111] According to an embodiment (not shown), the can 104 may include a reinforced cover covering the wide surface 1020c and the narrow surface 1020d.
[0112] According to an embodiment (not shown), the tank 104 may include a reinforced cover located on the floor of the tank 104 .
[0113] According to the embodiments (e.g. Fig.11E ), the tank 104 may include a fourth reinforcement cover 930d disposed on the wide surface 1020c of the tank 104. The fourth reinforcement cover 930d may include a corrugated reinforcement extending obliquely relative to the extension direction of the wide surface 1020c of the tank 104. The fourth reinforcement cover 930d may contact not only the side surface of the tank 104 but also the upper and lower parts of the tank 104. Due to the inclined arrangement of the fourth reinforcement cover 930d, the stability of the tank 104 may be improved.
[0114] According to an embodiment, the reinforcement covers 930 a , 930 b , and 930 c may be provided on the inner surface and / or the outer surface of the can 104 .
[0115] According to an embodiment, FIG. 11A to FIG. 11EAt least a portion of the reinforcement covers 930a, 930b, and 930c may be connected to the reinforcement area (eg, 9A to 9E The reinforced regions 1010a, 1010b and 1010c and / or FIG. 10A to FIG. 10F These reinforcement areas are used together with at least a portion of the support rods 920a, 920b and 920c), and these reinforcement areas have been described previously.
[0116] Fig. 12A is a top view of a battery device according to an embodiment. Fig. 12B is along Fig. 12A Cross-sectional view of the C-C' line. Fig.13 is a top view of a battery device according to an embodiment. Fig.14 is a top view of a battery cell according to an embodiment. Fig.15A is a top view of a battery cell according to an embodiment. Fig. 15B is a perspective view of a battery cell assembly according to an embodiment.
[0117] Reference Fig. 12A , Fig. 12B and / or Fig.13 , the battery device 1100 may include a battery cell assembly 1101 and a housing 1102. The battery device 1100 may be referred to as a battery module, a battery pack, or a power storage device.
[0118] The battery cell assembly 1101 may include a plurality of battery cells (eg Figure 1 In an embodiment, the battery cell assembly 1101 may be referred to as a battery stack.
[0119] The housing 1102 may accommodate the battery cell assembly 1101. For example, the housing 1102 may provide an accommodation space for accommodating the battery cell assembly 1101. In an embodiment, the housing 1102 may be referred to as a module housing or a battery pack housing.
[0120] According to an embodiment, the housing 1102 may include a bottom member 1102b supporting a bottom surface of the battery cell assembly 1101 and a sidewall member 1102a extending from the bottom member 1102b. The shape of the housing 1102 may be selectively changed according to the design of the battery device 1100.
[0121] According to an embodiment, the battery device 1100 may include a bus bar (not shown) connected to the battery cells 100 .
[0122] The battery cell 100 may include an electrode assembly (eg Figure 1 jelly roll 106), a cover assembly (e.g. Figure 2A A cover assembly 120 in the embodiment of the present invention and a can 104 for accommodating the electrode assembly.
[0123] right 9A to 9ETank 104, FIG. 10A to FIG. 10F Tank 104 and / or FIG. 11A to FIG. 11E The description of tank 104 may be applied to FIG. 12A to FIG. 1 5 of 104 cans.
[0124] For example, the reinforced region 900 of the tank 104 and the support region 1000 of the tank 104 may refer to a portion of the tank 104 having the thickness or shape of a conventional tank 104 .
[0125] The support area 1000 may be 9A to 9E The ironing areas 910a, 910b, 910c, FIG. 10A to FIG. 10F The support area 1020, and / or FIG. 11A to FIG. 11E Support area 1020.
[0126] The reinforced area 900 may be 9A to 9E The reinforced regions 1010a, 1010b and 1010c, FIG. 10A to FIG. 10F Support rods 920a, 920b and 920c, and / or FIG. 11A to FIG. 11E Reinforced covers 930a, 930b and 930c.
[0127] Each part of the tank 104 may have a different thickness. For example, the tank 104 may include a reinforcement area 900 and a support area 1000. The reinforcement area 900 may be disposed on the support area 1000. The reinforcement area 900 disposed on the support area 1000 may refer to a shape extending from the support area 1000 and / or a structure coupled to the support area 1000 by bonding or the like.
[0128] The support region 1000 may have a first thickness W1. The reinforcement region 900 may have a second thickness W2 different from the first thickness W1. The second thickness W2 may be greater than the first thickness W1. According to an embodiment, the thickness of the support region 1000 may be substantially the same as the thickness of the conventional can 104 that accommodates the electrode assembly. The reinforcement region 900 is thicker than the conventional can 104, and thus the strength and durability of the can 104 may be improved.
[0129] According to an embodiment, the battery device 1100 may include a heat dissipation space S. The heat dissipation space S may be an empty space located between the support regions 1000 of the plurality of battery cells 100. For example, the reinforcement region 900 may protrude from the support region 1000. Due to the protrusion of the reinforcement region 1000, an empty space may be formed between the plurality of support regions 1000. The heat dissipation space S may provide a path through which a fluid (e.g., air) flows. In an embodiment, the heat dissipation space S may be referred to as a heat dissipation channel.
[0130] According to an embodiment, the battery device 1100 may include a heat dissipation member 1103. The heat dissipation member 1103 may be attached to the can 104. For example, the heat dissipation member 1103 may be disposed on the support area 1000 of the can 104. In an embodiment, the heat dissipation member 1103 may be located in the heat dissipation space S. In an embodiment, the heat dissipation member 1103 may include a thermal interface material (TIM).
[0131] According to an embodiment, the battery device 1100 may include a thermal adhesive 1104 for connecting the battery cell assembly 1101 to the housing 1102. The thermal adhesive 1104 may be located between the battery cell assembly 1101 and the housing 1102. For example, the thermal adhesive 1104 may be provided between the lower surface of the can 104 and the bottom member 1102b of the housing 1102.
[0132] The shape of the can 104 may be designed in various ways. For example, if the reinforced area 900 can form the heat dissipation space S or improve the strength of the can 104, the structure of the can 104 may be changed.
[0133] According to the embodiments (e.g. Fig. 12A and Fig. 12B ), the reinforcement area 900 may include a first protrusion 901 and a second protrusion 902 extending in the same direction from the outer surface of the support area 1000. For example, the first protrusion 901 may protrude from one end or edge of one surface 1000a of the support area 1000 in the first direction (+X direction). The second protrusion 902 may protrude from the other end or edge of one surface 1000a of the support area 1000 in the first direction.
[0134] According to the embodiments (e.g. Fig.13 ), the reinforcement area 900 may include a third protrusion 903 and a fourth protrusion 904 extending from the outer surface of the support area 1000 in different directions. For example, the support area 1000 may include a first outer surface 1000a in a first direction (+X direction) and a second outer surface 1000b in a second direction (-X direction) opposite to the first direction (+X direction). The third protrusion 903 may protrude from a first end (e.g., one end in the +Y direction) of the first outer surface 1000a in the first direction (+X direction). The fourth protrusion 904 may protrude from a second end (e.g., one end in the -Y direction) of the second outer surface 1000b in the second direction (-X direction). According to an embodiment, the housing 1102 may have a shape corresponding to the reinforcement area 900. For example, the housing 1102 may include a protrusion 1102c protruding with a size corresponding to the protrusions 903 and 904.
[0135] According to the embodiments (e.g. Fig.14), the reinforcement area 900 may include a plurality of protrusions 905a and 905b protruding from two directions of the support area 1000. For example, the support area 1000 may include a first outer surface 1000a in a first direction (+X direction) and a second outer surface 1000b in a second direction (-X direction) opposite to the first direction (+X direction). The reinforcement area 900 may include a fifth protrusion 905a protruding from both ends of the first outer surface 1000a in the first direction (+X direction) and a sixth protrusion 905b protruding from both ends of the second outer surface 1000b in the second direction (-X direction).
[0136] According to the embodiments (e.g. Fig.15A and Fig. 15B ), the reinforcement area 900 may include a plurality of protrusions 906 and 907 protruding from two directions of the support area 1000. For example, the support area 1000 may include a first outer surface 1000a in a first direction (+X direction) and a second outer surface 1000b in a second direction (-X direction).
[0137] The reinforcement area 900 may include a seventh protrusion 906 and an eighth protrusion 907, which may be connected to each other. The eighth protrusion 907 may include a groove 907a for accommodating the seventh protrusion 906 and a protrusion member 907b forming the groove 907a. The seventh protrusion 906 may be inserted into the groove 907a.
[0138] According to the embodiments (e.g. Fig.15A ), the reinforcement region 900 may include a seventh protrusion 906 protruding from the second end of the first outer surface 1000a (the end toward the -Y direction) and the first end of the second outer surface 1000b (the end toward the +Y direction), and an eighth protrusion 907 protruding from the first end of the first outer surface 1000a (the end toward the +Y direction) and the second end of the second outer surface 1000b (the end toward the -Y direction).
[0139] According to the embodiments (e.g. Fig. 15B ), the reinforcement region 900 may include a seventh protrusion 906 protruding from both ends of the first outer surface 1000a along the first direction (+X direction) and an eighth protrusion 907 protruding from both ends of the second outer surface 1000b along the second direction (-X direction).
[0140] As described above, according to the present disclosure, a battery cell includes a housing having a reinforced region, and the durability of the battery cell can be improved by the reinforced region.
[0141] A heat dissipation space can be formed by strengthening the area. Due to the existence of the heat dissipation space, the heat dissipation performance of the battery cell can be improved.
[0142] The functions performed in the processes and methods may be implemented in different orders. In addition, the steps and operations outlined are provided only as examples, and some steps and operations may be optional, may be combined into fewer steps and operations, or may be expanded into additional steps and operations without departing from the essence of the disclosed embodiments.
Claims
1. A battery cell, comprising: Electrode assembly; as well as a housing accommodating the electrode assembly, The invention is characterized in that the shell comprises a support area surrounding at least a portion of the electrode assembly and a reinforcement area arranged on the support area.
2. The battery cell according to claim 1, characterized in that: The support area includes an ironing area formed by an ironing process, and The first thickness of the ironing area is smaller than the second thickness of the reinforcement area.
3. The battery cell according to claim 1, characterized in that: The reinforcement region includes at least one support rod connected to the support region.
4. The battery cell according to claim 1, characterized in that: The reinforcement region is connected to the support region and includes a reinforcement cover having a plurality of protrusions and a plurality of grooves.
5. The battery cell according to claim 1, characterized in that: The housing includes a wide surface, a narrow surface, and a corner portion between the wide surface and the narrow surface, and The reinforced area is provided on at least one of the wide surface, the narrow surface, and the corner.
6. A battery device comprising: A battery cell assembly, comprising a plurality of battery cells; as well as A housing for accommodating the battery cell assembly, It is characterized in that Each of the plurality of battery cells includes an electrode assembly and a casing accommodating the electrode assembly. The housing includes a support region surrounding at least a portion of the electrode assembly and a reinforcement region disposed on the support region, The cell assembly includes a heat dissipation space between the support areas of the plurality of battery cells.
7. The battery device according to claim 6, characterized in that: The support area includes an ironing area formed by an ironing process, The first thickness of the ironing area is smaller than the second thickness of the reinforcement area.
8. The battery device according to claim 6, characterized in that: The reinforcement region comprises at least one support rod connected to the support region.
9. The battery device according to claim 6, characterized in that: The reinforcement region is connected to the support region and includes a reinforcement cover having a plurality of protrusions and a plurality of grooves.
10. The battery device according to claim 6, characterized in that: Further including: A heat dissipation member is attached to the support area and is located in the heat dissipation space.
11. The battery device according to claim 6, characterized in that: Further including: A thermal adhesive connects the battery cell assembly and the housing.
12. The battery device according to claim 6, characterized in that: The reinforcement region includes a first protrusion extending from an outer surface of the support region in a first direction and a second protrusion extending from the outer surface of the support region in the first direction.
13. The battery device according to claim 6, characterized in that: The reinforcement region includes a third protrusion extending from a first end of a first outer surface of the support region in a first direction and a fourth protrusion extending from a second end of a second outer surface of the support region in a second direction, the second direction being opposite to the first direction, The third protrusion is located at the first end of the housing, and The fourth protrusion is located at a second end of the housing opposite to the first end.
14. The battery device according to claim 6, characterized in that: The reinforced areas include: a plurality of fifth protrusions extending from the first outer surface of the support region in a first direction; and A plurality of sixth protrusions extend from the second outer surface of the support region in a second direction, wherein the second direction is opposite to the first direction.
15. The battery device according to claim 14, characterized in that: The reinforced areas include: a seventh protrusion including an insertion portion; and An eighth protrusion in which a groove for receiving the insertion portion is formed.